Elapsed Time, Volts/Count, Torch On, Arc Good, Voltage Control, THC Up, THC Down, Set Point, Current Voltage
8344, V, 0, 0, 0, 0, 0, 704, 52
8344, V, 0, 0, 0, 0, 0, 704, 52
8601, V, 0, 0, 0, 0, 0, 704, 52
8601, V, 0, 0, 0, 0, 0, 704, 52
8858, V, 0, 0, 0, 0, 0, 704, 52
8858, V, 0, 0, 0, 0, 0, 704, 52
9115, V, 0, 0, 0, 0, 0, 704, 52
9115, V, 0, 0, 0, 0, 0, 704, 52
9372, V, 0, 0, 0, 0, 0, 704, 52
9372, V, 0, 0, 0, 0, 0, 704, 52
9629, V, 0, 0, 0, 0, 0, 704, 52
9629, V, 0, 0, 0, 0, 0, 704, 52
9886, V, 0, 0, 0, 0, 0, 704, 52
9886, V, 0, 0, 0, 0, 0, 704, 52
10143, V, 0, 0, 0, 0, 0, 704, 52
10143, V, 0, 0, 0, 0, 0, 704, 52
10400, V, 0, 0, 0, 0, 0, 704, 52
10400, V, 0, 0, 0, 0, 0, 704, 52
10657, V, 0, 0, 0, 0, 0, 704, 52
10657, V, 0, 0, 0, 0, 0, 704, 52
10914, V, 0, 0, 0, 0, 0, 704, 52
10914, V, 0, 0, 0, 0, 0, 704, 52
11171, V, 0, 0, 0, 0, 0, 704, 52
11171, V, 0, 0, 0, 0, 0, 704, 52
11428, V, 0, 0, 0, 0, 0, 704, 52
11428, V, 0, 0, 0, 0, 0, 704, 52
11685, V, 0, 0, 0, 0, 0, 704, 52
11685, V, 0, 0, 0, 0, 0, 704, 52
11942, V, 0, 0, 0, 0, 0, 704, 52
11942, V, 0, 0, 0, 0, 0, 704, 52
12199, V, 0, 0, 0, 0, 0, 704, 52
12199, V, 0, 0, 0, 0, 0, 704, 52
12456, V, 0, 0, 0, 0, 0, 704, 52
12456, V, 0, 0, 0, 0, 0, 704, 52
12713, V, 0, 0, 0, 0, 0, 704, 52
12713, V, 0, 0, 0, 0, 0, 704, 52
12971, V, 0, 0, 0, 0, 0, 704, 52
12971, V, 0, 0, 0, 0, 0, 704, 52
13228, V, 0, 0, 0, 0, 0, 704, 52
13228, V, 0, 0, 0, 0, 0, 704, 52
13485, V, 0, 0, 0, 0, 0, 704, 52
13485, V, 0, 0, 0, 0, 0, 704, 52
13742, V, 0, 0, 0, 0, 0, 704, 52
13742, V, 0, 0, 0, 0, 0, 704, 52
13999, V, 0, 0, 0, 0, 0, 704, 52
13999, V, 0, 0, 0, 0, 0, 704, 52
14256, V, 0, 0, 0, 0, 0, 704, 52
14256, V, 0, 0, 0, 0, 0, 704, 52
14513, V, 0, 0, 0, 0, 0, 704, 52
14513, V, 0, 0, 0, 0, 0, 704, 52
14770, V, 0, 0, 0, 0, 0, 704, 52
14770, V, 0, 0, 0, 0, 0, 704, 52
15027, V, 0, 0, 0, 0, 0, 704, 52
15027, V, 0, 0, 0, 0, 0, 704, 52
15284, V, 0, 0, 0, 0, 0, 704, 52
15284, V, 0, 0, 0, 0, 0, 704, 52
15541, V, 0, 0, 0, 0, 0, 704, 52
15541, V, 0, 0, 0, 0, 0, 704, 52
15798, V, 0, 0, 0, 0, 0, 704, 52
15798, V, 0, 0, 0, 0, 0, 704, 52
16055, V, 0, 0, 0, 0, 0, 704, 52
16055, V, 0, 0, 0, 0, 0, 704, 52
16312, V, 0, 0, 0, 0, 0, 704, 52
16312, V, 0, 0, 0, 0, 0, 704, 52
16569, V, 0, 0, 0, 0, 0, 704, 52
16569, V, 0, 0, 0, 0, 0, 704, 52
16826, V, 0, 0, 0, 0, 0, 704, 52
16826, V, 0, 0, 0, 0, 0, 704, 52
17083, V, 0, 0, 0, 0, 0, 704, 52
17083, V, 0, 0, 0, 0, 0, 704, 52
17340, V, 0, 0, 0, 0, 0, 704, 52
17340, V, 0, 0, 0, 0, 0, 704, 52
17597, V, 0, 0, 0, 0, 0, 704, 52
17597, V, 0, 0, 0, 0, 0, 704, 52
17854, V, 0, 0, 0, 0, 0, 704, 52
17854, V, 0, 0, 0, 0, 0, 704, 52
18111, V, 0, 0, 0, 0, 0, 704, 52
18111, V, 0, 0, 0, 0, 0, 704, 52
18368, V, 0, 0, 0, 0, 0, 704, 52
18368, V, 0, 0, 0, 0, 0, 704, 52
18625, V, 0, 0, 0, 0, 0, 704, 52
18625, V, 0, 0, 0, 0, 0, 704, 52
18882, V, 0, 0, 0, 0, 0, 704, 52
18882, V, 0, 0, 0, 0, 0, 704, 52
19139, V, 0, 0, 0, 0, 0, 704, 52
19139, V, 0, 0, 0, 0, 0, 704, 52
19396, V, 0, 0, 0, 0, 0, 704, 52
19396, V, 0, 0, 0, 0, 0, 704, 52
19653, V, 0, 0, 0, 0, 0, 704, 52
19653, V, 0, 0, 0, 0, 0, 704, 52
19910, V, 0, 0, 0, 0, 0, 704, 52
19910, V, 0, 0, 0, 0, 0, 704, 52
20167, V, 0, 0, 0, 0, 0, 704, 52
20167, V, 0, 0, 0, 0, 0, 704, 52
20424, V, 0, 0, 0, 0, 0, 704, 52
20424, V, 0, 0, 0, 0, 0, 704, 52
20681, V, 0, 0, 0, 0, 0, 704, 52
20681, V, 0, 0, 0, 0, 0, 704, 52
20938, V, 0, 0, 0, 0, 0, 704, 52
20938, V, 0, 0, 0, 0, 0, 704, 52
21195, V, 0, 0, 0, 0, 0, 704, 52
21195, V, 0, 0, 0, 0, 0, 704, 52
21452, V, 0, 0, 0, 0, 0, 704, 52
21452, V, 0, 0, 0, 0, 0, 704, 52
21709, V, 0, 0, 0, 0, 0, 704, 52
21709, V, 0, 0, 0, 0, 0, 704, 52
21966, V, 0, 0, 0, 0, 0, 704, 52
21966, V, 0, 0, 0, 0, 0, 704, 52
22223, V, 0, 0, 0, 0, 0, 704, 52
22223, V, 0, 0, 0, 0, 0, 704, 52
22480, V, 0, 0, 0, 0, 0, 704, 51
22480, V, 0, 0, 0, 0, 0, 704, 51
22737, V, 0, 0, 0, 0, 0, 704, 51
22737, V, 0, 0, 0, 0, 0, 704, 51
22994, V, 0, 0, 0, 0, 0, 704, 51
22994, V, 0, 0, 0, 0, 0, 704, 51
23251, V, 0, 0, 0, 0, 0, 704, 51
23251, V, 0, 0, 0, 0, 0, 704, 51
23508, V, 0, 0, 0, 0, 0, 704, 51
23508, V, 0, 0, 0, 0, 0, 704, 51
23766, V, 0, 0, 0, 0, 0, 704, 51
23766, V, 0, 0, 0, 0, 0, 704, 51
24023, V, 0, 0, 0, 0, 0, 704, 13
24023, V, 0, 0, 0, 0, 0, 704, 13
24280, V, 0, 0, 0, 0, 0, 704, 51
24280, V, 0, 0, 0, 0, 0, 704, 51
24537, V, 0, 0, 0, 0, 0, 704, 52
24537, V, 0, 0, 0, 0, 0, 704, 52
24670, V, 1, 0, 0, 0, 0, 704, 52
24671, V, 1, 0, 0, 0, 0, 704, 52
24672, V, 1, 0, 0, 0, 0, 704, 52
24673, V, 1, 0, 0, 0, 0, 704, 52
24674, V, 1, 0, 0, 0, 0, 704, 52
24675, V, 1, 0, 0, 0, 0, 704, 52
24676, V, 1, 0, 0, 0, 0, 704, 52
24677, V, 1, 0, 0, 0, 0, 704, 52
24678, V, 1, 0, 0, 0, 0, 704, 52
24679, V, 1, 0, 0, 0, 0, 704, 52
24680, V, 1, 0, 0, 0, 0, 704, 52
24681, V, 1, 0, 0, 0, 0, 704, 52
24682, V, 1, 0, 0, 0, 0, 704, 52
24683, V, 1, 0, 0, 0, 0, 704, 52
24684, V, 1, 0, 0, 0, 0, 704, 52
24685, V, 1, 0, 0, 0, 0, 704, 52
24686, V, 1, 0, 0, 0, 0, 704, 52
24687, V, 1, 0, 0, 0, 0, 704, 52
24688, V, 1, 0, 0, 0, 0, 704, 52
24689, V, 1, 0, 0, 0, 0, 704, 52
24690, V, 1, 0, 0, 0, 0, 704, 52
24691, V, 1, 0, 0, 0, 0, 704, 52
24692, V, 1, 0, 0, 0, 0, 704, 52
24693, V, 1, 0, 0, 0, 0, 704, 52
24694, V, 1, 0, 0, 0, 0, 704, 52
24695, V, 1, 0, 0, 0, 0, 704, 52
24696, V, 1, 0, 0, 0, 0, 704, 52
24697, V, 1, 0, 0, 0, 0, 704, 52
24698, V, 1, 0, 0, 0, 0, 704, 52
24699, V, 1, 0, 0, 0, 0, 704, 52
24700, V, 1, 0, 0, 0, 0, 704, 52
24701, V, 1, 0, 0, 0, 0, 704, 52
24702, V, 1, 0, 0, 0, 0, 704, 52
24704, V, 1, 0, 0, 0, 0, 704, 52
24705, V, 1, 0, 0, 0, 0, 704, 52
24706, V, 1, 0, 0, 0, 0, 704, 52
24707, V, 1, 0, 0, 0, 0, 704, 52
24708, V, 1, 0, 0, 0, 0, 704, 52
24709, V, 1, 0, 0, 0, 0, 704, 52
24710, V, 1, 0, 0, 0, 0, 704, 52
24711, V, 1, 0, 0, 0, 0, 704, 52
24712, V, 1, 0, 0, 0, 0, 704, 52
24713, V, 1, 0, 0, 0, 0, 704, 53
24714, V, 1, 0, 0, 0, 0, 704, 52
24715, V, 1, 0, 0, 0, 0, 704, 52
24716, V, 1, 0, 0, 0, 0, 704, 52
24717, V, 1, 0, 0, 0, 0, 704, 52
24718, V, 1, 0, 0, 0, 0, 704, 52
24719, V, 1, 0, 0, 0, 0, 704, 53
24720, V, 1, 0, 0, 0, 0, 704, 52
24721, V, 1, 0, 0, 0, 0, 704, 52
24722, V, 1, 0, 0, 0, 0, 704, 52
24723, V, 1, 0, 0, 0, 0, 704, 53
24724, V, 1, 0, 0, 0, 0, 704, 53
24725, V, 1, 0, 0, 0, 0, 704, 53
24726, V, 1, 0, 0, 0, 0, 704, 52
24727, V, 1, 0, 0, 0, 0, 704, 53
24728, V, 1, 0, 0, 0, 0, 704, 53
24729, V, 1, 0, 0, 0, 0, 704, 53
24730, V, 1, 0, 0, 0, 0, 704, 53
24731, V, 1, 0, 0, 0, 0, 704, 53
24732, V, 1, 0, 0, 0, 0, 704, 53
24733, V, 1, 0, 0, 0, 0, 704, 53
24734, V, 1, 0, 0, 0, 0, 704, 53
24735, V, 1, 0, 0, 0, 0, 704, 53
24736, V, 1, 0, 0, 0, 0, 704, 53
24737, V, 1, 0, 0, 0, 0, 704, 53
24738, V, 1, 0, 0, 0, 0, 704, 53
24739, V, 1, 0, 0, 0, 0, 704, 53
24740, V, 1, 0, 0, 0, 0, 704, 53
24741, V, 1, 0, 0, 0, 0, 704, 53
24742, V, 1, 0, 0, 0, 0, 704, 53
24743, V, 1, 0, 0, 0, 0, 704, 53
24744, V, 1, 0, 0, 0, 0, 704, 53
24745, V, 1, 0, 0, 0, 0, 704, 53
24747, V, 1, 0, 0, 0, 0, 704, 53
24748, V, 1, 0, 0, 0, 0, 704, 53
24749, V, 1, 0, 0, 0, 0, 704, 53
24750, V, 1, 0, 0, 0, 0, 704, 53
24751, V, 1, 0, 0, 0, 0, 704, 53
24752, V, 1, 0, 0, 0, 0, 704, 53
24753, V, 1, 0, 0, 0, 0, 704, 53
24754, V, 1, 0, 0, 0, 0, 704, 53
24755, V, 1, 0, 0, 0, 0, 704, 53
24756, V, 1, 0, 0, 0, 0, 704, 53
24757, V, 1, 0, 0, 0, 0, 704, 53
24758, V, 1, 0, 0, 0, 0, 704, 53
24759, V, 1, 0, 0, 0, 0, 704, 53
24760, V, 1, 0, 0, 0, 0, 704, 53
24761, V, 1, 0, 0, 0, 0, 704, 53
24762, V, 1, 0, 0, 0, 0, 704, 53
24763, V, 1, 0, 0, 0, 0, 704, 53
24764, V, 1, 0, 0, 0, 0, 704, 53
24765, V, 1, 0, 0, 0, 0, 704, 53
24766, V, 1, 0, 0, 0, 0, 704, 53
24767, V, 1, 0, 0, 0, 0, 704, 53
24768, V, 1, 0, 0, 0, 0, 704, 53
24769, V, 1, 0, 0, 0, 0, 704, 53
24770, V, 1, 0, 0, 0, 0, 704, 53
24771, V, 1, 0, 0, 0, 0, 704, 53
24772, V, 1, 0, 0, 0, 0, 704, 53
24773, V, 1, 0, 0, 0, 0, 704, 53
24774, V, 1, 0, 0, 0, 0, 704, 53
24775, V, 1, 0, 0, 0, 0, 704, 53
24776, V, 1, 0, 0, 0, 0, 704, 53
24777, V, 1, 0, 0, 0, 0, 704, 53
24778, V, 1, 0, 0, 0, 0, 704, 53
24779, V, 1, 0, 0, 0, 0, 704, 53
24780, V, 1, 0, 0, 0, 0, 704, 53
24781, V, 1, 0, 0, 0, 0, 704, 53
24782, V, 1, 0, 0, 0, 0, 704, 53
24783, V, 1, 0, 0, 0, 0, 704, 53
24784, V, 1, 0, 0, 0, 0, 704, 53
24785, V, 1, 0, 0, 0, 0, 704, 53
24786, V, 1, 0, 0, 0, 0, 704, 53
24787, V, 1, 0, 0, 0, 0, 704, 53
24788, V, 1, 0, 0, 0, 0, 704, 53
24790, V, 1, 0, 0, 0, 0, 704, 53
24791, V, 1, 0, 0, 0, 0, 704, 53
24792, V, 1, 0, 0, 0, 0, 704, 53
24793, V, 1, 0, 0, 0, 0, 704, 53
24794, V, 1, 0, 0, 0, 0, 704, 53
24795, V, 1, 0, 0, 0, 0, 704, 53
24796, V, 1, 0, 0, 0, 0, 704, 53
24797, V, 1, 0, 0, 0, 0, 704, 53
24798, V, 1, 0, 0, 0, 0, 704, 53
24799, V, 1, 0, 0, 0, 0, 704, 53
24800, V, 1, 0, 0, 0, 0, 704, 53
24801, V, 1, 0, 0, 0, 0, 704, 53
24802, V, 1, 0, 0, 0, 0, 704, 53
24803, V, 1, 0, 0, 0, 0, 704, 53
24804, V, 1, 0, 0, 0, 0, 704, 53
24805, V, 1, 0, 0, 0, 0, 704, 53
24806, V, 1, 0, 0, 0, 0, 704, 53
24807, V, 1, 0, 0, 0, 0, 704, 53
24808, V, 1, 0, 0, 0, 0, 704, 53
24809, V, 1, 0, 0, 0, 0, 704, 53
24810, V, 1, 0, 0, 0, 0, 704, 53
24811, V, 1, 0, 0, 0, 0, 704, 53
24812, V, 1, 0, 0, 0, 0, 704, 53
24813, V, 1, 0, 0, 0, 0, 704, 53
24814, V, 1, 0, 0, 0, 0, 704, 53
24815, V, 1, 0, 0, 0, 0, 704, 53
24816, V, 1, 0, 0, 0, 0, 704, 53
24817, V, 1, 0, 0, 0, 0, 704, 53
24818, V, 1, 0, 0, 0, 0, 704, 53
24819, V, 1, 0, 0, 0, 0, 704, 53
24820, V, 1, 0, 0, 0, 0, 704, 53
24821, V, 1, 0, 0, 0, 0, 704, 53
24822, V, 1, 0, 0, 0, 0, 704, 53
24823, V, 1, 0, 0, 0, 0, 704, 53
24824, V, 1, 0, 0, 0, 0, 704, 53
24825, V, 1, 0, 0, 0, 0, 704, 53
24826, V, 1, 0, 0, 0, 0, 704, 53
24827, V, 1, 0, 0, 0, 0, 704, 53
24828, V, 1, 0, 0, 0, 0, 704, 53
24829, V, 1, 0, 0, 0, 0, 704, 53
24830, V, 1, 0, 0, 0, 0, 704, 53
24832, V, 1, 0, 0, 0, 0, 704, 53
24833, V, 1, 0, 0, 0, 0, 704, 53
24834, V, 1, 0, 0, 0, 0, 704, 53
24835, V, 1, 0, 0, 0, 0, 704, 53
24836, V, 1, 0, 0, 0, 0, 704, 53
24837, V, 1, 0, 0, 0, 0, 704, 53
24838, V, 1, 0, 0, 0, 0, 704, 53
24839, V, 1, 0, 0, 0, 0, 704, 53
24840, V, 1, 0, 0, 0, 0, 704, 53
24841, V, 1, 0, 0, 0, 0, 704, 53
24842, V, 1, 0, 0, 0, 0, 704, 53
24843, V, 1, 0, 0, 0, 0, 704, 53
24844, V, 1, 0, 0, 0, 0, 704, 53
24845, V, 1, 0, 0, 0, 0, 704, 53
24846, V, 1, 0, 0, 0, 0, 704, 53
24847, V, 1, 0, 0, 0, 0, 704, 53
24848, V, 1, 0, 0, 0, 0, 704, 53
24849, V, 1, 0, 0, 0, 0, 704, 53
24850, V, 1, 0, 0, 0, 0, 704, 53
24851, V, 1, 0, 0, 0, 0, 704, 53
24852, V, 1, 0, 0, 0, 0, 704, 53
24853, V, 1, 0, 0, 0, 0, 704, 53
24854, V, 1, 0, 0, 0, 0, 704, 53
24855, V, 1, 0, 0, 0, 0, 704, 53
24856, V, 1, 0, 0, 0, 0, 704, 53
24857, V, 1, 0, 0, 0, 0, 704, 53
24858, V, 1, 0, 0, 0, 0, 704, 53
24859, V, 1, 0, 0, 0, 0, 704, 53
24860, V, 1, 0, 0, 0, 0, 704, 53
24861, V, 1, 0, 0, 0, 0, 704, 53
24862, V, 1, 0, 0, 0, 0, 704, 53
24863, V, 1, 0, 0, 0, 0, 704, 53
24864, V, 1, 0, 0, 0, 0, 704, 53
24865, V, 1, 0, 0, 0, 0, 704, 53
24866, V, 1, 0, 0, 0, 0, 704, 53
24867, V, 1, 0, 0, 0, 0, 704, 53
24868, V, 1, 0, 0, 0, 0, 704, 53
24869, V, 1, 0, 0, 0, 0, 704, 53
24870, V, 1, 0, 0, 0, 0, 704, 53
24871, V, 1, 0, 0, 0, 0, 704, 53
24872, V, 1, 0, 0, 0, 0, 704, 53
24873, V, 1, 0, 0, 0, 0, 704, 53
24875, V, 1, 0, 0, 0, 0, 704, 53
24876, V, 1, 0, 0, 0, 0, 704, 53
24877, V, 1, 0, 0, 0, 0, 704, 53
24878, V, 1, 0, 0, 0, 0, 704, 53
24879, V, 1, 0, 0, 0, 0, 704, 53
24880, V, 1, 0, 0, 0, 0, 704, 53
24881, V, 1, 0, 0, 0, 0, 704, 53
24882, V, 1, 0, 0, 0, 0, 704, 53
24883, V, 1, 0, 0, 0, 0, 704, 53
24884, V, 1, 0, 0, 0, 0, 704, 53
24885, V, 1, 0, 0, 0, 0, 704, 53
24886, V, 1, 0, 0, 0, 0, 704, 53
24887, V, 1, 0, 0, 0, 0, 704, 53
24888, V, 1, 0, 0, 0, 0, 704, 53
24889, V, 1, 0, 0, 0, 0, 704, 53
24890, V, 1, 0, 0, 0, 0, 704, 53
24891, V, 1, 0, 0, 0, 0, 704, 53
24892, V, 1, 0, 0, 0, 0, 704, 53
24893, V, 1, 0, 0, 0, 0, 704, 53
24894, V, 1, 0, 0, 0, 0, 704, 53
24895, V, 1, 0, 0, 0, 0, 704, 53
24896, V, 1, 0, 0, 0, 0, 704, 53
24897, V, 1, 0, 0, 0, 0, 704, 53
24898, V, 1, 0, 0, 0, 0, 704, 53
24899, V, 1, 0, 0, 0, 0, 704, 53
24900, V, 1, 0, 0, 0, 0, 704, 53
24901, V, 1, 0, 0, 0, 0, 704, 53
24902, V, 1, 0, 0, 0, 0, 704, 53
24903, V, 1, 0, 0, 0, 0, 704, 53
24904, V, 1, 0, 0, 0, 0, 704, 53
24905, V, 1, 0, 0, 0, 0, 704, 53
24906, V, 1, 0, 0, 0, 0, 704, 53
24907, V, 1, 0, 0, 0, 0, 704, 53
24908, V, 1, 0, 0, 0, 0, 704, 53
24909, V, 1, 0, 0, 0, 0, 704, 53
24910, V, 1, 0, 0, 0, 0, 704, 53
24911, V, 1, 0, 0, 0, 0, 704, 53
24912, V, 1, 0, 0, 0, 0, 704, 53
24913, V, 1, 0, 0, 0, 0, 704, 53
24914, V, 1, 0, 0, 0, 0, 704, 53
24915, V, 1, 0, 0, 0, 0, 704, 53
24916, V, 1, 0, 0, 0, 0, 704, 53
24918, V, 1, 0, 0, 0, 0, 704, 53
24919, V, 1, 0, 0, 0, 0, 704, 53
24920, V, 1, 0, 0, 0, 0, 704, 53
24921, V, 1, 0, 0, 0, 0, 704, 53
24922, V, 1, 0, 0, 0, 0, 704, 53
24923, V, 1, 0, 0, 0, 0, 704, 53
24924, V, 1, 0, 0, 0, 0, 704, 53
24925, V, 1, 0, 0, 0, 0, 704, 53
24926, V, 1, 0, 0, 0, 0, 704, 53
24927, V, 1, 0, 0, 0, 0, 704, 53
24928, V, 1, 0, 0, 0, 0, 704, 53
24929, V, 1, 0, 0, 0, 0, 704, 53
24930, V, 1, 0, 0, 0, 0, 704, 53
24931, V, 1, 0, 0, 0, 0, 704, 53
24932, V, 1, 0, 0, 0, 0, 704, 53
24933, V, 1, 0, 0, 0, 0, 704, 53
24934, V, 1, 0, 0, 0, 0, 704, 53
24935, V, 1, 0, 0, 0, 0, 704, 53
24936, V, 1, 0, 0, 0, 0, 704, 53
24937, V, 1, 0, 0, 0, 0, 704, 53
24938, V, 1, 0, 0, 0, 0, 704, 53
24939, V, 1, 0, 0, 0, 0, 704, 53
24940, V, 1, 0, 0, 0, 0, 704, 53
24941, V, 1, 0, 0, 0, 0, 704, 53
24942, V, 1, 0, 0, 0, 0, 704, 53
24943, V, 1, 0, 0, 0, 0, 704, 53
24944, V, 1, 0, 0, 0, 0, 704, 53
24945, V, 1, 0, 0, 0, 0, 704, 53
24946, V, 1, 0, 0, 0, 0, 704, 53
24947, V, 1, 0, 0, 0, 0, 704, 53
24948, V, 1, 0, 0, 0, 0, 704, 53
24949, V, 1, 0, 0, 0, 0, 704, 53
24950, V, 1, 0, 0, 0, 0, 704, 53
24951, V, 1, 0, 0, 0, 0, 704, 53
24952, V, 1, 0, 0, 0, 0, 704, 53
24953, V, 1, 0, 0, 0, 0, 704, 53
24954, V, 1, 0, 0, 0, 0, 704, 53
24955, V, 1, 0, 0, 0, 0, 704, 53
24956, V, 1, 0, 0, 0, 0, 704, 53
24957, V, 1, 0, 0, 0, 0, 704, 53
24958, V, 1, 0, 0, 0, 0, 704, 53
24960, V, 1, 0, 0, 0, 0, 704, 53
24961, V, 1, 0, 0, 0, 0, 704, 53
24962, V, 1, 0, 0, 0, 0, 704, 53
24963, V, 1, 0, 0, 0, 0, 704, 53
24964, V, 1, 0, 0, 0, 0, 704, 53
24965, V, 1, 0, 0, 0, 0, 704, 53
24966, V, 1, 0, 0, 0, 0, 704, 53
24967, V, 1, 0, 0, 0, 0, 704, 53
24968, V, 1, 0, 0, 0, 0, 704, 53
24969, V, 1, 0, 0, 0, 0, 704, 53
24970, V, 1, 0, 0, 0, 0, 704, 53
24971, V, 1, 0, 0, 0, 0, 704, 53
24972, V, 1, 0, 0, 0, 0, 704, 53
24973, V, 1, 0, 0, 0, 0, 704, 53
24974, V, 1, 0, 0, 0, 0, 704, 53
24975, V, 1, 0, 0, 0, 0, 704, 53
24976, V, 1, 0, 0, 0, 0, 704, 53
24977, V, 1, 0, 0, 0, 0, 704, 53
24978, V, 1, 0, 0, 0, 0, 704, 53
24979, V, 1, 0, 0, 0, 0, 704, 53
24980, V, 1, 0, 0, 0, 0, 704, 53
24981, V, 1, 0, 0, 0, 0, 704, 53
24982, V, 1, 0, 0, 0, 0, 704, 53
24983, V, 1, 0, 0, 0, 0, 704, 53
24984, V, 1, 0, 0, 0, 0, 704, 53
24985, V, 1, 0, 0, 0, 0, 704, 53
24986, V, 1, 0, 0, 0, 0, 704, 53
24987, V, 1, 0, 0, 0, 0, 704, 53
24988, V, 1, 0, 0, 0, 0, 704, 53
24989, V, 1, 0, 0, 0, 0, 704, 53
24990, V, 1, 0, 0, 0, 0, 704, 53
24991, V, 1, 0, 0, 0, 0, 704, 53
24992, V, 1, 0, 0, 0, 0, 704, 53
24993, V, 1, 0, 0, 0, 0, 704, 53
24994, V, 1, 0, 0, 0, 0, 704, 53
24995, V, 1, 0, 0, 0, 0, 704, 53
24996, V, 1, 0, 0, 0, 0, 704, 53
24997, V, 1, 0, 0, 0, 0, 704, 53
24998, V, 1, 0, 0, 0, 0, 704, 53
24999, V, 1, 0, 0, 0, 0, 704, 53
25000, V, 1, 0, 0, 0, 0, 704, 53
25001, V, 1, 0, 0, 0, 0, 704, 53
25003, V, 1, 0, 0, 0, 0, 704, 53
25004, V, 1, 0, 0, 0, 0, 704, 53
25005, V, 1, 0, 0, 0, 0, 704, 53
25006, V, 1, 0, 0, 0, 0, 704, 53
25007, V, 1, 0, 0, 0, 0, 704, 53
25008, V, 1, 0, 0, 0, 0, 704, 53
25009, V, 1, 0, 0, 0, 0, 704, 53
25010, V, 1, 0, 0, 0, 0, 704, 53
25011, V, 1, 0, 0, 0, 0, 704, 53
25012, V, 1, 0, 0, 0, 0, 704, 53
25013, V, 1, 0, 0, 0, 0, 704, 53
25014, V, 1, 0, 0, 0, 0, 704, 53
25015, V, 1, 0, 0, 0, 0, 704, 53
25016, V, 1, 0, 0, 0, 0, 704, 53
25017, V, 1, 0, 0, 0, 0, 704, 53
25018, V, 1, 0, 0, 0, 0, 704, 53
25019, V, 1, 0, 0, 0, 0, 704, 53
25020, V, 1, 0, 0, 0, 0, 704, 53
25021, V, 1, 0, 0, 0, 0, 704, 53
25022, V, 1, 0, 0, 0, 0, 704, 53
25023, V, 1, 0, 0, 0, 0, 704, 53
25024, V, 1, 0, 0, 0, 0, 704, 53
25025, V, 1, 0, 0, 0, 0, 704, 53
25026, V, 1, 0, 0, 0, 0, 704, 53
25027, V, 1, 0, 0, 0, 0, 704, 53
25028, V, 1, 0, 0, 0, 0, 704, 53
25029, V, 1, 0, 0, 0, 0, 704, 53
25030, V, 1, 0, 0, 0, 0, 704, 53
25031, V, 1, 0, 0, 0, 0, 704, 53
25032, V, 1, 0, 0, 0, 0, 704, 53
25033, V, 1, 0, 0, 0, 0, 704, 53
25034, V, 1, 0, 0, 0, 0, 704, 53
25035, V, 1, 0, 0, 0, 0, 704, 53
25036, V, 1, 0, 0, 0, 0, 704, 53
25037, V, 1, 0, 0, 0, 0, 704, 53
25038, V, 1, 0, 0, 0, 0, 704, 53
25039, V, 1, 0, 0, 0, 0, 704, 53
25040, V, 1, 0, 0, 0, 0, 704, 53
25041, V, 1, 0, 0, 0, 0, 704, 53
25042, V, 1, 0, 0, 0, 0, 704, 53
25043, V, 1, 0, 0, 0, 0, 704, 53
25044, V, 1, 0, 0, 0, 0, 704, 53
25046, V, 1, 0, 0, 0, 0, 704, 53
25047, V, 1, 0, 0, 0, 0, 704, 53
25048, V, 1, 0, 0, 0, 0, 704, 53
25049, V, 1, 0, 0, 0, 0, 704, 53
25050, V, 1, 0, 0, 0, 0, 704, 53
25051, V, 1, 0, 0, 0, 0, 704, 53
25052, V, 1, 0, 0, 0, 0, 704, 53
25053, V, 1, 0, 0, 0, 0, 704, 53
25054, V, 1, 0, 0, 0, 0, 704, 53
25055, V, 1, 0, 0, 0, 0, 704, 53
25056, V, 1, 0, 0, 0, 0, 704, 53
25057, V, 1, 0, 0, 0, 0, 704, 53
25058, V, 1, 0, 0, 0, 0, 704, 53
25059, V, 1, 0, 0, 0, 0, 704, 53
25060, V, 1, 0, 0, 0, 0, 704, 53
25061, V, 1, 0, 0, 0, 0, 704, 53
25062, V, 1, 0, 0, 0, 0, 704, 53
25063, V, 1, 0, 0, 0, 0, 704, 53
25064, V, 1, 0, 0, 0, 0, 704, 53
25065, V, 1, 0, 0, 0, 0, 704, 53
25066, V, 1, 0, 0, 0, 0, 704, 53
25067, V, 1, 0, 0, 0, 0, 704, 53
25068, V, 1, 0, 0, 0, 0, 704, 53
25069, V, 1, 0, 0, 0, 0, 704, 53
25070, V, 1, 0, 0, 0, 0, 704, 53
25071, V, 1, 0, 0, 0, 0, 704, 53
25072, V, 1, 0, 0, 0, 0, 704, 53
25073, V, 1, 0, 0, 0, 0, 704, 53
25074, V, 1, 0, 0, 0, 0, 704, 53
25075, V, 1, 0, 0, 0, 0, 704, 53
25076, V, 1, 0, 0, 0, 0, 704, 53
25077, V, 1, 0, 0, 0, 0, 704, 53
25078, V, 1, 0, 0, 0, 0, 704, 53
25079, V, 1, 0, 0, 0, 0, 704, 53
25080, V, 1, 0, 0, 0, 0, 704, 53
25081, V, 1, 0, 0, 0, 0, 704, 53
25082, V, 1, 0, 0, 0, 0, 704, 53
25083, V, 1, 0, 0, 0, 0, 704, 53
25084, V, 1, 0, 0, 0, 0, 704, 53
25085, V, 1, 0, 0, 0, 0, 704, 53
25086, V, 1, 0, 0, 0, 0, 704, 53
25088, V, 1, 0, 0, 0, 0, 704, 53
25089, V, 1, 0, 0, 0, 0, 704, 53
25090, V, 1, 0, 0, 0, 0, 704, 53
25091, V, 1, 0, 0, 0, 0, 704, 53
25092, V, 1, 0, 0, 0, 0, 704, 53
25093, V, 1, 0, 0, 0, 0, 704, 53
25094, V, 1, 0, 0, 0, 0, 704, 53
25095, V, 1, 0, 0, 0, 0, 704, 53
25096, V, 1, 0, 0, 0, 0, 704, 53
25097, V, 1, 0, 0, 0, 0, 704, 53
25098, V, 1, 0, 0, 0, 0, 704, 53
25099, V, 1, 0, 0, 0, 0, 704, 53
25100, V, 1, 0, 0, 0, 0, 704, 53
25101, V, 1, 0, 0, 0, 0, 704, 53
25102, V, 1, 0, 0, 0, 0, 704, 53
25103, V, 1, 0, 0, 0, 0, 704, 53
25104, V, 1, 0, 0, 0, 0, 704, 53
25105, V, 1, 0, 0, 0, 0, 704, 53
25106, V, 1, 0, 0, 0, 0, 704, 53
25107, V, 1, 0, 0, 0, 0, 704, 53
25108, V, 1, 0, 0, 0, 0, 704, 53
25109, V, 1, 0, 0, 0, 0, 704, 53
25110, V, 1, 0, 0, 0, 0, 704, 53
25111, V, 1, 0, 0, 0, 0, 704, 53
25112, V, 1, 0, 0, 0, 0, 704, 53
25113, V, 1, 0, 0, 0, 0, 704, 53
25114, V, 1, 0, 0, 0, 0, 704, 53
25115, V, 1, 0, 0, 0, 0, 704, 53
25116, V, 1, 0, 0, 0, 0, 704, 53
25117, V, 1, 0, 0, 0, 0, 704, 53
25118, V, 1, 0, 0, 0, 0, 704, 53
25119, V, 1, 0, 0, 0, 0, 704, 53
25120, V, 1, 0, 0, 0, 0, 704, 53
25121, V, 1, 0, 0, 0, 0, 704, 53
25122, V, 1, 0, 0, 0, 0, 704, 53
25123, V, 1, 0, 0, 0, 0, 704, 53
25124, V, 1, 0, 0, 0, 0, 704, 53
25125, V, 1, 0, 0, 0, 0, 704, 53
25126, V, 1, 0, 0, 0, 0, 704, 53
25127, V, 1, 0, 0, 0, 0, 704, 53
25128, V, 1, 0, 0, 0, 0, 704, 53
25129, V, 1, 0, 0, 0, 0, 704, 53
25131, V, 1, 0, 0, 0, 0, 704, 53
25132, V, 1, 0, 0, 0, 0, 704, 53
25133, V, 1, 0, 0, 0, 0, 704, 53
25134, V, 1, 0, 0, 0, 0, 704, 53
25135, V, 1, 0, 0, 0, 0, 704, 53
25136, V, 1, 0, 0, 0, 0, 704, 53
25137, V, 1, 0, 0, 0, 0, 704, 53
25138, V, 1, 0, 0, 0, 0, 704, 53
25139, V, 1, 0, 0, 0, 0, 704, 53
25140, V, 1, 0, 0, 0, 0, 704, 53
25141, V, 1, 0, 0, 0, 0, 704, 53
25142, V, 1, 0, 0, 0, 0, 704, 53
25143, V, 1, 0, 0, 0, 0, 704, 53
25144, V, 1, 0, 0, 0, 0, 704, 53
25145, V, 1, 0, 0, 0, 0, 704, 53
25146, V, 1, 0, 0, 0, 0, 704, 53
25147, V, 1, 0, 0, 0, 0, 704, 53
25148, V, 1, 0, 0, 0, 0, 704, 53
25149, V, 1, 0, 0, 0, 0, 704, 53
25150, V, 1, 0, 0, 0, 0, 704, 53
25151, V, 1, 0, 0, 0, 0, 704, 53
25152, V, 1, 0, 0, 0, 0, 704, 53
25153, V, 1, 0, 0, 0, 0, 704, 53
25154, V, 1, 0, 0, 0, 0, 704, 53
25155, V, 1, 0, 0, 0, 0, 704, 53
25156, V, 1, 0, 0, 0, 0, 704, 53
25157, V, 1, 0, 0, 0, 0, 704, 53
25158, V, 1, 0, 0, 0, 0, 704, 53
25159, V, 1, 0, 0, 0, 0, 704, 53
25160, V, 1, 0, 0, 0, 0, 704, 53
25161, V, 1, 0, 0, 0, 0, 704, 53
25162, V, 1, 0, 0, 0, 0, 704, 53
25163, V, 1, 0, 0, 0, 0, 704, 53
25164, V, 1, 0, 0, 0, 0, 704, 53
25165, V, 1, 0, 0, 0, 0, 704, 53
25166, V, 1, 0, 0, 0, 0, 704, 53
25167, V, 1, 0, 0, 0, 0, 704, 53
25168, V, 1, 0, 0, 0, 0, 704, 53
25169, V, 1, 0, 0, 0, 0, 704, 53
25170, V, 1, 0, 0, 0, 0, 704, 53
25171, V, 1, 0, 0, 0, 0, 704, 53
25172, V, 1, 0, 0, 0, 0, 704, 53
25174, V, 1, 0, 0, 0, 0, 704, 53
25175, V, 1, 0, 0, 0, 0, 704, 53
25176, V, 1, 0, 0, 0, 0, 704, 53
25177, V, 1, 0, 0, 0, 0, 704, 53
25178, V, 1, 0, 0, 0, 0, 704, 53
25179, V, 1, 0, 0, 0, 0, 704, 53
25180, V, 1, 0, 0, 0, 0, 704, 53
25181, V, 1, 0, 0, 0, 0, 704, 53
25182, V, 1, 0, 0, 0, 0, 704, 53
25183, V, 1, 0, 0, 0, 0, 704, 53
25184, V, 1, 0, 0, 0, 0, 704, 53
25185, V, 1, 0, 0, 0, 0, 704, 53
25186, V, 1, 0, 0, 0, 0, 704, 53
25187, V, 1, 0, 0, 0, 0, 704, 53
25188, V, 1, 0, 0, 0, 0, 704, 53
25189, V, 1, 0, 0, 0, 0, 704, 53
25190, V, 1, 0, 0, 0, 0, 704, 53
25191, V, 1, 0, 0, 0, 0, 704, 53
25192, V, 1, 0, 0, 0, 0, 704, 53
25193, V, 1, 0, 0, 0, 0, 704, 53
25194, V, 1, 0, 0, 0, 0, 704, 53
25195, V, 1, 0, 0, 0, 0, 704, 53
25196, V, 1, 0, 0, 0, 0, 704, 53
25197, V, 1, 0, 0, 0, 0, 704, 53
25198, V, 1, 0, 0, 0, 0, 704, 53
25199, V, 1, 0, 0, 0, 0, 704, 53
25200, V, 1, 0, 0, 0, 0, 704, 53
25201, V, 1, 0, 0, 0, 0, 704, 53
25202, V, 1, 0, 0, 0, 0, 704, 53
25203, V, 1, 0, 0, 0, 0, 704, 53
25204, V, 1, 0, 0, 0, 0, 704, 53
25205, V, 1, 0, 0, 0, 0, 704, 53
25206, V, 1, 0, 0, 0, 0, 704, 53
25207, V, 1, 0, 0, 0, 0, 704, 53
25208, V, 1, 0, 0, 0, 0, 704, 53
25209, V, 1, 0, 0, 0, 0, 704, 53
25210, V, 1, 0, 0, 0, 0, 704, 53
25211, V, 1, 0, 0, 0, 0, 704, 53
25212, V, 1, 0, 0, 0, 0, 704, 53
25213, V, 1, 0, 0, 0, 0, 704, 53
25214, V, 1, 0, 0, 0, 0, 704, 53
25216, V, 1, 0, 0, 0, 0, 704, 53
25217, V, 1, 0, 0, 0, 0, 704, 53
25218, V, 1, 0, 0, 0, 0, 704, 53
25219, V, 1, 0, 0, 0, 0, 704, 53
25220, V, 1, 0, 0, 0, 0, 704, 53
25221, V, 1, 0, 0, 0, 0, 704, 53
25222, V, 1, 0, 0, 0, 0, 704, 53
25223, V, 1, 0, 0, 0, 0, 704, 53
25224, V, 1, 0, 0, 0, 0, 704, 53
25225, V, 1, 0, 0, 0, 0, 704, 53
25226, V, 1, 0, 0, 0, 0, 704, 53
25227, V, 1, 0, 0, 0, 0, 704, 53
25228, V, 1, 0, 0, 0, 0, 704, 53
25229, V, 1, 0, 0, 0, 0, 704, 53
25230, V, 1, 0, 0, 0, 0, 704, 53
25231, V, 1, 0, 0, 0, 0, 704, 53
25232, V, 1, 0, 0, 0, 0, 704, 53
25233, V, 1, 0, 0, 0, 0, 704, 53
25234, V, 1, 0, 0, 0, 0, 704, 53
25235, V, 1, 0, 0, 0, 0, 704, 53
25236, V, 1, 0, 0, 0, 0, 704, 53
25237, V, 1, 0, 0, 0, 0, 704, 53
25238, V, 1, 0, 0, 0, 0, 704, 53
25239, V, 1, 0, 0, 0, 0, 704, 53
25240, V, 1, 0, 0, 0, 0, 704, 53
25241, V, 1, 0, 0, 0, 0, 704, 53
25242, V, 1, 0, 0, 0, 0, 704, 53
25243, V, 1, 0, 0, 0, 0, 704, 53
25244, V, 1, 0, 0, 0, 0, 704, 53
25245, V, 1, 0, 0, 0, 0, 704, 53
25246, V, 1, 0, 0, 0, 0, 704, 53
25247, V, 1, 0, 0, 0, 0, 704, 53
25248, V, 1, 0, 0, 0, 0, 704, 53
25249, V, 1, 0, 0, 0, 0, 704, 53
25250, V, 1, 0, 0, 0, 0, 704, 53
25251, V, 1, 0, 0, 0, 0, 704, 53
25252, V, 1, 0, 0, 0, 0, 704, 53
25253, V, 1, 0, 0, 0, 0, 704, 53
25254, V, 1, 0, 0, 0, 0, 704, 53
25255, V, 1, 0, 0, 0, 0, 704, 53
25256, V, 1, 0, 0, 0, 0, 704, 53
25257, V, 1, 0, 0, 0, 0, 704, 53
25259, V, 1, 0, 0, 0, 0, 704, 53
25260, V, 1, 0, 0, 0, 0, 704, 53
25261, V, 1, 0, 0, 0, 0, 704, 53
25262, V, 1, 0, 0, 0, 0, 704, 53
25263, V, 1, 0, 0, 0, 0, 704, 53
25264, V, 1, 0, 0, 0, 0, 704, 53
25265, V, 1, 0, 0, 0, 0, 704, 53
25266, V, 1, 0, 0, 0, 0, 704, 53
25267, V, 1, 0, 0, 0, 0, 704, 53
25268, V, 1, 0, 0, 0, 0, 704, 53
25269, V, 1, 0, 0, 0, 0, 704, 53
25270, V, 1, 0, 0, 0, 0, 704, 53
25271, V, 1, 0, 0, 0, 0, 704, 53
25272, V, 1, 0, 0, 0, 0, 704, 53
25273, V, 1, 0, 0, 0, 0, 704, 54
25274, V, 1, 0, 0, 0, 0, 704, 54
25275, V, 1, 0, 0, 0, 0, 704, 54
25276, V, 1, 0, 0, 0, 0, 704, 54
25277, V, 1, 0, 0, 0, 0, 704, 54
25278, V, 1, 0, 0, 0, 0, 704, 54
25279, V, 1, 0, 0, 0, 0, 704, 54
25280, V, 1, 0, 0, 0, 0, 704, 54
25281, V, 1, 0, 0, 0, 0, 704, 54
25282, V, 1, 0, 0, 0, 0, 704, 54
25283, V, 1, 0, 0, 0, 0, 704, 54
25284, V, 1, 0, 0, 0, 0, 704, 54
25285, V, 1, 0, 0, 0, 0, 704, 54
25286, V, 1, 0, 0, 0, 0, 704, 54
25287, V, 1, 0, 0, 0, 0, 704, 54
25288, V, 1, 0, 0, 0, 0, 704, 54
25289, V, 1, 0, 0, 0, 0, 704, 54
25290, V, 1, 0, 0, 0, 0, 704, 54
25291, V, 1, 0, 0, 0, 0, 704, 54
25292, V, 1, 0, 0, 0, 0, 704, 54
25293, V, 1, 0, 0, 0, 0, 704, 54
25294, V, 1, 0, 0, 0, 0, 704, 54
25295, V, 1, 0, 0, 0, 0, 704, 54
25296, V, 1, 0, 0, 0, 0, 704, 54
25297, V, 1, 0, 0, 0, 0, 704, 54
25298, V, 1, 0, 0, 0, 0, 704, 54
25299, V, 1, 0, 0, 0, 0, 704, 54
25300, V, 1, 0, 0, 0, 0, 704, 54
25302, V, 1, 0, 0, 0, 0, 704, 54
25303, V, 1, 0, 0, 0, 0, 704, 54
25304, V, 1, 0, 0, 0, 0, 704, 54
25305, V, 1, 0, 0, 0, 0, 704, 54
25306, V, 1, 0, 0, 0, 0, 704, 54
25307, V, 1, 0, 0, 0, 0, 704, 54
25308, V, 1, 0, 0, 0, 0, 704, 54
25309, V, 1, 0, 0, 0, 0, 704, 54
25310, V, 1, 0, 0, 0, 0, 704, 54
25311, V, 1, 0, 0, 0, 0, 704, 54
25312, V, 1, 0, 0, 0, 0, 704, 54
25313, V, 1, 0, 0, 0, 0, 704, 54
25314, V, 1, 0, 0, 0, 0, 704, 54
25315, V, 1, 0, 0, 0, 0, 704, 54
25316, V, 1, 0, 0, 0, 0, 704, 54
25317, V, 1, 0, 0, 0, 0, 704, 54
25318, V, 1, 0, 0, 0, 0, 704, 54
25319, V, 1, 0, 0, 0, 0, 704, 54
25320, V, 1, 0, 0, 0, 0, 704, 54
25321, V, 1, 0, 0, 0, 0, 704, 54
25322, V, 1, 0, 0, 0, 0, 704, 54
25323, V, 1, 0, 0, 0, 0, 704, 54
25324, V, 1, 0, 0, 0, 0, 704, 55
25325, V, 1, 0, 0, 0, 0, 704, 55
25326, V, 1, 0, 0, 0, 0, 704, 55
25327, V, 1, 0, 0, 0, 0, 704, 55
25328, V, 1, 0, 0, 0, 0, 704, 55
25329, V, 1, 0, 0, 0, 0, 704, 55
25330, V, 1, 0, 0, 0, 0, 704, 55
25331, V, 1, 0, 0, 0, 0, 704, 54
25332, V, 1, 0, 0, 0, 0, 704, 55
25333, V, 1, 0, 0, 0, 0, 704, 55
25334, V, 1, 0, 0, 0, 0, 704, 55
25335, V, 1, 0, 0, 0, 0, 704, 55
25336, V, 1, 0, 0, 0, 0, 704, 55
25337, V, 1, 0, 0, 0, 0, 704, 55
25338, V, 1, 0, 0, 0, 0, 704, 55
25339, V, 1, 0, 0, 0, 0, 704, 55
25340, V, 1, 0, 0, 0, 0, 704, 55
25341, V, 1, 0, 0, 0, 0, 704, 55
25342, V, 1, 0, 0, 0, 0, 704, 55
25344, V, 1, 0, 0, 0, 0, 704, 55
25345, V, 1, 0, 0, 0, 0, 704, 55
25346, V, 1, 0, 0, 0, 0, 704, 55
25347, V, 1, 0, 0, 0, 0, 704, 55
25348, V, 1, 0, 0, 0, 0, 704, 55
25349, V, 1, 0, 0, 0, 0, 704, 55
25350, V, 1, 0, 0, 0, 0, 704, 55
25351, V, 1, 0, 0, 0, 0, 704, 55
25352, V, 1, 0, 0, 0, 0, 704, 55
25353, V, 1, 0, 0, 0, 0, 704, 55
25354, V, 1, 0, 0, 0, 0, 704, 55
25355, V, 1, 0, 0, 0, 0, 704, 55
25356, V, 1, 0, 0, 0, 0, 704, 55
25357, V, 1, 0, 0, 0, 0, 704, 55
25358, V, 1, 0, 0, 0, 0, 704, 55
25359, V, 1, 0, 0, 0, 0, 704, 55
25360, V, 1, 0, 0, 0, 0, 704, 55
25361, V, 1, 0, 0, 0, 0, 704, 55
25362, V, 1, 0, 0, 0, 0, 704, 55
25363, V, 1, 0, 0, 0, 0, 704, 55
25364, V, 1, 0, 0, 0, 0, 704, 55
25365, V, 1, 0, 0, 0, 0, 704, 55
25366, V, 1, 0, 0, 0, 0, 704, 55
25367, V, 1, 0, 0, 0, 0, 704, 55
25368, V, 1, 0, 0, 0, 0, 704, 55
25369, V, 1, 0, 0, 0, 0, 704, 55
25370, V, 1, 0, 0, 0, 0, 704, 55
25371, V, 1, 0, 0, 0, 0, 704, 55
25372, V, 1, 0, 0, 0, 0, 704, 55
25373, V, 1, 0, 0, 0, 0, 704, 55
25374, V, 1, 0, 0, 0, 0, 704, 55
25375, V, 1, 0, 0, 0, 0, 704, 55
25376, V, 1, 0, 0, 0, 0, 704, 55
25377, V, 1, 0, 0, 0, 0, 704, 55
25378, V, 1, 0, 0, 0, 0, 704, 55
25379, V, 1, 0, 0, 0, 0, 704, 55
25380, V, 1, 0, 0, 0, 0, 704, 55
25381, V, 1, 0, 0, 0, 0, 704, 55
25382, V, 1, 0, 0, 0, 0, 704, 55
25383, V, 1, 0, 0, 0, 0, 704, 55
25384, V, 1, 0, 0, 0, 0, 704, 55
25385, V, 1, 0, 0, 0, 0, 704, 55
25387, V, 1, 0, 0, 0, 0, 704, 55
25388, V, 1, 0, 0, 0, 0, 704, 55
25389, V, 1, 0, 0, 0, 0, 704, 55
25390, V, 1, 0, 0, 0, 0, 704, 55
25391, V, 1, 0, 0, 0, 0, 704, 55
25392, V, 1, 0, 0, 0, 0, 704, 55
25393, V, 1, 0, 0, 0, 0, 704, 55
25394, V, 1, 0, 0, 0, 0, 704, 55
25395, V, 1, 0, 0, 0, 0, 704, 55
25396, V, 1, 0, 0, 0, 0, 704, 55
25397, V, 1, 0, 0, 0, 0, 704, 55
25398, V, 1, 0, 0, 0, 0, 704, 55
25399, V, 1, 0, 0, 0, 0, 704, 55
25400, V, 1, 0, 0, 0, 0, 704, 55
25401, V, 1, 0, 0, 0, 0, 704, 55
25402, V, 1, 0, 0, 0, 0, 704, 55
25403, V, 1, 0, 0, 0, 0, 704, 55
25404, V, 1, 0, 0, 0, 0, 704, 55
25405, V, 1, 0, 0, 0, 0, 704, 55
25406, V, 1, 0, 0, 0, 0, 704, 55
25407, V, 1, 0, 0, 0, 0, 704, 55
25408, V, 1, 0, 0, 0, 0, 704, 55
25409, V, 1, 0, 0, 0, 0, 704, 55
25410, V, 1, 0, 0, 0, 0, 704, 55
25411, V, 1, 0, 0, 0, 0, 704, 55
25412, V, 1, 0, 0, 0, 0, 704, 55
25413, V, 1, 0, 0, 0, 0, 704, 55
25414, V, 1, 0, 0, 0, 0, 704, 55
25415, V, 1, 0, 0, 0, 0, 704, 55
25416, V, 1, 0, 0, 0, 0, 704, 55
25417, V, 1, 0, 0, 0, 0, 704, 55
25418, V, 1, 0, 0, 0, 0, 704, 55
25419, V, 1, 0, 0, 0, 0, 704, 55
25420, V, 1, 0, 0, 0, 0, 704, 55
25421, V, 1, 0, 0, 0, 0, 704, 55
25422, V, 1, 0, 0, 0, 0, 704, 55
25423, V, 1, 0, 0, 0, 0, 704, 55
25424, V, 1, 0, 0, 0, 0, 704, 55
25425, V, 1, 0, 0, 0, 0, 704, 55
25426, V, 1, 0, 0, 0, 0, 704, 55
25427, V, 1, 0, 0, 0, 0, 704, 55
25428, V, 1, 0, 0, 0, 0, 704, 55
25430, V, 1, 0, 0, 0, 0, 704, 55
25431, V, 1, 0, 0, 0, 0, 704, 55
25432, V, 1, 0, 0, 0, 0, 704, 55
25433, V, 1, 0, 0, 0, 0, 704, 55
25434, V, 1, 0, 0, 0, 0, 704, 56
25435, V, 1, 0, 0, 0, 0, 704, 56
25436, V, 1, 0, 0, 0, 0, 704, 56
25437, V, 1, 0, 0, 0, 0, 704, 56
25438, V, 1, 0, 0, 0, 0, 704, 56
25439, V, 1, 0, 0, 0, 0, 704, 56
25440, V, 1, 0, 0, 0, 0, 704, 56
25441, V, 1, 0, 0, 0, 0, 704, 56
25442, V, 1, 0, 0, 0, 0, 704, 56
25443, V, 1, 0, 0, 0, 0, 704, 56
25444, V, 1, 0, 0, 0, 0, 704, 56
25445, V, 1, 0, 0, 0, 0, 704, 56
25446, V, 1, 0, 0, 0, 0, 704, 56
25447, V, 1, 0, 0, 0, 0, 704, 56
25448, V, 1, 0, 0, 0, 0, 704, 56
25449, V, 1, 0, 0, 0, 0, 704, 56
25450, V, 1, 0, 0, 0, 0, 704, 56
25451, V, 1, 0, 0, 0, 0, 704, 56
25452, V, 1, 0, 0, 0, 0, 704, 56
25453, V, 1, 0, 0, 0, 0, 704, 56
25454, V, 1, 0, 0, 0, 0, 704, 56
25455, V, 1, 0, 0, 0, 0, 704, 56
25456, V, 1, 0, 0, 0, 0, 704, 56
25457, V, 1, 0, 0, 0, 0, 704, 56
25458, V, 1, 0, 0, 0, 0, 704, 56
25459, V, 1, 0, 0, 0, 0, 704, 56
25460, V, 1, 0, 0, 0, 0, 704, 56
25461, V, 1, 0, 0, 0, 0, 704, 56
25462, V, 1, 0, 0, 0, 0, 704, 56
25463, V, 1, 0, 0, 0, 0, 704, 56
25464, V, 1, 0, 0, 0, 0, 704, 56
25465, V, 1, 0, 0, 0, 0, 704, 56
25466, V, 1, 0, 0, 0, 0, 704, 56
25467, V, 1, 0, 0, 0, 0, 704, 56
25468, V, 1, 0, 0, 0, 0, 704, 56
25469, V, 1, 0, 0, 0, 0, 704, 56
25470, V, 1, 0, 0, 0, 0, 704, 57
25472, V, 1, 0, 0, 0, 0, 704, 56
25473, V, 1, 0, 0, 0, 0, 704, 56
25474, V, 1, 0, 0, 0, 0, 704, 57
25475, V, 1, 0, 0, 0, 0, 704, 57
25476, V, 1, 0, 0, 0, 0, 704, 57
25477, V, 1, 0, 0, 0, 0, 704, 57
25478, V, 1, 0, 0, 0, 0, 704, 57
25479, V, 1, 0, 0, 0, 0, 704, 57
25480, V, 1, 0, 0, 0, 0, 704, 57
25481, V, 1, 0, 0, 0, 0, 704, 57
25482, V, 1, 0, 0, 0, 0, 704, 57
25483, V, 1, 0, 0, 0, 0, 704, 57
25484, V, 1, 0, 0, 0, 0, 704, 57
25485, V, 1, 0, 0, 0, 0, 704, 58
25486, V, 1, 0, 0, 0, 0, 704, 58
25487, V, 1, 0, 0, 0, 0, 704, 58
25488, V, 1, 0, 0, 0, 0, 704, 58
25489, V, 1, 0, 0, 0, 0, 704, 59
25490, V, 1, 0, 0, 0, 0, 704, 59
25491, V, 1, 0, 0, 0, 0, 704, 59
25492, V, 1, 0, 0, 0, 0, 704, 59
25493, V, 1, 0, 0, 0, 0, 704, 60
25494, V, 1, 0, 0, 0, 0, 704, 60
25495, V, 1, 0, 0, 0, 0, 704, 60
25496, V, 1, 0, 0, 0, 0, 704, 60
25497, V, 1, 0, 0, 0, 0, 704, 60
25498, V, 1, 0, 0, 0, 0, 704, 61
25499, V, 1, 0, 0, 0, 0, 704, 61
25500, V, 1, 0, 0, 0, 0, 704, 61
25501, V, 1, 0, 0, 0, 0, 704, 61
25502, V, 1, 0, 0, 0, 0, 704, 61
25503, V, 1, 0, 0, 0, 0, 704, 62
25504, V, 1, 0, 0, 0, 0, 704, 62
25505, V, 1, 0, 0, 0, 0, 704, 62
25506, V, 1, 0, 0, 0, 0, 704, 62
25507, V, 1, 0, 0, 0, 0, 704, 62
25508, V, 1, 0, 0, 0, 0, 704, 62
25509, V, 1, 0, 0, 0, 0, 704, 62
25510, V, 1, 0, 0, 0, 0, 704, 63
25511, V, 1, 0, 0, 0, 0, 704, 63
25512, V, 1, 0, 0, 0, 0, 704, 63
25513, V, 1, 0, 0, 0, 0, 704, 63
25515, V, 1, 0, 0, 0, 0, 704, 63
25516, V, 1, 0, 0, 0, 0, 704, 63
25517, V, 1, 0, 0, 0, 0, 704, 64
25518, V, 1, 0, 0, 0, 0, 704, 64
25519, V, 1, 0, 0, 0, 0, 704, 64
25520, V, 1, 0, 0, 0, 0, 704, 64
25521, V, 1, 0, 0, 0, 0, 704, 64
25522, V, 1, 0, 0, 0, 0, 704, 64
25523, V, 1, 0, 0, 0, 0, 704, 64
25524, V, 1, 0, 0, 0, 0, 704, 65
25525, V, 1, 0, 0, 0, 0, 704, 65
25526, V, 1, 0, 0, 0, 0, 704, 65
25527, V, 1, 0, 0, 0, 0, 704, 65
25528, V, 1, 0, 0, 0, 0, 704, 65
25529, V, 1, 0, 0, 0, 0, 704, 65
25530, V, 1, 0, 0, 0, 0, 704, 65
25531, V, 1, 0, 0, 0, 0, 704, 65
25532, V, 1, 0, 0, 0, 0, 704, 65
25533, V, 1, 0, 0, 0, 0, 704, 66
25534, V, 1, 0, 0, 0, 0, 704, 66
25535, V, 1, 0, 0, 0, 0, 704, 66
25536, V, 1, 0, 0, 0, 0, 704, 66
25537, V, 1, 0, 0, 0, 0, 704, 66
25538, V, 1, 0, 0, 0, 0, 704, 66
25539, V, 1, 0, 0, 0, 0, 704, 66
25540, V, 1, 0, 0, 0, 0, 704, 66
25541, V, 1, 0, 0, 0, 0, 704, 66
25542, V, 1, 0, 0, 0, 0, 704, 66
25543, V, 1, 0, 0, 0, 0, 704, 67
25544, V, 1, 0, 0, 0, 0, 704, 67
25545, V, 1, 0, 0, 0, 0, 704, 67
25546, V, 1, 0, 0, 0, 0, 704, 67
25547, V, 1, 0, 0, 0, 0, 704, 67
25548, V, 1, 0, 0, 0, 0, 704, 67
25549, V, 1, 0, 0, 0, 0, 704, 67
25550, V, 1, 0, 0, 0, 0, 704, 67
25551, V, 1, 0, 0, 0, 0, 704, 67
25552, V, 1, 0, 0, 0, 0, 704, 67
25553, V, 1, 0, 0, 0, 0, 704, 67
25554, V, 1, 0, 0, 0, 0, 704, 68
25555, V, 1, 0, 0, 0, 0, 704, 68
25556, V, 1, 0, 0, 0, 0, 704, 68
25558, V, 1, 0, 0, 0, 0, 704, 68
25559, V, 1, 0, 0, 0, 0, 704, 68
25560, V, 1, 0, 0, 0, 0, 704, 68
25561, V, 1, 0, 0, 0, 0, 704, 68
25562, V, 1, 0, 0, 0, 0, 704, 68
25563, V, 1, 0, 0, 0, 0, 704, 68
25564, V, 1, 0, 0, 0, 0, 704, 68
25565, V, 1, 0, 0, 0, 0, 704, 68
25566, V, 1, 0, 0, 0, 0, 704, 68
25567, V, 1, 0, 0, 0, 0, 704, 68
25568, V, 1, 0, 0, 0, 0, 704, 69
25569, V, 1, 0, 0, 0, 0, 704, 69
25570, V, 1, 0, 0, 0, 0, 704, 69
25571, V, 1, 0, 0, 0, 0, 704, 69
25572, V, 1, 0, 0, 0, 0, 704, 69
25573, V, 1, 1, 0, 0, 0, 704, 69
25573, V, 1, 1, 0, 0, 0, 704, 69
25574, V, 1, 0, 0, 0, 0, 704, 69
25574, V, 1, 0, 0, 0, 0, 704, 69
25575, V, 1, 0, 0, 0, 0, 704, 69
25576, V, 1, 0, 0, 0, 0, 704, 69
25577, V, 1, 0, 0, 0, 0, 704, 69
25578, V, 1, 0, 0, 0, 0, 704, 69
25579, V, 1, 0, 0, 0, 0, 704, 70
25580, V, 1, 0, 0, 0, 0, 704, 70
25581, V, 1, 0, 0, 0, 0, 704, 70
25582, V, 1, 0, 0, 0, 0, 704, 70
25583, V, 1, 0, 0, 0, 0, 704, 70
25584, V, 1, 0, 0, 0, 0, 704, 70
25585, V, 1, 0, 0, 0, 0, 704, 70
25586, V, 1, 0, 0, 0, 0, 704, 70
25587, V, 1, 0, 0, 0, 0, 704, 70
25588, V, 1, 0, 0, 0, 0, 704, 70
25589, V, 1, 1, 0, 0, 0, 704, 70
25589, V, 1, 1, 0, 0, 0, 704, 70
25590, V, 1, 0, 0, 0, 0, 704, 70
25590, V, 1, 0, 0, 0, 0, 704, 70
25591, V, 1, 0, 0, 0, 0, 704, 70
25592, V, 1, 0, 0, 0, 0, 704, 70
25593, V, 1, 0, 0, 0, 0, 704, 71
25594, V, 1, 0, 0, 0, 0, 704, 71
25595, V, 1, 0, 0, 0, 0, 704, 71
25596, V, 1, 0, 0, 0, 0, 704, 71
25597, V, 1, 0, 0, 0, 0, 704, 71
25598, V, 1, 0, 0, 0, 0, 704, 71
25600, V, 1, 0, 0, 0, 0, 704, 71
25601, V, 1, 0, 0, 0, 0, 704, 71
25602, V, 1, 0, 0, 0, 0, 704, 71
25603, V, 1, 1, 0, 0, 0, 704, 71
25603, V, 1, 1, 0, 0, 0, 704, 71
25604, V, 1, 0, 0, 0, 0, 704, 71
25604, V, 1, 0, 0, 0, 0, 704, 71
25605, V, 1, 0, 0, 0, 0, 704, 71
25606, V, 1, 0, 0, 0, 0, 704, 71
25607, V, 1, 0, 0, 0, 0, 704, 71
25608, V, 1, 0, 0, 0, 0, 704, 71
25609, V, 1, 0, 0, 0, 0, 704, 72
25610, V, 1, 0, 0, 0, 0, 704, 72
25611, V, 1, 0, 0, 0, 0, 704, 72
25612, V, 1, 0, 0, 0, 0, 704, 72
25613, V, 1, 0, 0, 0, 0, 704, 72
25614, V, 1, 0, 0, 0, 0, 704, 72
25615, V, 1, 0, 0, 0, 0, 704, 72
25616, V, 1, 0, 0, 0, 0, 704, 72
25617, V, 1, 0, 0, 0, 0, 704, 72
25618, V, 1, 0, 0, 0, 0, 704, 72
25619, V, 1, 0, 0, 0, 0, 704, 72
25620, V, 1, 0, 0, 0, 0, 704, 72
25621, V, 1, 0, 0, 0, 0, 704, 72
25622, V, 1, 0, 0, 0, 0, 704, 72
25623, V, 1, 0, 0, 0, 0, 704, 72
25624, V, 1, 0, 0, 0, 0, 704, 72
25625, V, 1, 0, 0, 0, 0, 704, 72
25626, V, 1, 0, 0, 0, 0, 704, 72
25627, V, 1, 1, 0, 0, 0, 704, 72
25627, V, 1, 1, 0, 0, 0, 704, 72
25628, V, 1, 0, 0, 0, 0, 704, 72
25628, V, 1, 0, 0, 0, 0, 704, 72
25629, V, 1, 0, 0, 0, 0, 704, 72
25630, V, 1, 0, 0, 0, 0, 704, 72
25631, V, 1, 0, 0, 0, 0, 704, 72
25632, V, 1, 0, 0, 0, 0, 704, 72
25633, V, 1, 0, 0, 0, 0, 704, 72
25634, V, 1, 0, 0, 0, 0, 704, 73
25635, V, 1, 0, 0, 0, 0, 704, 73
25636, V, 1, 0, 0, 0, 0, 704, 73
25637, V, 1, 0, 0, 0, 0, 704, 73
25638, V, 1, 0, 0, 0, 0, 704, 73
25639, V, 1, 0, 0, 0, 0, 704, 73
25640, V, 1, 0, 0, 0, 0, 704, 73
25641, V, 1, 0, 0, 0, 0, 704, 73
25643, V, 1, 0, 0, 0, 0, 704, 73
25644, V, 1, 0, 0, 0, 0, 704, 73
25645, V, 1, 0, 0, 0, 0, 704, 73
25646, V, 1, 0, 0, 0, 0, 704, 73
25647, V, 1, 0, 0, 0, 0, 704, 73
25648, V, 1, 0, 0, 0, 0, 704, 73
25649, V, 1, 0, 0, 0, 0, 704, 73
25650, V, 1, 0, 0, 0, 0, 704, 73
25651, V, 1, 0, 0, 0, 0, 704, 73
25652, V, 1, 0, 0, 0, 0, 704, 73
25653, V, 1, 0, 0, 0, 0, 704, 73
25654, V, 1, 0, 0, 0, 0, 704, 73
25655, V, 1, 0, 0, 0, 0, 704, 73
25656, V, 1, 0, 0, 0, 0, 704, 73
25657, V, 1, 0, 0, 0, 0, 704, 73
25658, V, 1, 0, 0, 0, 0, 704, 73
25659, V, 1, 0, 0, 0, 0, 704, 73
25660, V, 1, 0, 0, 0, 0, 704, 73
25661, V, 1, 0, 0, 0, 0, 704, 73
25662, V, 1, 0, 0, 0, 0, 704, 73
25663, V, 1, 0, 0, 0, 0, 704, 73
25664, V, 1, 0, 0, 0, 0, 704, 73
25665, V, 1, 0, 0, 0, 0, 704, 73
25666, V, 1, 0, 0, 0, 0, 704, 73
25667, V, 1, 0, 0, 0, 0, 704, 73
25668, V, 1, 0, 0, 0, 0, 704, 73
25669, V, 1, 0, 0, 0, 0, 704, 73
25670, V, 1, 0, 0, 0, 0, 704, 73
25671, V, 1, 0, 0, 0, 0, 704, 73
25672, V, 1, 0, 0, 0, 0, 704, 73
25673, V, 1, 0, 0, 0, 0, 704, 73
25674, V, 1, 0, 0, 0, 0, 704, 73
25675, V, 1, 0, 0, 0, 0, 704, 73
25676, V, 1, 0, 0, 0, 0, 704, 73
25677, V, 1, 0, 0, 0, 0, 704, 73
25678, V, 1, 0, 0, 0, 0, 704, 73
25679, V, 1, 0, 0, 0, 0, 704, 73
25680, V, 1, 0, 0, 0, 0, 704, 73
25681, V, 1, 0, 0, 0, 0, 704, 73
25682, V, 1, 0, 0, 0, 0, 704, 73
25683, V, 1, 0, 0, 0, 0, 704, 73
25684, V, 1, 0, 0, 0, 0, 704, 73
25686, V, 1, 0, 0, 0, 0, 704, 73
25687, V, 1, 0, 0, 0, 0, 704, 73
25688, V, 1, 0, 0, 0, 0, 704, 73
25689, V, 1, 0, 0, 0, 0, 704, 73
25690, V, 1, 0, 0, 0, 0, 704, 73
25691, V, 1, 0, 0, 0, 0, 704, 73
25692, V, 1, 0, 0, 0, 0, 704, 73
25693, V, 1, 0, 0, 0, 0, 704, 73
25694, V, 1, 0, 0, 0, 0, 704, 73
25695, V, 1, 0, 0, 0, 0, 704, 73
25696, V, 1, 0, 0, 0, 0, 704, 73
25697, V, 1, 0, 0, 0, 0, 704, 73
25698, V, 1, 0, 0, 0, 0, 704, 74
25699, V, 1, 0, 0, 0, 0, 704, 74
25700, V, 1, 0, 0, 0, 0, 704, 74
25701, V, 1, 0, 0, 0, 0, 704, 74
25702, V, 1, 0, 0, 0, 0, 704, 74
25703, V, 1, 0, 0, 0, 0, 704, 74
25704, V, 1, 0, 0, 0, 0, 704, 74
25705, V, 1, 0, 0, 0, 0, 704, 74
25706, V, 1, 0, 0, 0, 0, 704, 74
25707, V, 1, 0, 0, 0, 0, 704, 74
25708, V, 1, 0, 0, 0, 0, 704, 74
25709, V, 1, 0, 0, 0, 0, 704, 74
25710, V, 1, 0, 0, 0, 0, 704, 74
25711, V, 1, 0, 0, 0, 0, 704, 74
25712, V, 1, 0, 0, 0, 0, 704, 74
25713, V, 1, 0, 0, 0, 0, 704, 74
25714, V, 1, 0, 0, 0, 0, 704, 74
25715, V, 1, 0, 0, 0, 0, 704, 74
25716, V, 1, 0, 0, 0, 0, 704, 74
25717, V, 1, 0, 0, 0, 0, 704, 74
25718, V, 1, 0, 0, 0, 0, 704, 74
25719, V, 1, 0, 0, 0, 0, 704, 74
25720, V, 1, 0, 0, 0, 0, 704, 74
25721, V, 1, 0, 0, 0, 0, 704, 74
25722, V, 1, 0, 0, 0, 0, 704, 74
25723, V, 1, 0, 0, 0, 0, 704, 74
25724, V, 1, 0, 0, 0, 0, 704, 74
25725, V, 1, 0, 0, 0, 0, 704, 74
25726, V, 1, 0, 0, 0, 0, 704, 74
25728, V, 1, 0, 0, 0, 0, 704, 74
25729, V, 1, 0, 0, 0, 0, 704, 74
25730, V, 1, 0, 0, 0, 0, 704, 74
25731, V, 1, 0, 0, 0, 0, 704, 74
25732, V, 1, 0, 0, 0, 0, 704, 74
25733, V, 1, 0, 0, 0, 0, 704, 74
25734, V, 1, 0, 0, 0, 0, 704, 74
25735, V, 1, 0, 0, 0, 0, 704, 74
25736, V, 1, 0, 0, 0, 0, 704, 74
25737, V, 1, 1, 0, 0, 0, 704, 74
25737, V, 1, 1, 0, 0, 0, 704, 74
25738, V, 1, 0, 0, 0, 0, 704, 74
25738, V, 1, 0, 0, 0, 0, 704, 74
25739, V, 1, 0, 0, 0, 0, 704, 74
25740, V, 1, 0, 0, 0, 0, 704, 74
25741, V, 1, 0, 0, 0, 0, 704, 74
25742, V, 1, 0, 0, 0, 0, 704, 74
25743, V, 1, 0, 0, 0, 0, 704, 74
25744, V, 1, 0, 0, 0, 0, 704, 74
25745, V, 1, 0, 0, 0, 0, 704, 75
25746, V, 1, 0, 0, 0, 0, 704, 75
25747, V, 1, 0, 0, 0, 0, 704, 75
25748, V, 1, 0, 0, 0, 0, 704, 74
25749, V, 1, 0, 0, 0, 0, 704, 75
25750, V, 1, 0, 0, 0, 0, 704, 74
25751, V, 1, 0, 0, 0, 0, 704, 74
25752, V, 1, 0, 0, 0, 0, 704, 74
25753, V, 1, 0, 0, 0, 0, 704, 74
25754, V, 1, 0, 0, 0, 0, 704, 74
25755, V, 1, 0, 0, 0, 0, 704, 74
25756, V, 1, 0, 0, 0, 0, 704, 74
25757, V, 1, 0, 0, 0, 0, 704, 74
25758, V, 1, 0, 0, 0, 0, 704, 74
25759, V, 1, 0, 0, 0, 0, 704, 75
25760, V, 1, 0, 0, 0, 0, 704, 75
25761, V, 1, 0, 0, 0, 0, 704, 75
25762, V, 1, 0, 0, 0, 0, 704, 74
25763, V, 1, 0, 0, 0, 0, 704, 75
25764, V, 1, 0, 0, 0, 0, 704, 75
25765, V, 1, 0, 0, 0, 0, 704, 75
25766, V, 1, 0, 0, 0, 0, 704, 74
25767, V, 1, 0, 0, 0, 0, 704, 74
25768, V, 1, 0, 0, 0, 0, 704, 74
25769, V, 1, 0, 0, 0, 0, 704, 74
25771, V, 1, 0, 0, 0, 0, 704, 74
25772, V, 1, 0, 0, 0, 0, 704, 74
25773, V, 1, 0, 0, 0, 0, 704, 74
25774, V, 1, 0, 0, 0, 0, 704, 74
25775, V, 1, 0, 0, 0, 0, 704, 74
25776, V, 1, 0, 0, 0, 0, 704, 74
25777, V, 1, 0, 0, 0, 0, 704, 74
25778, V, 1, 0, 0, 0, 0, 704, 74
25779, V, 1, 0, 0, 0, 0, 704, 75
25780, V, 1, 0, 0, 0, 0, 704, 75
25781, V, 1, 0, 0, 0, 0, 704, 75
25782, V, 1, 0, 0, 0, 0, 704, 75
25783, V, 1, 0, 0, 0, 0, 704, 75
25784, V, 1, 0, 0, 0, 0, 704, 75
25785, V, 1, 0, 0, 0, 0, 704, 75
25786, V, 1, 0, 0, 0, 0, 704, 75
25787, V, 1, 0, 0, 0, 0, 704, 75
25788, V, 1, 0, 0, 0, 0, 704, 75
25789, V, 1, 0, 0, 0, 0, 704, 75
25790, V, 1, 0, 0, 0, 0, 704, 74
25791, V, 1, 0, 0, 0, 0, 704, 74
25792, V, 1, 1, 0, 0, 0, 704, 75
25792, V, 1, 1, 0, 0, 0, 704, 75
25793, V, 1, 0, 0, 0, 0, 704, 74
25793, V, 1, 0, 0, 0, 0, 704, 74
25794, V, 1, 0, 0, 0, 0, 704, 75
25795, V, 1, 0, 0, 0, 0, 704, 74
25796, V, 1, 0, 0, 0, 0, 704, 75
25797, V, 1, 0, 0, 0, 0, 704, 75
25798, V, 1, 0, 0, 0, 0, 704, 75
25799, V, 1, 0, 0, 0, 0, 704, 75
25800, V, 1, 1, 0, 0, 0, 704, 75
25800, V, 1, 1, 0, 0, 0, 704, 75
25801, V, 1, 0, 0, 0, 0, 704, 75
25801, V, 1, 0, 0, 0, 0, 704, 75
25802, V, 1, 0, 0, 0, 0, 704, 75
25803, V, 1, 0, 0, 0, 0, 704, 75
25804, V, 1, 0, 0, 0, 0, 704, 75
25805, V, 1, 0, 0, 0, 0, 704, 75
25806, V, 1, 0, 0, 0, 0, 704, 75
25807, V, 1, 0, 0, 0, 0, 704, 75
25808, V, 1, 0, 0, 0, 0, 704, 75
25809, V, 1, 0, 0, 0, 0, 704, 75
25810, V, 1, 0, 0, 0, 0, 704, 75
25811, V, 1, 0, 0, 0, 0, 704, 75
25812, V, 1, 0, 0, 0, 0, 704, 75
25814, V, 1, 0, 0, 0, 0, 704, 75
25815, V, 1, 0, 0, 0, 0, 704, 75
25816, V, 1, 1, 0, 0, 0, 704, 75
25816, V, 1, 1, 0, 0, 0, 704, 75
25817, V, 1, 0, 0, 0, 0, 704, 75
25817, V, 1, 0, 0, 0, 0, 704, 75
25818, V, 1, 0, 0, 0, 0, 704, 75
25819, V, 1, 0, 0, 0, 0, 704, 75
25820, V, 1, 0, 0, 0, 0, 704, 75
25821, V, 1, 0, 0, 0, 0, 704, 75
25822, V, 1, 0, 0, 0, 0, 704, 75
25823, V, 1, 0, 0, 0, 0, 704, 76
25824, V, 1, 0, 0, 0, 0, 704, 76
25825, V, 1, 1, 0, 0, 0, 704, 76
25825, V, 1, 1, 0, 0, 0, 704, 76
25826, V, 1, 0, 0, 0, 0, 704, 75
25826, V, 1, 0, 0, 0, 0, 704, 75
25827, V, 1, 0, 0, 0, 0, 704, 75
25828, V, 1, 0, 0, 0, 0, 704, 75
25829, V, 1, 0, 0, 0, 0, 704, 75
25830, V, 1, 0, 0, 0, 0, 704, 76
25831, V, 1, 0, 0, 0, 0, 704, 76
25832, V, 1, 0, 0, 0, 0, 704, 76
25833, V, 1, 0, 0, 0, 0, 704, 76
25834, V, 1, 0, 0, 0, 0, 704, 76
25835, V, 1, 0, 0, 0, 0, 704, 76
25836, V, 1, 0, 0, 0, 0, 704, 76
25837, V, 1, 0, 0, 0, 0, 704, 76
25838, V, 1, 0, 0, 0, 0, 704, 76
25839, V, 1, 0, 0, 0, 0, 704, 76
25840, V, 1, 0, 0, 0, 0, 704, 76
25841, V, 1, 0, 0, 0, 0, 704, 76
25842, V, 1, 0, 0, 0, 0, 704, 76
25843, V, 1, 0, 0, 0, 0, 704, 75
25844, V, 1, 0, 0, 0, 0, 704, 76
25845, V, 1, 0, 0, 0, 0, 704, 75
25846, V, 1, 0, 0, 0, 0, 704, 75
25847, V, 1, 0, 0, 0, 0, 704, 75
25848, V, 1, 0, 0, 0, 0, 704, 75
25849, V, 1, 0, 0, 0, 0, 704, 75
25850, V, 1, 0, 0, 0, 0, 704, 75
25851, V, 1, 0, 0, 0, 0, 704, 75
25852, V, 1, 0, 0, 0, 0, 704, 75
25853, V, 1, 0, 0, 0, 0, 704, 75
25854, V, 1, 0, 0, 0, 0, 704, 75
25856, V, 1, 0, 0, 0, 0, 704, 75
25857, V, 1, 0, 0, 0, 0, 704, 75
25858, V, 1, 0, 0, 0, 0, 704, 75
25859, V, 1, 0, 0, 0, 0, 704, 75
25860, V, 1, 0, 0, 0, 0, 704, 75
25861, V, 1, 0, 0, 0, 0, 704, 75
25862, V, 1, 0, 0, 0, 0, 704, 75
25863, V, 1, 0, 0, 0, 0, 704, 75
25864, V, 1, 0, 0, 0, 0, 704, 75
25865, V, 1, 0, 0, 0, 0, 704, 75
25866, V, 1, 0, 0, 0, 0, 704, 75
25867, V, 1, 0, 0, 0, 0, 704, 75
25868, V, 1, 0, 0, 0, 0, 704, 75
25869, V, 1, 0, 0, 0, 0, 704, 75
25870, V, 1, 0, 0, 0, 0, 704, 75
25871, V, 1, 0, 0, 0, 0, 704, 75
25872, V, 1, 0, 0, 0, 0, 704, 75
25873, V, 1, 0, 0, 0, 0, 704, 75
25874, V, 1, 0, 0, 0, 0, 704, 75
25875, V, 1, 0, 0, 0, 0, 704, 75
25876, V, 1, 0, 0, 0, 0, 704, 75
25877, V, 1, 1, 0, 0, 0, 704, 75
25877, V, 1, 1, 0, 0, 0, 704, 75
25878, V, 1, 0, 0, 0, 0, 704, 74
25878, V, 1, 0, 0, 0, 0, 704, 74
25879, V, 1, 0, 0, 0, 0, 704, 74
25880, V, 1, 0, 0, 0, 0, 704, 74
25881, V, 1, 0, 0, 0, 0, 704, 75
25882, V, 1, 0, 0, 0, 0, 704, 74
25883, V, 1, 0, 0, 0, 0, 704, 75
25884, V, 1, 0, 0, 0, 0, 704, 75
25885, V, 1, 0, 0, 0, 0, 704, 75
25886, V, 1, 0, 0, 0, 0, 704, 75
25887, V, 1, 0, 0, 0, 0, 704, 75
25888, V, 1, 0, 0, 0, 0, 704, 74
25889, V, 1, 0, 0, 0, 0, 704, 74
25890, V, 1, 0, 0, 0, 0, 704, 74
25891, V, 1, 0, 0, 0, 0, 704, 74
25892, V, 1, 0, 0, 0, 0, 704, 74
25893, V, 1, 0, 0, 0, 0, 704, 74
25894, V, 1, 0, 0, 0, 0, 704, 74
25895, V, 1, 0, 0, 0, 0, 704, 74
25896, V, 1, 0, 0, 0, 0, 704, 74
25897, V, 1, 0, 0, 0, 0, 704, 74
25899, V, 1, 0, 0, 0, 0, 704, 74
25900, V, 1, 0, 0, 0, 0, 704, 74
25901, V, 1, 0, 0, 0, 0, 704, 73
25902, V, 1, 0, 0, 0, 0, 704, 73
25903, V, 1, 0, 0, 0, 0, 704, 73
25904, V, 1, 0, 0, 0, 0, 704, 73
25905, V, 1, 0, 0, 0, 0, 704, 73
25906, V, 1, 0, 0, 0, 0, 704, 73
25907, V, 1, 0, 0, 0, 0, 704, 73
25908, V, 1, 0, 0, 0, 0, 704, 73
25909, V, 1, 0, 0, 0, 0, 704, 73
25910, V, 1, 0, 0, 0, 0, 704, 73
25911, V, 1, 0, 0, 0, 0, 704, 73
25912, V, 1, 0, 0, 0, 0, 704, 73
25913, V, 1, 0, 0, 0, 0, 704, 73
25914, V, 1, 0, 0, 0, 0, 704, 73
25915, V, 1, 0, 0, 0, 0, 704, 73
25916, V, 1, 0, 0, 0, 0, 704, 72
25917, V, 1, 0, 0, 0, 0, 704, 72
25918, V, 1, 0, 0, 0, 0, 704, 72
25919, V, 1, 0, 0, 0, 0, 704, 72
25920, V, 1, 0, 0, 0, 0, 704, 72
25921, V, 1, 0, 0, 0, 0, 704, 72
25922, V, 1, 0, 0, 0, 0, 704, 72
25923, V, 1, 0, 0, 0, 0, 704, 72
25924, V, 1, 0, 0, 0, 0, 704, 72
25925, V, 1, 0, 0, 0, 0, 704, 72
25926, V, 1, 0, 0, 0, 0, 704, 72
25927, V, 1, 0, 0, 0, 0, 704, 72
25928, V, 1, 0, 0, 0, 0, 704, 72
25929, V, 1, 0, 0, 0, 0, 704, 72
25930, V, 1, 0, 0, 0, 0, 704, 72
25931, V, 1, 0, 0, 0, 0, 704, 72
25932, V, 1, 0, 0, 0, 0, 704, 72
25933, V, 1, 0, 0, 0, 0, 704, 72
25934, V, 1, 0, 0, 0, 0, 704, 72
25935, V, 1, 0, 0, 0, 0, 704, 72
25936, V, 1, 0, 0, 0, 0, 704, 72
25937, V, 1, 0, 0, 0, 0, 704, 72
25938, V, 1, 0, 0, 0, 0, 704, 71
25939, V, 1, 0, 0, 0, 0, 704, 72
25940, V, 1, 0, 0, 0, 0, 704, 71
25942, V, 1, 0, 0, 0, 0, 704, 71
25943, V, 1, 0, 0, 0, 0, 704, 71
25944, V, 1, 0, 0, 0, 0, 704, 71
25945, V, 1, 0, 0, 0, 0, 704, 71
25946, V, 1, 0, 0, 0, 0, 704, 71
25947, V, 1, 0, 0, 0, 0, 704, 71
25948, V, 1, 0, 0, 0, 0, 704, 71
25949, V, 1, 0, 0, 0, 0, 704, 71
25950, V, 1, 0, 0, 0, 0, 704, 71
25951, V, 1, 0, 0, 0, 0, 704, 71
25952, V, 1, 0, 0, 0, 0, 704, 71
25953, V, 1, 0, 0, 0, 0, 704, 71
25954, V, 1, 0, 0, 0, 0, 704, 71
25955, V, 1, 0, 0, 0, 0, 704, 71
25956, V, 1, 0, 0, 0, 0, 704, 71
25957, V, 1, 0, 0, 0, 0, 704, 71
25958, V, 1, 0, 0, 0, 0, 704, 71
25959, V, 1, 0, 0, 0, 0, 704, 71
25960, V, 1, 0, 0, 0, 0, 704, 71
25961, V, 1, 0, 0, 0, 0, 704, 71
25962, V, 1, 0, 0, 0, 0, 704, 71
25963, V, 1, 0, 0, 0, 0, 704, 71
25964, V, 1, 0, 0, 0, 0, 704, 71
25965, V, 1, 0, 0, 0, 0, 704, 71
25966, V, 1, 0, 0, 0, 0, 704, 71
25967, V, 1, 0, 0, 0, 0, 704, 71
25968, V, 1, 0, 0, 0, 0, 704, 71
25969, V, 1, 0, 0, 0, 0, 704, 71
25970, V, 1, 0, 0, 0, 0, 704, 71
25971, V, 1, 0, 0, 0, 0, 704, 71
25972, V, 1, 0, 0, 0, 0, 704, 70
25973, V, 1, 0, 0, 0, 0, 704, 70
25974, V, 1, 0, 0, 0, 0, 704, 70
25975, V, 1, 0, 0, 0, 0, 704, 71
25976, V, 1, 0, 0, 0, 0, 704, 70
25977, V, 1, 0, 0, 0, 0, 704, 71
25978, V, 1, 0, 0, 0, 0, 704, 70
25979, V, 1, 0, 0, 0, 0, 704, 71
25980, V, 1, 0, 0, 0, 0, 704, 71
25981, V, 1, 0, 0, 0, 0, 704, 70
25982, V, 1, 0, 0, 0, 0, 704, 71
25984, V, 1, 0, 0, 0, 0, 704, 71
25985, V, 1, 0, 0, 0, 0, 704, 71
25986, V, 1, 0, 0, 0, 0, 704, 70
25987, V, 1, 0, 0, 0, 0, 704, 70
25988, V, 1, 0, 0, 0, 0, 704, 70
25989, V, 1, 1, 0, 0, 0, 704, 70
25989, V, 1, 1, 0, 0, 0, 704, 70
25990, V, 1, 0, 0, 0, 0, 704, 70
25990, V, 1, 0, 0, 0, 0, 704, 70
25991, V, 1, 0, 0, 0, 0, 704, 70
25992, V, 1, 0, 0, 0, 0, 704, 70
25993, V, 1, 0, 0, 0, 0, 704, 70
25994, V, 1, 0, 0, 0, 0, 704, 70
25995, V, 1, 1, 0, 0, 0, 704, 71
25995, V, 1, 1, 0, 0, 0, 704, 71
25996, V, 1, 0, 0, 0, 0, 704, 71
25996, V, 1, 0, 0, 0, 0, 704, 71
25997, V, 1, 1, 0, 0, 0, 704, 71
25997, V, 1, 1, 0, 0, 0, 704, 71
25998, V, 1, 0, 0, 0, 0, 704, 71
25998, V, 1, 0, 0, 0, 0, 704, 71
25999, V, 1, 0, 0, 0, 0, 704, 71
26000, V, 1, 1, 0, 0, 0, 704, 71
26000, V, 1, 1, 0, 0, 0, 704, 71
26001, V, 1, 0, 0, 0, 0, 704, 71
26001, V, 1, 0, 0, 0, 0, 704, 71
26002, V, 1, 0, 0, 0, 0, 704, 71
26003, V, 1, 0, 0, 0, 0, 704, 71
26004, V, 1, 0, 0, 0, 0, 704, 71
26005, V, 1, 0, 0, 0, 0, 704, 72
26006, V, 1, 0, 0, 0, 0, 704, 72
26007, V, 1, 0, 0, 0, 0, 704, 72
26008, V, 1, 0, 0, 0, 0, 704, 72
26009, V, 1, 0, 0, 0, 0, 704, 72
26010, V, 1, 0, 0, 0, 0, 704, 72
26011, V, 1, 0, 0, 0, 0, 704, 72
26012, V, 1, 0, 0, 0, 0, 704, 72
26013, V, 1, 0, 0, 0, 0, 704, 72
26014, V, 1, 0, 0, 0, 0, 704, 72
26015, V, 1, 0, 0, 0, 0, 704, 71
26016, V, 1, 0, 0, 0, 0, 704, 71
26017, V, 1, 0, 0, 0, 0, 704, 71
26018, V, 1, 0, 0, 0, 0, 704, 71
26019, V, 1, 0, 0, 0, 0, 704, 71
26020, V, 1, 0, 0, 0, 0, 704, 71
26021, V, 1, 0, 0, 0, 0, 704, 71
26022, V, 1, 0, 0, 0, 0, 704, 71
26023, V, 1, 0, 0, 0, 0, 704, 71
26024, V, 1, 1, 0, 0, 0, 704, 71
26024, V, 1, 1, 0, 0, 0, 704, 71
26025, V, 1, 0, 0, 0, 0, 704, 71
26025, V, 1, 0, 0, 0, 0, 704, 71
26027, V, 1, 0, 0, 0, 0, 704, 71
26028, V, 1, 0, 0, 0, 0, 704, 71
26029, V, 1, 0, 0, 0, 0, 704, 71
26030, V, 1, 0, 0, 0, 0, 704, 71
26031, V, 1, 0, 0, 0, 0, 704, 71
26032, V, 1, 0, 0, 0, 0, 704, 71
26033, V, 1, 0, 0, 0, 0, 704, 71
26034, V, 1, 0, 0, 0, 0, 704, 71
26035, V, 1, 0, 0, 0, 0, 704, 71
26036, V, 1, 0, 0, 0, 0, 704, 71
26037, V, 1, 1, 0, 0, 0, 704, 71
26037, V, 1, 1, 0, 0, 0, 704, 71
26038, V, 1, 0, 0, 0, 0, 704, 71
26038, V, 1, 0, 0, 0, 0, 704, 71
26039, V, 1, 0, 0, 0, 0, 704, 71
26040, V, 1, 0, 0, 0, 0, 704, 71
26041, V, 1, 0, 0, 0, 0, 704, 71
26042, V, 1, 0, 0, 0, 0, 704, 71
26043, V, 1, 0, 0, 0, 0, 704, 71
26044, V, 1, 0, 0, 0, 0, 704, 71
26045, V, 1, 1, 0, 0, 0, 704, 71
26045, V, 1, 1, 0, 0, 0, 704, 71
26046, V, 1, 0, 0, 0, 0, 704, 71
26046, V, 1, 0, 0, 0, 0, 704, 71
26047, V, 1, 0, 0, 0, 0, 704, 71
26048, V, 1, 0, 0, 0, 0, 704, 71
26049, V, 1, 1, 0, 0, 0, 704, 71
26049, V, 1, 1, 0, 0, 0, 704, 71
26050, V, 1, 0, 0, 0, 0, 704, 71
26050, V, 1, 0, 0, 0, 0, 704, 71
26051, V, 1, 0, 0, 0, 0, 704, 71
26052, V, 1, 0, 0, 0, 0, 704, 71
26053, V, 1, 0, 0, 0, 0, 704, 71
26054, V, 1, 0, 0, 0, 0, 704, 72
26055, V, 1, 0, 0, 0, 0, 704, 72
26056, V, 1, 0, 0, 0, 0, 704, 72
26057, V, 1, 0, 0, 0, 0, 704, 72
26058, V, 1, 0, 0, 0, 0, 704, 72
26059, V, 1, 0, 0, 0, 0, 704, 72
26060, V, 1, 0, 0, 0, 0, 704, 72
26061, V, 1, 0, 0, 0, 0, 704, 72
26062, V, 1, 0, 0, 0, 0, 704, 72
26063, V, 1, 0, 0, 0, 0, 704, 71
26064, V, 1, 0, 0, 0, 0, 704, 71
26065, V, 1, 0, 0, 0, 0, 704, 71
26066, V, 1, 0, 0, 0, 0, 704, 71
26067, V, 1, 0, 0, 0, 0, 704, 71
26068, V, 1, 0, 0, 0, 0, 704, 71
26070, V, 1, 0, 0, 0, 0, 704, 71
26071, V, 1, 0, 0, 0, 0, 704, 71
26072, V, 1, 0, 0, 0, 0, 704, 71
26073, V, 1, 0, 0, 0, 0, 704, 71
26074, V, 1, 0, 0, 0, 0, 704, 71
26075, V, 1, 1, 0, 0, 0, 704, 71
26075, V, 1, 1, 0, 0, 0, 704, 71
26076, V, 1, 0, 0, 0, 0, 704, 71
26076, V, 1, 0, 0, 0, 0, 704, 71
26077, V, 1, 0, 0, 0, 0, 704, 71
26078, V, 1, 0, 0, 0, 0, 704, 71
26079, V, 1, 0, 0, 0, 0, 704, 71
26080, V, 1, 0, 0, 0, 0, 704, 71
26081, V, 1, 0, 0, 0, 0, 704, 71
26082, V, 1, 1, 0, 0, 0, 704, 71
26082, V, 1, 1, 0, 0, 0, 704, 71
26083, V, 1, 1, 1, 1, 0, 704, 71
26084, V, 1, 0, 0, 1, 0, 704, 71
26084, V, 1, 0, 0, 0, 0, 704, 71
26085, V, 1, 0, 0, 0, 0, 704, 71
26086, V, 1, 0, 0, 0, 0, 704, 72
26087, V, 1, 0, 0, 0, 0, 704, 72
26088, V, 1, 0, 0, 0, 0, 704, 72
26089, V, 1, 0, 0, 0, 0, 704, 72
26090, V, 1, 0, 0, 0, 0, 704, 72
26091, V, 1, 0, 0, 0, 0, 704, 72
26092, V, 1, 0, 0, 0, 0, 704, 72
26093, V, 1, 0, 0, 0, 0, 704, 72
26094, V, 1, 1, 0, 0, 0, 704, 72
26094, V, 1, 1, 0, 0, 0, 704, 72
26095, V, 1, 0, 0, 0, 0, 704, 72
26095, V, 1, 0, 0, 0, 0, 704, 72
26096, V, 1, 0, 0, 0, 0, 704, 72
26097, V, 1, 0, 0, 0, 0, 704, 73
26098, V, 1, 0, 0, 0, 0, 704, 73
26099, V, 1, 1, 0, 0, 0, 704, 73
26099, V, 1, 1, 0, 0, 0, 704, 73
26100, V, 1, 0, 0, 0, 0, 704, 73
26100, V, 1, 0, 0, 0, 0, 704, 73
26101, V, 1, 0, 0, 0, 0, 704, 73
26102, V, 1, 0, 0, 0, 0, 704, 73
26103, V, 1, 0, 0, 0, 0, 704, 73
26104, V, 1, 0, 0, 0, 0, 704, 73
26105, V, 1, 0, 0, 0, 0, 704, 73
26106, V, 1, 0, 0, 0, 0, 704, 73
26107, V, 1, 0, 0, 0, 0, 704, 73
26108, V, 1, 0, 0, 0, 0, 704, 73
26109, V, 1, 0, 0, 0, 0, 704, 73
26110, V, 1, 0, 0, 0, 0, 704, 73
26112, V, 1, 0, 0, 0, 0, 704, 73
26113, V, 1, 0, 0, 0, 0, 704, 73
26114, V, 1, 0, 0, 0, 0, 704, 73
26115, V, 1, 0, 0, 0, 0, 704, 73
26116, V, 1, 0, 0, 0, 0, 704, 73
26117, V, 1, 0, 0, 0, 0, 704, 73
26118, V, 1, 0, 0, 0, 0, 704, 73
26119, V, 1, 0, 0, 0, 0, 704, 72
26120, V, 1, 0, 0, 0, 0, 704, 72
26121, V, 1, 0, 0, 0, 0, 704, 72
26122, V, 1, 0, 0, 0, 0, 704, 72
26123, V, 1, 0, 0, 0, 0, 704, 72
26124, V, 1, 0, 0, 0, 0, 704, 72
26125, V, 1, 0, 0, 0, 0, 704, 72
26126, V, 1, 0, 0, 0, 0, 704, 72
26127, V, 1, 0, 0, 0, 0, 704, 72
26128, V, 1, 0, 0, 0, 0, 704, 72
26129, V, 1, 1, 0, 0, 0, 704, 72
26129, V, 1, 1, 0, 0, 0, 704, 72
26130, V, 1, 1, 1, 1, 0, 704, 72
26131, V, 1, 1, 1, 1, 0, 704, 73
26132, V, 1, 1, 1, 1, 0, 704, 73
26133, V, 1, 1, 1, 1, 0, 704, 73
26134, V, 1, 1, 1, 1, 0, 704, 74
26135, V, 1, 1, 1, 1, 0, 704, 74
26136, V, 1, 1, 1, 1, 0, 704, 75
26137, V, 1, 1, 1, 1, 0, 704, 75
26138, V, 1, 1, 1, 1, 0, 704, 76
26139, V, 1, 1, 1, 1, 0, 704, 77
26140, V, 1, 1, 1, 1, 0, 704, 78
26141, V, 1, 1, 1, 1, 0, 704, 78
26142, V, 1, 1, 1, 1, 0, 704, 79
26143, V, 1, 1, 1, 1, 0, 704, 80
26144, V, 1, 1, 1, 1, 0, 704, 80
26145, V, 1, 1, 1, 1, 0, 704, 81
26146, V, 1, 1, 1, 1, 0, 704, 81
26147, V, 1, 1, 1, 1, 0, 704, 82
26148, V, 1, 1, 1, 1, 0, 704, 82
26149, V, 1, 1, 1, 1, 0, 704, 83
26150, V, 1, 1, 1, 1, 0, 704, 83
26151, V, 1, 1, 1, 1, 0, 704, 84
26152, V, 1, 1, 1, 1, 0, 704, 84
26153, V, 1, 1, 1, 1, 0, 704, 85
26155, V, 1, 1, 1, 1, 0, 704, 85
26156, V, 1, 1, 1, 1, 0, 704, 86
26157, V, 1, 1, 1, 1, 0, 704, 86
26158, V, 1, 1, 1, 1, 0, 704, 87
26159, V, 1, 1, 1, 1, 0, 704, 87
26160, V, 1, 1, 1, 1, 0, 704, 87
26161, V, 1, 1, 1, 1, 0, 704, 88
26162, V, 1, 1, 1, 1, 0, 704, 88
26163, V, 1, 1, 1, 1, 0, 704, 88
26164, V, 1, 1, 1, 1, 0, 704, 89
26165, V, 1, 1, 1, 1, 0, 704, 89
26166, V, 1, 1, 1, 1, 0, 704, 89
26167, V, 1, 1, 1, 1, 0, 704, 90
26168, V, 1, 1, 1, 1, 0, 704, 90
26169, V, 1, 1, 1, 1, 0, 704, 90
26170, V, 1, 1, 1, 1, 0, 704, 91
26171, V, 1, 1, 1, 1, 0, 704, 91
26172, V, 1, 1, 1, 1, 0, 704, 91
26173, V, 1, 1, 1, 1, 0, 704, 91
26174, V, 1, 1, 1, 1, 0, 704, 92
26175, V, 1, 1, 1, 1, 0, 704, 92
26176, V, 1, 1, 1, 1, 0, 704, 92
26177, V, 1, 1, 1, 1, 0, 704, 92
26178, V, 1, 1, 1, 1, 0, 704, 93
26179, V, 1, 1, 1, 1, 0, 704, 93
26180, V, 1, 1, 1, 1, 0, 704, 93
26181, V, 1, 1, 1, 1, 0, 704, 93
26182, V, 1, 1, 1, 1, 0, 704, 93
26183, V, 1, 1, 1, 1, 0, 704, 94
26184, V, 1, 1, 1, 1, 0, 704, 94
26185, V, 1, 1, 1, 1, 0, 704, 94
26186, V, 1, 1, 1, 1, 0, 704, 94
26187, V, 1, 1, 1, 1, 0, 704, 94
26188, V, 1, 1, 1, 1, 0, 704, 94
26189, V, 1, 1, 1, 1, 0, 704, 95
26190, V, 1, 1, 1, 1, 0, 704, 95
26191, V, 1, 1, 1, 1, 0, 704, 95
26192, V, 1, 1, 1, 1, 0, 704, 95
26193, V, 1, 1, 1, 1, 0, 704, 95
26194, V, 1, 1, 1, 1, 0, 704, 95
26195, V, 1, 1, 1, 1, 0, 704, 95
26196, V, 1, 1, 1, 1, 0, 704, 96
26198, V, 1, 1, 1, 1, 0, 704, 96
26199, V, 1, 1, 1, 1, 0, 704, 96
26200, V, 1, 1, 1, 1, 0, 704, 96
26201, V, 1, 1, 1, 1, 0, 704, 96
26202, V, 1, 1, 1, 1, 0, 704, 96
26203, V, 1, 1, 1, 1, 0, 704, 96
26204, V, 1, 1, 1, 1, 0, 704, 96
26205, V, 1, 1, 1, 1, 0, 704, 96
26206, V, 1, 1, 1, 1, 0, 704, 96
26207, V, 1, 1, 1, 1, 0, 704, 97
26208, V, 1, 1, 1, 1, 0, 704, 97
26209, V, 1, 1, 1, 1, 0, 704, 97
26210, V, 1, 1, 1, 1, 0, 704, 97
26211, V, 1, 1, 1, 1, 0, 704, 97
26212, V, 1, 1, 1, 1, 0, 704, 97
26213, V, 1, 1, 1, 1, 0, 704, 97
26214, V, 1, 1, 1, 1, 0, 704, 97
26215, V, 1, 1, 1, 1, 0, 704, 97
26216, V, 1, 1, 1, 1, 0, 704, 97
26217, V, 1, 1, 1, 1, 0, 704, 97
26218, V, 1, 1, 1, 1, 0, 704, 97
26219, V, 1, 1, 1, 1, 0, 704, 97
26220, V, 1, 1, 1, 1, 0, 704, 98
26221, V, 1, 1, 1, 1, 0, 704, 98
26222, V, 1, 1, 1, 1, 0, 704, 98
26223, V, 1, 1, 1, 1, 0, 704, 98
26224, V, 1, 1, 1, 1, 0, 704, 98
26225, V, 1, 1, 1, 1, 0, 704, 98
26226, V, 1, 1, 1, 1, 0, 704, 98
26227, V, 1, 1, 1, 1, 0, 704, 98
26228, V, 1, 1, 1, 1, 0, 704, 98
26229, V, 1, 1, 1, 1, 0, 704, 98
26230, V, 1, 1, 1, 1, 0, 704, 98
26231, V, 1, 1, 1, 1, 0, 704, 98
26232, V, 1, 1, 1, 1, 0, 704, 98
26233, V, 1, 1, 1, 1, 0, 704, 98
26234, V, 1, 1, 1, 1, 0, 704, 98
26235, V, 1, 1, 1, 1, 0, 704, 98
26236, V, 1, 1, 1, 1, 0, 704, 98
26237, V, 1, 1, 1, 1, 0, 704, 98
26238, V, 1, 1, 1, 1, 0, 704, 98
26240, V, 1, 1, 1, 1, 0, 704, 98
26241, V, 1, 1, 1, 1, 0, 704, 98
26242, V, 1, 1, 1, 1, 0, 704, 99
26243, V, 1, 1, 1, 1, 0, 704, 99
26244, V, 1, 1, 1, 1, 0, 704, 99
26245, V, 1, 1, 1, 1, 0, 704, 99
26246, V, 1, 1, 1, 1, 0, 704, 99
26247, V, 1, 1, 1, 1, 0, 704, 99
26248, V, 1, 1, 1, 1, 0, 704, 99
26249, V, 1, 1, 1, 1, 0, 704, 99
26250, V, 1, 1, 1, 1, 0, 704, 99
26251, V, 1, 1, 1, 1, 0, 704, 99
26252, V, 1, 1, 1, 1, 0, 704, 99
26253, V, 1, 1, 1, 1, 0, 704, 99
26254, V, 1, 1, 1, 1, 0, 704, 99
26255, V, 1, 1, 1, 1, 0, 704, 99
26256, V, 1, 1, 1, 1, 0, 704, 99
26257, V, 1, 1, 1, 1, 0, 704, 99
26258, V, 1, 1, 1, 1, 0, 704, 99
26259, V, 1, 1, 1, 1, 0, 704, 99
26260, V, 1, 1, 1, 1, 0, 704, 99
26261, V, 1, 1, 1, 1, 0, 704, 99
26262, V, 1, 1, 1, 1, 0, 704, 99
26263, V, 1, 1, 1, 1, 0, 704, 99
26264, V, 1, 1, 1, 1, 0, 704, 99
26265, V, 1, 1, 1, 1, 0, 704, 99
26266, V, 1, 1, 1, 1, 0, 704, 99
26267, V, 1, 1, 1, 1, 0, 704, 99
26268, V, 1, 1, 1, 1, 0, 704, 99
26269, V, 1, 1, 1, 1, 0, 704, 99
26270, V, 1, 1, 1, 1, 0, 704, 99
26271, V, 1, 1, 1, 1, 0, 704, 99
26272, V, 1, 1, 1, 1, 0, 704, 99
26273, V, 1, 1, 1, 1, 0, 704, 99
26274, V, 1, 1, 1, 1, 0, 704, 99
26275, V, 1, 1, 1, 1, 0, 704, 99
26276, V, 1, 1, 1, 1, 0, 704, 99
26277, V, 1, 1, 1, 1, 0, 704, 99
26278, V, 1, 1, 1, 1, 0, 704, 99
26279, V, 1, 1, 1, 1, 0, 704, 99
26280, V, 1, 1, 1, 1, 0, 704, 99
26281, V, 1, 1, 1, 1, 0, 704, 99
26283, V, 1, 1, 1, 1, 0, 704, 99
26284, V, 1, 1, 1, 1, 0, 704, 99
26285, V, 1, 1, 1, 1, 0, 704, 99
26286, V, 1, 1, 1, 1, 0, 704, 99
26287, V, 1, 1, 1, 1, 0, 704, 99
26288, V, 1, 1, 1, 1, 0, 704, 99
26289, V, 1, 1, 1, 1, 0, 704, 99
26290, V, 1, 1, 1, 1, 0, 704, 99
26291, V, 1, 1, 1, 1, 0, 704, 99
26292, V, 1, 1, 1, 1, 0, 704, 99
26293, V, 1, 1, 1, 1, 0, 704, 99
26294, V, 1, 1, 1, 1, 0, 704, 99
26295, V, 1, 1, 1, 1, 0, 704, 99
26296, V, 1, 1, 1, 1, 0, 704, 99
26297, V, 1, 1, 1, 1, 0, 704, 99
26298, V, 1, 1, 1, 1, 0, 704, 99
26299, V, 1, 1, 1, 1, 0, 704, 99
26300, V, 1, 1, 1, 1, 0, 704, 99
26301, V, 1, 1, 1, 1, 0, 704, 99
26302, V, 1, 1, 1, 1, 0, 704, 100
26303, V, 1, 1, 1, 1, 0, 704, 100
26304, V, 1, 1, 1, 1, 0, 704, 100
26305, V, 1, 1, 1, 1, 0, 704, 100
26306, V, 1, 1, 1, 1, 0, 704, 100
26307, V, 1, 1, 1, 1, 0, 704, 100
26308, V, 1, 1, 1, 1, 0, 704, 100
26309, V, 1, 1, 1, 1, 0, 704, 100
26310, V, 1, 1, 1, 1, 0, 704, 100
26311, V, 1, 1, 1, 1, 0, 704, 100
26312, V, 1, 1, 1, 1, 0, 704, 100
26313, V, 1, 1, 1, 1, 0, 704, 100
26314, V, 1, 1, 1, 1, 0, 704, 100
26315, V, 1, 1, 1, 1, 0, 704, 100
26316, V, 1, 1, 1, 1, 0, 704, 100
26317, V, 1, 1, 1, 1, 0, 704, 100
26318, V, 1, 1, 1, 1, 0, 704, 100
26319, V, 1, 1, 1, 1, 0, 704, 100
26320, V, 1, 1, 1, 1, 0, 704, 100
26321, V, 1, 1, 1, 1, 0, 704, 100
26322, V, 1, 1, 1, 1, 0, 704, 100
26323, V, 1, 1, 1, 1, 0, 704, 100
26324, V, 1, 1, 1, 1, 0, 704, 100
26326, V, 1, 1, 1, 1, 0, 704, 100
26327, V, 1, 1, 1, 1, 0, 704, 100
26328, V, 1, 1, 1, 1, 0, 704, 100
26329, V, 1, 1, 1, 1, 0, 704, 100
26330, V, 1, 1, 1, 1, 0, 704, 100
26331, V, 1, 1, 1, 1, 0, 704, 100
26332, V, 1, 1, 1, 1, 0, 704, 100
26333, V, 1, 1, 1, 1, 0, 704, 100
26334, V, 1, 1, 1, 1, 0, 704, 100
26335, V, 1, 1, 1, 1, 0, 704, 100
26336, V, 1, 1, 1, 1, 0, 704, 100
26337, V, 1, 1, 1, 1, 0, 704, 100
26338, V, 1, 1, 1, 1, 0, 704, 100
26339, V, 1, 1, 1, 1, 0, 704, 100
26340, V, 1, 1, 1, 1, 0, 704, 100
26341, V, 1, 1, 1, 1, 0, 704, 100
26342, V, 1, 1, 1, 1, 0, 704, 100
26343, V, 1, 1, 1, 1, 0, 704, 100
26344, V, 1, 1, 1, 1, 0, 704, 100
26345, V, 1, 1, 1, 1, 0, 704, 100
26346, V, 1, 1, 1, 1, 0, 704, 100
26347, V, 1, 1, 1, 1, 0, 704, 100
26348, V, 1, 1, 1, 1, 0, 704, 100
26349, V, 1, 1, 1, 1, 0, 704, 100
26350, V, 1, 1, 1, 1, 0, 704, 100
26351, V, 1, 1, 1, 1, 0, 704, 100
26352, V, 1, 1, 1, 1, 0, 704, 100
26353, V, 1, 1, 1, 1, 0, 704, 100
26354, V, 1, 1, 1, 1, 0, 704, 99
26355, V, 1, 1, 1, 1, 0, 704, 100
26356, V, 1, 1, 1, 1, 0, 704, 99
26357, V, 1, 1, 1, 1, 0, 704, 100
26358, V, 1, 1, 1, 1, 0, 704, 100
26359, V, 1, 1, 1, 1, 0, 704, 99
26360, V, 1, 1, 1, 1, 0, 704, 100
26361, V, 1, 1, 1, 1, 0, 704, 100
26362, V, 1, 1, 1, 1, 0, 704, 100
26363, V, 1, 1, 1, 1, 0, 704, 100
26364, V, 1, 1, 1, 1, 0, 704, 100
26365, V, 1, 1, 1, 1, 0, 704, 100
26366, V, 1, 1, 1, 1, 0, 704, 100
26368, V, 1, 1, 1, 1, 0, 704, 100
26369, V, 1, 1, 1, 1, 0, 704, 100
26370, V, 1, 1, 1, 1, 0, 704, 99
26371, V, 1, 1, 1, 1, 0, 704, 100
26372, V, 1, 1, 1, 1, 0, 704, 100
26373, V, 1, 1, 1, 1, 0, 704, 100
26374, V, 1, 1, 1, 1, 0, 704, 100
26375, V, 1, 1, 1, 1, 0, 704, 100
26376, V, 1, 1, 1, 1, 0, 704, 100
26377, V, 1, 1, 1, 1, 0, 704, 100
26378, V, 1, 1, 1, 1, 0, 704, 100
26379, V, 1, 1, 1, 1, 0, 704, 100
26380, V, 1, 1, 1, 1, 0, 704, 100
26381, V, 1, 1, 1, 1, 0, 704, 100
26382, V, 1, 1, 1, 1, 0, 704, 100
26383, V, 1, 1, 1, 1, 0, 704, 100
26384, V, 1, 1, 1, 1, 0, 704, 100
26385, V, 1, 1, 1, 1, 0, 704, 100
26386, V, 1, 1, 1, 1, 0, 704, 100
26387, V, 1, 1, 1, 1, 0, 704, 100
26388, V, 1, 1, 1, 1, 0, 704, 100
26389, V, 1, 1, 1, 1, 0, 704, 100
26390, V, 1, 1, 1, 1, 0, 704, 100
26391, V, 1, 1, 1, 1, 0, 704, 100
26392, V, 1, 1, 1, 1, 0, 704, 100
26393, V, 1, 1, 1, 1, 0, 704, 100
26394, V, 1, 1, 1, 1, 0, 704, 100
26395, V, 1, 1, 1, 1, 0, 704, 100
26396, V, 1, 1, 1, 1, 0, 704, 100
26397, V, 1, 1, 1, 1, 0, 704, 100
26398, V, 1, 1, 1, 1, 0, 704, 100
26399, V, 1, 1, 1, 1, 0, 704, 100
26400, V, 1, 1, 1, 1, 0, 704, 100
26401, V, 1, 1, 1, 1, 0, 704, 100
26402, V, 1, 1, 1, 1, 0, 704, 100
26403, V, 1, 1, 1, 1, 0, 704, 100
26404, V, 1, 1, 1, 1, 0, 704, 100
26405, V, 1, 1, 1, 1, 0, 704, 100
26406, V, 1, 1, 1, 1, 0, 704, 100
26407, V, 1, 1, 1, 1, 0, 704, 100
26408, V, 1, 1, 1, 1, 0, 704, 100
26409, V, 1, 1, 1, 1, 0, 704, 100
26411, V, 1, 1, 1, 1, 0, 704, 100
26412, V, 1, 1, 1, 1, 0, 704, 100
26413, V, 1, 1, 1, 1, 0, 704, 100
26414, V, 1, 1, 1, 1, 0, 704, 100
26415, V, 1, 1, 1, 1, 0, 704, 100
26416, V, 1, 1, 1, 1, 0, 704, 100
26417, V, 1, 1, 1, 1, 0, 704, 100
26418, V, 1, 1, 1, 1, 0, 704, 100
26419, V, 1, 1, 1, 1, 0, 704, 100
26420, V, 1, 1, 1, 1, 0, 704, 100
26421, V, 1, 1, 1, 1, 0, 704, 100
26422, V, 1, 1, 1, 1, 0, 704, 100
26423, V, 1, 1, 1, 1, 0, 704, 100
26424, V, 1, 1, 1, 1, 0, 704, 100
26425, V, 1, 1, 1, 1, 0, 704, 100
26426, V, 1, 1, 1, 1, 0, 704, 100
26427, V, 1, 1, 1, 1, 0, 704, 100
26428, V, 1, 1, 1, 1, 0, 704, 100
26429, V, 1, 1, 1, 1, 0, 704, 100
26430, V, 1, 1, 1, 1, 0, 704, 100
26431, V, 1, 1, 1, 1, 0, 704, 100
26432, V, 1, 1, 1, 1, 0, 704, 100
26433, V, 1, 1, 1, 1, 0, 704, 100
26434, V, 1, 1, 1, 1, 0, 704, 100
26435, V, 1, 1, 1, 1, 0, 704, 100
26436, V, 1, 1, 1, 1, 0, 704, 100
26437, V, 1, 1, 1, 1, 0, 704, 100
26438, V, 1, 1, 1, 1, 0, 704, 100
26439, V, 1, 1, 1, 1, 0, 704, 100
26440, V, 1, 1, 1, 1, 0, 704, 100
26441, V, 1, 1, 1, 1, 0, 704, 100
26442, V, 1, 1, 1, 1, 0, 704, 100
26443, V, 1, 1, 1, 1, 0, 704, 100
26444, V, 1, 1, 1, 1, 0, 704, 100
26445, V, 1, 1, 1, 1, 0, 704, 100
26446, V, 1, 1, 1, 1, 0, 704, 100
26447, V, 1, 1, 1, 1, 0, 704, 100
26448, V, 1, 1, 1, 1, 0, 704, 100
26449, V, 1, 1, 1, 1, 0, 704, 100
26450, V, 1, 1, 1, 1, 0, 704, 100
26451, V, 1, 1, 1, 1, 0, 704, 100
26452, V, 1, 1, 1, 1, 0, 704, 100
26454, V, 1, 1, 1, 1, 0, 704, 100
26455, V, 1, 1, 1, 1, 0, 704, 100
26456, V, 1, 1, 1, 1, 0, 704, 100
26457, V, 1, 1, 1, 1, 0, 704, 100
26458, V, 1, 1, 1, 1, 0, 704, 100
26459, V, 1, 1, 1, 1, 0, 704, 100
26460, V, 1, 1, 1, 1, 0, 704, 100
26461, V, 1, 1, 1, 1, 0, 704, 100
26462, V, 1, 1, 1, 1, 0, 704, 100
26463, V, 1, 1, 1, 1, 0, 704, 100
26464, V, 1, 1, 1, 1, 0, 704, 100
26465, V, 1, 1, 1, 1, 0, 704, 100
26466, V, 1, 1, 1, 1, 0, 704, 100
26467, V, 1, 1, 1, 1, 0, 704, 100
26468, V, 1, 1, 1, 1, 0, 704, 100
26469, V, 1, 1, 1, 1, 0, 704, 100
26470, V, 1, 1, 1, 1, 0, 704, 100
26471, V, 1, 1, 1, 1, 0, 704, 100
26472, V, 1, 1, 1, 1, 0, 704, 100
26473, V, 1, 1, 1, 1, 0, 704, 100
26474, V, 1, 1, 1, 1, 0, 704, 100
26475, V, 1, 1, 1, 1, 0, 704, 100
26476, V, 1, 1, 1, 1, 0, 704, 100
26477, V, 1, 1, 1, 1, 0, 704, 100
26478, V, 1, 1, 1, 1, 0, 704, 100
26479, V, 1, 1, 1, 1, 0, 704, 100
26480, V, 1, 1, 1, 1, 0, 704, 100
26481, V, 1, 1, 1, 1, 0, 704, 100
26482, V, 1, 1, 1, 1, 0, 704, 100
26483, V, 1, 1, 1, 1, 0, 704, 100
26484, V, 1, 1, 1, 1, 0, 704, 100
26485, V, 1, 1, 1, 1, 0, 704, 100
26486, V, 1, 1, 1, 1, 0, 704, 100
26487, V, 1, 1, 1, 1, 0, 704, 100
26488, V, 1, 1, 1, 1, 0, 704, 100
26489, V, 1, 1, 1, 1, 0, 704, 100
26490, V, 1, 1, 1, 1, 0, 704, 100
26491, V, 1, 1, 1, 1, 0, 704, 100
26492, V, 1, 1, 1, 1, 0, 704, 100
26493, V, 1, 1, 1, 1, 0, 704, 100
26494, V, 1, 1, 1, 1, 0, 704, 100
26496, V, 1, 1, 1, 1, 0, 704, 100
26497, V, 1, 1, 1, 1, 0, 704, 100
26498, V, 1, 1, 1, 1, 0, 704, 100
26499, V, 1, 1, 1, 1, 0, 704, 100
26500, V, 1, 1, 1, 1, 0, 704, 100
26501, V, 1, 1, 1, 1, 0, 704, 100
26502, V, 1, 1, 1, 1, 0, 704, 100
26503, V, 1, 1, 1, 1, 0, 704, 100
26504, V, 1, 1, 1, 1, 0, 704, 100
26505, V, 1, 1, 1, 1, 0, 704, 100
26506, V, 1, 1, 1, 1, 0, 704, 100
26507, V, 1, 1, 1, 1, 0, 704, 100
26508, V, 1, 1, 1, 1, 0, 704, 100
26509, V, 1, 1, 1, 1, 0, 704, 100
26510, V, 1, 1, 1, 1, 0, 704, 100
26511, V, 1, 1, 1, 1, 0, 704, 100
26512, V, 1, 1, 1, 1, 0, 704, 100
26513, V, 1, 1, 1, 1, 0, 704, 100
26514, V, 1, 1, 1, 1, 0, 704, 100
26515, V, 1, 1, 1, 1, 0, 704, 100
26516, V, 1, 1, 1, 1, 0, 704, 100
26517, V, 1, 1, 1, 1, 0, 704, 100
26518, V, 1, 1, 1, 1, 0, 704, 100
26519, V, 1, 1, 1, 1, 0, 704, 100
26520, V, 1, 1, 1, 1, 0, 704, 100
26521, V, 1, 1, 1, 1, 0, 704, 100
26522, V, 1, 1, 1, 1, 0, 704, 100
26523, V, 1, 1, 1, 1, 0, 704, 100
26524, V, 1, 1, 1, 1, 0, 704, 100
26525, V, 1, 1, 1, 1, 0, 704, 100
26526, V, 1, 1, 1, 1, 0, 704, 100
26527, V, 1, 1, 1, 1, 0, 704, 100
26528, V, 1, 1, 1, 1, 0, 704, 100
26529, V, 1, 0, 0, 1, 0, 704, 100
26529, V, 1, 0, 0, 0, 0, 704, 100
26530, V, 1, 1, 0, 0, 0, 704, 100
26530, V, 1, 1, 0, 0, 0, 704, 100
26531, V, 1, 1, 1, 1, 0, 704, 100
26532, V, 1, 1, 1, 1, 0, 704, 100
26533, V, 1, 1, 1, 1, 0, 704, 100
26534, V, 1, 1, 1, 1, 0, 704, 99
26535, V, 1, 1, 1, 1, 0, 704, 99
26536, V, 1, 1, 1, 1, 0, 704, 99
26537, V, 1, 1, 1, 1, 0, 704, 99
26539, V, 1, 1, 1, 1, 0, 704, 99
26540, V, 1, 1, 1, 1, 0, 704, 99
26541, V, 1, 1, 1, 1, 0, 704, 99
26542, V, 1, 1, 1, 1, 0, 704, 99
26543, V, 1, 1, 1, 1, 0, 704, 99
26544, V, 1, 1, 1, 1, 0, 704, 99
26545, V, 1, 1, 1, 1, 0, 704, 99
26546, V, 1, 1, 1, 1, 0, 704, 99
26547, V, 1, 1, 1, 1, 0, 704, 99
26548, V, 1, 1, 1, 1, 0, 704, 99
26549, V, 1, 1, 1, 1, 0, 704, 99
26550, V, 1, 1, 1, 1, 0, 704, 99
26551, V, 1, 1, 1, 1, 0, 704, 99
26552, V, 1, 1, 1, 1, 0, 704, 99
26553, V, 1, 1, 1, 1, 0, 704, 99
26554, V, 1, 1, 1, 1, 0, 704, 99
26555, V, 1, 1, 1, 1, 0, 704, 99
26556, V, 1, 1, 1, 1, 0, 704, 99
26557, V, 1, 1, 1, 1, 0, 704, 99
26558, V, 1, 1, 1, 1, 0, 704, 99
26559, V, 1, 1, 1, 1, 0, 704, 99
26560, V, 1, 1, 1, 1, 0, 704, 99
26561, V, 1, 1, 1, 1, 0, 704, 99
26562, V, 1, 1, 1, 1, 0, 704, 99
26563, V, 1, 1, 1, 1, 0, 704, 99
26564, V, 1, 1, 1, 1, 0, 704, 99
26565, V, 1, 1, 1, 1, 0, 704, 99
26566, V, 1, 1, 1, 1, 0, 704, 99
26567, V, 1, 1, 1, 1, 0, 704, 99
26568, V, 1, 1, 1, 1, 0, 704, 99
26569, V, 1, 1, 1, 1, 0, 704, 99
26570, V, 1, 1, 1, 1, 0, 704, 99
26571, V, 1, 1, 1, 1, 0, 704, 99
26572, V, 1, 1, 1, 1, 0, 704, 99
26573, V, 1, 1, 1, 1, 0, 704, 99
26574, V, 1, 1, 1, 1, 0, 704, 99
26575, V, 1, 1, 1, 1, 0, 704, 99
26576, V, 1, 1, 1, 1, 0, 704, 99
26577, V, 1, 1, 1, 1, 0, 704, 99
26578, V, 1, 1, 1, 1, 0, 704, 99
26579, V, 1, 1, 1, 1, 0, 704, 99
26580, V, 1, 1, 1, 1, 0, 704, 99
26582, V, 1, 1, 1, 1, 0, 704, 99
26583, V, 1, 1, 1, 1, 0, 704, 99
26584, V, 1, 1, 1, 1, 0, 704, 100
26585, V, 1, 1, 1, 1, 0, 704, 99
26586, V, 1, 1, 1, 1, 0, 704, 99
26587, V, 1, 1, 1, 1, 0, 704, 99
26588, V, 1, 1, 1, 1, 0, 704, 99
26589, V, 1, 1, 1, 1, 0, 704, 99
26590, V, 1, 1, 1, 1, 0, 704, 99
26591, V, 1, 1, 1, 1, 0, 704, 99
26592, V, 1, 1, 1, 1, 0, 704, 99
26593, V, 1, 1, 1, 1, 0, 704, 99
26594, V, 1, 1, 1, 1, 0, 704, 99
26595, V, 1, 1, 1, 1, 0, 704, 99
26596, V, 1, 1, 1, 1, 0, 704, 100
26597, V, 1, 1, 1, 1, 0, 704, 99
26598, V, 1, 1, 1, 1, 0, 704, 99
26599, V, 1, 1, 1, 1, 0, 704, 100
26600, V, 1, 1, 1, 1, 0, 704, 100
26601, V, 1, 1, 1, 1, 0, 704, 100
26602, V, 1, 1, 1, 1, 0, 704, 100
26603, V, 1, 1, 1, 1, 0, 704, 100
26604, V, 1, 1, 1, 1, 0, 704, 100
26605, V, 1, 1, 1, 1, 0, 704, 100
26606, V, 1, 1, 1, 1, 0, 704, 100
26607, V, 1, 1, 1, 1, 0, 704, 100
26608, V, 1, 1, 1, 1, 0, 704, 100
26609, V, 1, 1, 1, 1, 0, 704, 100
26610, V, 1, 1, 1, 1, 0, 704, 100
26611, V, 1, 1, 1, 1, 0, 704, 100
26612, V, 1, 1, 1, 1, 0, 704, 100
26613, V, 1, 1, 1, 1, 0, 704, 100
26614, V, 1, 1, 1, 1, 0, 704, 100
26615, V, 1, 1, 1, 1, 0, 704, 100
26616, V, 1, 1, 1, 1, 0, 704, 100
26617, V, 1, 1, 1, 1, 0, 704, 100
26618, V, 1, 1, 1, 1, 0, 704, 100
26619, V, 1, 1, 1, 1, 0, 704, 100
26620, V, 1, 1, 1, 1, 0, 704, 100
26621, V, 1, 1, 1, 1, 0, 704, 100
26622, V, 1, 1, 1, 1, 0, 704, 100
26624, V, 1, 1, 1, 1, 0, 704, 100
26625, V, 1, 1, 1, 1, 0, 704, 100
26626, V, 1, 1, 1, 1, 0, 704, 100
26627, V, 1, 1, 1, 1, 0, 704, 100
26628, V, 1, 1, 1, 1, 0, 704, 100
26629, V, 1, 1, 1, 1, 0, 704, 100
26630, V, 1, 1, 1, 1, 0, 704, 100
26631, V, 1, 1, 1, 1, 0, 704, 100
26632, V, 1, 1, 1, 1, 0, 704, 100
26633, V, 1, 1, 1, 1, 0, 704, 100
26634, V, 1, 1, 1, 1, 0, 704, 100
26635, V, 1, 1, 1, 1, 0, 704, 100
26636, V, 1, 1, 1, 1, 0, 704, 100
26637, V, 1, 1, 1, 1, 0, 704, 100
26638, V, 1, 1, 1, 1, 0, 704, 100
26639, V, 1, 1, 1, 1, 0, 704, 100
26640, V, 1, 1, 1, 1, 0, 704, 100
26641, V, 1, 1, 1, 1, 0, 704, 100
26642, V, 1, 1, 1, 1, 0, 704, 100
26643, V, 1, 1, 1, 1, 0, 704, 100
26644, V, 1, 1, 1, 1, 0, 704, 100
26645, V, 1, 1, 1, 1, 0, 704, 100
26646, V, 1, 1, 1, 1, 0, 704, 100
26647, V, 1, 1, 1, 1, 0, 704, 100
26648, V, 1, 1, 1, 1, 0, 704, 100
26649, V, 1, 1, 1, 1, 0, 704, 100
26650, V, 1, 1, 1, 1, 0, 704, 99
26651, V, 1, 1, 1, 1, 0, 704, 100
26652, V, 1, 1, 1, 1, 0, 704, 100
26653, V, 1, 1, 1, 1, 0, 704, 99
26654, V, 1, 1, 1, 1, 0, 704, 100
26655, V, 1, 1, 1, 1, 0, 704, 100
26656, V, 1, 1, 1, 1, 0, 704, 100
26657, V, 1, 1, 1, 1, 0, 704, 100
26658, V, 1, 1, 1, 1, 0, 704, 99
26659, V, 1, 1, 1, 1, 0, 704, 100
26660, V, 1, 1, 1, 1, 0, 704, 100
26661, V, 1, 1, 1, 1, 0, 704, 100
26662, V, 1, 1, 1, 1, 0, 704, 100
26663, V, 1, 1, 1, 1, 0, 704, 100
26664, V, 1, 1, 1, 1, 0, 704, 100
26665, V, 1, 1, 1, 1, 0, 704, 100
26667, V, 1, 1, 1, 1, 0, 704, 100
26668, V, 1, 1, 1, 1, 0, 704, 100
26669, V, 1, 1, 1, 1, 0, 704, 100
26670, V, 1, 1, 1, 1, 0, 704, 100
26671, V, 1, 1, 1, 1, 0, 704, 99
26672, V, 1, 1, 1, 1, 0, 704, 100
26673, V, 1, 1, 1, 1, 0, 704, 99
26674, V, 1, 1, 1, 1, 0, 704, 100
26675, V, 1, 1, 1, 1, 0, 704, 100
26676, V, 1, 1, 1, 1, 0, 704, 100
26677, V, 1, 1, 1, 1, 0, 704, 100
26678, V, 1, 1, 1, 1, 0, 704, 100
26679, V, 1, 1, 1, 1, 0, 704, 100
26680, V, 1, 1, 1, 1, 0, 704, 100
26681, V, 1, 1, 1, 1, 0, 704, 100
26682, V, 1, 1, 1, 1, 0, 704, 100
26683, V, 1, 1, 1, 1, 0, 704, 100
26684, V, 1, 1, 1, 1, 0, 704, 100
26685, V, 1, 1, 1, 1, 0, 704, 100
26686, V, 1, 1, 1, 1, 0, 704, 100
26687, V, 1, 1, 1, 1, 0, 704, 100
26688, V, 1, 1, 1, 1, 0, 704, 100
26689, V, 1, 1, 1, 1, 0, 704, 100
26690, V, 1, 1, 1, 1, 0, 704, 100
26691, V, 1, 1, 1, 1, 0, 704, 100
26692, V, 1, 1, 1, 1, 0, 704, 100
26693, V, 1, 1, 1, 1, 0, 704, 100
26694, V, 1, 1, 1, 1, 0, 704, 100
26695, V, 1, 1, 1, 1, 0, 704, 100
26696, V, 1, 1, 1, 1, 0, 704, 100
26697, V, 1, 1, 1, 1, 0, 704, 100
26698, V, 1, 1, 1, 1, 0, 704, 100
26699, V, 1, 1, 1, 1, 0, 704, 100
26700, V, 1, 1, 1, 1, 0, 704, 100
26701, V, 1, 1, 1, 1, 0, 704, 100
26702, V, 1, 1, 1, 1, 0, 704, 100
26703, V, 1, 1, 1, 1, 0, 704, 100
26704, V, 1, 1, 1, 1, 0, 704, 100
26705, V, 1, 1, 1, 1, 0, 704, 100
26706, V, 1, 1, 1, 1, 0, 704, 100
26707, V, 1, 1, 1, 1, 0, 704, 100
26708, V, 1, 1, 1, 1, 0, 704, 100
26710, V, 1, 1, 1, 1, 0, 704, 100
26711, V, 1, 1, 1, 1, 0, 704, 100
26712, V, 1, 1, 1, 1, 0, 704, 100
26713, V, 1, 1, 1, 1, 0, 704, 100
26714, V, 1, 1, 1, 1, 0, 704, 99
26715, V, 1, 1, 1, 1, 0, 704, 100
26716, V, 1, 1, 1, 1, 0, 704, 100
26717, V, 1, 1, 1, 1, 0, 704, 100
26718, V, 1, 1, 1, 1, 0, 704, 100
26719, V, 1, 1, 1, 1, 0, 704, 100
26720, V, 1, 1, 1, 1, 0, 704, 100
26721, V, 1, 1, 1, 1, 0, 704, 100
26722, V, 1, 1, 1, 1, 0, 704, 100
26723, V, 1, 1, 1, 1, 0, 704, 100
26724, V, 1, 1, 1, 1, 0, 704, 100
26725, V, 1, 1, 1, 1, 0, 704, 100
26726, V, 1, 1, 1, 1, 0, 704, 100
26727, V, 1, 1, 1, 1, 0, 704, 100
26728, V, 1, 1, 1, 1, 0, 704, 100
26729, V, 1, 1, 1, 1, 0, 704, 100
26730, V, 1, 1, 1, 1, 0, 704, 99
26731, V, 1, 1, 1, 1, 0, 704, 100
26732, V, 1, 1, 1, 1, 0, 704, 100
26733, V, 1, 1, 1, 1, 0, 704, 99
26734, V, 1, 1, 1, 1, 0, 704, 99
26735, V, 1, 1, 1, 1, 0, 704, 100
26736, V, 1, 1, 1, 1, 0, 704, 100
26737, V, 1, 1, 1, 1, 0, 704, 100
26738, V, 1, 1, 1, 1, 0, 704, 100
26739, V, 1, 1, 1, 1, 0, 704, 100
26740, V, 1, 1, 1, 1, 0, 704, 100
26741, V, 1, 1, 1, 1, 0, 704, 99
26742, V, 1, 1, 1, 1, 0, 704, 100
26743, V, 1, 1, 1, 1, 0, 704, 100
26744, V, 1, 1, 1, 1, 0, 704, 100
26745, V, 1, 1, 1, 1, 0, 704, 100
26746, V, 1, 1, 1, 1, 0, 704, 100
26747, V, 1, 1, 1, 1, 0, 704, 100
26748, V, 1, 1, 1, 1, 0, 704, 100
26749, V, 1, 1, 1, 1, 0, 704, 99
26750, V, 1, 1, 1, 1, 0, 704, 100
26752, V, 1, 1, 1, 1, 0, 704, 100
26753, V, 1, 1, 1, 1, 0, 704, 100
26754, V, 1, 1, 1, 1, 0, 704, 100
26755, V, 1, 1, 1, 1, 0, 704, 100
26756, V, 1, 1, 1, 1, 0, 704, 100
26757, V, 1, 1, 1, 1, 0, 704, 100
26758, V, 1, 1, 1, 1, 0, 704, 100
26759, V, 1, 1, 1, 1, 0, 704, 100
26760, V, 1, 1, 1, 1, 0, 704, 100
26761, V, 1, 1, 1, 1, 0, 704, 100
26762, V, 1, 1, 1, 1, 0, 704, 100
26763, V, 1, 1, 1, 1, 0, 704, 100
26764, V, 1, 1, 1, 1, 0, 704, 100
26765, V, 1, 1, 1, 1, 0, 704, 100
26766, V, 1, 1, 1, 1, 0, 704, 100
26767, V, 1, 1, 1, 1, 0, 704, 100
26768, V, 1, 1, 1, 1, 0, 704, 100
26769, V, 1, 1, 1, 1, 0, 704, 100
26770, V, 1, 1, 1, 1, 0, 704, 100
26771, V, 1, 1, 1, 1, 0, 704, 100
26772, V, 1, 1, 1, 1, 0, 704, 100
26773, V, 1, 1, 1, 1, 0, 704, 100
26774, V, 1, 1, 1, 1, 0, 704, 100
26775, V, 1, 1, 1, 1, 0, 704, 100
26776, V, 1, 1, 1, 1, 0, 704, 100
26777, V, 1, 1, 1, 1, 0, 704, 100
26778, V, 1, 1, 1, 1, 0, 704, 100
26779, V, 1, 1, 1, 1, 0, 704, 100
26780, V, 1, 1, 1, 1, 0, 704, 100
26781, V, 1, 1, 1, 1, 0, 704, 100
26782, V, 1, 1, 1, 1, 0, 704, 100
26783, V, 1, 1, 1, 1, 0, 704, 100
26784, V, 1, 1, 1, 1, 0, 704, 100
26785, V, 1, 1, 1, 1, 0, 704, 100
26786, V, 1, 1, 1, 1, 0, 704, 100
26787, V, 1, 1, 1, 1, 0, 704, 100
26788, V, 1, 1, 1, 1, 0, 704, 100
26789, V, 1, 1, 1, 1, 0, 704, 100
26790, V, 1, 1, 1, 1, 0, 704, 100
26791, V, 1, 1, 1, 1, 0, 704, 100
26792, V, 1, 1, 1, 1, 0, 704, 99
26793, V, 1, 1, 1, 1, 0, 704, 100
26795, V, 1, 1, 1, 1, 0, 704, 100
26796, V, 1, 1, 1, 1, 0, 704, 99
26797, V, 1, 1, 1, 1, 0, 704, 99
26798, V, 1, 1, 1, 1, 0, 704, 100
26799, V, 1, 1, 1, 1, 0, 704, 99
26800, V, 1, 1, 1, 1, 0, 704, 100
26801, V, 1, 1, 1, 1, 0, 704, 99
26802, V, 1, 1, 1, 1, 0, 704, 99
26803, V, 1, 1, 1, 1, 0, 704, 99
26804, V, 1, 1, 1, 1, 0, 704, 99
26805, V, 1, 1, 1, 1, 0, 704, 99
26806, V, 1, 1, 1, 1, 0, 704, 99
26807, V, 1, 1, 1, 1, 0, 704, 99
26808, V, 1, 1, 1, 1, 0, 704, 99
26809, V, 1, 1, 1, 1, 0, 704, 99
26810, V, 1, 1, 1, 1, 0, 704, 99
26811, V, 1, 1, 1, 1, 0, 704, 99
26812, V, 1, 1, 1, 1, 0, 704, 99
26813, V, 1, 1, 1, 1, 0, 704, 99
26814, V, 1, 1, 1, 1, 0, 704, 100
26815, V, 1, 1, 1, 1, 0, 704, 99
26816, V, 1, 1, 1, 1, 0, 704, 100
26817, V, 1, 1, 1, 1, 0, 704, 99
26818, V, 1, 1, 1, 1, 0, 704, 99
26819, V, 1, 1, 1, 1, 0, 704, 100
26820, V, 1, 1, 1, 1, 0, 704, 99
26821, V, 1, 1, 1, 1, 0, 704, 100
26822, V, 1, 1, 1, 1, 0, 704, 100
26823, V, 1, 1, 1, 1, 0, 704, 100
26824, V, 1, 1, 1, 1, 0, 704, 100
26825, V, 1, 1, 1, 1, 0, 704, 99
26826, V, 1, 1, 1, 1, 0, 704, 100
26827, V, 1, 1, 1, 1, 0, 704, 100
26828, V, 1, 1, 1, 1, 0, 704, 100
26829, V, 1, 1, 1, 1, 0, 704, 100
26830, V, 1, 1, 1, 1, 0, 704, 100
26831, V, 1, 1, 1, 1, 0, 704, 100
26832, V, 1, 1, 1, 1, 0, 704, 100
26833, V, 1, 1, 1, 1, 0, 704, 100
26834, V, 1, 1, 1, 1, 0, 704, 100
26835, V, 1, 1, 1, 1, 0, 704, 100
26836, V, 1, 1, 1, 1, 0, 704, 100
26838, V, 1, 1, 1, 1, 0, 704, 100
26839, V, 1, 1, 1, 1, 0, 704, 100
26840, V, 1, 1, 1, 1, 0, 704, 100
26841, V, 1, 1, 1, 1, 0, 704, 100
26842, V, 1, 1, 1, 1, 0, 704, 100
26843, V, 1, 1, 1, 1, 0, 704, 100
26844, V, 1, 1, 1, 1, 0, 704, 100
26845, V, 1, 1, 1, 1, 0, 704, 100
26846, V, 1, 1, 1, 1, 0, 704, 100
26847, V, 1, 1, 1, 1, 0, 704, 100
26848, V, 1, 1, 1, 1, 0, 704, 100
26849, V, 1, 1, 1, 1, 0, 704, 100
26850, V, 1, 1, 1, 1, 0, 704, 100
26851, V, 1, 1, 1, 1, 0, 704, 100
26852, V, 1, 1, 1, 1, 0, 704, 100
26853, V, 1, 1, 1, 1, 0, 704, 100
26854, V, 1, 1, 1, 1, 0, 704, 100
26855, V, 1, 1, 1, 1, 0, 704, 100
26856, V, 1, 1, 1, 1, 0, 704, 99
26857, V, 1, 1, 1, 1, 0, 704, 100
26858, V, 1, 1, 1, 1, 0, 704, 100
26859, V, 1, 1, 1, 1, 0, 704, 100
26860, V, 1, 1, 1, 1, 0, 704, 100
26861, V, 1, 1, 1, 1, 0, 704, 100
26862, V, 1, 1, 1, 1, 0, 704, 100
26863, V, 1, 1, 1, 1, 0, 704, 100
26864, V, 1, 1, 1, 1, 0, 704, 100
26865, V, 1, 1, 1, 1, 0, 704, 100
26866, V, 1, 1, 1, 1, 0, 704, 100
26867, V, 1, 1, 1, 1, 0, 704, 100
26868, V, 1, 1, 1, 1, 0, 704, 100
26869, V, 1, 1, 1, 1, 0, 704, 100
26870, V, 1, 1, 1, 1, 0, 704, 100
26871, V, 1, 1, 1, 1, 0, 704, 100
26872, V, 1, 1, 1, 1, 0, 704, 100
26873, V, 1, 1, 1, 1, 0, 704, 99
26874, V, 1, 1, 1, 1, 0, 704, 100
26875, V, 1, 1, 1, 1, 0, 704, 100
26876, V, 1, 1, 1, 1, 0, 704, 100
26877, V, 1, 1, 1, 1, 0, 704, 100
26878, V, 1, 1, 1, 1, 0, 704, 100
26880, V, 1, 1, 1, 1, 0, 704, 100
26881, V, 1, 1, 1, 1, 0, 704, 100
26882, V, 1, 1, 1, 1, 0, 704, 100
26883, V, 1, 1, 1, 1, 0, 704, 100
26884, V, 1, 1, 1, 1, 0, 704, 99
26885, V, 1, 1, 1, 1, 0, 704, 100
26886, V, 1, 1, 1, 1, 0, 704, 99
26887, V, 1, 1, 1, 1, 0, 704, 100
26888, V, 1, 1, 1, 1, 0, 704, 100
26889, V, 1, 1, 1, 1, 0, 704, 100
26890, V, 1, 1, 1, 1, 0, 704, 100
26891, V, 1, 1, 1, 1, 0, 704, 100
26892, V, 1, 1, 1, 1, 0, 704, 100
26893, V, 1, 1, 1, 1, 0, 704, 100
26894, V, 1, 1, 1, 1, 0, 704, 99
26895, V, 1, 1, 1, 1, 0, 704, 100
26896, V, 1, 1, 1, 1, 0, 704, 100
26897, V, 1, 1, 1, 1, 0, 704, 100
26898, V, 1, 1, 1, 1, 0, 704, 100
26899, V, 1, 1, 1, 1, 0, 704, 100
26900, V, 1, 1, 1, 1, 0, 704, 100
26901, V, 1, 1, 1, 1, 0, 704, 100
26902, V, 1, 1, 1, 1, 0, 704, 100
26903, V, 1, 1, 1, 1, 0, 704, 100
26904, V, 1, 1, 1, 1, 0, 704, 100
26905, V, 1, 1, 1, 1, 0, 704, 100
26906, V, 1, 1, 1, 1, 0, 704, 100
26907, V, 1, 1, 1, 1, 0, 704, 100
26908, V, 1, 1, 1, 1, 0, 704, 100
26909, V, 1, 1, 1, 1, 0, 704, 100
26910, V, 1, 1, 1, 1, 0, 704, 100
26911, V, 1, 1, 1, 1, 0, 704, 100
26912, V, 1, 1, 1, 1, 0, 704, 100
26913, V, 1, 1, 1, 1, 0, 704, 100
26914, V, 1, 1, 1, 1, 0, 704, 100
26915, V, 1, 1, 1, 1, 0, 704, 100
26916, V, 1, 1, 1, 1, 0, 704, 100
26917, V, 1, 1, 1, 1, 0, 704, 100
26918, V, 1, 1, 1, 1, 0, 704, 100
26919, V, 1, 1, 1, 1, 0, 704, 100
26920, V, 1, 1, 1, 1, 0, 704, 100
26921, V, 1, 1, 1, 1, 0, 704, 100
26923, V, 1, 1, 1, 1, 0, 704, 100
26924, V, 1, 1, 1, 1, 0, 704, 100
26925, V, 1, 1, 1, 1, 0, 704, 100
26926, V, 1, 1, 1, 1, 0, 704, 100
26927, V, 1, 1, 1, 1, 0, 704, 100
26928, V, 1, 1, 1, 1, 0, 704, 100
26929, V, 1, 1, 1, 1, 0, 704, 100
26930, V, 1, 1, 1, 1, 0, 704, 100
26931, V, 1, 1, 1, 1, 0, 704, 100
26932, V, 1, 1, 1, 1, 0, 704, 100
26933, V, 1, 1, 1, 1, 0, 704, 100
26934, V, 1, 1, 1, 1, 0, 704, 100
26935, V, 1, 1, 1, 1, 0, 704, 100
26936, V, 1, 1, 1, 1, 0, 704, 100
26937, V, 1, 1, 1, 1, 0, 704, 100
26938, V, 1, 1, 1, 1, 0, 704, 100
26939, V, 1, 1, 1, 1, 0, 704, 100
26940, V, 1, 1, 1, 1, 0, 704, 100
26941, V, 1, 1, 1, 1, 0, 704, 100
26942, V, 1, 1, 1, 1, 0, 704, 100
26943, V, 1, 1, 1, 1, 0, 704, 100
26944, V, 1, 1, 1, 1, 0, 704, 100
26945, V, 1, 1, 1, 1, 0, 704, 100
26946, V, 1, 1, 1, 1, 0, 704, 100
26947, V, 1, 1, 1, 1, 0, 704, 100
26948, V, 1, 1, 1, 1, 0, 704, 100
26949, V, 1, 1, 1, 1, 0, 704, 100
26950, V, 1, 1, 1, 1, 0, 704, 100
26951, V, 1, 1, 1, 1, 0, 704, 100
26952, V, 1, 1, 1, 1, 0, 704, 100
26953, V, 1, 1, 1, 1, 0, 704, 100
26954, V, 1, 1, 1, 1, 0, 704, 100
26955, V, 1, 1, 1, 1, 0, 704, 100
26956, V, 1, 1, 1, 1, 0, 704, 100
26957, V, 1, 1, 1, 1, 0, 704, 100
26958, V, 1, 1, 1, 1, 0, 704, 100
26959, V, 1, 1, 1, 1, 0, 704, 100
26960, V, 1, 1, 1, 1, 0, 704, 100
26961, V, 1, 1, 1, 1, 0, 704, 100
26962, V, 1, 1, 1, 1, 0, 704, 100
26963, V, 1, 1, 1, 1, 0, 704, 100
26964, V, 1, 1, 1, 1, 0, 704, 100
26966, V, 1, 1, 1, 1, 0, 704, 100
26967, V, 1, 1, 1, 1, 0, 704, 100
26968, V, 1, 1, 1, 1, 0, 704, 100
26969, V, 1, 1, 1, 1, 0, 704, 100
26970, V, 1, 1, 1, 1, 0, 704, 100
26971, V, 1, 1, 1, 1, 0, 704, 100
26972, V, 1, 1, 1, 1, 0, 704, 100
26973, V, 1, 1, 1, 1, 0, 704, 100
26974, V, 1, 1, 1, 1, 0, 704, 100
26975, V, 1, 1, 1, 1, 0, 704, 100
26976, V, 1, 1, 1, 1, 0, 704, 100
26977, V, 1, 1, 1, 1, 0, 704, 100
26978, V, 1, 1, 1, 1, 0, 704, 100
26979, V, 1, 1, 1, 1, 0, 704, 100
26980, V, 1, 1, 1, 1, 0, 704, 100
26981, V, 1, 1, 1, 1, 0, 704, 100
26982, V, 1, 1, 1, 1, 0, 704, 100
26983, V, 1, 1, 1, 1, 0, 704, 100
26984, V, 1, 1, 1, 1, 0, 704, 100
26985, V, 1, 1, 1, 1, 0, 704, 100
26986, V, 1, 1, 1, 1, 0, 704, 100
26987, V, 1, 1, 1, 1, 0, 704, 100
26988, V, 1, 1, 1, 1, 0, 704, 100
26989, V, 1, 1, 1, 1, 0, 704, 100
26990, V, 1, 1, 1, 1, 0, 704, 100
26991, V, 1, 1, 1, 1, 0, 704, 100
26992, V, 1, 1, 1, 1, 0, 704, 100
26993, V, 1, 1, 1, 1, 0, 704, 100
26994, V, 1, 1, 1, 1, 0, 704, 100
26995, V, 1, 1, 1, 1, 0, 704, 100
26996, V, 1, 1, 1, 1, 0, 704, 100
26997, V, 1, 1, 1, 1, 0, 704, 100
26998, V, 1, 1, 1, 1, 0, 704, 100
26999, V, 1, 1, 1, 1, 0, 704, 100
27000, V, 1, 1, 1, 1, 0, 704, 100
27001, V, 1, 1, 1, 1, 0, 704, 100
27002, V, 1, 1, 1, 1, 0, 704, 100
27003, V, 1, 1, 1, 1, 0, 704, 100
27004, V, 1, 1, 1, 1, 0, 704, 100
27005, V, 1, 1, 1, 1, 0, 704, 100
27006, V, 1, 1, 1, 1, 0, 704, 100
27008, V, 1, 1, 1, 1, 0, 704, 100
27009, V, 1, 1, 1, 1, 0, 704, 100
27010, V, 1, 1, 1, 1, 0, 704, 100
27011, V, 1, 1, 1, 1, 0, 704, 100
27012, V, 1, 1, 1, 1, 0, 704, 100
27013, V, 1, 1, 1, 1, 0, 704, 100
27014, V, 1, 1, 1, 1, 0, 704, 100
27015, V, 1, 1, 1, 1, 0, 704, 100
27016, V, 1, 1, 1, 1, 0, 704, 100
27017, V, 1, 1, 1, 1, 0, 704, 100
27018, V, 1, 1, 1, 1, 0, 704, 100
27019, V, 1, 1, 1, 1, 0, 704, 100
27020, V, 1, 1, 1, 1, 0, 704, 100
27021, V, 1, 1, 1, 1, 0, 704, 100
27022, V, 1, 1, 1, 1, 0, 704, 100
27023, V, 1, 1, 1, 1, 0, 704, 100
27024, V, 1, 1, 1, 1, 0, 704, 100
27025, V, 1, 1, 1, 1, 0, 704, 100
27026, V, 1, 1, 1, 1, 0, 704, 100
27027, V, 1, 1, 1, 1, 0, 704, 100
27028, V, 1, 1, 1, 1, 0, 704, 100
27029, V, 1, 1, 1, 1, 0, 704, 100
27030, V, 1, 1, 1, 1, 0, 704, 100
27031, V, 1, 1, 1, 1, 0, 704, 100
27032, V, 1, 1, 1, 1, 0, 704, 100
27033, V, 1, 1, 1, 1, 0, 704, 100
27034, V, 1, 1, 1, 1, 0, 704, 100
27035, V, 1, 1, 1, 1, 0, 704, 100
27036, V, 1, 1, 1, 1, 0, 704, 100
27037, V, 1, 1, 1, 1, 0, 704, 100
27038, V, 1, 1, 1, 1, 0, 704, 100
27039, V, 1, 1, 1, 1, 0, 704, 100
27040, V, 1, 1, 1, 1, 0, 704, 100
27041, V, 1, 1, 1, 1, 0, 704, 100
27042, V, 1, 1, 1, 1, 0, 704, 100
27043, V, 1, 1, 1, 1, 0, 704, 100
27044, V, 1, 1, 1, 1, 0, 704, 100
27045, V, 1, 1, 1, 1, 0, 704, 100
27046, V, 1, 1, 1, 1, 0, 704, 100
27047, V, 1, 1, 1, 1, 0, 704, 100
27048, V, 1, 1, 1, 1, 0, 704, 100
27049, V, 1, 1, 1, 1, 0, 704, 100
27051, V, 1, 1, 1, 1, 0, 704, 100
27052, V, 1, 1, 1, 1, 0, 704, 100
27053, V, 1, 1, 1, 1, 0, 704, 100
27054, V, 1, 1, 1, 1, 0, 704, 100
27055, V, 1, 1, 1, 1, 0, 704, 100
27056, V, 1, 1, 1, 1, 0, 704, 100
27057, V, 1, 1, 1, 1, 0, 704, 100
27058, V, 1, 1, 1, 1, 0, 704, 100
27059, V, 1, 1, 1, 1, 0, 704, 100
27060, V, 1, 1, 1, 1, 0, 704, 100
27061, V, 1, 1, 1, 1, 0, 704, 100
27062, V, 1, 1, 1, 1, 0, 704, 100
27063, V, 1, 1, 1, 1, 0, 704, 100
27064, V, 1, 1, 1, 1, 0, 704, 100
27065, V, 1, 1, 1, 1, 0, 704, 100
27066, V, 1, 1, 1, 1, 0, 704, 100
27067, V, 1, 1, 1, 1, 0, 704, 100
27068, V, 1, 1, 1, 1, 0, 704, 100
27069, V, 1, 1, 1, 1, 0, 704, 100
27070, V, 1, 1, 1, 1, 0, 704, 100
27071, V, 1, 1, 1, 1, 0, 704, 100
27072, V, 1, 1, 1, 1, 0, 704, 100
27073, V, 1, 1, 1, 1, 0, 704, 100
27074, V, 1, 1, 1, 1, 0, 704, 100
27075, V, 1, 1, 1, 1, 0, 704, 100
27076, V, 1, 1, 1, 1, 0, 704, 100
27077, V, 1, 1, 1, 1, 0, 704, 100
27078, V, 1, 1, 1, 1, 0, 704, 100
27079, V, 1, 1, 1, 1, 0, 704, 100
27080, V, 1, 1, 1, 1, 0, 704, 100
27081, V, 1, 1, 1, 1, 0, 704, 100
27082, V, 1, 1, 1, 1, 0, 704, 100
27083, V, 1, 1, 1, 1, 0, 704, 100
27084, V, 1, 1, 1, 1, 0, 704, 100
27085, V, 1, 1, 1, 1, 0, 704, 100
27086, V, 1, 1, 1, 1, 0, 704, 100
27087, V, 1, 1, 1, 1, 0, 704, 100
27088, V, 1, 1, 1, 1, 0, 704, 100
27089, V, 1, 1, 1, 1, 0, 704, 100
27090, V, 1, 1, 1, 1, 0, 704, 100
27091, V, 1, 1, 1, 1, 0, 704, 100
27092, V, 1, 1, 1, 1, 0, 704, 100
27094, V, 1, 1, 1, 1, 0, 704, 100
27095, V, 1, 1, 1, 1, 0, 704, 100
27096, V, 1, 1, 1, 1, 0, 704, 100
27097, V, 1, 1, 1, 1, 0, 704, 100
27098, V, 1, 1, 1, 1, 0, 704, 100
27099, V, 1, 1, 1, 1, 0, 704, 100
27100, V, 1, 1, 1, 1, 0, 704, 100
27101, V, 1, 1, 1, 1, 0, 704, 100
27102, V, 1, 1, 1, 1, 0, 704, 100
27103, V, 1, 1, 1, 1, 0, 704, 100
27104, V, 1, 1, 1, 1, 0, 704, 100
27105, V, 1, 1, 1, 1, 0, 704, 100
27106, V, 1, 1, 1, 1, 0, 704, 99
27107, V, 1, 1, 1, 1, 0, 704, 100
27108, V, 1, 1, 1, 1, 0, 704, 99
27109, V, 1, 1, 1, 1, 0, 704, 99
27110, V, 1, 1, 1, 1, 0, 704, 100
27111, V, 1, 1, 1, 1, 0, 704, 99
27112, V, 1, 1, 1, 1, 0, 704, 100
27113, V, 1, 1, 1, 1, 0, 704, 100
27114, V, 1, 1, 1, 1, 0, 704, 100
27115, V, 1, 1, 1, 1, 0, 704, 100
27116, V, 1, 1, 1, 1, 0, 704, 100
27117, V, 1, 1, 1, 1, 0, 704, 100
27118, V, 1, 1, 1, 1, 0, 704, 100
27119, V, 1, 1, 1, 1, 0, 704, 100
27120, V, 1, 1, 1, 1, 0, 704, 100
27121, V, 1, 1, 1, 1, 0, 704, 100
27122, V, 1, 1, 1, 1, 0, 704, 100
27123, V, 1, 1, 1, 1, 0, 704, 100
27124, V, 1, 1, 1, 1, 0, 704, 100
27125, V, 1, 1, 1, 1, 0, 704, 100
27126, V, 1, 1, 1, 1, 0, 704, 100
27127, V, 1, 1, 1, 1, 0, 704, 100
27128, V, 1, 1, 1, 1, 0, 704, 100
27129, V, 1, 1, 1, 1, 0, 704, 100
27130, V, 1, 1, 1, 1, 0, 704, 99
27131, V, 1, 1, 1, 1, 0, 704, 100
27132, V, 1, 1, 1, 1, 0, 704, 100
27133, V, 1, 1, 1, 1, 0, 704, 100
27134, V, 1, 1, 1, 1, 0, 704, 100
27136, V, 1, 1, 1, 1, 0, 704, 100
27137, V, 1, 1, 1, 1, 0, 704, 100
27138, V, 1, 1, 1, 1, 0, 704, 100
27139, V, 1, 1, 1, 1, 0, 704, 100
27140, V, 1, 1, 1, 1, 0, 704, 100
27141, V, 1, 1, 1, 1, 0, 704, 100
27142, V, 1, 1, 1, 1, 0, 704, 100
27143, V, 1, 1, 1, 1, 0, 704, 100
27144, V, 1, 1, 1, 1, 0, 704, 100
27145, V, 1, 1, 1, 1, 0, 704, 100
27146, V, 1, 1, 1, 1, 0, 704, 100
27147, V, 1, 1, 1, 1, 0, 704, 100
27148, V, 1, 1, 1, 1, 0, 704, 100
27149, V, 1, 1, 1, 1, 0, 704, 100
27150, V, 1, 1, 1, 1, 0, 704, 100
27151, V, 1, 1, 1, 1, 0, 704, 100
27152, V, 1, 1, 1, 1, 0, 704, 100
27153, V, 1, 1, 1, 1, 0, 704, 100
27154, V, 1, 1, 1, 1, 0, 704, 100
27155, V, 1, 1, 1, 1, 0, 704, 100
27156, V, 1, 1, 1, 1, 0, 704, 100
27157, V, 1, 1, 1, 1, 0, 704, 100
27158, V, 1, 1, 1, 1, 0, 704, 100
27159, V, 1, 1, 1, 1, 0, 704, 100
27160, V, 1, 1, 1, 1, 0, 704, 100
27161, V, 1, 1, 1, 1, 0, 704, 100
27162, V, 1, 1, 1, 1, 0, 704, 100
27163, V, 1, 1, 1, 1, 0, 704, 100
27164, V, 1, 1, 1, 1, 0, 704, 100
27165, V, 1, 1, 1, 1, 0, 704, 100
27166, V, 1, 1, 1, 1, 0, 704, 100
27167, V, 1, 1, 1, 1, 0, 704, 100
27168, V, 1, 0, 0, 1, 0, 704, 100
27168, V, 1, 0, 0, 0, 0, 704, 100
27169, V, 1, 1, 0, 0, 0, 704, 100
27169, V, 1, 1, 0, 0, 0, 704, 100
27170, V, 1, 1, 1, 1, 0, 704, 100
27171, V, 1, 1, 1, 1, 0, 704, 100
27172, V, 1, 1, 1, 1, 0, 704, 100
27173, V, 1, 1, 1, 1, 0, 704, 99
27174, V, 1, 1, 1, 1, 0, 704, 99
27175, V, 1, 1, 1, 1, 0, 704, 99
27176, V, 1, 1, 1, 1, 0, 704, 99
27177, V, 1, 1, 1, 1, 0, 704, 99
27179, V, 1, 1, 1, 1, 0, 704, 99
27180, V, 1, 1, 1, 1, 0, 704, 99
27181, V, 1, 1, 1, 1, 0, 704, 99
27182, V, 1, 1, 1, 1, 0, 704, 99
27183, V, 1, 1, 1, 1, 0, 704, 99
27184, V, 1, 1, 1, 1, 0, 704, 99
27185, V, 1, 1, 1, 1, 0, 704, 99
27186, V, 1, 1, 1, 1, 0, 704, 99
27187, V, 1, 1, 1, 1, 0, 704, 99
27188, V, 1, 1, 1, 1, 0, 704, 99
27189, V, 1, 1, 1, 1, 0, 704, 99
27190, V, 1, 1, 1, 1, 0, 704, 99
27191, V, 1, 1, 1, 1, 0, 704, 99
27192, V, 1, 1, 1, 1, 0, 704, 99
27193, V, 1, 1, 1, 1, 0, 704, 99
27194, V, 1, 1, 1, 1, 0, 704, 99
27195, V, 1, 1, 1, 1, 0, 704, 99
27196, V, 1, 1, 1, 1, 0, 704, 99
27197, V, 1, 1, 1, 1, 0, 704, 99
27198, V, 1, 1, 1, 1, 0, 704, 99
27199, V, 1, 1, 1, 1, 0, 704, 99
27200, V, 1, 1, 1, 1, 0, 704, 99
27201, V, 1, 1, 1, 1, 0, 704, 99
27202, V, 1, 1, 1, 1, 0, 704, 99
27203, V, 1, 1, 1, 1, 0, 704, 99
27204, V, 1, 1, 1, 1, 0, 704, 99
27205, V, 1, 1, 1, 1, 0, 704, 99
27206, V, 1, 1, 1, 1, 0, 704, 99
27207, V, 1, 1, 1, 1, 0, 704, 99
27208, V, 1, 1, 1, 1, 0, 704, 99
27209, V, 1, 1, 1, 1, 0, 704, 99
27210, V, 1, 1, 1, 1, 0, 704, 99
27211, V, 1, 1, 1, 1, 0, 704, 99
27212, V, 1, 1, 1, 1, 0, 704, 99
27213, V, 1, 1, 1, 1, 0, 704, 99
27214, V, 1, 1, 1, 1, 0, 704, 99
27215, V, 1, 1, 1, 1, 0, 704, 99
27216, V, 1, 1, 1, 1, 0, 704, 99
27217, V, 1, 1, 1, 1, 0, 704, 99
27218, V, 1, 1, 1, 1, 0, 704, 99
27219, V, 1, 1, 1, 1, 0, 704, 99
27220, V, 1, 1, 1, 1, 0, 704, 100
27222, V, 1, 1, 1, 1, 0, 704, 100
27223, V, 1, 1, 1, 1, 0, 704, 100
27224, V, 1, 1, 1, 1, 0, 704, 100
27225, V, 1, 1, 1, 1, 0, 704, 100
27226, V, 1, 1, 1, 1, 0, 704, 100
27227, V, 1, 1, 1, 1, 0, 704, 100
27228, V, 1, 1, 1, 1, 0, 704, 100
27229, V, 1, 1, 1, 1, 0, 704, 99
27230, V, 1, 1, 1, 1, 0, 704, 100
27231, V, 1, 1, 1, 1, 0, 704, 100
27232, V, 1, 1, 1, 1, 0, 704, 100
27233, V, 1, 1, 1, 1, 0, 704, 100
27234, V, 1, 1, 1, 1, 0, 704, 100
27235, V, 1, 1, 1, 1, 0, 704, 100
27236, V, 1, 1, 1, 1, 0, 704, 99
27237, V, 1, 1, 1, 1, 0, 704, 99
27238, V, 1, 1, 1, 1, 0, 704, 100
27239, V, 1, 1, 1, 1, 0, 704, 99
27240, V, 1, 1, 1, 1, 0, 704, 100
27241, V, 1, 1, 1, 1, 0, 704, 99
27242, V, 1, 1, 1, 1, 0, 704, 99
27243, V, 1, 1, 1, 1, 0, 704, 100
27244, V, 1, 1, 1, 1, 0, 704, 99
27245, V, 1, 1, 1, 1, 0, 704, 100
27246, V, 1, 1, 1, 1, 0, 704, 99
27247, V, 1, 1, 1, 1, 0, 704, 99
27248, V, 1, 1, 1, 1, 0, 704, 99
27249, V, 1, 1, 1, 1, 0, 704, 99
27250, V, 1, 1, 1, 1, 0, 704, 99
27251, V, 1, 1, 1, 1, 0, 704, 99
27252, V, 1, 1, 1, 1, 0, 704, 99
27253, V, 1, 1, 1, 1, 0, 704, 99
27254, V, 1, 1, 1, 1, 0, 704, 99
27255, V, 1, 1, 1, 1, 0, 704, 99
27256, V, 1, 1, 1, 1, 0, 704, 99
27257, V, 1, 1, 1, 1, 0, 704, 99
27258, V, 1, 1, 1, 1, 0, 704, 99
27259, V, 1, 1, 1, 1, 0, 704, 99
27260, V, 1, 1, 1, 1, 0, 704, 99
27261, V, 1, 1, 1, 1, 0, 704, 99
27262, V, 1, 1, 1, 1, 0, 704, 99
27264, V, 1, 1, 1, 1, 0, 704, 99
27265, V, 1, 1, 1, 1, 0, 704, 99
27266, V, 1, 1, 1, 1, 0, 704, 99
27267, V, 1, 1, 1, 1, 0, 704, 99
27268, V, 1, 1, 1, 1, 0, 704, 99
27269, V, 1, 1, 1, 1, 0, 704, 99
27270, V, 1, 1, 1, 1, 0, 704, 99
27271, V, 1, 1, 1, 1, 0, 704, 99
27272, V, 1, 1, 1, 1, 0, 704, 99
27273, V, 1, 1, 1, 1, 0, 704, 99
27274, V, 1, 1, 1, 1, 0, 704, 99
27275, V, 1, 1, 1, 1, 0, 704, 99
27276, V, 1, 1, 1, 1, 0, 704, 99
27277, V, 1, 1, 1, 1, 0, 704, 99
27278, V, 1, 1, 1, 1, 0, 704, 100
27279, V, 1, 1, 1, 1, 0, 704, 99
27280, V, 1, 1, 1, 1, 0, 704, 99
27281, V, 1, 1, 1, 1, 0, 704, 100
27282, V, 1, 1, 1, 1, 0, 704, 100
27283, V, 1, 1, 1, 1, 0, 704, 99
27284, V, 1, 1, 1, 1, 0, 704, 99
27285, V, 1, 1, 1, 1, 0, 704, 100
27286, V, 1, 1, 1, 1, 0, 704, 100
27287, V, 1, 1, 1, 1, 0, 704, 100
27288, V, 1, 1, 1, 1, 0, 704, 100
27289, V, 1, 1, 1, 1, 0, 704, 99
27290, V, 1, 1, 1, 1, 0, 704, 100
27291, V, 1, 1, 1, 1, 0, 704, 100
27292, V, 1, 1, 1, 1, 0, 704, 100
27293, V, 1, 1, 1, 1, 0, 704, 100
27294, V, 1, 1, 1, 1, 0, 704, 100
27295, V, 1, 1, 1, 1, 0, 704, 100
27296, V, 1, 1, 1, 1, 0, 704, 100
27297, V, 1, 1, 1, 1, 0, 704, 100
27298, V, 1, 1, 1, 1, 0, 704, 100
27299, V, 1, 1, 1, 1, 0, 704, 100
27300, V, 1, 1, 1, 1, 0, 704, 100
27301, V, 1, 1, 1, 1, 0, 704, 100
27302, V, 1, 1, 1, 1, 0, 704, 100
27303, V, 1, 1, 1, 1, 0, 704, 100
27304, V, 1, 1, 1, 1, 0, 704, 100
27305, V, 1, 1, 1, 1, 0, 704, 100
27307, V, 1, 1, 1, 1, 0, 704, 100
27308, V, 1, 1, 1, 1, 0, 704, 100
27309, V, 1, 1, 1, 1, 0, 704, 100
27310, V, 1, 1, 1, 1, 0, 704, 100
27311, V, 1, 1, 1, 1, 0, 704, 100
27312, V, 1, 1, 1, 1, 0, 704, 100
27313, V, 1, 1, 1, 1, 0, 704, 100
27314, V, 1, 1, 1, 1, 0, 704, 100
27315, V, 1, 1, 1, 1, 0, 704, 100
27316, V, 1, 1, 1, 1, 0, 704, 100
27317, V, 1, 1, 1, 1, 0, 704, 100
27318, V, 1, 1, 1, 1, 0, 704, 100
27319, V, 1, 1, 1, 1, 0, 704, 99
27320, V, 1, 1, 1, 1, 0, 704, 100
27321, V, 1, 1, 1, 1, 0, 704, 100
27322, V, 1, 1, 1, 1, 0, 704, 100
27323, V, 1, 1, 1, 1, 0, 704, 100
27324, V, 1, 1, 1, 1, 0, 704, 100
27325, V, 1, 1, 1, 1, 0, 704, 100
27326, V, 1, 0, 0, 1, 0, 704, 100
27326, V, 1, 0, 0, 0, 0, 704, 100
27327, V, 1, 1, 0, 0, 0, 704, 100
27327, V, 1, 1, 0, 0, 0, 704, 100
27328, V, 1, 1, 1, 1, 0, 704, 99
27329, V, 1, 1, 1, 1, 0, 704, 100
27330, V, 1, 1, 1, 1, 0, 704, 99
27331, V, 1, 1, 1, 1, 0, 704, 99
27332, V, 1, 1, 1, 1, 0, 704, 99
27333, V, 1, 1, 1, 1, 0, 704, 99
27334, V, 1, 1, 1, 1, 0, 704, 99
27335, V, 1, 1, 1, 1, 0, 704, 99
27336, V, 1, 1, 1, 1, 0, 704, 99
27337, V, 1, 1, 1, 1, 0, 704, 99
27338, V, 1, 1, 1, 1, 0, 704, 99
27339, V, 1, 1, 1, 1, 0, 704, 99
27340, V, 1, 1, 1, 1, 0, 704, 99
27341, V, 1, 1, 1, 1, 0, 704, 99
27342, V, 1, 1, 1, 1, 0, 704, 99
27343, V, 1, 1, 1, 1, 0, 704, 99
27344, V, 1, 1, 1, 1, 0, 704, 99
27345, V, 1, 1, 1, 1, 0, 704, 99
27346, V, 1, 1, 1, 1, 0, 704, 99
27347, V, 1, 1, 1, 1, 0, 704, 99
27348, V, 1, 1, 1, 1, 0, 704, 99
27350, V, 1, 1, 1, 1, 0, 704, 99
27351, V, 1, 1, 1, 1, 0, 704, 99
27352, V, 1, 1, 1, 1, 0, 704, 99
27353, V, 1, 1, 1, 1, 0, 704, 99
27354, V, 1, 1, 1, 1, 0, 704, 99
27355, V, 1, 1, 1, 1, 0, 704, 99
27356, V, 1, 1, 1, 1, 0, 704, 99
27357, V, 1, 1, 1, 1, 0, 704, 99
27358, V, 1, 1, 1, 1, 0, 704, 99
27359, V, 1, 1, 1, 1, 0, 704, 99
27360, V, 1, 1, 1, 1, 0, 704, 99
27361, V, 1, 1, 1, 1, 0, 704, 99
27362, V, 1, 1, 1, 1, 0, 704, 99
27363, V, 1, 1, 1, 1, 0, 704, 99
27364, V, 1, 1, 1, 1, 0, 704, 99
27365, V, 1, 1, 1, 1, 0, 704, 99
27366, V, 1, 1, 1, 1, 0, 704, 99
27367, V, 1, 1, 1, 1, 0, 704, 99
27368, V, 1, 1, 1, 1, 0, 704, 99
27369, V, 1, 1, 1, 1, 0, 704, 99
27370, V, 1, 1, 1, 1, 0, 704, 99
27371, V, 1, 1, 1, 1, 0, 704, 99
27372, V, 1, 1, 1, 1, 0, 704, 99
27373, V, 1, 1, 1, 1, 0, 704, 99
27374, V, 1, 1, 1, 1, 0, 704, 99
27375, V, 1, 1, 1, 1, 0, 704, 99
27376, V, 1, 1, 1, 1, 0, 704, 99
27377, V, 1, 1, 1, 1, 0, 704, 99
27378, V, 1, 1, 1, 1, 0, 704, 99
27379, V, 1, 1, 1, 1, 0, 704, 99
27380, V, 1, 1, 1, 1, 0, 704, 99
27381, V, 1, 1, 1, 1, 0, 704, 99
27382, V, 1, 1, 1, 1, 0, 704, 99
27383, V, 1, 1, 1, 1, 0, 704, 99
27384, V, 1, 1, 1, 1, 0, 704, 99
27385, V, 1, 1, 1, 1, 0, 704, 100
27386, V, 1, 1, 1, 1, 0, 704, 99
27387, V, 1, 1, 1, 1, 0, 704, 99
27388, V, 1, 1, 1, 1, 0, 704, 99
27389, V, 1, 1, 1, 1, 0, 704, 99
27390, V, 1, 1, 1, 1, 0, 704, 99
27392, V, 1, 1, 1, 1, 0, 704, 99
27393, V, 1, 1, 1, 1, 0, 704, 99
27394, V, 1, 1, 1, 1, 0, 704, 99
27395, V, 1, 1, 1, 1, 0, 704, 99
27396, V, 1, 1, 1, 1, 0, 704, 99
27397, V, 1, 1, 1, 1, 0, 704, 99
27398, V, 1, 1, 1, 1, 0, 704, 99
27399, V, 1, 1, 1, 1, 0, 704, 99
27400, V, 1, 1, 1, 1, 0, 704, 99
27401, V, 1, 1, 1, 1, 0, 704, 99
27402, V, 1, 1, 1, 1, 0, 704, 99
27403, V, 1, 1, 1, 1, 0, 704, 99
27404, V, 1, 1, 1, 1, 0, 704, 99
27405, V, 1, 1, 1, 1, 0, 704, 99
27406, V, 1, 1, 1, 1, 0, 704, 99
27407, V, 1, 1, 1, 1, 0, 704, 99
27408, V, 1, 1, 1, 1, 0, 704, 99
27409, V, 1, 1, 1, 1, 0, 704, 99
27410, V, 1, 1, 1, 1, 0, 704, 99
27411, V, 1, 1, 1, 1, 0, 704, 99
27412, V, 1, 1, 1, 1, 0, 704, 99
27413, V, 1, 1, 1, 1, 0, 704, 99
27414, V, 1, 1, 1, 1, 0, 704, 99
27415, V, 1, 1, 1, 1, 0, 704, 99
27416, V, 1, 1, 1, 1, 0, 704, 99
27417, V, 1, 1, 1, 1, 0, 704, 99
27418, V, 1, 1, 1, 1, 0, 704, 99
27419, V, 1, 1, 1, 1, 0, 704, 99
27420, V, 1, 1, 1, 1, 0, 704, 99
27421, V, 1, 1, 1, 1, 0, 704, 99
27422, V, 1, 1, 1, 1, 0, 704, 99
27423, V, 1, 1, 1, 1, 0, 704, 99
27424, V, 1, 1, 1, 1, 0, 704, 99
27425, V, 1, 1, 1, 1, 0, 704, 99
27426, V, 1, 1, 1, 1, 0, 704, 99
27427, V, 1, 1, 1, 1, 0, 704, 99
27428, V, 1, 1, 1, 1, 0, 704, 99
27429, V, 1, 1, 1, 1, 0, 704, 99
27430, V, 1, 1, 1, 1, 0, 704, 99
27431, V, 1, 1, 1, 1, 0, 704, 99
27432, V, 1, 1, 1, 1, 0, 704, 99
27433, V, 1, 1, 1, 1, 0, 704, 99
27435, V, 1, 1, 1, 1, 0, 704, 99
27436, V, 1, 1, 1, 1, 0, 704, 99
27437, V, 1, 1, 1, 1, 0, 704, 99
27438, V, 1, 1, 1, 1, 0, 704, 99
27439, V, 1, 1, 1, 1, 0, 704, 99
27440, V, 1, 1, 1, 1, 0, 704, 99
27441, V, 1, 1, 1, 1, 0, 704, 100
27442, V, 1, 1, 1, 1, 0, 704, 100
27443, V, 1, 1, 1, 1, 0, 704, 99
27444, V, 1, 1, 1, 1, 0, 704, 99
27445, V, 1, 1, 1, 1, 0, 704, 99
27446, V, 1, 1, 1, 1, 0, 704, 99
27447, V, 1, 1, 1, 1, 0, 704, 99
27448, V, 1, 1, 1, 1, 0, 704, 100
27449, V, 1, 1, 1, 1, 0, 704, 99
27450, V, 1, 1, 1, 1, 0, 704, 99
27451, V, 1, 1, 1, 1, 0, 704, 100
27452, V, 1, 1, 1, 1, 0, 704, 99
27453, V, 1, 1, 1, 1, 0, 704, 100
27454, V, 1, 1, 1, 1, 0, 704, 100
27455, V, 1, 1, 1, 1, 0, 704, 99
27456, V, 1, 1, 1, 1, 0, 704, 100
27457, V, 1, 1, 1, 1, 0, 704, 100
27458, V, 1, 1, 1, 1, 0, 704, 99
27459, V, 1, 1, 1, 1, 0, 704, 99
27460, V, 1, 1, 1, 1, 0, 704, 100
27461, V, 1, 1, 1, 1, 0, 704, 100
27462, V, 1, 1, 1, 1, 0, 704, 100
27463, V, 1, 1, 1, 1, 0, 704, 100
27464, V, 1, 1, 1, 1, 0, 704, 100
27465, V, 1, 1, 1, 1, 0, 704, 100
27466, V, 1, 1, 1, 1, 0, 704, 100
27467, V, 1, 1, 1, 1, 0, 704, 99
27468, V, 1, 1, 1, 1, 0, 704, 100
27469, V, 1, 1, 1, 1, 0, 704, 99
27470, V, 1, 1, 1, 1, 0, 704, 99
27471, V, 1, 1, 1, 1, 0, 704, 100
27472, V, 1, 1, 1, 1, 0, 704, 99
27473, V, 1, 1, 1, 1, 0, 704, 100
27474, V, 1, 1, 1, 1, 0, 704, 99
27475, V, 1, 1, 1, 1, 0, 704, 99
27476, V, 1, 1, 1, 1, 0, 704, 100
27478, V, 1, 1, 1, 1, 0, 704, 99
27479, V, 1, 1, 1, 1, 0, 704, 99
27480, V, 1, 1, 1, 1, 0, 704, 99
27481, V, 1, 1, 1, 1, 0, 704, 99
27482, V, 1, 1, 1, 1, 0, 704, 100
27483, V, 1, 1, 1, 1, 0, 704, 100
27484, V, 1, 1, 1, 1, 0, 704, 100
27485, V, 1, 1, 1, 1, 0, 704, 99
27486, V, 1, 1, 1, 1, 0, 704, 99
27487, V, 1, 1, 1, 1, 0, 704, 99
27488, V, 1, 1, 1, 1, 0, 704, 100
27489, V, 1, 1, 1, 1, 0, 704, 100
27490, V, 1, 1, 1, 1, 0, 704, 99
27491, V, 1, 1, 1, 1, 0, 704, 100
27492, V, 1, 1, 1, 1, 0, 704, 99
27493, V, 1, 1, 1, 1, 0, 704, 99
27494, V, 1, 1, 1, 1, 0, 704, 100
27495, V, 1, 1, 1, 1, 0, 704, 99
27496, V, 1, 1, 1, 1, 0, 704, 100
27497, V, 1, 1, 1, 1, 0, 704, 99
27498, V, 1, 1, 1, 1, 0, 704, 100
27499, V, 1, 1, 1, 1, 0, 704, 100
27500, V, 1, 1, 1, 1, 0, 704, 100
27501, V, 1, 1, 1, 1, 0, 704, 100
27502, V, 1, 1, 1, 1, 0, 704, 100
27503, V, 1, 1, 1, 1, 0, 704, 100
27504, V, 1, 1, 1, 1, 0, 704, 100
27505, V, 1, 1, 1, 1, 0, 704, 99
27506, V, 1, 1, 1, 1, 0, 704, 100
27507, V, 1, 1, 1, 1, 0, 704, 100
27508, V, 1, 1, 1, 1, 0, 704, 100
27509, V, 1, 1, 1, 1, 0, 704, 100
27510, V, 1, 1, 1, 1, 0, 704, 100
27511, V, 1, 1, 1, 1, 0, 704, 100
27512, V, 1, 1, 1, 1, 0, 704, 100
27513, V, 1, 1, 1, 1, 0, 704, 100
27514, V, 1, 1, 1, 1, 0, 704, 100
27515, V, 1, 1, 1, 1, 0, 704, 100
27516, V, 1, 1, 1, 1, 0, 704, 100
27517, V, 1, 1, 1, 1, 0, 704, 100
27518, V, 1, 1, 1, 1, 0, 704, 100
27520, V, 1, 1, 1, 1, 0, 704, 100
27521, V, 1, 1, 1, 1, 0, 704, 100
27522, V, 1, 1, 1, 1, 0, 704, 100
27523, V, 1, 1, 1, 1, 0, 704, 100
27524, V, 1, 1, 1, 1, 0, 704, 100
27525, V, 1, 1, 1, 1, 0, 704, 100
27526, V, 1, 1, 1, 1, 0, 704, 100
27527, V, 1, 1, 1, 1, 0, 704, 100
27528, V, 1, 1, 1, 1, 0, 704, 100
27529, V, 1, 1, 1, 1, 0, 704, 100
27530, V, 1, 1, 1, 1, 0, 704, 100
27531, V, 1, 0, 0, 1, 0, 704, 100
27531, V, 1, 0, 0, 0, 0, 704, 100
27532, V, 1, 1, 0, 0, 0, 704, 100
27532, V, 1, 1, 0, 0, 0, 704, 100
27533, V, 1, 1, 1, 1, 0, 704, 100
27534, V, 1, 1, 1, 1, 0, 704, 100
27535, V, 1, 1, 1, 1, 0, 704, 99
27536, V, 1, 1, 1, 1, 0, 704, 99
27537, V, 1, 1, 1, 1, 0, 704, 99
27538, V, 1, 1, 1, 1, 0, 704, 99
27539, V, 1, 1, 1, 1, 0, 704, 99
27540, V, 1, 1, 1, 1, 0, 704, 99
27541, V, 1, 1, 1, 1, 0, 704, 99
27542, V, 1, 1, 1, 1, 0, 704, 99
27543, V, 1, 1, 1, 1, 0, 704, 99
27544, V, 1, 1, 1, 1, 0, 704, 99
27545, V, 1, 1, 1, 1, 0, 704, 99
27546, V, 1, 1, 1, 1, 0, 704, 99
27547, V, 1, 1, 1, 1, 0, 704, 99
27548, V, 1, 1, 1, 1, 0, 704, 99
27549, V, 1, 1, 1, 1, 0, 704, 99
27550, V, 1, 1, 1, 1, 0, 704, 99
27551, V, 1, 1, 1, 1, 0, 704, 99
27552, V, 1, 1, 1, 1, 0, 704, 99
27553, V, 1, 1, 1, 1, 0, 704, 99
27554, V, 1, 1, 1, 1, 0, 704, 99
27555, V, 1, 1, 1, 1, 0, 704, 99
27556, V, 1, 1, 1, 1, 0, 704, 99
27557, V, 1, 1, 1, 1, 0, 704, 99
27558, V, 1, 1, 1, 1, 0, 704, 99
27559, V, 1, 1, 1, 1, 0, 704, 99
27560, V, 1, 1, 1, 1, 0, 704, 99
27561, V, 1, 1, 1, 1, 0, 704, 99
27563, V, 1, 1, 1, 1, 0, 704, 99
27564, V, 1, 1, 1, 1, 0, 704, 99
27565, V, 1, 1, 1, 1, 0, 704, 99
27566, V, 1, 1, 1, 1, 0, 704, 99
27567, V, 1, 1, 1, 1, 0, 704, 99
27568, V, 1, 1, 1, 1, 0, 704, 99
27569, V, 1, 1, 1, 1, 0, 704, 99
27570, V, 1, 1, 1, 1, 0, 704, 99
27571, V, 1, 1, 1, 1, 0, 704, 99
27572, V, 1, 1, 1, 1, 0, 704, 99
27573, V, 1, 1, 1, 1, 0, 704, 99
27574, V, 1, 1, 1, 1, 0, 704, 99
27575, V, 1, 1, 1, 1, 0, 704, 99
27576, V, 1, 1, 1, 1, 0, 704, 99
27577, V, 1, 1, 1, 1, 0, 704, 99
27578, V, 1, 1, 1, 1, 0, 704, 99
27579, V, 1, 1, 1, 1, 0, 704, 99
27580, V, 1, 1, 1, 1, 0, 704, 99
27581, V, 1, 1, 1, 1, 0, 704, 99
27582, V, 1, 1, 1, 1, 0, 704, 99
27583, V, 1, 1, 1, 1, 0, 704, 99
27584, V, 1, 1, 1, 1, 0, 704, 99
27585, V, 1, 1, 1, 1, 0, 704, 99
27586, V, 1, 1, 1, 1, 0, 704, 99
27587, V, 1, 1, 1, 1, 0, 704, 99
27588, V, 1, 1, 1, 1, 0, 704, 99
27589, V, 1, 1, 1, 1, 0, 704, 99
27590, V, 1, 1, 1, 1, 0, 704, 99
27591, V, 1, 1, 1, 1, 0, 704, 99
27592, V, 1, 1, 1, 1, 0, 704, 99
27593, V, 1, 1, 1, 1, 0, 704, 100
27594, V, 1, 1, 1, 1, 0, 704, 99
27595, V, 1, 1, 1, 1, 0, 704, 99
27596, V, 1, 1, 1, 1, 0, 704, 99
27597, V, 1, 1, 1, 1, 0, 704, 99
27598, V, 1, 1, 1, 1, 0, 704, 100
27599, V, 1, 1, 1, 1, 0, 704, 100
27600, V, 1, 1, 1, 1, 0, 704, 100
27601, V, 1, 1, 1, 1, 0, 704, 100
27602, V, 1, 1, 1, 1, 0, 704, 100
27603, V, 1, 1, 1, 1, 0, 704, 100
27604, V, 1, 1, 1, 1, 0, 704, 99
27606, V, 1, 1, 1, 1, 0, 704, 100
27607, V, 1, 1, 1, 1, 0, 704, 100
27608, V, 1, 1, 1, 1, 0, 704, 100
27609, V, 1, 1, 1, 1, 0, 704, 100
27610, V, 1, 1, 1, 1, 0, 704, 100
27611, V, 1, 1, 1, 1, 0, 704, 100
27612, V, 1, 1, 1, 1, 0, 704, 100
27613, V, 1, 1, 1, 1, 0, 704, 100
27614, V, 1, 1, 1, 1, 0, 704, 100
27615, V, 1, 1, 1, 1, 0, 704, 100
27616, V, 1, 1, 1, 1, 0, 704, 100
27617, V, 1, 1, 1, 1, 0, 704, 100
27618, V, 1, 1, 1, 1, 0, 704, 100
27619, V, 1, 1, 1, 1, 0, 704, 100
27620, V, 1, 1, 1, 1, 0, 704, 100
27621, V, 1, 1, 1, 1, 0, 704, 100
27622, V, 1, 1, 1, 1, 0, 704, 100
27623, V, 1, 1, 1, 1, 0, 704, 100
27624, V, 1, 1, 1, 1, 0, 704, 100
27625, V, 1, 1, 1, 1, 0, 704, 100
27626, V, 1, 1, 1, 1, 0, 704, 100
27627, V, 1, 1, 1, 1, 0, 704, 100
27628, V, 1, 1, 1, 1, 0, 704, 100
27629, V, 1, 1, 1, 1, 0, 704, 100
27630, V, 1, 1, 1, 1, 0, 704, 99
27631, V, 1, 1, 1, 1, 0, 704, 100
27632, V, 1, 1, 1, 1, 0, 704, 100
27633, V, 1, 1, 1, 1, 0, 704, 100
27634, V, 1, 1, 1, 1, 0, 704, 100
27635, V, 1, 1, 1, 1, 0, 704, 100
27636, V, 1, 1, 1, 1, 0, 704, 100
27637, V, 1, 1, 1, 1, 0, 704, 100
27638, V, 1, 1, 1, 1, 0, 704, 100
27639, V, 1, 1, 1, 1, 0, 704, 100
27640, V, 1, 1, 1, 1, 0, 704, 100
27641, V, 1, 1, 1, 1, 0, 704, 100
27642, V, 1, 1, 1, 1, 0, 704, 100
27643, V, 1, 1, 1, 1, 0, 704, 100
27644, V, 1, 1, 1, 1, 0, 704, 100
27645, V, 1, 1, 1, 1, 0, 704, 100
27646, V, 1, 1, 1, 1, 0, 704, 100
27648, V, 1, 1, 1, 1, 0, 704, 100
27649, V, 1, 1, 1, 1, 0, 704, 100
27650, V, 1, 1, 1, 1, 0, 704, 100
27651, V, 1, 0, 0, 1, 0, 704, 100
27651, V, 1, 0, 0, 0, 0, 704, 100
27652, V, 1, 1, 0, 0, 0, 704, 100
27652, V, 1, 1, 0, 0, 0, 704, 100
27653, V, 1, 1, 1, 1, 0, 704, 100
27654, V, 1, 1, 1, 1, 0, 704, 100
27655, V, 1, 1, 1, 1, 0, 704, 99
27656, V, 1, 1, 1, 1, 0, 704, 99
27657, V, 1, 1, 1, 1, 0, 704, 99
27658, V, 1, 1, 1, 1, 0, 704, 99
27659, V, 1, 1, 1, 1, 0, 704, 99
27660, V, 1, 1, 1, 1, 0, 704, 99
27661, V, 1, 1, 1, 1, 0, 704, 99
27662, V, 1, 1, 1, 1, 0, 704, 99
27663, V, 1, 1, 1, 1, 0, 704, 99
27664, V, 1, 1, 1, 1, 0, 704, 99
27665, V, 1, 1, 1, 1, 0, 704, 99
27666, V, 1, 1, 1, 1, 0, 704, 99
27667, V, 1, 1, 1, 1, 0, 704, 99
27668, V, 1, 1, 1, 1, 0, 704, 99
27669, V, 1, 1, 1, 1, 0, 704, 99
27670, V, 1, 1, 1, 1, 0, 704, 99
27671, V, 1, 1, 1, 1, 0, 704, 99
27672, V, 1, 1, 1, 1, 0, 704, 99
27673, V, 1, 1, 1, 1, 0, 704, 99
27674, V, 1, 1, 1, 1, 0, 704, 100
27675, V, 1, 1, 1, 1, 0, 704, 100
27676, V, 1, 1, 1, 1, 0, 704, 100
27677, V, 1, 1, 1, 1, 0, 704, 100
27678, V, 1, 1, 1, 1, 0, 704, 100
27679, V, 1, 1, 1, 1, 0, 704, 100
27680, V, 1, 1, 1, 1, 0, 704, 100
27681, V, 1, 1, 1, 1, 0, 704, 100
27682, V, 1, 1, 1, 1, 0, 704, 100
27683, V, 1, 1, 1, 1, 0, 704, 100
27684, V, 1, 1, 1, 1, 0, 704, 100
27685, V, 1, 1, 1, 1, 0, 704, 100
27686, V, 1, 1, 1, 1, 0, 704, 100
27687, V, 1, 1, 1, 1, 0, 704, 100
27688, V, 1, 1, 1, 1, 0, 704, 100
27689, V, 1, 1, 1, 1, 0, 704, 100
27691, V, 1, 1, 1, 1, 0, 704, 100
27692, V, 1, 1, 1, 1, 0, 704, 100
27693, V, 1, 1, 1, 1, 0, 704, 100
27694, V, 1, 1, 1, 1, 0, 704, 100
27695, V, 1, 1, 1, 1, 0, 704, 100
27696, V, 1, 1, 1, 1, 0, 704, 100
27697, V, 1, 1, 1, 1, 0, 704, 100
27698, V, 1, 1, 1, 1, 0, 704, 100
27699, V, 1, 1, 1, 1, 0, 704, 100
27700, V, 1, 1, 1, 1, 0, 704, 100
27701, V, 1, 1, 1, 1, 0, 704, 100
27702, V, 1, 1, 1, 1, 0, 704, 100
27703, V, 1, 1, 1, 1, 0, 704, 100
27704, V, 1, 1, 1, 1, 0, 704, 100
27705, V, 1, 1, 1, 1, 0, 704, 100
27706, V, 1, 1, 1, 1, 0, 704, 100
27707, V, 1, 1, 1, 1, 0, 704, 100
27708, V, 1, 1, 1, 1, 0, 704, 100
27709, V, 1, 1, 1, 1, 0, 704, 100
27710, V, 1, 1, 1, 1, 0, 704, 100
27711, V, 1, 1, 1, 1, 0, 704, 100
27712, V, 1, 1, 1, 1, 0, 704, 100
27713, V, 1, 1, 1, 1, 0, 704, 100
27714, V, 1, 1, 1, 1, 0, 704, 100
27715, V, 1, 1, 1, 1, 0, 704, 100
27716, V, 1, 1, 1, 1, 0, 704, 100
27717, V, 1, 1, 1, 1, 0, 704, 100
27718, V, 1, 1, 1, 1, 0, 704, 100
27719, V, 1, 1, 1, 1, 0, 704, 100
27720, V, 1, 1, 1, 1, 0, 704, 100
27721, V, 1, 1, 1, 1, 0, 704, 100
27722, V, 1, 1, 1, 1, 0, 704, 100
27723, V, 1, 1, 1, 1, 0, 704, 100
27724, V, 1, 1, 1, 1, 0, 704, 100
27725, V, 1, 1, 1, 1, 0, 704, 100
27726, V, 1, 1, 1, 1, 0, 704, 100
27727, V, 1, 1, 1, 1, 0, 704, 100
27728, V, 1, 1, 1, 1, 0, 704, 100
27729, V, 1, 1, 1, 1, 0, 704, 100
27730, V, 1, 1, 1, 1, 0, 704, 100
27731, V, 1, 1, 1, 1, 0, 704, 100
27732, V, 1, 1, 1, 1, 0, 704, 100
27734, V, 1, 1, 1, 1, 0, 704, 100
27735, V, 1, 1, 1, 1, 0, 704, 100
27736, V, 1, 1, 1, 1, 0, 704, 100
27737, V, 1, 1, 1, 1, 0, 704, 100
27738, V, 1, 1, 1, 1, 0, 704, 100
27739, V, 1, 1, 1, 1, 0, 704, 100
27740, V, 1, 1, 1, 1, 0, 704, 100
27741, V, 1, 1, 1, 1, 0, 704, 100
27742, V, 1, 1, 1, 1, 0, 704, 100
27743, V, 1, 1, 1, 1, 0, 704, 100
27744, V, 1, 1, 1, 1, 0, 704, 100
27745, V, 1, 1, 1, 1, 0, 704, 100
27746, V, 1, 1, 1, 1, 0, 704, 100
27747, V, 1, 1, 1, 1, 0, 704, 100
27748, V, 1, 1, 1, 1, 0, 704, 100
27749, V, 1, 1, 1, 1, 0, 704, 100
27750, V, 1, 1, 1, 1, 0, 704, 100
27751, V, 1, 1, 1, 1, 0, 704, 100
27752, V, 1, 1, 1, 1, 0, 704, 100
27753, V, 1, 1, 1, 1, 0, 704, 100
27754, V, 1, 1, 1, 1, 0, 704, 100
27755, V, 1, 1, 1, 1, 0, 704, 100
27756, V, 1, 1, 1, 1, 0, 704, 100
27757, V, 1, 1, 1, 1, 0, 704, 100
27758, V, 1, 1, 1, 1, 0, 704, 100
27759, V, 1, 1, 1, 1, 0, 704, 100
27760, V, 1, 1, 1, 1, 0, 704, 100
27761, V, 1, 1, 1, 1, 0, 704, 100
27762, V, 1, 1, 1, 1, 0, 704, 100
27763, V, 1, 1, 1, 1, 0, 704, 100
27764, V, 1, 1, 1, 1, 0, 704, 100
27765, V, 1, 1, 1, 1, 0, 704, 100
27766, V, 1, 1, 1, 1, 0, 704, 100
27767, V, 1, 1, 1, 1, 0, 704, 100
27768, V, 1, 1, 1, 1, 0, 704, 100
27769, V, 1, 1, 1, 1, 0, 704, 100
27770, V, 1, 1, 1, 1, 0, 704, 100
27771, V, 1, 1, 1, 1, 0, 704, 100
27772, V, 1, 1, 1, 1, 0, 704, 100
27773, V, 1, 1, 1, 1, 0, 704, 100
27774, V, 1, 1, 1, 1, 0, 704, 100
27776, V, 1, 1, 1, 1, 0, 704, 100
27777, V, 1, 1, 1, 1, 0, 704, 100
27778, V, 1, 1, 1, 1, 0, 704, 100
27779, V, 1, 1, 1, 1, 0, 704, 100
27780, V, 1, 1, 1, 1, 0, 704, 100
27781, V, 1, 1, 1, 1, 0, 704, 100
27782, V, 1, 1, 1, 1, 0, 704, 100
27783, V, 1, 1, 1, 1, 0, 704, 100
27784, V, 1, 1, 1, 1, 0, 704, 100
27785, V, 1, 1, 1, 1, 0, 704, 100
27786, V, 1, 1, 1, 1, 0, 704, 100
27787, V, 1, 1, 1, 1, 0, 704, 100
27788, V, 1, 1, 1, 1, 0, 704, 100
27789, V, 1, 1, 1, 1, 0, 704, 100
27790, V, 1, 1, 1, 1, 0, 704, 100
27791, V, 1, 1, 1, 1, 0, 704, 100
27792, V, 1, 1, 1, 1, 0, 704, 100
27793, V, 1, 1, 1, 1, 0, 704, 100
27794, V, 1, 1, 1, 1, 0, 704, 100
27795, V, 1, 1, 1, 1, 0, 704, 100
27796, V, 1, 1, 1, 1, 0, 704, 100
27797, V, 1, 1, 1, 1, 0, 704, 100
27798, V, 1, 1, 1, 1, 0, 704, 100
27799, V, 1, 1, 1, 1, 0, 704, 100
27800, V, 1, 1, 1, 1, 0, 704, 100
27801, V, 1, 1, 1, 1, 0, 704, 100
27802, V, 1, 1, 1, 1, 0, 704, 100
27803, V, 1, 1, 1, 1, 0, 704, 100
27804, V, 1, 1, 1, 1, 0, 704, 100
27805, V, 1, 1, 1, 1, 0, 704, 100
27806, V, 1, 1, 1, 1, 0, 704, 100
27807, V, 1, 1, 1, 1, 0, 704, 100
27808, V, 1, 1, 1, 1, 0, 704, 100
27809, V, 1, 1, 1, 1, 0, 704, 100
27810, V, 1, 1, 1, 1, 0, 704, 100
27811, V, 1, 1, 1, 1, 0, 704, 100
27812, V, 1, 1, 1, 1, 0, 704, 100
27813, V, 1, 1, 1, 1, 0, 704, 100
27814, V, 1, 1, 1, 1, 0, 704, 100
27815, V, 1, 1, 1, 1, 0, 704, 100
27816, V, 1, 1, 1, 1, 0, 704, 100
27817, V, 1, 1, 1, 1, 0, 704, 100
27819, V, 1, 1, 1, 1, 0, 704, 100
27820, V, 1, 1, 1, 1, 0, 704, 100
27821, V, 1, 1, 1, 1, 0, 704, 100
27822, V, 1, 1, 1, 1, 0, 704, 100
27823, V, 1, 1, 1, 1, 0, 704, 100
27824, V, 1, 1, 1, 1, 0, 704, 101
27825, V, 1, 1, 1, 1, 0, 704, 101
27826, V, 1, 1, 1, 1, 0, 704, 101
27827, V, 1, 1, 1, 1, 0, 704, 101
27828, V, 1, 1, 1, 1, 0, 704, 100
27829, V, 1, 1, 1, 1, 0, 704, 101
27830, V, 1, 1, 1, 1, 0, 704, 101
27831, V, 1, 1, 1, 1, 0, 704, 101
27832, V, 1, 1, 1, 1, 0, 704, 100
27833, V, 1, 1, 1, 1, 0, 704, 100
27834, V, 1, 1, 1, 1, 0, 704, 100
27835, V, 1, 1, 1, 1, 0, 704, 101
27836, V, 1, 1, 1, 1, 0, 704, 101
27837, V, 1, 1, 1, 1, 0, 704, 101
27838, V, 1, 1, 1, 1, 0, 704, 101
27839, V, 1, 1, 1, 1, 0, 704, 100
27840, V, 1, 1, 1, 1, 0, 704, 100
27841, V, 1, 1, 1, 1, 0, 704, 101
27842, V, 1, 1, 1, 1, 0, 704, 101
27843, V, 1, 1, 1, 1, 0, 704, 100
27844, V, 1, 1, 1, 1, 0, 704, 100
27845, V, 1, 1, 1, 1, 0, 704, 100
27846, V, 1, 1, 1, 1, 0, 704, 100
27847, V, 1, 1, 1, 1, 0, 704, 100
27848, V, 1, 1, 1, 1, 0, 704, 100
27849, V, 1, 1, 1, 1, 0, 704, 100
27850, V, 1, 1, 1, 1, 0, 704, 100
27851, V, 1, 1, 1, 1, 0, 704, 100
27852, V, 1, 1, 1, 1, 0, 704, 100
27853, V, 1, 1, 1, 1, 0, 704, 100
27854, V, 1, 1, 1, 1, 0, 704, 100
27855, V, 1, 1, 1, 1, 0, 704, 100
27856, V, 1, 1, 1, 1, 0, 704, 100
27857, V, 1, 1, 1, 1, 0, 704, 100
27858, V, 1, 1, 1, 1, 0, 704, 100
27859, V, 1, 1, 1, 1, 0, 704, 100
27860, V, 1, 1, 1, 1, 0, 704, 100
27862, V, 1, 1, 1, 1, 0, 704, 100
27863, V, 1, 1, 1, 1, 0, 704, 100
27864, V, 1, 1, 1, 1, 0, 704, 100
27865, V, 1, 1, 1, 1, 0, 704, 100
27866, V, 1, 1, 1, 1, 0, 704, 100
27867, V, 1, 1, 1, 1, 0, 704, 100
27868, V, 1, 1, 1, 1, 0, 704, 100
27869, V, 1, 1, 1, 1, 0, 704, 100
27870, V, 1, 1, 1, 1, 0, 704, 100
27871, V, 1, 1, 1, 1, 0, 704, 100
27872, V, 1, 1, 1, 1, 0, 704, 100
27873, V, 1, 1, 1, 1, 0, 704, 100
27874, V, 1, 1, 1, 1, 0, 704, 100
27875, V, 1, 1, 1, 1, 0, 704, 100
27876, V, 1, 1, 1, 1, 0, 704, 100
27877, V, 1, 1, 1, 1, 0, 704, 100
27878, V, 1, 1, 1, 1, 0, 704, 100
27879, V, 1, 1, 1, 1, 0, 704, 100
27880, V, 1, 1, 1, 1, 0, 704, 100
27881, V, 1, 1, 1, 1, 0, 704, 100
27882, V, 1, 1, 1, 1, 0, 704, 100
27883, V, 1, 1, 1, 1, 0, 704, 100
27884, V, 1, 1, 1, 1, 0, 704, 100
27885, V, 1, 1, 1, 1, 0, 704, 100
27886, V, 1, 1, 1, 1, 0, 704, 100
27887, V, 1, 1, 1, 1, 0, 704, 100
27888, V, 1, 1, 1, 1, 0, 704, 100
27889, V, 1, 1, 1, 1, 0, 704, 100
27890, V, 1, 1, 1, 1, 0, 704, 100
27891, V, 1, 1, 1, 1, 0, 704, 100
27892, V, 1, 1, 1, 1, 0, 704, 100
27893, V, 1, 1, 1, 1, 0, 704, 100
27894, V, 1, 1, 1, 1, 0, 704, 100
27895, V, 1, 1, 1, 1, 0, 704, 100
27896, V, 1, 1, 1, 1, 0, 704, 100
27897, V, 1, 1, 1, 1, 0, 704, 100
27898, V, 1, 1, 1, 1, 0, 704, 100
27899, V, 1, 1, 1, 1, 0, 704, 100
27900, V, 1, 1, 1, 1, 0, 704, 100
27901, V, 1, 1, 1, 1, 0, 704, 100
27902, V, 1, 1, 1, 1, 0, 704, 100
27904, V, 1, 1, 1, 1, 0, 704, 100
27905, V, 1, 1, 1, 1, 0, 704, 100
27906, V, 1, 1, 1, 1, 0, 704, 100
27907, V, 1, 1, 1, 1, 0, 704, 100
27908, V, 1, 1, 1, 1, 0, 704, 100
27909, V, 1, 1, 1, 1, 0, 704, 100
27910, V, 1, 1, 1, 1, 0, 704, 100
27911, V, 1, 1, 1, 1, 0, 704, 100
27912, V, 1, 1, 1, 1, 0, 704, 100
27913, V, 1, 1, 1, 1, 0, 704, 100
27914, V, 1, 1, 1, 1, 0, 704, 100
27915, V, 1, 1, 1, 1, 0, 704, 100
27916, V, 1, 1, 1, 1, 0, 704, 100
27917, V, 1, 1, 1, 1, 0, 704, 100
27918, V, 1, 1, 1, 1, 0, 704, 100
27919, V, 1, 1, 1, 1, 0, 704, 100
27920, V, 1, 1, 1, 1, 0, 704, 100
27921, V, 1, 1, 1, 1, 0, 704, 100
27922, V, 1, 1, 1, 1, 0, 704, 100
27923, V, 1, 1, 1, 1, 0, 704, 100
27924, V, 1, 1, 1, 1, 0, 704, 100
27925, V, 1, 1, 1, 1, 0, 704, 100
27926, V, 1, 1, 1, 1, 0, 704, 100
27927, V, 1, 1, 1, 1, 0, 704, 100
27928, V, 1, 1, 1, 1, 0, 704, 100
27929, V, 1, 1, 1, 1, 0, 704, 100
27930, V, 1, 1, 1, 1, 0, 704, 100
27931, V, 1, 1, 1, 1, 0, 704, 100
27932, V, 1, 1, 1, 1, 0, 704, 100
27933, V, 1, 1, 1, 1, 0, 704, 100
27934, V, 1, 1, 1, 1, 0, 704, 100
27935, V, 1, 1, 1, 1, 0, 704, 100
27936, V, 1, 1, 1, 1, 0, 704, 100
27937, V, 1, 1, 1, 1, 0, 704, 100
27938, V, 1, 1, 1, 1, 0, 704, 100
27939, V, 1, 1, 1, 1, 0, 704, 100
27940, V, 1, 1, 1, 1, 0, 704, 100
27941, V, 1, 1, 1, 1, 0, 704, 100
27942, V, 1, 1, 1, 1, 0, 704, 100
27943, V, 1, 1, 1, 1, 0, 704, 100
27944, V, 1, 1, 1, 1, 0, 704, 100
27945, V, 1, 1, 1, 1, 0, 704, 100
27947, V, 1, 1, 1, 1, 0, 704, 100
27948, V, 1, 1, 1, 1, 0, 704, 100
27949, V, 1, 1, 1, 1, 0, 704, 100
27950, V, 1, 1, 1, 1, 0, 704, 100
27951, V, 1, 1, 1, 1, 0, 704, 100
27952, V, 1, 1, 1, 1, 0, 704, 100
27953, V, 1, 1, 1, 1, 0, 704, 100
27954, V, 1, 1, 1, 1, 0, 704, 100
27955, V, 1, 1, 1, 1, 0, 704, 100
27956, V, 1, 1, 1, 1, 0, 704, 100
27957, V, 1, 1, 1, 1, 0, 704, 100
27958, V, 1, 1, 1, 1, 0, 704, 100
27959, V, 1, 1, 1, 1, 0, 704, 100
27960, V, 1, 1, 1, 1, 0, 704, 100
27961, V, 1, 1, 1, 1, 0, 704, 100
27962, V, 1, 1, 1, 1, 0, 704, 100
27963, V, 1, 1, 1, 1, 0, 704, 100
27964, V, 1, 1, 1, 1, 0, 704, 100
27965, V, 1, 1, 1, 1, 0, 704, 100
27966, V, 1, 1, 1, 1, 0, 704, 100
27967, V, 1, 1, 1, 1, 0, 704, 100
27968, V, 1, 1, 1, 1, 0, 704, 100
27969, V, 1, 1, 1, 1, 0, 704, 100
27970, V, 1, 1, 1, 1, 0, 704, 100
27971, V, 1, 1, 1, 1, 0, 704, 100
27972, V, 1, 1, 1, 1, 0, 704, 100
27973, V, 1, 1, 1, 1, 0, 704, 100
27974, V, 1, 1, 1, 1, 0, 704, 100
27975, V, 1, 1, 1, 1, 0, 704, 100
27976, V, 1, 1, 1, 1, 0, 704, 100
27977, V, 1, 1, 1, 1, 0, 704, 100
27978, V, 1, 1, 1, 1, 0, 704, 100
27979, V, 1, 1, 1, 1, 0, 704, 100
27980, V, 1, 1, 1, 1, 0, 704, 100
27981, V, 1, 1, 1, 1, 0, 704, 100
27982, V, 1, 1, 1, 1, 0, 704, 100
27983, V, 1, 1, 1, 1, 0, 704, 100
27984, V, 1, 1, 1, 1, 0, 704, 100
27985, V, 1, 1, 1, 1, 0, 704, 100
27986, V, 1, 1, 1, 1, 0, 704, 100
27987, V, 1, 1, 1, 1, 0, 704, 100
27988, V, 1, 1, 1, 1, 0, 704, 100
27990, V, 1, 1, 1, 1, 0, 704, 100
27991, V, 1, 1, 1, 1, 0, 704, 100
27992, V, 1, 1, 1, 1, 0, 704, 100
27993, V, 1, 1, 1, 1, 0, 704, 100
27994, V, 1, 1, 1, 1, 0, 704, 100
27995, V, 1, 1, 1, 1, 0, 704, 100
27996, V, 1, 1, 1, 1, 0, 704, 100
27997, V, 1, 1, 1, 1, 0, 704, 100
27998, V, 1, 1, 1, 1, 0, 704, 100
27999, V, 1, 1, 1, 1, 0, 704, 100
28000, V, 1, 1, 1, 1, 0, 704, 100
28001, V, 1, 1, 1, 1, 0, 704, 100
28002, V, 1, 1, 1, 1, 0, 704, 100
28003, V, 1, 1, 1, 1, 0, 704, 100
28004, V, 1, 1, 1, 1, 0, 704, 100
28005, V, 1, 1, 1, 1, 0, 704, 100
28006, V, 1, 1, 1, 1, 0, 704, 100
28007, V, 1, 1, 1, 1, 0, 704, 100
28008, V, 1, 1, 1, 1, 0, 704, 100
28009, V, 1, 1, 1, 1, 0, 704, 100
28010, V, 1, 1, 1, 1, 0, 704, 100
28011, V, 1, 1, 1, 1, 0, 704, 100
28012, V, 1, 1, 1, 1, 0, 704, 100
28013, V, 1, 1, 1, 1, 0, 704, 100
28014, V, 1, 1, 1, 1, 0, 704, 100
28015, V, 1, 1, 1, 1, 0, 704, 100
28016, V, 1, 1, 1, 1, 0, 704, 100
28017, V, 1, 1, 1, 1, 0, 704, 100
28018, V, 1, 1, 1, 1, 0, 704, 100
28019, V, 1, 1, 1, 1, 0, 704, 100
28020, V, 1, 1, 1, 1, 0, 704, 100
28021, V, 1, 1, 1, 1, 0, 704, 100
28022, V, 1, 1, 1, 1, 0, 704, 100
28023, V, 1, 1, 1, 1, 0, 704, 100
28024, V, 1, 1, 1, 1, 0, 704, 100
28025, V, 1, 1, 1, 1, 0, 704, 100
28026, V, 1, 1, 1, 1, 0, 704, 100
28027, V, 1, 1, 1, 1, 0, 704, 100
28028, V, 1, 1, 1, 1, 0, 704, 100
28029, V, 1, 1, 1, 1, 0, 704, 100
28030, V, 1, 1, 1, 1, 0, 704, 100
28032, V, 1, 1, 1, 1, 0, 704, 100
28033, V, 1, 1, 1, 1, 0, 704, 100
28034, V, 1, 1, 1, 1, 0, 704, 100
28035, V, 1, 1, 1, 1, 0, 704, 100
28036, V, 1, 1, 1, 1, 0, 704, 100
28037, V, 1, 1, 1, 1, 0, 704, 100
28038, V, 1, 1, 1, 1, 0, 704, 100
28039, V, 1, 1, 1, 1, 0, 704, 100
28040, V, 1, 1, 1, 1, 0, 704, 100
28041, V, 1, 1, 1, 1, 0, 704, 100
28042, V, 1, 1, 1, 1, 0, 704, 100
28043, V, 1, 1, 1, 1, 0, 704, 100
28044, V, 1, 1, 1, 1, 0, 704, 100
28045, V, 1, 1, 1, 1, 0, 704, 100
28046, V, 1, 1, 1, 1, 0, 704, 100
28047, V, 1, 1, 1, 1, 0, 704, 100
28048, V, 1, 1, 1, 1, 0, 704, 100
28049, V, 1, 1, 1, 1, 0, 704, 100
28050, V, 1, 1, 1, 1, 0, 704, 100
28051, V, 1, 1, 1, 1, 0, 704, 100
28052, V, 1, 1, 1, 1, 0, 704, 100
28053, V, 1, 1, 1, 1, 0, 704, 100
28054, V, 1, 1, 1, 1, 0, 704, 100
28055, V, 1, 1, 1, 1, 0, 704, 100
28056, V, 1, 1, 1, 1, 0, 704, 100
28057, V, 1, 1, 1, 1, 0, 704, 100
28058, V, 1, 1, 1, 1, 0, 704, 100
28059, V, 1, 1, 1, 1, 0, 704, 100
28060, V, 1, 1, 1, 1, 0, 704, 100
28061, V, 1, 1, 1, 1, 0, 704, 100
28062, V, 1, 1, 1, 1, 0, 704, 100
28063, V, 1, 1, 1, 1, 0, 704, 100
28064, V, 1, 1, 1, 1, 0, 704, 100
28065, V, 1, 1, 1, 1, 0, 704, 100
28066, V, 1, 1, 1, 1, 0, 704, 100
28067, V, 1, 1, 1, 1, 0, 704, 100
28068, V, 1, 1, 1, 1, 0, 704, 100
28069, V, 1, 1, 1, 1, 0, 704, 100
28070, V, 1, 1, 1, 1, 0, 704, 100
28071, V, 1, 1, 1, 1, 0, 704, 100
28072, V, 1, 1, 1, 1, 0, 704, 100
28073, V, 1, 1, 1, 1, 0, 704, 100
28075, V, 1, 1, 1, 1, 0, 704, 100
28076, V, 1, 1, 1, 1, 0, 704, 100
28077, V, 1, 1, 1, 1, 0, 704, 100
28078, V, 1, 1, 1, 1, 0, 704, 100
28079, V, 1, 1, 1, 1, 0, 704, 100
28080, V, 1, 1, 1, 1, 0, 704, 100
28081, V, 1, 1, 1, 1, 0, 704, 100
28082, V, 1, 1, 1, 1, 0, 704, 100
28083, V, 1, 1, 1, 1, 0, 704, 100
28084, V, 1, 1, 1, 1, 0, 704, 100
28085, V, 1, 1, 1, 1, 0, 704, 100
28086, V, 1, 1, 1, 1, 0, 704, 100
28087, V, 1, 1, 1, 1, 0, 704, 100
28088, V, 1, 1, 1, 1, 0, 704, 100
28089, V, 1, 1, 1, 1, 0, 704, 100
28090, V, 1, 1, 1, 1, 0, 704, 100
28091, V, 1, 1, 1, 1, 0, 704, 100
28092, V, 1, 1, 1, 1, 0, 704, 100
28093, V, 1, 1, 1, 1, 0, 704, 100
28094, V, 1, 1, 1, 1, 0, 704, 100
28095, V, 1, 1, 1, 1, 0, 704, 100
28096, V, 1, 1, 1, 1, 0, 704, 100
28097, V, 1, 1, 1, 1, 0, 704, 100
28098, V, 1, 1, 1, 1, 0, 704, 100
28099, V, 1, 1, 1, 1, 0, 704, 100
28100, V, 1, 1, 1, 1, 0, 704, 100
28101, V, 1, 1, 1, 1, 0, 704, 100
28102, V, 1, 1, 1, 1, 0, 704, 100
28103, V, 1, 1, 1, 1, 0, 704, 100
28104, V, 1, 1, 1, 1, 0, 704, 100
28105, V, 1, 1, 1, 1, 0, 704, 100
28106, V, 1, 1, 1, 1, 0, 704, 100
28107, V, 1, 1, 1, 1, 0, 704, 100
28108, V, 1, 1, 1, 1, 0, 704, 100
28109, V, 1, 1, 1, 1, 0, 704, 100
28110, V, 1, 1, 1, 1, 0, 704, 100
28111, V, 1, 1, 1, 1, 0, 704, 100
28112, V, 1, 1, 1, 1, 0, 704, 100
28113, V, 1, 1, 1, 1, 0, 704, 100
28114, V, 1, 1, 1, 1, 0, 704, 100
28115, V, 1, 1, 1, 1, 0, 704, 100
28116, V, 1, 1, 1, 1, 0, 704, 100
28118, V, 1, 1, 1, 1, 0, 704, 100
28119, V, 1, 1, 1, 1, 0, 704, 100
28120, V, 1, 1, 1, 1, 0, 704, 100
28121, V, 1, 1, 1, 1, 0, 704, 100
28122, V, 1, 1, 1, 1, 0, 704, 100
28123, V, 1, 1, 1, 1, 0, 704, 100
28124, V, 1, 1, 1, 1, 0, 704, 100
28125, V, 1, 1, 1, 1, 0, 704, 100
28126, V, 1, 1, 1, 1, 0, 704, 100
28127, V, 1, 1, 1, 1, 0, 704, 100
28128, V, 1, 1, 1, 1, 0, 704, 100
28129, V, 1, 1, 1, 1, 0, 704, 100
28130, V, 1, 1, 1, 1, 0, 704, 100
28131, V, 1, 1, 1, 1, 0, 704, 100
28132, V, 1, 1, 1, 1, 0, 704, 100
28133, V, 1, 1, 1, 1, 0, 704, 100
28134, V, 1, 1, 1, 1, 0, 704, 100
28135, V, 1, 1, 1, 1, 0, 704, 100
28136, V, 1, 1, 1, 1, 0, 704, 100
28137, V, 1, 1, 1, 1, 0, 704, 100
28138, V, 1, 1, 1, 1, 0, 704, 100
28139, V, 1, 1, 1, 1, 0, 704, 100
28140, V, 1, 1, 1, 1, 0, 704, 100
28141, V, 1, 1, 1, 1, 0, 704, 100
28142, V, 1, 1, 1, 1, 0, 704, 100
28143, V, 1, 1, 1, 1, 0, 704, 100
28144, V, 1, 1, 1, 1, 0, 704, 100
28145, V, 1, 1, 1, 1, 0, 704, 100
28146, V, 1, 1, 1, 1, 0, 704, 100
28147, V, 1, 1, 1, 1, 0, 704, 100
28148, V, 1, 1, 1, 1, 0, 704, 100
28149, V, 1, 1, 1, 1, 0, 704, 100
28150, V, 1, 1, 1, 1, 0, 704, 100
28151, V, 1, 1, 1, 1, 0, 704, 100
28152, V, 1, 1, 1, 1, 0, 704, 100
28153, V, 1, 0, 0, 1, 0, 704, 100
28153, V, 1, 0, 0, 0, 0, 704, 100
28154, V, 1, 1, 0, 0, 0, 704, 100
28154, V, 1, 1, 0, 0, 0, 704, 100
28155, V, 1, 1, 1, 1, 0, 704, 100
28156, V, 1, 1, 1, 1, 0, 704, 100
28157, V, 1, 1, 1, 1, 0, 704, 100
28158, V, 1, 1, 1, 1, 0, 704, 100
28160, V, 1, 1, 1, 1, 0, 704, 100
28161, V, 1, 1, 1, 1, 0, 704, 100
28162, V, 1, 1, 1, 1, 0, 704, 100
28163, V, 1, 1, 1, 1, 0, 704, 100
28164, V, 1, 1, 1, 1, 0, 704, 100
28165, V, 1, 1, 1, 1, 0, 704, 100
28166, V, 1, 1, 1, 1, 0, 704, 100
28167, V, 1, 1, 1, 1, 0, 704, 100
28168, V, 1, 1, 1, 1, 0, 704, 100
28169, V, 1, 1, 1, 1, 0, 704, 100
28170, V, 1, 1, 1, 1, 0, 704, 100
28171, V, 1, 1, 1, 1, 0, 704, 100
28172, V, 1, 1, 1, 1, 0, 704, 100
28173, V, 1, 1, 1, 1, 0, 704, 100
28174, V, 1, 1, 1, 1, 0, 704, 100
28175, V, 1, 1, 1, 1, 0, 704, 100
28176, V, 1, 1, 1, 1, 0, 704, 100
28177, V, 1, 1, 1, 1, 0, 704, 100
28178, V, 1, 1, 1, 1, 0, 704, 100
28179, V, 1, 1, 1, 1, 0, 704, 100
28180, V, 1, 1, 1, 1, 0, 704, 100
28181, V, 1, 1, 1, 1, 0, 704, 100
28182, V, 1, 1, 1, 1, 0, 704, 100
28183, V, 1, 1, 1, 1, 0, 704, 100
28184, V, 1, 1, 1, 1, 0, 704, 100
28185, V, 1, 1, 1, 1, 0, 704, 100
28186, V, 1, 1, 1, 1, 0, 704, 100
28187, V, 1, 1, 1, 1, 0, 704, 100
28188, V, 1, 1, 1, 1, 0, 704, 100
28189, V, 1, 1, 1, 1, 0, 704, 100
28190, V, 1, 1, 1, 1, 0, 704, 100
28191, V, 1, 1, 1, 1, 0, 704, 100
28192, V, 1, 1, 1, 1, 0, 704, 100
28193, V, 1, 1, 1, 1, 0, 704, 100
28194, V, 1, 1, 1, 1, 0, 704, 100
28195, V, 1, 1, 1, 1, 0, 704, 100
28196, V, 1, 1, 1, 1, 0, 704, 100
28197, V, 1, 1, 1, 1, 0, 704, 100
28198, V, 1, 1, 1, 1, 0, 704, 100
28199, V, 1, 1, 1, 1, 0, 704, 100
28200, V, 1, 1, 1, 1, 0, 704, 100
28201, V, 1, 1, 1, 1, 0, 704, 100
28203, V, 1, 1, 1, 1, 0, 704, 100
28204, V, 1, 1, 1, 1, 0, 704, 100
28205, V, 1, 1, 1, 1, 0, 704, 100
28206, V, 1, 1, 1, 1, 0, 704, 100
28207, V, 1, 1, 1, 1, 0, 704, 100
28208, V, 1, 1, 1, 1, 0, 704, 100
28209, V, 1, 1, 1, 1, 0, 704, 100
28210, V, 1, 1, 1, 1, 0, 704, 100
28211, V, 1, 1, 1, 1, 0, 704, 100
28212, V, 1, 1, 1, 1, 0, 704, 100
28213, V, 1, 1, 1, 1, 0, 704, 100
28214, V, 1, 1, 1, 1, 0, 704, 100
28215, V, 1, 1, 1, 1, 0, 704, 100
28216, V, 1, 1, 1, 1, 0, 704, 100
28217, V, 1, 1, 1, 1, 0, 704, 100
28218, V, 1, 1, 1, 1, 0, 704, 100
28219, V, 1, 1, 1, 1, 0, 704, 100
28220, V, 1, 1, 1, 1, 0, 704, 100
28221, V, 1, 1, 1, 1, 0, 704, 100
28222, V, 1, 1, 1, 1, 0, 704, 100
28223, V, 1, 1, 1, 1, 0, 704, 100
28224, V, 1, 1, 1, 1, 0, 704, 100
28225, V, 1, 1, 1, 1, 0, 704, 100
28226, V, 1, 1, 1, 1, 0, 704, 100
28227, V, 1, 1, 1, 1, 0, 704, 100
28228, V, 1, 1, 1, 1, 0, 704, 100
28229, V, 1, 1, 1, 1, 0, 704, 100
28230, V, 1, 1, 1, 1, 0, 704, 100
28231, V, 1, 1, 1, 1, 0, 704, 100
28232, V, 1, 1, 1, 1, 0, 704, 100
28233, V, 1, 1, 1, 1, 0, 704, 100
28234, V, 1, 1, 1, 1, 0, 704, 100
28235, V, 1, 1, 1, 1, 0, 704, 100
28236, V, 1, 1, 1, 1, 0, 704, 100
28237, V, 1, 1, 1, 1, 0, 704, 100
28238, V, 1, 1, 1, 1, 0, 704, 100
28239, V, 1, 1, 1, 1, 0, 704, 100
28240, V, 1, 1, 1, 1, 0, 704, 100
28241, V, 1, 1, 1, 1, 0, 704, 100
28242, V, 1, 1, 1, 1, 0, 704, 100
28243, V, 1, 1, 1, 1, 0, 704, 100
28244, V, 1, 1, 1, 1, 0, 704, 100
28246, V, 1, 1, 1, 1, 0, 704, 100
28247, V, 1, 1, 1, 1, 0, 704, 100
28248, V, 1, 1, 1, 1, 0, 704, 100
28249, V, 1, 1, 1, 1, 0, 704, 100
28250, V, 1, 1, 1, 1, 0, 704, 100
28251, V, 1, 1, 1, 1, 0, 704, 100
28252, V, 1, 1, 1, 1, 0, 704, 100
28253, V, 1, 1, 1, 1, 0, 704, 100
28254, V, 1, 1, 1, 1, 0, 704, 100
28255, V, 1, 1, 1, 1, 0, 704, 100
28256, V, 1, 1, 1, 1, 0, 704, 100
28257, V, 1, 1, 1, 1, 0, 704, 100
28258, V, 1, 1, 1, 1, 0, 704, 100
28259, V, 1, 1, 1, 1, 0, 704, 100
28260, V, 1, 1, 1, 1, 0, 704, 100
28261, V, 1, 1, 1, 1, 0, 704, 100
28262, V, 1, 1, 1, 1, 0, 704, 100
28263, V, 1, 1, 1, 1, 0, 704, 100
28264, V, 1, 1, 1, 1, 0, 704, 100
28265, V, 1, 1, 1, 1, 0, 704, 100
28266, V, 1, 1, 1, 1, 0, 704, 100
28267, V, 1, 1, 1, 1, 0, 704, 100
28268, V, 1, 1, 1, 1, 0, 704, 100
28269, V, 1, 1, 1, 1, 0, 704, 100
28270, V, 1, 1, 1, 1, 0, 704, 100
28271, V, 1, 1, 1, 1, 0, 704, 100
28272, V, 1, 1, 1, 1, 0, 704, 100
28273, V, 1, 1, 1, 1, 0, 704, 100
28274, V, 1, 1, 1, 1, 0, 704, 100
28275, V, 1, 1, 1, 1, 0, 704, 100
28276, V, 1, 1, 1, 1, 0, 704, 100
28277, V, 1, 1, 1, 1, 0, 704, 100
28278, V, 1, 1, 1, 1, 0, 704, 100
28279, V, 1, 1, 1, 1, 0, 704, 100
28280, V, 1, 1, 1, 1, 0, 704, 100
28281, V, 1, 1, 1, 1, 0, 704, 100
28282, V, 1, 1, 1, 1, 0, 704, 100
28283, V, 1, 1, 1, 1, 0, 704, 100
28284, V, 1, 1, 1, 1, 0, 704, 100
28285, V, 1, 1, 1, 1, 0, 704, 100
28286, V, 1, 1, 1, 1, 0, 704, 100
28288, V, 1, 1, 1, 1, 0, 704, 100
28289, V, 1, 1, 1, 1, 0, 704, 100
28290, V, 1, 1, 1, 1, 0, 704, 100
28291, V, 1, 1, 1, 1, 0, 704, 100
28292, V, 1, 1, 1, 1, 0, 704, 100
28293, V, 1, 1, 1, 1, 0, 704, 100
28294, V, 1, 1, 1, 1, 0, 704, 100
28295, V, 1, 1, 1, 1, 0, 704, 100
28296, V, 1, 1, 1, 1, 0, 704, 100
28297, V, 1, 1, 1, 1, 0, 704, 100
28298, V, 1, 1, 1, 1, 0, 704, 100
28299, V, 1, 1, 1, 1, 0, 704, 100
28300, V, 1, 1, 1, 1, 0, 704, 100
28301, V, 1, 1, 1, 1, 0, 704, 100
28302, V, 1, 1, 1, 1, 0, 704, 100
28303, V, 1, 1, 1, 1, 0, 704, 100
28304, V, 1, 1, 1, 1, 0, 704, 100
28305, V, 1, 1, 1, 1, 0, 704, 100
28306, V, 1, 1, 1, 1, 0, 704, 100
28307, V, 1, 1, 1, 1, 0, 704, 100
28308, V, 1, 1, 1, 1, 0, 704, 100
28309, V, 1, 1, 1, 1, 0, 704, 100
28310, V, 1, 1, 1, 1, 0, 704, 100
28311, V, 1, 1, 1, 1, 0, 704, 100
28312, V, 1, 1, 1, 1, 0, 704, 100
28313, V, 1, 1, 1, 1, 0, 704, 100
28314, V, 1, 1, 1, 1, 0, 704, 100
28315, V, 1, 1, 1, 1, 0, 704, 100
28316, V, 1, 1, 1, 1, 0, 704, 100
28317, V, 1, 1, 1, 1, 0, 704, 100
28318, V, 1, 1, 1, 1, 0, 704, 100
28319, V, 1, 1, 1, 1, 0, 704, 100
28320, V, 1, 1, 1, 1, 0, 704, 100
28321, V, 1, 1, 1, 1, 0, 704, 100
28322, V, 1, 1, 1, 1, 0, 704, 100
28323, V, 1, 1, 1, 1, 0, 704, 100
28324, V, 1, 1, 1, 1, 0, 704, 100
28325, V, 1, 1, 1, 1, 0, 704, 100
28326, V, 1, 1, 1, 1, 0, 704, 100
28327, V, 1, 1, 1, 1, 0, 704, 100
28328, V, 1, 1, 1, 1, 0, 704, 100
28329, V, 1, 1, 1, 1, 0, 704, 100
28331, V, 1, 1, 1, 1, 0, 704, 100
28332, V, 1, 1, 1, 1, 0, 704, 100
28333, V, 1, 1, 1, 1, 0, 704, 100
28334, V, 1, 1, 1, 1, 0, 704, 100
28335, V, 1, 1, 1, 1, 0, 704, 100
28336, V, 1, 1, 1, 1, 0, 704, 100
28337, V, 1, 1, 1, 1, 0, 704, 100
28338, V, 1, 1, 1, 1, 0, 704, 100
28339, V, 1, 1, 1, 1, 0, 704, 100
28340, V, 1, 1, 1, 1, 0, 704, 100
28341, V, 1, 1, 1, 1, 0, 704, 100
28342, V, 1, 1, 1, 1, 0, 704, 100
28343, V, 1, 1, 1, 1, 0, 704, 100
28344, V, 1, 1, 1, 1, 0, 704, 100
28345, V, 1, 1, 1, 1, 0, 704, 100
28346, V, 1, 1, 1, 1, 0, 704, 100
28347, V, 1, 1, 1, 1, 0, 704, 100
28348, V, 1, 1, 1, 1, 0, 704, 100
28349, V, 1, 1, 1, 1, 0, 704, 100
28350, V, 1, 1, 1, 1, 0, 704, 100
28351, V, 1, 1, 1, 1, 0, 704, 100
28352, V, 1, 1, 1, 1, 0, 704, 100
28353, V, 1, 1, 1, 1, 0, 704, 100
28354, V, 1, 1, 1, 1, 0, 704, 100
28355, V, 1, 1, 1, 1, 0, 704, 100
28356, V, 1, 1, 1, 1, 0, 704, 100
28357, V, 1, 1, 1, 1, 0, 704, 100
28358, V, 1, 1, 1, 1, 0, 704, 100
28359, V, 1, 1, 1, 1, 0, 704, 100
28360, V, 1, 1, 1, 1, 0, 704, 100
28361, V, 1, 1, 1, 1, 0, 704, 100
28362, V, 1, 1, 1, 1, 0, 704, 100
28363, V, 1, 1, 1, 1, 0, 704, 100
28364, V, 1, 1, 1, 1, 0, 704, 100
28365, V, 1, 1, 1, 1, 0, 704, 100
28366, V, 1, 1, 1, 1, 0, 704, 100
28367, V, 1, 1, 1, 1, 0, 704, 100
28368, V, 1, 1, 1, 1, 0, 704, 100
28369, V, 1, 1, 1, 1, 0, 704, 100
28370, V, 1, 1, 1, 1, 0, 704, 100
28371, V, 1, 1, 1, 1, 0, 704, 100
28372, V, 1, 1, 1, 1, 0, 704, 100
28374, V, 1, 1, 1, 1, 0, 704, 100
28375, V, 1, 1, 1, 1, 0, 704, 100
28376, V, 1, 1, 1, 1, 0, 704, 100
28377, V, 1, 1, 1, 1, 0, 704, 100
28378, V, 1, 1, 1, 1, 0, 704, 100
28379, V, 1, 1, 1, 1, 0, 704, 100
28380, V, 1, 1, 1, 1, 0, 704, 100
28381, V, 1, 1, 1, 1, 0, 704, 100
28382, V, 1, 1, 1, 1, 0, 704, 100
28383, V, 1, 1, 1, 1, 0, 704, 100
28384, V, 1, 1, 1, 1, 0, 704, 100
28385, V, 1, 1, 1, 1, 0, 704, 100
28386, V, 1, 1, 1, 1, 0, 704, 100
28387, V, 1, 1, 1, 1, 0, 704, 100
28388, V, 1, 1, 1, 1, 0, 704, 100
28389, V, 1, 1, 1, 1, 0, 704, 100
28390, V, 1, 1, 1, 1, 0, 704, 100
28391, V, 1, 1, 1, 1, 0, 704, 100
28392, V, 1, 1, 1, 1, 0, 704, 100
28393, V, 1, 1, 1, 1, 0, 704, 100
28394, V, 1, 1, 1, 1, 0, 704, 100
28395, V, 1, 1, 1, 1, 0, 704, 100
28396, V, 1, 1, 1, 1, 0, 704, 100
28397, V, 1, 1, 1, 1, 0, 704, 100
28398, V, 1, 1, 1, 1, 0, 704, 100
28399, V, 1, 1, 1, 1, 0, 704, 100
28400, V, 1, 1, 1, 1, 0, 704, 100
28401, V, 1, 1, 1, 1, 0, 704, 100
28402, V, 1, 1, 1, 1, 0, 704, 100
28403, V, 1, 1, 1, 1, 0, 704, 100
28404, V, 1, 1, 1, 1, 0, 704, 100
28405, V, 1, 1, 1, 1, 0, 704, 100
28406, V, 1, 1, 1, 1, 0, 704, 100
28407, V, 1, 1, 1, 1, 0, 704, 100
28408, V, 1, 1, 1, 1, 0, 704, 100
28409, V, 1, 1, 1, 1, 0, 704, 100
28410, V, 1, 1, 1, 1, 0, 704, 100
28411, V, 1, 1, 1, 1, 0, 704, 100
28412, V, 1, 1, 1, 1, 0, 704, 100
28413, V, 1, 1, 1, 1, 0, 704, 100
28414, V, 1, 1, 1, 1, 0, 704, 100
28416, V, 1, 1, 1, 1, 0, 704, 100
28417, V, 1, 1, 1, 1, 0, 704, 100
28418, V, 1, 1, 1, 1, 0, 704, 100
28419, V, 1, 1, 1, 1, 0, 704, 100
28420, V, 1, 1, 1, 1, 0, 704, 100
28421, V, 1, 1, 1, 1, 0, 704, 100
28422, V, 1, 1, 1, 1, 0, 704, 100
28423, V, 1, 1, 1, 1, 0, 704, 100
28424, V, 1, 1, 1, 1, 0, 704, 100
28425, V, 1, 1, 1, 1, 0, 704, 100
28426, V, 1, 1, 1, 1, 0, 704, 100
28427, V, 1, 1, 1, 1, 0, 704, 100
28428, V, 1, 1, 1, 1, 0, 704, 100
28429, V, 1, 1, 1, 1, 0, 704, 100
28430, V, 1, 1, 1, 1, 0, 704, 100
28431, V, 1, 1, 1, 1, 0, 704, 100
28432, V, 1, 1, 1, 1, 0, 704, 100
28433, V, 1, 1, 1, 1, 0, 704, 100
28434, V, 1, 1, 1, 1, 0, 704, 100
28435, V, 1, 1, 1, 1, 0, 704, 100
28436, V, 1, 1, 1, 1, 0, 704, 100
28437, V, 1, 1, 1, 1, 0, 704, 100
28438, V, 1, 1, 1, 1, 0, 704, 100
28439, V, 1, 1, 1, 1, 0, 704, 100
28440, V, 1, 1, 1, 1, 0, 704, 100
28441, V, 1, 1, 1, 1, 0, 704, 100
28442, V, 1, 1, 1, 1, 0, 704, 100
28443, V, 1, 1, 1, 1, 0, 704, 100
28444, V, 1, 1, 1, 1, 0, 704, 100
28445, V, 1, 1, 1, 1, 0, 704, 100
28446, V, 1, 1, 1, 1, 0, 704, 100
28447, V, 1, 1, 1, 1, 0, 704, 100
28448, V, 1, 1, 1, 1, 0, 704, 100
28449, V, 1, 1, 1, 1, 0, 704, 100
28450, V, 1, 1, 1, 1, 0, 704, 100
28451, V, 1, 1, 1, 1, 0, 704, 100
28452, V, 1, 1, 1, 1, 0, 704, 100
28453, V, 1, 1, 1, 1, 0, 704, 100
28454, V, 1, 1, 1, 1, 0, 704, 100
28455, V, 1, 1, 1, 1, 0, 704, 100
28456, V, 1, 1, 1, 1, 0, 704, 100
28457, V, 1, 1, 1, 1, 0, 704, 100
28459, V, 1, 1, 1, 1, 0, 704, 100
28460, V, 1, 1, 1, 1, 0, 704, 100
28461, V, 1, 1, 1, 1, 0, 704, 100
28462, V, 1, 1, 1, 1, 0, 704, 100
28463, V, 1, 1, 1, 1, 0, 704, 100
28464, V, 1, 1, 1, 1, 0, 704, 100
28465, V, 1, 1, 1, 1, 0, 704, 100
28466, V, 1, 1, 1, 1, 0, 704, 100
28467, V, 1, 1, 1, 1, 0, 704, 100
28468, V, 1, 1, 1, 1, 0, 704, 100
28469, V, 1, 1, 1, 1, 0, 704, 100
28470, V, 1, 1, 1, 1, 0, 704, 100
28471, V, 1, 1, 1, 1, 0, 704, 100
28472, V, 1, 1, 1, 1, 0, 704, 100
28473, V, 1, 1, 1, 1, 0, 704, 100
28474, V, 1, 1, 1, 1, 0, 704, 100
28475, V, 1, 1, 1, 1, 0, 704, 100
28476, V, 1, 1, 1, 1, 0, 704, 100
28477, V, 1, 1, 1, 1, 0, 704, 100
28478, V, 1, 1, 1, 1, 0, 704, 100
28479, V, 1, 1, 1, 1, 0, 704, 100
28480, V, 1, 1, 1, 1, 0, 704, 100
28481, V, 1, 1, 1, 1, 0, 704, 100
28482, V, 1, 1, 1, 1, 0, 704, 100
28483, V, 1, 1, 1, 1, 0, 704, 100
28484, V, 1, 1, 1, 1, 0, 704, 100
28485, V, 1, 1, 1, 1, 0, 704, 100
28486, V, 1, 1, 1, 1, 0, 704, 100
28487, V, 1, 1, 1, 1, 0, 704, 100
28488, V, 1, 1, 1, 1, 0, 704, 100
28489, V, 1, 1, 1, 1, 0, 704, 100
28490, V, 1, 1, 1, 1, 0, 704, 100
28491, V, 1, 1, 1, 1, 0, 704, 100
28492, V, 1, 1, 1, 1, 0, 704, 100
28493, V, 1, 1, 1, 1, 0, 704, 100
28494, V, 1, 1, 1, 1, 0, 704, 100
28495, V, 1, 1, 1, 1, 0, 704, 100
28496, V, 1, 1, 1, 1, 0, 704, 100
28497, V, 1, 1, 1, 1, 0, 704, 100
28498, V, 1, 1, 1, 1, 0, 704, 100
28499, V, 1, 1, 1, 1, 0, 704, 100
28500, V, 1, 1, 1, 1, 0, 704, 100
28502, V, 1, 1, 1, 1, 0, 704, 100
28503, V, 1, 1, 1, 1, 0, 704, 100
28504, V, 1, 1, 1, 1, 0, 704, 100
28505, V, 1, 1, 1, 1, 0, 704, 100
28506, V, 1, 1, 1, 1, 0, 704, 100
28507, V, 1, 1, 1, 1, 0, 704, 100
28508, V, 1, 1, 1, 1, 0, 704, 100
28509, V, 1, 1, 1, 1, 0, 704, 100
28510, V, 1, 1, 1, 1, 0, 704, 100
28511, V, 1, 1, 1, 1, 0, 704, 100
28512, V, 1, 1, 1, 1, 0, 704, 100
28513, V, 1, 1, 1, 1, 0, 704, 100
28514, V, 1, 1, 1, 1, 0, 704, 100
28515, V, 1, 1, 1, 1, 0, 704, 100
28516, V, 1, 1, 1, 1, 0, 704, 100
28517, V, 1, 1, 1, 1, 0, 704, 100
28518, V, 1, 1, 1, 1, 0, 704, 100
28519, V, 1, 1, 1, 1, 0, 704, 100
28520, V, 1, 1, 1, 1, 0, 704, 100
28521, V, 1, 1, 1, 1, 0, 704, 100
28522, V, 1, 1, 1, 1, 0, 704, 100
28523, V, 1, 1, 1, 1, 0, 704, 100
28524, V, 1, 1, 1, 1, 0, 704, 100
28525, V, 1, 1, 1, 1, 0, 704, 100
28526, V, 1, 1, 1, 1, 0, 704, 100
28527, V, 1, 1, 1, 1, 0, 704, 100
28528, V, 1, 1, 1, 1, 0, 704, 100
28529, V, 1, 1, 1, 1, 0, 704, 100
28530, V, 1, 1, 1, 1, 0, 704, 100
28531, V, 1, 1, 1, 1, 0, 704, 100
28532, V, 1, 1, 1, 1, 0, 704, 100
28533, V, 1, 1, 1, 1, 0, 704, 100
28534, V, 1, 1, 1, 1, 0, 704, 100
28535, V, 1, 1, 1, 1, 0, 704, 100
28536, V, 1, 1, 1, 1, 0, 704, 100
28537, V, 1, 1, 1, 1, 0, 704, 100
28538, V, 1, 1, 1, 1, 0, 704, 100
28539, V, 1, 1, 1, 1, 0, 704, 100
28540, V, 1, 1, 1, 1, 0, 704, 100
28541, V, 1, 1, 1, 1, 0, 704, 100
28542, V, 1, 1, 1, 1, 0, 704, 100
28544, V, 1, 1, 1, 1, 0, 704, 100
28545, V, 1, 1, 1, 1, 0, 704, 100
28546, V, 1, 1, 1, 1, 0, 704, 100
28547, V, 1, 1, 1, 1, 0, 704, 100
28548, V, 1, 1, 1, 1, 0, 704, 100
28549, V, 1, 1, 1, 1, 0, 704, 100
28550, V, 1, 1, 1, 1, 0, 704, 100
28551, V, 1, 1, 1, 1, 0, 704, 100
28552, V, 1, 1, 1, 1, 0, 704, 100
28553, V, 1, 1, 1, 1, 0, 704, 100
28554, V, 1, 1, 1, 1, 0, 704, 100
28555, V, 1, 1, 1, 1, 0, 704, 100
28556, V, 1, 1, 1, 1, 0, 704, 100
28557, V, 1, 1, 1, 1, 0, 704, 100
28558, V, 1, 1, 1, 1, 0, 704, 100
28559, V, 1, 1, 1, 1, 0, 704, 100
28560, V, 1, 1, 1, 1, 0, 704, 100
28561, V, 1, 1, 1, 1, 0, 704, 100
28562, V, 1, 1, 1, 1, 0, 704, 100
28563, V, 1, 1, 1, 1, 0, 704, 100
28564, V, 1, 1, 1, 1, 0, 704, 100
28565, V, 1, 1, 1, 1, 0, 704, 100
28566, V, 1, 1, 1, 1, 0, 704, 100
28567, V, 1, 1, 1, 1, 0, 704, 100
28568, V, 1, 1, 1, 1, 0, 704, 100
28569, V, 1, 1, 1, 1, 0, 704, 100
28570, V, 1, 1, 1, 1, 0, 704, 100
28571, V, 1, 1, 1, 1, 0, 704, 100
28572, V, 1, 1, 1, 1, 0, 704, 100
28573, V, 1, 1, 1, 1, 0, 704, 100
28574, V, 1, 1, 1, 1, 0, 704, 100
28575, V, 1, 1, 1, 1, 0, 704, 100
28576, V, 1, 1, 1, 1, 0, 704, 100
28577, V, 1, 1, 1, 1, 0, 704, 100
28578, V, 1, 1, 1, 1, 0, 704, 100
28579, V, 1, 1, 1, 1, 0, 704, 100
28580, V, 1, 1, 1, 1, 0, 704, 100
28581, V, 1, 1, 1, 1, 0, 704, 100
28582, V, 1, 1, 1, 1, 0, 704, 100
28583, V, 1, 1, 1, 1, 0, 704, 100
28584, V, 1, 1, 1, 1, 0, 704, 100
28585, V, 1, 1, 1, 1, 0, 704, 100
28587, V, 1, 1, 1, 1, 0, 704, 100
28588, V, 1, 1, 1, 1, 0, 704, 100
28589, V, 1, 1, 1, 1, 0, 704, 100
28590, V, 1, 1, 1, 1, 0, 704, 100
28591, V, 1, 1, 1, 1, 0, 704, 100
28592, V, 1, 1, 1, 1, 0, 704, 100
28593, V, 1, 1, 1, 1, 0, 704, 100
28594, V, 1, 1, 1, 1, 0, 704, 100
28595, V, 1, 1, 1, 1, 0, 704, 100
28596, V, 1, 1, 1, 1, 0, 704, 100
28597, V, 1, 1, 1, 1, 0, 704, 100
28598, V, 1, 1, 1, 1, 0, 704, 100
28599, V, 1, 1, 1, 1, 0, 704, 100
28600, V, 1, 1, 1, 1, 0, 704, 100
28601, V, 1, 1, 1, 1, 0, 704, 100
28602, V, 1, 1, 1, 1, 0, 704, 100
28603, V, 1, 1, 1, 1, 0, 704, 100
28604, V, 1, 1, 1, 1, 0, 704, 100
28605, V, 1, 1, 1, 1, 0, 704, 100
28606, V, 1, 1, 1, 1, 0, 704, 100
28607, V, 1, 1, 1, 1, 0, 704, 100
28608, V, 1, 1, 1, 1, 0, 704, 100
28609, V, 1, 1, 1, 1, 0, 704, 100
28610, V, 1, 1, 1, 1, 0, 704, 100
28611, V, 1, 1, 1, 1, 0, 704, 100
28612, V, 1, 1, 1, 1, 0, 704, 100
28613, V, 1, 1, 1, 1, 0, 704, 100
28614, V, 1, 1, 1, 1, 0, 704, 100
28615, V, 1, 1, 1, 1, 0, 704, 100
28616, V, 1, 1, 1, 1, 0, 704, 100
28617, V, 1, 1, 1, 1, 0, 704, 100
28618, V, 1, 1, 1, 1, 0, 704, 100
28619, V, 1, 1, 1, 1, 0, 704, 100
28620, V, 1, 1, 1, 1, 0, 704, 100
28621, V, 1, 1, 1, 1, 0, 704, 100
28622, V, 1, 1, 1, 1, 0, 704, 100
28623, V, 1, 1, 1, 1, 0, 704, 100
28624, V, 1, 1, 1, 1, 0, 704, 100
28625, V, 1, 1, 1, 1, 0, 704, 100
28626, V, 1, 1, 1, 1, 0, 704, 100
28627, V, 1, 1, 1, 1, 0, 704, 100
28628, V, 1, 1, 1, 1, 0, 704, 100
28630, V, 1, 1, 1, 1, 0, 704, 100
28631, V, 1, 1, 1, 1, 0, 704, 100
28632, V, 1, 1, 1, 1, 0, 704, 100
28633, V, 1, 1, 1, 1, 0, 704, 100
28634, V, 1, 1, 1, 1, 0, 704, 100
28635, V, 1, 1, 1, 1, 0, 704, 100
28636, V, 1, 1, 1, 1, 0, 704, 100
28637, V, 1, 1, 1, 1, 0, 704, 100
28638, V, 1, 1, 1, 1, 0, 704, 100
28639, V, 1, 1, 1, 1, 0, 704, 100
28640, V, 1, 1, 1, 1, 0, 704, 100
28641, V, 1, 1, 1, 1, 0, 704, 100
28642, V, 1, 1, 1, 1, 0, 704, 100
28643, V, 1, 1, 1, 1, 0, 704, 100
28644, V, 1, 1, 1, 1, 0, 704, 100
28645, V, 1, 1, 1, 1, 0, 704, 100
28646, V, 1, 1, 1, 1, 0, 704, 100
28647, V, 1, 1, 1, 1, 0, 704, 100
28648, V, 1, 1, 1, 1, 0, 704, 100
28649, V, 1, 1, 1, 1, 0, 704, 100
28650, V, 1, 1, 1, 1, 0, 704, 100
28651, V, 1, 1, 1, 1, 0, 704, 100
28652, V, 1, 1, 1, 1, 0, 704, 100
28653, V, 1, 1, 1, 1, 0, 704, 100
28654, V, 1, 1, 1, 1, 0, 704, 100
28655, V, 1, 1, 1, 1, 0, 704, 100
28656, V, 1, 1, 1, 1, 0, 704, 100
28657, V, 1, 1, 1, 1, 0, 704, 100
28658, V, 1, 1, 1, 1, 0, 704, 100
28659, V, 1, 1, 1, 1, 0, 704, 100
28660, V, 1, 1, 1, 1, 0, 704, 100
28661, V, 1, 1, 1, 1, 0, 704, 100
28662, V, 1, 1, 1, 1, 0, 704, 100
28663, V, 1, 1, 1, 1, 0, 704, 100
28664, V, 1, 1, 1, 1, 0, 704, 100
28665, V, 1, 1, 1, 1, 0, 704, 100
28666, V, 1, 1, 1, 1, 0, 704, 100
28667, V, 1, 1, 1, 1, 0, 704, 100
28668, V, 1, 1, 1, 1, 0, 704, 100
28669, V, 1, 1, 1, 1, 0, 704, 100
28670, V, 1, 1, 1, 1, 0, 704, 100
28672, V, 1, 1, 1, 1, 0, 704, 100
28673, V, 1, 1, 1, 1, 0, 704, 100
28674, V, 1, 1, 1, 1, 0, 704, 100
28675, V, 1, 1, 1, 1, 0, 704, 100
28676, V, 1, 1, 1, 1, 0, 704, 100
28677, V, 1, 1, 1, 1, 0, 704, 100
28678, V, 1, 1, 1, 1, 0, 704, 100
28679, V, 1, 1, 1, 1, 0, 704, 100
28680, V, 1, 1, 1, 1, 0, 704, 100
28681, V, 1, 1, 1, 1, 0, 704, 100
28682, V, 1, 1, 1, 1, 0, 704, 100
28683, V, 1, 1, 1, 1, 0, 704, 100
28684, V, 1, 1, 1, 1, 0, 704, 100
28685, V, 1, 1, 1, 1, 0, 704, 100
28686, V, 1, 1, 1, 1, 0, 704, 100
28687, V, 1, 1, 1, 1, 0, 704, 100
28688, V, 1, 1, 1, 1, 0, 704, 100
28689, V, 1, 1, 1, 1, 0, 704, 100
28690, V, 1, 1, 1, 1, 0, 704, 100
28691, V, 1, 1, 1, 1, 0, 704, 100
28692, V, 1, 1, 1, 1, 0, 704, 100
28693, V, 1, 1, 1, 1, 0, 704, 100
28694, V, 1, 1, 1, 1, 0, 704, 100
28695, V, 1, 1, 1, 1, 0, 704, 100
28696, V, 1, 1, 1, 1, 0, 704, 100
28697, V, 1, 1, 1, 1, 0, 704, 100
28698, V, 1, 1, 1, 1, 0, 704, 100
28699, V, 1, 1, 1, 1, 0, 704, 100
28700, V, 1, 1, 1, 1, 0, 704, 100
28701, V, 1, 1, 1, 1, 0, 704, 100
28702, V, 1, 1, 1, 1, 0, 704, 100
28703, V, 1, 1, 1, 1, 0, 704, 100
28704, V, 1, 1, 1, 1, 0, 704, 100
28705, V, 1, 1, 1, 1, 0, 704, 100
28706, V, 1, 1, 1, 1, 0, 704, 100
28707, V, 1, 1, 1, 1, 0, 704, 100
28708, V, 1, 1, 1, 1, 0, 704, 100
28709, V, 1, 1, 1, 1, 0, 704, 100
28710, V, 1, 1, 1, 1, 0, 704, 100
28711, V, 1, 1, 1, 1, 0, 704, 100
28712, V, 1, 1, 1, 1, 0, 704, 100
28713, V, 1, 1, 1, 1, 0, 704, 100
28715, V, 1, 1, 1, 1, 0, 704, 100
28716, V, 1, 1, 1, 1, 0, 704, 100
28717, V, 1, 1, 1, 1, 0, 704, 100
28718, V, 1, 1, 1, 1, 0, 704, 100
28719, V, 1, 1, 1, 1, 0, 704, 100
28720, V, 1, 1, 1, 1, 0, 704, 100
28721, V, 1, 1, 1, 1, 0, 704, 100
28722, V, 1, 1, 1, 1, 0, 704, 100
28723, V, 1, 1, 1, 1, 0, 704, 100
28724, V, 1, 1, 1, 1, 0, 704, 100
28725, V, 1, 1, 1, 1, 0, 704, 100
28726, V, 1, 1, 1, 1, 0, 704, 100
28727, V, 1, 1, 1, 1, 0, 704, 100
28728, V, 1, 1, 1, 1, 0, 704, 100
28729, V, 1, 1, 1, 1, 0, 704, 100
28730, V, 1, 1, 1, 1, 0, 704, 100
28731, V, 1, 1, 1, 1, 0, 704, 100
28732, V, 1, 1, 1, 1, 0, 704, 100
28733, V, 1, 1, 1, 1, 0, 704, 100
28734, V, 1, 1, 1, 1, 0, 704, 100
28735, V, 1, 1, 1, 1, 0, 704, 100
28736, V, 1, 1, 1, 1, 0, 704, 100
28737, V, 1, 1, 1, 1, 0, 704, 100
28738, V, 1, 1, 1, 1, 0, 704, 100
28739, V, 1, 1, 1, 1, 0, 704, 100
28740, V, 1, 1, 1, 1, 0, 704, 100
28741, V, 1, 1, 1, 1, 0, 704, 100
28742, V, 1, 1, 1, 1, 0, 704, 100
28743, V, 1, 1, 1, 1, 0, 704, 100
28744, V, 1, 1, 1, 1, 0, 704, 100
28745, V, 1, 1, 1, 1, 0, 704, 100
28746, V, 1, 1, 1, 1, 0, 704, 100
28747, V, 1, 1, 1, 1, 0, 704, 100
28748, V, 1, 1, 1, 1, 0, 704, 100
28749, V, 1, 1, 1, 1, 0, 704, 100
28750, V, 1, 1, 1, 1, 0, 704, 100
28751, V, 1, 1, 1, 1, 0, 704, 100
28752, V, 1, 1, 1, 1, 0, 704, 100
28753, V, 1, 1, 1, 1, 0, 704, 100
28754, V, 1, 1, 1, 1, 0, 704, 100
28755, V, 1, 1, 1, 1, 0, 704, 100
28756, V, 1, 1, 1, 1, 0, 704, 100
28758, V, 1, 1, 1, 1, 0, 704, 100
28759, V, 1, 1, 1, 1, 0, 704, 100
28760, V, 1, 1, 1, 1, 0, 704, 100
28761, V, 1, 1, 1, 1, 0, 704, 100
28762, V, 1, 1, 1, 1, 0, 704, 100
28763, V, 1, 1, 1, 1, 0, 704, 100
28764, V, 1, 1, 1, 1, 0, 704, 100
28765, V, 1, 1, 1, 1, 0, 704, 100
28766, V, 1, 1, 1, 1, 0, 704, 100
28767, V, 1, 1, 1, 1, 0, 704, 100
28768, V, 1, 1, 1, 1, 0, 704, 100
28769, V, 1, 1, 1, 1, 0, 704, 100
28770, V, 1, 1, 1, 1, 0, 704, 100
28771, V, 1, 1, 1, 1, 0, 704, 100
28772, V, 1, 1, 1, 1, 0, 704, 100
28773, V, 1, 1, 1, 1, 0, 704, 100
28774, V, 1, 1, 1, 1, 0, 704, 100
28775, V, 1, 1, 1, 1, 0, 704, 100
28776, V, 1, 1, 1, 1, 0, 704, 100
28777, V, 1, 1, 1, 1, 0, 704, 100
28778, V, 1, 1, 1, 1, 0, 704, 100
28779, V, 1, 1, 1, 1, 0, 704, 100
28780, V, 1, 1, 1, 1, 0, 704, 100
28781, V, 1, 1, 1, 1, 0, 704, 100
28782, V, 1, 1, 1, 1, 0, 704, 100
28783, V, 1, 1, 1, 1, 0, 704, 100
28784, V, 1, 1, 1, 1, 0, 704, 100
28785, V, 1, 1, 1, 1, 0, 704, 100
28786, V, 1, 1, 1, 1, 0, 704, 100
28787, V, 1, 1, 1, 1, 0, 704, 100
28788, V, 1, 1, 1, 1, 0, 704, 100
28789, V, 1, 1, 1, 1, 0, 704, 100
28790, V, 1, 1, 1, 1, 0, 704, 100
28791, V, 1, 1, 1, 1, 0, 704, 100
28792, V, 1, 1, 1, 1, 0, 704, 100
28793, V, 1, 1, 1, 1, 0, 704, 100
28794, V, 1, 1, 1, 1, 0, 704, 100
28795, V, 1, 1, 1, 1, 0, 704, 100
28796, V, 1, 1, 1, 1, 0, 704, 100
28797, V, 1, 1, 1, 1, 0, 704, 100
28798, V, 1, 1, 1, 1, 0, 704, 100
28800, V, 1, 1, 1, 1, 0, 704, 100
28801, V, 1, 1, 1, 1, 0, 704, 100
28802, V, 1, 1, 1, 1, 0, 704, 100
28803, V, 1, 1, 1, 1, 0, 704, 100
28804, V, 1, 1, 1, 1, 0, 704, 100
28805, V, 1, 1, 1, 1, 0, 704, 100
28806, V, 1, 1, 1, 1, 0, 704, 100
28807, V, 1, 1, 1, 1, 0, 704, 100
28808, V, 1, 1, 1, 1, 0, 704, 100
28809, V, 1, 1, 1, 1, 0, 704, 100
28810, V, 1, 1, 1, 1, 0, 704, 100
28811, V, 1, 1, 1, 1, 0, 704, 100
28812, V, 1, 1, 1, 1, 0, 704, 100
28813, V, 1, 1, 1, 1, 0, 704, 100
28814, V, 1, 1, 1, 1, 0, 704, 100
28815, V, 1, 1, 1, 1, 0, 704, 100
28816, V, 1, 1, 1, 1, 0, 704, 100
28817, V, 1, 1, 1, 1, 0, 704, 100
28818, V, 1, 1, 1, 1, 0, 704, 100
28819, V, 1, 1, 1, 1, 0, 704, 100
28820, V, 1, 1, 1, 1, 0, 704, 100
28821, V, 1, 1, 1, 1, 0, 704, 100
28822, V, 1, 1, 1, 1, 0, 704, 100
28823, V, 1, 1, 1, 1, 0, 704, 100
28824, V, 1, 1, 1, 1, 0, 704, 100
28825, V, 1, 1, 1, 1, 0, 704, 100
28826, V, 1, 1, 1, 1, 0, 704, 100
28827, V, 1, 1, 1, 1, 0, 704, 100
28828, V, 1, 1, 1, 1, 0, 704, 100
28829, V, 1, 1, 1, 1, 0, 704, 100
28830, V, 1, 1, 1, 1, 0, 704, 100
28831, V, 1, 1, 1, 1, 0, 704, 100
28832, V, 1, 1, 1, 1, 0, 704, 100
28833, V, 1, 1, 1, 1, 0, 704, 100
28834, V, 1, 1, 1, 1, 0, 704, 100
28835, V, 1, 1, 1, 1, 0, 704, 100
28836, V, 1, 1, 1, 1, 0, 704, 100
28837, V, 1, 1, 1, 1, 0, 704, 100
28838, V, 1, 1, 1, 1, 0, 704, 100
28839, V, 1, 1, 1, 1, 0, 704, 100
28840, V, 1, 1, 1, 1, 0, 704, 100
28841, V, 1, 1, 1, 1, 0, 704, 100
28843, V, 1, 1, 1, 1, 0, 704, 100
28844, V, 1, 1, 1, 1, 0, 704, 100
28845, V, 1, 1, 1, 1, 0, 704, 100
28846, V, 1, 1, 1, 1, 0, 704, 100
28847, V, 1, 1, 1, 1, 0, 704, 100
28848, V, 1, 1, 1, 1, 0, 704, 100
28849, V, 1, 1, 1, 1, 0, 704, 100
28850, V, 1, 1, 1, 1, 0, 704, 100
28851, V, 1, 1, 1, 1, 0, 704, 100
28852, V, 1, 1, 1, 1, 0, 704, 100
28853, V, 1, 1, 1, 1, 0, 704, 100
28854, V, 1, 1, 1, 1, 0, 704, 100
28855, V, 1, 1, 1, 1, 0, 704, 100
28856, V, 1, 1, 1, 1, 0, 704, 100
28857, V, 1, 1, 1, 1, 0, 704, 100
28858, V, 1, 1, 1, 1, 0, 704, 100
28859, V, 1, 1, 1, 1, 0, 704, 100
28860, V, 1, 1, 1, 1, 0, 704, 100
28861, V, 1, 1, 1, 1, 0, 704, 100
28862, V, 1, 1, 1, 1, 0, 704, 100
28863, V, 1, 1, 1, 1, 0, 704, 100
28864, V, 1, 1, 1, 1, 0, 704, 100
28865, V, 1, 1, 1, 1, 0, 704, 100
28866, V, 1, 1, 1, 1, 0, 704, 100
28867, V, 1, 1, 1, 1, 0, 704, 100
28868, V, 1, 1, 1, 1, 0, 704, 100
28869, V, 1, 1, 1, 1, 0, 704, 100
28870, V, 1, 1, 1, 1, 0, 704, 100
28871, V, 1, 1, 1, 1, 0, 704, 100
28872, V, 1, 1, 1, 1, 0, 704, 100
28873, V, 1, 1, 1, 1, 0, 704, 100
28874, V, 1, 1, 1, 1, 0, 704, 100
28875, V, 1, 1, 1, 1, 0, 704, 100
28876, V, 1, 1, 1, 1, 0, 704, 100
28877, V, 1, 1, 1, 1, 0, 704, 100
28878, V, 1, 1, 1, 1, 0, 704, 100
28879, V, 1, 1, 1, 1, 0, 704, 100
28880, V, 1, 1, 1, 1, 0, 704, 100
28881, V, 1, 1, 1, 1, 0, 704, 100
28882, V, 1, 1, 1, 1, 0, 704, 100
28883, V, 1, 1, 1, 1, 0, 704, 100
28884, V, 1, 1, 1, 1, 0, 704, 100
28886, V, 1, 1, 1, 1, 0, 704, 100
28887, V, 1, 1, 1, 1, 0, 704, 100
28888, V, 1, 1, 1, 1, 0, 704, 100
28889, V, 1, 1, 1, 1, 0, 704, 100
28890, V, 1, 1, 1, 1, 0, 704, 100
28891, V, 1, 1, 1, 1, 0, 704, 100
28892, V, 1, 1, 1, 1, 0, 704, 100
28893, V, 1, 1, 1, 1, 0, 704, 100
28894, V, 1, 1, 1, 1, 0, 704, 100
28895, V, 1, 1, 1, 1, 0, 704, 100
28896, V, 1, 1, 1, 1, 0, 704, 100
28897, V, 1, 1, 1, 1, 0, 704, 100
28898, V, 1, 1, 1, 1, 0, 704, 100
28899, V, 1, 1, 1, 1, 0, 704, 100
28900, V, 1, 1, 1, 1, 0, 704, 100
28901, V, 1, 1, 1, 1, 0, 704, 100
28902, V, 1, 1, 1, 1, 0, 704, 100
28903, V, 1, 1, 1, 1, 0, 704, 100
28904, V, 1, 1, 1, 1, 0, 704, 100
28905, V, 1, 1, 1, 1, 0, 704, 100
28906, V, 1, 1, 1, 1, 0, 704, 100
28907, V, 1, 1, 1, 1, 0, 704, 100
28908, V, 1, 1, 1, 1, 0, 704, 100
28909, V, 1, 1, 1, 1, 0, 704, 100
28910, V, 1, 1, 1, 1, 0, 704, 100
28911, V, 1, 1, 1, 1, 0, 704, 100
28912, V, 1, 1, 1, 1, 0, 704, 100
28913, V, 1, 1, 1, 1, 0, 704, 100
28914, V, 1, 1, 1, 1, 0, 704, 100
28915, V, 1, 1, 1, 1, 0, 704, 100
28916, V, 1, 1, 1, 1, 0, 704, 100
28917, V, 1, 1, 1, 1, 0, 704, 100
28918, V, 1, 1, 1, 1, 0, 704, 100
28919, V, 1, 1, 1, 1, 0, 704, 100
28920, V, 1, 1, 1, 1, 0, 704, 100
28921, V, 1, 1, 1, 1, 0, 704, 100
28922, V, 1, 1, 1, 1, 0, 704, 100
28923, V, 1, 1, 1, 1, 0, 704, 100
28924, V, 1, 1, 1, 1, 0, 704, 100
28925, V, 1, 1, 1, 1, 0, 704, 100
28926, V, 1, 1, 1, 1, 0, 704, 100
28928, V, 1, 1, 1, 1, 0, 704, 100
28929, V, 1, 1, 1, 1, 0, 704, 100
28930, V, 1, 1, 1, 1, 0, 704, 100
28931, V, 1, 1, 1, 1, 0, 704, 100
28932, V, 1, 1, 1, 1, 0, 704, 100
28933, V, 1, 1, 1, 1, 0, 704, 100
28934, V, 1, 1, 1, 1, 0, 704, 100
28935, V, 1, 1, 1, 1, 0, 704, 100
28936, V, 1, 1, 1, 1, 0, 704, 100
28937, V, 1, 1, 1, 1, 0, 704, 100
28938, V, 1, 1, 1, 1, 0, 704, 100
28939, V, 1, 1, 1, 1, 0, 704, 100
28940, V, 1, 1, 1, 1, 0, 704, 100
28941, V, 1, 1, 1, 1, 0, 704, 100
28942, V, 1, 1, 1, 1, 0, 704, 100
28943, V, 1, 1, 1, 1, 0, 704, 100
28944, V, 1, 1, 1, 1, 0, 704, 100
28945, V, 1, 1, 1, 1, 0, 704, 100
28946, V, 1, 1, 1, 1, 0, 704, 100
28947, V, 1, 1, 1, 1, 0, 704, 100
28948, V, 1, 1, 1, 1, 0, 704, 100
28949, V, 1, 1, 1, 1, 0, 704, 100
28950, V, 1, 1, 1, 1, 0, 704, 100
28951, V, 1, 1, 1, 1, 0, 704, 100
28952, V, 1, 1, 1, 1, 0, 704, 100
28953, V, 1, 1, 1, 1, 0, 704, 100
28954, V, 1, 1, 1, 1, 0, 704, 100
28955, V, 1, 1, 1, 1, 0, 704, 100
28956, V, 1, 1, 1, 1, 0, 704, 100
28957, V, 1, 1, 1, 1, 0, 704, 100
28958, V, 1, 1, 1, 1, 0, 704, 100
28959, V, 1, 1, 1, 1, 0, 704, 100
28960, V, 1, 1, 1, 1, 0, 704, 100
28961, V, 1, 1, 1, 1, 0, 704, 100
28962, V, 1, 1, 1, 1, 0, 704, 100
28963, V, 1, 1, 1, 1, 0, 704, 100
28964, V, 1, 1, 1, 1, 0, 704, 100
28965, V, 1, 1, 1, 1, 0, 704, 100
28966, V, 1, 1, 1, 1, 0, 704, 100
28967, V, 1, 1, 1, 1, 0, 704, 100
28968, V, 1, 1, 1, 1, 0, 704, 100
28969, V, 1, 1, 1, 1, 0, 704, 100
28971, V, 1, 1, 1, 1, 0, 704, 100
28972, V, 1, 1, 1, 1, 0, 704, 100
28973, V, 1, 1, 1, 1, 0, 704, 100
28974, V, 1, 1, 1, 1, 0, 704, 100
28975, V, 1, 1, 1, 1, 0, 704, 100
28976, V, 1, 1, 1, 1, 0, 704, 100
28977, V, 1, 1, 1, 1, 0, 704, 100
28978, V, 1, 1, 1, 1, 0, 704, 100
28979, V, 1, 1, 1, 1, 0, 704, 100
28980, V, 1, 1, 1, 1, 0, 704, 100
28981, V, 1, 1, 1, 1, 0, 704, 100
28982, V, 1, 1, 1, 1, 0, 704, 100
28983, V, 1, 1, 1, 1, 0, 704, 100
28984, V, 1, 1, 1, 1, 0, 704, 100
28985, V, 1, 1, 1, 1, 0, 704, 100
28986, V, 1, 1, 1, 1, 0, 704, 100
28987, V, 1, 1, 1, 1, 0, 704, 100
28988, V, 1, 1, 1, 1, 0, 704, 100
28989, V, 1, 1, 1, 1, 0, 704, 100
28990, V, 1, 1, 1, 1, 0, 704, 100
28991, V, 1, 1, 1, 1, 0, 704, 100
28992, V, 1, 1, 1, 1, 0, 704, 100
28993, V, 1, 1, 1, 1, 0, 704, 100
28994, V, 1, 1, 1, 1, 0, 704, 100
28995, V, 1, 1, 1, 1, 0, 704, 100
28996, V, 1, 1, 1, 1, 0, 704, 100
28997, V, 1, 1, 1, 1, 0, 704, 100
28998, V, 1, 1, 1, 1, 0, 704, 100
28999, V, 1, 1, 1, 1, 0, 704, 100
29000, V, 1, 1, 1, 1, 0, 704, 100
29001, V, 1, 1, 1, 1, 0, 704, 100
29002, V, 1, 1, 1, 1, 0, 704, 100
29003, V, 1, 1, 1, 1, 0, 704, 100
29004, V, 1, 1, 1, 1, 0, 704, 100
29005, V, 1, 1, 1, 1, 0, 704, 100
29006, V, 1, 1, 1, 1, 0, 704, 100
29007, V, 1, 1, 1, 1, 0, 704, 100
29008, V, 1, 1, 1, 1, 0, 704, 100
29009, V, 1, 1, 1, 1, 0, 704, 100
29010, V, 1, 1, 1, 1, 0, 704, 100
29011, V, 1, 1, 1, 1, 0, 704, 100
29012, V, 1, 1, 1, 1, 0, 704, 100
29014, V, 1, 1, 1, 1, 0, 704, 100
29015, V, 1, 1, 1, 1, 0, 704, 100
29016, V, 1, 1, 1, 1, 0, 704, 100
29017, V, 1, 1, 1, 1, 0, 704, 100
29018, V, 1, 1, 1, 1, 0, 704, 100
29019, V, 1, 1, 1, 1, 0, 704, 100
29020, V, 1, 1, 1, 1, 0, 704, 100
29021, V, 1, 1, 1, 1, 0, 704, 100
29022, V, 1, 1, 1, 1, 0, 704, 100
29023, V, 1, 1, 1, 1, 0, 704, 100
29024, V, 1, 1, 1, 1, 0, 704, 100
29025, V, 1, 1, 1, 1, 0, 704, 100
29026, V, 1, 1, 1, 1, 0, 704, 100
29027, V, 1, 1, 1, 1, 0, 704, 100
29028, V, 1, 1, 1, 1, 0, 704, 100
29029, V, 1, 1, 1, 1, 0, 704, 100
29030, V, 1, 1, 1, 1, 0, 704, 100
29031, V, 1, 1, 1, 1, 0, 704, 100
29032, V, 1, 1, 1, 1, 0, 704, 100
29033, V, 1, 1, 1, 1, 0, 704, 100
29034, V, 1, 1, 1, 1, 0, 704, 100
29035, V, 1, 1, 1, 1, 0, 704, 100
29036, V, 1, 1, 1, 1, 0, 704, 100
29037, V, 1, 1, 1, 1, 0, 704, 100
29038, V, 1, 1, 1, 1, 0, 704, 100
29039, V, 1, 1, 1, 1, 0, 704, 100
29040, V, 1, 1, 1, 1, 0, 704, 100
29041, V, 1, 1, 1, 1, 0, 704, 100
29042, V, 1, 1, 1, 1, 0, 704, 100
29043, V, 1, 1, 1, 1, 0, 704, 100
29044, V, 1, 1, 1, 1, 0, 704, 100
29045, V, 1, 1, 1, 1, 0, 704, 100
29046, V, 1, 1, 1, 1, 0, 704, 100
29047, V, 1, 1, 1, 1, 0, 704, 100
29048, V, 1, 1, 1, 1, 0, 704, 100
29049, V, 1, 1, 1, 1, 0, 704, 100
29050, V, 1, 1, 1, 1, 0, 704, 100
29051, V, 1, 1, 1, 1, 0, 704, 100
29052, V, 1, 1, 1, 1, 0, 704, 100
29053, V, 1, 1, 1, 1, 0, 704, 100
29054, V, 1, 1, 1, 1, 0, 704, 100
29056, V, 1, 1, 1, 1, 0, 704, 100
29057, V, 1, 1, 1, 1, 0, 704, 100
29058, V, 1, 1, 1, 1, 0, 704, 100
29059, V, 1, 1, 1, 1, 0, 704, 100
29060, V, 1, 1, 1, 1, 0, 704, 100
29061, V, 1, 1, 1, 1, 0, 704, 100
29062, V, 1, 1, 1, 1, 0, 704, 100
29063, V, 1, 1, 1, 1, 0, 704, 100
29064, V, 1, 1, 1, 1, 0, 704, 100
29065, V, 1, 1, 1, 1, 0, 704, 100
29066, V, 1, 1, 1, 1, 0, 704, 100
29067, V, 1, 1, 1, 1, 0, 704, 100
29068, V, 1, 1, 1, 1, 0, 704, 100
29069, V, 1, 1, 1, 1, 0, 704, 100
29070, V, 1, 1, 1, 1, 0, 704, 100
29071, V, 1, 1, 1, 1, 0, 704, 100
29072, V, 1, 1, 1, 1, 0, 704, 100
29073, V, 1, 1, 1, 1, 0, 704, 100
29074, V, 1, 1, 1, 1, 0, 704, 100
29075, V, 1, 1, 1, 1, 0, 704, 100
29076, V, 1, 1, 1, 1, 0, 704, 100
29077, V, 1, 1, 1, 1, 0, 704, 100
29078, V, 1, 1, 1, 1, 0, 704, 100
29079, V, 1, 1, 1, 1, 0, 704, 100
29080, V, 1, 1, 1, 1, 0, 704, 100
29081, V, 1, 1, 1, 1, 0, 704, 100
29082, V, 1, 1, 1, 1, 0, 704, 100
29083, V, 1, 1, 1, 1, 0, 704, 100
29084, V, 1, 1, 1, 1, 0, 704, 100
29085, V, 1, 1, 1, 1, 0, 704, 100
29086, V, 1, 1, 1, 1, 0, 704, 100
29087, V, 1, 1, 1, 1, 0, 704, 100
29088, V, 1, 1, 1, 1, 0, 704, 100
29089, V, 1, 1, 1, 1, 0, 704, 100
29090, V, 1, 1, 1, 1, 0, 704, 100
29091, V, 1, 1, 1, 1, 0, 704, 100
29092, V, 1, 1, 1, 1, 0, 704, 100
29093, V, 1, 1, 1, 1, 0, 704, 100
29094, V, 1, 1, 1, 1, 0, 704, 100
29095, V, 1, 1, 1, 1, 0, 704, 100
29096, V, 1, 1, 1, 1, 0, 704, 100
29097, V, 1, 1, 1, 1, 0, 704, 100
29099, V, 1, 1, 1, 1, 0, 704, 100
29100, V, 1, 1, 1, 1, 0, 704, 100
29101, V, 1, 1, 1, 1, 0, 704, 100
29102, V, 1, 1, 1, 1, 0, 704, 100
29103, V, 1, 1, 1, 1, 0, 704, 100
29104, V, 1, 1, 1, 1, 0, 704, 100
29105, V, 1, 1, 1, 1, 0, 704, 100
29106, V, 1, 1, 1, 1, 0, 704, 100
29107, V, 1, 1, 1, 1, 0, 704, 100
29108, V, 1, 1, 1, 1, 0, 704, 100
29109, V, 1, 1, 1, 1, 0, 704, 100
29110, V, 1, 1, 1, 1, 0, 704, 100
29111, V, 1, 1, 1, 1, 0, 704, 100
29112, V, 1, 1, 1, 1, 0, 704, 100
29113, V, 1, 1, 1, 1, 0, 704, 100
29114, V, 1, 1, 1, 1, 0, 704, 100
29115, V, 1, 1, 1, 1, 0, 704, 100
29116, V, 1, 1, 1, 1, 0, 704, 100
29117, V, 1, 1, 1, 1, 0, 704, 100
29118, V, 1, 1, 1, 1, 0, 704, 100
29119, V, 1, 1, 1, 1, 0, 704, 100
29120, V, 1, 1, 1, 1, 0, 704, 100
29121, V, 1, 0, 0, 1, 0, 704, 100
29121, V, 1, 0, 0, 0, 0, 704, 100
29122, V, 1, 1, 0, 0, 0, 704, 100
29122, V, 1, 1, 0, 0, 0, 704, 100
29123, V, 1, 1, 1, 1, 0, 704, 100
29124, V, 1, 1, 1, 1, 0, 704, 100
29125, V, 1, 1, 1, 1, 0, 704, 100
29126, V, 1, 1, 1, 1, 0, 704, 100
29127, V, 1, 1, 1, 1, 0, 704, 100
29128, V, 1, 1, 1, 1, 0, 704, 100
29129, V, 1, 1, 1, 1, 0, 704, 100
29130, V, 1, 1, 1, 1, 0, 704, 100
29131, V, 1, 1, 1, 1, 0, 704, 100
29132, V, 1, 1, 1, 1, 0, 704, 100
29133, V, 1, 1, 1, 1, 0, 704, 100
29134, V, 1, 1, 1, 1, 0, 704, 100
29135, V, 1, 1, 1, 1, 0, 704, 100
29136, V, 1, 1, 1, 1, 0, 704, 100
29137, V, 1, 1, 1, 1, 0, 704, 100
29138, V, 1, 1, 1, 1, 0, 704, 100
29139, V, 1, 1, 1, 1, 0, 704, 100
29140, V, 1, 1, 1, 1, 0, 704, 100
29142, V, 1, 1, 1, 1, 0, 704, 100
29143, V, 1, 1, 1, 1, 0, 704, 100
29144, V, 1, 1, 1, 1, 0, 704, 100
29145, V, 1, 1, 1, 1, 0, 704, 100
29146, V, 1, 1, 1, 1, 0, 704, 100
29147, V, 1, 1, 1, 1, 0, 704, 100
29148, V, 1, 1, 1, 1, 0, 704, 100
29149, V, 1, 1, 1, 1, 0, 704, 100
29150, V, 1, 1, 1, 1, 0, 704, 100
29151, V, 1, 1, 1, 1, 0, 704, 100
29152, V, 1, 1, 1, 1, 0, 704, 100
29153, V, 1, 1, 1, 1, 0, 704, 100
29154, V, 1, 1, 1, 1, 0, 704, 100
29155, V, 1, 1, 1, 1, 0, 704, 100
29156, V, 1, 1, 1, 1, 0, 704, 100
29157, V, 1, 1, 1, 1, 0, 704, 100
29158, V, 1, 1, 1, 1, 0, 704, 100
29159, V, 1, 1, 1, 1, 0, 704, 100
29160, V, 1, 1, 1, 1, 0, 704, 100
29161, V, 1, 1, 1, 1, 0, 704, 100
29162, V, 1, 1, 1, 1, 0, 704, 100
29163, V, 1, 1, 1, 1, 0, 704, 100
29164, V, 1, 1, 1, 1, 0, 704, 100
29165, V, 1, 1, 1, 1, 0, 704, 100
29166, V, 1, 1, 1, 1, 0, 704, 100
29167, V, 1, 1, 1, 1, 0, 704, 100
29168, V, 1, 1, 1, 1, 0, 704, 100
29169, V, 1, 1, 1, 1, 0, 704, 100
29170, V, 1, 1, 1, 1, 0, 704, 100
29171, V, 1, 1, 1, 1, 0, 704, 100
29172, V, 1, 1, 1, 1, 0, 704, 100
29173, V, 1, 1, 1, 1, 0, 704, 100
29174, V, 1, 1, 1, 1, 0, 704, 100
29175, V, 1, 1, 1, 1, 0, 704, 100
29176, V, 1, 1, 1, 1, 0, 704, 100
29177, V, 1, 1, 1, 1, 0, 704, 100
29178, V, 1, 1, 1, 1, 0, 704, 100
29179, V, 1, 1, 1, 1, 0, 704, 100
29180, V, 1, 1, 1, 1, 0, 704, 100
29181, V, 1, 1, 1, 1, 0, 704, 100
29182, V, 1, 1, 1, 1, 0, 704, 100
29184, V, 1, 1, 1, 1, 0, 704, 100
29185, V, 1, 1, 1, 1, 0, 704, 100
29186, V, 1, 1, 1, 1, 0, 704, 100
29187, V, 1, 1, 1, 1, 0, 704, 100
29188, V, 1, 1, 1, 1, 0, 704, 100
29189, V, 1, 1, 1, 1, 0, 704, 100
29190, V, 1, 1, 1, 1, 0, 704, 100
29191, V, 1, 1, 1, 1, 0, 704, 100
29192, V, 1, 1, 1, 1, 0, 704, 100
29193, V, 1, 1, 1, 1, 0, 704, 100
29194, V, 1, 1, 1, 1, 0, 704, 100
29195, V, 1, 1, 1, 1, 0, 704, 100
29196, V, 1, 1, 1, 1, 0, 704, 100
29197, V, 1, 1, 1, 1, 0, 704, 100
29198, V, 1, 1, 1, 1, 0, 704, 100
29199, V, 1, 1, 1, 1, 0, 704, 100
29200, V, 1, 1, 1, 1, 0, 704, 100
29201, V, 1, 1, 1, 1, 0, 704, 100
29202, V, 1, 1, 1, 1, 0, 704, 100
29203, V, 1, 1, 1, 1, 0, 704, 100
29204, V, 1, 1, 1, 1, 0, 704, 100
29205, V, 1, 1, 1, 1, 0, 704, 100
29206, V, 1, 1, 1, 1, 0, 704, 100
29207, V, 1, 1, 1, 1, 0, 704, 100
29208, V, 1, 1, 1, 1, 0, 704, 100
29209, V, 1, 1, 1, 1, 0, 704, 100
29210, V, 1, 1, 1, 1, 0, 704, 100
29211, V, 1, 1, 1, 1, 0, 704, 100
29212, V, 1, 1, 1, 1, 0, 704, 100
29213, V, 1, 1, 1, 1, 0, 704, 100
29214, V, 1, 1, 1, 1, 0, 704, 100
29215, V, 1, 1, 1, 1, 0, 704, 100
29216, V, 1, 1, 1, 1, 0, 704, 100
29217, V, 1, 1, 1, 1, 0, 704, 100
29218, V, 1, 1, 1, 1, 0, 704, 100
29219, V, 1, 1, 1, 1, 0, 704, 100
29220, V, 1, 1, 1, 1, 0, 704, 100
29221, V, 1, 1, 1, 1, 0, 704, 100
29222, V, 1, 1, 1, 1, 0, 704, 100
29223, V, 1, 1, 1, 1, 0, 704, 100
29224, V, 1, 1, 1, 1, 0, 704, 100
29225, V, 1, 1, 1, 1, 0, 704, 100
29227, V, 1, 1, 1, 1, 0, 704, 100
29228, V, 1, 1, 1, 1, 0, 704, 100
29229, V, 1, 1, 1, 1, 0, 704, 100
29230, V, 1, 1, 1, 1, 0, 704, 100
29231, V, 1, 1, 1, 1, 0, 704, 100
29232, V, 1, 1, 1, 1, 0, 704, 100
29233, V, 1, 1, 1, 1, 0, 704, 100
29234, V, 1, 1, 1, 1, 0, 704, 100
29235, V, 1, 1, 1, 1, 0, 704, 100
29236, V, 1, 1, 1, 1, 0, 704, 100
29237, V, 1, 1, 1, 1, 0, 704, 100
29238, V, 1, 1, 1, 1, 0, 704, 100
29239, V, 1, 1, 1, 1, 0, 704, 100
29240, V, 1, 1, 1, 1, 0, 704, 100
29241, V, 1, 1, 1, 1, 0, 704, 100
29242, V, 1, 1, 1, 1, 0, 704, 100
29243, V, 1, 1, 1, 1, 0, 704, 100
29244, V, 1, 1, 1, 1, 0, 704, 100
29245, V, 1, 1, 1, 1, 0, 704, 100
29246, V, 1, 1, 1, 1, 0, 704, 100
29247, V, 1, 1, 1, 1, 0, 704, 100
29248, V, 1, 1, 1, 1, 0, 704, 100
29249, V, 1, 1, 1, 1, 0, 704, 100
29250, V, 1, 1, 1, 1, 0, 704, 100
29251, V, 1, 1, 1, 1, 0, 704, 100
29252, V, 1, 1, 1, 1, 0, 704, 100
29253, V, 1, 1, 1, 1, 0, 704, 100
29254, V, 1, 1, 1, 1, 0, 704, 100
29255, V, 1, 1, 1, 1, 0, 704, 100
29256, V, 1, 1, 1, 1, 0, 704, 100
29257, V, 1, 1, 1, 1, 0, 704, 100
29258, V, 1, 1, 1, 1, 0, 704, 100
29259, V, 1, 1, 1, 1, 0, 704, 100
29260, V, 1, 1, 1, 1, 0, 704, 100
29261, V, 1, 1, 1, 1, 0, 704, 100
29262, V, 1, 1, 1, 1, 0, 704, 100
29263, V, 1, 1, 1, 1, 0, 704, 100
29264, V, 1, 1, 1, 1, 0, 704, 100
29265, V, 1, 1, 1, 1, 0, 704, 100
29266, V, 1, 1, 1, 1, 0, 704, 100
29267, V, 1, 1, 1, 1, 0, 704, 100
29268, V, 1, 1, 1, 1, 0, 704, 100
29270, V, 1, 1, 1, 1, 0, 704, 100
29271, V, 1, 1, 1, 1, 0, 704, 100
29272, V, 1, 1, 1, 1, 0, 704, 100
29273, V, 1, 1, 1, 1, 0, 704, 100
29274, V, 1, 1, 1, 1, 0, 704, 100
29275, V, 1, 1, 1, 1, 0, 704, 100
29276, V, 1, 1, 1, 1, 0, 704, 100
29277, V, 1, 1, 1, 1, 0, 704, 100
29278, V, 1, 1, 1, 1, 0, 704, 100
29279, V, 1, 1, 1, 1, 0, 704, 100
29280, V, 1, 1, 1, 1, 0, 704, 100
29281, V, 1, 1, 1, 1, 0, 704, 100
29282, V, 1, 1, 1, 1, 0, 704, 100
29283, V, 1, 1, 1, 1, 0, 704, 100
29284, V, 1, 1, 1, 1, 0, 704, 100
29285, V, 1, 1, 1, 1, 0, 704, 100
29286, V, 1, 1, 1, 1, 0, 704, 100
29287, V, 1, 1, 1, 1, 0, 704, 100
29288, V, 1, 1, 1, 1, 0, 704, 100
29289, V, 1, 1, 1, 1, 0, 704, 100
29290, V, 1, 1, 1, 1, 0, 704, 100
29291, V, 1, 1, 1, 1, 0, 704, 100
29292, V, 1, 1, 1, 1, 0, 704, 100
29293, V, 1, 1, 1, 1, 0, 704, 100
29294, V, 1, 1, 1, 1, 0, 704, 100
29295, V, 1, 1, 1, 1, 0, 704, 100
29296, V, 1, 1, 1, 1, 0, 704, 100
29297, V, 1, 1, 1, 1, 0, 704, 100
29298, V, 1, 1, 1, 1, 0, 704, 100
29299, V, 1, 1, 1, 1, 0, 704, 100
29300, V, 1, 1, 1, 1, 0, 704, 100
29301, V, 1, 1, 1, 1, 0, 704, 100
29302, V, 1, 1, 1, 1, 0, 704, 100
29303, V, 1, 1, 1, 1, 0, 704, 100
29304, V, 1, 1, 1, 1, 0, 704, 100
29305, V, 1, 1, 1, 1, 0, 704, 100
29306, V, 1, 1, 1, 1, 0, 704, 100
29307, V, 1, 1, 1, 1, 0, 704, 100
29308, V, 1, 1, 1, 1, 0, 704, 100
29309, V, 1, 1, 1, 1, 0, 704, 100
29310, V, 1, 1, 1, 1, 0, 704, 100
29312, V, 1, 1, 1, 1, 0, 704, 100
29313, V, 1, 1, 1, 1, 0, 704, 100
29314, V, 1, 1, 1, 1, 0, 704, 100
29315, V, 1, 1, 1, 1, 0, 704, 100
29316, V, 1, 1, 1, 1, 0, 704, 100
29317, V, 1, 1, 1, 1, 0, 704, 100
29318, V, 1, 1, 1, 1, 0, 704, 100
29319, V, 1, 1, 1, 1, 0, 704, 100
29320, V, 1, 1, 1, 1, 0, 704, 100
29321, V, 1, 1, 1, 1, 0, 704, 100
29322, V, 1, 1, 1, 1, 0, 704, 100
29323, V, 1, 1, 1, 1, 0, 704, 100
29324, V, 1, 1, 1, 1, 0, 704, 100
29325, V, 1, 1, 1, 1, 0, 704, 100
29326, V, 1, 1, 1, 1, 0, 704, 100
29327, V, 1, 1, 1, 1, 0, 704, 100
29328, V, 1, 1, 1, 1, 0, 704, 100
29329, V, 1, 1, 1, 1, 0, 704, 100
29330, V, 1, 1, 1, 1, 0, 704, 100
29331, V, 1, 1, 1, 1, 0, 704, 100
29332, V, 1, 1, 1, 1, 0, 704, 100
29333, V, 1, 1, 1, 1, 0, 704, 100
29334, V, 1, 1, 1, 1, 0, 704, 100
29335, V, 1, 1, 1, 1, 0, 704, 100
29336, V, 1, 1, 1, 1, 0, 704, 100
29337, V, 1, 1, 1, 1, 0, 704, 100
29338, V, 1, 1, 1, 1, 0, 704, 100
29339, V, 1, 1, 1, 1, 0, 704, 100
29340, V, 1, 1, 1, 1, 0, 704, 100
29341, V, 1, 1, 1, 1, 0, 704, 100
29342, V, 1, 1, 1, 1, 0, 704, 100
29343, V, 1, 1, 1, 1, 0, 704, 100
29344, V, 1, 1, 1, 1, 0, 704, 100
29345, V, 1, 1, 1, 1, 0, 704, 100
29346, V, 1, 1, 1, 1, 0, 704, 100
29347, V, 1, 1, 1, 1, 0, 704, 100
29348, V, 1, 1, 1, 1, 0, 704, 100
29349, V, 1, 1, 1, 1, 0, 704, 100
29350, V, 1, 1, 1, 1, 0, 704, 100
29351, V, 1, 1, 1, 1, 0, 704, 100
29352, V, 1, 1, 1, 1, 0, 704, 100
29353, V, 1, 1, 1, 1, 0, 704, 100
29355, V, 1, 1, 1, 1, 0, 704, 100
29356, V, 1, 1, 1, 1, 0, 704, 100
29357, V, 1, 1, 1, 1, 0, 704, 100
29358, V, 1, 1, 1, 1, 0, 704, 100
29359, V, 1, 1, 1, 1, 0, 704, 100
29360, V, 1, 1, 1, 1, 0, 704, 100
29361, V, 1, 1, 1, 1, 0, 704, 100
29362, V, 1, 1, 1, 1, 0, 704, 100
29363, V, 1, 1, 1, 1, 0, 704, 100
29364, V, 1, 1, 1, 1, 0, 704, 100
29365, V, 1, 1, 1, 1, 0, 704, 100
29366, V, 1, 1, 1, 1, 0, 704, 100
29367, V, 1, 1, 1, 1, 0, 704, 100
29368, V, 1, 1, 1, 1, 0, 704, 100
29369, V, 1, 1, 1, 1, 0, 704, 100
29370, V, 1, 1, 1, 1, 0, 704, 100
29371, V, 1, 1, 1, 1, 0, 704, 100
29372, V, 1, 1, 1, 1, 0, 704, 100
29373, V, 1, 1, 1, 1, 0, 704, 100
29374, V, 1, 1, 1, 1, 0, 704, 100
29375, V, 1, 1, 1, 1, 0, 704, 100
29376, V, 1, 1, 1, 1, 0, 704, 100
29377, V, 1, 1, 1, 1, 0, 704, 100
29378, V, 1, 1, 1, 1, 0, 704, 100
29379, V, 1, 1, 1, 1, 0, 704, 100
29380, V, 1, 1, 1, 1, 0, 704, 100
29381, V, 1, 1, 1, 1, 0, 704, 100
29382, V, 1, 1, 1, 1, 0, 704, 100
29383, V, 1, 1, 1, 1, 0, 704, 100
29384, V, 1, 1, 1, 1, 0, 704, 100
29385, V, 1, 1, 1, 1, 0, 704, 100
29386, V, 1, 1, 1, 1, 0, 704, 100
29387, V, 1, 1, 1, 1, 0, 704, 100
29388, V, 1, 1, 1, 1, 0, 704, 100
29389, V, 1, 1, 1, 1, 0, 704, 100
29390, V, 1, 1, 1, 1, 0, 704, 100
29391, V, 1, 1, 1, 1, 0, 704, 100
29392, V, 1, 1, 1, 1, 0, 704, 100
29393, V, 1, 1, 1, 1, 0, 704, 100
29394, V, 1, 1, 1, 1, 0, 704, 100
29395, V, 1, 1, 1, 1, 0, 704, 100
29396, V, 1, 1, 1, 1, 0, 704, 100
29398, V, 1, 1, 1, 1, 0, 704, 100
29399, V, 1, 1, 1, 1, 0, 704, 100
29400, V, 1, 1, 1, 1, 0, 704, 100
29401, V, 1, 1, 1, 1, 0, 704, 100
29402, V, 1, 1, 1, 1, 0, 704, 100
29403, V, 1, 1, 1, 1, 0, 704, 100
29404, V, 1, 1, 1, 1, 0, 704, 100
29405, V, 1, 1, 1, 1, 0, 704, 100
29406, V, 1, 1, 1, 1, 0, 704, 100
29407, V, 1, 1, 1, 1, 0, 704, 100
29408, V, 1, 1, 1, 1, 0, 704, 100
29409, V, 1, 1, 1, 1, 0, 704, 100
29410, V, 1, 1, 1, 1, 0, 704, 100
29411, V, 1, 1, 1, 1, 0, 704, 100
29412, V, 1, 1, 1, 1, 0, 704, 100
29413, V, 1, 1, 1, 1, 0, 704, 100
29414, V, 1, 1, 1, 1, 0, 704, 100
29415, V, 1, 1, 1, 1, 0, 704, 100
29416, V, 1, 1, 1, 1, 0, 704, 100
29417, V, 1, 1, 1, 1, 0, 704, 100
29418, V, 1, 1, 1, 1, 0, 704, 100
29419, V, 1, 1, 1, 1, 0, 704, 100
29420, V, 1, 1, 1, 1, 0, 704, 100
29421, V, 1, 1, 1, 1, 0, 704, 100
29422, V, 1, 1, 1, 1, 0, 704, 100
29423, V, 1, 1, 1, 1, 0, 704, 100
29424, V, 1, 1, 1, 1, 0, 704, 100
29425, V, 1, 1, 1, 1, 0, 704, 100
29426, V, 1, 1, 1, 1, 0, 704, 100
29427, V, 1, 1, 1, 1, 0, 704, 100
29428, V, 1, 1, 1, 1, 0, 704, 100
29429, V, 1, 1, 1, 1, 0, 704, 100
29430, V, 1, 1, 1, 1, 0, 704, 100
29431, V, 1, 1, 1, 1, 0, 704, 100
29432, V, 1, 1, 1, 1, 0, 704, 100
29433, V, 1, 1, 1, 1, 0, 704, 100
29434, V, 1, 1, 1, 1, 0, 704, 100
29435, V, 1, 1, 1, 1, 0, 704, 100
29436, V, 1, 1, 1, 1, 0, 704, 100
29437, V, 1, 1, 1, 1, 0, 704, 100
29438, V, 1, 1, 1, 1, 0, 704, 100
29440, V, 1, 1, 1, 1, 0, 704, 100
29441, V, 1, 1, 1, 1, 0, 704, 100
29442, V, 1, 1, 1, 1, 0, 704, 100
29443, V, 1, 1, 1, 1, 0, 704, 100
29444, V, 1, 1, 1, 1, 0, 704, 100
29445, V, 1, 1, 1, 1, 0, 704, 100
29446, V, 1, 1, 1, 1, 0, 704, 100
29447, V, 1, 1, 1, 1, 0, 704, 100
29448, V, 1, 1, 1, 1, 0, 704, 100
29449, V, 1, 1, 1, 1, 0, 704, 100
29450, V, 1, 1, 1, 1, 0, 704, 100
29451, V, 1, 1, 1, 1, 0, 704, 100
29452, V, 1, 1, 1, 1, 0, 704, 100
29453, V, 1, 1, 1, 1, 0, 704, 100
29454, V, 1, 1, 1, 1, 0, 704, 100
29455, V, 1, 1, 1, 1, 0, 704, 100
29456, V, 1, 1, 1, 1, 0, 704, 100
29457, V, 1, 1, 1, 1, 0, 704, 100
29458, V, 1, 1, 1, 1, 0, 704, 100
29459, V, 1, 1, 1, 1, 0, 704, 100
29460, V, 1, 1, 1, 1, 0, 704, 100
29461, V, 1, 1, 1, 1, 0, 704, 100
29462, V, 1, 1, 1, 1, 0, 704, 100
29463, V, 1, 1, 1, 1, 0, 704, 100
29464, V, 1, 1, 1, 1, 0, 704, 100
29465, V, 1, 1, 1, 1, 0, 704, 100
29466, V, 1, 1, 1, 1, 0, 704, 100
29467, V, 1, 1, 1, 1, 0, 704, 100
29468, V, 1, 1, 1, 1, 0, 704, 100
29469, V, 1, 1, 1, 1, 0, 704, 100
29470, V, 1, 1, 1, 1, 0, 704, 100
29471, V, 1, 1, 1, 1, 0, 704, 100
29472, V, 1, 1, 1, 1, 0, 704, 100
29473, V, 1, 1, 1, 1, 0, 704, 100
29474, V, 1, 1, 1, 1, 0, 704, 100
29475, V, 1, 1, 1, 1, 0, 704, 100
29476, V, 1, 1, 1, 1, 0, 704, 100
29477, V, 1, 1, 1, 1, 0, 704, 100
29478, V, 1, 1, 1, 1, 0, 704, 100
29479, V, 1, 1, 1, 1, 0, 704, 100
29480, V, 1, 1, 1, 1, 0, 704, 100
29481, V, 1, 1, 1, 1, 0, 704, 100
29483, V, 1, 1, 1, 1, 0, 704, 100
29484, V, 1, 1, 1, 1, 0, 704, 100
29485, V, 1, 1, 1, 1, 0, 704, 100
29486, V, 1, 1, 1, 1, 0, 704, 100
29487, V, 1, 1, 1, 1, 0, 704, 100
29488, V, 1, 1, 1, 1, 0, 704, 100
29489, V, 1, 1, 1, 1, 0, 704, 100
29490, V, 1, 1, 1, 1, 0, 704, 100
29491, V, 1, 1, 1, 1, 0, 704, 100
29492, V, 1, 1, 1, 1, 0, 704, 100
29493, V, 1, 1, 1, 1, 0, 704, 100
29494, V, 1, 1, 1, 1, 0, 704, 100
29495, V, 1, 1, 1, 1, 0, 704, 100
29496, V, 1, 1, 1, 1, 0, 704, 100
29497, V, 1, 1, 1, 1, 0, 704, 100
29498, V, 1, 1, 1, 1, 0, 704, 100
29499, V, 1, 1, 1, 1, 0, 704, 100
29500, V, 1, 1, 1, 1, 0, 704, 100
29501, V, 1, 1, 1, 1, 0, 704, 100
29502, V, 1, 1, 1, 1, 0, 704, 100
29503, V, 1, 1, 1, 1, 0, 704, 100
29504, V, 1, 1, 1, 1, 0, 704, 100
29505, V, 1, 1, 1, 1, 0, 704, 100
29506, V, 1, 1, 1, 1, 0, 704, 100
29507, V, 1, 1, 1, 1, 0, 704, 100
29508, V, 1, 1, 1, 1, 0, 704, 100
29509, V, 1, 1, 1, 1, 0, 704, 100
29510, V, 1, 1, 1, 1, 0, 704, 100
29511, V, 1, 1, 1, 1, 0, 704, 100
29512, V, 1, 1, 1, 1, 0, 704, 100
29513, V, 1, 1, 1, 1, 0, 704, 100
29514, V, 1, 1, 1, 1, 0, 704, 100
29515, V, 1, 1, 1, 1, 0, 704, 100
29516, V, 1, 1, 1, 1, 0, 704, 100
29517, V, 1, 1, 1, 1, 0, 704, 100
29518, V, 1, 1, 1, 1, 0, 704, 100
29519, V, 1, 1, 1, 1, 0, 704, 100
29520, V, 1, 1, 1, 1, 0, 704, 100
29521, V, 1, 1, 1, 1, 0, 704, 100
29522, V, 1, 1, 1, 1, 0, 704, 100
29523, V, 1, 1, 1, 1, 0, 704, 100
29524, V, 1, 1, 1, 1, 0, 704, 100
29526, V, 1, 1, 1, 1, 0, 704, 100
29527, V, 1, 1, 1, 1, 0, 704, 100
29528, V, 1, 1, 1, 1, 0, 704, 100
29529, V, 1, 1, 1, 1, 0, 704, 100
29530, V, 1, 1, 1, 1, 0, 704, 100
29531, V, 1, 1, 1, 1, 0, 704, 100
29532, V, 1, 1, 1, 1, 0, 704, 100
29533, V, 1, 1, 1, 1, 0, 704, 100
29534, V, 1, 1, 1, 1, 0, 704, 100
29535, V, 1, 1, 1, 1, 0, 704, 100
29536, V, 1, 1, 1, 1, 0, 704, 100
29537, V, 1, 1, 1, 1, 0, 704, 100
29538, V, 1, 1, 1, 1, 0, 704, 100
29539, V, 1, 1, 1, 1, 0, 704, 100
29540, V, 1, 1, 1, 1, 0, 704, 100
29541, V, 1, 1, 1, 1, 0, 704, 100
29542, V, 1, 1, 1, 1, 0, 704, 100
29543, V, 1, 1, 1, 1, 0, 704, 100
29544, V, 1, 1, 1, 1, 0, 704, 100
29545, V, 1, 1, 1, 1, 0, 704, 100
29546, V, 1, 1, 1, 1, 0, 704, 100
29547, V, 1, 1, 1, 1, 0, 704, 100
29548, V, 1, 1, 1, 1, 0, 704, 100
29549, V, 1, 1, 1, 1, 0, 704, 100
29550, V, 1, 1, 1, 1, 0, 704, 100
29551, V, 1, 1, 1, 1, 0, 704, 100
29552, V, 1, 1, 1, 1, 0, 704, 100
29553, V, 1, 1, 1, 1, 0, 704, 100
29554, V, 1, 1, 1, 1, 0, 704, 100
29555, V, 1, 1, 1, 1, 0, 704, 100
29556, V, 1, 1, 1, 1, 0, 704, 100
29557, V, 1, 1, 1, 1, 0, 704, 100
29558, V, 1, 1, 1, 1, 0, 704, 100
29559, V, 1, 1, 1, 1, 0, 704, 100
29560, V, 1, 1, 1, 1, 0, 704, 100
29561, V, 1, 1, 1, 1, 0, 704, 100
29562, V, 1, 1, 1, 1, 0, 704, 100
29563, V, 1, 1, 1, 1, 0, 704, 100
29564, V, 1, 1, 1, 1, 0, 704, 100
29565, V, 1, 1, 1, 1, 0, 704, 100
29566, V, 1, 1, 1, 1, 0, 704, 100
29568, V, 1, 1, 1, 1, 0, 704, 100
29569, V, 1, 1, 1, 1, 0, 704, 100
29570, V, 1, 1, 1, 1, 0, 704, 100
29571, V, 1, 1, 1, 1, 0, 704, 100
29572, V, 1, 1, 1, 1, 0, 704, 100
29573, V, 1, 1, 1, 1, 0, 704, 100
29574, V, 1, 1, 1, 1, 0, 704, 100
29575, V, 1, 1, 1, 1, 0, 704, 100
29576, V, 1, 1, 1, 1, 0, 704, 100
29577, V, 1, 1, 1, 1, 0, 704, 100
29578, V, 1, 1, 1, 1, 0, 704, 100
29579, V, 1, 1, 1, 1, 0, 704, 100
29580, V, 1, 1, 1, 1, 0, 704, 100
29581, V, 1, 1, 1, 1, 0, 704, 100
29582, V, 1, 1, 1, 1, 0, 704, 100
29583, V, 1, 1, 1, 1, 0, 704, 100
29584, V, 1, 1, 1, 1, 0, 704, 100
29585, V, 1, 1, 1, 1, 0, 704, 100
29586, V, 1, 1, 1, 1, 0, 704, 100
29587, V, 1, 1, 1, 1, 0, 704, 100
29588, V, 1, 1, 1, 1, 0, 704, 100
29589, V, 1, 1, 1, 1, 0, 704, 100
29590, V, 1, 1, 1, 1, 0, 704, 100
29591, V, 1, 1, 1, 1, 0, 704, 100
29592, V, 1, 1, 1, 1, 0, 704, 100
29593, V, 1, 1, 1, 1, 0, 704, 100
29594, V, 1, 1, 1, 1, 0, 704, 100
29595, V, 1, 1, 1, 1, 0, 704, 100
29596, V, 1, 1, 1, 1, 0, 704, 100
29597, V, 1, 1, 1, 1, 0, 704, 100
29598, V, 1, 1, 1, 1, 0, 704, 100
29599, V, 1, 1, 1, 1, 0, 704, 100
29600, V, 1, 1, 1, 1, 0, 704, 100
29601, V, 1, 1, 1, 1, 0, 704, 100
29602, V, 1, 1, 1, 1, 0, 704, 100
29603, V, 1, 1, 1, 1, 0, 704, 100
29604, V, 1, 1, 1, 1, 0, 704, 100
29605, V, 1, 1, 1, 1, 0, 704, 100
29606, V, 1, 1, 1, 1, 0, 704, 100
29607, V, 1, 1, 1, 1, 0, 704, 100
29608, V, 1, 1, 1, 1, 0, 704, 100
29609, V, 1, 1, 1, 1, 0, 704, 100
29611, V, 1, 1, 1, 1, 0, 704, 100
29612, V, 1, 1, 1, 1, 0, 704, 100
29613, V, 1, 1, 1, 1, 0, 704, 100
29614, V, 1, 1, 1, 1, 0, 704, 100
29615, V, 1, 1, 1, 1, 0, 704, 100
29616, V, 1, 1, 1, 1, 0, 704, 100
29617, V, 1, 1, 1, 1, 0, 704, 100
29618, V, 1, 1, 1, 1, 0, 704, 100
29619, V, 1, 1, 1, 1, 0, 704, 100
29620, V, 1, 1, 1, 1, 0, 704, 100
29621, V, 1, 1, 1, 1, 0, 704, 100
29622, V, 1, 1, 1, 1, 0, 704, 100
29623, V, 1, 1, 1, 1, 0, 704, 100
29624, V, 1, 1, 1, 1, 0, 704, 100
29625, V, 1, 1, 1, 1, 0, 704, 100
29626, V, 1, 1, 1, 1, 0, 704, 100
29627, V, 1, 1, 1, 1, 0, 704, 100
29628, V, 1, 1, 1, 1, 0, 704, 100
29629, V, 1, 1, 1, 1, 0, 704, 100
29630, V, 1, 1, 1, 1, 0, 704, 100
29631, V, 1, 1, 1, 1, 0, 704, 100
29632, V, 1, 1, 1, 1, 0, 704, 100
29633, V, 1, 1, 1, 1, 0, 704, 100
29634, V, 1, 1, 1, 1, 0, 704, 100
29635, V, 1, 1, 1, 1, 0, 704, 100
29636, V, 1, 1, 1, 1, 0, 704, 100
29637, V, 1, 1, 1, 1, 0, 704, 100
29638, V, 1, 1, 1, 1, 0, 704, 100
29639, V, 1, 0, 0, 1, 0, 704, 100
29639, V, 1, 0, 0, 0, 0, 704, 100
29640, V, 1, 1, 0, 0, 0, 704, 100
29640, V, 1, 1, 0, 0, 0, 704, 100
29641, V, 1, 1, 1, 1, 0, 704, 100
29642, V, 1, 1, 1, 1, 0, 704, 100
29643, V, 1, 1, 1, 1, 0, 704, 100
29644, V, 1, 1, 1, 1, 0, 704, 100
29645, V, 1, 1, 1, 1, 0, 704, 100
29646, V, 1, 1, 1, 1, 0, 704, 100
29647, V, 1, 1, 1, 1, 0, 704, 100
29648, V, 1, 1, 1, 1, 0, 704, 100
29649, V, 1, 1, 1, 1, 0, 704, 100
29650, V, 1, 1, 1, 1, 0, 704, 100
29651, V, 1, 1, 1, 1, 0, 704, 100
29652, V, 1, 1, 1, 1, 0, 704, 100
29654, V, 1, 1, 1, 1, 0, 704, 100
29655, V, 1, 1, 1, 1, 0, 704, 100
29656, V, 1, 1, 1, 1, 0, 704, 100
29657, V, 1, 1, 1, 1, 0, 704, 100
29658, V, 1, 1, 1, 1, 0, 704, 100
29659, V, 1, 1, 1, 1, 0, 704, 100
29660, V, 1, 1, 1, 1, 0, 704, 100
29661, V, 1, 1, 1, 1, 0, 704, 100
29662, V, 1, 1, 1, 1, 0, 704, 100
29663, V, 1, 1, 1, 1, 0, 704, 100
29664, V, 1, 1, 1, 1, 0, 704, 100
29665, V, 1, 1, 1, 1, 0, 704, 100
29666, V, 1, 1, 1, 1, 0, 704, 100
29667, V, 1, 1, 1, 1, 0, 704, 100
29668, V, 1, 1, 1, 1, 0, 704, 100
29669, V, 1, 1, 1, 1, 0, 704, 100
29670, V, 1, 1, 1, 1, 0, 704, 100
29671, V, 1, 1, 1, 1, 0, 704, 100
29672, V, 1, 1, 1, 1, 0, 704, 100
29673, V, 1, 1, 1, 1, 0, 704, 100
29674, V, 1, 1, 1, 1, 0, 704, 100
29675, V, 1, 1, 1, 1, 0, 704, 100
29676, V, 1, 1, 1, 1, 0, 704, 100
29677, V, 1, 1, 1, 1, 0, 704, 100
29678, V, 1, 1, 1, 1, 0, 704, 100
29679, V, 1, 1, 1, 1, 0, 704, 100
29680, V, 1, 1, 1, 1, 0, 704, 100
29681, V, 1, 1, 1, 1, 0, 704, 100
29682, V, 1, 1, 1, 1, 0, 704, 100
29683, V, 1, 1, 1, 1, 0, 704, 100
29684, V, 1, 1, 1, 1, 0, 704, 100
29685, V, 1, 1, 1, 1, 0, 704, 100
29686, V, 1, 1, 1, 1, 0, 704, 100
29687, V, 1, 1, 1, 1, 0, 704, 100
29688, V, 1, 1, 1, 1, 0, 704, 100
29689, V, 1, 1, 1, 1, 0, 704, 100
29690, V, 1, 1, 1, 1, 0, 704, 100
29691, V, 1, 1, 1, 1, 0, 704, 100
29692, V, 1, 1, 1, 1, 0, 704, 100
29693, V, 1, 1, 1, 1, 0, 704, 100
29694, V, 1, 1, 1, 1, 0, 704, 100
29696, V, 1, 1, 1, 1, 0, 704, 100
29697, V, 1, 1, 1, 1, 0, 704, 100
29698, V, 1, 1, 1, 1, 0, 704, 100
29699, V, 1, 1, 1, 1, 0, 704, 100
29700, V, 1, 1, 1, 1, 0, 704, 100
29701, V, 1, 1, 1, 1, 0, 704, 100
29702, V, 1, 1, 1, 1, 0, 704, 100
29703, V, 1, 1, 1, 1, 0, 704, 100
29704, V, 1, 1, 1, 1, 0, 704, 100
29705, V, 1, 1, 1, 1, 0, 704, 100
29706, V, 1, 1, 1, 1, 0, 704, 100
29707, V, 1, 1, 1, 1, 0, 704, 100
29708, V, 1, 1, 1, 1, 0, 704, 100
29709, V, 1, 1, 1, 1, 0, 704, 100
29710, V, 1, 1, 1, 1, 0, 704, 100
29711, V, 1, 1, 1, 1, 0, 704, 100
29712, V, 1, 1, 1, 1, 0, 704, 100
29713, V, 1, 1, 1, 1, 0, 704, 100
29714, V, 1, 1, 1, 1, 0, 704, 100
29715, V, 1, 1, 1, 1, 0, 704, 100
29716, V, 1, 1, 1, 1, 0, 704, 100
29717, V, 1, 1, 1, 1, 0, 704, 100
29718, V, 1, 1, 1, 1, 0, 704, 100
29719, V, 1, 1, 1, 1, 0, 704, 100
29720, V, 1, 1, 1, 1, 0, 704, 100
29721, V, 1, 1, 1, 1, 0, 704, 100
29722, V, 1, 1, 1, 1, 0, 704, 100
29723, V, 1, 1, 1, 1, 0, 704, 100
29724, V, 1, 1, 1, 1, 0, 704, 100
29725, V, 1, 1, 1, 1, 0, 704, 100
29726, V, 1, 1, 1, 1, 0, 704, 100
29727, V, 1, 1, 1, 1, 0, 704, 100
29728, V, 1, 1, 1, 1, 0, 704, 100
29729, V, 1, 1, 1, 1, 0, 704, 100
29730, V, 1, 1, 1, 1, 0, 704, 100
29731, V, 1, 1, 1, 1, 0, 704, 100
29732, V, 1, 1, 1, 1, 0, 704, 100
29733, V, 1, 1, 1, 1, 0, 704, 100
29734, V, 1, 1, 1, 1, 0, 704, 100
29735, V, 1, 1, 1, 1, 0, 704, 100
29736, V, 1, 1, 1, 1, 0, 704, 100
29737, V, 1, 1, 1, 1, 0, 704, 100
29739, V, 1, 1, 1, 1, 0, 704, 100
29740, V, 1, 1, 1, 1, 0, 704, 100
29741, V, 1, 1, 1, 1, 0, 704, 100
29742, V, 1, 1, 1, 1, 0, 704, 100
29743, V, 1, 1, 1, 1, 0, 704, 100
29744, V, 1, 1, 1, 1, 0, 704, 100
29745, V, 1, 1, 1, 1, 0, 704, 100
29746, V, 1, 1, 1, 1, 0, 704, 100
29747, V, 1, 1, 1, 1, 0, 704, 100
29748, V, 1, 1, 1, 1, 0, 704, 100
29749, V, 1, 1, 1, 1, 0, 704, 100
29750, V, 1, 1, 1, 1, 0, 704, 100
29751, V, 1, 1, 1, 1, 0, 704, 100
29752, V, 1, 1, 1, 1, 0, 704, 100
29753, V, 1, 1, 1, 1, 0, 704, 100
29754, V, 1, 1, 1, 1, 0, 704, 100
29755, V, 1, 1, 1, 1, 0, 704, 100
29756, V, 1, 1, 1, 1, 0, 704, 100
29757, V, 1, 1, 1, 1, 0, 704, 100
29758, V, 1, 1, 1, 1, 0, 704, 100
29759, V, 1, 1, 1, 1, 0, 704, 100
29760, V, 1, 1, 1, 1, 0, 704, 100
29761, V, 1, 1, 1, 1, 0, 704, 100
29762, V, 1, 1, 1, 1, 0, 704, 100
29763, V, 1, 1, 1, 1, 0, 704, 100
29764, V, 1, 1, 1, 1, 0, 704, 100
29765, V, 1, 1, 1, 1, 0, 704, 100
29766, V, 1, 1, 1, 1, 0, 704, 100
29767, V, 1, 1, 1, 1, 0, 704, 100
29768, V, 1, 1, 1, 1, 0, 704, 100
29769, V, 1, 1, 1, 1, 0, 704, 100
29770, V, 1, 1, 1, 1, 0, 704, 100
29771, V, 1, 1, 1, 1, 0, 704, 100
29772, V, 1, 1, 1, 1, 0, 704, 100
29773, V, 1, 1, 1, 1, 0, 704, 100
29774, V, 1, 1, 1, 1, 0, 704, 100
29775, V, 1, 1, 1, 1, 0, 704, 100
29776, V, 1, 1, 1, 1, 0, 704, 100
29777, V, 1, 1, 1, 1, 0, 704, 100
29778, V, 1, 1, 1, 1, 0, 704, 100
29779, V, 1, 1, 1, 1, 0, 704, 100
29780, V, 1, 1, 1, 1, 0, 704, 100
29782, V, 1, 1, 1, 1, 0, 704, 100
29783, V, 1, 1, 1, 1, 0, 704, 100
29784, V, 1, 1, 1, 1, 0, 704, 100
29785, V, 1, 1, 1, 1, 0, 704, 100
29786, V, 1, 1, 1, 1, 0, 704, 100
29787, V, 1, 1, 1, 1, 0, 704, 100
29788, V, 1, 1, 1, 1, 0, 704, 100
29789, V, 1, 1, 1, 1, 0, 704, 100
29790, V, 1, 1, 1, 1, 0, 704, 100
29791, V, 1, 1, 1, 1, 0, 704, 100
29792, V, 1, 1, 1, 1, 0, 704, 100
29793, V, 1, 1, 1, 1, 0, 704, 100
29794, V, 1, 1, 1, 1, 0, 704, 100
29795, V, 1, 1, 1, 1, 0, 704, 100
29796, V, 1, 1, 1, 1, 0, 704, 100
29797, V, 1, 1, 1, 1, 0, 704, 100
29798, V, 1, 1, 1, 1, 0, 704, 100
29799, V, 1, 1, 1, 1, 0, 704, 100
29800, V, 1, 1, 1, 1, 0, 704, 100
29801, V, 1, 1, 1, 1, 0, 704, 100
29802, V, 1, 1, 1, 1, 0, 704, 100
29803, V, 1, 1, 1, 1, 0, 704, 100
29804, V, 1, 1, 1, 1, 0, 704, 100
29805, V, 1, 1, 1, 1, 0, 704, 100
29806, V, 1, 1, 1, 1, 0, 704, 100
29807, V, 1, 1, 1, 1, 0, 704, 100
29808, V, 1, 1, 1, 1, 0, 704, 100
29809, V, 1, 1, 1, 1, 0, 704, 100
29810, V, 1, 1, 1, 1, 0, 704, 100
29811, V, 1, 1, 1, 1, 0, 704, 100
29812, V, 1, 1, 1, 1, 0, 704, 100
29813, V, 1, 1, 1, 1, 0, 704, 100
29814, V, 1, 1, 1, 1, 0, 704, 100
29815, V, 1, 1, 1, 1, 0, 704, 100
29816, V, 1, 1, 1, 1, 0, 704, 100
29817, V, 1, 1, 1, 1, 0, 704, 100
29818, V, 1, 1, 1, 1, 0, 704, 100
29819, V, 1, 1, 1, 1, 0, 704, 100
29820, V, 1, 1, 1, 1, 0, 704, 100
29821, V, 1, 1, 1, 1, 0, 704, 100
29822, V, 1, 1, 1, 1, 0, 704, 100
29824, V, 1, 1, 1, 1, 0, 704, 100
29825, V, 1, 1, 1, 1, 0, 704, 100
29826, V, 1, 1, 1, 1, 0, 704, 100
29827, V, 1, 1, 1, 1, 0, 704, 100
29828, V, 1, 1, 1, 1, 0, 704, 100
29829, V, 1, 1, 1, 1, 0, 704, 100
29830, V, 1, 1, 1, 1, 0, 704, 100
29831, V, 1, 1, 1, 1, 0, 704, 100
29832, V, 1, 1, 1, 1, 0, 704, 100
29833, V, 1, 1, 1, 1, 0, 704, 100
29834, V, 1, 1, 1, 1, 0, 704, 100
29835, V, 1, 1, 1, 1, 0, 704, 100
29836, V, 1, 1, 1, 1, 0, 704, 100
29837, V, 1, 1, 1, 1, 0, 704, 100
29838, V, 1, 1, 1, 1, 0, 704, 100
29839, V, 1, 1, 1, 1, 0, 704, 100
29840, V, 1, 1, 1, 1, 0, 704, 100
29841, V, 1, 1, 1, 1, 0, 704, 100
29842, V, 1, 1, 1, 1, 0, 704, 100
29843, V, 1, 1, 1, 1, 0, 704, 100
29844, V, 1, 1, 1, 1, 0, 704, 100
29845, V, 1, 1, 1, 1, 0, 704, 100
29846, V, 1, 1, 1, 1, 0, 704, 100
29847, V, 1, 1, 1, 1, 0, 704, 100
29848, V, 1, 1, 1, 1, 0, 704, 100
29849, V, 1, 1, 1, 1, 0, 704, 100
29850, V, 1, 1, 1, 1, 0, 704, 100
29851, V, 1, 1, 1, 1, 0, 704, 100
29852, V, 1, 1, 1, 1, 0, 704, 100
29853, V, 1, 1, 1, 1, 0, 704, 100
29854, V, 1, 1, 1, 1, 0, 704, 100
29855, V, 1, 1, 1, 1, 0, 704, 100
29856, V, 1, 1, 1, 1, 0, 704, 100
29857, V, 1, 1, 1, 1, 0, 704, 100
29858, V, 1, 1, 1, 1, 0, 704, 100
29859, V, 1, 1, 1, 1, 0, 704, 100
29860, V, 1, 1, 1, 1, 0, 704, 100
29861, V, 1, 1, 1, 1, 0, 704, 100
29862, V, 1, 1, 1, 1, 0, 704, 100
29863, V, 1, 1, 1, 1, 0, 704, 100
29864, V, 1, 1, 1, 1, 0, 704, 100
29865, V, 1, 1, 1, 1, 0, 704, 100
29867, V, 1, 1, 1, 1, 0, 704, 100
29868, V, 1, 1, 1, 1, 0, 704, 100
29869, V, 1, 1, 1, 1, 0, 704, 100
29870, V, 1, 1, 1, 1, 0, 704, 100
29871, V, 1, 1, 1, 1, 0, 704, 100
29872, V, 1, 1, 1, 1, 0, 704, 100
29873, V, 1, 1, 1, 1, 0, 704, 100
29874, V, 1, 1, 1, 1, 0, 704, 100
29875, V, 1, 1, 1, 1, 0, 704, 100
29876, V, 1, 1, 1, 1, 0, 704, 100
29877, V, 1, 1, 1, 1, 0, 704, 100
29878, V, 1, 1, 1, 1, 0, 704, 100
29879, V, 1, 1, 1, 1, 0, 704, 100
29880, V, 1, 1, 1, 1, 0, 704, 100
29881, V, 1, 1, 1, 1, 0, 704, 100
29882, V, 1, 1, 1, 1, 0, 704, 100
29883, V, 1, 1, 1, 1, 0, 704, 100
29884, V, 1, 1, 1, 1, 0, 704, 100
29885, V, 1, 1, 1, 1, 0, 704, 100
29886, V, 1, 1, 1, 1, 0, 704, 100
29887, V, 1, 1, 1, 1, 0, 704, 100
29888, V, 1, 1, 1, 1, 0, 704, 100
29889, V, 1, 1, 1, 1, 0, 704, 100
29890, V, 1, 1, 1, 1, 0, 704, 100
29891, V, 1, 1, 1, 1, 0, 704, 100
29892, V, 1, 1, 1, 1, 0, 704, 100
29893, V, 1, 1, 1, 1, 0, 704, 100
29894, V, 1, 1, 1, 1, 0, 704, 100
29895, V, 1, 1, 1, 1, 0, 704, 100
29896, V, 1, 1, 1, 1, 0, 704, 100
29897, V, 1, 1, 1, 1, 0, 704, 100
29898, V, 1, 1, 1, 1, 0, 704, 100
29899, V, 1, 1, 1, 1, 0, 704, 100
29900, V, 1, 1, 1, 1, 0, 704, 100
29901, V, 1, 1, 1, 1, 0, 704, 100
29902, V, 1, 1, 1, 1, 0, 704, 100
29903, V, 1, 1, 1, 1, 0, 704, 100
29904, V, 1, 1, 1, 1, 0, 704, 100
29905, V, 1, 1, 1, 1, 0, 704, 100
29906, V, 1, 1, 1, 1, 0, 704, 100
29907, V, 1, 1, 1, 1, 0, 704, 100
29908, V, 1, 1, 1, 1, 0, 704, 100
29910, V, 1, 1, 1, 1, 0, 704, 100
29911, V, 1, 1, 1, 1, 0, 704, 100
29912, V, 1, 1, 1, 1, 0, 704, 100
29913, V, 1, 1, 1, 1, 0, 704, 100
29914, V, 1, 1, 1, 1, 0, 704, 100
29915, V, 1, 1, 1, 1, 0, 704, 100
29916, V, 1, 1, 1, 1, 0, 704, 100
29917, V, 1, 1, 1, 1, 0, 704, 100
29918, V, 1, 1, 1, 1, 0, 704, 100
29919, V, 1, 1, 1, 1, 0, 704, 100
29920, V, 1, 1, 1, 1, 0, 704, 100
29921, V, 1, 1, 1, 1, 0, 704, 100
29922, V, 1, 1, 1, 1, 0, 704, 100
29923, V, 1, 1, 1, 1, 0, 704, 100
29924, V, 1, 1, 1, 1, 0, 704, 100
29925, V, 1, 1, 1, 1, 0, 704, 100
29926, V, 1, 1, 1, 1, 0, 704, 100
29927, V, 1, 1, 1, 1, 0, 704, 100
29928, V, 1, 1, 1, 1, 0, 704, 100
29929, V, 1, 1, 1, 1, 0, 704, 100
29930, V, 1, 1, 1, 1, 0, 704, 100
29931, V, 1, 1, 1, 1, 0, 704, 100
29932, V, 1, 1, 1, 1, 0, 704, 100
29933, V, 1, 1, 1, 1, 0, 704, 100
29934, V, 1, 1, 1, 1, 0, 704, 100
29935, V, 1, 1, 1, 1, 0, 704, 100
29936, V, 1, 1, 1, 1, 0, 704, 100
29937, V, 1, 1, 1, 1, 0, 704, 100
29938, V, 1, 1, 1, 1, 0, 704, 100
29939, V, 1, 1, 1, 1, 0, 704, 100
29940, V, 1, 1, 1, 1, 0, 704, 100
29941, V, 1, 1, 1, 1, 0, 704, 100
29942, V, 1, 1, 1, 1, 0, 704, 100
29943, V, 1, 1, 1, 1, 0, 704, 100
29944, V, 1, 1, 1, 1, 0, 704, 100
29945, V, 1, 1, 1, 1, 0, 704, 100
29946, V, 1, 1, 1, 1, 0, 704, 100
29947, V, 1, 1, 1, 1, 0, 704, 100
29948, V, 1, 1, 1, 1, 0, 704, 100
29949, V, 1, 1, 1, 1, 0, 704, 100
29950, V, 1, 1, 1, 1, 0, 704, 100
29952, V, 1, 1, 1, 1, 0, 704, 100
29953, V, 1, 1, 1, 1, 0, 704, 100
29954, V, 1, 1, 1, 1, 0, 704, 100
29955, V, 1, 1, 1, 1, 0, 704, 100
29956, V, 1, 1, 1, 1, 0, 704, 100
29957, V, 1, 1, 1, 1, 0, 704, 100
29958, V, 1, 1, 1, 1, 0, 704, 100
29959, V, 1, 1, 1, 1, 0, 704, 100
29960, V, 1, 1, 1, 1, 0, 704, 100
29961, V, 1, 1, 1, 1, 0, 704, 100
29962, V, 1, 1, 1, 1, 0, 704, 100
29963, V, 1, 1, 1, 1, 0, 704, 100
29964, V, 1, 1, 1, 1, 0, 704, 100
29965, V, 1, 1, 1, 1, 0, 704, 100
29966, V, 1, 1, 1, 1, 0, 704, 100
29967, V, 1, 1, 1, 1, 0, 704, 100
29968, V, 1, 1, 1, 1, 0, 704, 100
29969, V, 1, 1, 1, 1, 0, 704, 100
29970, V, 1, 1, 1, 1, 0, 704, 100
29971, V, 1, 1, 1, 1, 0, 704, 100
29972, V, 1, 1, 1, 1, 0, 704, 100
29973, V, 1, 1, 1, 1, 0, 704, 100
29974, V, 1, 1, 1, 1, 0, 704, 100
29975, V, 1, 1, 1, 1, 0, 704, 100
29976, V, 1, 1, 1, 1, 0, 704, 100
29977, V, 1, 1, 1, 1, 0, 704, 100
29978, V, 1, 1, 1, 1, 0, 704, 100
29979, V, 1, 1, 1, 1, 0, 704, 100
29980, V, 1, 1, 1, 1, 0, 704, 100
29981, V, 1, 1, 1, 1, 0, 704, 100
29982, V, 1, 1, 1, 1, 0, 704, 100
29983, V, 1, 1, 1, 1, 0, 704, 100
29984, V, 1, 1, 1, 1, 0, 704, 100
29985, V, 1, 1, 1, 1, 0, 704, 100
29986, V, 1, 1, 1, 1, 0, 704, 100
29987, V, 1, 1, 1, 1, 0, 704, 100
29988, V, 1, 1, 1, 1, 0, 704, 100
29989, V, 1, 1, 1, 1, 0, 704, 100
29990, V, 1, 1, 1, 1, 0, 704, 100
29991, V, 1, 1, 1, 1, 0, 704, 100
29992, V, 1, 1, 1, 1, 0, 704, 100
29993, V, 1, 1, 1, 1, 0, 704, 100
29995, V, 1, 1, 1, 1, 0, 704, 100
29996, V, 1, 1, 1, 1, 0, 704, 100
29997, V, 1, 1, 1, 1, 0, 704, 100
29998, V, 1, 1, 1, 1, 0, 704, 100
29999, V, 1, 1, 1, 1, 0, 704, 100
30000, V, 1, 1, 1, 1, 0, 704, 100
30001, V, 1, 1, 1, 1, 0, 704, 100
30002, V, 1, 1, 1, 1, 0, 704, 100
30003, V, 1, 1, 1, 1, 0, 704, 100
30004, V, 1, 1, 1, 1, 0, 704, 100
30005, V, 1, 1, 1, 1, 0, 704, 100
30006, V, 1, 1, 1, 1, 0, 704, 100
30007, V, 1, 1, 1, 1, 0, 704, 100
30008, V, 1, 1, 1, 1, 0, 704, 100
30009, V, 1, 1, 1, 1, 0, 704, 100
30010, V, 1, 1, 1, 1, 0, 704, 100
30011, V, 1, 1, 1, 1, 0, 704, 100
30012, V, 1, 1, 1, 1, 0, 704, 100
30013, V, 1, 1, 1, 1, 0, 704, 100
30014, V, 1, 1, 1, 1, 0, 704, 100
30015, V, 1, 1, 1, 1, 0, 704, 100
30016, V, 1, 1, 1, 1, 0, 704, 100
30017, V, 1, 1, 1, 1, 0, 704, 100
30018, V, 1, 1, 1, 1, 0, 704, 100
30019, V, 1, 1, 1, 1, 0, 704, 100
30020, V, 1, 1, 1, 1, 0, 704, 100
30021, V, 1, 1, 1, 1, 0, 704, 100
30022, V, 1, 1, 1, 1, 0, 704, 100
30023, V, 1, 1, 1, 1, 0, 704, 100
30024, V, 1, 1, 1, 1, 0, 704, 100
30025, V, 1, 1, 1, 1, 0, 704, 100
30026, V, 1, 1, 1, 1, 0, 704, 100
30027, V, 1, 1, 1, 1, 0, 704, 100
30028, V, 1, 1, 1, 1, 0, 704, 100
30029, V, 1, 1, 1, 1, 0, 704, 100
30030, V, 1, 1, 1, 1, 0, 704, 100
30031, V, 1, 1, 1, 1, 0, 704, 100
30032, V, 1, 1, 1, 1, 0, 704, 100
30033, V, 1, 1, 1, 1, 0, 704, 100
30034, V, 1, 1, 1, 1, 0, 704, 100
30035, V, 1, 1, 1, 1, 0, 704, 100
30036, V, 1, 1, 1, 1, 0, 704, 100
30038, V, 1, 1, 1, 1, 0, 704, 100
30039, V, 1, 1, 1, 1, 0, 704, 100
30040, V, 1, 1, 1, 1, 0, 704, 100
30041, V, 1, 1, 1, 1, 0, 704, 100
30042, V, 1, 1, 1, 1, 0, 704, 100
30043, V, 1, 1, 1, 1, 0, 704, 100
30044, V, 1, 1, 1, 1, 0, 704, 100
30045, V, 1, 1, 1, 1, 0, 704, 100
30046, V, 1, 1, 1, 1, 0, 704, 100
30047, V, 1, 1, 1, 1, 0, 704, 100
30048, V, 1, 1, 1, 1, 0, 704, 100
30049, V, 1, 1, 1, 1, 0, 704, 100
30050, V, 1, 1, 1, 1, 0, 704, 100
30051, V, 1, 1, 1, 1, 0, 704, 100
30052, V, 1, 1, 1, 1, 0, 704, 100
30053, V, 1, 1, 1, 1, 0, 704, 100
30054, V, 1, 1, 1, 1, 0, 704, 100
30055, V, 1, 1, 1, 1, 0, 704, 100
30056, V, 1, 1, 1, 1, 0, 704, 100
30057, V, 1, 1, 1, 1, 0, 704, 100
30058, V, 1, 1, 1, 1, 0, 704, 100
30059, V, 1, 1, 1, 1, 0, 704, 100
30060, V, 1, 1, 1, 1, 0, 704, 100
30061, V, 1, 1, 1, 1, 0, 704, 100
30062, V, 1, 1, 1, 1, 0, 704, 100
30063, V, 1, 1, 1, 1, 0, 704, 100
30064, V, 1, 1, 1, 1, 0, 704, 100
30065, V, 1, 1, 1, 1, 0, 704, 100
30066, V, 1, 1, 1, 1, 0, 704, 100
30067, V, 1, 1, 1, 1, 0, 704, 100
30068, V, 1, 1, 1, 1, 0, 704, 100
30069, V, 1, 1, 1, 1, 0, 704, 100
30070, V, 1, 1, 1, 1, 0, 704, 100
30071, V, 1, 1, 1, 1, 0, 704, 100
30072, V, 1, 1, 1, 1, 0, 704, 100
30073, V, 1, 1, 1, 1, 0, 704, 100
30074, V, 1, 1, 1, 1, 0, 704, 100
30075, V, 1, 1, 1, 1, 0, 704, 100
30076, V, 1, 1, 1, 1, 0, 704, 100
30077, V, 1, 1, 1, 1, 0, 704, 100
30078, V, 1, 1, 1, 1, 0, 704, 100
30080, V, 1, 1, 1, 1, 0, 704, 100
30081, V, 1, 1, 1, 1, 0, 704, 100
30082, V, 1, 1, 1, 1, 0, 704, 100
30083, V, 1, 1, 1, 1, 0, 704, 100
30084, V, 1, 1, 1, 1, 0, 704, 100
30085, V, 1, 1, 1, 1, 0, 704, 100
30086, V, 1, 1, 1, 1, 0, 704, 100
30087, V, 1, 1, 1, 1, 0, 704, 100
30088, V, 1, 1, 1, 1, 0, 704, 100
30089, V, 1, 1, 1, 1, 0, 704, 100
30090, V, 1, 1, 1, 1, 0, 704, 100
30091, V, 1, 1, 1, 1, 0, 704, 100
30092, V, 1, 1, 1, 1, 0, 704, 100
30093, V, 1, 1, 1, 1, 0, 704, 100
30094, V, 1, 1, 1, 1, 0, 704, 100
30095, V, 1, 1, 1, 1, 0, 704, 100
30096, V, 1, 1, 1, 1, 0, 704, 100
30097, V, 1, 1, 1, 1, 0, 704, 100
30098, V, 1, 1, 1, 1, 0, 704, 100
30099, V, 1, 1, 1, 1, 0, 704, 100
30100, V, 1, 1, 1, 1, 0, 704, 100
30101, V, 1, 1, 1, 1, 0, 704, 100
30102, V, 1, 1, 1, 1, 0, 704, 100
30103, V, 1, 1, 1, 1, 0, 704, 100
30104, V, 1, 1, 1, 1, 0, 704, 100
30105, V, 1, 1, 1, 1, 0, 704, 100
30106, V, 1, 1, 1, 1, 0, 704, 100
30107, V, 1, 1, 1, 1, 0, 704, 100
30108, V, 1, 1, 1, 1, 0, 704, 100
30109, V, 1, 1, 1, 1, 0, 704, 100
30110, V, 1, 1, 1, 1, 0, 704, 100
30111, V, 1, 1, 1, 1, 0, 704, 100
30112, V, 1, 1, 1, 1, 0, 704, 100
30113, V, 1, 1, 1, 1, 0, 704, 100
30114, V, 1, 1, 1, 1, 0, 704, 100
30115, V, 1, 1, 1, 1, 0, 704, 100
30116, V, 1, 1, 1, 1, 0, 704, 100
30117, V, 1, 1, 1, 1, 0, 704, 100
30118, V, 1, 1, 1, 1, 0, 704, 100
30119, V, 1, 1, 1, 1, 0, 704, 100
30120, V, 1, 1, 1, 1, 0, 704, 100
30121, V, 1, 1, 1, 1, 0, 704, 100
30123, V, 1, 1, 1, 1, 0, 704, 100
30124, V, 1, 1, 1, 1, 0, 704, 100
30125, V, 1, 1, 1, 1, 0, 704, 100
30126, V, 1, 1, 1, 1, 0, 704, 100
30127, V, 1, 1, 1, 1, 0, 704, 100
30128, V, 1, 1, 1, 1, 0, 704, 100
30129, V, 1, 1, 1, 1, 0, 704, 100
30130, V, 1, 1, 1, 1, 0, 704, 100
30131, V, 1, 1, 1, 1, 0, 704, 100
30132, V, 1, 1, 1, 1, 0, 704, 100
30133, V, 1, 1, 1, 1, 0, 704, 100
30134, V, 1, 1, 1, 1, 0, 704, 100
30135, V, 1, 1, 1, 1, 0, 704, 100
30136, V, 1, 1, 1, 1, 0, 704, 100
30137, V, 1, 1, 1, 1, 0, 704, 100
30138, V, 1, 1, 1, 1, 0, 704, 100
30139, V, 1, 1, 1, 1, 0, 704, 100
30140, V, 1, 1, 1, 1, 0, 704, 100
30141, V, 1, 1, 1, 1, 0, 704, 100
30142, V, 1, 1, 1, 1, 0, 704, 100
30143, V, 1, 1, 1, 1, 0, 704, 100
30144, V, 1, 1, 1, 1, 0, 704, 100
30145, V, 1, 1, 1, 1, 0, 704, 100
30146, V, 1, 1, 1, 1, 0, 704, 100
30147, V, 1, 1, 1, 1, 0, 704, 100
30148, V, 1, 1, 1, 1, 0, 704, 100
30149, V, 1, 1, 1, 1, 0, 704, 100
30150, V, 1, 1, 1, 1, 0, 704, 100
30151, V, 1, 1, 1, 1, 0, 704, 100
30152, V, 1, 1, 1, 1, 0, 704, 100
30153, V, 1, 1, 1, 1, 0, 704, 100
30154, V, 1, 1, 1, 1, 0, 704, 100
30155, V, 1, 1, 1, 1, 0, 704, 100
30156, V, 1, 1, 1, 1, 0, 704, 100
30157, V, 1, 1, 1, 1, 0, 704, 100
30158, V, 1, 1, 1, 1, 0, 704, 100
30159, V, 1, 1, 1, 1, 0, 704, 100
30160, V, 1, 1, 1, 1, 0, 704, 100
30161, V, 1, 1, 1, 1, 0, 704, 100
30162, V, 1, 1, 1, 1, 0, 704, 100
30163, V, 1, 1, 1, 1, 0, 704, 100
30164, V, 1, 1, 1, 1, 0, 704, 100
30166, V, 1, 1, 1, 1, 0, 704, 100
30167, V, 1, 1, 1, 1, 0, 704, 100
30168, V, 1, 1, 1, 1, 0, 704, 100
30169, V, 1, 1, 1, 1, 0, 704, 100
30170, V, 1, 1, 1, 1, 0, 704, 100
30171, V, 1, 1, 1, 1, 0, 704, 100
30172, V, 1, 1, 1, 1, 0, 704, 100
30173, V, 1, 1, 1, 1, 0, 704, 100
30174, V, 1, 1, 1, 1, 0, 704, 100
30175, V, 1, 1, 1, 1, 0, 704, 100
30176, V, 1, 1, 1, 1, 0, 704, 100
30177, V, 1, 1, 1, 1, 0, 704, 100
30178, V, 1, 1, 1, 1, 0, 704, 100
30179, V, 1, 1, 1, 1, 0, 704, 100
30180, V, 1, 1, 1, 1, 0, 704, 100
30181, V, 1, 1, 1, 1, 0, 704, 100
30182, V, 1, 1, 1, 1, 0, 704, 100
30183, V, 1, 1, 1, 1, 0, 704, 100
30184, V, 1, 1, 1, 1, 0, 704, 100
30185, V, 1, 1, 1, 1, 0, 704, 100
30186, V, 1, 1, 1, 1, 0, 704, 100
30187, V, 1, 1, 1, 1, 0, 704, 100
30188, V, 1, 1, 1, 1, 0, 704, 100
30189, V, 1, 1, 1, 1, 0, 704, 100
30190, V, 1, 1, 1, 1, 0, 704, 100
30191, V, 1, 1, 1, 1, 0, 704, 100
30192, V, 1, 1, 1, 1, 0, 704, 100
30193, V, 1, 1, 1, 1, 0, 704, 100
30194, V, 1, 1, 1, 1, 0, 704, 100
30195, V, 1, 1, 1, 1, 0, 704, 100
30196, V, 1, 1, 1, 1, 0, 704, 100
30197, V, 1, 1, 1, 1, 0, 704, 100
30198, V, 1, 1, 1, 1, 0, 704, 100
30199, V, 1, 1, 1, 1, 0, 704, 100
30200, V, 1, 1, 1, 1, 0, 704, 100
30201, V, 1, 1, 1, 1, 0, 704, 100
30202, V, 1, 1, 1, 1, 0, 704, 100
30203, V, 1, 1, 1, 1, 0, 704, 100
30204, V, 1, 1, 1, 1, 0, 704, 100
30205, V, 1, 1, 1, 1, 0, 704, 100
30206, V, 1, 1, 1, 1, 0, 704, 100
30208, V, 1, 1, 1, 1, 0, 704, 100
30209, V, 1, 1, 1, 1, 0, 704, 100
30210, V, 1, 1, 1, 1, 0, 704, 100
30211, V, 1, 1, 1, 1, 0, 704, 100
30212, V, 1, 1, 1, 1, 0, 704, 100
30213, V, 1, 1, 1, 1, 0, 704, 100
30214, V, 1, 1, 1, 1, 0, 704, 100
30215, V, 1, 1, 1, 1, 0, 704, 100
30216, V, 1, 1, 1, 1, 0, 704, 100
30217, V, 1, 1, 1, 1, 0, 704, 100
30218, V, 1, 1, 1, 1, 0, 704, 100
30219, V, 1, 1, 1, 1, 0, 704, 100
30220, V, 1, 1, 1, 1, 0, 704, 100
30221, V, 1, 1, 1, 1, 0, 704, 100
30222, V, 1, 1, 1, 1, 0, 704, 100
30223, V, 1, 1, 1, 1, 0, 704, 100
30224, V, 1, 1, 1, 1, 0, 704, 100
30225, V, 1, 1, 1, 1, 0, 704, 100
30226, V, 1, 1, 1, 1, 0, 704, 100
30227, V, 1, 1, 1, 1, 0, 704, 100
30228, V, 1, 1, 1, 1, 0, 704, 100
30229, V, 1, 1, 1, 1, 0, 704, 100
30230, V, 1, 1, 1, 1, 0, 704, 100
30231, V, 1, 1, 1, 1, 0, 704, 100
30232, V, 1, 1, 1, 1, 0, 704, 100
30233, V, 1, 1, 1, 1, 0, 704, 100
30234, V, 1, 1, 1, 1, 0, 704, 100
30235, V, 1, 1, 1, 1, 0, 704, 100
30236, V, 1, 1, 1, 1, 0, 704, 100
30237, V, 1, 1, 1, 1, 0, 704, 100
30238, V, 1, 1, 1, 1, 0, 704, 100
30239, V, 1, 1, 1, 1, 0, 704, 100
30240, V, 1, 1, 1, 1, 0, 704, 100
30241, V, 1, 1, 1, 1, 0, 704, 100
30242, V, 1, 1, 1, 1, 0, 704, 100
30243, V, 1, 1, 1, 1, 0, 704, 100
30244, V, 1, 1, 1, 1, 0, 704, 100
30245, V, 1, 1, 1, 1, 0, 704, 100
30246, V, 1, 1, 1, 1, 0, 704, 100
30247, V, 1, 1, 1, 1, 0, 704, 100
30248, V, 1, 1, 1, 1, 0, 704, 100
30249, V, 1, 1, 1, 1, 0, 704, 100
30251, V, 1, 1, 1, 1, 0, 704, 100
30252, V, 1, 1, 1, 1, 0, 704, 100
30253, V, 1, 1, 1, 1, 0, 704, 100
30254, V, 1, 1, 1, 1, 0, 704, 100
30255, V, 1, 1, 1, 1, 0, 704, 100
30256, V, 1, 1, 1, 1, 0, 704, 100
30257, V, 1, 1, 1, 1, 0, 704, 100
30258, V, 1, 1, 1, 1, 0, 704, 100
30259, V, 1, 1, 1, 1, 0, 704, 100
30260, V, 1, 1, 1, 1, 0, 704, 100
30261, V, 1, 1, 1, 1, 0, 704, 100
30262, V, 1, 1, 1, 1, 0, 704, 100
30263, V, 1, 1, 1, 1, 0, 704, 100
30264, V, 1, 1, 1, 1, 0, 704, 100
30265, V, 1, 1, 1, 1, 0, 704, 100
30266, V, 1, 1, 1, 1, 0, 704, 100
30267, V, 1, 1, 1, 1, 0, 704, 100
30268, V, 1, 1, 1, 1, 0, 704, 100
30269, V, 1, 1, 1, 1, 0, 704, 100
30270, V, 1, 1, 1, 1, 0, 704, 100
30271, V, 1, 1, 1, 1, 0, 704, 100
30272, V, 1, 1, 1, 1, 0, 704, 100
30273, V, 1, 1, 1, 1, 0, 704, 100
30274, V, 1, 1, 1, 1, 0, 704, 100
30275, V, 1, 1, 1, 1, 0, 704, 100
30276, V, 1, 1, 1, 1, 0, 704, 100
30277, V, 1, 1, 1, 1, 0, 704, 100
30278, V, 1, 1, 1, 1, 0, 704, 100
30279, V, 1, 1, 1, 1, 0, 704, 100
30280, V, 1, 1, 1, 1, 0, 704, 100
30281, V, 1, 1, 1, 1, 0, 704, 100
30282, V, 1, 1, 1, 1, 0, 704, 100
30283, V, 1, 1, 1, 1, 0, 704, 100
30284, V, 1, 1, 1, 1, 0, 704, 100
30285, V, 1, 1, 1, 1, 0, 704, 100
30286, V, 1, 1, 1, 1, 0, 704, 100
30287, V, 1, 1, 1, 1, 0, 704, 100
30288, V, 1, 1, 1, 1, 0, 704, 100
30289, V, 1, 1, 1, 1, 0, 704, 100
30290, V, 1, 1, 1, 1, 0, 704, 100
30291, V, 1, 1, 1, 1, 0, 704, 100
30292, V, 1, 1, 1, 1, 0, 704, 100
30294, V, 1, 1, 1, 1, 0, 704, 100
30295, V, 1, 1, 1, 1, 0, 704, 100
30296, V, 1, 1, 1, 1, 0, 704, 100
30297, V, 1, 1, 1, 1, 0, 704, 100
30298, V, 1, 1, 1, 1, 0, 704, 100
30299, V, 1, 1, 1, 1, 0, 704, 100
30300, V, 1, 1, 1, 1, 0, 704, 100
30301, V, 1, 1, 1, 1, 0, 704, 100
30302, V, 1, 1, 1, 1, 0, 704, 100
30303, V, 1, 1, 1, 1, 0, 704, 100
30304, V, 1, 1, 1, 1, 0, 704, 100
30305, V, 1, 1, 1, 1, 0, 704, 100
30306, V, 1, 1, 1, 1, 0, 704, 100
30307, V, 1, 1, 1, 1, 0, 704, 100
30308, V, 1, 1, 1, 1, 0, 704, 100
30309, V, 1, 1, 1, 1, 0, 704, 100
30310, V, 1, 1, 1, 1, 0, 704, 100
30311, V, 1, 1, 1, 1, 0, 704, 100
30312, V, 1, 1, 1, 1, 0, 704, 100
30313, V, 1, 1, 1, 1, 0, 704, 100
30314, V, 1, 1, 1, 1, 0, 704, 100
30315, V, 1, 1, 1, 1, 0, 704, 100
30316, V, 1, 1, 1, 1, 0, 704, 100
30317, V, 1, 1, 1, 1, 0, 704, 100
30318, V, 1, 1, 1, 1, 0, 704, 100
30319, V, 1, 1, 1, 1, 0, 704, 100
30320, V, 1, 1, 1, 1, 0, 704, 100
30321, V, 1, 1, 1, 1, 0, 704, 100
30322, V, 1, 1, 1, 1, 0, 704, 100
30323, V, 1, 1, 1, 1, 0, 704, 100
30324, V, 1, 1, 1, 1, 0, 704, 100
30325, V, 1, 1, 1, 1, 0, 704, 100
30326, V, 1, 1, 1, 1, 0, 704, 100
30327, V, 1, 1, 1, 1, 0, 704, 100
30328, V, 1, 1, 1, 1, 0, 704, 100
30329, V, 1, 1, 1, 1, 0, 704, 100
30330, V, 1, 1, 1, 1, 0, 704, 100
30331, V, 1, 1, 1, 1, 0, 704, 100
30332, V, 1, 1, 1, 1, 0, 704, 100
30333, V, 1, 1, 1, 1, 0, 704, 100
30334, V, 1, 1, 1, 1, 0, 704, 100
30336, V, 1, 1, 1, 1, 0, 704, 100
30337, V, 1, 1, 1, 1, 0, 704, 100
30338, V, 1, 1, 1, 1, 0, 704, 100
30339, V, 1, 1, 1, 1, 0, 704, 100
30340, V, 1, 1, 1, 1, 0, 704, 100
30341, V, 1, 1, 1, 1, 0, 704, 100
30342, V, 1, 1, 1, 1, 0, 704, 100
30343, V, 1, 1, 1, 1, 0, 704, 100
30344, V, 1, 1, 1, 1, 0, 704, 100
30345, V, 1, 1, 1, 1, 0, 704, 100
30346, V, 1, 1, 1, 1, 0, 704, 100
30347, V, 1, 1, 1, 1, 0, 704, 100
30348, V, 1, 1, 1, 1, 0, 704, 100
30349, V, 1, 1, 1, 1, 0, 704, 100
30350, V, 1, 1, 1, 1, 0, 704, 100
30351, V, 1, 1, 1, 1, 0, 704, 100
30352, V, 1, 1, 1, 1, 0, 704, 100
30353, V, 1, 1, 1, 1, 0, 704, 100
30354, V, 1, 1, 1, 1, 0, 704, 100
30355, V, 1, 1, 1, 1, 0, 704, 100
30356, V, 1, 1, 1, 1, 0, 704, 100
30357, V, 1, 1, 1, 1, 0, 704, 100
30358, V, 1, 1, 1, 1, 0, 704, 100
30359, V, 1, 1, 1, 1, 0, 704, 100
30360, V, 1, 1, 1, 1, 0, 704, 100
30361, V, 1, 1, 1, 1, 0, 704, 100
30362, V, 1, 1, 1, 1, 0, 704, 100
30363, V, 1, 1, 1, 1, 0, 704, 100
30364, V, 1, 1, 1, 1, 0, 704, 100
30365, V, 1, 1, 1, 1, 0, 704, 100
30366, V, 1, 1, 1, 1, 0, 704, 100
30367, V, 1, 1, 1, 1, 0, 704, 100
30368, V, 1, 1, 1, 1, 0, 704, 100
30369, V, 1, 1, 1, 1, 0, 704, 100
30370, V, 1, 1, 1, 1, 0, 704, 100
30371, V, 1, 1, 1, 1, 0, 704, 100
30372, V, 1, 1, 1, 1, 0, 704, 100
30373, V, 1, 1, 1, 1, 0, 704, 100
30374, V, 1, 1, 1, 1, 0, 704, 100
30375, V, 1, 1, 1, 1, 0, 704, 100
30376, V, 1, 1, 1, 1, 0, 704, 100
30377, V, 1, 1, 1, 1, 0, 704, 100
30379, V, 1, 1, 1, 1, 0, 704, 100
30380, V, 1, 1, 1, 1, 0, 704, 100
30381, V, 1, 1, 1, 1, 0, 704, 100
30382, V, 1, 1, 1, 1, 0, 704, 100
30383, V, 1, 1, 1, 1, 0, 704, 100
30384, V, 1, 1, 1, 1, 0, 704, 100
30385, V, 1, 1, 1, 1, 0, 704, 100
30386, V, 1, 1, 1, 1, 0, 704, 100
30387, V, 1, 1, 1, 1, 0, 704, 100
30388, V, 1, 1, 1, 1, 0, 704, 100
30389, V, 1, 1, 1, 1, 0, 704, 100
30390, V, 1, 1, 1, 1, 0, 704, 100
30391, V, 1, 1, 1, 1, 0, 704, 100
30392, V, 1, 1, 1, 1, 0, 704, 100
30393, V, 1, 1, 1, 1, 0, 704, 100
30394, V, 1, 1, 1, 1, 0, 704, 100
30395, V, 1, 1, 1, 1, 0, 704, 100
30396, V, 1, 1, 1, 1, 0, 704, 100
30397, V, 1, 1, 1, 1, 0, 704, 100
30398, V, 1, 1, 1, 1, 0, 704, 100
30399, V, 1, 1, 1, 1, 0, 704, 100
30400, V, 1, 1, 1, 1, 0, 704, 100
30401, V, 1, 1, 1, 1, 0, 704, 100
30402, V, 1, 1, 1, 1, 0, 704, 100
30403, V, 1, 1, 1, 1, 0, 704, 100
30404, V, 1, 1, 1, 1, 0, 704, 100
30405, V, 1, 1, 1, 1, 0, 704, 100
30406, V, 1, 1, 1, 1, 0, 704, 100
30407, V, 1, 1, 1, 1, 0, 704, 100
30408, V, 1, 1, 1, 1, 0, 704, 100
30409, V, 1, 1, 1, 1, 0, 704, 100
30410, V, 1, 1, 1, 1, 0, 704, 100
30411, V, 1, 1, 1, 1, 0, 704, 100
30412, V, 1, 1, 1, 1, 0, 704, 100
30413, V, 1, 1, 1, 1, 0, 704, 100
30414, V, 1, 1, 1, 1, 0, 704, 100
30415, V, 1, 1, 1, 1, 0, 704, 100
30416, V, 1, 1, 1, 1, 0, 704, 100
30417, V, 1, 1, 1, 1, 0, 704, 100
30418, V, 1, 1, 1, 1, 0, 704, 100
30419, V, 1, 1, 1, 1, 0, 704, 100
30420, V, 1, 1, 1, 1, 0, 704, 100
30422, V, 1, 1, 1, 1, 0, 704, 100
30423, V, 1, 1, 1, 1, 0, 704, 100
30424, V, 1, 1, 1, 1, 0, 704, 100
30425, V, 1, 1, 1, 1, 0, 704, 100
30426, V, 1, 1, 1, 1, 0, 704, 100
30427, V, 1, 1, 1, 1, 0, 704, 100
30428, V, 1, 1, 1, 1, 0, 704, 100
30429, V, 1, 1, 1, 1, 0, 704, 100
30430, V, 1, 1, 1, 1, 0, 704, 100
30431, V, 1, 1, 1, 1, 0, 704, 100
30432, V, 1, 1, 1, 1, 0, 704, 100
30433, V, 1, 1, 1, 1, 0, 704, 100
30434, V, 1, 1, 1, 1, 0, 704, 100
30435, V, 1, 1, 1, 1, 0, 704, 100
30436, V, 1, 1, 1, 1, 0, 704, 100
30437, V, 1, 1, 1, 1, 0, 704, 100
30438, V, 1, 1, 1, 1, 0, 704, 100
30439, V, 1, 1, 1, 1, 0, 704, 100
30440, V, 1, 1, 1, 1, 0, 704, 100
30441, V, 1, 1, 1, 1, 0, 704, 100
30442, V, 1, 1, 1, 1, 0, 704, 100
30443, V, 1, 1, 1, 1, 0, 704, 100
30444, V, 1, 1, 1, 1, 0, 704, 100
30445, V, 1, 1, 1, 1, 0, 704, 100
30446, V, 1, 1, 1, 1, 0, 704, 100
30447, V, 1, 1, 1, 1, 0, 704, 100
30448, V, 1, 1, 1, 1, 0, 704, 100
30449, V, 1, 1, 1, 1, 0, 704, 100
30450, V, 1, 1, 1, 1, 0, 704, 100
30451, V, 1, 1, 1, 1, 0, 704, 100
30452, V, 1, 1, 1, 1, 0, 704, 100
30453, V, 1, 1, 1, 1, 0, 704, 100
30454, V, 1, 1, 1, 1, 0, 704, 100
30455, V, 1, 1, 1, 1, 0, 704, 100
30456, V, 1, 1, 1, 1, 0, 704, 100
30457, V, 1, 1, 1, 1, 0, 704, 100
30458, V, 1, 1, 1, 1, 0, 704, 100
30459, V, 1, 1, 1, 1, 0, 704, 100
30460, V, 1, 1, 1, 1, 0, 704, 100
30461, V, 1, 1, 1, 1, 0, 704, 100
30462, V, 1, 1, 1, 1, 0, 704, 100
30464, V, 1, 1, 1, 1, 0, 704, 100
30465, V, 1, 1, 1, 1, 0, 704, 100
30466, V, 1, 1, 1, 1, 0, 704, 100
30467, V, 1, 1, 1, 1, 0, 704, 100
30468, V, 1, 1, 1, 1, 0, 704, 100
30469, V, 1, 1, 1, 1, 0, 704, 100
30470, V, 1, 1, 1, 1, 0, 704, 100
30471, V, 1, 1, 1, 1, 0, 704, 100
30472, V, 1, 1, 1, 1, 0, 704, 100
30473, V, 1, 1, 1, 1, 0, 704, 100
30474, V, 1, 1, 1, 1, 0, 704, 100
30475, V, 1, 1, 1, 1, 0, 704, 100
30476, V, 1, 1, 1, 1, 0, 704, 100
30477, V, 1, 1, 1, 1, 0, 704, 100
30478, V, 1, 1, 1, 1, 0, 704, 100
30479, V, 1, 1, 1, 1, 0, 704, 100
30480, V, 1, 1, 1, 1, 0, 704, 100
30481, V, 1, 1, 1, 1, 0, 704, 100
30482, V, 1, 1, 1, 1, 0, 704, 100
30483, V, 1, 1, 1, 1, 0, 704, 100
30484, V, 1, 1, 1, 1, 0, 704, 100
30485, V, 1, 1, 1, 1, 0, 704, 100
30486, V, 1, 1, 1, 1, 0, 704, 100
30487, V, 1, 1, 1, 1, 0, 704, 100
30488, V, 1, 1, 1, 1, 0, 704, 100
30489, V, 1, 1, 1, 1, 0, 704, 100
30490, V, 1, 1, 1, 1, 0, 704, 100
30491, V, 1, 1, 1, 1, 0, 704, 100
30492, V, 1, 1, 1, 1, 0, 704, 100
30493, V, 1, 1, 1, 1, 0, 704, 100
30494, V, 1, 1, 1, 1, 0, 704, 100
30495, V, 1, 1, 1, 1, 0, 704, 100
30496, V, 1, 1, 1, 1, 0, 704, 100
30497, V, 1, 1, 1, 1, 0, 704, 100
30498, V, 1, 1, 1, 1, 0, 704, 100
30499, V, 1, 1, 1, 1, 0, 704, 100
30500, V, 1, 1, 1, 1, 0, 704, 100
30501, V, 1, 1, 1, 1, 0, 704, 100
30502, V, 1, 1, 1, 1, 0, 704, 100
30503, V, 1, 1, 1, 1, 0, 704, 100
30504, V, 1, 1, 1, 1, 0, 704, 100
30505, V, 1, 1, 1, 1, 0, 704, 100
30507, V, 1, 1, 1, 1, 0, 704, 100
30508, V, 1, 1, 1, 1, 0, 704, 100
30509, V, 1, 1, 1, 1, 0, 704, 100
30510, V, 1, 1, 1, 1, 0, 704, 100
30511, V, 1, 1, 1, 1, 0, 704, 100
30512, V, 1, 1, 1, 1, 0, 704, 100
30513, V, 1, 1, 1, 1, 0, 704, 100
30514, V, 1, 1, 1, 1, 0, 704, 100
30515, V, 1, 1, 1, 1, 0, 704, 100
30516, V, 1, 1, 1, 1, 0, 704, 100
30517, V, 1, 1, 1, 1, 0, 704, 100
30518, V, 1, 1, 1, 1, 0, 704, 100
30519, V, 1, 1, 1, 1, 0, 704, 100
30520, V, 1, 1, 1, 1, 0, 704, 100
30521, V, 1, 1, 1, 1, 0, 704, 100
30522, V, 1, 1, 1, 1, 0, 704, 100
30523, V, 1, 1, 1, 1, 0, 704, 100
30524, V, 1, 1, 1, 1, 0, 704, 100
30525, V, 1, 1, 1, 1, 0, 704, 100
30526, V, 1, 1, 1, 1, 0, 704, 100
30527, V, 1, 1, 1, 1, 0, 704, 100
30528, V, 1, 1, 1, 1, 0, 704, 100
30529, V, 1, 1, 1, 1, 0, 704, 100
30530, V, 1, 1, 1, 1, 0, 704, 100
30531, V, 1, 1, 1, 1, 0, 704, 100
30532, V, 1, 1, 1, 1, 0, 704, 100
30533, V, 1, 1, 1, 1, 0, 704, 100
30534, V, 1, 1, 1, 1, 0, 704, 100
30535, V, 1, 1, 1, 1, 0, 704, 100
30536, V, 1, 1, 1, 1, 0, 704, 100
30537, V, 1, 1, 1, 1, 0, 704, 100
30538, V, 1, 1, 1, 1, 0, 704, 100
30539, V, 1, 1, 1, 1, 0, 704, 100
30540, V, 1, 1, 1, 1, 0, 704, 100
30541, V, 1, 1, 1, 1, 0, 704, 100
30542, V, 1, 1, 1, 1, 0, 704, 100
30543, V, 1, 1, 1, 1, 0, 704, 100
30544, V, 1, 1, 1, 1, 0, 704, 100
30545, V, 1, 1, 1, 1, 0, 704, 100
30546, V, 1, 1, 1, 1, 0, 704, 100
30547, V, 1, 1, 1, 1, 0, 704, 100
30548, V, 1, 1, 1, 1, 0, 704, 100
30550, V, 1, 1, 1, 1, 0, 704, 100
30551, V, 1, 1, 1, 1, 0, 704, 100
30552, V, 1, 1, 1, 1, 0, 704, 100
30553, V, 1, 1, 1, 1, 0, 704, 100
30554, V, 1, 1, 1, 1, 0, 704, 100
30555, V, 1, 1, 1, 1, 0, 704, 100
30556, V, 1, 1, 1, 1, 0, 704, 100
30557, V, 1, 1, 1, 1, 0, 704, 100
30558, V, 1, 1, 1, 1, 0, 704, 100
30559, V, 1, 1, 1, 1, 0, 704, 100
30560, V, 1, 1, 1, 1, 0, 704, 100
30561, V, 1, 1, 1, 1, 0, 704, 100
30562, V, 1, 1, 1, 1, 0, 704, 100
30563, V, 1, 1, 1, 1, 0, 704, 100
30564, V, 1, 1, 1, 1, 0, 704, 100
30565, V, 1, 1, 1, 1, 0, 704, 100
30566, V, 1, 1, 1, 1, 0, 704, 100
30567, V, 1, 1, 1, 1, 0, 704, 100
30568, V, 1, 1, 1, 1, 0, 704, 100
30569, V, 1, 1, 1, 1, 0, 704, 100
30570, V, 1, 1, 1, 1, 0, 704, 100
30571, V, 1, 1, 1, 1, 0, 704, 100
30572, V, 1, 1, 1, 1, 0, 704, 100
30573, V, 1, 1, 1, 1, 0, 704, 100
30574, V, 1, 1, 1, 1, 0, 704, 100
30575, V, 1, 1, 1, 1, 0, 704, 100
30576, V, 1, 1, 1, 1, 0, 704, 100
30577, V, 1, 1, 1, 1, 0, 704, 100
30578, V, 1, 1, 1, 1, 0, 704, 100
30579, V, 1, 1, 1, 1, 0, 704, 100
30580, V, 1, 1, 1, 1, 0, 704, 100
30581, V, 1, 1, 1, 1, 0, 704, 100
30582, V, 1, 1, 1, 1, 0, 704, 100
30583, V, 1, 1, 1, 1, 0, 704, 100
30584, V, 1, 1, 1, 1, 0, 704, 100
30585, V, 1, 1, 1, 1, 0, 704, 100
30586, V, 1, 1, 1, 1, 0, 704, 100
30587, V, 1, 1, 1, 1, 0, 704, 100
30588, V, 1, 1, 1, 1, 0, 704, 100
30589, V, 1, 1, 1, 1, 0, 704, 100
30590, V, 1, 1, 1, 1, 0, 704, 100
30592, V, 1, 1, 1, 1, 0, 704, 100
30593, V, 1, 1, 1, 1, 0, 704, 100
30594, V, 1, 1, 1, 1, 0, 704, 100
30595, V, 1, 1, 1, 1, 0, 704, 100
30596, V, 1, 1, 1, 1, 0, 704, 100
30597, V, 1, 1, 1, 1, 0, 704, 100
30598, V, 1, 1, 1, 1, 0, 704, 100
30599, V, 1, 1, 1, 1, 0, 704, 100
30600, V, 1, 1, 1, 1, 0, 704, 100
30601, V, 1, 1, 1, 1, 0, 704, 100
30602, V, 1, 1, 1, 1, 0, 704, 100
30603, V, 1, 1, 1, 1, 0, 704, 100
30604, V, 1, 1, 1, 1, 0, 704, 100
30605, V, 1, 1, 1, 1, 0, 704, 100
30606, V, 1, 1, 1, 1, 0, 704, 100
30607, V, 1, 1, 1, 1, 0, 704, 100
30608, V, 1, 1, 1, 1, 0, 704, 100
30609, V, 1, 1, 1, 1, 0, 704, 100
30610, V, 1, 1, 1, 1, 0, 704, 100
30611, V, 1, 1, 1, 1, 0, 704, 100
30612, V, 1, 1, 1, 1, 0, 704, 100
30613, V, 1, 1, 1, 1, 0, 704, 100
30614, V, 1, 1, 1, 1, 0, 704, 100
30615, V, 1, 1, 1, 1, 0, 704, 100
30616, V, 1, 1, 1, 1, 0, 704, 100
30617, V, 1, 1, 1, 1, 0, 704, 100
30618, V, 1, 1, 1, 1, 0, 704, 100
30619, V, 1, 1, 1, 1, 0, 704, 100
30620, V, 1, 1, 1, 1, 0, 704, 100
30621, V, 1, 1, 1, 1, 0, 704, 100
30622, V, 1, 1, 1, 1, 0, 704, 100
30623, V, 1, 1, 1, 1, 0, 704, 100
30624, V, 1, 1, 1, 1, 0, 704, 100
30625, V, 1, 1, 1, 1, 0, 704, 100
30626, V, 1, 1, 1, 1, 0, 704, 100
30627, V, 1, 1, 1, 1, 0, 704, 100
30628, V, 1, 1, 1, 1, 0, 704, 100
30629, V, 1, 1, 1, 1, 0, 704, 100
30630, V, 1, 1, 1, 1, 0, 704, 100
30631, V, 1, 1, 1, 1, 0, 704, 100
30632, V, 1, 1, 1, 1, 0, 704, 100
30633, V, 1, 1, 1, 1, 0, 704, 100
30635, V, 1, 1, 1, 1, 0, 704, 100
30636, V, 1, 1, 1, 1, 0, 704, 100
30637, V, 1, 1, 1, 1, 0, 704, 100
30638, V, 1, 1, 1, 1, 0, 704, 100
30639, V, 1, 1, 1, 1, 0, 704, 100
30640, V, 1, 1, 1, 1, 0, 704, 100
30641, V, 1, 1, 1, 1, 0, 704, 100
30642, V, 1, 1, 1, 1, 0, 704, 100
30643, V, 1, 1, 1, 1, 0, 704, 100
30644, V, 1, 1, 1, 1, 0, 704, 100
30645, V, 1, 1, 1, 1, 0, 704, 100
30646, V, 1, 1, 1, 1, 0, 704, 100
30647, V, 1, 1, 1, 1, 0, 704, 100
30648, V, 1, 1, 1, 1, 0, 704, 100
30649, V, 1, 1, 1, 1, 0, 704, 100
30650, V, 1, 1, 1, 1, 0, 704, 100
30651, V, 1, 1, 1, 1, 0, 704, 100
30652, V, 1, 1, 1, 1, 0, 704, 100
30653, V, 1, 1, 1, 1, 0, 704, 100
30654, V, 1, 1, 1, 1, 0, 704, 100
30655, V, 1, 1, 1, 1, 0, 704, 100
30656, V, 1, 1, 1, 1, 0, 704, 100
30657, V, 1, 1, 1, 1, 0, 704, 100
30658, V, 1, 1, 1, 1, 0, 704, 100
30659, V, 1, 1, 1, 1, 0, 704, 100
30660, V, 1, 1, 1, 1, 0, 704, 100
30661, V, 1, 1, 1, 1, 0, 704, 100
30662, V, 1, 1, 1, 1, 0, 704, 100
30663, V, 1, 1, 1, 1, 0, 704, 100
30664, V, 1, 1, 1, 1, 0, 704, 100
30665, V, 1, 1, 1, 1, 0, 704, 100
30666, V, 1, 1, 1, 1, 0, 704, 100
30667, V, 1, 1, 1, 1, 0, 704, 100
30668, V, 1, 1, 1, 1, 0, 704, 100
30669, V, 1, 1, 1, 1, 0, 704, 100
30670, V, 1, 1, 1, 1, 0, 704, 100
30671, V, 1, 1, 1, 1, 0, 704, 100
30672, V, 1, 1, 1, 1, 0, 704, 100
30673, V, 1, 1, 1, 1, 0, 704, 100
30674, V, 1, 1, 1, 1, 0, 704, 100
30675, V, 1, 1, 1, 1, 0, 704, 100
30676, V, 1, 1, 1, 1, 0, 704, 100
30678, V, 1, 1, 1, 1, 0, 704, 100
30679, V, 1, 1, 1, 1, 0, 704, 100
30680, V, 1, 1, 1, 1, 0, 704, 100
30681, V, 1, 1, 1, 1, 0, 704, 100
30682, V, 1, 1, 1, 1, 0, 704, 100
30683, V, 1, 1, 1, 1, 0, 704, 100
30684, V, 1, 1, 1, 1, 0, 704, 100
30685, V, 1, 1, 1, 1, 0, 704, 100
30686, V, 1, 1, 1, 1, 0, 704, 100
30687, V, 1, 1, 1, 1, 0, 704, 100
30688, V, 1, 1, 1, 1, 0, 704, 100
30689, V, 1, 1, 1, 1, 0, 704, 100
30690, V, 1, 1, 1, 1, 0, 704, 100
30691, V, 1, 1, 1, 1, 0, 704, 100
30692, V, 1, 1, 1, 1, 0, 704, 100
30693, V, 1, 1, 1, 1, 0, 704, 100
30694, V, 1, 1, 1, 1, 0, 704, 100
30695, V, 1, 1, 1, 1, 0, 704, 100
30696, V, 1, 1, 1, 1, 0, 704, 100
30697, V, 1, 1, 1, 1, 0, 704, 100
30698, V, 1, 1, 1, 1, 0, 704, 100
30699, V, 1, 1, 1, 1, 0, 704, 100
30700, V, 1, 1, 1, 1, 0, 704, 100
30701, V, 1, 1, 1, 1, 0, 704, 100
30702, V, 1, 1, 1, 1, 0, 704, 100
30703, V, 1, 1, 1, 1, 0, 704, 100
30704, V, 1, 1, 1, 1, 0, 704, 100
30705, V, 1, 1, 1, 1, 0, 704, 100
30706, V, 1, 1, 1, 1, 0, 704, 100
30707, V, 1, 1, 1, 1, 0, 704, 100
30708, V, 1, 1, 1, 1, 0, 704, 100
30709, V, 1, 1, 1, 1, 0, 704, 100
30710, V, 1, 1, 1, 1, 0, 704, 100
30711, V, 1, 1, 1, 1, 0, 704, 100
30712, V, 1, 1, 1, 1, 0, 704, 100
30713, V, 1, 1, 1, 1, 0, 704, 100
30714, V, 1, 1, 1, 1, 0, 704, 100
30715, V, 1, 1, 1, 1, 0, 704, 100
30716, V, 1, 1, 1, 1, 0, 704, 100
30717, V, 1, 1, 1, 1, 0, 704, 100
30718, V, 1, 1, 1, 1, 0, 704, 100
30720, V, 1, 1, 1, 1, 0, 704, 100
30721, V, 1, 1, 1, 1, 0, 704, 100
30722, V, 1, 1, 1, 1, 0, 704, 100
30723, V, 1, 1, 1, 1, 0, 704, 100
30724, V, 1, 1, 1, 1, 0, 704, 100
30725, V, 1, 1, 1, 1, 0, 704, 100
30726, V, 1, 1, 1, 1, 0, 704, 100
30727, V, 1, 1, 1, 1, 0, 704, 100
30728, V, 1, 1, 1, 1, 0, 704, 100
30729, V, 1, 1, 1, 1, 0, 704, 100
30730, V, 1, 1, 1, 1, 0, 704, 100
30731, V, 1, 1, 1, 1, 0, 704, 100
30732, V, 1, 1, 1, 1, 0, 704, 100
30733, V, 1, 1, 1, 1, 0, 704, 100
30734, V, 1, 1, 1, 1, 0, 704, 100
30735, V, 1, 1, 1, 1, 0, 704, 100
30736, V, 1, 1, 1, 1, 0, 704, 100
30737, V, 1, 1, 1, 1, 0, 704, 100
30738, V, 1, 1, 1, 1, 0, 704, 100
30739, V, 1, 1, 1, 1, 0, 704, 100
30740, V, 1, 1, 1, 1, 0, 704, 100
30741, V, 1, 1, 1, 1, 0, 704, 100
30742, V, 1, 1, 1, 1, 0, 704, 100
30743, V, 1, 1, 1, 1, 0, 704, 100
30744, V, 1, 1, 1, 1, 0, 704, 100
30745, V, 1, 1, 1, 1, 0, 704, 100
30746, V, 1, 1, 1, 1, 0, 704, 100
30747, V, 1, 1, 1, 1, 0, 704, 100
30748, V, 1, 1, 1, 1, 0, 704, 100
30749, V, 1, 1, 1, 1, 0, 704, 100
30750, V, 1, 1, 1, 1, 0, 704, 100
30751, V, 1, 1, 1, 1, 0, 704, 100
30752, V, 1, 1, 1, 1, 0, 704, 100
30753, V, 1, 1, 1, 1, 0, 704, 100
30754, V, 1, 1, 1, 1, 0, 704, 100
30755, V, 1, 1, 1, 1, 0, 704, 100
30756, V, 1, 1, 1, 1, 0, 704, 100
30757, V, 1, 1, 1, 1, 0, 704, 100
30758, V, 1, 1, 1, 1, 0, 704, 100
30759, V, 1, 1, 1, 1, 0, 704, 100
30760, V, 1, 1, 1, 1, 0, 704, 100
30761, V, 1, 1, 1, 1, 0, 704, 100
30763, V, 1, 1, 1, 1, 0, 704, 100
30764, V, 1, 1, 1, 1, 0, 704, 100
30765, V, 1, 1, 1, 1, 0, 704, 100
30766, V, 1, 1, 1, 1, 0, 704, 100
30767, V, 1, 1, 1, 1, 0, 704, 100
30768, V, 1, 1, 1, 1, 0, 704, 100
30769, V, 1, 1, 1, 1, 0, 704, 100
30770, V, 1, 1, 1, 1, 0, 704, 100
30771, V, 1, 1, 1, 1, 0, 704, 100
30772, V, 1, 1, 1, 1, 0, 704, 100
30773, V, 1, 1, 1, 1, 0, 704, 100
30774, V, 1, 1, 1, 1, 0, 704, 100
30775, V, 1, 1, 1, 1, 0, 704, 100
30776, V, 1, 1, 1, 1, 0, 704, 100
30777, V, 1, 1, 1, 1, 0, 704, 100
30778, V, 1, 1, 1, 1, 0, 704, 100
30779, V, 1, 1, 1, 1, 0, 704, 100
30780, V, 1, 1, 1, 1, 0, 704, 100
30781, V, 1, 1, 1, 1, 0, 704, 100
30782, V, 1, 1, 1, 1, 0, 704, 100
30783, V, 1, 1, 1, 1, 0, 704, 100
30784, V, 1, 1, 1, 1, 0, 704, 100
30785, V, 1, 1, 1, 1, 0, 704, 100
30786, V, 1, 1, 1, 1, 0, 704, 100
30787, V, 1, 1, 1, 1, 0, 704, 100
30788, V, 1, 1, 1, 1, 0, 704, 100
30789, V, 1, 1, 1, 1, 0, 704, 100
30790, V, 1, 1, 1, 1, 0, 704, 100
30791, V, 1, 1, 1, 1, 0, 704, 100
30792, V, 1, 1, 1, 1, 0, 704, 100
30793, V, 1, 1, 1, 1, 0, 704, 100
30794, V, 1, 1, 1, 1, 0, 704, 100
30795, V, 1, 1, 1, 1, 0, 704, 100
30796, V, 1, 1, 1, 1, 0, 704, 100
30797, V, 1, 1, 1, 1, 0, 704, 100
30798, V, 1, 1, 1, 1, 0, 704, 100
30799, V, 1, 1, 1, 1, 0, 704, 100
30800, V, 1, 1, 1, 1, 0, 704, 100
30801, V, 1, 1, 1, 1, 0, 704, 100
30802, V, 1, 1, 1, 1, 0, 704, 100
30803, V, 1, 1, 1, 1, 0, 704, 100
30804, V, 1, 1, 1, 1, 0, 704, 100
30806, V, 1, 1, 1, 1, 0, 704, 100
30807, V, 1, 1, 1, 1, 0, 704, 100
30808, V, 1, 1, 1, 1, 0, 704, 100
30809, V, 1, 1, 1, 1, 0, 704, 100
30810, V, 1, 1, 1, 1, 0, 704, 100
30811, V, 1, 1, 1, 1, 0, 704, 100
30812, V, 1, 1, 1, 1, 0, 704, 100
30813, V, 1, 1, 1, 1, 0, 704, 100
30814, V, 1, 1, 1, 1, 0, 704, 100
30815, V, 1, 1, 1, 1, 0, 704, 100
30816, V, 1, 1, 1, 1, 0, 704, 100
30817, V, 1, 1, 1, 1, 0, 704, 100
30818, V, 1, 1, 1, 1, 0, 704, 100
30819, V, 1, 1, 1, 1, 0, 704, 100
30820, V, 1, 1, 1, 1, 0, 704, 100
30821, V, 1, 1, 1, 1, 0, 704, 100
30822, V, 1, 1, 1, 1, 0, 704, 100
30823, V, 1, 1, 1, 1, 0, 704, 100
30824, V, 1, 1, 1, 1, 0, 704, 100
30825, V, 1, 1, 1, 1, 0, 704, 100
30826, V, 1, 1, 1, 1, 0, 704, 100
30827, V, 1, 1, 1, 1, 0, 704, 100
30828, V, 1, 1, 1, 1, 0, 704, 100
30829, V, 1, 1, 1, 1, 0, 704, 100
30830, V, 1, 1, 1, 1, 0, 704, 100
30831, V, 1, 1, 1, 1, 0, 704, 100
30832, V, 1, 1, 1, 1, 0, 704, 100
30833, V, 1, 1, 1, 1, 0, 704, 100
30834, V, 1, 1, 1, 1, 0, 704, 100
30835, V, 1, 1, 1, 1, 0, 704, 100
30836, V, 1, 1, 1, 1, 0, 704, 100
30837, V, 1, 1, 1, 1, 0, 704, 100
30838, V, 1, 1, 1, 1, 0, 704, 100
30839, V, 1, 1, 1, 1, 0, 704, 100
30840, V, 1, 1, 1, 1, 0, 704, 100
30841, V, 1, 1, 1, 1, 0, 704, 100
30842, V, 1, 1, 1, 1, 0, 704, 100
30843, V, 1, 1, 1, 1, 0, 704, 100
30844, V, 1, 1, 1, 1, 0, 704, 100
30845, V, 1, 1, 1, 1, 0, 704, 100
30846, V, 1, 1, 1, 1, 0, 704, 100
30848, V, 1, 1, 1, 1, 0, 704, 100
30849, V, 1, 1, 1, 1, 0, 704, 100
30850, V, 1, 1, 1, 1, 0, 704, 100
30851, V, 1, 1, 1, 1, 0, 704, 100
30852, V, 1, 1, 1, 1, 0, 704, 100
30853, V, 1, 1, 1, 1, 0, 704, 100
30854, V, 1, 1, 1, 1, 0, 704, 100
30855, V, 1, 1, 1, 1, 0, 704, 100
30856, V, 1, 1, 1, 1, 0, 704, 100
30857, V, 1, 1, 1, 1, 0, 704, 100
30858, V, 1, 1, 1, 1, 0, 704, 100
30859, V, 1, 1, 1, 1, 0, 704, 100
30860, V, 1, 1, 1, 1, 0, 704, 100
30861, V, 1, 1, 1, 1, 0, 704, 100
30862, V, 1, 1, 1, 1, 0, 704, 100
30863, V, 1, 1, 1, 1, 0, 704, 100
30864, V, 1, 1, 1, 1, 0, 704, 100
30865, V, 1, 1, 1, 1, 0, 704, 100
30866, V, 1, 1, 1, 1, 0, 704, 100
30867, V, 1, 1, 1, 1, 0, 704, 100
30868, V, 1, 1, 1, 1, 0, 704, 100
30869, V, 1, 1, 1, 1, 0, 704, 100
30870, V, 1, 1, 1, 1, 0, 704, 100
30871, V, 1, 1, 1, 1, 0, 704, 100
30872, V, 1, 1, 1, 1, 0, 704, 100
30873, V, 1, 1, 1, 1, 0, 704, 100
30874, V, 1, 1, 1, 1, 0, 704, 100
30875, V, 1, 1, 1, 1, 0, 704, 100
30876, V, 1, 1, 1, 1, 0, 704, 100
30877, V, 1, 1, 1, 1, 0, 704, 100
30878, V, 1, 1, 1, 1, 0, 704, 100
30879, V, 1, 1, 1, 1, 0, 704, 100
30880, V, 1, 1, 1, 1, 0, 704, 100
30881, V, 1, 1, 1, 1, 0, 704, 100
30882, V, 1, 1, 1, 1, 0, 704, 100
30883, V, 1, 1, 1, 1, 0, 704, 100
30884, V, 1, 1, 1, 1, 0, 704, 100
30885, V, 1, 1, 1, 1, 0, 704, 100
30886, V, 1, 1, 1, 1, 0, 704, 100
30887, V, 1, 1, 1, 1, 0, 704, 100
30888, V, 1, 1, 1, 1, 0, 704, 100
30889, V, 1, 1, 1, 1, 0, 704, 100
30891, V, 1, 1, 1, 1, 0, 704, 100
30892, V, 1, 1, 1, 1, 0, 704, 100
30893, V, 1, 1, 1, 1, 0, 704, 100
30894, V, 1, 1, 1, 1, 0, 704, 100
30895, V, 1, 1, 1, 1, 0, 704, 100
30896, V, 1, 1, 1, 1, 0, 704, 100
30897, V, 1, 1, 1, 1, 0, 704, 100
30898, V, 1, 1, 1, 1, 0, 704, 100
30899, V, 1, 1, 1, 1, 0, 704, 100
30900, V, 1, 1, 1, 1, 0, 704, 100
30901, V, 1, 1, 1, 1, 0, 704, 100
30902, V, 1, 1, 1, 1, 0, 704, 100
30903, V, 1, 1, 1, 1, 0, 704, 100
30904, V, 1, 1, 1, 1, 0, 704, 100
30905, V, 1, 1, 1, 1, 0, 704, 100
30906, V, 1, 1, 1, 1, 0, 704, 100
30907, V, 1, 1, 1, 1, 0, 704, 100
30908, V, 1, 1, 1, 1, 0, 704, 100
30909, V, 1, 1, 1, 1, 0, 704, 100
30910, V, 1, 1, 1, 1, 0, 704, 100
30911, V, 1, 1, 1, 1, 0, 704, 100
30912, V, 1, 1, 1, 1, 0, 704, 100
30913, V, 1, 1, 1, 1, 0, 704, 100
30914, V, 1, 1, 1, 1, 0, 704, 100
30915, V, 1, 1, 1, 1, 0, 704, 100
30916, V, 1, 1, 1, 1, 0, 704, 100
30917, V, 1, 1, 1, 1, 0, 704, 100
30918, V, 1, 1, 1, 1, 0, 704, 100
30919, V, 1, 1, 1, 1, 0, 704, 100
30920, V, 1, 1, 1, 1, 0, 704, 100
30921, V, 1, 1, 1, 1, 0, 704, 100
30922, V, 1, 1, 1, 1, 0, 704, 100
30923, V, 1, 1, 1, 1, 0, 704, 100
30924, V, 1, 1, 1, 1, 0, 704, 100
30925, V, 1, 1, 1, 1, 0, 704, 100
30926, V, 1, 1, 1, 1, 0, 704, 100
30927, V, 1, 1, 1, 1, 0, 704, 100
30928, V, 1, 1, 1, 1, 0, 704, 100
30929, V, 1, 1, 1, 1, 0, 704, 100
30930, V, 1, 1, 1, 1, 0, 704, 100
30931, V, 1, 1, 1, 1, 0, 704, 100
30932, V, 1, 1, 1, 1, 0, 704, 100
30934, V, 1, 1, 1, 1, 0, 704, 100
30935, V, 1, 1, 1, 1, 0, 704, 100
30936, V, 1, 1, 1, 1, 0, 704, 100
30937, V, 1, 1, 1, 1, 0, 704, 100
30938, V, 1, 1, 1, 1, 0, 704, 100
30939, V, 1, 1, 1, 1, 0, 704, 100
30940, V, 1, 1, 1, 1, 0, 704, 100
30941, V, 1, 1, 1, 1, 0, 704, 100
30942, V, 1, 1, 1, 1, 0, 704, 100
30943, V, 1, 1, 1, 1, 0, 704, 100
30944, V, 1, 1, 1, 1, 0, 704, 100
30945, V, 1, 1, 1, 1, 0, 704, 100
30946, V, 1, 1, 1, 1, 0, 704, 100
30947, V, 1, 1, 1, 1, 0, 704, 100
30948, V, 1, 1, 1, 1, 0, 704, 100
30949, V, 1, 1, 1, 1, 0, 704, 100
30950, V, 1, 1, 1, 1, 0, 704, 100
30951, V, 1, 1, 1, 1, 0, 704, 100
30952, V, 1, 1, 1, 1, 0, 704, 100
30953, V, 1, 1, 1, 1, 0, 704, 100
30954, V, 1, 1, 1, 1, 0, 704, 100
30955, V, 1, 1, 1, 1, 0, 704, 100
30956, V, 1, 1, 1, 1, 0, 704, 100
30957, V, 1, 1, 1, 1, 0, 704, 100
30958, V, 1, 1, 1, 1, 0, 704, 100
30959, V, 1, 1, 1, 1, 0, 704, 100
30960, V, 1, 1, 1, 1, 0, 704, 100
30961, V, 1, 1, 1, 1, 0, 704, 100
30962, V, 1, 1, 1, 1, 0, 704, 100
30963, V, 1, 1, 1, 1, 0, 704, 100
30964, V, 1, 1, 1, 1, 0, 704, 100
30965, V, 1, 1, 1, 1, 0, 704, 100
30966, V, 1, 1, 1, 1, 0, 704, 100
30967, V, 1, 1, 1, 1, 0, 704, 100
30968, V, 1, 1, 1, 1, 0, 704, 100
30969, V, 1, 1, 1, 1, 0, 704, 100
30970, V, 1, 1, 1, 1, 0, 704, 100
30971, V, 1, 1, 1, 1, 0, 704, 100
30972, V, 1, 1, 1, 1, 0, 704, 100
30973, V, 1, 1, 1, 1, 0, 704, 100
30974, V, 1, 1, 1, 1, 0, 704, 100
30976, V, 1, 1, 1, 1, 0, 704, 100
30977, V, 1, 1, 1, 1, 0, 704, 100
30978, V, 1, 1, 1, 1, 0, 704, 100
30979, V, 1, 1, 1, 1, 0, 704, 100
30980, V, 1, 1, 1, 1, 0, 704, 100
30981, V, 1, 1, 1, 1, 0, 704, 100
30982, V, 1, 1, 1, 1, 0, 704, 100
30983, V, 1, 1, 1, 1, 0, 704, 100
30984, V, 1, 1, 1, 1, 0, 704, 100
30985, V, 1, 1, 1, 1, 0, 704, 100
30986, V, 1, 1, 1, 1, 0, 704, 100
30987, V, 1, 1, 1, 1, 0, 704, 100
30988, V, 1, 1, 1, 1, 0, 704, 100
30989, V, 1, 1, 1, 1, 0, 704, 100
30990, V, 1, 1, 1, 1, 0, 704, 100
30991, V, 1, 1, 1, 1, 0, 704, 100
30992, V, 1, 1, 1, 1, 0, 704, 100
30993, V, 1, 1, 1, 1, 0, 704, 100
30994, V, 1, 1, 1, 1, 0, 704, 100
30995, V, 1, 1, 1, 1, 0, 704, 100
30996, V, 1, 1, 1, 1, 0, 704, 100
30997, V, 1, 1, 1, 1, 0, 704, 100
30998, V, 1, 1, 1, 1, 0, 704, 100
30999, V, 1, 1, 1, 1, 0, 704, 100
31000, V, 1, 1, 1, 1, 0, 704, 100
31001, V, 1, 1, 1, 1, 0, 704, 100
31002, V, 1, 1, 1, 1, 0, 704, 100
31003, V, 1, 1, 1, 1, 0, 704, 100
31004, V, 1, 1, 1, 1, 0, 704, 100
31005, V, 1, 1, 1, 1, 0, 704, 100
31006, V, 1, 1, 1, 1, 0, 704, 100
31007, V, 1, 1, 1, 1, 0, 704, 100
31008, V, 1, 1, 1, 1, 0, 704, 100
31009, V, 1, 1, 1, 1, 0, 704, 100
31010, V, 1, 1, 1, 1, 0, 704, 100
31011, V, 1, 1, 1, 1, 0, 704, 100
31012, V, 1, 1, 1, 1, 0, 704, 100
31013, V, 1, 1, 1, 1, 0, 704, 100
31014, V, 1, 1, 1, 1, 0, 704, 100
31015, V, 1, 1, 1, 1, 0, 704, 100
31016, V, 1, 1, 1, 1, 0, 704, 100
31017, V, 1, 1, 1, 1, 0, 704, 100
31019, V, 1, 1, 1, 1, 0, 704, 100
31020, V, 1, 1, 1, 1, 0, 704, 100
31021, V, 1, 1, 1, 1, 0, 704, 100
31022, V, 1, 1, 1, 1, 0, 704, 100
31023, V, 1, 1, 1, 1, 0, 704, 100
31024, V, 1, 1, 1, 1, 0, 704, 100
31025, V, 1, 1, 1, 1, 0, 704, 100
31026, V, 1, 1, 1, 1, 0, 704, 100
31027, V, 1, 1, 1, 1, 0, 704, 100
31028, V, 1, 1, 1, 1, 0, 704, 100
31029, V, 1, 1, 1, 1, 0, 704, 100
31030, V, 1, 1, 1, 1, 0, 704, 100
31031, V, 1, 1, 1, 1, 0, 704, 100
31032, V, 1, 1, 1, 1, 0, 704, 100
31033, V, 1, 1, 1, 1, 0, 704, 100
31034, V, 1, 1, 1, 1, 0, 704, 100
31035, V, 1, 1, 1, 1, 0, 704, 100
31036, V, 1, 1, 1, 1, 0, 704, 100
31037, V, 1, 1, 1, 1, 0, 704, 100
31038, V, 1, 1, 1, 1, 0, 704, 100
31039, V, 1, 1, 1, 1, 0, 704, 100
31040, V, 1, 1, 1, 1, 0, 704, 100
31041, V, 1, 1, 1, 1, 0, 704, 100
31042, V, 1, 1, 1, 1, 0, 704, 100
31043, V, 1, 1, 1, 1, 0, 704, 100
31044, V, 1, 1, 1, 1, 0, 704, 100
31045, V, 1, 1, 1, 1, 0, 704, 100
31046, V, 1, 1, 1, 1, 0, 704, 100
31047, V, 1, 1, 1, 1, 0, 704, 100
31048, V, 1, 1, 1, 1, 0, 704, 100
31049, V, 1, 1, 1, 1, 0, 704, 100
31050, V, 1, 1, 1, 1, 0, 704, 100
31051, V, 1, 1, 1, 1, 0, 704, 100
31052, V, 1, 1, 1, 1, 0, 704, 100
31053, V, 1, 1, 1, 1, 0, 704, 100
31054, V, 1, 1, 1, 1, 0, 704, 100
31055, V, 1, 1, 1, 1, 0, 704, 100
31056, V, 1, 1, 1, 1, 0, 704, 100
31057, V, 1, 1, 1, 1, 0, 704, 100
31058, V, 1, 1, 1, 1, 0, 704, 100
31059, V, 1, 1, 1, 1, 0, 704, 100
31060, V, 1, 1, 1, 1, 0, 704, 100
31062, V, 1, 1, 1, 1, 0, 704, 100
31063, V, 1, 1, 1, 1, 0, 704, 100
31064, V, 1, 1, 1, 1, 0, 704, 100
31065, V, 1, 1, 1, 1, 0, 704, 100
31066, V, 1, 1, 1, 1, 0, 704, 100
31067, V, 1, 1, 1, 1, 0, 704, 100
31068, V, 1, 1, 1, 1, 0, 704, 100
31069, V, 1, 1, 1, 1, 0, 704, 100
31070, V, 1, 1, 1, 1, 0, 704, 100
31071, V, 1, 1, 1, 1, 0, 704, 100
31072, V, 1, 1, 1, 1, 0, 704, 100
31073, V, 1, 1, 1, 1, 0, 704, 100
31074, V, 1, 1, 1, 1, 0, 704, 100
31075, V, 1, 1, 1, 1, 0, 704, 100
31076, V, 1, 1, 1, 1, 0, 704, 100
31077, V, 1, 1, 1, 1, 0, 704, 100
31078, V, 1, 1, 1, 1, 0, 704, 100
31079, V, 1, 1, 1, 1, 0, 704, 100
31080, V, 1, 1, 1, 1, 0, 704, 100
31081, V, 1, 1, 1, 1, 0, 704, 100
31082, V, 1, 1, 1, 1, 0, 704, 100
31083, V, 1, 1, 1, 1, 0, 704, 100
31084, V, 1, 1, 1, 1, 0, 704, 100
31085, V, 1, 1, 1, 1, 0, 704, 100
31086, V, 1, 1, 1, 1, 0, 704, 100
31087, V, 1, 1, 1, 1, 0, 704, 100
31088, V, 1, 1, 1, 1, 0, 704, 100
31089, V, 1, 1, 1, 1, 0, 704, 100
31090, V, 1, 1, 1, 1, 0, 704, 100
31091, V, 1, 1, 1, 1, 0, 704, 100
31092, V, 1, 1, 1, 1, 0, 704, 100
31093, V, 1, 1, 1, 1, 0, 704, 100
31094, V, 1, 1, 1, 1, 0, 704, 100
31095, V, 1, 1, 1, 1, 0, 704, 100
31096, V, 1, 1, 1, 1, 0, 704, 100
31097, V, 1, 1, 1, 1, 0, 704, 100
31098, V, 1, 1, 1, 1, 0, 704, 100
31099, V, 1, 1, 1, 1, 0, 704, 100
31100, V, 1, 1, 1, 1, 0, 704, 100
31101, V, 1, 1, 1, 1, 0, 704, 100
31102, V, 1, 1, 1, 1, 0, 704, 100
31104, V, 1, 1, 1, 1, 0, 704, 100
31105, V, 1, 1, 1, 1, 0, 704, 100
31106, V, 1, 1, 1, 1, 0, 704, 100
31107, V, 1, 1, 1, 1, 0, 704, 100
31108, V, 1, 1, 1, 1, 0, 704, 100
31109, V, 1, 1, 1, 1, 0, 704, 100
31110, V, 1, 1, 1, 1, 0, 704, 100
31111, V, 1, 1, 1, 1, 0, 704, 100
31112, V, 1, 1, 1, 1, 0, 704, 100
31113, V, 1, 1, 1, 1, 0, 704, 100
31114, V, 1, 1, 1, 1, 0, 704, 100
31115, V, 1, 1, 1, 1, 0, 704, 100
31116, V, 1, 1, 1, 1, 0, 704, 100
31117, V, 1, 1, 1, 1, 0, 704, 100
31118, V, 1, 1, 1, 1, 0, 704, 100
31119, V, 1, 1, 1, 1, 0, 704, 100
31120, V, 1, 1, 1, 1, 0, 704, 100
31121, V, 1, 1, 1, 1, 0, 704, 100
31122, V, 1, 1, 1, 1, 0, 704, 100
31123, V, 1, 1, 1, 1, 0, 704, 100
31124, V, 1, 1, 1, 1, 0, 704, 100
31125, V, 1, 1, 1, 1, 0, 704, 100
31126, V, 1, 1, 1, 1, 0, 704, 100
31127, V, 1, 1, 1, 1, 0, 704, 100
31128, V, 1, 1, 1, 1, 0, 704, 100
31129, V, 1, 1, 1, 1, 0, 704, 100
31130, V, 1, 1, 1, 1, 0, 704, 100
31131, V, 1, 1, 1, 1, 0, 704, 100
31132, V, 1, 1, 1, 1, 0, 704, 100
31133, V, 1, 1, 1, 1, 0, 704, 100
31134, V, 1, 1, 1, 1, 0, 704, 100
31135, V, 1, 1, 1, 1, 0, 704, 100
31136, V, 1, 1, 1, 1, 0, 704, 100
31137, V, 1, 1, 1, 1, 0, 704, 100
31138, V, 1, 1, 1, 1, 0, 704, 100
31139, V, 1, 1, 1, 1, 0, 704, 100
31140, V, 1, 1, 1, 1, 0, 704, 100
31141, V, 1, 1, 1, 1, 0, 704, 100
31142, V, 1, 1, 1, 1, 0, 704, 100
31143, V, 1, 1, 1, 1, 0, 704, 100
31144, V, 1, 1, 1, 1, 0, 704, 100
31145, V, 1, 1, 1, 1, 0, 704, 100
31147, V, 1, 1, 1, 1, 0, 704, 100
31148, V, 1, 1, 1, 1, 0, 704, 100
31149, V, 1, 1, 1, 1, 0, 704, 100
31150, V, 1, 1, 1, 1, 0, 704, 100
31151, V, 1, 1, 1, 1, 0, 704, 100
31152, V, 1, 1, 1, 1, 0, 704, 100
31153, V, 1, 1, 1, 1, 0, 704, 100
31154, V, 1, 1, 1, 1, 0, 704, 100
31155, V, 1, 1, 1, 1, 0, 704, 100
31156, V, 1, 1, 1, 1, 0, 704, 100
31157, V, 1, 1, 1, 1, 0, 704, 100
31158, V, 1, 1, 1, 1, 0, 704, 100
31159, V, 1, 1, 1, 1, 0, 704, 100
31160, V, 1, 1, 1, 1, 0, 704, 100
31161, V, 1, 1, 1, 1, 0, 704, 100
31162, V, 1, 1, 1, 1, 0, 704, 100
31163, V, 1, 1, 1, 1, 0, 704, 100
31164, V, 1, 1, 1, 1, 0, 704, 100
31165, V, 1, 1, 1, 1, 0, 704, 100
31166, V, 1, 1, 1, 1, 0, 704, 100
31167, V, 1, 1, 1, 1, 0, 704, 100
31168, V, 1, 1, 1, 1, 0, 704, 100
31169, V, 1, 1, 1, 1, 0, 704, 100
31170, V, 1, 1, 1, 1, 0, 704, 100
31171, V, 1, 1, 1, 1, 0, 704, 100
31172, V, 1, 1, 1, 1, 0, 704, 100
31173, V, 1, 1, 1, 1, 0, 704, 100
31174, V, 1, 1, 1, 1, 0, 704, 100
31175, V, 1, 1, 1, 1, 0, 704, 100
31176, V, 1, 1, 1, 1, 0, 704, 100
31177, V, 1, 1, 1, 1, 0, 704, 100
31178, V, 1, 1, 1, 1, 0, 704, 100
31179, V, 1, 1, 1, 1, 0, 704, 100
31180, V, 1, 1, 1, 1, 0, 704, 100
31181, V, 1, 1, 1, 1, 0, 704, 100
31182, V, 1, 1, 1, 1, 0, 704, 100
31183, V, 1, 1, 1, 1, 0, 704, 100
31184, V, 1, 1, 1, 1, 0, 704, 100
31185, V, 1, 1, 1, 1, 0, 704, 100
31186, V, 1, 1, 1, 1, 0, 704, 100
31187, V, 1, 1, 1, 1, 0, 704, 100
31188, V, 1, 1, 1, 1, 0, 704, 100
31190, V, 1, 1, 1, 1, 0, 704, 100
31191, V, 1, 1, 1, 1, 0, 704, 100
31192, V, 1, 1, 1, 1, 0, 704, 100
31193, V, 1, 1, 1, 1, 0, 704, 100
31194, V, 1, 1, 1, 1, 0, 704, 100
31195, V, 1, 1, 1, 1, 0, 704, 100
31196, V, 1, 1, 1, 1, 0, 704, 100
31197, V, 1, 1, 1, 1, 0, 704, 100
31198, V, 1, 1, 1, 1, 0, 704, 100
31199, V, 1, 1, 1, 1, 0, 704, 100
31200, V, 1, 1, 1, 1, 0, 704, 100
31201, V, 1, 1, 1, 1, 0, 704, 100
31202, V, 1, 1, 1, 1, 0, 704, 100
31203, V, 1, 1, 1, 1, 0, 704, 100
31204, V, 1, 1, 1, 1, 0, 704, 100
31205, V, 1, 1, 1, 1, 0, 704, 100
31206, V, 1, 1, 1, 1, 0, 704, 100
31207, V, 1, 1, 1, 1, 0, 704, 100
31208, V, 1, 1, 1, 1, 0, 704, 100
31209, V, 1, 1, 1, 1, 0, 704, 100
31210, V, 1, 1, 1, 1, 0, 704, 100
31211, V, 1, 1, 1, 1, 0, 704, 100
31212, V, 1, 1, 1, 1, 0, 704, 100
31213, V, 1, 1, 1, 1, 0, 704, 100
31214, V, 1, 1, 1, 1, 0, 704, 100
31215, V, 1, 1, 1, 1, 0, 704, 100
31216, V, 1, 1, 1, 1, 0, 704, 100
31217, V, 1, 1, 1, 1, 0, 704, 100
31218, V, 1, 1, 1, 1, 0, 704, 100
31219, V, 1, 1, 1, 1, 0, 704, 100
31220, V, 1, 1, 1, 1, 0, 704, 100
31221, V, 1, 1, 1, 1, 0, 704, 100
31222, V, 1, 1, 1, 1, 0, 704, 100
31223, V, 1, 1, 1, 1, 0, 704, 100
31224, V, 1, 1, 1, 1, 0, 704, 100
31225, V, 1, 1, 1, 1, 0, 704, 100
31226, V, 1, 1, 1, 1, 0, 704, 100
31227, V, 1, 1, 1, 1, 0, 704, 100
31228, V, 1, 1, 1, 1, 0, 704, 100
31229, V, 1, 1, 1, 1, 0, 704, 100
31230, V, 1, 1, 1, 1, 0, 704, 100
31232, V, 1, 1, 1, 1, 0, 704, 100
31233, V, 1, 1, 1, 1, 0, 704, 100
31234, V, 1, 1, 1, 1, 0, 704, 100
31235, V, 1, 1, 1, 1, 0, 704, 100
31236, V, 1, 1, 1, 1, 0, 704, 100
31237, V, 1, 1, 1, 1, 0, 704, 100
31238, V, 1, 1, 1, 1, 0, 704, 100
31239, V, 1, 1, 1, 1, 0, 704, 100
31240, V, 1, 1, 1, 1, 0, 704, 100
31241, V, 1, 0, 0, 1, 0, 704, 100
31241, V, 1, 0, 0, 0, 0, 704, 100
31242, V, 1, 1, 0, 0, 0, 704, 100
31242, V, 1, 1, 0, 0, 0, 704, 100
31243, V, 1, 1, 1, 1, 0, 704, 100
31244, V, 1, 1, 1, 1, 0, 704, 100
31245, V, 1, 1, 1, 1, 0, 704, 100
31246, V, 1, 1, 1, 1, 0, 704, 100
31247, V, 1, 1, 1, 1, 0, 704, 100
31248, V, 1, 1, 1, 1, 0, 704, 100
31249, V, 1, 1, 1, 1, 0, 704, 99
31250, V, 1, 1, 1, 1, 0, 704, 99
31251, V, 1, 1, 1, 1, 0, 704, 99
31252, V, 1, 1, 1, 1, 0, 704, 99
31253, V, 1, 1, 1, 1, 0, 704, 99
31254, V, 1, 1, 1, 1, 0, 704, 99
31255, V, 1, 1, 1, 1, 0, 704, 99
31256, V, 1, 1, 1, 1, 0, 704, 99
31257, V, 1, 1, 1, 1, 0, 704, 99
31258, V, 1, 1, 1, 1, 0, 704, 100
31259, V, 1, 1, 1, 1, 0, 704, 100
31260, V, 1, 1, 1, 1, 0, 704, 100
31261, V, 1, 1, 1, 1, 0, 704, 100
31262, V, 1, 1, 1, 1, 0, 704, 100
31263, V, 1, 1, 1, 1, 0, 704, 100
31264, V, 1, 1, 1, 1, 0, 704, 100
31265, V, 1, 1, 1, 1, 0, 704, 100
31266, V, 1, 1, 1, 1, 0, 704, 100
31267, V, 1, 1, 1, 1, 0, 704, 100
31268, V, 1, 1, 1, 1, 0, 704, 100
31269, V, 1, 1, 1, 1, 0, 704, 100
31270, V, 1, 1, 1, 1, 0, 704, 100
31271, V, 1, 1, 1, 1, 0, 704, 100
31272, V, 1, 1, 1, 1, 0, 704, 100
31273, V, 1, 1, 1, 1, 0, 704, 100
31275, V, 1, 1, 1, 1, 0, 704, 100
31276, V, 1, 1, 1, 1, 0, 704, 100
31277, V, 1, 1, 1, 1, 0, 704, 100
31278, V, 1, 1, 1, 1, 0, 704, 100
31279, V, 1, 1, 1, 1, 0, 704, 100
31280, V, 1, 1, 1, 1, 0, 704, 100
31281, V, 1, 1, 1, 1, 0, 704, 100
31282, V, 1, 1, 1, 1, 0, 704, 100
31283, V, 1, 1, 1, 1, 0, 704, 100
31284, V, 1, 1, 1, 1, 0, 704, 100
31285, V, 1, 1, 1, 1, 0, 704, 100
31286, V, 1, 1, 1, 1, 0, 704, 100
31287, V, 1, 1, 1, 1, 0, 704, 100
31288, V, 1, 1, 1, 1, 0, 704, 100
31289, V, 1, 1, 1, 1, 0, 704, 100
31290, V, 1, 1, 1, 1, 0, 704, 100
31291, V, 1, 1, 1, 1, 0, 704, 100
31292, V, 1, 1, 1, 1, 0, 704, 100
31293, V, 1, 1, 1, 1, 0, 704, 100
31294, V, 1, 1, 1, 1, 0, 704, 100
31295, V, 1, 1, 1, 1, 0, 704, 100
31296, V, 1, 1, 1, 1, 0, 704, 100
31297, V, 1, 1, 1, 1, 0, 704, 100
31298, V, 1, 1, 1, 1, 0, 704, 100
31299, V, 1, 1, 1, 1, 0, 704, 100
31300, V, 1, 1, 1, 1, 0, 704, 100
31301, V, 1, 1, 1, 1, 0, 704, 100
31302, V, 1, 1, 1, 1, 0, 704, 100
31303, V, 1, 1, 1, 1, 0, 704, 100
31304, V, 1, 1, 1, 1, 0, 704, 100
31305, V, 1, 1, 1, 1, 0, 704, 100
31306, V, 1, 1, 1, 1, 0, 704, 100
31307, V, 1, 1, 1, 1, 0, 704, 100
31308, V, 1, 1, 1, 1, 0, 704, 100
31309, V, 1, 1, 1, 1, 0, 704, 100
31310, V, 1, 1, 1, 1, 0, 704, 100
31311, V, 1, 1, 1, 1, 0, 704, 100
31312, V, 1, 1, 1, 1, 0, 704, 100
31313, V, 1, 1, 1, 1, 0, 704, 100
31314, V, 1, 1, 1, 1, 0, 704, 100
31315, V, 1, 1, 1, 1, 0, 704, 100
31316, V, 1, 1, 1, 1, 0, 704, 100
31318, V, 1, 1, 1, 1, 0, 704, 100
31319, V, 1, 1, 1, 1, 0, 704, 100
31320, V, 1, 1, 1, 1, 0, 704, 100
31321, V, 1, 1, 1, 1, 0, 704, 100
31322, V, 1, 1, 1, 1, 0, 704, 100
31323, V, 1, 1, 1, 1, 0, 704, 100
31324, V, 1, 1, 1, 1, 0, 704, 100
31325, V, 1, 1, 1, 1, 0, 704, 100
31326, V, 1, 1, 1, 1, 0, 704, 100
31327, V, 1, 1, 1, 1, 0, 704, 100
31328, V, 1, 1, 1, 1, 0, 704, 100
31329, V, 1, 1, 1, 1, 0, 704, 100
31330, V, 1, 1, 1, 1, 0, 704, 100
31331, V, 1, 1, 1, 1, 0, 704, 100
31332, V, 1, 1, 1, 1, 0, 704, 100
31333, V, 1, 1, 1, 1, 0, 704, 100
31334, V, 1, 1, 1, 1, 0, 704, 100
31335, V, 1, 1, 1, 1, 0, 704, 100
31336, V, 1, 1, 1, 1, 0, 704, 100
31337, V, 1, 1, 1, 1, 0, 704, 100
31338, V, 1, 1, 1, 1, 0, 704, 100
31339, V, 1, 1, 1, 1, 0, 704, 100
31340, V, 1, 1, 1, 1, 0, 704, 100
31341, V, 1, 1, 1, 1, 0, 704, 100
31342, V, 1, 1, 1, 1, 0, 704, 100
31343, V, 1, 1, 1, 1, 0, 704, 100
31344, V, 1, 1, 1, 1, 0, 704, 100
31345, V, 1, 1, 1, 1, 0, 704, 100
31346, V, 1, 1, 1, 1, 0, 704, 100
31347, V, 1, 1, 1, 1, 0, 704, 100
31348, V, 1, 1, 1, 1, 0, 704, 100
31349, V, 1, 1, 1, 1, 0, 704, 100
31350, V, 1, 1, 1, 1, 0, 704, 100
31351, V, 1, 1, 1, 1, 0, 704, 100
31352, V, 1, 1, 1, 1, 0, 704, 100
31353, V, 1, 1, 1, 1, 0, 704, 100
31354, V, 1, 1, 1, 1, 0, 704, 100
31355, V, 1, 1, 1, 1, 0, 704, 100
31356, V, 1, 1, 1, 1, 0, 704, 100
31357, V, 1, 1, 1, 1, 0, 704, 100
31358, V, 1, 1, 1, 1, 0, 704, 100
31360, V, 1, 1, 1, 1, 0, 704, 100
31361, V, 1, 1, 1, 1, 0, 704, 100
31362, V, 1, 1, 1, 1, 0, 704, 100
31363, V, 1, 1, 1, 1, 0, 704, 100
31364, V, 1, 1, 1, 1, 0, 704, 100
31365, V, 1, 1, 1, 1, 0, 704, 100
31366, V, 1, 1, 1, 1, 0, 704, 100
31367, V, 1, 1, 1, 1, 0, 704, 100
31368, V, 1, 1, 1, 1, 0, 704, 100
31369, V, 1, 1, 1, 1, 0, 704, 100
31370, V, 1, 1, 1, 1, 0, 704, 100
31371, V, 1, 1, 1, 1, 0, 704, 100
31372, V, 1, 1, 1, 1, 0, 704, 100
31373, V, 1, 1, 1, 1, 0, 704, 100
31374, V, 1, 1, 1, 1, 0, 704, 100
31375, V, 1, 1, 1, 1, 0, 704, 100
31376, V, 1, 1, 1, 1, 0, 704, 100
31377, V, 1, 1, 1, 1, 0, 704, 100
31378, V, 1, 1, 1, 1, 0, 704, 100
31379, V, 1, 1, 1, 1, 0, 704, 100
31380, V, 1, 1, 1, 1, 0, 704, 100
31381, V, 1, 1, 1, 1, 0, 704, 100
31382, V, 1, 1, 1, 1, 0, 704, 100
31383, V, 1, 1, 1, 1, 0, 704, 100
31384, V, 1, 1, 1, 1, 0, 704, 100
31385, V, 1, 1, 1, 1, 0, 704, 100
31386, V, 1, 1, 1, 1, 0, 704, 100
31387, V, 1, 1, 1, 1, 0, 704, 100
31388, V, 1, 1, 1, 1, 0, 704, 100
31389, V, 1, 1, 1, 1, 0, 704, 100
31390, V, 1, 1, 1, 1, 0, 704, 100
31391, V, 1, 1, 1, 1, 0, 704, 100
31392, V, 1, 1, 1, 1, 0, 704, 100
31393, V, 1, 1, 1, 1, 0, 704, 100
31394, V, 1, 1, 1, 1, 0, 704, 100
31395, V, 1, 1, 1, 1, 0, 704, 100
31396, V, 1, 1, 1, 1, 0, 704, 100
31397, V, 1, 1, 1, 1, 0, 704, 100
31398, V, 1, 1, 1, 1, 0, 704, 100
31399, V, 1, 1, 1, 1, 0, 704, 100
31400, V, 1, 1, 1, 1, 0, 704, 100
31401, V, 1, 1, 1, 1, 0, 704, 100
31403, V, 1, 1, 1, 1, 0, 704, 100
31404, V, 1, 1, 1, 1, 0, 704, 100
31405, V, 1, 1, 1, 1, 0, 704, 100
31406, V, 1, 1, 1, 1, 0, 704, 100
31407, V, 1, 1, 1, 1, 0, 704, 100
31408, V, 1, 1, 1, 1, 0, 704, 100
31409, V, 1, 1, 1, 1, 0, 704, 100
31410, V, 1, 1, 1, 1, 0, 704, 100
31411, V, 1, 1, 1, 1, 0, 704, 100
31412, V, 1, 1, 1, 1, 0, 704, 100
31413, V, 1, 1, 1, 1, 0, 704, 100
31414, V, 1, 1, 1, 1, 0, 704, 100
31415, V, 1, 1, 1, 1, 0, 704, 100
31416, V, 1, 1, 1, 1, 0, 704, 100
31417, V, 1, 1, 1, 1, 0, 704, 100
31418, V, 1, 1, 1, 1, 0, 704, 100
31419, V, 1, 1, 1, 1, 0, 704, 100
31420, V, 1, 1, 1, 1, 0, 704, 100
31421, V, 1, 1, 1, 1, 0, 704, 100
31422, V, 1, 1, 1, 1, 0, 704, 100
31423, V, 1, 1, 1, 1, 0, 704, 100
31424, V, 1, 1, 1, 1, 0, 704, 100
31425, V, 1, 1, 1, 1, 0, 704, 100
31426, V, 1, 1, 1, 1, 0, 704, 100
31427, V, 1, 1, 1, 1, 0, 704, 100
31428, V, 1, 1, 1, 1, 0, 704, 100
31429, V, 1, 1, 1, 1, 0, 704, 100
31430, V, 1, 1, 1, 1, 0, 704, 100
31431, V, 1, 1, 1, 1, 0, 704, 100
31432, V, 1, 1, 1, 1, 0, 704, 100
31433, V, 1, 1, 1, 1, 0, 704, 100
31434, V, 1, 1, 1, 1, 0, 704, 100
31435, V, 1, 1, 1, 1, 0, 704, 100
31436, V, 1, 1, 1, 1, 0, 704, 100
31437, V, 1, 1, 1, 1, 0, 704, 100
31438, V, 1, 1, 1, 1, 0, 704, 100
31439, V, 1, 1, 1, 1, 0, 704, 100
31440, V, 1, 1, 1, 1, 0, 704, 100
31441, V, 1, 1, 1, 1, 0, 704, 100
31442, V, 1, 1, 1, 1, 0, 704, 100
31443, V, 1, 1, 1, 1, 0, 704, 100
31444, V, 1, 1, 1, 1, 0, 704, 100
31446, V, 1, 1, 1, 1, 0, 704, 100
31447, V, 1, 1, 1, 1, 0, 704, 100
31448, V, 1, 1, 1, 1, 0, 704, 100
31449, V, 1, 1, 1, 1, 0, 704, 100
31450, V, 1, 1, 1, 1, 0, 704, 100
31451, V, 1, 1, 1, 1, 0, 704, 100
31452, V, 1, 1, 1, 1, 0, 704, 100
31453, V, 1, 1, 1, 1, 0, 704, 100
31454, V, 1, 1, 1, 1, 0, 704, 100
31455, V, 1, 1, 1, 1, 0, 704, 100
31456, V, 1, 1, 1, 1, 0, 704, 100
31457, V, 1, 1, 1, 1, 0, 704, 100
31458, V, 1, 1, 1, 1, 0, 704, 100
31459, V, 1, 1, 1, 1, 0, 704, 100
31460, V, 1, 1, 1, 1, 0, 704, 100
31461, V, 1, 1, 1, 1, 0, 704, 100
31462, V, 1, 1, 1, 1, 0, 704, 100
31463, V, 1, 1, 1, 1, 0, 704, 100
31464, V, 1, 1, 1, 1, 0, 704, 100
31465, V, 1, 1, 1, 1, 0, 704, 100
31466, V, 1, 1, 1, 1, 0, 704, 100
31467, V, 1, 1, 1, 1, 0, 704, 100
31468, V, 1, 1, 1, 1, 0, 704, 100
31469, V, 1, 1, 1, 1, 0, 704, 100
31470, V, 1, 1, 1, 1, 0, 704, 100
31471, V, 1, 1, 1, 1, 0, 704, 100
31472, V, 1, 1, 1, 1, 0, 704, 100
31473, V, 1, 1, 1, 1, 0, 704, 100
31474, V, 1, 1, 1, 1, 0, 704, 100
31475, V, 1, 1, 1, 1, 0, 704, 100
31476, V, 1, 1, 1, 1, 0, 704, 100
31477, V, 1, 1, 1, 1, 0, 704, 100
31478, V, 1, 1, 1, 1, 0, 704, 100
31479, V, 1, 1, 1, 1, 0, 704, 100
31480, V, 1, 1, 1, 1, 0, 704, 100
31481, V, 1, 1, 1, 1, 0, 704, 100
31482, V, 1, 1, 1, 1, 0, 704, 100
31483, V, 1, 1, 1, 1, 0, 704, 100
31484, V, 1, 1, 1, 1, 0, 704, 100
31485, V, 1, 1, 1, 1, 0, 704, 100
31486, V, 1, 1, 1, 1, 0, 704, 100
31488, V, 1, 1, 1, 1, 0, 704, 100
31489, V, 1, 1, 1, 1, 0, 704, 100
31490, V, 1, 1, 1, 1, 0, 704, 100
31491, V, 1, 1, 1, 1, 0, 704, 100
31492, V, 1, 1, 1, 1, 0, 704, 100
31493, V, 1, 1, 1, 1, 0, 704, 100
31494, V, 1, 1, 1, 1, 0, 704, 100
31495, V, 1, 1, 1, 1, 0, 704, 100
31496, V, 1, 1, 1, 1, 0, 704, 100
31497, V, 1, 1, 1, 1, 0, 704, 100
31498, V, 1, 1, 1, 1, 0, 704, 100
31499, V, 1, 1, 1, 1, 0, 704, 100
31500, V, 1, 1, 1, 1, 0, 704, 100
31501, V, 1, 1, 1, 1, 0, 704, 100
31502, V, 1, 1, 1, 1, 0, 704, 100
31503, V, 1, 1, 1, 1, 0, 704, 100
31504, V, 1, 1, 1, 1, 0, 704, 100
31505, V, 1, 1, 1, 1, 0, 704, 100
31506, V, 1, 1, 1, 1, 0, 704, 100
31507, V, 1, 1, 1, 1, 0, 704, 100
31508, V, 1, 1, 1, 1, 0, 704, 100
31509, V, 1, 1, 1, 1, 0, 704, 100
31510, V, 1, 1, 1, 1, 0, 704, 100
31511, V, 1, 1, 1, 1, 0, 704, 100
31512, V, 1, 1, 1, 1, 0, 704, 100
31513, V, 1, 1, 1, 1, 0, 704, 100
31514, V, 1, 1, 1, 1, 0, 704, 100
31515, V, 1, 1, 1, 1, 0, 704, 100
31516, V, 1, 1, 1, 1, 0, 704, 100
31517, V, 1, 1, 1, 1, 0, 704, 100
31518, V, 1, 1, 1, 1, 0, 704, 100
31519, V, 1, 1, 1, 1, 0, 704, 100
31520, V, 1, 1, 1, 1, 0, 704, 100
31521, V, 1, 1, 1, 1, 0, 704, 100
31522, V, 1, 1, 1, 1, 0, 704, 100
31523, V, 1, 1, 1, 1, 0, 704, 100
31524, V, 1, 1, 1, 1, 0, 704, 100
31525, V, 1, 1, 1, 1, 0, 704, 100
31526, V, 1, 1, 1, 1, 0, 704, 100
31527, V, 1, 1, 1, 1, 0, 704, 100
31528, V, 1, 1, 1, 1, 0, 704, 100
31529, V, 1, 1, 1, 1, 0, 704, 100
31531, V, 1, 1, 1, 1, 0, 704, 100
31532, V, 1, 1, 1, 1, 0, 704, 100
31533, V, 1, 1, 1, 1, 0, 704, 100
31534, V, 1, 1, 1, 1, 0, 704, 100
31535, V, 1, 1, 1, 1, 0, 704, 100
31536, V, 1, 1, 1, 1, 0, 704, 100
31537, V, 1, 1, 1, 1, 0, 704, 100
31538, V, 1, 1, 1, 1, 0, 704, 100
31539, V, 1, 1, 1, 1, 0, 704, 100
31540, V, 1, 1, 1, 1, 0, 704, 100
31541, V, 1, 1, 1, 1, 0, 704, 100
31542, V, 1, 1, 1, 1, 0, 704, 100
31543, V, 1, 1, 1, 1, 0, 704, 100
31544, V, 1, 1, 1, 1, 0, 704, 100
31545, V, 1, 1, 1, 1, 0, 704, 100
31546, V, 1, 1, 1, 1, 0, 704, 100
31547, V, 1, 1, 1, 1, 0, 704, 100
31548, V, 1, 1, 1, 1, 0, 704, 100
31549, V, 1, 1, 1, 1, 0, 704, 100
31550, V, 1, 1, 1, 1, 0, 704, 100
31551, V, 1, 1, 1, 1, 0, 704, 100
31552, V, 1, 1, 1, 1, 0, 704, 100
31553, V, 1, 1, 1, 1, 0, 704, 100
31554, V, 1, 1, 1, 1, 0, 704, 100
31555, V, 1, 1, 1, 1, 0, 704, 100
31556, V, 1, 1, 1, 1, 0, 704, 100
31557, V, 1, 1, 1, 1, 0, 704, 100
31558, V, 1, 1, 1, 1, 0, 704, 100
31559, V, 1, 1, 1, 1, 0, 704, 100
31560, V, 1, 1, 1, 1, 0, 704, 100
31561, V, 1, 1, 1, 1, 0, 704, 100
31562, V, 1, 1, 1, 1, 0, 704, 100
31563, V, 1, 1, 1, 1, 0, 704, 100
31564, V, 1, 1, 1, 1, 0, 704, 100
31565, V, 1, 1, 1, 1, 0, 704, 100
31566, V, 1, 1, 1, 1, 0, 704, 100
31567, V, 1, 1, 1, 1, 0, 704, 100
31568, V, 1, 1, 1, 1, 0, 704, 100
31569, V, 1, 1, 1, 1, 0, 704, 100
31570, V, 1, 1, 1, 1, 0, 704, 100
31571, V, 1, 1, 1, 1, 0, 704, 100
31572, V, 1, 1, 1, 1, 0, 704, 100
31574, V, 1, 1, 1, 1, 0, 704, 100
31575, V, 1, 1, 1, 1, 0, 704, 100
31576, V, 1, 1, 1, 1, 0, 704, 100
31577, V, 1, 1, 1, 1, 0, 704, 100
31578, V, 1, 1, 1, 1, 0, 704, 100
31579, V, 1, 1, 1, 1, 0, 704, 100
31580, V, 1, 1, 1, 1, 0, 704, 100
31581, V, 1, 1, 1, 1, 0, 704, 100
31582, V, 1, 1, 1, 1, 0, 704, 100
31583, V, 1, 1, 1, 1, 0, 704, 100
31584, V, 1, 1, 1, 1, 0, 704, 100
31585, V, 1, 1, 1, 1, 0, 704, 100
31586, V, 1, 1, 1, 1, 0, 704, 100
31587, V, 1, 1, 1, 1, 0, 704, 100
31588, V, 1, 1, 1, 1, 0, 704, 100
31589, V, 1, 1, 1, 1, 0, 704, 100
31590, V, 1, 1, 1, 1, 0, 704, 100
31591, V, 1, 1, 1, 1, 0, 704, 100
31592, V, 1, 1, 1, 1, 0, 704, 100
31593, V, 1, 1, 1, 1, 0, 704, 100
31594, V, 1, 1, 1, 1, 0, 704, 100
31595, V, 1, 1, 1, 1, 0, 704, 100
31596, V, 1, 1, 1, 1, 0, 704, 100
31597, V, 1, 1, 1, 1, 0, 704, 100
31598, V, 1, 1, 1, 1, 0, 704, 100
31599, V, 1, 1, 1, 1, 0, 704, 100
31600, V, 1, 1, 1, 1, 0, 704, 100
31601, V, 1, 1, 1, 1, 0, 704, 100
31602, V, 1, 1, 1, 1, 0, 704, 100
31603, V, 1, 1, 1, 1, 0, 704, 100
31604, V, 1, 1, 1, 1, 0, 704, 100
31605, V, 1, 1, 1, 1, 0, 704, 100
31606, V, 1, 1, 1, 1, 0, 704, 100
31607, V, 1, 1, 1, 1, 0, 704, 100
31608, V, 1, 1, 1, 1, 0, 704, 100
31609, V, 1, 1, 1, 1, 0, 704, 100
31610, V, 1, 1, 1, 1, 0, 704, 100
31611, V, 1, 1, 1, 1, 0, 704, 100
31612, V, 1, 1, 1, 1, 0, 704, 100
31613, V, 1, 1, 1, 1, 0, 704, 100
31614, V, 1, 1, 1, 1, 0, 704, 100
31616, V, 1, 1, 1, 1, 0, 704, 100
31617, V, 1, 1, 1, 1, 0, 704, 100
31618, V, 1, 1, 1, 1, 0, 704, 100
31619, V, 1, 1, 1, 1, 0, 704, 100
31620, V, 1, 1, 1, 1, 0, 704, 100
31621, V, 1, 1, 1, 1, 0, 704, 100
31622, V, 1, 1, 1, 1, 0, 704, 100
31623, V, 1, 1, 1, 1, 0, 704, 100
31624, V, 1, 1, 1, 1, 0, 704, 100
31625, V, 1, 1, 1, 1, 0, 704, 100
31626, V, 1, 1, 1, 1, 0, 704, 100
31627, V, 1, 1, 1, 1, 0, 704, 100
31628, V, 1, 1, 1, 1, 0, 704, 100
31629, V, 1, 1, 1, 1, 0, 704, 100
31630, V, 1, 1, 1, 1, 0, 704, 100
31631, V, 1, 1, 1, 1, 0, 704, 100
31632, V, 1, 1, 1, 1, 0, 704, 100
31633, V, 1, 1, 1, 1, 0, 704, 100
31634, V, 1, 1, 1, 1, 0, 704, 100
31635, V, 1, 1, 1, 1, 0, 704, 100
31636, V, 1, 1, 1, 1, 0, 704, 100
31637, V, 1, 1, 1, 1, 0, 704, 100
31638, V, 1, 1, 1, 1, 0, 704, 100
31639, V, 1, 1, 1, 1, 0, 704, 100
31640, V, 1, 1, 1, 1, 0, 704, 100
31641, V, 1, 1, 1, 1, 0, 704, 100
31642, V, 1, 1, 1, 1, 0, 704, 100
31643, V, 1, 1, 1, 1, 0, 704, 100
31644, V, 1, 1, 1, 1, 0, 704, 100
31645, V, 1, 1, 1, 1, 0, 704, 100
31646, V, 1, 1, 1, 1, 0, 704, 100
31647, V, 1, 1, 1, 1, 0, 704, 100
31648, V, 1, 1, 1, 1, 0, 704, 100
31649, V, 1, 1, 1, 1, 0, 704, 100
31650, V, 1, 1, 1, 1, 0, 704, 100
31651, V, 1, 1, 1, 1, 0, 704, 100
31652, V, 1, 1, 1, 1, 0, 704, 100
31653, V, 1, 1, 1, 1, 0, 704, 100
31654, V, 1, 1, 1, 1, 0, 704, 100
31655, V, 1, 1, 1, 1, 0, 704, 100
31656, V, 1, 1, 1, 1, 0, 704, 100
31657, V, 1, 1, 1, 1, 0, 704, 100
31659, V, 1, 1, 1, 1, 0, 704, 100
31660, V, 1, 1, 1, 1, 0, 704, 100
31661, V, 1, 1, 1, 1, 0, 704, 100
31662, V, 1, 1, 1, 1, 0, 704, 100
31663, V, 1, 1, 1, 1, 0, 704, 100
31664, V, 1, 1, 1, 1, 0, 704, 100
31665, V, 1, 1, 1, 1, 0, 704, 100
31666, V, 1, 1, 1, 1, 0, 704, 100
31667, V, 1, 1, 1, 1, 0, 704, 100
31668, V, 1, 1, 1, 1, 0, 704, 100
31669, V, 1, 1, 1, 1, 0, 704, 100
31670, V, 1, 1, 1, 1, 0, 704, 100
31671, V, 1, 1, 1, 1, 0, 704, 100
31672, V, 1, 1, 1, 1, 0, 704, 100
31673, V, 1, 1, 1, 1, 0, 704, 100
31674, V, 1, 1, 1, 1, 0, 704, 100
31675, V, 1, 1, 1, 1, 0, 704, 100
31676, V, 1, 1, 1, 1, 0, 704, 100
31677, V, 1, 1, 1, 1, 0, 704, 100
31678, V, 1, 1, 1, 1, 0, 704, 100
31679, V, 1, 1, 1, 1, 0, 704, 100
31680, V, 1, 1, 1, 1, 0, 704, 100
31681, V, 1, 1, 1, 1, 0, 704, 100
31682, V, 1, 1, 1, 1, 0, 704, 100
31683, V, 1, 1, 1, 1, 0, 704, 100
31684, V, 1, 1, 1, 1, 0, 704, 100
31685, V, 1, 1, 1, 1, 0, 704, 100
31686, V, 1, 1, 1, 1, 0, 704, 100
31687, V, 1, 1, 1, 1, 0, 704, 100
31688, V, 1, 1, 1, 1, 0, 704, 100
31689, V, 1, 1, 1, 1, 0, 704, 100
31690, V, 1, 1, 1, 1, 0, 704, 100
31691, V, 1, 1, 1, 1, 0, 704, 100
31692, V, 1, 1, 1, 1, 0, 704, 100
31693, V, 1, 1, 1, 1, 0, 704, 100
31694, V, 1, 1, 1, 1, 0, 704, 100
31695, V, 1, 1, 1, 1, 0, 704, 100
31696, V, 1, 1, 1, 1, 0, 704, 100
31697, V, 1, 1, 1, 1, 0, 704, 100
31698, V, 1, 1, 1, 1, 0, 704, 100
31699, V, 1, 1, 1, 1, 0, 704, 100
31700, V, 1, 1, 1, 1, 0, 704, 100
31702, V, 1, 1, 1, 1, 0, 704, 100
31703, V, 1, 1, 1, 1, 0, 704, 100
31704, V, 1, 1, 1, 1, 0, 704, 100
31705, V, 1, 1, 1, 1, 0, 704, 100
31706, V, 1, 1, 1, 1, 0, 704, 100
31707, V, 1, 1, 1, 1, 0, 704, 100
31708, V, 1, 1, 1, 1, 0, 704, 100
31709, V, 1, 1, 1, 1, 0, 704, 100
31710, V, 1, 1, 1, 1, 0, 704, 100
31711, V, 1, 1, 1, 1, 0, 704, 100
31712, V, 1, 1, 1, 1, 0, 704, 100
31713, V, 1, 1, 1, 1, 0, 704, 100
31714, V, 1, 1, 1, 1, 0, 704, 100
31715, V, 1, 1, 1, 1, 0, 704, 100
31716, V, 1, 1, 1, 1, 0, 704, 100
31717, V, 1, 1, 1, 1, 0, 704, 100
31718, V, 1, 1, 1, 1, 0, 704, 100
31719, V, 1, 1, 1, 1, 0, 704, 100
31720, V, 1, 1, 1, 1, 0, 704, 100
31721, V, 1, 1, 1, 1, 0, 704, 100
31722, V, 1, 1, 1, 1, 0, 704, 100
31723, V, 1, 1, 1, 1, 0, 704, 100
31724, V, 1, 1, 1, 1, 0, 704, 100
31725, V, 1, 1, 1, 1, 0, 704, 100
31726, V, 1, 1, 1, 1, 0, 704, 100
31727, V, 1, 1, 1, 1, 0, 704, 100
31728, V, 1, 1, 1, 1, 0, 704, 100
31729, V, 1, 1, 1, 1, 0, 704, 100
31730, V, 1, 1, 1, 1, 0, 704, 100
31731, V, 1, 1, 1, 1, 0, 704, 100
31732, V, 1, 1, 1, 1, 0, 704, 100
31733, V, 1, 1, 1, 1, 0, 704, 100
31734, V, 1, 1, 1, 1, 0, 704, 100
31735, V, 1, 1, 1, 1, 0, 704, 100
31736, V, 1, 1, 1, 1, 0, 704, 100
31737, V, 1, 1, 1, 1, 0, 704, 100
31738, V, 1, 1, 1, 1, 0, 704, 100
31739, V, 1, 1, 1, 1, 0, 704, 100
31740, V, 1, 1, 1, 1, 0, 704, 100
31741, V, 1, 1, 1, 1, 0, 704, 100
31742, V, 1, 1, 1, 1, 0, 704, 100
31744, V, 1, 1, 1, 1, 0, 704, 100
31745, V, 1, 1, 1, 1, 0, 704, 100
31746, V, 1, 1, 1, 1, 0, 704, 100
31747, V, 1, 1, 1, 1, 0, 704, 100
31748, V, 1, 1, 1, 1, 0, 704, 100
31749, V, 1, 1, 1, 1, 0, 704, 100
31750, V, 1, 1, 1, 1, 0, 704, 100
31751, V, 1, 1, 1, 1, 0, 704, 100
31752, V, 1, 1, 1, 1, 0, 704, 100
31753, V, 1, 1, 1, 1, 0, 704, 100
31754, V, 1, 1, 1, 1, 0, 704, 100
31755, V, 1, 1, 1, 1, 0, 704, 100
31756, V, 1, 1, 1, 1, 0, 704, 100
31757, V, 1, 1, 1, 1, 0, 704, 100
31758, V, 1, 1, 1, 1, 0, 704, 100
31759, V, 1, 1, 1, 1, 0, 704, 100
31760, V, 1, 1, 1, 1, 0, 704, 100
31761, V, 1, 1, 1, 1, 0, 704, 100
31762, V, 1, 1, 1, 1, 0, 704, 100
31763, V, 1, 1, 1, 1, 0, 704, 100
31764, V, 1, 1, 1, 1, 0, 704, 100
31765, V, 1, 1, 1, 1, 0, 704, 100
31766, V, 1, 1, 1, 1, 0, 704, 100
31767, V, 1, 1, 1, 1, 0, 704, 100
31768, V, 1, 1, 1, 1, 0, 704, 100
31769, V, 1, 1, 1, 1, 0, 704, 100
31770, V, 1, 1, 1, 1, 0, 704, 100
31771, V, 1, 1, 1, 1, 0, 704, 100
31772, V, 1, 1, 1, 1, 0, 704, 100
31773, V, 1, 1, 1, 1, 0, 704, 100
31774, V, 1, 1, 1, 1, 0, 704, 100
31775, V, 1, 1, 1, 1, 0, 704, 100
31776, V, 1, 1, 1, 1, 0, 704, 100
31777, V, 1, 1, 1, 1, 0, 704, 100
31778, V, 1, 1, 1, 1, 0, 704, 100
31779, V, 1, 1, 1, 1, 0, 704, 100
31780, V, 1, 1, 1, 1, 0, 704, 100
31781, V, 1, 1, 1, 1, 0, 704, 100
31782, V, 1, 1, 1, 1, 0, 704, 100
31783, V, 1, 1, 1, 1, 0, 704, 100
31784, V, 1, 1, 1, 1, 0, 704, 100
31785, V, 1, 1, 1, 1, 0, 704, 100
31787, V, 1, 1, 1, 1, 0, 704, 100
31788, V, 1, 1, 1, 1, 0, 704, 100
31789, V, 1, 1, 1, 1, 0, 704, 100
31790, V, 1, 1, 1, 1, 0, 704, 100
31791, V, 1, 1, 1, 1, 0, 704, 100
31792, V, 1, 1, 1, 1, 0, 704, 100
31793, V, 1, 1, 1, 1, 0, 704, 100
31794, V, 1, 1, 1, 1, 0, 704, 100
31795, V, 1, 1, 1, 1, 0, 704, 100
31796, V, 1, 1, 1, 1, 0, 704, 100
31797, V, 1, 1, 1, 1, 0, 704, 100
31798, V, 1, 1, 1, 1, 0, 704, 100
31799, V, 1, 1, 1, 1, 0, 704, 100
31800, V, 1, 1, 1, 1, 0, 704, 100
31801, V, 1, 1, 1, 1, 0, 704, 100
31802, V, 1, 1, 1, 1, 0, 704, 100
31803, V, 1, 1, 1, 1, 0, 704, 100
31804, V, 1, 1, 1, 1, 0, 704, 100
31805, V, 1, 1, 1, 1, 0, 704, 100
31806, V, 1, 1, 1, 1, 0, 704, 100
31807, V, 1, 1, 1, 1, 0, 704, 100
31808, V, 1, 1, 1, 1, 0, 704, 100
31809, V, 1, 1, 1, 1, 0, 704, 100
31810, V, 1, 1, 1, 1, 0, 704, 100
31811, V, 1, 1, 1, 1, 0, 704, 100
31812, V, 1, 1, 1, 1, 0, 704, 100
31813, V, 1, 1, 1, 1, 0, 704, 100
31814, V, 1, 1, 1, 1, 0, 704, 100
31815, V, 1, 1, 1, 1, 0, 704, 100
31816, V, 1, 1, 1, 1, 0, 704, 100
31817, V, 1, 1, 1, 1, 0, 704, 100
31818, V, 1, 1, 1, 1, 0, 704, 100
31819, V, 1, 1, 1, 1, 0, 704, 100
31820, V, 1, 1, 1, 1, 0, 704, 100
31821, V, 1, 1, 1, 1, 0, 704, 100
31822, V, 1, 1, 1, 1, 0, 704, 100
31823, V, 1, 1, 1, 1, 0, 704, 100
31824, V, 1, 1, 1, 1, 0, 704, 100
31825, V, 1, 1, 1, 1, 0, 704, 100
31826, V, 1, 1, 1, 1, 0, 704, 100
31827, V, 1, 1, 1, 1, 0, 704, 100
31828, V, 1, 1, 1, 1, 0, 704, 100
31830, V, 1, 1, 1, 1, 0, 704, 100
31831, V, 1, 1, 1, 1, 0, 704, 100
31832, V, 1, 1, 1, 1, 0, 704, 100
31833, V, 1, 1, 1, 1, 0, 704, 100
31834, V, 1, 1, 1, 1, 0, 704, 100
31835, V, 1, 1, 1, 1, 0, 704, 100
31836, V, 1, 1, 1, 1, 0, 704, 100
31837, V, 1, 1, 1, 1, 0, 704, 100
31838, V, 1, 1, 1, 1, 0, 704, 100
31839, V, 1, 1, 1, 1, 0, 704, 100
31840, V, 1, 1, 1, 1, 0, 704, 100
31841, V, 1, 1, 1, 1, 0, 704, 100
31842, V, 1, 1, 1, 1, 0, 704, 100
31843, V, 1, 1, 1, 1, 0, 704, 100
31844, V, 1, 1, 1, 1, 0, 704, 100
31845, V, 1, 1, 1, 1, 0, 704, 100
31846, V, 1, 1, 1, 1, 0, 704, 100
31847, V, 1, 1, 1, 1, 0, 704, 100
31848, V, 1, 1, 1, 1, 0, 704, 100
31849, V, 1, 1, 1, 1, 0, 704, 100
31850, V, 1, 1, 1, 1, 0, 704, 100
31851, V, 1, 1, 1, 1, 0, 704, 100
31852, V, 1, 1, 1, 1, 0, 704, 100
31853, V, 1, 1, 1, 1, 0, 704, 100
31854, V, 1, 1, 1, 1, 0, 704, 100
31855, V, 1, 1, 1, 1, 0, 704, 100
31856, V, 1, 1, 1, 1, 0, 704, 100
31857, V, 1, 1, 1, 1, 0, 704, 100
31858, V, 1, 1, 1, 1, 0, 704, 100
31859, V, 1, 1, 1, 1, 0, 704, 100
31860, V, 1, 1, 1, 1, 0, 704, 100
31861, V, 1, 1, 1, 1, 0, 704, 100
31862, V, 1, 1, 1, 1, 0, 704, 100
31863, V, 1, 1, 1, 1, 0, 704, 100
31864, V, 1, 1, 1, 1, 0, 704, 100
31865, V, 1, 1, 1, 1, 0, 704, 100
31866, V, 1, 1, 1, 1, 0, 704, 100
31867, V, 1, 1, 1, 1, 0, 704, 100
31868, V, 1, 1, 1, 1, 0, 704, 100
31869, V, 1, 1, 1, 1, 0, 704, 100
31870, V, 1, 1, 1, 1, 0, 704, 100
31872, V, 1, 1, 1, 1, 0, 704, 100
31873, V, 1, 1, 1, 1, 0, 704, 100
31874, V, 1, 1, 1, 1, 0, 704, 100
31875, V, 1, 1, 1, 1, 0, 704, 100
31876, V, 1, 1, 1, 1, 0, 704, 100
31877, V, 1, 1, 1, 1, 0, 704, 100
31878, V, 1, 1, 1, 1, 0, 704, 100
31879, V, 1, 1, 1, 1, 0, 704, 100
31880, V, 1, 1, 1, 1, 0, 704, 100
31881, V, 1, 1, 1, 1, 0, 704, 100
31882, V, 1, 1, 1, 1, 0, 704, 100
31883, V, 1, 1, 1, 1, 0, 704, 100
31884, V, 1, 1, 1, 1, 0, 704, 100
31885, V, 1, 1, 1, 1, 0, 704, 100
31886, V, 1, 1, 1, 1, 0, 704, 100
31887, V, 1, 1, 1, 1, 0, 704, 100
31888, V, 1, 1, 1, 1, 0, 704, 100
31889, V, 1, 1, 1, 1, 0, 704, 100
31890, V, 1, 1, 1, 1, 0, 704, 100
31891, V, 1, 1, 1, 1, 0, 704, 100
31892, V, 1, 1, 1, 1, 0, 704, 100
31893, V, 1, 1, 1, 1, 0, 704, 100
31894, V, 1, 1, 1, 1, 0, 704, 100
31895, V, 1, 1, 1, 1, 0, 704, 100
31896, V, 1, 1, 1, 1, 0, 704, 100
31897, V, 1, 1, 1, 1, 0, 704, 100
31898, V, 1, 1, 1, 1, 0, 704, 100
31899, V, 1, 1, 1, 1, 0, 704, 100
31900, V, 1, 1, 1, 1, 0, 704, 100
31901, V, 1, 1, 1, 1, 0, 704, 100
31902, V, 1, 1, 1, 1, 0, 704, 100
31903, V, 1, 1, 1, 1, 0, 704, 100
31904, V, 1, 1, 1, 1, 0, 704, 100
31905, V, 1, 1, 1, 1, 0, 704, 100
31906, V, 1, 1, 1, 1, 0, 704, 100
31907, V, 1, 1, 1, 1, 0, 704, 100
31908, V, 1, 1, 1, 1, 0, 704, 100
31909, V, 1, 1, 1, 1, 0, 704, 100
31910, V, 1, 1, 1, 1, 0, 704, 100
31911, V, 1, 1, 1, 1, 0, 704, 100
31912, V, 1, 1, 1, 1, 0, 704, 100
31913, V, 1, 1, 1, 1, 0, 704, 100
31915, V, 1, 1, 1, 1, 0, 704, 100
31916, V, 1, 1, 1, 1, 0, 704, 100
31917, V, 1, 1, 1, 1, 0, 704, 100
31918, V, 1, 1, 1, 1, 0, 704, 100
31919, V, 1, 1, 1, 1, 0, 704, 100
31920, V, 1, 1, 1, 1, 0, 704, 100
31921, V, 1, 1, 1, 1, 0, 704, 100
31922, V, 1, 1, 1, 1, 0, 704, 100
31923, V, 1, 1, 1, 1, 0, 704, 100
31924, V, 1, 1, 1, 1, 0, 704, 100
31925, V, 1, 1, 1, 1, 0, 704, 100
31926, V, 1, 1, 1, 1, 0, 704, 100
31927, V, 1, 1, 1, 1, 0, 704, 100
31928, V, 1, 1, 1, 1, 0, 704, 100
31929, V, 1, 1, 1, 1, 0, 704, 100
31930, V, 1, 1, 1, 1, 0, 704, 100
31931, V, 1, 1, 1, 1, 0, 704, 100
31932, V, 1, 1, 1, 1, 0, 704, 100
31933, V, 1, 1, 1, 1, 0, 704, 100
31934, V, 1, 1, 1, 1, 0, 704, 100
31935, V, 1, 1, 1, 1, 0, 704, 100
31936, V, 1, 1, 1, 1, 0, 704, 100
31937, V, 1, 1, 1, 1, 0, 704, 100
31938, V, 1, 1, 1, 1, 0, 704, 100
31939, V, 1, 1, 1, 1, 0, 704, 100
31940, V, 1, 1, 1, 1, 0, 704, 100
31941, V, 1, 1, 1, 1, 0, 704, 100
31942, V, 1, 1, 1, 1, 0, 704, 100
31943, V, 1, 1, 1, 1, 0, 704, 100
31944, V, 1, 1, 1, 1, 0, 704, 100
31945, V, 1, 1, 1, 1, 0, 704, 100
31946, V, 1, 1, 1, 1, 0, 704, 100
31947, V, 1, 1, 1, 1, 0, 704, 100
31948, V, 1, 1, 1, 1, 0, 704, 100
31949, V, 1, 1, 1, 1, 0, 704, 100
31950, V, 1, 1, 1, 1, 0, 704, 100
31951, V, 1, 1, 1, 1, 0, 704, 100
31952, V, 1, 1, 1, 1, 0, 704, 100
31953, V, 1, 1, 1, 1, 0, 704, 100
31954, V, 1, 1, 1, 1, 0, 704, 100
31955, V, 1, 1, 1, 1, 0, 704, 100
31956, V, 1, 1, 1, 1, 0, 704, 100
31958, V, 1, 1, 1, 1, 0, 704, 100
31959, V, 1, 1, 1, 1, 0, 704, 100
31960, V, 1, 1, 1, 1, 0, 704, 100
31961, V, 1, 1, 1, 1, 0, 704, 100
31962, V, 1, 1, 1, 1, 0, 704, 100
31963, V, 1, 1, 1, 1, 0, 704, 100
31964, V, 1, 1, 1, 1, 0, 704, 100
31965, V, 1, 1, 1, 1, 0, 704, 100
31966, V, 1, 1, 1, 1, 0, 704, 100
31967, V, 1, 1, 1, 1, 0, 704, 100
31968, V, 1, 1, 1, 1, 0, 704, 100
31969, V, 1, 1, 1, 1, 0, 704, 100
31970, V, 1, 1, 1, 1, 0, 704, 100
31971, V, 1, 1, 1, 1, 0, 704, 100
31972, V, 1, 1, 1, 1, 0, 704, 100
31973, V, 1, 1, 1, 1, 0, 704, 100
31974, V, 1, 1, 1, 1, 0, 704, 100
31975, V, 1, 1, 1, 1, 0, 704, 100
31976, V, 1, 1, 1, 1, 0, 704, 100
31977, V, 1, 1, 1, 1, 0, 704, 100
31978, V, 1, 1, 1, 1, 0, 704, 100
31979, V, 1, 1, 1, 1, 0, 704, 100
31980, V, 1, 1, 1, 1, 0, 704, 100
31981, V, 1, 1, 1, 1, 0, 704, 100
31982, V, 1, 1, 1, 1, 0, 704, 100
31983, V, 1, 1, 1, 1, 0, 704, 100
31984, V, 1, 1, 1, 1, 0, 704, 100
31985, V, 1, 1, 1, 1, 0, 704, 100
31986, V, 1, 1, 1, 1, 0, 704, 100
31987, V, 1, 1, 1, 1, 0, 704, 100
31988, V, 1, 1, 1, 1, 0, 704, 100
31989, V, 1, 1, 1, 1, 0, 704, 100
31990, V, 1, 1, 1, 1, 0, 704, 100
31991, V, 1, 1, 1, 1, 0, 704, 100
31992, V, 1, 1, 1, 1, 0, 704, 100
31993, V, 1, 1, 1, 1, 0, 704, 100
31994, V, 1, 1, 1, 1, 0, 704, 100
31995, V, 1, 1, 1, 1, 0, 704, 100
31996, V, 1, 1, 1, 1, 0, 704, 100
31997, V, 1, 1, 1, 1, 0, 704, 100
31998, V, 1, 1, 1, 1, 0, 704, 100
32000, V, 1, 1, 1, 1, 0, 704, 100
32001, V, 1, 1, 1, 1, 0, 704, 100
32002, V, 1, 1, 1, 1, 0, 704, 100
32003, V, 1, 1, 1, 1, 0, 704, 100
32004, V, 1, 1, 1, 1, 0, 704, 100
32005, V, 1, 1, 1, 1, 0, 704, 100
32006, V, 1, 1, 1, 1, 0, 704, 100
32007, V, 1, 1, 1, 1, 0, 704, 100
32008, V, 1, 1, 1, 1, 0, 704, 100
32009, V, 1, 1, 1, 1, 0, 704, 100
32010, V, 1, 1, 1, 1, 0, 704, 100
32011, V, 1, 1, 1, 1, 0, 704, 100
32012, V, 1, 1, 1, 1, 0, 704, 100
32013, V, 1, 1, 1, 1, 0, 704, 100
32014, V, 1, 1, 1, 1, 0, 704, 100
32015, V, 1, 1, 1, 1, 0, 704, 100
32016, V, 1, 1, 1, 1, 0, 704, 100
32017, V, 1, 1, 1, 1, 0, 704, 100
32018, V, 1, 1, 1, 1, 0, 704, 100
32019, V, 1, 1, 1, 1, 0, 704, 100
32020, V, 1, 1, 1, 1, 0, 704, 100
32021, V, 1, 1, 1, 1, 0, 704, 100
32022, V, 1, 1, 1, 1, 0, 704, 100
32023, V, 1, 1, 1, 1, 0, 704, 100
32024, V, 1, 1, 1, 1, 0, 704, 100
32025, V, 1, 1, 1, 1, 0, 704, 100
32026, V, 1, 1, 1, 1, 0, 704, 100
32027, V, 1, 1, 1, 1, 0, 704, 100
32028, V, 1, 1, 1, 1, 0, 704, 100
32029, V, 1, 1, 1, 1, 0, 704, 100
32030, V, 1, 1, 1, 1, 0, 704, 100
32031, V, 1, 1, 1, 1, 0, 704, 100
32032, V, 1, 1, 1, 1, 0, 704, 100
32033, V, 1, 1, 1, 1, 0, 704, 100
32034, V, 1, 1, 1, 1, 0, 704, 100
32035, V, 1, 1, 1, 1, 0, 704, 100
32036, V, 1, 1, 1, 1, 0, 704, 100
32037, V, 1, 1, 1, 1, 0, 704, 100
32038, V, 1, 1, 1, 1, 0, 704, 100
32039, V, 1, 1, 1, 1, 0, 704, 100
32040, V, 1, 1, 1, 1, 0, 704, 100
32041, V, 1, 1, 1, 1, 0, 704, 100
32043, V, 1, 1, 1, 1, 0, 704, 100
32044, V, 1, 1, 1, 1, 0, 704, 100
32045, V, 1, 1, 1, 1, 0, 704, 100
32046, V, 1, 1, 1, 1, 0, 704, 100
32047, V, 1, 1, 1, 1, 0, 704, 100
32048, V, 1, 1, 1, 1, 0, 704, 100
32049, V, 1, 1, 1, 1, 0, 704, 100
32050, V, 1, 1, 1, 1, 0, 704, 100
32051, V, 1, 1, 1, 1, 0, 704, 100
32052, V, 1, 1, 1, 1, 0, 704, 100
32053, V, 1, 1, 1, 1, 0, 704, 100
32054, V, 1, 1, 1, 1, 0, 704, 100
32055, V, 1, 1, 1, 1, 0, 704, 100
32056, V, 1, 1, 1, 1, 0, 704, 100
32057, V, 1, 1, 1, 1, 0, 704, 100
32058, V, 1, 1, 1, 1, 0, 704, 100
32059, V, 1, 1, 1, 1, 0, 704, 100
32060, V, 1, 1, 1, 1, 0, 704, 100
32061, V, 1, 1, 1, 1, 0, 704, 100
32062, V, 1, 1, 1, 1, 0, 704, 100
32063, V, 1, 1, 1, 1, 0, 704, 100
32064, V, 1, 1, 1, 1, 0, 704, 100
32065, V, 1, 1, 1, 1, 0, 704, 100
32066, V, 1, 1, 1, 1, 0, 704, 100
32067, V, 1, 1, 1, 1, 0, 704, 100
32068, V, 1, 1, 1, 1, 0, 704, 100
32069, V, 1, 1, 1, 1, 0, 704, 100
32070, V, 1, 1, 1, 1, 0, 704, 100
32071, V, 1, 1, 1, 1, 0, 704, 100
32072, V, 1, 1, 1, 1, 0, 704, 100
32073, V, 1, 1, 1, 1, 0, 704, 100
32074, V, 1, 1, 1, 1, 0, 704, 100
32075, V, 1, 1, 1, 1, 0, 704, 100
32076, V, 1, 1, 1, 1, 0, 704, 100
32077, V, 1, 1, 1, 1, 0, 704, 100
32078, V, 1, 1, 1, 1, 0, 704, 100
32079, V, 1, 1, 1, 1, 0, 704, 100
32080, V, 1, 1, 1, 1, 0, 704, 100
32081, V, 1, 1, 1, 1, 0, 704, 100
32082, V, 1, 1, 1, 1, 0, 704, 100
32083, V, 1, 1, 1, 1, 0, 704, 100
32084, V, 1, 1, 1, 1, 0, 704, 100
32086, V, 1, 1, 1, 1, 0, 704, 100
32087, V, 1, 1, 1, 1, 0, 704, 100
32088, V, 1, 1, 1, 1, 0, 704, 100
32089, V, 1, 1, 1, 1, 0, 704, 100
32090, V, 1, 1, 1, 1, 0, 704, 100
32091, V, 1, 1, 1, 1, 0, 704, 100
32092, V, 1, 1, 1, 1, 0, 704, 100
32093, V, 1, 1, 1, 1, 0, 704, 100
32094, V, 1, 1, 1, 1, 0, 704, 100
32095, V, 1, 1, 1, 1, 0, 704, 100
32096, V, 1, 1, 1, 1, 0, 704, 100
32097, V, 1, 1, 1, 1, 0, 704, 100
32098, V, 1, 1, 1, 1, 0, 704, 100
32099, V, 1, 1, 1, 1, 0, 704, 100
32100, V, 1, 1, 1, 1, 0, 704, 100
32101, V, 1, 1, 1, 1, 0, 704, 100
32102, V, 1, 1, 1, 1, 0, 704, 100
32103, V, 1, 1, 1, 1, 0, 704, 100
32104, V, 1, 1, 1, 1, 0, 704, 100
32105, V, 1, 1, 1, 1, 0, 704, 100
32106, V, 1, 1, 1, 1, 0, 704, 100
32107, V, 1, 1, 1, 1, 0, 704, 100
32108, V, 1, 1, 1, 1, 0, 704, 100
32109, V, 1, 1, 1, 1, 0, 704, 100
32110, V, 1, 1, 1, 1, 0, 704, 100
32111, V, 1, 1, 1, 1, 0, 704, 100
32112, V, 1, 1, 1, 1, 0, 704, 100
32113, V, 1, 1, 1, 1, 0, 704, 100
32114, V, 1, 1, 1, 1, 0, 704, 100
32115, V, 1, 1, 1, 1, 0, 704, 100
32116, V, 1, 1, 1, 1, 0, 704, 100
32117, V, 1, 1, 1, 1, 0, 704, 100
32118, V, 1, 1, 1, 1, 0, 704, 100
32119, V, 1, 1, 1, 1, 0, 704, 100
32120, V, 1, 1, 1, 1, 0, 704, 100
32121, V, 1, 1, 1, 1, 0, 704, 100
32122, V, 1, 1, 1, 1, 0, 704, 100
32123, V, 1, 1, 1, 1, 0, 704, 100
32124, V, 1, 1, 1, 1, 0, 704, 100
32125, V, 1, 1, 1, 1, 0, 704, 100
32126, V, 1, 1, 1, 1, 0, 704, 100
32128, V, 1, 1, 1, 1, 0, 704, 100
32129, V, 1, 1, 1, 1, 0, 704, 100
32130, V, 1, 1, 1, 1, 0, 704, 100
32131, V, 1, 1, 1, 1, 0, 704, 100
32132, V, 1, 1, 1, 1, 0, 704, 100
32133, V, 1, 1, 1, 1, 0, 704, 100
32134, V, 1, 1, 1, 1, 0, 704, 100
32135, V, 1, 1, 1, 1, 0, 704, 100
32136, V, 1, 1, 1, 1, 0, 704, 100
32137, V, 1, 1, 1, 1, 0, 704, 100
32138, V, 1, 1, 1, 1, 0, 704, 100
32139, V, 1, 1, 1, 1, 0, 704, 100
32140, V, 1, 1, 1, 1, 0, 704, 100
32141, V, 1, 1, 1, 1, 0, 704, 100
32142, V, 1, 1, 1, 1, 0, 704, 100
32143, V, 1, 1, 1, 1, 0, 704, 100
32144, V, 1, 1, 1, 1, 0, 704, 100
32145, V, 1, 1, 1, 1, 0, 704, 100
32146, V, 1, 1, 1, 1, 0, 704, 100
32147, V, 1, 1, 1, 1, 0, 704, 100
32148, V, 1, 1, 1, 1, 0, 704, 100
32149, V, 1, 1, 1, 1, 0, 704, 100
32150, V, 1, 1, 1, 1, 0, 704, 100
32151, V, 1, 1, 1, 1, 0, 704, 100
32152, V, 1, 1, 1, 1, 0, 704, 100
32153, V, 1, 1, 1, 1, 0, 704, 100
32154, V, 1, 1, 1, 1, 0, 704, 100
32155, V, 1, 1, 1, 1, 0, 704, 100
32156, V, 1, 1, 1, 1, 0, 704, 100
32157, V, 1, 1, 1, 1, 0, 704, 100
32158, V, 1, 1, 1, 1, 0, 704, 100
32159, V, 1, 1, 1, 1, 0, 704, 100
32160, V, 1, 1, 1, 1, 0, 704, 100
32161, V, 1, 1, 1, 1, 0, 704, 100
32162, V, 1, 1, 1, 1, 0, 704, 100
32163, V, 1, 1, 1, 1, 0, 704, 100
32164, V, 1, 1, 1, 1, 0, 704, 100
32165, V, 1, 1, 1, 1, 0, 704, 100
32166, V, 1, 1, 1, 1, 0, 704, 100
32167, V, 1, 1, 1, 1, 0, 704, 100
32168, V, 1, 1, 1, 1, 0, 704, 100
32169, V, 1, 1, 1, 1, 0, 704, 100
32171, V, 1, 1, 1, 1, 0, 704, 100
32172, V, 1, 1, 1, 1, 0, 704, 100
32173, V, 1, 1, 1, 1, 0, 704, 100
32174, V, 1, 1, 1, 1, 0, 704, 100
32175, V, 1, 1, 1, 1, 0, 704, 100
32176, V, 1, 1, 1, 1, 0, 704, 100
32177, V, 1, 1, 1, 1, 0, 704, 100
32178, V, 1, 1, 1, 1, 0, 704, 100
32179, V, 1, 1, 1, 1, 0, 704, 100
32180, V, 1, 1, 1, 1, 0, 704, 100
32181, V, 1, 1, 1, 1, 0, 704, 100
32182, V, 1, 1, 1, 1, 0, 704, 100
32183, V, 1, 1, 1, 1, 0, 704, 100
32184, V, 1, 1, 1, 1, 0, 704, 100
32185, V, 1, 1, 1, 1, 0, 704, 100
32186, V, 1, 1, 1, 1, 0, 704, 100
32187, V, 1, 1, 1, 1, 0, 704, 100
32188, V, 1, 1, 1, 1, 0, 704, 100
32189, V, 1, 1, 1, 1, 0, 704, 100
32190, V, 1, 1, 1, 1, 0, 704, 100
32191, V, 1, 1, 1, 1, 0, 704, 100
32192, V, 1, 1, 1, 1, 0, 704, 100
32193, V, 1, 1, 1, 1, 0, 704, 100
32194, V, 1, 1, 1, 1, 0, 704, 100
32195, V, 1, 1, 1, 1, 0, 704, 100
32196, V, 1, 1, 1, 1, 0, 704, 100
32197, V, 1, 1, 1, 1, 0, 704, 100
32198, V, 1, 1, 1, 1, 0, 704, 100
32199, V, 1, 1, 1, 1, 0, 704, 100
32200, V, 1, 1, 1, 1, 0, 704, 100
32201, V, 1, 1, 1, 1, 0, 704, 100
32202, V, 1, 1, 1, 1, 0, 704, 100
32203, V, 1, 1, 1, 1, 0, 704, 100
32204, V, 1, 1, 1, 1, 0, 704, 100
32205, V, 1, 1, 1, 1, 0, 704, 100
32206, V, 1, 1, 1, 1, 0, 704, 100
32207, V, 1, 1, 1, 1, 0, 704, 100
32208, V, 1, 1, 1, 1, 0, 704, 100
32209, V, 1, 1, 1, 1, 0, 704, 100
32210, V, 1, 1, 1, 1, 0, 704, 100
32211, V, 1, 1, 1, 1, 0, 704, 100
32212, V, 1, 1, 1, 1, 0, 704, 100
32214, V, 1, 1, 1, 1, 0, 704, 100
32215, V, 1, 1, 1, 1, 0, 704, 100
32216, V, 1, 1, 1, 1, 0, 704, 100
32217, V, 1, 1, 1, 1, 0, 704, 100
32218, V, 1, 1, 1, 1, 0, 704, 100
32219, V, 1, 1, 1, 1, 0, 704, 100
32220, V, 1, 1, 1, 1, 0, 704, 100
32221, V, 1, 1, 1, 1, 0, 704, 100
32222, V, 1, 1, 1, 1, 0, 704, 100
32223, V, 1, 1, 1, 1, 0, 704, 100
32224, V, 1, 1, 1, 1, 0, 704, 100
32225, V, 1, 1, 1, 1, 0, 704, 100
32226, V, 1, 1, 1, 1, 0, 704, 100
32227, V, 1, 1, 1, 1, 0, 704, 100
32228, V, 1, 1, 1, 1, 0, 704, 100
32229, V, 1, 1, 1, 1, 0, 704, 100
32230, V, 1, 1, 1, 1, 0, 704, 100
32231, V, 1, 1, 1, 1, 0, 704, 100
32232, V, 1, 1, 1, 1, 0, 704, 100
32233, V, 1, 1, 1, 1, 0, 704, 100
32234, V, 1, 1, 1, 1, 0, 704, 100
32235, V, 1, 1, 1, 1, 0, 704, 100
32236, V, 1, 1, 1, 1, 0, 704, 100
32237, V, 1, 1, 1, 1, 0, 704, 100
32238, V, 1, 1, 1, 1, 0, 704, 100
32239, V, 1, 1, 1, 1, 0, 704, 100
32240, V, 1, 1, 1, 1, 0, 704, 100
32241, V, 1, 1, 1, 1, 0, 704, 100
32242, V, 1, 1, 1, 1, 0, 704, 100
32243, V, 1, 1, 1, 1, 0, 704, 100
32244, V, 1, 1, 1, 1, 0, 704, 100
32245, V, 1, 1, 1, 1, 0, 704, 100
32246, V, 1, 1, 1, 1, 0, 704, 100
32247, V, 1, 1, 1, 1, 0, 704, 100
32248, V, 1, 1, 1, 1, 0, 704, 100
32249, V, 1, 1, 1, 1, 0, 704, 100
32250, V, 1, 1, 1, 1, 0, 704, 100
32251, V, 1, 1, 1, 1, 0, 704, 100
32252, V, 1, 1, 1, 1, 0, 704, 100
32253, V, 1, 1, 1, 1, 0, 704, 100
32254, V, 1, 1, 1, 1, 0, 704, 100
32256, V, 1, 1, 1, 1, 0, 704, 100
32257, V, 1, 1, 1, 1, 0, 704, 100
32258, V, 1, 1, 1, 1, 0, 704, 100
32259, V, 1, 1, 1, 1, 0, 704, 100
32260, V, 1, 1, 1, 1, 0, 704, 100
32261, V, 1, 1, 1, 1, 0, 704, 100
32262, V, 1, 1, 1, 1, 0, 704, 100
32263, V, 1, 1, 1, 1, 0, 704, 100
32264, V, 1, 1, 1, 1, 0, 704, 100
32265, V, 1, 1, 1, 1, 0, 704, 100
32266, V, 1, 1, 1, 1, 0, 704, 100
32267, V, 1, 1, 1, 1, 0, 704, 100
32268, V, 1, 1, 1, 1, 0, 704, 100
32269, V, 1, 1, 1, 1, 0, 704, 100
32270, V, 1, 1, 1, 1, 0, 704, 100
32271, V, 1, 1, 1, 1, 0, 704, 100
32272, V, 1, 1, 1, 1, 0, 704, 100
32273, V, 1, 1, 1, 1, 0, 704, 100
32274, V, 1, 1, 1, 1, 0, 704, 100
32275, V, 1, 1, 1, 1, 0, 704, 100
32276, V, 1, 1, 1, 1, 0, 704, 100
32277, V, 1, 1, 1, 1, 0, 704, 100
32278, V, 1, 1, 1, 1, 0, 704, 100
32279, V, 1, 1, 1, 1, 0, 704, 100
32280, V, 1, 1, 1, 1, 0, 704, 100
32281, V, 1, 1, 1, 1, 0, 704, 100
32282, V, 1, 1, 1, 1, 0, 704, 100
32283, V, 1, 1, 1, 1, 0, 704, 100
32284, V, 1, 1, 1, 1, 0, 704, 100
32285, V, 1, 1, 1, 1, 0, 704, 100
32286, V, 1, 1, 1, 1, 0, 704, 100
32287, V, 1, 1, 1, 1, 0, 704, 100
32288, V, 1, 1, 1, 1, 0, 704, 100
32289, V, 1, 1, 1, 1, 0, 704, 100
32290, V, 1, 1, 1, 1, 0, 704, 100
32291, V, 1, 1, 1, 1, 0, 704, 100
32292, V, 1, 1, 1, 1, 0, 704, 100
32293, V, 1, 1, 1, 1, 0, 704, 100
32294, V, 1, 1, 1, 1, 0, 704, 100
32295, V, 1, 1, 1, 1, 0, 704, 100
32296, V, 1, 1, 1, 1, 0, 704, 100
32297, V, 1, 1, 1, 1, 0, 704, 100
32299, V, 1, 1, 1, 1, 0, 704, 100
32300, V, 1, 1, 1, 1, 0, 704, 100
32301, V, 1, 1, 1, 1, 0, 704, 100
32302, V, 1, 1, 1, 1, 0, 704, 100
32303, V, 1, 1, 1, 1, 0, 704, 100
32304, V, 1, 1, 1, 1, 0, 704, 100
32305, V, 1, 1, 1, 1, 0, 704, 100
32306, V, 1, 1, 1, 1, 0, 704, 100
32307, V, 1, 1, 1, 1, 0, 704, 100
32308, V, 1, 1, 1, 1, 0, 704, 100
32309, V, 1, 1, 1, 1, 0, 704, 100
32310, V, 1, 1, 1, 1, 0, 704, 100
32311, V, 1, 1, 1, 1, 0, 704, 100
32312, V, 1, 1, 1, 1, 0, 704, 100
32313, V, 1, 1, 1, 1, 0, 704, 100
32314, V, 1, 1, 1, 1, 0, 704, 100
32315, V, 1, 1, 1, 1, 0, 704, 100
32316, V, 1, 1, 1, 1, 0, 704, 100
32317, V, 1, 1, 1, 1, 0, 704, 100
32318, V, 1, 1, 1, 1, 0, 704, 100
32319, V, 1, 1, 1, 1, 0, 704, 100
32320, V, 1, 1, 1, 1, 0, 704, 100
32321, V, 1, 1, 1, 1, 0, 704, 100
32322, V, 1, 1, 1, 1, 0, 704, 100
32323, V, 1, 1, 1, 1, 0, 704, 100
32324, V, 1, 1, 1, 1, 0, 704, 100
32325, V, 1, 1, 1, 1, 0, 704, 100
32326, V, 1, 1, 1, 1, 0, 704, 100
32327, V, 1, 1, 1, 1, 0, 704, 100
32328, V, 1, 1, 1, 1, 0, 704, 100
32329, V, 1, 1, 1, 1, 0, 704, 100
32330, V, 1, 1, 1, 1, 0, 704, 100
32331, V, 1, 1, 1, 1, 0, 704, 100
32332, V, 1, 1, 1, 1, 0, 704, 100
32333, V, 1, 1, 1, 1, 0, 704, 100
32334, V, 1, 1, 1, 1, 0, 704, 100
32335, V, 1, 1, 1, 1, 0, 704, 100
32336, V, 1, 1, 1, 1, 0, 704, 100
32337, V, 1, 1, 1, 1, 0, 704, 100
32338, V, 1, 1, 1, 1, 0, 704, 100
32339, V, 1, 1, 1, 1, 0, 704, 100
32340, V, 1, 1, 1, 1, 0, 704, 100
32342, V, 1, 1, 1, 1, 0, 704, 100
32343, V, 1, 1, 1, 1, 0, 704, 100
32344, V, 1, 1, 1, 1, 0, 704, 100
32345, V, 1, 1, 1, 1, 0, 704, 100
32346, V, 1, 1, 1, 1, 0, 704, 100
32347, V, 1, 1, 1, 1, 0, 704, 100
32348, V, 1, 1, 1, 1, 0, 704, 100
32349, V, 1, 1, 1, 1, 0, 704, 100
32350, V, 1, 1, 1, 1, 0, 704, 100
32351, V, 1, 1, 1, 1, 0, 704, 100
32352, V, 1, 1, 1, 1, 0, 704, 100
32353, V, 1, 1, 1, 1, 0, 704, 100
32354, V, 1, 1, 1, 1, 0, 704, 100
32355, V, 1, 1, 1, 1, 0, 704, 100
32356, V, 1, 1, 1, 1, 0, 704, 100
32357, V, 1, 1, 1, 1, 0, 704, 100
32358, V, 1, 1, 1, 1, 0, 704, 100
32359, V, 1, 0, 0, 1, 0, 704, 100
32359, V, 1, 0, 0, 0, 0, 704, 100
32360, V, 1, 1, 0, 0, 0, 704, 100
32360, V, 1, 1, 0, 0, 0, 704, 100
32361, V, 1, 1, 1, 1, 0, 704, 100
32362, V, 1, 1, 1, 1, 0, 704, 100
32363, V, 1, 1, 1, 1, 0, 704, 100
32364, V, 1, 1, 1, 1, 0, 704, 100
32365, V, 1, 1, 1, 1, 0, 704, 99
32366, V, 1, 1, 1, 1, 0, 704, 99
32367, V, 1, 1, 1, 1, 0, 704, 99
32368, V, 1, 1, 1, 1, 0, 704, 99
32369, V, 1, 1, 1, 1, 0, 704, 99
32370, V, 1, 1, 1, 1, 0, 704, 99
32371, V, 1, 1, 1, 1, 0, 704, 99
32372, V, 1, 1, 1, 1, 0, 704, 99
32373, V, 1, 1, 1, 1, 0, 704, 99
32374, V, 1, 1, 1, 1, 0, 704, 99
32375, V, 1, 1, 1, 1, 0, 704, 99
32376, V, 1, 1, 1, 1, 0, 704, 99
32377, V, 1, 1, 1, 1, 0, 704, 99
32378, V, 1, 1, 1, 1, 0, 704, 99
32379, V, 1, 1, 1, 1, 0, 704, 99
32380, V, 1, 1, 1, 1, 0, 704, 100
32381, V, 1, 1, 1, 1, 0, 704, 100
32382, V, 1, 1, 1, 1, 0, 704, 99
32384, V, 1, 1, 1, 1, 0, 704, 100
32385, V, 1, 1, 1, 1, 0, 704, 99
32386, V, 1, 1, 1, 1, 0, 704, 100
32387, V, 1, 1, 1, 1, 0, 704, 100
32388, V, 1, 1, 1, 1, 0, 704, 100
32389, V, 1, 1, 1, 1, 0, 704, 100
32390, V, 1, 1, 1, 1, 0, 704, 100
32391, V, 1, 1, 1, 1, 0, 704, 100
32392, V, 1, 1, 1, 1, 0, 704, 100
32393, V, 1, 1, 1, 1, 0, 704, 100
32394, V, 1, 1, 1, 1, 0, 704, 100
32395, V, 1, 1, 1, 1, 0, 704, 100
32396, V, 1, 1, 1, 1, 0, 704, 100
32397, V, 1, 1, 1, 1, 0, 704, 100
32398, V, 1, 1, 1, 1, 0, 704, 100
32399, V, 1, 1, 1, 1, 0, 704, 100
32400, V, 1, 1, 1, 1, 0, 704, 100
32401, V, 1, 1, 1, 1, 0, 704, 100
32402, V, 1, 1, 1, 1, 0, 704, 100
32403, V, 1, 1, 1, 1, 0, 704, 100
32404, V, 1, 1, 1, 1, 0, 704, 100
32405, V, 1, 1, 1, 1, 0, 704, 100
32406, V, 1, 1, 1, 1, 0, 704, 100
32407, V, 1, 1, 1, 1, 0, 704, 100
32408, V, 1, 1, 1, 1, 0, 704, 100
32409, V, 1, 1, 1, 1, 0, 704, 100
32410, V, 1, 1, 1, 1, 0, 704, 100
32411, V, 1, 1, 1, 1, 0, 704, 100
32412, V, 1, 1, 1, 1, 0, 704, 100
32413, V, 1, 1, 1, 1, 0, 704, 100
32414, V, 1, 1, 1, 1, 0, 704, 100
32415, V, 1, 1, 1, 1, 0, 704, 100
32416, V, 1, 1, 1, 1, 0, 704, 100
32417, V, 1, 1, 1, 1, 0, 704, 100
32418, V, 1, 1, 1, 1, 0, 704, 100
32419, V, 1, 1, 1, 1, 0, 704, 100
32420, V, 1, 1, 1, 1, 0, 704, 100
32421, V, 1, 1, 1, 1, 0, 704, 100
32422, V, 1, 1, 1, 1, 0, 704, 100
32423, V, 1, 1, 1, 1, 0, 704, 100
32424, V, 1, 1, 1, 1, 0, 704, 100
32425, V, 1, 1, 1, 1, 0, 704, 100
32427, V, 1, 1, 1, 1, 0, 704, 100
32428, V, 1, 1, 1, 1, 0, 704, 100
32429, V, 1, 1, 1, 1, 0, 704, 100
32430, V, 1, 1, 1, 1, 0, 704, 100
32431, V, 1, 1, 1, 1, 0, 704, 100
32432, V, 1, 1, 1, 1, 0, 704, 100
32433, V, 1, 1, 1, 1, 0, 704, 100
32434, V, 1, 1, 1, 1, 0, 704, 100
32435, V, 1, 1, 1, 1, 0, 704, 100
32436, V, 1, 1, 1, 1, 0, 704, 100
32437, V, 1, 1, 1, 1, 0, 704, 100
32438, V, 1, 1, 1, 1, 0, 704, 100
32439, V, 1, 1, 1, 1, 0, 704, 100
32440, V, 1, 1, 1, 1, 0, 704, 100
32441, V, 1, 1, 1, 1, 0, 704, 100
32442, V, 1, 1, 1, 1, 0, 704, 100
32443, V, 1, 1, 1, 1, 0, 704, 100
32444, V, 1, 1, 1, 1, 0, 704, 100
32445, V, 1, 1, 1, 1, 0, 704, 100
32446, V, 1, 1, 1, 1, 0, 704, 100
32447, V, 1, 1, 1, 1, 0, 704, 100
32448, V, 1, 1, 1, 1, 0, 704, 100
32449, V, 1, 1, 1, 1, 0, 704, 100
32450, V, 1, 1, 1, 1, 0, 704, 100
32451, V, 1, 1, 1, 1, 0, 704, 100
32452, V, 1, 1, 1, 1, 0, 704, 100
32453, V, 1, 1, 1, 1, 0, 704, 100
32454, V, 1, 1, 1, 1, 0, 704, 100
32455, V, 1, 1, 1, 1, 0, 704, 100
32456, V, 1, 1, 1, 1, 0, 704, 100
32457, V, 1, 1, 1, 1, 0, 704, 100
32458, V, 1, 1, 1, 1, 0, 704, 100
32459, V, 1, 1, 1, 1, 0, 704, 100
32460, V, 1, 1, 1, 1, 0, 704, 100
32461, V, 1, 1, 1, 1, 0, 704, 100
32462, V, 1, 1, 1, 1, 0, 704, 100
32463, V, 1, 1, 1, 1, 0, 704, 100
32464, V, 1, 1, 1, 1, 0, 704, 100
32465, V, 1, 1, 1, 1, 0, 704, 100
32466, V, 1, 1, 1, 1, 0, 704, 100
32467, V, 1, 1, 1, 1, 0, 704, 100
32468, V, 1, 1, 1, 1, 0, 704, 100
32470, V, 1, 1, 1, 1, 0, 704, 100
32471, V, 1, 1, 1, 1, 0, 704, 100
32472, V, 1, 1, 1, 1, 0, 704, 100
32473, V, 1, 1, 1, 1, 0, 704, 100
32474, V, 1, 1, 1, 1, 0, 704, 100
32475, V, 1, 1, 1, 1, 0, 704, 100
32476, V, 1, 1, 1, 1, 0, 704, 100
32477, V, 1, 1, 1, 1, 0, 704, 100
32478, V, 1, 1, 1, 1, 0, 704, 100
32479, V, 1, 1, 1, 1, 0, 704, 100
32480, V, 1, 1, 1, 1, 0, 704, 100
32481, V, 1, 1, 1, 1, 0, 704, 100
32482, V, 1, 1, 1, 1, 0, 704, 100
32483, V, 1, 1, 1, 1, 0, 704, 100
32484, V, 1, 1, 1, 1, 0, 704, 100
32485, V, 1, 1, 1, 1, 0, 704, 100
32486, V, 1, 1, 1, 1, 0, 704, 100
32487, V, 1, 1, 1, 1, 0, 704, 100
32488, V, 1, 1, 1, 1, 0, 704, 100
32489, V, 1, 1, 1, 1, 0, 704, 100
32490, V, 1, 1, 1, 1, 0, 704, 100
32491, V, 1, 1, 1, 1, 0, 704, 100
32492, V, 1, 1, 1, 1, 0, 704, 100
32493, V, 1, 1, 1, 1, 0, 704, 100
32494, V, 1, 1, 1, 1, 0, 704, 100
32495, V, 1, 1, 1, 1, 0, 704, 100
32496, V, 1, 1, 1, 1, 0, 704, 100
32497, V, 1, 1, 1, 1, 0, 704, 100
32498, V, 1, 1, 1, 1, 0, 704, 100
32499, V, 1, 1, 1, 1, 0, 704, 100
32500, V, 1, 1, 1, 1, 0, 704, 100
32501, V, 1, 1, 1, 1, 0, 704, 100
32502, V, 1, 1, 1, 1, 0, 704, 100
32503, V, 1, 1, 1, 1, 0, 704, 100
32504, V, 1, 1, 1, 1, 0, 704, 100
32505, V, 1, 1, 1, 1, 0, 704, 100
32506, V, 1, 1, 1, 1, 0, 704, 100
32507, V, 1, 1, 1, 1, 0, 704, 100
32508, V, 1, 1, 1, 1, 0, 704, 100
32509, V, 1, 1, 1, 1, 0, 704, 100
32510, V, 1, 1, 1, 1, 0, 704, 100
32512, V, 1, 1, 1, 1, 0, 704, 100
32513, V, 1, 1, 1, 1, 0, 704, 100
32514, V, 1, 1, 1, 1, 0, 704, 100
32515, V, 1, 1, 1, 1, 0, 704, 100
32516, V, 1, 1, 1, 1, 0, 704, 100
32517, V, 1, 1, 1, 1, 0, 704, 100
32518, V, 1, 1, 1, 1, 0, 704, 100
32519, V, 1, 1, 1, 1, 0, 704, 100
32520, V, 1, 1, 1, 1, 0, 704, 100
32521, V, 1, 1, 1, 1, 0, 704, 100
32522, V, 1, 1, 1, 1, 0, 704, 100
32523, V, 1, 1, 1, 1, 0, 704, 100
32524, V, 1, 1, 1, 1, 0, 704, 100
32525, V, 1, 1, 1, 1, 0, 704, 100
32526, V, 1, 1, 1, 1, 0, 704, 100
32527, V, 1, 1, 1, 1, 0, 704, 100
32528, V, 1, 1, 1, 1, 0, 704, 100
32529, V, 1, 1, 1, 1, 0, 704, 100
32530, V, 1, 1, 1, 1, 0, 704, 100
32531, V, 1, 1, 1, 1, 0, 704, 100
32532, V, 1, 1, 1, 1, 0, 704, 100
32533, V, 1, 1, 1, 1, 0, 704, 100
32534, V, 1, 1, 1, 1, 0, 704, 100
32535, V, 1, 1, 1, 1, 0, 704, 100
32536, V, 1, 1, 1, 1, 0, 704, 100
32537, V, 1, 1, 1, 1, 0, 704, 100
32538, V, 1, 1, 1, 1, 0, 704, 100
32539, V, 1, 1, 1, 1, 0, 704, 100
32540, V, 1, 1, 1, 1, 0, 704, 100
32541, V, 1, 1, 1, 1, 0, 704, 100
32542, V, 1, 1, 1, 1, 0, 704, 100
32543, V, 1, 1, 1, 1, 0, 704, 100
32544, V, 1, 1, 1, 1, 0, 704, 100
32545, V, 1, 1, 1, 1, 0, 704, 100
32546, V, 1, 1, 1, 1, 0, 704, 100
32547, V, 1, 1, 1, 1, 0, 704, 100
32548, V, 1, 1, 1, 1, 0, 704, 100
32549, V, 1, 1, 1, 1, 0, 704, 100
32550, V, 1, 1, 1, 1, 0, 704, 100
32551, V, 1, 1, 1, 1, 0, 704, 100
32552, V, 1, 1, 1, 1, 0, 704, 100
32553, V, 1, 1, 1, 1, 0, 704, 100
32555, V, 1, 1, 1, 1, 0, 704, 100
32556, V, 1, 1, 1, 1, 0, 704, 100
32557, V, 1, 1, 1, 1, 0, 704, 100
32558, V, 1, 1, 1, 1, 0, 704, 100
32559, V, 1, 1, 1, 1, 0, 704, 100
32560, V, 1, 1, 1, 1, 0, 704, 100
32561, V, 1, 1, 1, 1, 0, 704, 100
32562, V, 1, 1, 1, 1, 0, 704, 100
32563, V, 1, 1, 1, 1, 0, 704, 100
32564, V, 1, 1, 1, 1, 0, 704, 100
32565, V, 1, 1, 1, 1, 0, 704, 100
32566, V, 1, 1, 1, 1, 0, 704, 100
32567, V, 1, 1, 1, 1, 0, 704, 100
32568, V, 1, 1, 1, 1, 0, 704, 100
32569, V, 1, 1, 1, 1, 0, 704, 100
32570, V, 1, 1, 1, 1, 0, 704, 100
32571, V, 1, 1, 1, 1, 0, 704, 100
32572, V, 1, 1, 1, 1, 0, 704, 100
32573, V, 1, 1, 1, 1, 0, 704, 100
32574, V, 1, 1, 1, 1, 0, 704, 100
32575, V, 1, 1, 1, 1, 0, 704, 100
32576, V, 1, 1, 1, 1, 0, 704, 100
32577, V, 1, 1, 1, 1, 0, 704, 100
32578, V, 1, 1, 1, 1, 0, 704, 100
32579, V, 1, 1, 1, 1, 0, 704, 100
32580, V, 1, 1, 1, 1, 0, 704, 100
32581, V, 1, 1, 1, 1, 0, 704, 100
32582, V, 1, 1, 1, 1, 0, 704, 100
32583, V, 1, 1, 1, 1, 0, 704, 100
32584, V, 1, 1, 1, 1, 0, 704, 100
32585, V, 1, 1, 1, 1, 0, 704, 100
32586, V, 1, 1, 1, 1, 0, 704, 100
32587, V, 1, 1, 1, 1, 0, 704, 100
32588, V, 1, 1, 1, 1, 0, 704, 100
32589, V, 1, 1, 1, 1, 0, 704, 100
32590, V, 1, 1, 1, 1, 0, 704, 100
32591, V, 1, 1, 1, 1, 0, 704, 100
32592, V, 1, 1, 1, 1, 0, 704, 100
32593, V, 1, 1, 1, 1, 0, 704, 100
32594, V, 1, 1, 1, 1, 0, 704, 100
32595, V, 1, 1, 1, 1, 0, 704, 100
32596, V, 1, 1, 1, 1, 0, 704, 100
32598, V, 1, 1, 1, 1, 0, 704, 100
32599, V, 1, 1, 1, 1, 0, 704, 100
32600, V, 1, 1, 1, 1, 0, 704, 100
32601, V, 1, 1, 1, 1, 0, 704, 100
32602, V, 1, 1, 1, 1, 0, 704, 100
32603, V, 1, 1, 1, 1, 0, 704, 100
32604, V, 1, 1, 1, 1, 0, 704, 100
32605, V, 1, 1, 1, 1, 0, 704, 100
32606, V, 1, 1, 1, 1, 0, 704, 100
32607, V, 1, 1, 1, 1, 0, 704, 100
32608, V, 1, 1, 1, 1, 0, 704, 100
32609, V, 1, 1, 1, 1, 0, 704, 100
32610, V, 1, 1, 1, 1, 0, 704, 100
32611, V, 1, 1, 1, 1, 0, 704, 100
32612, V, 1, 1, 1, 1, 0, 704, 100
32613, V, 1, 1, 1, 1, 0, 704, 100
32614, V, 1, 1, 1, 1, 0, 704, 100
32615, V, 1, 1, 1, 1, 0, 704, 100
32616, V, 1, 1, 1, 1, 0, 704, 100
32617, V, 1, 1, 1, 1, 0, 704, 100
32618, V, 1, 1, 1, 1, 0, 704, 100
32619, V, 1, 1, 1, 1, 0, 704, 100
32620, V, 1, 1, 1, 1, 0, 704, 100
32621, V, 1, 1, 1, 1, 0, 704, 100
32622, V, 1, 1, 1, 1, 0, 704, 100
32623, V, 1, 1, 1, 1, 0, 704, 100
32624, V, 1, 1, 1, 1, 0, 704, 100
32625, V, 1, 1, 1, 1, 0, 704, 100
32626, V, 1, 1, 1, 1, 0, 704, 100
32627, V, 1, 1, 1, 1, 0, 704, 100
32628, V, 1, 1, 1, 1, 0, 704, 100
32629, V, 1, 1, 1, 1, 0, 704, 100
32630, V, 1, 1, 1, 1, 0, 704, 100
32631, V, 1, 1, 1, 1, 0, 704, 100
32632, V, 1, 1, 1, 1, 0, 704, 100
32633, V, 1, 1, 1, 1, 0, 704, 100
32634, V, 1, 1, 1, 1, 0, 704, 100
32635, V, 1, 1, 1, 1, 0, 704, 100
32636, V, 1, 1, 1, 1, 0, 704, 100
32637, V, 1, 1, 1, 1, 0, 704, 100
32638, V, 1, 1, 1, 1, 0, 704, 100
32640, V, 1, 1, 1, 1, 0, 704, 100
32641, V, 1, 1, 1, 1, 0, 704, 100
32642, V, 1, 1, 1, 1, 0, 704, 100
32643, V, 1, 1, 1, 1, 0, 704, 100
32644, V, 1, 1, 1, 1, 0, 704, 100
32645, V, 1, 1, 1, 1, 0, 704, 100
32646, V, 1, 1, 1, 1, 0, 704, 100
32647, V, 1, 1, 1, 1, 0, 704, 100
32648, V, 1, 1, 1, 1, 0, 704, 100
32649, V, 1, 1, 1, 1, 0, 704, 100
32650, V, 1, 1, 1, 1, 0, 704, 100
32651, V, 1, 1, 1, 1, 0, 704, 100
32652, V, 1, 1, 1, 1, 0, 704, 100
32653, V, 1, 1, 1, 1, 0, 704, 100
32654, V, 1, 1, 1, 1, 0, 704, 100
32655, V, 1, 1, 1, 1, 0, 704, 100
32656, V, 1, 1, 1, 1, 0, 704, 100
32657, V, 1, 1, 1, 1, 0, 704, 100
32658, V, 1, 1, 1, 1, 0, 704, 100
32659, V, 1, 1, 1, 1, 0, 704, 100
32660, V, 1, 1, 1, 1, 0, 704, 100
32661, V, 1, 1, 1, 1, 0, 704, 100
32662, V, 1, 1, 1, 1, 0, 704, 100
32663, V, 1, 1, 1, 1, 0, 704, 100
32664, V, 1, 1, 1, 1, 0, 704, 100
32665, V, 1, 1, 1, 1, 0, 704, 100
32666, V, 1, 1, 1, 1, 0, 704, 100
32667, V, 1, 1, 1, 1, 0, 704, 100
32668, V, 1, 1, 1, 1, 0, 704, 100
32669, V, 1, 1, 1, 1, 0, 704, 100
32670, V, 1, 1, 1, 1, 0, 704, 100
32671, V, 1, 1, 1, 1, 0, 704, 100
32672, V, 1, 1, 1, 1, 0, 704, 100
32673, V, 1, 1, 1, 1, 0, 704, 100
32674, V, 1, 1, 1, 1, 0, 704, 100
32675, V, 1, 1, 1, 1, 0, 704, 100
32676, V, 1, 1, 1, 1, 0, 704, 100
32677, V, 1, 1, 1, 1, 0, 704, 100
32678, V, 1, 1, 1, 1, 0, 704, 100
32679, V, 1, 1, 1, 1, 0, 704, 100
32680, V, 1, 1, 1, 1, 0, 704, 100
32681, V, 1, 1, 1, 1, 0, 704, 100
32683, V, 1, 1, 1, 1, 0, 704, 100
32684, V, 1, 1, 1, 1, 0, 704, 100
32685, V, 1, 1, 1, 1, 0, 704, 100
32686, V, 1, 1, 1, 1, 0, 704, 100
32687, V, 1, 1, 1, 1, 0, 704, 100
32688, V, 1, 1, 1, 1, 0, 704, 100
32689, V, 1, 1, 1, 1, 0, 704, 100
32690, V, 1, 1, 1, 1, 0, 704, 100
32691, V, 1, 1, 1, 1, 0, 704, 100
32692, V, 1, 1, 1, 1, 0, 704, 100
32693, V, 1, 1, 1, 1, 0, 704, 100
32694, V, 1, 1, 1, 1, 0, 704, 100
32695, V, 1, 1, 1, 1, 0, 704, 100
32696, V, 1, 1, 1, 1, 0, 704, 100
32697, V, 1, 1, 1, 1, 0, 704, 100
32698, V, 1, 1, 1, 1, 0, 704, 100
32699, V, 1, 1, 1, 1, 0, 704, 100
32700, V, 1, 1, 1, 1, 0, 704, 100
32701, V, 1, 1, 1, 1, 0, 704, 100
32702, V, 1, 1, 1, 1, 0, 704, 100
32703, V, 1, 1, 1, 1, 0, 704, 100
32704, V, 1, 1, 1, 1, 0, 704, 100
32705, V, 1, 1, 1, 1, 0, 704, 100
32706, V, 1, 1, 1, 1, 0, 704, 100
32707, V, 1, 1, 1, 1, 0, 704, 100
32708, V, 1, 1, 1, 1, 0, 704, 100
32709, V, 1, 1, 1, 1, 0, 704, 100
32710, V, 1, 1, 1, 1, 0, 704, 100
32711, V, 1, 1, 1, 1, 0, 704, 100
32712, V, 1, 1, 1, 1, 0, 704, 100
32713, V, 1, 1, 1, 1, 0, 704, 100
32714, V, 1, 1, 1, 1, 0, 704, 100
32715, V, 1, 1, 1, 1, 0, 704, 100
32716, V, 1, 1, 1, 1, 0, 704, 100
32717, V, 1, 1, 1, 1, 0, 704, 100
32718, V, 1, 1, 1, 1, 0, 704, 100
32719, V, 1, 1, 1, 1, 0, 704, 100
32720, V, 1, 1, 1, 1, 0, 704, 100
32721, V, 1, 1, 1, 1, 0, 704, 100
32722, V, 1, 1, 1, 1, 0, 704, 100
32723, V, 1, 1, 1, 1, 0, 704, 100
32724, V, 1, 1, 1, 1, 0, 704, 100
32726, V, 1, 1, 1, 1, 0, 704, 100
32727, V, 1, 1, 1, 1, 0, 704, 100
32728, V, 1, 1, 1, 1, 0, 704, 100
32729, V, 1, 1, 1, 1, 0, 704, 100
32730, V, 1, 1, 1, 1, 0, 704, 100
32731, V, 1, 1, 1, 1, 0, 704, 100
32732, V, 1, 1, 1, 1, 0, 704, 100
32733, V, 1, 1, 1, 1, 0, 704, 100
32734, V, 1, 1, 1, 1, 0, 704, 100
32735, V, 1, 1, 1, 1, 0, 704, 100
32736, V, 1, 1, 1, 1, 0, 704, 100
32737, V, 1, 1, 1, 1, 0, 704, 100
32738, V, 1, 1, 1, 1, 0, 704, 100
32739, V, 1, 1, 1, 1, 0, 704, 100
32740, V, 1, 1, 1, 1, 0, 704, 100
32741, V, 1, 1, 1, 1, 0, 704, 100
32742, V, 1, 1, 1, 1, 0, 704, 100
32743, V, 1, 1, 1, 1, 0, 704, 100
32744, V, 1, 1, 1, 1, 0, 704, 100
32745, V, 1, 1, 1, 1, 0, 704, 100
32746, V, 1, 1, 1, 1, 0, 704, 100
32747, V, 1, 1, 1, 1, 0, 704, 100
32748, V, 1, 1, 1, 1, 0, 704, 100
32749, V, 1, 1, 1, 1, 0, 704, 100
32750, V, 1, 1, 1, 1, 0, 704, 100
32751, V, 1, 1, 1, 1, 0, 704, 100
32752, V, 1, 1, 1, 1, 0, 704, 100
32753, V, 1, 1, 1, 1, 0, 704, 100
32754, V, 1, 1, 1, 1, 0, 704, 100
32755, V, 1, 1, 1, 1, 0, 704, 100
32756, V, 1, 1, 1, 1, 0, 704, 100
32757, V, 1, 1, 1, 1, 0, 704, 100
32758, V, 1, 1, 1, 1, 0, 704, 100
32759, V, 1, 1, 1, 1, 0, 704, 100
32760, V, 1, 1, 1, 1, 0, 704, 100
32761, V, 1, 1, 1, 1, 0, 704, 100
32762, V, 1, 1, 1, 1, 0, 704, 100
32763, V, 1, 1, 1, 1, 0, 704, 100
32764, V, 1, 1, 1, 1, 0, 704, 100
32765, V, 1, 1, 1, 1, 0, 704, 100
32766, V, 1, 1, 1, 1, 0, 704, 100
32768, V, 1, 1, 1, 1, 0, 704, 100
32769, V, 1, 1, 1, 1, 0, 704, 100
32770, V, 1, 1, 1, 1, 0, 704, 100
32771, V, 1, 1, 1, 1, 0, 704, 100
32772, V, 1, 1, 1, 1, 0, 704, 100
32773, V, 1, 1, 1, 1, 0, 704, 100
32774, V, 1, 1, 1, 1, 0, 704, 100
32775, V, 1, 1, 1, 1, 0, 704, 100
32776, V, 1, 1, 1, 1, 0, 704, 100
32777, V, 1, 1, 1, 1, 0, 704, 100
32778, V, 1, 1, 1, 1, 0, 704, 100
32779, V, 1, 1, 1, 1, 0, 704, 100
32780, V, 1, 1, 1, 1, 0, 704, 100
32781, V, 1, 1, 1, 1, 0, 704, 100
32782, V, 1, 1, 1, 1, 0, 704, 100
32783, V, 1, 1, 1, 1, 0, 704, 100
32784, V, 1, 1, 1, 1, 0, 704, 100
32785, V, 1, 1, 1, 1, 0, 704, 100
32786, V, 1, 1, 1, 1, 0, 704, 100
32787, V, 1, 1, 1, 1, 0, 704, 100
32788, V, 1, 1, 1, 1, 0, 704, 100
32789, V, 1, 1, 1, 1, 0, 704, 100
32790, V, 1, 1, 1, 1, 0, 704, 100
32791, V, 1, 1, 1, 1, 0, 704, 100
32792, V, 1, 1, 1, 1, 0, 704, 100
32793, V, 1, 1, 1, 1, 0, 704, 100
32794, V, 1, 1, 1, 1, 0, 704, 100
32795, V, 1, 1, 1, 1, 0, 704, 100
32796, V, 1, 1, 1, 1, 0, 704, 100
32797, V, 1, 1, 1, 1, 0, 704, 100
32798, V, 1, 1, 1, 1, 0, 704, 100
32799, V, 1, 1, 1, 1, 0, 704, 100
32800, V, 1, 1, 1, 1, 0, 704, 100
32801, V, 1, 1, 1, 1, 0, 704, 100
32802, V, 1, 1, 1, 1, 0, 704, 100
32803, V, 1, 1, 1, 1, 0, 704, 100
32804, V, 1, 1, 1, 1, 0, 704, 100
32805, V, 1, 1, 1, 1, 0, 704, 100
32806, V, 1, 1, 1, 1, 0, 704, 100
32807, V, 1, 1, 1, 1, 0, 704, 100
32808, V, 1, 1, 1, 1, 0, 704, 100
32809, V, 1, 1, 1, 1, 0, 704, 100
32811, V, 1, 1, 1, 1, 0, 704, 100
32812, V, 1, 1, 1, 1, 0, 704, 100
32813, V, 1, 1, 1, 1, 0, 704, 100
32814, V, 1, 1, 1, 1, 0, 704, 100
32815, V, 1, 1, 1, 1, 0, 704, 100
32816, V, 1, 1, 1, 1, 0, 704, 100
32817, V, 1, 1, 1, 1, 0, 704, 100
32818, V, 1, 1, 1, 1, 0, 704, 100
32819, V, 1, 1, 1, 1, 0, 704, 100
32820, V, 1, 1, 1, 1, 0, 704, 100
32821, V, 1, 1, 1, 1, 0, 704, 100
32822, V, 1, 1, 1, 1, 0, 704, 100
32823, V, 1, 1, 1, 1, 0, 704, 100
32824, V, 1, 1, 1, 1, 0, 704, 100
32825, V, 1, 1, 1, 1, 0, 704, 100
32826, V, 1, 1, 1, 1, 0, 704, 100
32827, V, 1, 1, 1, 1, 0, 704, 100
32828, V, 1, 1, 1, 1, 0, 704, 100
32829, V, 1, 1, 1, 1, 0, 704, 100
32830, V, 1, 1, 1, 1, 0, 704, 100
32831, V, 1, 1, 1, 1, 0, 704, 100
32832, V, 1, 1, 1, 1, 0, 704, 100
32833, V, 1, 1, 1, 1, 0, 704, 100
32834, V, 1, 1, 1, 1, 0, 704, 100
32835, V, 1, 1, 1, 1, 0, 704, 100
32836, V, 1, 1, 1, 1, 0, 704, 100
32837, V, 1, 1, 1, 1, 0, 704, 100
32838, V, 1, 1, 1, 1, 0, 704, 100
32839, V, 1, 1, 1, 1, 0, 704, 100
32840, V, 1, 1, 1, 1, 0, 704, 100
32841, V, 1, 1, 1, 1, 0, 704, 100
32842, V, 1, 1, 1, 1, 0, 704, 100
32843, V, 1, 1, 1, 1, 0, 704, 100
32844, V, 1, 1, 1, 1, 0, 704, 100
32845, V, 1, 1, 1, 1, 0, 704, 100
32846, V, 1, 1, 1, 1, 0, 704, 100
32847, V, 1, 1, 1, 1, 0, 704, 100
32848, V, 1, 1, 1, 1, 0, 704, 100
32849, V, 1, 1, 1, 1, 0, 704, 100
32850, V, 1, 1, 1, 1, 0, 704, 100
32851, V, 1, 1, 1, 1, 0, 704, 100
32852, V, 1, 1, 1, 1, 0, 704, 100
32854, V, 1, 1, 1, 1, 0, 704, 100
32855, V, 1, 1, 1, 1, 0, 704, 100
32856, V, 1, 1, 1, 1, 0, 704, 100
32857, V, 1, 1, 1, 1, 0, 704, 100
32858, V, 1, 1, 1, 1, 0, 704, 100
32859, V, 1, 1, 1, 1, 0, 704, 100
32860, V, 1, 1, 1, 1, 0, 704, 100
32861, V, 1, 1, 1, 1, 0, 704, 100
32862, V, 1, 1, 1, 1, 0, 704, 100
32863, V, 1, 1, 1, 1, 0, 704, 100
32864, V, 1, 1, 1, 1, 0, 704, 100
32865, V, 1, 1, 1, 1, 0, 704, 100
32866, V, 1, 1, 1, 1, 0, 704, 100
32867, V, 1, 1, 1, 1, 0, 704, 100
32868, V, 1, 1, 1, 1, 0, 704, 100
32869, V, 1, 1, 1, 1, 0, 704, 100
32870, V, 1, 1, 1, 1, 0, 704, 100
32871, V, 1, 1, 1, 1, 0, 704, 100
32872, V, 1, 1, 1, 1, 0, 704, 100
32873, V, 1, 1, 1, 1, 0, 704, 100
32874, V, 1, 1, 1, 1, 0, 704, 100
32875, V, 1, 1, 1, 1, 0, 704, 100
32876, V, 1, 1, 1, 1, 0, 704, 100
32877, V, 1, 1, 1, 1, 0, 704, 100
32878, V, 1, 1, 1, 1, 0, 704, 100
32879, V, 1, 1, 1, 1, 0, 704, 100
32880, V, 1, 1, 1, 1, 0, 704, 100
32881, V, 1, 1, 1, 1, 0, 704, 100
32882, V, 1, 1, 1, 1, 0, 704, 100
32883, V, 1, 1, 1, 1, 0, 704, 100
32884, V, 1, 1, 1, 1, 0, 704, 100
32885, V, 1, 1, 1, 1, 0, 704, 100
32886, V, 1, 1, 1, 1, 0, 704, 100
32887, V, 1, 1, 1, 1, 0, 704, 100
32888, V, 1, 1, 1, 1, 0, 704, 100
32889, V, 1, 1, 1, 1, 0, 704, 100
32890, V, 1, 1, 1, 1, 0, 704, 100
32891, V, 1, 1, 1, 1, 0, 704, 100
32892, V, 1, 1, 1, 1, 0, 704, 100
32893, V, 1, 1, 1, 1, 0, 704, 100
32894, V, 1, 1, 1, 1, 0, 704, 100
32896, V, 1, 1, 1, 1, 0, 704, 100
32897, V, 1, 1, 1, 1, 0, 704, 100
32898, V, 1, 1, 1, 1, 0, 704, 100
32899, V, 1, 1, 1, 1, 0, 704, 100
32900, V, 1, 1, 1, 1, 0, 704, 100
32901, V, 1, 1, 1, 1, 0, 704, 100
32902, V, 1, 1, 1, 1, 0, 704, 100
32903, V, 1, 1, 1, 1, 0, 704, 100
32904, V, 1, 1, 1, 1, 0, 704, 100
32905, V, 1, 1, 1, 1, 0, 704, 100
32906, V, 1, 1, 1, 1, 0, 704, 100
32907, V, 1, 1, 1, 1, 0, 704, 100
32908, V, 1, 1, 1, 1, 0, 704, 100
32909, V, 1, 1, 1, 1, 0, 704, 100
32910, V, 1, 1, 1, 1, 0, 704, 100
32911, V, 1, 1, 1, 1, 0, 704, 100
32912, V, 1, 1, 1, 1, 0, 704, 100
32913, V, 1, 1, 1, 1, 0, 704, 100
32914, V, 1, 1, 1, 1, 0, 704, 100
32915, V, 1, 1, 1, 1, 0, 704, 100
32916, V, 1, 1, 1, 1, 0, 704, 100
32917, V, 1, 1, 1, 1, 0, 704, 100
32918, V, 1, 1, 1, 1, 0, 704, 100
32919, V, 1, 1, 1, 1, 0, 704, 100
32920, V, 1, 1, 1, 1, 0, 704, 100
32921, V, 1, 1, 1, 1, 0, 704, 100
32922, V, 1, 1, 1, 1, 0, 704, 100
32923, V, 1, 1, 1, 1, 0, 704, 100
32924, V, 1, 1, 1, 1, 0, 704, 100
32925, V, 1, 1, 1, 1, 0, 704, 100
32926, V, 1, 1, 1, 1, 0, 704, 100
32927, V, 1, 1, 1, 1, 0, 704, 100
32928, V, 1, 1, 1, 1, 0, 704, 100
32929, V, 1, 1, 1, 1, 0, 704, 100
32930, V, 1, 1, 1, 1, 0, 704, 100
32931, V, 1, 1, 1, 1, 0, 704, 100
32932, V, 1, 1, 1, 1, 0, 704, 100
32933, V, 1, 1, 1, 1, 0, 704, 100
32934, V, 1, 1, 1, 1, 0, 704, 100
32935, V, 1, 1, 1, 1, 0, 704, 100
32936, V, 1, 1, 1, 1, 0, 704, 100
32937, V, 1, 1, 1, 1, 0, 704, 100
32939, V, 1, 1, 1, 1, 0, 704, 100
32940, V, 1, 1, 1, 1, 0, 704, 100
32941, V, 1, 1, 1, 1, 0, 704, 100
32942, V, 1, 1, 1, 1, 0, 704, 100
32943, V, 1, 1, 1, 1, 0, 704, 100
32944, V, 1, 1, 1, 1, 0, 704, 100
32945, V, 1, 1, 1, 1, 0, 704, 100
32946, V, 1, 1, 1, 1, 0, 704, 100
32947, V, 1, 1, 1, 1, 0, 704, 100
32948, V, 1, 1, 1, 1, 0, 704, 100
32949, V, 1, 1, 1, 1, 0, 704, 100
32950, V, 1, 1, 1, 1, 0, 704, 100
32951, V, 1, 1, 1, 1, 0, 704, 100
32952, V, 1, 1, 1, 1, 0, 704, 100
32953, V, 1, 1, 1, 1, 0, 704, 100
32954, V, 1, 1, 1, 1, 0, 704, 100
32955, V, 1, 1, 1, 1, 0, 704, 100
32956, V, 1, 1, 1, 1, 0, 704, 100
32957, V, 1, 1, 1, 1, 0, 704, 100
32958, V, 1, 1, 1, 1, 0, 704, 100
32959, V, 1, 1, 1, 1, 0, 704, 100
32960, V, 1, 1, 1, 1, 0, 704, 100
32961, V, 1, 1, 1, 1, 0, 704, 100
32962, V, 1, 1, 1, 1, 0, 704, 100
32963, V, 1, 1, 1, 1, 0, 704, 100
32964, V, 1, 1, 1, 1, 0, 704, 100
32965, V, 1, 1, 1, 1, 0, 704, 100
32966, V, 1, 1, 1, 1, 0, 704, 100
32967, V, 1, 1, 1, 1, 0, 704, 100
32968, V, 1, 1, 1, 1, 0, 704, 100
32969, V, 1, 1, 1, 1, 0, 704, 100
32970, V, 1, 1, 1, 1, 0, 704, 100
32971, V, 1, 1, 1, 1, 0, 704, 100
32972, V, 1, 1, 1, 1, 0, 704, 100
32973, V, 1, 1, 1, 1, 0, 704, 100
32974, V, 1, 1, 1, 1, 0, 704, 100
32975, V, 1, 1, 1, 1, 0, 704, 100
32976, V, 1, 1, 1, 1, 0, 704, 100
32977, V, 1, 1, 1, 1, 0, 704, 100
32978, V, 1, 1, 1, 1, 0, 704, 100
32979, V, 1, 1, 1, 1, 0, 704, 100
32980, V, 1, 1, 1, 1, 0, 704, 100
32982, V, 1, 1, 1, 1, 0, 704, 100
32983, V, 1, 1, 1, 1, 0, 704, 100
32984, V, 1, 1, 1, 1, 0, 704, 100
32985, V, 1, 1, 1, 1, 0, 704, 100
32986, V, 1, 1, 1, 1, 0, 704, 100
32987, V, 1, 1, 1, 1, 0, 704, 100
32988, V, 1, 1, 1, 1, 0, 704, 100
32989, V, 1, 1, 1, 1, 0, 704, 100
32990, V, 1, 1, 1, 1, 0, 704, 100
32991, V, 1, 1, 1, 1, 0, 704, 100
32992, V, 1, 1, 1, 1, 0, 704, 100
32993, V, 1, 1, 1, 1, 0, 704, 100
32994, V, 1, 1, 1, 1, 0, 704, 100
32995, V, 1, 1, 1, 1, 0, 704, 100
32996, V, 1, 1, 1, 1, 0, 704, 100
32997, V, 1, 1, 1, 1, 0, 704, 100
32998, V, 1, 1, 1, 1, 0, 704, 100
32999, V, 1, 1, 1, 1, 0, 704, 100
33000, V, 1, 1, 1, 1, 0, 704, 100
33001, V, 1, 1, 1, 1, 0, 704, 100
33002, V, 1, 1, 1, 1, 0, 704, 100
33003, V, 1, 1, 1, 1, 0, 704, 100
33004, V, 1, 1, 1, 1, 0, 704, 100
33005, V, 1, 1, 1, 1, 0, 704, 100
33006, V, 1, 1, 1, 1, 0, 704, 100
33007, V, 1, 1, 1, 1, 0, 704, 100
33008, V, 1, 1, 1, 1, 0, 704, 100
33009, V, 1, 1, 1, 1, 0, 704, 100
33010, V, 1, 1, 1, 1, 0, 704, 100
33011, V, 1, 1, 1, 1, 0, 704, 100
33012, V, 1, 1, 1, 1, 0, 704, 100
33013, V, 1, 1, 1, 1, 0, 704, 100
33014, V, 1, 1, 1, 1, 0, 704, 100
33015, V, 1, 1, 1, 1, 0, 704, 100
33016, V, 1, 1, 1, 1, 0, 704, 100
33017, V, 1, 1, 1, 1, 0, 704, 100
33018, V, 1, 1, 1, 1, 0, 704, 100
33019, V, 1, 1, 1, 1, 0, 704, 100
33020, V, 1, 1, 1, 1, 0, 704, 100
33021, V, 1, 1, 1, 1, 0, 704, 100
33022, V, 1, 1, 1, 1, 0, 704, 100
33024, V, 1, 1, 1, 1, 0, 704, 100
33025, V, 1, 1, 1, 1, 0, 704, 100
33026, V, 1, 1, 1, 1, 0, 704, 100
33027, V, 1, 1, 1, 1, 0, 704, 100
33028, V, 1, 1, 1, 1, 0, 704, 100
33029, V, 1, 1, 1, 1, 0, 704, 100
33030, V, 1, 1, 1, 1, 0, 704, 100
33031, V, 1, 1, 1, 1, 0, 704, 100
33032, V, 1, 1, 1, 1, 0, 704, 100
33033, V, 1, 1, 1, 1, 0, 704, 100
33034, V, 1, 1, 1, 1, 0, 704, 100
33035, V, 1, 1, 1, 1, 0, 704, 100
33036, V, 1, 1, 1, 1, 0, 704, 100
33037, V, 1, 1, 1, 1, 0, 704, 100
33038, V, 1, 1, 1, 1, 0, 704, 100
33039, V, 1, 1, 1, 1, 0, 704, 100
33040, V, 1, 1, 1, 1, 0, 704, 100
33041, V, 1, 1, 1, 1, 0, 704, 100
33042, V, 1, 1, 1, 1, 0, 704, 100
33043, V, 1, 1, 1, 1, 0, 704, 100
33044, V, 1, 1, 1, 1, 0, 704, 100
33045, V, 1, 1, 1, 1, 0, 704, 100
33046, V, 1, 1, 1, 1, 0, 704, 100
33047, V, 1, 1, 1, 1, 0, 704, 100
33048, V, 1, 1, 1, 1, 0, 704, 100
33049, V, 1, 1, 1, 1, 0, 704, 100
33050, V, 1, 1, 1, 1, 0, 704, 100
33051, V, 1, 1, 1, 1, 0, 704, 100
33052, V, 1, 1, 1, 1, 0, 704, 100
33053, V, 1, 1, 1, 1, 0, 704, 100
33054, V, 1, 1, 1, 1, 0, 704, 100
33055, V, 1, 1, 1, 1, 0, 704, 100
33056, V, 1, 1, 1, 1, 0, 704, 100
33057, V, 1, 1, 1, 1, 0, 704, 100
33058, V, 1, 1, 1, 1, 0, 704, 100
33059, V, 1, 1, 1, 1, 0, 704, 100
33060, V, 1, 1, 1, 1, 0, 704, 100
33061, V, 1, 1, 1, 1, 0, 704, 100
33062, V, 1, 1, 1, 1, 0, 704, 100
33063, V, 1, 1, 1, 1, 0, 704, 100
33064, V, 1, 1, 1, 1, 0, 704, 100
33065, V, 1, 1, 1, 1, 0, 704, 100
33067, V, 1, 1, 1, 1, 0, 704, 100
33068, V, 1, 1, 1, 1, 0, 704, 100
33069, V, 1, 1, 1, 1, 0, 704, 100
33070, V, 1, 1, 1, 1, 0, 704, 100
33071, V, 1, 1, 1, 1, 0, 704, 100
33072, V, 1, 1, 1, 1, 0, 704, 100
33073, V, 1, 1, 1, 1, 0, 704, 100
33074, V, 1, 1, 1, 1, 0, 704, 100
33075, V, 1, 1, 1, 1, 0, 704, 100
33076, V, 1, 1, 1, 1, 0, 704, 100
33077, V, 1, 1, 1, 1, 0, 704, 100
33078, V, 1, 1, 1, 1, 0, 704, 100
33079, V, 1, 1, 1, 1, 0, 704, 100
33080, V, 1, 1, 1, 1, 0, 704, 100
33081, V, 1, 1, 1, 1, 0, 704, 100
33082, V, 1, 1, 1, 1, 0, 704, 100
33083, V, 1, 1, 1, 1, 0, 704, 100
33084, V, 1, 1, 1, 1, 0, 704, 100
33085, V, 1, 1, 1, 1, 0, 704, 100
33086, V, 1, 1, 1, 1, 0, 704, 100
33087, V, 1, 1, 1, 1, 0, 704, 100
33088, V, 1, 1, 1, 1, 0, 704, 100
33089, V, 1, 1, 1, 1, 0, 704, 100
33090, V, 1, 1, 1, 1, 0, 704, 100
33091, V, 1, 1, 1, 1, 0, 704, 100
33092, V, 1, 1, 1, 1, 0, 704, 100
33093, V, 1, 1, 1, 1, 0, 704, 100
33094, V, 1, 1, 1, 1, 0, 704, 100
33095, V, 1, 1, 1, 1, 0, 704, 100
33096, V, 1, 1, 1, 1, 0, 704, 100
33097, V, 1, 1, 1, 1, 0, 704, 100
33098, V, 1, 1, 1, 1, 0, 704, 100
33099, V, 1, 1, 1, 1, 0, 704, 100
33100, V, 1, 1, 1, 1, 0, 704, 100
33101, V, 1, 1, 1, 1, 0, 704, 100
33102, V, 1, 1, 1, 1, 0, 704, 100
33103, V, 1, 1, 1, 1, 0, 704, 100
33104, V, 1, 1, 1, 1, 0, 704, 100
33105, V, 1, 1, 1, 1, 0, 704, 100
33106, V, 1, 1, 1, 1, 0, 704, 100
33107, V, 1, 1, 1, 1, 0, 704, 100
33108, V, 1, 1, 1, 1, 0, 704, 100
33110, V, 1, 1, 1, 1, 0, 704, 100
33111, V, 1, 1, 1, 1, 0, 704, 100
33112, V, 1, 1, 1, 1, 0, 704, 100
33113, V, 1, 1, 1, 1, 0, 704, 100
33114, V, 1, 1, 1, 1, 0, 704, 100
33115, V, 1, 1, 1, 1, 0, 704, 100
33116, V, 1, 1, 1, 1, 0, 704, 100
33117, V, 1, 1, 1, 1, 0, 704, 100
33118, V, 1, 1, 1, 1, 0, 704, 100
33119, V, 1, 1, 1, 1, 0, 704, 100
33120, V, 1, 1, 1, 1, 0, 704, 100
33121, V, 1, 1, 1, 1, 0, 704, 100
33122, V, 1, 1, 1, 1, 0, 704, 100
33123, V, 1, 1, 1, 1, 0, 704, 100
33124, V, 1, 1, 1, 1, 0, 704, 100
33125, V, 1, 1, 1, 1, 0, 704, 100
33126, V, 1, 1, 1, 1, 0, 704, 100
33127, V, 1, 1, 1, 1, 0, 704, 100
33128, V, 1, 1, 1, 1, 0, 704, 100
33129, V, 1, 1, 1, 1, 0, 704, 100
33130, V, 1, 1, 1, 1, 0, 704, 100
33131, V, 1, 1, 1, 1, 0, 704, 100
33132, V, 1, 1, 1, 1, 0, 704, 100
33133, V, 1, 1, 1, 1, 0, 704, 100
33134, V, 1, 1, 1, 1, 0, 704, 100
33135, V, 1, 1, 1, 1, 0, 704, 100
33136, V, 1, 1, 1, 1, 0, 704, 100
33137, V, 1, 1, 1, 1, 0, 704, 100
33138, V, 1, 1, 1, 1, 0, 704, 100
33139, V, 1, 1, 1, 1, 0, 704, 100
33140, V, 1, 1, 1, 1, 0, 704, 100
33141, V, 1, 1, 1, 1, 0, 704, 100
33142, V, 1, 1, 1, 1, 0, 704, 100
33143, V, 1, 1, 1, 1, 0, 704, 100
33144, V, 1, 1, 1, 1, 0, 704, 100
33145, V, 1, 1, 1, 1, 0, 704, 100
33146, V, 1, 1, 1, 1, 0, 704, 100
33147, V, 1, 1, 1, 1, 0, 704, 100
33148, V, 1, 1, 1, 1, 0, 704, 100
33149, V, 1, 1, 1, 1, 0, 704, 100
33150, V, 1, 1, 1, 1, 0, 704, 100
33152, V, 1, 1, 1, 1, 0, 704, 100
33153, V, 1, 1, 1, 1, 0, 704, 100
33154, V, 1, 1, 1, 1, 0, 704, 100
33155, V, 1, 1, 1, 1, 0, 704, 100
33156, V, 1, 1, 1, 1, 0, 704, 100
33157, V, 1, 1, 1, 1, 0, 704, 100
33158, V, 1, 1, 1, 1, 0, 704, 100
33159, V, 1, 1, 1, 1, 0, 704, 100
33160, V, 1, 1, 1, 1, 0, 704, 100
33161, V, 1, 1, 1, 1, 0, 704, 100
33162, V, 1, 1, 1, 1, 0, 704, 100
33163, V, 1, 1, 1, 1, 0, 704, 100
33164, V, 1, 1, 1, 1, 0, 704, 100
33165, V, 1, 1, 1, 1, 0, 704, 100
33166, V, 1, 1, 1, 1, 0, 704, 100
33167, V, 1, 1, 1, 1, 0, 704, 100
33168, V, 1, 1, 1, 1, 0, 704, 100
33169, V, 1, 1, 1, 1, 0, 704, 100
33170, V, 1, 1, 1, 1, 0, 704, 100
33171, V, 1, 1, 1, 1, 0, 704, 100
33172, V, 1, 1, 1, 1, 0, 704, 100
33173, V, 1, 1, 1, 1, 0, 704, 100
33174, V, 1, 1, 1, 1, 0, 704, 100
33175, V, 1, 1, 1, 1, 0, 704, 100
33176, V, 1, 1, 1, 1, 0, 704, 100
33177, V, 1, 1, 1, 1, 0, 704, 100
33178, V, 1, 1, 1, 1, 0, 704, 100
33179, V, 1, 1, 1, 1, 0, 704, 100
33180, V, 1, 1, 1, 1, 0, 704, 100
33181, V, 1, 1, 1, 1, 0, 704, 100
33182, V, 1, 1, 1, 1, 0, 704, 100
33183, V, 1, 1, 1, 1, 0, 704, 100
33184, V, 1, 1, 1, 1, 0, 704, 100
33185, V, 1, 1, 1, 1, 0, 704, 100
33186, V, 1, 1, 1, 1, 0, 704, 100
33187, V, 1, 1, 1, 1, 0, 704, 100
33188, V, 1, 1, 1, 1, 0, 704, 100
33189, V, 1, 1, 1, 1, 0, 704, 100
33190, V, 1, 1, 1, 1, 0, 704, 100
33191, V, 1, 1, 1, 1, 0, 704, 100
33192, V, 1, 1, 1, 1, 0, 704, 100
33193, V, 1, 1, 1, 1, 0, 704, 100
33195, V, 1, 1, 1, 1, 0, 704, 100
33196, V, 1, 1, 1, 1, 0, 704, 100
33197, V, 1, 1, 1, 1, 0, 704, 100
33198, V, 1, 1, 1, 1, 0, 704, 100
33199, V, 1, 1, 1, 1, 0, 704, 100
33200, V, 1, 1, 1, 1, 0, 704, 100
33201, V, 1, 1, 1, 1, 0, 704, 100
33202, V, 1, 1, 1, 1, 0, 704, 100
33203, V, 1, 1, 1, 1, 0, 704, 100
33204, V, 1, 1, 1, 1, 0, 704, 100
33205, V, 1, 1, 1, 1, 0, 704, 100
33206, V, 1, 1, 1, 1, 0, 704, 100
33207, V, 1, 1, 1, 1, 0, 704, 100
33208, V, 1, 1, 1, 1, 0, 704, 100
33209, V, 1, 1, 1, 1, 0, 704, 100
33210, V, 1, 1, 1, 1, 0, 704, 100
33211, V, 1, 1, 1, 1, 0, 704, 100
33212, V, 1, 1, 1, 1, 0, 704, 100
33213, V, 1, 1, 1, 1, 0, 704, 100
33214, V, 1, 1, 1, 1, 0, 704, 100
33215, V, 1, 1, 1, 1, 0, 704, 100
33216, V, 1, 1, 1, 1, 0, 704, 100
33217, V, 1, 1, 1, 1, 0, 704, 100
33218, V, 1, 1, 1, 1, 0, 704, 100
33219, V, 1, 1, 1, 1, 0, 704, 100
33220, V, 1, 1, 1, 1, 0, 704, 100
33221, V, 1, 1, 1, 1, 0, 704, 100
33222, V, 1, 1, 1, 1, 0, 704, 100
33223, V, 1, 1, 1, 1, 0, 704, 100
33224, V, 1, 1, 1, 1, 0, 704, 100
33225, V, 1, 1, 1, 1, 0, 704, 100
33226, V, 1, 1, 1, 1, 0, 704, 100
33227, V, 1, 1, 1, 1, 0, 704, 100
33228, V, 1, 1, 1, 1, 0, 704, 100
33229, V, 1, 1, 1, 1, 0, 704, 100
33230, V, 1, 1, 1, 1, 0, 704, 100
33231, V, 1, 1, 1, 1, 0, 704, 100
33232, V, 1, 1, 1, 1, 0, 704, 100
33233, V, 1, 1, 1, 1, 0, 704, 100
33234, V, 1, 1, 1, 1, 0, 704, 100
33235, V, 1, 1, 1, 1, 0, 704, 100
33236, V, 1, 1, 1, 1, 0, 704, 100
33238, V, 1, 1, 1, 1, 0, 704, 100
33239, V, 1, 1, 1, 1, 0, 704, 100
33240, V, 1, 1, 1, 1, 0, 704, 100
33241, V, 1, 1, 1, 1, 0, 704, 100
33242, V, 1, 1, 1, 1, 0, 704, 100
33243, V, 1, 1, 1, 1, 0, 704, 100
33244, V, 1, 1, 1, 1, 0, 704, 100
33245, V, 1, 1, 1, 1, 0, 704, 100
33246, V, 1, 1, 1, 1, 0, 704, 100
33247, V, 1, 1, 1, 1, 0, 704, 100
33248, V, 1, 1, 1, 1, 0, 704, 100
33249, V, 1, 1, 1, 1, 0, 704, 100
33250, V, 1, 1, 1, 1, 0, 704, 100
33251, V, 1, 1, 1, 1, 0, 704, 100
33252, V, 1, 1, 1, 1, 0, 704, 100
33253, V, 1, 1, 1, 1, 0, 704, 100
33254, V, 1, 1, 1, 1, 0, 704, 100
33255, V, 1, 1, 1, 1, 0, 704, 100
33256, V, 1, 1, 1, 1, 0, 704, 100
33257, V, 1, 1, 1, 1, 0, 704, 100
33258, V, 1, 1, 1, 1, 0, 704, 100
33259, V, 1, 1, 1, 1, 0, 704, 100
33260, V, 1, 1, 1, 1, 0, 704, 100
33261, V, 1, 1, 1, 1, 0, 704, 100
33262, V, 1, 1, 1, 1, 0, 704, 100
33263, V, 1, 1, 1, 1, 0, 704, 100
33264, V, 1, 1, 1, 1, 0, 704, 100
33265, V, 1, 1, 1, 1, 0, 704, 100
33266, V, 1, 1, 1, 1, 0, 704, 100
33267, V, 1, 1, 1, 1, 0, 704, 100
33268, V, 1, 1, 1, 1, 0, 704, 100
33269, V, 1, 1, 1, 1, 0, 704, 100
33270, V, 1, 1, 1, 1, 0, 704, 100
33271, V, 1, 1, 1, 1, 0, 704, 100
33272, V, 1, 1, 1, 1, 0, 704, 100
33273, V, 1, 1, 1, 1, 0, 704, 100
33274, V, 1, 1, 1, 1, 0, 704, 100
33275, V, 1, 1, 1, 1, 0, 704, 100
33276, V, 1, 1, 1, 1, 0, 704, 100
33277, V, 1, 1, 1, 1, 0, 704, 100
33278, V, 1, 1, 1, 1, 0, 704, 100
33280, V, 1, 1, 1, 1, 0, 704, 100
33281, V, 1, 1, 1, 1, 0, 704, 100
33282, V, 1, 1, 1, 1, 0, 704, 100
33283, V, 1, 1, 1, 1, 0, 704, 100
33284, V, 1, 1, 1, 1, 0, 704, 100
33285, V, 1, 1, 1, 1, 0, 704, 100
33286, V, 1, 1, 1, 1, 0, 704, 100
33287, V, 1, 1, 1, 1, 0, 704, 100
33288, V, 1, 1, 1, 1, 0, 704, 100
33289, V, 1, 1, 1, 1, 0, 704, 100
33290, V, 1, 1, 1, 1, 0, 704, 100
33291, V, 1, 1, 1, 1, 0, 704, 100
33292, V, 1, 1, 1, 1, 0, 704, 100
33293, V, 1, 1, 1, 1, 0, 704, 100
33294, V, 1, 1, 1, 1, 0, 704, 100
33295, V, 1, 1, 1, 1, 0, 704, 100
33296, V, 1, 1, 1, 1, 0, 704, 100
33297, V, 1, 1, 1, 1, 0, 704, 100
33298, V, 1, 1, 1, 1, 0, 704, 100
33299, V, 1, 1, 1, 1, 0, 704, 100
33300, V, 1, 1, 1, 1, 0, 704, 100
33301, V, 1, 1, 1, 1, 0, 704, 100
33302, V, 1, 1, 1, 1, 0, 704, 100
33303, V, 1, 1, 1, 1, 0, 704, 100
33304, V, 1, 1, 1, 1, 0, 704, 100
33305, V, 1, 1, 1, 1, 0, 704, 100
33306, V, 1, 1, 1, 1, 0, 704, 100
33307, V, 1, 1, 1, 1, 0, 704, 100
33308, V, 1, 1, 1, 1, 0, 704, 100
33309, V, 1, 1, 1, 1, 0, 704, 100
33310, V, 1, 1, 1, 1, 0, 704, 100
33311, V, 1, 1, 1, 1, 0, 704, 100
33312, V, 1, 1, 1, 1, 0, 704, 100
33313, V, 1, 1, 1, 1, 0, 704, 100
33314, V, 1, 1, 1, 1, 0, 704, 100
33315, V, 1, 1, 1, 1, 0, 704, 100
33316, V, 1, 1, 1, 1, 0, 704, 100
33317, V, 1, 1, 1, 1, 0, 704, 100
33318, V, 1, 1, 1, 1, 0, 704, 100
33319, V, 1, 1, 1, 1, 0, 704, 100
33320, V, 1, 1, 1, 1, 0, 704, 100
33321, V, 1, 1, 1, 1, 0, 704, 100
33323, V, 1, 1, 1, 1, 0, 704, 100
33324, V, 1, 1, 1, 1, 0, 704, 100
33325, V, 1, 1, 1, 1, 0, 704, 100
33326, V, 1, 1, 1, 1, 0, 704, 100
33327, V, 1, 1, 1, 1, 0, 704, 100
33328, V, 1, 1, 1, 1, 0, 704, 100
33329, V, 1, 1, 1, 1, 0, 704, 100
33330, V, 1, 1, 1, 1, 0, 704, 100
33331, V, 1, 1, 1, 1, 0, 704, 100
33332, V, 1, 1, 1, 1, 0, 704, 100
33333, V, 1, 1, 1, 1, 0, 704, 100
33334, V, 1, 1, 1, 1, 0, 704, 100
33335, V, 1, 1, 1, 1, 0, 704, 100
33336, V, 1, 1, 1, 1, 0, 704, 100
33337, V, 1, 1, 1, 1, 0, 704, 100
33338, V, 1, 1, 1, 1, 0, 704, 100
33339, V, 1, 1, 1, 1, 0, 704, 100
33340, V, 1, 1, 1, 1, 0, 704, 100
33341, V, 1, 1, 1, 1, 0, 704, 100
33342, V, 1, 1, 1, 1, 0, 704, 100
33343, V, 1, 1, 1, 1, 0, 704, 100
33344, V, 1, 1, 1, 1, 0, 704, 100
33345, V, 1, 1, 1, 1, 0, 704, 100
33346, V, 1, 1, 1, 1, 0, 704, 100
33347, V, 1, 1, 1, 1, 0, 704, 100
33348, V, 1, 1, 1, 1, 0, 704, 100
33349, V, 1, 1, 1, 1, 0, 704, 100
33350, V, 1, 1, 1, 1, 0, 704, 100
33351, V, 1, 1, 1, 1, 0, 704, 100
33352, V, 1, 1, 1, 1, 0, 704, 100
33353, V, 1, 1, 1, 1, 0, 704, 100
33354, V, 1, 1, 1, 1, 0, 704, 100
33355, V, 1, 1, 1, 1, 0, 704, 100
33356, V, 1, 1, 1, 1, 0, 704, 100
33357, V, 1, 1, 1, 1, 0, 704, 100
33358, V, 1, 1, 1, 1, 0, 704, 100
33359, V, 1, 1, 1, 1, 0, 704, 100
33360, V, 1, 1, 1, 1, 0, 704, 100
33361, V, 1, 1, 1, 1, 0, 704, 100
33362, V, 1, 1, 1, 1, 0, 704, 100
33363, V, 1, 1, 1, 1, 0, 704, 100
33364, V, 1, 1, 1, 1, 0, 704, 100
33366, V, 1, 1, 1, 1, 0, 704, 100
33367, V, 1, 1, 1, 1, 0, 704, 100
33368, V, 1, 1, 1, 1, 0, 704, 100
33369, V, 1, 1, 1, 1, 0, 704, 100
33370, V, 1, 1, 1, 1, 0, 704, 100
33371, V, 1, 1, 1, 1, 0, 704, 100
33372, V, 1, 1, 1, 1, 0, 704, 100
33373, V, 1, 1, 1, 1, 0, 704, 100
33374, V, 1, 1, 1, 1, 0, 704, 100
33375, V, 1, 1, 1, 1, 0, 704, 100
33376, V, 1, 1, 1, 1, 0, 704, 100
33377, V, 1, 1, 1, 1, 0, 704, 100
33378, V, 1, 1, 1, 1, 0, 704, 100
33379, V, 1, 1, 1, 1, 0, 704, 100
33380, V, 1, 1, 1, 1, 0, 704, 100
33381, V, 1, 1, 1, 1, 0, 704, 100
33382, V, 1, 1, 1, 1, 0, 704, 100
33383, V, 1, 1, 1, 1, 0, 704, 100
33384, V, 1, 1, 1, 1, 0, 704, 100
33385, V, 1, 1, 1, 1, 0, 704, 100
33386, V, 1, 1, 1, 1, 0, 704, 100
33387, V, 1, 1, 1, 1, 0, 704, 100
33388, V, 1, 1, 1, 1, 0, 704, 100
33389, V, 1, 1, 1, 1, 0, 704, 100
33390, V, 1, 1, 1, 1, 0, 704, 100
33391, V, 1, 1, 1, 1, 0, 704, 100
33392, V, 1, 1, 1, 1, 0, 704, 100
33393, V, 1, 1, 1, 1, 0, 704, 100
33394, V, 1, 1, 1, 1, 0, 704, 100
33395, V, 1, 1, 1, 1, 0, 704, 100
33396, V, 1, 1, 1, 1, 0, 704, 100
33397, V, 1, 1, 1, 1, 0, 704, 100
33398, V, 1, 1, 1, 1, 0, 704, 100
33399, V, 1, 1, 1, 1, 0, 704, 100
33400, V, 1, 1, 1, 1, 0, 704, 100
33401, V, 1, 1, 1, 1, 0, 704, 100
33402, V, 1, 1, 1, 1, 0, 704, 100
33403, V, 1, 1, 1, 1, 0, 704, 100
33404, V, 1, 1, 1, 1, 0, 704, 100
33405, V, 1, 1, 1, 1, 0, 704, 100
33406, V, 1, 1, 1, 1, 0, 704, 100
33408, V, 1, 1, 1, 1, 0, 704, 100
33409, V, 1, 1, 1, 1, 0, 704, 100
33410, V, 1, 1, 1, 1, 0, 704, 100
33411, V, 1, 1, 1, 1, 0, 704, 100
33412, V, 1, 1, 1, 1, 0, 704, 100
33413, V, 1, 1, 1, 1, 0, 704, 100
33414, V, 1, 1, 1, 1, 0, 704, 100
33415, V, 1, 1, 1, 1, 0, 704, 100
33416, V, 1, 1, 1, 1, 0, 704, 100
33417, V, 1, 1, 1, 1, 0, 704, 100
33418, V, 1, 1, 1, 1, 0, 704, 100
33419, V, 1, 1, 1, 1, 0, 704, 100
33420, V, 1, 1, 1, 1, 0, 704, 100
33421, V, 1, 1, 1, 1, 0, 704, 100
33422, V, 1, 1, 1, 1, 0, 704, 100
33423, V, 1, 1, 1, 1, 0, 704, 100
33424, V, 1, 1, 1, 1, 0, 704, 100
33425, V, 1, 1, 1, 1, 0, 704, 100
33426, V, 1, 1, 1, 1, 0, 704, 100
33427, V, 1, 1, 1, 1, 0, 704, 100
33428, V, 1, 1, 1, 1, 0, 704, 100
33429, V, 1, 1, 1, 1, 0, 704, 100
33430, V, 1, 1, 1, 1, 0, 704, 100
33431, V, 1, 1, 1, 1, 0, 704, 100
33432, V, 1, 1, 1, 1, 0, 704, 100
33433, V, 1, 1, 1, 1, 0, 704, 100
33434, V, 1, 1, 1, 1, 0, 704, 100
33435, V, 1, 1, 1, 1, 0, 704, 100
33436, V, 1, 1, 1, 1, 0, 704, 100
33437, V, 1, 1, 1, 1, 0, 704, 100
33438, V, 1, 1, 1, 1, 0, 704, 100
33439, V, 1, 1, 1, 1, 0, 704, 100
33440, V, 1, 1, 1, 1, 0, 704, 100
33441, V, 1, 1, 1, 1, 0, 704, 100
33442, V, 1, 1, 1, 1, 0, 704, 100
33443, V, 1, 1, 1, 1, 0, 704, 100
33444, V, 1, 1, 1, 1, 0, 704, 100
33445, V, 1, 1, 1, 1, 0, 704, 100
33446, V, 1, 1, 1, 1, 0, 704, 100
33447, V, 1, 1, 1, 1, 0, 704, 100
33448, V, 1, 1, 1, 1, 0, 704, 100
33449, V, 1, 1, 1, 1, 0, 704, 100
33451, V, 1, 1, 1, 1, 0, 704, 100
33452, V, 1, 1, 1, 1, 0, 704, 100
33453, V, 1, 1, 1, 1, 0, 704, 100
33454, V, 1, 1, 1, 1, 0, 704, 100
33455, V, 1, 1, 1, 1, 0, 704, 100
33456, V, 1, 1, 1, 1, 0, 704, 100
33457, V, 1, 1, 1, 1, 0, 704, 100
33458, V, 1, 1, 1, 1, 0, 704, 100
33459, V, 1, 1, 1, 1, 0, 704, 100
33460, V, 1, 1, 1, 1, 0, 704, 100
33461, V, 1, 1, 1, 1, 0, 704, 100
33462, V, 1, 1, 1, 1, 0, 704, 100
33463, V, 1, 1, 1, 1, 0, 704, 100
33464, V, 1, 1, 1, 1, 0, 704, 100
33465, V, 1, 1, 1, 1, 0, 704, 100
33466, V, 1, 1, 1, 1, 0, 704, 100
33467, V, 1, 1, 1, 1, 0, 704, 100
33468, V, 1, 1, 1, 1, 0, 704, 100
33469, V, 1, 1, 1, 1, 0, 704, 100
33470, V, 1, 1, 1, 1, 0, 704, 100
33471, V, 1, 1, 1, 1, 0, 704, 100
33472, V, 1, 1, 1, 1, 0, 704, 100
33473, V, 1, 1, 1, 1, 0, 704, 100
33474, V, 1, 1, 1, 1, 0, 704, 100
33475, V, 1, 1, 1, 1, 0, 704, 100
33476, V, 1, 1, 1, 1, 0, 704, 100
33477, V, 1, 1, 1, 1, 0, 704, 100
33478, V, 1, 1, 1, 1, 0, 704, 100
33479, V, 1, 1, 1, 1, 0, 704, 100
33480, V, 1, 1, 1, 1, 0, 704, 100
33481, V, 1, 1, 1, 1, 0, 704, 100
33482, V, 1, 1, 1, 1, 0, 704, 100
33483, V, 1, 1, 1, 1, 0, 704, 100
33484, V, 1, 1, 1, 1, 0, 704, 100
33485, V, 1, 1, 1, 1, 0, 704, 100
33486, V, 1, 1, 1, 1, 0, 704, 100
33487, V, 1, 1, 1, 1, 0, 704, 100
33488, V, 1, 1, 1, 1, 0, 704, 100
33489, V, 1, 1, 1, 1, 0, 704, 100
33490, V, 1, 1, 1, 1, 0, 704, 100
33491, V, 1, 1, 1, 1, 0, 704, 100
33492, V, 1, 1, 1, 1, 0, 704, 100
33494, V, 1, 1, 1, 1, 0, 704, 100
33495, V, 1, 1, 1, 1, 0, 704, 100
33496, V, 1, 1, 1, 1, 0, 704, 100
33497, V, 1, 1, 1, 1, 0, 704, 100
33498, V, 1, 1, 1, 1, 0, 704, 100
33499, V, 1, 1, 1, 1, 0, 704, 100
33500, V, 1, 1, 1, 1, 0, 704, 100
33501, V, 1, 1, 1, 1, 0, 704, 100
33502, V, 1, 1, 1, 1, 0, 704, 100
33503, V, 1, 1, 1, 1, 0, 704, 100
33504, V, 1, 1, 1, 1, 0, 704, 100
33505, V, 1, 1, 1, 1, 0, 704, 100
33506, V, 1, 1, 1, 1, 0, 704, 100
33507, V, 1, 1, 1, 1, 0, 704, 100
33508, V, 1, 1, 1, 1, 0, 704, 100
33509, V, 1, 1, 1, 1, 0, 704, 100
33510, V, 1, 1, 1, 1, 0, 704, 100
33511, V, 1, 1, 1, 1, 0, 704, 100
33512, V, 1, 1, 1, 1, 0, 704, 100
33513, V, 1, 1, 1, 1, 0, 704, 100
33514, V, 1, 1, 1, 1, 0, 704, 100
33515, V, 1, 1, 1, 1, 0, 704, 100
33516, V, 1, 1, 1, 1, 0, 704, 100
33517, V, 1, 1, 1, 1, 0, 704, 100
33518, V, 1, 1, 1, 1, 0, 704, 100
33519, V, 1, 1, 1, 1, 0, 704, 100
33520, V, 1, 1, 1, 1, 0, 704, 100
33521, V, 1, 1, 1, 1, 0, 704, 100
33522, V, 1, 1, 1, 1, 0, 704, 100
33523, V, 1, 1, 1, 1, 0, 704, 100
33524, V, 1, 1, 1, 1, 0, 704, 100
33525, V, 1, 1, 1, 1, 0, 704, 100
33526, V, 1, 1, 1, 1, 0, 704, 100
33527, V, 1, 1, 1, 1, 0, 704, 100
33528, V, 1, 1, 1, 1, 0, 704, 100
33529, V, 1, 1, 1, 1, 0, 704, 100
33530, V, 1, 1, 1, 1, 0, 704, 100
33531, V, 1, 1, 1, 1, 0, 704, 100
33532, V, 1, 1, 1, 1, 0, 704, 100
33533, V, 1, 1, 1, 1, 0, 704, 100
33534, V, 1, 1, 1, 1, 0, 704, 100
33536, V, 1, 1, 1, 1, 0, 704, 100
33537, V, 1, 1, 1, 1, 0, 704, 100
33538, V, 1, 1, 1, 1, 0, 704, 100
33539, V, 1, 1, 1, 1, 0, 704, 100
33540, V, 1, 1, 1, 1, 0, 704, 100
33541, V, 1, 1, 1, 1, 0, 704, 100
33542, V, 1, 1, 1, 1, 0, 704, 100
33543, V, 1, 1, 1, 1, 0, 704, 100
33544, V, 1, 1, 1, 1, 0, 704, 100
33545, V, 1, 1, 1, 1, 0, 704, 100
33546, V, 1, 1, 1, 1, 0, 704, 100
33547, V, 1, 1, 1, 1, 0, 704, 100
33548, V, 1, 1, 1, 1, 0, 704, 100
33549, V, 1, 1, 1, 1, 0, 704, 100
33550, V, 1, 1, 1, 1, 0, 704, 100
33551, V, 1, 1, 1, 1, 0, 704, 100
33552, V, 1, 1, 1, 1, 0, 704, 100
33553, V, 1, 1, 1, 1, 0, 704, 100
33554, V, 1, 1, 1, 1, 0, 704, 100
33555, V, 1, 1, 1, 1, 0, 704, 100
33556, V, 1, 1, 1, 1, 0, 704, 100
33557, V, 1, 1, 1, 1, 0, 704, 100
33558, V, 1, 1, 1, 1, 0, 704, 100
33559, V, 1, 1, 1, 1, 0, 704, 100
33560, V, 1, 1, 1, 1, 0, 704, 100
33561, V, 1, 1, 1, 1, 0, 704, 100
33562, V, 1, 1, 1, 1, 0, 704, 100
33563, V, 1, 1, 1, 1, 0, 704, 100
33564, V, 1, 1, 1, 1, 0, 704, 100
33565, V, 1, 1, 1, 1, 0, 704, 100
33566, V, 1, 1, 1, 1, 0, 704, 100
33567, V, 1, 1, 1, 1, 0, 704, 100
33568, V, 1, 1, 1, 1, 0, 704, 100
33569, V, 1, 1, 1, 1, 0, 704, 100
33570, V, 1, 1, 1, 1, 0, 704, 100
33571, V, 1, 1, 1, 1, 0, 704, 100
33572, V, 1, 1, 1, 1, 0, 704, 100
33573, V, 1, 1, 1, 1, 0, 704, 100
33574, V, 1, 1, 1, 1, 0, 704, 100
33575, V, 1, 1, 1, 1, 0, 704, 100
33576, V, 1, 1, 1, 1, 0, 704, 100
33577, V, 1, 1, 1, 1, 0, 704, 100
33579, V, 1, 1, 1, 1, 0, 704, 100
33580, V, 1, 1, 1, 1, 0, 704, 100
33581, V, 1, 1, 1, 1, 0, 704, 100
33582, V, 1, 1, 1, 1, 0, 704, 100
33583, V, 1, 1, 1, 1, 0, 704, 100
33584, V, 1, 1, 1, 1, 0, 704, 100
33585, V, 1, 1, 1, 1, 0, 704, 100
33586, V, 1, 1, 1, 1, 0, 704, 100
33587, V, 1, 1, 1, 1, 0, 704, 100
33588, V, 1, 1, 1, 1, 0, 704, 100
33589, V, 1, 1, 1, 1, 0, 704, 100
33590, V, 1, 1, 1, 1, 0, 704, 100
33591, V, 1, 1, 1, 1, 0, 704, 100
33592, V, 1, 1, 1, 1, 0, 704, 100
33593, V, 1, 1, 1, 1, 0, 704, 100
33594, V, 1, 1, 1, 1, 0, 704, 100
33595, V, 1, 1, 1, 1, 0, 704, 100
33596, V, 1, 1, 1, 1, 0, 704, 100
33597, V, 1, 1, 1, 1, 0, 704, 100
33598, V, 1, 1, 1, 1, 0, 704, 100
33599, V, 1, 1, 1, 1, 0, 704, 100
33600, V, 1, 1, 1, 1, 0, 704, 100
33601, V, 1, 1, 1, 1, 0, 704, 100
33602, V, 1, 1, 1, 1, 0, 704, 100
33603, V, 1, 1, 1, 1, 0, 704, 100
33604, V, 1, 1, 1, 1, 0, 704, 100
33605, V, 1, 1, 1, 1, 0, 704, 100
33606, V, 1, 1, 1, 1, 0, 704, 100
33607, V, 1, 1, 1, 1, 0, 704, 100
33608, V, 1, 1, 1, 1, 0, 704, 100
33609, V, 1, 1, 1, 1, 0, 704, 100
33610, V, 1, 1, 1, 1, 0, 704, 100
33611, V, 1, 1, 1, 1, 0, 704, 100
33612, V, 1, 1, 1, 1, 0, 704, 100
33613, V, 1, 1, 1, 1, 0, 704, 100
33614, V, 1, 1, 1, 1, 0, 704, 100
33615, V, 1, 1, 1, 1, 0, 704, 100
33616, V, 1, 1, 1, 1, 0, 704, 100
33617, V, 1, 1, 1, 1, 0, 704, 100
33618, V, 1, 1, 1, 1, 0, 704, 100
33619, V, 1, 1, 1, 1, 0, 704, 100
33620, V, 1, 1, 1, 1, 0, 704, 100
33622, V, 1, 1, 1, 1, 0, 704, 100
33623, V, 1, 1, 1, 1, 0, 704, 100
33624, V, 1, 1, 1, 1, 0, 704, 100
33625, V, 1, 1, 1, 1, 0, 704, 100
33626, V, 1, 1, 1, 1, 0, 704, 100
33627, V, 1, 1, 1, 1, 0, 704, 100
33628, V, 1, 1, 1, 1, 0, 704, 100
33629, V, 1, 1, 1, 1, 0, 704, 100
33630, V, 1, 1, 1, 1, 0, 704, 100
33631, V, 1, 1, 1, 1, 0, 704, 100
33632, V, 1, 1, 1, 1, 0, 704, 100
33633, V, 1, 1, 1, 1, 0, 704, 100
33634, V, 1, 1, 1, 1, 0, 704, 100
33635, V, 1, 1, 1, 1, 0, 704, 100
33636, V, 1, 1, 1, 1, 0, 704, 100
33637, V, 1, 1, 1, 1, 0, 704, 100
33638, V, 1, 1, 1, 1, 0, 704, 100
33639, V, 1, 1, 1, 1, 0, 704, 100
33640, V, 1, 1, 1, 1, 0, 704, 100
33641, V, 1, 1, 1, 1, 0, 704, 100
33642, V, 1, 1, 1, 1, 0, 704, 100
33643, V, 1, 1, 1, 1, 0, 704, 100
33644, V, 1, 1, 1, 1, 0, 704, 100
33645, V, 1, 1, 1, 1, 0, 704, 100
33646, V, 1, 1, 1, 1, 0, 704, 100
33647, V, 1, 1, 1, 1, 0, 704, 100
33648, V, 1, 1, 1, 1, 0, 704, 100
33649, V, 1, 1, 1, 1, 0, 704, 100
33650, V, 1, 1, 1, 1, 0, 704, 100
33651, V, 1, 1, 1, 1, 0, 704, 100
33652, V, 1, 1, 1, 1, 0, 704, 100
33653, V, 1, 1, 1, 1, 0, 704, 100
33654, V, 1, 1, 1, 1, 0, 704, 100
33655, V, 1, 1, 1, 1, 0, 704, 100
33656, V, 1, 1, 1, 1, 0, 704, 100
33657, V, 1, 1, 1, 1, 0, 704, 100
33658, V, 1, 1, 1, 1, 0, 704, 100
33659, V, 1, 1, 1, 1, 0, 704, 100
33660, V, 1, 1, 1, 1, 0, 704, 100
33661, V, 1, 1, 1, 1, 0, 704, 100
33662, V, 1, 1, 1, 1, 0, 704, 100
33664, V, 1, 1, 1, 1, 0, 704, 100
33665, V, 1, 1, 1, 1, 0, 704, 100
33666, V, 1, 1, 1, 1, 0, 704, 100
33667, V, 1, 1, 1, 1, 0, 704, 100
33668, V, 1, 1, 1, 1, 0, 704, 100
33669, V, 1, 1, 1, 1, 0, 704, 100
33670, V, 1, 1, 1, 1, 0, 704, 100
33671, V, 1, 1, 1, 1, 0, 704, 100
33672, V, 1, 1, 1, 1, 0, 704, 100
33673, V, 1, 1, 1, 1, 0, 704, 100
33674, V, 1, 1, 1, 1, 0, 704, 100
33675, V, 1, 1, 1, 1, 0, 704, 100
33676, V, 1, 1, 1, 1, 0, 704, 100
33677, V, 1, 1, 1, 1, 0, 704, 100
33678, V, 1, 1, 1, 1, 0, 704, 100
33679, V, 1, 1, 1, 1, 0, 704, 100
33680, V, 1, 1, 1, 1, 0, 704, 100
33681, V, 1, 1, 1, 1, 0, 704, 100
33682, V, 1, 1, 1, 1, 0, 704, 100
33683, V, 1, 1, 1, 1, 0, 704, 100
33684, V, 1, 1, 1, 1, 0, 704, 100
33685, V, 1, 1, 1, 1, 0, 704, 100
33686, V, 1, 1, 1, 1, 0, 704, 100
33687, V, 1, 1, 1, 1, 0, 704, 100
33688, V, 1, 1, 1, 1, 0, 704, 100
33689, V, 1, 1, 1, 1, 0, 704, 100
33690, V, 1, 1, 1, 1, 0, 704, 100
33691, V, 1, 1, 1, 1, 0, 704, 100
33692, V, 1, 1, 1, 1, 0, 704, 100
33693, V, 1, 1, 1, 1, 0, 704, 100
33694, V, 1, 1, 1, 1, 0, 704, 100
33695, V, 1, 1, 1, 1, 0, 704, 100
33696, V, 1, 1, 1, 1, 0, 704, 100
33697, V, 1, 1, 1, 1, 0, 704, 100
33698, V, 1, 1, 1, 1, 0, 704, 100
33699, V, 1, 1, 1, 1, 0, 704, 100
33700, V, 1, 1, 1, 1, 0, 704, 100
33701, V, 1, 1, 1, 1, 0, 704, 100
33702, V, 1, 1, 1, 1, 0, 704, 100
33703, V, 1, 1, 1, 1, 0, 704, 100
33704, V, 1, 1, 1, 1, 0, 704, 100
33705, V, 1, 1, 1, 1, 0, 704, 100
33707, V, 1, 1, 1, 1, 0, 704, 100
33708, V, 1, 1, 1, 1, 0, 704, 100
33709, V, 1, 1, 1, 1, 0, 704, 100
33710, V, 1, 1, 1, 1, 0, 704, 100
33711, V, 1, 1, 1, 1, 0, 704, 100
33712, V, 1, 1, 1, 1, 0, 704, 100
33713, V, 1, 1, 1, 1, 0, 704, 100
33714, V, 1, 1, 1, 1, 0, 704, 100
33715, V, 1, 1, 1, 1, 0, 704, 100
33716, V, 1, 1, 1, 1, 0, 704, 100
33717, V, 1, 1, 1, 1, 0, 704, 100
33718, V, 1, 1, 1, 1, 0, 704, 100
33719, V, 1, 1, 1, 1, 0, 704, 100
33720, V, 1, 1, 1, 1, 0, 704, 100
33721, V, 1, 1, 1, 1, 0, 704, 100
33722, V, 1, 1, 1, 1, 0, 704, 100
33723, V, 1, 1, 1, 1, 0, 704, 100
33724, V, 1, 1, 1, 1, 0, 704, 100
33725, V, 1, 1, 1, 1, 0, 704, 100
33726, V, 1, 1, 1, 1, 0, 704, 100
33727, V, 1, 1, 1, 1, 0, 704, 100
33728, V, 1, 1, 1, 1, 0, 704, 100
33729, V, 1, 1, 1, 1, 0, 704, 100
33730, V, 1, 1, 1, 1, 0, 704, 100
33731, V, 1, 1, 1, 1, 0, 704, 100
33732, V, 1, 1, 1, 1, 0, 704, 100
33733, V, 1, 1, 1, 1, 0, 704, 100
33734, V, 1, 1, 1, 1, 0, 704, 100
33735, V, 1, 1, 1, 1, 0, 704, 100
33736, V, 1, 1, 1, 1, 0, 704, 100
33737, V, 1, 1, 1, 1, 0, 704, 100
33738, V, 1, 1, 1, 1, 0, 704, 100
33739, V, 1, 1, 1, 1, 0, 704, 100
33740, V, 1, 1, 1, 1, 0, 704, 100
33741, V, 1, 1, 1, 1, 0, 704, 100
33742, V, 1, 1, 1, 1, 0, 704, 100
33743, V, 1, 1, 1, 1, 0, 704, 100
33744, V, 1, 1, 1, 1, 0, 704, 100
33745, V, 1, 1, 1, 1, 0, 704, 100
33746, V, 1, 1, 1, 1, 0, 704, 100
33747, V, 1, 1, 1, 1, 0, 704, 100
33748, V, 1, 1, 1, 1, 0, 704, 100
33750, V, 1, 1, 1, 1, 0, 704, 100
33751, V, 1, 1, 1, 1, 0, 704, 100
33752, V, 1, 1, 1, 1, 0, 704, 100
33753, V, 1, 1, 1, 1, 0, 704, 100
33754, V, 1, 1, 1, 1, 0, 704, 100
33755, V, 1, 1, 1, 1, 0, 704, 100
33756, V, 1, 1, 1, 1, 0, 704, 100
33757, V, 1, 1, 1, 1, 0, 704, 100
33758, V, 1, 1, 1, 1, 0, 704, 100
33759, V, 1, 1, 1, 1, 0, 704, 100
33760, V, 1, 1, 1, 1, 0, 704, 100
33761, V, 1, 1, 1, 1, 0, 704, 100
33762, V, 1, 1, 1, 1, 0, 704, 100
33763, V, 1, 1, 1, 1, 0, 704, 100
33764, V, 1, 1, 1, 1, 0, 704, 100
33765, V, 1, 1, 1, 1, 0, 704, 100
33766, V, 1, 1, 1, 1, 0, 704, 100
33767, V, 1, 1, 1, 1, 0, 704, 100
33768, V, 1, 1, 1, 1, 0, 704, 100
33769, V, 1, 1, 1, 1, 0, 704, 100
33770, V, 1, 1, 1, 1, 0, 704, 100
33771, V, 1, 1, 1, 1, 0, 704, 100
33772, V, 1, 1, 1, 1, 0, 704, 100
33773, V, 1, 1, 1, 1, 0, 704, 100
33774, V, 1, 1, 1, 1, 0, 704, 100
33775, V, 1, 1, 1, 1, 0, 704, 100
33776, V, 1, 1, 1, 1, 0, 704, 100
33777, V, 1, 1, 1, 1, 0, 704, 100
33778, V, 1, 1, 1, 1, 0, 704, 100
33779, V, 1, 1, 1, 1, 0, 704, 100
33780, V, 1, 1, 1, 1, 0, 704, 100
33781, V, 1, 1, 1, 1, 0, 704, 100
33782, V, 1, 1, 1, 1, 0, 704, 100
33783, V, 1, 1, 1, 1, 0, 704, 100
33784, V, 1, 1, 1, 1, 0, 704, 100
33785, V, 1, 1, 1, 1, 0, 704, 100
33786, V, 1, 1, 1, 1, 0, 704, 100
33787, V, 1, 1, 1, 1, 0, 704, 100
33788, V, 1, 1, 1, 1, 0, 704, 100
33789, V, 1, 1, 1, 1, 0, 704, 100
33790, V, 1, 1, 1, 1, 0, 704, 100
33792, V, 1, 1, 1, 1, 0, 704, 100
33793, V, 1, 1, 1, 1, 0, 704, 100
33794, V, 1, 1, 1, 1, 0, 704, 100
33795, V, 1, 1, 1, 1, 0, 704, 100
33796, V, 1, 1, 1, 1, 0, 704, 100
33797, V, 1, 1, 1, 1, 0, 704, 100
33798, V, 1, 1, 1, 1, 0, 704, 100
33799, V, 1, 1, 1, 1, 0, 704, 100
33800, V, 1, 1, 1, 1, 0, 704, 100
33801, V, 1, 1, 1, 1, 0, 704, 100
33802, V, 1, 1, 1, 1, 0, 704, 100
33803, V, 1, 1, 1, 1, 0, 704, 100
33804, V, 1, 1, 1, 1, 0, 704, 100
33805, V, 1, 1, 1, 1, 0, 704, 100
33806, V, 1, 1, 1, 1, 0, 704, 100
33807, V, 1, 1, 1, 1, 0, 704, 100
33808, V, 1, 1, 1, 1, 0, 704, 100
33809, V, 1, 1, 1, 1, 0, 704, 100
33810, V, 1, 1, 1, 1, 0, 704, 100
33811, V, 1, 1, 1, 1, 0, 704, 100
33812, V, 1, 1, 1, 1, 0, 704, 100
33813, V, 1, 1, 1, 1, 0, 704, 100
33814, V, 1, 1, 1, 1, 0, 704, 100
33815, V, 1, 1, 1, 1, 0, 704, 100
33816, V, 1, 1, 1, 1, 0, 704, 100
33817, V, 1, 1, 1, 1, 0, 704, 100
33818, V, 1, 1, 1, 1, 0, 704, 100
33819, V, 1, 1, 1, 1, 0, 704, 100
33820, V, 1, 1, 1, 1, 0, 704, 100
33821, V, 1, 1, 1, 1, 0, 704, 100
33822, V, 1, 1, 1, 1, 0, 704, 100
33823, V, 1, 1, 1, 1, 0, 704, 100
33824, V, 1, 1, 1, 1, 0, 704, 100
33825, V, 1, 1, 1, 1, 0, 704, 100
33826, V, 1, 1, 1, 1, 0, 704, 100
33827, V, 1, 1, 1, 1, 0, 704, 100
33828, V, 1, 1, 1, 1, 0, 704, 100
33829, V, 1, 1, 1, 1, 0, 704, 100
33830, V, 1, 1, 1, 1, 0, 704, 100
33831, V, 1, 1, 1, 1, 0, 704, 100
33832, V, 1, 1, 1, 1, 0, 704, 100
33833, V, 1, 1, 1, 1, 0, 704, 100
33835, V, 1, 1, 1, 1, 0, 704, 100
33836, V, 1, 1, 1, 1, 0, 704, 100
33837, V, 1, 1, 1, 1, 0, 704, 100
33838, V, 1, 1, 1, 1, 0, 704, 100
33839, V, 1, 1, 1, 1, 0, 704, 100
33840, V, 1, 1, 1, 1, 0, 704, 100
33841, V, 1, 1, 1, 1, 0, 704, 100
33842, V, 1, 1, 1, 1, 0, 704, 100
33843, V, 1, 1, 1, 1, 0, 704, 100
33844, V, 1, 1, 1, 1, 0, 704, 100
33845, V, 1, 1, 1, 1, 0, 704, 100
33846, V, 1, 1, 1, 1, 0, 704, 100
33847, V, 1, 1, 1, 1, 0, 704, 100
33848, V, 1, 1, 1, 1, 0, 704, 100
33849, V, 1, 1, 1, 1, 0, 704, 100
33850, V, 1, 1, 1, 1, 0, 704, 100
33851, V, 1, 1, 1, 1, 0, 704, 100
33852, V, 1, 1, 1, 1, 0, 704, 100
33853, V, 1, 1, 1, 1, 0, 704, 100
33854, V, 1, 1, 1, 1, 0, 704, 100
33855, V, 1, 1, 1, 1, 0, 704, 100
33856, V, 1, 1, 1, 1, 0, 704, 100
33857, V, 1, 1, 1, 1, 0, 704, 100
33858, V, 1, 1, 1, 1, 0, 704, 100
33859, V, 1, 1, 1, 1, 0, 704, 99
33860, V, 1, 1, 1, 1, 0, 704, 100
33861, V, 1, 1, 1, 1, 0, 704, 100
33862, V, 1, 1, 1, 1, 0, 704, 99
33863, V, 1, 1, 1, 1, 0, 704, 100
33864, V, 1, 1, 1, 1, 0, 704, 99
33865, V, 1, 1, 1, 1, 0, 704, 99
33866, V, 1, 1, 1, 1, 0, 704, 99
33867, V, 1, 1, 1, 1, 0, 704, 99
33868, V, 1, 1, 1, 1, 0, 704, 99
33869, V, 1, 1, 1, 1, 0, 704, 99
33870, V, 1, 1, 1, 1, 0, 704, 99
33871, V, 1, 1, 1, 1, 0, 704, 99
33872, V, 1, 1, 1, 1, 0, 704, 99
33873, V, 1, 1, 1, 1, 0, 704, 99
33874, V, 1, 1, 1, 1, 0, 704, 99
33875, V, 1, 1, 1, 1, 0, 704, 99
33876, V, 1, 1, 1, 1, 0, 704, 99
33878, V, 1, 1, 1, 1, 0, 704, 99
33879, V, 1, 1, 1, 1, 0, 704, 99
33880, V, 1, 1, 1, 1, 0, 704, 99
33881, V, 1, 1, 1, 1, 0, 704, 99
33882, V, 1, 1, 1, 1, 0, 704, 99
33883, V, 1, 1, 1, 1, 0, 704, 99
33884, V, 1, 1, 1, 1, 0, 704, 99
33885, V, 1, 1, 1, 1, 0, 704, 99
33886, V, 1, 1, 1, 1, 0, 704, 99
33887, V, 1, 1, 1, 1, 0, 704, 99
33888, V, 1, 1, 1, 1, 0, 704, 99
33889, V, 1, 1, 1, 1, 0, 704, 99
33890, V, 1, 1, 1, 1, 0, 704, 99
33891, V, 1, 1, 1, 1, 0, 704, 99
33892, V, 1, 1, 1, 1, 0, 704, 99
33893, V, 1, 1, 1, 1, 0, 704, 99
33894, V, 1, 1, 1, 1, 0, 704, 99
33895, V, 1, 1, 1, 1, 0, 704, 99
33896, V, 1, 1, 1, 1, 0, 704, 99
33897, V, 1, 1, 1, 1, 0, 704, 99
33898, V, 1, 1, 1, 1, 0, 704, 99
33899, V, 1, 1, 1, 1, 0, 704, 99
33900, V, 1, 1, 1, 1, 0, 704, 99
33901, V, 1, 1, 1, 1, 0, 704, 99
33902, V, 1, 1, 1, 1, 0, 704, 99
33903, V, 1, 1, 1, 1, 0, 704, 99
33904, V, 1, 1, 1, 1, 0, 704, 99
33905, V, 1, 1, 1, 1, 0, 704, 99
33906, V, 1, 1, 1, 1, 0, 704, 99
33907, V, 1, 1, 1, 1, 0, 704, 99
33908, V, 1, 1, 1, 1, 0, 704, 99
33909, V, 1, 1, 1, 1, 0, 704, 99
33910, V, 1, 1, 1, 1, 0, 704, 99
33911, V, 1, 1, 1, 1, 0, 704, 99
33912, V, 1, 1, 1, 1, 0, 704, 99
33913, V, 1, 1, 1, 1, 0, 704, 99
33914, V, 1, 1, 1, 1, 0, 704, 99
33915, V, 1, 1, 1, 1, 0, 704, 99
33916, V, 1, 1, 1, 1, 0, 704, 99
33917, V, 1, 1, 1, 1, 0, 704, 99
33918, V, 1, 1, 1, 1, 0, 704, 99
33920, V, 1, 1, 1, 1, 0, 704, 99
33921, V, 1, 1, 1, 1, 0, 704, 99
33922, V, 1, 1, 1, 1, 0, 704, 99
33923, V, 1, 1, 1, 1, 0, 704, 99
33924, V, 1, 1, 1, 1, 0, 704, 99
33925, V, 1, 1, 1, 1, 0, 704, 99
33926, V, 1, 1, 1, 1, 0, 704, 99
33927, V, 1, 1, 1, 1, 0, 704, 99
33928, V, 1, 1, 1, 1, 0, 704, 99
33929, V, 1, 1, 1, 1, 0, 704, 99
33930, V, 1, 1, 1, 1, 0, 704, 99
33931, V, 1, 1, 1, 1, 0, 704, 99
33932, V, 1, 1, 1, 1, 0, 704, 99
33933, V, 1, 1, 1, 1, 0, 704, 99
33934, V, 1, 1, 1, 1, 0, 704, 99
33935, V, 1, 1, 1, 1, 0, 704, 99
33936, V, 1, 1, 1, 1, 0, 704, 99
33937, V, 1, 1, 1, 1, 0, 704, 99
33938, V, 1, 1, 1, 1, 0, 704, 99
33939, V, 1, 1, 1, 1, 0, 704, 99
33940, V, 1, 1, 1, 1, 0, 704, 99
33941, V, 1, 1, 1, 1, 0, 704, 99
33942, V, 1, 1, 1, 1, 0, 704, 99
33943, V, 1, 1, 1, 1, 0, 704, 99
33944, V, 1, 1, 1, 1, 0, 704, 99
33945, V, 1, 1, 1, 1, 0, 704, 99
33946, V, 1, 1, 1, 1, 0, 704, 99
33947, V, 1, 1, 1, 1, 0, 704, 99
33948, V, 1, 1, 1, 1, 0, 704, 99
33949, V, 1, 1, 1, 1, 0, 704, 99
33950, V, 1, 1, 1, 1, 0, 704, 99
33951, V, 1, 1, 1, 1, 0, 704, 99
33952, V, 1, 1, 1, 1, 0, 704, 99
33953, V, 1, 1, 1, 1, 0, 704, 99
33954, V, 1, 1, 1, 1, 0, 704, 99
33955, V, 1, 1, 1, 1, 0, 704, 99
33956, V, 1, 1, 1, 1, 0, 704, 99
33957, V, 1, 1, 1, 1, 0, 704, 99
33958, V, 1, 1, 1, 1, 0, 704, 99
33959, V, 1, 1, 1, 1, 0, 704, 99
33960, V, 1, 1, 1, 1, 0, 704, 99
33961, V, 1, 1, 1, 1, 0, 704, 99
33963, V, 1, 1, 1, 1, 0, 704, 99
33964, V, 1, 1, 1, 1, 0, 704, 99
33965, V, 1, 1, 1, 1, 0, 704, 99
33966, V, 1, 1, 1, 1, 0, 704, 99
33967, V, 1, 1, 1, 1, 0, 704, 99
33968, V, 1, 1, 1, 1, 0, 704, 99
33969, V, 1, 1, 1, 1, 0, 704, 99
33970, V, 1, 1, 1, 1, 0, 704, 99
33971, V, 1, 1, 1, 1, 0, 704, 99
33972, V, 1, 1, 1, 1, 0, 704, 99
33973, V, 1, 1, 1, 1, 0, 704, 99
33974, V, 1, 1, 1, 1, 0, 704, 99
33975, V, 1, 1, 1, 1, 0, 704, 99
33976, V, 1, 1, 1, 1, 0, 704, 99
33977, V, 1, 1, 1, 1, 0, 704, 99
33978, V, 1, 1, 1, 1, 0, 704, 99
33979, V, 1, 1, 1, 1, 0, 704, 99
33980, V, 1, 1, 1, 1, 0, 704, 99
33981, V, 1, 1, 1, 1, 0, 704, 99
33982, V, 1, 1, 1, 1, 0, 704, 99
33983, V, 1, 1, 1, 1, 0, 704, 99
33984, V, 1, 1, 1, 1, 0, 704, 99
33985, V, 1, 1, 1, 1, 0, 704, 99
33986, V, 1, 1, 1, 1, 0, 704, 99
33987, V, 1, 1, 1, 1, 0, 704, 99
33988, V, 1, 1, 1, 1, 0, 704, 99
33989, V, 1, 1, 1, 1, 0, 704, 99
33990, V, 1, 1, 1, 1, 0, 704, 99
33991, V, 1, 1, 1, 1, 0, 704, 99
33992, V, 1, 1, 1, 1, 0, 704, 99
33993, V, 1, 1, 1, 1, 0, 704, 99
33994, V, 1, 1, 1, 1, 0, 704, 99
33995, V, 1, 1, 1, 1, 0, 704, 99
33996, V, 1, 1, 1, 1, 0, 704, 99
33997, V, 1, 1, 1, 1, 0, 704, 99
33998, V, 1, 1, 1, 1, 0, 704, 99
33999, V, 1, 1, 1, 1, 0, 704, 99
34000, V, 1, 1, 1, 1, 0, 704, 99
34001, V, 1, 1, 1, 1, 0, 704, 99
34002, V, 1, 1, 1, 1, 0, 704, 99
34003, V, 1, 1, 1, 1, 0, 704, 99
34004, V, 1, 1, 1, 1, 0, 704, 99
34006, V, 1, 1, 1, 1, 0, 704, 99
34007, V, 1, 1, 1, 1, 0, 704, 99
34008, V, 1, 1, 1, 1, 0, 704, 99
34009, V, 1, 1, 1, 1, 0, 704, 99
34010, V, 1, 1, 1, 1, 0, 704, 99
34011, V, 1, 1, 1, 1, 0, 704, 99
34012, V, 1, 1, 1, 1, 0, 704, 99
34013, V, 1, 1, 1, 1, 0, 704, 99
34014, V, 1, 1, 1, 1, 0, 704, 99
34015, V, 1, 1, 1, 1, 0, 704, 99
34016, V, 1, 1, 1, 1, 0, 704, 99
34017, V, 1, 1, 1, 1, 0, 704, 99
34018, V, 1, 1, 1, 1, 0, 704, 99
34019, V, 1, 1, 1, 1, 0, 704, 99
34020, V, 1, 1, 1, 1, 0, 704, 99
34021, V, 1, 1, 1, 1, 0, 704, 99
34022, V, 1, 1, 1, 1, 0, 704, 99
34023, V, 1, 1, 1, 1, 0, 704, 99
34024, V, 1, 1, 1, 1, 0, 704, 99
34025, V, 1, 1, 1, 1, 0, 704, 99
34026, V, 1, 1, 1, 1, 0, 704, 99
34027, V, 1, 1, 1, 1, 0, 704, 99
34028, V, 1, 1, 1, 1, 0, 704, 99
34029, V, 1, 1, 1, 1, 0, 704, 99
34030, V, 1, 1, 1, 1, 0, 704, 99
34031, V, 1, 1, 1, 1, 0, 704, 99
34032, V, 1, 1, 1, 1, 0, 704, 99
34033, V, 1, 1, 1, 1, 0, 704, 99
34034, V, 1, 1, 1, 1, 0, 704, 99
34035, V, 1, 1, 1, 1, 0, 704, 99
34036, V, 1, 1, 1, 1, 0, 704, 99
34037, V, 1, 1, 1, 1, 0, 704, 99
34038, V, 1, 1, 1, 1, 0, 704, 99
34039, V, 1, 1, 1, 1, 0, 704, 99
34040, V, 1, 1, 1, 1, 0, 704, 99
34041, V, 1, 1, 1, 1, 0, 704, 99
34042, V, 1, 1, 1, 1, 0, 704, 99
34043, V, 1, 1, 1, 1, 0, 704, 99
34044, V, 1, 1, 1, 1, 0, 704, 99
34045, V, 1, 1, 1, 1, 0, 704, 99
34046, V, 1, 1, 1, 1, 0, 704, 99
34048, V, 1, 1, 1, 1, 0, 704, 99
34049, V, 1, 1, 1, 1, 0, 704, 99
34050, V, 1, 1, 1, 1, 0, 704, 99
34051, V, 1, 1, 1, 1, 0, 704, 99
34052, V, 1, 1, 1, 1, 0, 704, 99
34053, V, 1, 1, 1, 1, 0, 704, 99
34054, V, 1, 1, 1, 1, 0, 704, 99
34055, V, 1, 1, 1, 1, 0, 704, 99
34056, V, 1, 1, 1, 1, 0, 704, 99
34057, V, 1, 1, 1, 1, 0, 704, 99
34058, V, 1, 1, 1, 1, 0, 704, 99
34059, V, 1, 1, 1, 1, 0, 704, 99
34060, V, 1, 1, 1, 1, 0, 704, 99
34061, V, 1, 1, 1, 1, 0, 704, 99
34062, V, 1, 1, 1, 1, 0, 704, 99
34063, V, 1, 1, 1, 1, 0, 704, 99
34064, V, 1, 1, 1, 1, 0, 704, 99
34065, V, 1, 1, 1, 1, 0, 704, 99
34066, V, 1, 1, 1, 1, 0, 704, 99
34067, V, 1, 1, 1, 1, 0, 704, 99
34068, V, 1, 1, 1, 1, 0, 704, 99
34069, V, 1, 1, 1, 1, 0, 704, 99
34070, V, 1, 1, 1, 1, 0, 704, 99
34071, V, 1, 1, 1, 1, 0, 704, 99
34072, V, 1, 1, 1, 1, 0, 704, 99
34073, V, 1, 1, 1, 1, 0, 704, 99
34074, V, 1, 1, 1, 1, 0, 704, 99
34075, V, 1, 1, 1, 1, 0, 704, 99
34076, V, 1, 1, 1, 1, 0, 704, 99
34077, V, 1, 1, 1, 1, 0, 704, 99
34078, V, 1, 1, 1, 1, 0, 704, 99
34079, V, 1, 1, 1, 1, 0, 704, 99
34080, V, 1, 1, 1, 1, 0, 704, 99
34081, V, 1, 1, 1, 1, 0, 704, 99
34082, V, 1, 1, 1, 1, 0, 704, 99
34083, V, 1, 1, 1, 1, 0, 704, 99
34084, V, 1, 1, 1, 1, 0, 704, 99
34085, V, 1, 1, 1, 1, 0, 704, 99
34086, V, 1, 1, 1, 1, 0, 704, 99
34087, V, 1, 1, 1, 1, 0, 704, 99
34088, V, 1, 1, 1, 1, 0, 704, 99
34089, V, 1, 1, 1, 1, 0, 704, 99
34091, V, 1, 1, 1, 1, 0, 704, 99
34092, V, 1, 1, 1, 1, 0, 704, 99
34093, V, 1, 1, 1, 1, 0, 704, 99
34094, V, 1, 1, 1, 1, 0, 704, 99
34095, V, 1, 1, 1, 1, 0, 704, 99
34096, V, 1, 1, 1, 1, 0, 704, 99
34097, V, 1, 1, 1, 1, 0, 704, 99
34098, V, 1, 1, 1, 1, 0, 704, 99
34099, V, 1, 1, 1, 1, 0, 704, 99
34100, V, 1, 1, 1, 1, 0, 704, 99
34101, V, 1, 1, 1, 1, 0, 704, 99
34102, V, 1, 1, 1, 1, 0, 704, 99
34103, V, 1, 1, 1, 1, 0, 704, 99
34104, V, 1, 1, 1, 1, 0, 704, 99
34105, V, 1, 1, 1, 1, 0, 704, 99
34106, V, 1, 1, 1, 1, 0, 704, 99
34107, V, 1, 1, 1, 1, 0, 704, 99
34108, V, 1, 1, 1, 1, 0, 704, 99
34109, V, 1, 1, 1, 1, 0, 704, 99
34110, V, 1, 1, 1, 1, 0, 704, 99
34111, V, 1, 1, 1, 1, 0, 704, 99
34112, V, 1, 1, 1, 1, 0, 704, 99
34113, V, 1, 1, 1, 1, 0, 704, 99
34114, V, 1, 1, 1, 1, 0, 704, 99
34115, V, 1, 1, 1, 1, 0, 704, 99
34116, V, 1, 1, 1, 1, 0, 704, 99
34117, V, 1, 1, 1, 1, 0, 704, 99
34118, V, 1, 1, 1, 1, 0, 704, 99
34119, V, 1, 1, 1, 1, 0, 704, 99
34120, V, 1, 1, 1, 1, 0, 704, 99
34121, V, 1, 1, 1, 1, 0, 704, 99
34122, V, 1, 1, 1, 1, 0, 704, 99
34123, V, 1, 1, 1, 1, 0, 704, 99
34124, V, 1, 1, 1, 1, 0, 704, 99
34125, V, 1, 1, 1, 1, 0, 704, 99
34126, V, 1, 1, 1, 1, 0, 704, 99
34127, V, 1, 1, 1, 1, 0, 704, 99
34128, V, 1, 1, 1, 1, 0, 704, 99
34129, V, 1, 1, 1, 1, 0, 704, 99
34130, V, 1, 1, 1, 1, 0, 704, 99
34131, V, 1, 1, 1, 1, 0, 704, 99
34132, V, 1, 1, 1, 1, 0, 704, 99
34134, V, 1, 1, 1, 1, 0, 704, 99
34135, V, 1, 1, 1, 1, 0, 704, 99
34136, V, 1, 1, 1, 1, 0, 704, 99
34137, V, 1, 1, 1, 1, 0, 704, 99
34138, V, 1, 1, 1, 1, 0, 704, 99
34139, V, 1, 1, 1, 1, 0, 704, 99
34140, V, 1, 1, 1, 1, 0, 704, 99
34141, V, 1, 1, 1, 1, 0, 704, 99
34142, V, 1, 1, 1, 1, 0, 704, 99
34143, V, 1, 1, 1, 1, 0, 704, 99
34144, V, 1, 1, 1, 1, 0, 704, 99
34145, V, 1, 1, 1, 1, 0, 704, 99
34146, V, 1, 1, 1, 1, 0, 704, 99
34147, V, 1, 1, 1, 1, 0, 704, 99
34148, V, 1, 1, 1, 1, 0, 704, 99
34149, V, 1, 1, 1, 1, 0, 704, 99
34150, V, 1, 1, 1, 1, 0, 704, 99
34151, V, 1, 1, 1, 1, 0, 704, 99
34152, V, 1, 1, 1, 1, 0, 704, 99
34153, V, 1, 1, 1, 1, 0, 704, 99
34154, V, 1, 1, 1, 1, 0, 704, 99
34155, V, 1, 1, 1, 1, 0, 704, 99
34156, V, 1, 1, 1, 1, 0, 704, 99
34157, V, 1, 1, 1, 1, 0, 704, 99
34158, V, 1, 1, 1, 1, 0, 704, 99
34159, V, 1, 1, 1, 1, 0, 704, 99
34160, V, 1, 1, 1, 1, 0, 704, 99
34161, V, 1, 1, 1, 1, 0, 704, 99
34162, V, 1, 1, 1, 1, 0, 704, 99
34163, V, 1, 1, 1, 1, 0, 704, 99
34164, V, 1, 1, 1, 1, 0, 704, 99
34165, V, 1, 1, 1, 1, 0, 704, 99
34166, V, 1, 1, 1, 1, 0, 704, 99
34167, V, 1, 1, 1, 1, 0, 704, 99
34168, V, 1, 1, 1, 1, 0, 704, 99
34169, V, 1, 1, 1, 1, 0, 704, 99
34170, V, 1, 1, 1, 1, 0, 704, 99
34171, V, 1, 1, 1, 1, 0, 704, 99
34172, V, 1, 1, 1, 1, 0, 704, 99
34173, V, 1, 1, 1, 1, 0, 704, 99
34174, V, 1, 1, 1, 1, 0, 704, 99
34176, V, 1, 1, 1, 1, 0, 704, 99
34177, V, 1, 1, 1, 1, 0, 704, 99
34178, V, 1, 1, 1, 1, 0, 704, 99
34179, V, 1, 1, 1, 1, 0, 704, 99
34180, V, 1, 1, 1, 1, 0, 704, 99
34181, V, 1, 1, 1, 1, 0, 704, 99
34182, V, 1, 1, 1, 1, 0, 704, 99
34183, V, 1, 1, 1, 1, 0, 704, 99
34184, V, 1, 1, 1, 1, 0, 704, 99
34185, V, 1, 1, 1, 1, 0, 704, 99
34186, V, 1, 1, 1, 1, 0, 704, 99
34187, V, 1, 1, 1, 1, 0, 704, 99
34188, V, 1, 1, 1, 1, 0, 704, 99
34189, V, 1, 1, 1, 1, 0, 704, 99
34190, V, 1, 1, 1, 1, 0, 704, 99
34191, V, 1, 1, 1, 1, 0, 704, 99
34192, V, 1, 1, 1, 1, 0, 704, 99
34193, V, 1, 1, 1, 1, 0, 704, 99
34194, V, 1, 1, 1, 1, 0, 704, 99
34195, V, 1, 1, 1, 1, 0, 704, 99
34196, V, 1, 1, 1, 1, 0, 704, 99
34197, V, 1, 1, 1, 1, 0, 704, 99
34198, V, 1, 1, 1, 1, 0, 704, 99
34199, V, 1, 1, 1, 1, 0, 704, 99
34200, V, 1, 1, 1, 1, 0, 704, 99
34201, V, 1, 1, 1, 1, 0, 704, 99
34202, V, 1, 1, 1, 1, 0, 704, 99
34203, V, 1, 1, 1, 1, 0, 704, 99
34204, V, 1, 1, 1, 1, 0, 704, 99
34205, V, 1, 1, 1, 1, 0, 704, 99
34206, V, 1, 1, 1, 1, 0, 704, 99
34207, V, 1, 1, 1, 1, 0, 704, 99
34208, V, 1, 1, 1, 1, 0, 704, 99
34209, V, 1, 1, 1, 1, 0, 704, 99
34210, V, 1, 1, 1, 1, 0, 704, 99
34211, V, 1, 1, 1, 1, 0, 704, 99
34212, V, 1, 1, 1, 1, 0, 704, 99
34213, V, 1, 1, 1, 1, 0, 704, 99
34214, V, 1, 1, 1, 1, 0, 704, 99
34215, V, 1, 1, 1, 1, 0, 704, 99
34216, V, 1, 1, 1, 1, 0, 704, 99
34217, V, 1, 1, 1, 1, 0, 704, 99
34219, V, 1, 1, 1, 1, 0, 704, 99
34220, V, 1, 1, 1, 1, 0, 704, 99
34221, V, 1, 1, 1, 1, 0, 704, 99
34222, V, 1, 1, 1, 1, 0, 704, 99
34223, V, 1, 1, 1, 1, 0, 704, 99
34224, V, 1, 1, 1, 1, 0, 704, 99
34225, V, 1, 1, 1, 1, 0, 704, 99
34226, V, 1, 1, 1, 1, 0, 704, 99
34227, V, 1, 1, 1, 1, 0, 704, 99
34228, V, 1, 1, 1, 1, 0, 704, 99
34229, V, 1, 1, 1, 1, 0, 704, 99
34230, V, 1, 1, 1, 1, 0, 704, 99
34231, V, 1, 1, 1, 1, 0, 704, 99
34232, V, 1, 1, 1, 1, 0, 704, 99
34233, V, 1, 1, 1, 1, 0, 704, 99
34234, V, 1, 1, 1, 1, 0, 704, 99
34235, V, 1, 1, 1, 1, 0, 704, 99
34236, V, 1, 1, 1, 1, 0, 704, 99
34237, V, 1, 1, 1, 1, 0, 704, 99
34238, V, 1, 1, 1, 1, 0, 704, 99
34239, V, 1, 1, 1, 1, 0, 704, 99
34240, V, 1, 1, 1, 1, 0, 704, 99
34241, V, 1, 1, 1, 1, 0, 704, 99
34242, V, 1, 1, 1, 1, 0, 704, 99
34243, V, 1, 1, 1, 1, 0, 704, 99
34244, V, 1, 1, 1, 1, 0, 704, 99
34245, V, 1, 1, 1, 1, 0, 704, 99
34246, V, 1, 1, 1, 1, 0, 704, 99
34247, V, 1, 1, 1, 1, 0, 704, 99
34248, V, 1, 1, 1, 1, 0, 704, 99
34249, V, 1, 1, 1, 1, 0, 704, 99
34250, V, 1, 1, 1, 1, 0, 704, 99
34251, V, 1, 1, 1, 1, 0, 704, 99
34252, V, 1, 1, 1, 1, 0, 704, 99
34253, V, 1, 1, 1, 1, 0, 704, 99
34254, V, 1, 1, 1, 1, 0, 704, 99
34255, V, 1, 1, 1, 1, 0, 704, 99
34256, V, 1, 1, 1, 1, 0, 704, 99
34257, V, 1, 1, 1, 1, 0, 704, 99
34258, V, 1, 1, 1, 1, 0, 704, 99
34259, V, 1, 1, 1, 1, 0, 704, 99
34260, V, 1, 1, 1, 1, 0, 704, 99
34262, V, 1, 1, 1, 1, 0, 704, 99
34263, V, 1, 1, 1, 1, 0, 704, 99
34264, V, 1, 1, 1, 1, 0, 704, 99
34265, V, 1, 1, 1, 1, 0, 704, 99
34266, V, 1, 1, 1, 1, 0, 704, 99
34267, V, 1, 1, 1, 1, 0, 704, 99
34268, V, 1, 1, 1, 1, 0, 704, 99
34269, V, 1, 1, 1, 1, 0, 704, 99
34270, V, 1, 1, 1, 1, 0, 704, 99
34271, V, 1, 1, 1, 1, 0, 704, 99
34272, V, 1, 1, 1, 1, 0, 704, 99
34273, V, 1, 1, 1, 1, 0, 704, 99
34274, V, 1, 1, 1, 1, 0, 704, 99
34275, V, 1, 1, 1, 1, 0, 704, 99
34276, V, 1, 1, 1, 1, 0, 704, 99
34277, V, 1, 1, 1, 1, 0, 704, 99
34278, V, 1, 1, 1, 1, 0, 704, 99
34279, V, 1, 1, 1, 1, 0, 704, 99
34280, V, 1, 1, 1, 1, 0, 704, 99
34281, V, 1, 1, 1, 1, 0, 704, 99
34282, V, 1, 1, 1, 1, 0, 704, 99
34283, V, 1, 1, 1, 1, 0, 704, 99
34284, V, 1, 1, 1, 1, 0, 704, 99
34285, V, 1, 1, 1, 1, 0, 704, 99
34286, V, 1, 1, 1, 1, 0, 704, 99
34287, V, 1, 1, 1, 1, 0, 704, 99
34288, V, 1, 1, 1, 1, 0, 704, 99
34289, V, 1, 1, 1, 1, 0, 704, 99
34290, V, 1, 1, 1, 1, 0, 704, 99
34291, V, 1, 1, 1, 1, 0, 704, 99
34292, V, 1, 1, 1, 1, 0, 704, 99
34293, V, 1, 1, 1, 1, 0, 704, 99
34294, V, 1, 1, 1, 1, 0, 704, 99
34295, V, 1, 1, 1, 1, 0, 704, 99
34296, V, 1, 1, 1, 1, 0, 704, 99
34297, V, 1, 1, 1, 1, 0, 704, 99
34298, V, 1, 1, 1, 1, 0, 704, 99
34299, V, 1, 1, 1, 1, 0, 704, 99
34300, V, 1, 1, 1, 1, 0, 704, 99
34301, V, 1, 1, 1, 1, 0, 704, 99
34302, V, 1, 1, 1, 1, 0, 704, 99
34304, V, 1, 1, 1, 1, 0, 704, 99
34305, V, 1, 1, 1, 1, 0, 704, 99
34306, V, 1, 1, 1, 1, 0, 704, 99
34307, V, 1, 1, 1, 1, 0, 704, 99
34308, V, 1, 1, 1, 1, 0, 704, 99
34309, V, 1, 1, 1, 1, 0, 704, 99
34310, V, 1, 1, 1, 1, 0, 704, 99
34311, V, 1, 1, 1, 1, 0, 704, 99
34312, V, 1, 1, 1, 1, 0, 704, 99
34313, V, 1, 1, 1, 1, 0, 704, 99
34314, V, 1, 1, 1, 1, 0, 704, 99
34315, V, 1, 1, 1, 1, 0, 704, 99
34316, V, 1, 1, 1, 1, 0, 704, 99
34317, V, 1, 1, 1, 1, 0, 704, 99
34318, V, 1, 1, 1, 1, 0, 704, 99
34319, V, 1, 1, 1, 1, 0, 704, 99
34320, V, 1, 1, 1, 1, 0, 704, 99
34321, V, 1, 1, 1, 1, 0, 704, 99
34322, V, 1, 1, 1, 1, 0, 704, 99
34323, V, 1, 1, 1, 1, 0, 704, 99
34324, V, 1, 1, 1, 1, 0, 704, 99
34325, V, 1, 1, 1, 1, 0, 704, 99
34326, V, 1, 1, 1, 1, 0, 704, 99
34327, V, 1, 1, 1, 1, 0, 704, 99
34328, V, 1, 1, 1, 1, 0, 704, 99
34329, V, 1, 1, 1, 1, 0, 704, 99
34330, V, 1, 1, 1, 1, 0, 704, 99
34331, V, 1, 1, 1, 1, 0, 704, 99
34332, V, 1, 1, 1, 1, 0, 704, 99
34333, V, 1, 1, 1, 1, 0, 704, 99
34334, V, 1, 1, 1, 1, 0, 704, 99
34335, V, 1, 1, 1, 1, 0, 704, 99
34336, V, 1, 1, 1, 1, 0, 704, 99
34337, V, 1, 1, 1, 1, 0, 704, 99
34338, V, 1, 1, 1, 1, 0, 704, 99
34339, V, 1, 1, 1, 1, 0, 704, 99
34340, V, 1, 1, 1, 1, 0, 704, 99
34341, V, 1, 1, 1, 1, 0, 704, 99
34342, V, 1, 1, 1, 1, 0, 704, 99
34343, V, 1, 1, 1, 1, 0, 704, 99
34344, V, 1, 1, 1, 1, 0, 704, 99
34345, V, 1, 1, 1, 1, 0, 704, 99
34347, V, 1, 1, 1, 1, 0, 704, 99
34348, V, 1, 1, 1, 1, 0, 704, 99
34349, V, 1, 1, 1, 1, 0, 704, 99
34350, V, 1, 1, 1, 1, 0, 704, 99
34351, V, 1, 1, 1, 1, 0, 704, 99
34352, V, 1, 1, 1, 1, 0, 704, 99
34353, V, 1, 1, 1, 1, 0, 704, 99
34354, V, 1, 1, 1, 1, 0, 704, 99
34355, V, 1, 1, 1, 1, 0, 704, 99
34356, V, 1, 1, 1, 1, 0, 704, 99
34357, V, 1, 1, 1, 1, 0, 704, 99
34358, V, 1, 1, 1, 1, 0, 704, 99
34359, V, 1, 1, 1, 1, 0, 704, 99
34360, V, 1, 1, 1, 1, 0, 704, 99
34361, V, 1, 1, 1, 1, 0, 704, 99
34362, V, 1, 1, 1, 1, 0, 704, 99
34363, V, 1, 1, 1, 1, 0, 704, 99
34364, V, 1, 1, 1, 1, 0, 704, 99
34365, V, 1, 1, 1, 1, 0, 704, 99
34366, V, 1, 1, 1, 1, 0, 704, 99
34367, V, 1, 1, 1, 1, 0, 704, 99
34368, V, 1, 1, 1, 1, 0, 704, 99
34369, V, 1, 1, 1, 1, 0, 704, 99
34370, V, 1, 1, 1, 1, 0, 704, 99
34371, V, 1, 1, 1, 1, 0, 704, 99
34372, V, 1, 1, 1, 1, 0, 704, 99
34373, V, 1, 1, 1, 1, 0, 704, 99
34374, V, 1, 1, 1, 1, 0, 704, 99
34375, V, 1, 1, 1, 1, 0, 704, 99
34376, V, 1, 1, 1, 1, 0, 704, 99
34377, V, 1, 1, 1, 1, 0, 704, 99
34378, V, 1, 1, 1, 1, 0, 704, 99
34379, V, 1, 1, 1, 1, 0, 704, 99
34380, V, 1, 1, 1, 1, 0, 704, 99
34381, V, 1, 1, 1, 1, 0, 704, 99
34382, V, 1, 1, 1, 1, 0, 704, 99
34383, V, 1, 1, 1, 1, 0, 704, 99
34384, V, 1, 1, 1, 1, 0, 704, 99
34385, V, 1, 1, 1, 1, 0, 704, 99
34386, V, 1, 1, 1, 1, 0, 704, 99
34387, V, 1, 1, 1, 1, 0, 704, 99
34388, V, 1, 1, 1, 1, 0, 704, 99
34390, V, 1, 1, 1, 1, 0, 704, 99
34391, V, 1, 1, 1, 1, 0, 704, 99
34392, V, 1, 1, 1, 1, 0, 704, 99
34393, V, 1, 1, 1, 1, 0, 704, 99
34394, V, 1, 1, 1, 1, 0, 704, 99
34395, V, 1, 1, 1, 1, 0, 704, 99
34396, V, 1, 1, 1, 1, 0, 704, 99
34397, V, 1, 1, 1, 1, 0, 704, 99
34398, V, 1, 1, 1, 1, 0, 704, 99
34399, V, 1, 1, 1, 1, 0, 704, 99
34400, V, 1, 1, 1, 1, 0, 704, 99
34401, V, 1, 1, 1, 1, 0, 704, 99
34402, V, 1, 1, 1, 1, 0, 704, 99
34403, V, 1, 1, 1, 1, 0, 704, 99
34404, V, 1, 1, 1, 1, 0, 704, 99
34405, V, 1, 1, 1, 1, 0, 704, 99
34406, V, 1, 1, 1, 1, 0, 704, 99
34407, V, 1, 1, 1, 1, 0, 704, 99
34408, V, 1, 1, 1, 1, 0, 704, 99
34409, V, 1, 1, 1, 1, 0, 704, 99
34410, V, 1, 1, 1, 1, 0, 704, 99
34411, V, 1, 1, 1, 1, 0, 704, 99
34412, V, 1, 1, 1, 1, 0, 704, 99
34413, V, 1, 1, 1, 1, 0, 704, 99
34414, V, 1, 1, 1, 1, 0, 704, 99
34415, V, 1, 1, 1, 1, 0, 704, 99
34416, V, 1, 1, 1, 1, 0, 704, 99
34417, V, 1, 1, 1, 1, 0, 704, 99
34418, V, 1, 1, 1, 1, 0, 704, 99
34419, V, 1, 1, 1, 1, 0, 704, 99
34420, V, 1, 1, 1, 1, 0, 704, 99
34421, V, 1, 1, 1, 1, 0, 704, 99
34422, V, 1, 1, 1, 1, 0, 704, 99
34423, V, 1, 1, 1, 1, 0, 704, 99
34424, V, 1, 1, 1, 1, 0, 704, 99
34425, V, 1, 1, 1, 1, 0, 704, 99
34426, V, 1, 1, 1, 1, 0, 704, 99
34427, V, 1, 1, 1, 1, 0, 704, 99
34428, V, 1, 1, 1, 1, 0, 704, 99
34429, V, 1, 1, 1, 1, 0, 704, 99
34430, V, 1, 1, 1, 1, 0, 704, 99
34432, V, 1, 1, 1, 1, 0, 704, 99
34433, V, 1, 1, 1, 1, 0, 704, 99
34434, V, 1, 1, 1, 1, 0, 704, 99
34435, V, 1, 1, 1, 1, 0, 704, 99
34436, V, 1, 1, 1, 1, 0, 704, 99
34437, V, 1, 1, 1, 1, 0, 704, 99
34438, V, 1, 1, 1, 1, 0, 704, 99
34439, V, 1, 1, 1, 1, 0, 704, 99
34440, V, 1, 1, 1, 1, 0, 704, 99
34441, V, 1, 1, 1, 1, 0, 704, 99
34442, V, 1, 1, 1, 1, 0, 704, 99
34443, V, 1, 1, 1, 1, 0, 704, 99
34444, V, 1, 1, 1, 1, 0, 704, 99
34445, V, 1, 1, 1, 1, 0, 704, 99
34446, V, 1, 1, 1, 1, 0, 704, 99
34447, V, 1, 1, 1, 1, 0, 704, 99
34448, V, 1, 1, 1, 1, 0, 704, 99
34449, V, 1, 1, 1, 1, 0, 704, 99
34450, V, 1, 1, 1, 1, 0, 704, 99
34451, V, 1, 1, 1, 1, 0, 704, 99
34452, V, 1, 1, 1, 1, 0, 704, 99
34453, V, 1, 1, 1, 1, 0, 704, 99
34454, V, 1, 1, 1, 1, 0, 704, 99
34455, V, 1, 1, 1, 1, 0, 704, 99
34456, V, 1, 1, 1, 1, 0, 704, 99
34457, V, 1, 1, 1, 1, 0, 704, 99
34458, V, 1, 1, 1, 1, 0, 704, 99
34459, V, 1, 1, 1, 1, 0, 704, 99
34460, V, 1, 1, 1, 1, 0, 704, 99
34461, V, 1, 1, 1, 1, 0, 704, 99
34462, V, 1, 1, 1, 1, 0, 704, 99
34463, V, 1, 1, 1, 1, 0, 704, 99
34464, V, 1, 1, 1, 1, 0, 704, 99
34465, V, 1, 1, 1, 1, 0, 704, 99
34466, V, 1, 1, 1, 1, 0, 704, 99
34467, V, 1, 1, 1, 1, 0, 704, 99
34468, V, 1, 1, 1, 1, 0, 704, 99
34469, V, 1, 1, 1, 1, 0, 704, 99
34470, V, 1, 1, 1, 1, 0, 704, 99
34471, V, 1, 1, 1, 1, 0, 704, 99
34472, V, 1, 1, 1, 1, 0, 704, 99
34473, V, 1, 1, 1, 1, 0, 704, 99
34475, V, 1, 1, 1, 1, 0, 704, 99
34476, V, 1, 1, 1, 1, 0, 704, 99
34477, V, 1, 1, 1, 1, 0, 704, 99
34478, V, 1, 1, 1, 1, 0, 704, 99
34479, V, 1, 1, 1, 1, 0, 704, 99
34480, V, 1, 1, 1, 1, 0, 704, 99
34481, V, 1, 1, 1, 1, 0, 704, 99
34482, V, 1, 1, 1, 1, 0, 704, 99
34483, V, 1, 1, 1, 1, 0, 704, 99
34484, V, 1, 1, 1, 1, 0, 704, 99
34485, V, 1, 1, 1, 1, 0, 704, 99
34486, V, 1, 1, 1, 1, 0, 704, 99
34487, V, 1, 1, 1, 1, 0, 704, 99
34488, V, 1, 1, 1, 1, 0, 704, 99
34489, V, 1, 1, 1, 1, 0, 704, 99
34490, V, 1, 1, 1, 1, 0, 704, 99
34491, V, 1, 1, 1, 1, 0, 704, 99
34492, V, 1, 1, 1, 1, 0, 704, 99
34493, V, 1, 1, 1, 1, 0, 704, 99
34494, V, 1, 1, 1, 1, 0, 704, 99
34495, V, 1, 1, 1, 1, 0, 704, 99
34496, V, 1, 1, 1, 1, 0, 704, 99
34497, V, 1, 1, 1, 1, 0, 704, 99
34498, V, 1, 1, 1, 1, 0, 704, 99
34499, V, 1, 1, 1, 1, 0, 704, 99
34500, V, 1, 1, 1, 1, 0, 704, 99
34501, V, 1, 1, 1, 1, 0, 704, 99
34502, V, 1, 1, 1, 1, 0, 704, 99
34503, V, 1, 1, 1, 1, 0, 704, 99
34504, V, 1, 1, 1, 1, 0, 704, 99
34505, V, 1, 1, 1, 1, 0, 704, 99
34506, V, 1, 1, 1, 1, 0, 704, 99
34507, V, 1, 1, 1, 1, 0, 704, 99
34508, V, 1, 1, 1, 1, 0, 704, 99
34509, V, 1, 1, 1, 1, 0, 704, 99
34510, V, 1, 1, 1, 1, 0, 704, 99
34511, V, 1, 1, 1, 1, 0, 704, 99
34512, V, 1, 1, 1, 1, 0, 704, 99
34513, V, 1, 1, 1, 1, 0, 704, 99
34514, V, 1, 1, 1, 1, 0, 704, 99
34515, V, 1, 1, 1, 1, 0, 704, 99
34516, V, 1, 1, 1, 1, 0, 704, 99
34518, V, 1, 1, 1, 1, 0, 704, 99
34519, V, 1, 1, 1, 1, 0, 704, 99
34520, V, 1, 1, 1, 1, 0, 704, 99
34521, V, 1, 1, 1, 1, 0, 704, 99
34522, V, 1, 1, 1, 1, 0, 704, 99
34523, V, 1, 1, 1, 1, 0, 704, 99
34524, V, 1, 1, 1, 1, 0, 704, 99
34525, V, 1, 1, 1, 1, 0, 704, 99
34526, V, 1, 1, 1, 1, 0, 704, 99
34527, V, 1, 1, 1, 1, 0, 704, 99
34528, V, 1, 1, 1, 1, 0, 704, 99
34529, V, 1, 1, 1, 1, 0, 704, 99
34530, V, 1, 1, 1, 1, 0, 704, 99
34531, V, 1, 1, 1, 1, 0, 704, 99
34532, V, 1, 1, 1, 1, 0, 704, 99
34533, V, 1, 1, 1, 1, 0, 704, 99
34534, V, 1, 1, 1, 1, 0, 704, 99
34535, V, 1, 1, 1, 1, 0, 704, 99
34536, V, 1, 1, 1, 1, 0, 704, 99
34537, V, 1, 1, 1, 1, 0, 704, 99
34538, V, 1, 1, 1, 1, 0, 704, 99
34539, V, 1, 1, 1, 1, 0, 704, 99
34540, V, 1, 1, 1, 1, 0, 704, 99
34541, V, 1, 1, 1, 1, 0, 704, 99
34542, V, 1, 1, 1, 1, 0, 704, 99
34543, V, 1, 1, 1, 1, 0, 704, 99
34544, V, 1, 1, 1, 1, 0, 704, 99
34545, V, 1, 1, 1, 1, 0, 704, 99
34546, V, 1, 1, 1, 1, 0, 704, 99
34547, V, 1, 1, 1, 1, 0, 704, 99
34548, V, 1, 1, 1, 1, 0, 704, 99
34549, V, 1, 1, 1, 1, 0, 704, 99
34550, V, 1, 1, 1, 1, 0, 704, 99
34551, V, 1, 1, 1, 1, 0, 704, 99
34552, V, 1, 1, 1, 1, 0, 704, 99
34553, V, 1, 1, 1, 1, 0, 704, 99
34554, V, 1, 1, 1, 1, 0, 704, 99
34555, V, 1, 1, 1, 1, 0, 704, 99
34556, V, 1, 1, 1, 1, 0, 704, 99
34557, V, 1, 1, 1, 1, 0, 704, 99
34558, V, 1, 1, 1, 1, 0, 704, 99
34560, V, 1, 1, 1, 1, 0, 704, 99
34561, V, 1, 1, 1, 1, 0, 704, 99
34562, V, 1, 1, 1, 1, 0, 704, 99
34563, V, 1, 1, 1, 1, 0, 704, 99
34564, V, 1, 1, 1, 1, 0, 704, 99
34565, V, 1, 1, 1, 1, 0, 704, 99
34566, V, 1, 1, 1, 1, 0, 704, 99
34567, V, 1, 1, 1, 1, 0, 704, 99
34568, V, 1, 1, 1, 1, 0, 704, 99
34569, V, 1, 1, 1, 1, 0, 704, 99
34570, V, 1, 1, 1, 1, 0, 704, 99
34571, V, 1, 1, 1, 1, 0, 704, 99
34572, V, 1, 1, 1, 1, 0, 704, 99
34573, V, 1, 1, 1, 1, 0, 704, 99
34574, V, 1, 1, 1, 1, 0, 704, 99
34575, V, 1, 1, 1, 1, 0, 704, 99
34576, V, 1, 1, 1, 1, 0, 704, 99
34577, V, 1, 1, 1, 1, 0, 704, 99
34578, V, 1, 1, 1, 1, 0, 704, 99
34579, V, 1, 1, 1, 1, 0, 704, 99
34580, V, 1, 1, 1, 1, 0, 704, 99
34581, V, 1, 1, 1, 1, 0, 704, 99
34582, V, 1, 1, 1, 1, 0, 704, 99
34583, V, 1, 1, 1, 1, 0, 704, 99
34584, V, 1, 1, 1, 1, 0, 704, 99
34585, V, 1, 1, 1, 1, 0, 704, 99
34586, V, 1, 1, 1, 1, 0, 704, 99
34587, V, 1, 1, 1, 1, 0, 704, 99
34588, V, 1, 1, 1, 1, 0, 704, 99
34589, V, 1, 1, 1, 1, 0, 704, 99
34590, V, 1, 1, 1, 1, 0, 704, 99
34591, V, 1, 1, 1, 1, 0, 704, 99
34592, V, 1, 1, 1, 1, 0, 704, 99
34593, V, 1, 1, 1, 1, 0, 704, 99
34594, V, 1, 1, 1, 1, 0, 704, 99
34595, V, 1, 1, 1, 1, 0, 704, 99
34596, V, 1, 1, 1, 1, 0, 704, 99
34597, V, 1, 1, 1, 1, 0, 704, 99
34598, V, 1, 1, 1, 1, 0, 704, 99
34599, V, 1, 1, 1, 1, 0, 704, 99
34600, V, 1, 1, 1, 1, 0, 704, 99
34601, V, 1, 1, 1, 1, 0, 704, 99
34603, V, 1, 1, 1, 1, 0, 704, 99
34604, V, 1, 1, 1, 1, 0, 704, 99
34605, V, 1, 1, 1, 1, 0, 704, 99
34606, V, 1, 1, 1, 1, 0, 704, 99
34607, V, 1, 1, 1, 1, 0, 704, 99
34608, V, 1, 1, 1, 1, 0, 704, 99
34609, V, 1, 1, 1, 1, 0, 704, 99
34610, V, 1, 1, 1, 1, 0, 704, 99
34611, V, 1, 1, 1, 1, 0, 704, 99
34612, V, 1, 1, 1, 1, 0, 704, 99
34613, V, 1, 1, 1, 1, 0, 704, 99
34614, V, 1, 1, 1, 1, 0, 704, 99
34615, V, 1, 1, 1, 1, 0, 704, 99
34616, V, 1, 1, 1, 1, 0, 704, 99
34617, V, 1, 1, 1, 1, 0, 704, 99
34618, V, 1, 1, 1, 1, 0, 704, 99
34619, V, 1, 1, 1, 1, 0, 704, 99
34620, V, 1, 1, 1, 1, 0, 704, 99
34621, V, 1, 1, 1, 1, 0, 704, 99
34622, V, 1, 1, 1, 1, 0, 704, 99
34623, V, 1, 1, 1, 1, 0, 704, 99
34624, V, 1, 1, 1, 1, 0, 704, 99
34625, V, 1, 1, 1, 1, 0, 704, 99
34626, V, 1, 1, 1, 1, 0, 704, 99
34627, V, 1, 1, 1, 1, 0, 704, 99
34628, V, 1, 1, 1, 1, 0, 704, 99
34629, V, 1, 1, 1, 1, 0, 704, 99
34630, V, 1, 1, 1, 1, 0, 704, 99
34631, V, 1, 1, 1, 1, 0, 704, 99
34632, V, 1, 1, 1, 1, 0, 704, 99
34633, V, 1, 1, 1, 1, 0, 704, 99
34634, V, 1, 1, 1, 1, 0, 704, 99
34635, V, 1, 1, 1, 1, 0, 704, 99
34636, V, 1, 1, 1, 1, 0, 704, 99
34637, V, 1, 1, 1, 1, 0, 704, 99
34638, V, 1, 1, 1, 1, 0, 704, 99
34639, V, 1, 1, 1, 1, 0, 704, 99
34640, V, 1, 1, 1, 1, 0, 704, 99
34641, V, 1, 1, 1, 1, 0, 704, 99
34642, V, 1, 1, 1, 1, 0, 704, 99
34643, V, 1, 1, 1, 1, 0, 704, 99
34644, V, 1, 1, 1, 1, 0, 704, 99
34646, V, 1, 1, 1, 1, 0, 704, 99
34647, V, 1, 1, 1, 1, 0, 704, 99
34648, V, 1, 1, 1, 1, 0, 704, 99
34649, V, 1, 1, 1, 1, 0, 704, 99
34650, V, 1, 1, 1, 1, 0, 704, 99
34651, V, 1, 1, 1, 1, 0, 704, 99
34652, V, 1, 1, 1, 1, 0, 704, 99
34653, V, 1, 1, 1, 1, 0, 704, 99
34654, V, 1, 1, 1, 1, 0, 704, 99
34655, V, 1, 1, 1, 1, 0, 704, 99
34656, V, 1, 1, 1, 1, 0, 704, 99
34657, V, 1, 1, 1, 1, 0, 704, 99
34658, V, 1, 1, 1, 1, 0, 704, 99
34659, V, 1, 1, 1, 1, 0, 704, 99
34660, V, 1, 1, 1, 1, 0, 704, 99
34661, V, 1, 1, 1, 1, 0, 704, 99
34662, V, 1, 1, 1, 1, 0, 704, 99
34663, V, 1, 1, 1, 1, 0, 704, 99
34664, V, 1, 1, 1, 1, 0, 704, 99
34665, V, 1, 1, 1, 1, 0, 704, 99
34666, V, 1, 1, 1, 1, 0, 704, 99
34667, V, 1, 1, 1, 1, 0, 704, 99
34668, V, 1, 1, 1, 1, 0, 704, 99
34669, V, 1, 1, 1, 1, 0, 704, 99
34670, V, 1, 1, 1, 1, 0, 704, 99
34671, V, 1, 1, 1, 1, 0, 704, 99
34672, V, 1, 1, 1, 1, 0, 704, 99
34673, V, 1, 1, 1, 1, 0, 704, 99
34674, V, 1, 1, 1, 1, 0, 704, 99
34675, V, 1, 1, 1, 1, 0, 704, 99
34676, V, 1, 1, 1, 1, 0, 704, 99
34677, V, 1, 1, 1, 1, 0, 704, 99
34678, V, 1, 1, 1, 1, 0, 704, 99
34679, V, 1, 1, 1, 1, 0, 704, 99
34680, V, 1, 1, 1, 1, 0, 704, 99
34681, V, 1, 1, 1, 1, 0, 704, 99
34682, V, 1, 1, 1, 1, 0, 704, 99
34683, V, 1, 1, 1, 1, 0, 704, 99
34684, V, 1, 1, 1, 1, 0, 704, 99
34685, V, 1, 1, 1, 1, 0, 704, 99
34686, V, 1, 1, 1, 1, 0, 704, 99
34688, V, 1, 1, 1, 1, 0, 704, 99
34689, V, 1, 1, 1, 1, 0, 704, 99
34690, V, 1, 1, 1, 1, 0, 704, 99
34691, V, 1, 1, 1, 1, 0, 704, 99
34692, V, 1, 1, 1, 1, 0, 704, 99
34693, V, 1, 1, 1, 1, 0, 704, 99
34694, V, 1, 1, 1, 1, 0, 704, 99
34695, V, 1, 1, 1, 1, 0, 704, 99
34696, V, 1, 1, 1, 1, 0, 704, 99
34697, V, 1, 1, 1, 1, 0, 704, 99
34698, V, 1, 1, 1, 1, 0, 704, 99
34699, V, 1, 1, 1, 1, 0, 704, 99
34700, V, 1, 1, 1, 1, 0, 704, 99
34701, V, 1, 1, 1, 1, 0, 704, 99
34702, V, 1, 1, 1, 1, 0, 704, 99
34703, V, 1, 1, 1, 1, 0, 704, 99
34704, V, 1, 1, 1, 1, 0, 704, 99
34705, V, 1, 1, 1, 1, 0, 704, 99
34706, V, 1, 1, 1, 1, 0, 704, 99
34707, V, 1, 1, 1, 1, 0, 704, 99
34708, V, 1, 1, 1, 1, 0, 704, 99
34709, V, 1, 1, 1, 1, 0, 704, 99
34710, V, 1, 1, 1, 1, 0, 704, 99
34711, V, 1, 1, 1, 1, 0, 704, 99
34712, V, 1, 1, 1, 1, 0, 704, 99
34713, V, 1, 1, 1, 1, 0, 704, 99
34714, V, 1, 1, 1, 1, 0, 704, 99
34715, V, 1, 1, 1, 1, 0, 704, 99
34716, V, 1, 1, 1, 1, 0, 704, 99
34717, V, 1, 1, 1, 1, 0, 704, 99
34718, V, 1, 1, 1, 1, 0, 704, 99
34719, V, 1, 1, 1, 1, 0, 704, 99
34720, V, 1, 1, 1, 1, 0, 704, 99
34721, V, 1, 1, 1, 1, 0, 704, 99
34722, V, 1, 1, 1, 1, 0, 704, 99
34723, V, 1, 1, 1, 1, 0, 704, 99
34724, V, 1, 1, 1, 1, 0, 704, 99
34725, V, 1, 1, 1, 1, 0, 704, 99
34726, V, 1, 1, 1, 1, 0, 704, 99
34727, V, 1, 1, 1, 1, 0, 704, 99
34728, V, 1, 1, 1, 1, 0, 704, 99
34729, V, 1, 1, 1, 1, 0, 704, 99
34731, V, 1, 1, 1, 1, 0, 704, 99
34732, V, 1, 1, 1, 1, 0, 704, 99
34733, V, 1, 1, 1, 1, 0, 704, 99
34734, V, 1, 1, 1, 1, 0, 704, 99
34735, V, 1, 1, 1, 1, 0, 704, 99
34736, V, 1, 1, 1, 1, 0, 704, 99
34737, V, 1, 1, 1, 1, 0, 704, 99
34738, V, 1, 1, 1, 1, 0, 704, 99
34739, V, 1, 1, 1, 1, 0, 704, 99
34740, V, 1, 1, 1, 1, 0, 704, 99
34741, V, 1, 1, 1, 1, 0, 704, 99
34742, V, 1, 1, 1, 1, 0, 704, 99
34743, V, 1, 1, 1, 1, 0, 704, 99
34744, V, 1, 1, 1, 1, 0, 704, 99
34745, V, 1, 1, 1, 1, 0, 704, 99
34746, V, 1, 1, 1, 1, 0, 704, 99
34747, V, 1, 1, 1, 1, 0, 704, 99
34748, V, 1, 1, 1, 1, 0, 704, 99
34749, V, 1, 1, 1, 1, 0, 704, 99
34750, V, 1, 1, 1, 1, 0, 704, 99
34751, V, 1, 1, 1, 1, 0, 704, 99
34752, V, 1, 1, 1, 1, 0, 704, 99
34753, V, 1, 1, 1, 1, 0, 704, 99
34754, V, 1, 1, 1, 1, 0, 704, 99
34755, V, 1, 1, 1, 1, 0, 704, 99
34756, V, 1, 1, 1, 1, 0, 704, 99
34757, V, 1, 1, 1, 1, 0, 704, 99
34758, V, 1, 1, 1, 1, 0, 704, 99
34759, V, 1, 1, 1, 1, 0, 704, 99
34760, V, 1, 1, 1, 1, 0, 704, 99
34761, V, 1, 1, 1, 1, 0, 704, 99
34762, V, 1, 1, 1, 1, 0, 704, 99
34763, V, 1, 1, 1, 1, 0, 704, 99
34764, V, 1, 1, 1, 1, 0, 704, 99
34765, V, 1, 1, 1, 1, 0, 704, 99
34766, V, 1, 1, 1, 1, 0, 704, 99
34767, V, 1, 1, 1, 1, 0, 704, 99
34768, V, 1, 1, 1, 1, 0, 704, 99
34769, V, 1, 1, 1, 1, 0, 704, 99
34770, V, 1, 1, 1, 1, 0, 704, 99
34771, V, 1, 1, 1, 1, 0, 704, 99
34772, V, 1, 1, 1, 1, 0, 704, 99
34774, V, 1, 1, 1, 1, 0, 704, 99
34775, V, 1, 1, 1, 1, 0, 704, 99
34776, V, 1, 1, 1, 1, 0, 704, 99
34777, V, 1, 1, 1, 1, 0, 704, 99
34778, V, 1, 1, 1, 1, 0, 704, 99
34779, V, 1, 1, 1, 1, 0, 704, 99
34780, V, 1, 1, 1, 1, 0, 704, 99
34781, V, 1, 1, 1, 1, 0, 704, 99
34782, V, 1, 1, 1, 1, 0, 704, 99
34783, V, 1, 1, 1, 1, 0, 704, 99
34784, V, 1, 1, 1, 1, 0, 704, 99
34785, V, 1, 1, 1, 1, 0, 704, 99
34786, V, 1, 1, 1, 1, 0, 704, 99
34787, V, 1, 1, 1, 1, 0, 704, 99
34788, V, 1, 1, 1, 1, 0, 704, 99
34789, V, 1, 1, 1, 1, 0, 704, 99
34790, V, 1, 1, 1, 1, 0, 704, 99
34791, V, 1, 1, 1, 1, 0, 704, 99
34792, V, 1, 1, 1, 1, 0, 704, 99
34793, V, 1, 1, 1, 1, 0, 704, 99
34794, V, 1, 1, 1, 1, 0, 704, 99
34795, V, 1, 1, 1, 1, 0, 704, 99
34796, V, 1, 1, 1, 1, 0, 704, 99
34797, V, 1, 1, 1, 1, 0, 704, 99
34798, V, 1, 1, 1, 1, 0, 704, 99
34799, V, 1, 1, 1, 1, 0, 704, 99
34800, V, 1, 1, 1, 1, 0, 704, 99
34801, V, 1, 1, 1, 1, 0, 704, 99
34802, V, 1, 1, 1, 1, 0, 704, 99
34803, V, 1, 1, 1, 1, 0, 704, 99
34804, V, 1, 1, 1, 1, 0, 704, 99
34805, V, 1, 1, 1, 1, 0, 704, 99
34806, V, 1, 1, 1, 1, 0, 704, 99
34807, V, 1, 1, 1, 1, 0, 704, 99
34808, V, 1, 1, 1, 1, 0, 704, 99
34809, V, 1, 1, 1, 1, 0, 704, 99
34810, V, 1, 1, 1, 1, 0, 704, 99
34811, V, 1, 1, 1, 1, 0, 704, 99
34812, V, 1, 1, 1, 1, 0, 704, 99
34813, V, 1, 1, 1, 1, 0, 704, 99
34814, V, 1, 1, 1, 1, 0, 704, 99
34816, V, 1, 1, 1, 1, 0, 704, 99
34817, V, 1, 1, 1, 1, 0, 704, 99
34818, V, 1, 1, 1, 1, 0, 704, 99
34819, V, 1, 1, 1, 1, 0, 704, 99
34820, V, 1, 1, 1, 1, 0, 704, 99
34821, V, 1, 1, 1, 1, 0, 704, 99
34822, V, 1, 1, 1, 1, 0, 704, 99
34823, V, 1, 1, 1, 1, 0, 704, 99
34824, V, 1, 1, 1, 1, 0, 704, 99
34825, V, 1, 1, 1, 1, 0, 704, 99
34826, V, 1, 1, 1, 1, 0, 704, 99
34827, V, 1, 1, 1, 1, 0, 704, 99
34828, V, 1, 1, 1, 1, 0, 704, 99
34829, V, 1, 1, 1, 1, 0, 704, 99
34830, V, 1, 1, 1, 1, 0, 704, 99
34831, V, 1, 1, 1, 1, 0, 704, 99
34832, V, 1, 1, 1, 1, 0, 704, 99
34833, V, 1, 1, 1, 1, 0, 704, 99
34834, V, 1, 1, 1, 1, 0, 704, 99
34835, V, 1, 1, 1, 1, 0, 704, 99
34836, V, 1, 1, 1, 1, 0, 704, 99
34837, V, 1, 1, 1, 1, 0, 704, 99
34838, V, 1, 1, 1, 1, 0, 704, 99
34839, V, 1, 1, 1, 1, 0, 704, 99
34840, V, 1, 1, 1, 1, 0, 704, 99
34841, V, 1, 1, 1, 1, 0, 704, 99
34842, V, 1, 1, 1, 1, 0, 704, 99
34843, V, 1, 1, 1, 1, 0, 704, 99
34844, V, 1, 1, 1, 1, 0, 704, 99
34845, V, 1, 1, 1, 1, 0, 704, 99
34846, V, 1, 1, 1, 1, 0, 704, 99
34847, V, 1, 1, 1, 1, 0, 704, 99
34848, V, 1, 1, 1, 1, 0, 704, 99
34849, V, 1, 1, 1, 1, 0, 704, 99
34850, V, 1, 1, 1, 1, 0, 704, 99
34851, V, 1, 1, 1, 1, 0, 704, 99
34852, V, 1, 1, 1, 1, 0, 704, 99
34853, V, 1, 1, 1, 1, 0, 704, 99
34854, V, 1, 1, 1, 1, 0, 704, 99
34855, V, 1, 1, 1, 1, 0, 704, 99
34856, V, 1, 1, 1, 1, 0, 704, 99
34857, V, 1, 1, 1, 1, 0, 704, 99
34859, V, 1, 1, 1, 1, 0, 704, 99
34860, V, 1, 1, 1, 1, 0, 704, 99
34861, V, 1, 1, 1, 1, 0, 704, 99
34862, V, 1, 1, 1, 1, 0, 704, 99
34863, V, 1, 1, 1, 1, 0, 704, 99
34864, V, 1, 1, 1, 1, 0, 704, 99
34865, V, 1, 1, 1, 1, 0, 704, 99
34866, V, 1, 1, 1, 1, 0, 704, 99
34867, V, 1, 1, 1, 1, 0, 704, 99
34868, V, 1, 1, 1, 1, 0, 704, 99
34869, V, 1, 1, 1, 1, 0, 704, 99
34870, V, 1, 1, 1, 1, 0, 704, 99
34871, V, 1, 1, 1, 1, 0, 704, 99
34872, V, 1, 1, 1, 1, 0, 704, 99
34873, V, 1, 1, 1, 1, 0, 704, 99
34874, V, 1, 1, 1, 1, 0, 704, 99
34875, V, 1, 1, 1, 1, 0, 704, 99
34876, V, 1, 1, 1, 1, 0, 704, 99
34877, V, 1, 1, 1, 1, 0, 704, 99
34878, V, 1, 1, 1, 1, 0, 704, 99
34879, V, 1, 1, 1, 1, 0, 704, 99
34880, V, 1, 1, 1, 1, 0, 704, 99
34881, V, 1, 1, 1, 1, 0, 704, 99
34882, V, 1, 1, 1, 1, 0, 704, 99
34883, V, 1, 1, 1, 1, 0, 704, 99
34884, V, 1, 1, 1, 1, 0, 704, 99
34885, V, 1, 1, 1, 1, 0, 704, 99
34886, V, 1, 1, 1, 1, 0, 704, 99
34887, V, 1, 1, 1, 1, 0, 704, 99
34888, V, 1, 1, 1, 1, 0, 704, 99
34889, V, 1, 1, 1, 1, 0, 704, 99
34890, V, 1, 1, 1, 1, 0, 704, 99
34891, V, 1, 1, 1, 1, 0, 704, 99
34892, V, 1, 1, 1, 1, 0, 704, 99
34893, V, 1, 1, 1, 1, 0, 704, 99
34894, V, 1, 1, 1, 1, 0, 704, 99
34895, V, 1, 1, 1, 1, 0, 704, 99
34896, V, 1, 1, 1, 1, 0, 704, 99
34897, V, 1, 1, 1, 1, 0, 704, 99
34898, V, 1, 1, 1, 1, 0, 704, 99
34899, V, 1, 1, 1, 1, 0, 704, 99
34900, V, 1, 1, 1, 1, 0, 704, 99
34902, V, 1, 1, 1, 1, 0, 704, 99
34903, V, 1, 1, 1, 1, 0, 704, 99
34904, V, 1, 1, 1, 1, 0, 704, 99
34905, V, 1, 1, 1, 1, 0, 704, 99
34906, V, 1, 1, 1, 1, 0, 704, 99
34907, V, 1, 1, 1, 1, 0, 704, 99
34908, V, 1, 1, 1, 1, 0, 704, 99
34909, V, 1, 1, 1, 1, 0, 704, 99
34910, V, 1, 1, 1, 1, 0, 704, 99
34911, V, 1, 1, 1, 1, 0, 704, 99
34912, V, 1, 1, 1, 1, 0, 704, 99
34913, V, 1, 1, 1, 1, 0, 704, 99
34914, V, 1, 1, 1, 1, 0, 704, 99
34915, V, 1, 1, 1, 1, 0, 704, 99
34916, V, 1, 1, 1, 1, 0, 704, 99
34917, V, 1, 1, 1, 1, 0, 704, 99
34918, V, 1, 1, 1, 1, 0, 704, 99
34919, V, 1, 1, 1, 1, 0, 704, 99
34920, V, 1, 1, 1, 1, 0, 704, 99
34921, V, 1, 1, 1, 1, 0, 704, 99
34922, V, 1, 1, 1, 1, 0, 704, 99
34923, V, 1, 1, 1, 1, 0, 704, 99
34924, V, 1, 1, 1, 1, 0, 704, 99
34925, V, 1, 1, 1, 1, 0, 704, 99
34926, V, 1, 1, 1, 1, 0, 704, 99
34927, V, 1, 1, 1, 1, 0, 704, 99
34928, V, 1, 1, 1, 1, 0, 704, 99
34929, V, 1, 1, 1, 1, 0, 704, 99
34930, V, 1, 1, 1, 1, 0, 704, 99
34931, V, 1, 1, 1, 1, 0, 704, 99
34932, V, 1, 1, 1, 1, 0, 704, 99
34933, V, 1, 1, 1, 1, 0, 704, 99
34934, V, 1, 1, 1, 1, 0, 704, 99
34935, V, 1, 1, 1, 1, 0, 704, 99
34936, V, 1, 1, 1, 1, 0, 704, 99
34937, V, 1, 1, 1, 1, 0, 704, 99
34938, V, 1, 1, 1, 1, 0, 704, 99
34939, V, 1, 1, 1, 1, 0, 704, 99
34940, V, 1, 1, 1, 1, 0, 704, 99
34941, V, 1, 1, 1, 1, 0, 704, 99
34942, V, 1, 1, 1, 1, 0, 704, 99
34944, V, 1, 1, 1, 1, 0, 704, 99
34945, V, 1, 1, 1, 1, 0, 704, 99
34946, V, 1, 1, 1, 1, 0, 704, 99
34947, V, 1, 1, 1, 1, 0, 704, 99
34948, V, 1, 1, 1, 1, 0, 704, 99
34949, V, 1, 1, 1, 1, 0, 704, 99
34950, V, 1, 1, 1, 1, 0, 704, 99
34951, V, 1, 1, 1, 1, 0, 704, 99
34952, V, 1, 1, 1, 1, 0, 704, 99
34953, V, 1, 1, 1, 1, 0, 704, 99
34954, V, 1, 1, 1, 1, 0, 704, 99
34955, V, 1, 1, 1, 1, 0, 704, 99
34956, V, 1, 1, 1, 1, 0, 704, 99
34957, V, 1, 1, 1, 1, 0, 704, 99
34958, V, 1, 1, 1, 1, 0, 704, 99
34959, V, 1, 1, 1, 1, 0, 704, 99
34960, V, 1, 1, 1, 1, 0, 704, 99
34961, V, 1, 1, 1, 1, 0, 704, 99
34962, V, 1, 1, 1, 1, 0, 704, 99
34963, V, 1, 1, 1, 1, 0, 704, 99
34964, V, 1, 1, 1, 1, 0, 704, 99
34965, V, 1, 1, 1, 1, 0, 704, 99
34966, V, 1, 1, 1, 1, 0, 704, 99
34967, V, 1, 1, 1, 1, 0, 704, 99
34968, V, 1, 1, 1, 1, 0, 704, 99
34969, V, 1, 1, 1, 1, 0, 704, 99
34970, V, 1, 1, 1, 1, 0, 704, 99
34971, V, 1, 1, 1, 1, 0, 704, 99
34972, V, 1, 1, 1, 1, 0, 704, 99
34973, V, 1, 1, 1, 1, 0, 704, 99
34974, V, 1, 1, 1, 1, 0, 704, 99
34975, V, 1, 1, 1, 1, 0, 704, 99
34976, V, 1, 1, 1, 1, 0, 704, 99
34977, V, 1, 1, 1, 1, 0, 704, 99
34978, V, 1, 1, 1, 1, 0, 704, 99
34979, V, 1, 1, 1, 1, 0, 704, 99
34980, V, 1, 1, 1, 1, 0, 704, 99
34981, V, 1, 1, 1, 1, 0, 704, 99
34982, V, 1, 1, 1, 1, 0, 704, 99
34983, V, 1, 1, 1, 1, 0, 704, 99
34984, V, 1, 1, 1, 1, 0, 704, 99
34985, V, 1, 1, 1, 1, 0, 704, 99
34987, V, 1, 1, 1, 1, 0, 704, 99
34988, V, 1, 1, 1, 1, 0, 704, 99
34989, V, 1, 1, 1, 1, 0, 704, 99
34990, V, 1, 1, 1, 1, 0, 704, 99
34991, V, 1, 1, 1, 1, 0, 704, 99
34992, V, 1, 1, 1, 1, 0, 704, 99
34993, V, 1, 1, 1, 1, 0, 704, 99
34994, V, 1, 1, 1, 1, 0, 704, 99
34995, V, 1, 1, 1, 1, 0, 704, 99
34996, V, 1, 1, 1, 1, 0, 704, 99
34997, V, 1, 1, 1, 1, 0, 704, 99
34998, V, 1, 1, 1, 1, 0, 704, 99
34999, V, 1, 1, 1, 1, 0, 704, 99
35000, V, 1, 1, 1, 1, 0, 704, 99
35001, V, 1, 1, 1, 1, 0, 704, 99
35002, V, 1, 1, 1, 1, 0, 704, 99
35003, V, 1, 1, 1, 1, 0, 704, 99
35004, V, 1, 1, 1, 1, 0, 704, 99
35005, V, 1, 1, 1, 1, 0, 704, 99
35006, V, 1, 1, 1, 1, 0, 704, 99
35007, V, 1, 1, 1, 1, 0, 704, 99
35008, V, 1, 1, 1, 1, 0, 704, 99
35009, V, 1, 1, 1, 1, 0, 704, 99
35010, V, 1, 1, 1, 1, 0, 704, 99
35011, V, 1, 1, 1, 1, 0, 704, 99
35012, V, 1, 1, 1, 1, 0, 704, 99
35013, V, 1, 1, 1, 1, 0, 704, 99
35014, V, 1, 1, 1, 1, 0, 704, 99
35015, V, 1, 1, 1, 1, 0, 704, 99
35016, V, 1, 1, 1, 1, 0, 704, 99
35017, V, 1, 1, 1, 1, 0, 704, 99
35018, V, 1, 1, 1, 1, 0, 704, 99
35019, V, 1, 1, 1, 1, 0, 704, 99
35020, V, 1, 1, 1, 1, 0, 704, 99
35021, V, 1, 1, 1, 1, 0, 704, 99
35022, V, 1, 1, 1, 1, 0, 704, 99
35023, V, 1, 1, 1, 1, 0, 704, 99
35024, V, 1, 1, 1, 1, 0, 704, 99
35025, V, 1, 1, 1, 1, 0, 704, 99
35026, V, 1, 1, 1, 1, 0, 704, 99
35027, V, 1, 1, 1, 1, 0, 704, 99
35028, V, 1, 1, 1, 1, 0, 704, 99
35030, V, 1, 1, 1, 1, 0, 704, 99
35031, V, 1, 1, 1, 1, 0, 704, 99
35032, V, 1, 1, 1, 1, 0, 704, 99
35033, V, 1, 1, 1, 1, 0, 704, 99
35034, V, 1, 1, 1, 1, 0, 704, 99
35035, V, 1, 1, 1, 1, 0, 704, 99
35036, V, 1, 1, 1, 1, 0, 704, 99
35037, V, 1, 1, 1, 1, 0, 704, 99
35038, V, 1, 1, 1, 1, 0, 704, 99
35039, V, 1, 1, 1, 1, 0, 704, 99
35040, V, 1, 1, 1, 1, 0, 704, 99
35041, V, 1, 1, 1, 1, 0, 704, 99
35042, V, 1, 1, 1, 1, 0, 704, 99
35043, V, 1, 1, 1, 1, 0, 704, 99
35044, V, 1, 1, 1, 1, 0, 704, 99
35045, V, 1, 1, 1, 1, 0, 704, 99
35046, V, 1, 1, 1, 1, 0, 704, 99
35047, V, 1, 1, 1, 1, 0, 704, 99
35048, V, 1, 1, 1, 1, 0, 704, 99
35049, V, 1, 1, 1, 1, 0, 704, 99
35050, V, 1, 1, 1, 1, 0, 704, 99
35051, V, 1, 1, 1, 1, 0, 704, 99
35052, V, 1, 1, 1, 1, 0, 704, 99
35053, V, 1, 1, 1, 1, 0, 704, 99
35054, V, 1, 1, 1, 1, 0, 704, 99
35055, V, 1, 1, 1, 1, 0, 704, 99
35056, V, 1, 1, 1, 1, 0, 704, 99
35057, V, 1, 1, 1, 1, 0, 704, 99
35058, V, 1, 1, 1, 1, 0, 704, 99
35059, V, 1, 1, 1, 1, 0, 704, 99
35060, V, 1, 1, 1, 1, 0, 704, 99
35061, V, 1, 1, 1, 1, 0, 704, 99
35062, V, 1, 1, 1, 1, 0, 704, 99
35063, V, 1, 1, 1, 1, 0, 704, 99
35064, V, 1, 1, 1, 1, 0, 704, 99
35065, V, 1, 1, 1, 1, 0, 704, 99
35066, V, 1, 1, 1, 1, 0, 704, 99
35067, V, 1, 1, 1, 1, 0, 704, 99
35068, V, 1, 1, 1, 1, 0, 704, 99
35069, V, 1, 1, 1, 1, 0, 704, 99
35070, V, 1, 1, 1, 1, 0, 704, 99
35072, V, 1, 1, 1, 1, 0, 704, 99
35073, V, 1, 1, 1, 1, 0, 704, 99
35074, V, 1, 1, 1, 1, 0, 704, 99
35075, V, 1, 1, 1, 1, 0, 704, 99
35076, V, 1, 1, 1, 1, 0, 704, 99
35077, V, 1, 1, 1, 1, 0, 704, 99
35078, V, 1, 1, 1, 1, 0, 704, 99
35079, V, 1, 1, 1, 1, 0, 704, 99
35080, V, 1, 1, 1, 1, 0, 704, 99
35081, V, 1, 1, 1, 1, 0, 704, 99
35082, V, 1, 1, 1, 1, 0, 704, 99
35083, V, 1, 1, 1, 1, 0, 704, 99
35084, V, 1, 1, 1, 1, 0, 704, 99
35085, V, 1, 1, 1, 1, 0, 704, 99
35086, V, 1, 1, 1, 1, 0, 704, 99
35087, V, 1, 1, 1, 1, 0, 704, 99
35088, V, 1, 1, 1, 1, 0, 704, 99
35089, V, 1, 1, 1, 1, 0, 704, 99
35090, V, 1, 1, 1, 1, 0, 704, 99
35091, V, 1, 1, 1, 1, 0, 704, 99
35092, V, 1, 1, 1, 1, 0, 704, 99
35093, V, 1, 1, 1, 1, 0, 704, 99
35094, V, 1, 1, 1, 1, 0, 704, 99
35095, V, 1, 1, 1, 1, 0, 704, 99
35096, V, 1, 1, 1, 1, 0, 704, 99
35097, V, 1, 1, 1, 1, 0, 704, 99
35098, V, 1, 1, 1, 1, 0, 704, 99
35099, V, 1, 1, 1, 1, 0, 704, 99
35100, V, 1, 1, 1, 1, 0, 704, 99
35101, V, 1, 1, 1, 1, 0, 704, 99
35102, V, 1, 1, 1, 1, 0, 704, 99
35103, V, 1, 1, 1, 1, 0, 704, 99
35104, V, 1, 1, 1, 1, 0, 704, 99
35105, V, 1, 1, 1, 1, 0, 704, 99
35106, V, 1, 1, 1, 1, 0, 704, 99
35107, V, 1, 1, 1, 1, 0, 704, 99
35108, V, 1, 1, 1, 1, 0, 704, 99
35109, V, 1, 1, 1, 1, 0, 704, 99
35110, V, 1, 1, 1, 1, 0, 704, 99
35111, V, 1, 1, 1, 1, 0, 704, 99
35112, V, 1, 1, 1, 1, 0, 704, 99
35113, V, 1, 1, 1, 1, 0, 704, 99
35115, V, 1, 1, 1, 1, 0, 704, 99
35116, V, 1, 1, 1, 1, 0, 704, 99
35117, V, 1, 1, 1, 1, 0, 704, 99
35118, V, 1, 1, 1, 1, 0, 704, 99
35119, V, 1, 1, 1, 1, 0, 704, 99
35120, V, 1, 1, 1, 1, 0, 704, 99
35121, V, 1, 1, 1, 1, 0, 704, 99
35122, V, 1, 1, 1, 1, 0, 704, 99
35123, V, 1, 1, 1, 1, 0, 704, 99
35124, V, 1, 1, 1, 1, 0, 704, 99
35125, V, 1, 1, 1, 1, 0, 704, 99
35126, V, 1, 1, 1, 1, 0, 704, 99
35127, V, 1, 1, 1, 1, 0, 704, 99
35128, V, 1, 1, 1, 1, 0, 704, 99
35129, V, 1, 1, 1, 1, 0, 704, 99
35130, V, 1, 1, 1, 1, 0, 704, 99
35131, V, 1, 1, 1, 1, 0, 704, 99
35132, V, 1, 1, 1, 1, 0, 704, 99
35133, V, 1, 1, 1, 1, 0, 704, 99
35134, V, 1, 1, 1, 1, 0, 704, 99
35135, V, 1, 1, 1, 1, 0, 704, 99
35136, V, 1, 1, 1, 1, 0, 704, 99
35137, V, 1, 1, 1, 1, 0, 704, 99
35138, V, 1, 1, 1, 1, 0, 704, 99
35139, V, 1, 1, 1, 1, 0, 704, 99
35140, V, 1, 1, 1, 1, 0, 704, 99
35141, V, 1, 1, 1, 1, 0, 704, 99
35142, V, 1, 1, 1, 1, 0, 704, 99
35143, V, 1, 1, 1, 1, 0, 704, 99
35144, V, 1, 1, 1, 1, 0, 704, 99
35145, V, 1, 1, 1, 1, 0, 704, 99
35146, V, 1, 1, 1, 1, 0, 704, 99
35147, V, 1, 1, 1, 1, 0, 704, 99
35148, V, 1, 1, 1, 1, 0, 704, 99
35149, V, 1, 1, 1, 1, 0, 704, 99
35150, V, 1, 1, 1, 1, 0, 704, 99
35151, V, 1, 1, 1, 1, 0, 704, 99
35152, V, 1, 1, 1, 1, 0, 704, 99
35153, V, 1, 1, 1, 1, 0, 704, 99
35154, V, 1, 1, 1, 1, 0, 704, 99
35155, V, 1, 1, 1, 1, 0, 704, 99
35156, V, 1, 1, 1, 1, 0, 704, 99
35158, V, 1, 1, 1, 1, 0, 704, 99
35159, V, 1, 1, 1, 1, 0, 704, 99
35160, V, 1, 1, 1, 1, 0, 704, 99
35161, V, 1, 1, 1, 1, 0, 704, 99
35162, V, 1, 1, 1, 1, 0, 704, 99
35163, V, 1, 1, 1, 1, 0, 704, 99
35164, V, 1, 1, 1, 1, 0, 704, 99
35165, V, 1, 1, 1, 1, 0, 704, 99
35166, V, 1, 1, 1, 1, 0, 704, 99
35167, V, 1, 1, 1, 1, 0, 704, 99
35168, V, 1, 1, 1, 1, 0, 704, 99
35169, V, 1, 1, 1, 1, 0, 704, 99
35170, V, 1, 1, 1, 1, 0, 704, 99
35171, V, 1, 1, 1, 1, 0, 704, 99
35172, V, 1, 1, 1, 1, 0, 704, 99
35173, V, 1, 1, 1, 1, 0, 704, 99
35174, V, 1, 1, 1, 1, 0, 704, 99
35175, V, 1, 1, 1, 1, 0, 704, 99
35176, V, 1, 1, 1, 1, 0, 704, 99
35177, V, 1, 1, 1, 1, 0, 704, 99
35178, V, 1, 1, 1, 1, 0, 704, 99
35179, V, 1, 1, 1, 1, 0, 704, 99
35180, V, 1, 1, 1, 1, 0, 704, 99
35181, V, 1, 1, 1, 1, 0, 704, 99
35182, V, 1, 1, 1, 1, 0, 704, 99
35183, V, 1, 1, 1, 1, 0, 704, 99
35184, V, 1, 1, 1, 1, 0, 704, 99
35185, V, 1, 1, 1, 1, 0, 704, 99
35186, V, 1, 1, 1, 1, 0, 704, 99
35187, V, 1, 1, 1, 1, 0, 704, 99
35188, V, 1, 1, 1, 1, 0, 704, 99
35189, V, 1, 1, 1, 1, 0, 704, 99
35190, V, 1, 1, 1, 1, 0, 704, 99
35191, V, 1, 1, 1, 1, 0, 704, 99
35192, V, 1, 1, 1, 1, 0, 704, 99
35193, V, 1, 1, 1, 1, 0, 704, 99
35194, V, 1, 1, 1, 1, 0, 704, 99
35195, V, 1, 1, 1, 1, 0, 704, 99
35196, V, 1, 1, 1, 1, 0, 704, 99
35197, V, 1, 1, 1, 1, 0, 704, 99
35198, V, 1, 1, 1, 1, 0, 704, 99
35200, V, 1, 1, 1, 1, 0, 704, 99
35201, V, 1, 1, 1, 1, 0, 704, 99
35202, V, 1, 1, 1, 1, 0, 704, 99
35203, V, 1, 1, 1, 1, 0, 704, 99
35204, V, 1, 1, 1, 1, 0, 704, 99
35205, V, 1, 1, 1, 1, 0, 704, 99
35206, V, 1, 1, 1, 1, 0, 704, 99
35207, V, 1, 1, 1, 1, 0, 704, 99
35208, V, 1, 1, 1, 1, 0, 704, 99
35209, V, 1, 1, 1, 1, 0, 704, 99
35210, V, 1, 1, 1, 1, 0, 704, 99
35211, V, 1, 1, 1, 1, 0, 704, 99
35212, V, 1, 1, 1, 1, 0, 704, 99
35213, V, 1, 1, 1, 1, 0, 704, 99
35214, V, 1, 1, 1, 1, 0, 704, 99
35215, V, 1, 1, 1, 1, 0, 704, 99
35216, V, 1, 1, 1, 1, 0, 704, 99
35217, V, 1, 1, 1, 1, 0, 704, 99
35218, V, 1, 1, 1, 1, 0, 704, 99
35219, V, 1, 1, 1, 1, 0, 704, 99
35220, V, 1, 1, 1, 1, 0, 704, 99
35221, V, 1, 1, 1, 1, 0, 704, 99
35222, V, 1, 1, 1, 1, 0, 704, 99
35223, V, 1, 1, 1, 1, 0, 704, 99
35224, V, 1, 1, 1, 1, 0, 704, 99
35225, V, 1, 1, 1, 1, 0, 704, 99
35226, V, 1, 1, 1, 1, 0, 704, 99
35227, V, 1, 1, 1, 1, 0, 704, 99
35228, V, 1, 1, 1, 1, 0, 704, 99
35229, V, 1, 1, 1, 1, 0, 704, 99
35230, V, 1, 1, 1, 1, 0, 704, 99
35231, V, 1, 1, 1, 1, 0, 704, 99
35232, V, 1, 1, 1, 1, 0, 704, 99
35233, V, 1, 1, 1, 1, 0, 704, 99
35234, V, 1, 1, 1, 1, 0, 704, 99
35235, V, 1, 1, 1, 1, 0, 704, 99
35236, V, 1, 1, 1, 1, 0, 704, 99
35237, V, 1, 1, 1, 1, 0, 704, 99
35238, V, 1, 1, 1, 1, 0, 704, 99
35239, V, 1, 1, 1, 1, 0, 704, 99
35240, V, 1, 1, 1, 1, 0, 704, 99
35241, V, 1, 1, 1, 1, 0, 704, 99
35243, V, 1, 1, 1, 1, 0, 704, 99
35244, V, 1, 1, 1, 1, 0, 704, 99
35245, V, 1, 1, 1, 1, 0, 704, 99
35246, V, 1, 1, 1, 1, 0, 704, 99
35247, V, 1, 1, 1, 1, 0, 704, 99
35248, V, 1, 1, 1, 1, 0, 704, 99
35249, V, 1, 1, 1, 1, 0, 704, 99
35250, V, 1, 1, 1, 1, 0, 704, 99
35251, V, 1, 1, 1, 1, 0, 704, 99
35252, V, 1, 1, 1, 1, 0, 704, 99
35253, V, 1, 1, 1, 1, 0, 704, 99
35254, V, 1, 1, 1, 1, 0, 704, 99
35255, V, 1, 1, 1, 1, 0, 704, 99
35256, V, 1, 1, 1, 1, 0, 704, 99
35257, V, 1, 1, 1, 1, 0, 704, 99
35258, V, 1, 1, 1, 1, 0, 704, 99
35259, V, 1, 1, 1, 1, 0, 704, 99
35260, V, 1, 1, 1, 1, 0, 704, 99
35261, V, 1, 1, 1, 1, 0, 704, 99
35262, V, 1, 1, 1, 1, 0, 704, 99
35263, V, 1, 1, 1, 1, 0, 704, 99
35264, V, 1, 1, 1, 1, 0, 704, 99
35265, V, 1, 1, 1, 1, 0, 704, 99
35266, V, 1, 1, 1, 1, 0, 704, 99
35267, V, 1, 1, 1, 1, 0, 704, 99
35268, V, 1, 1, 1, 1, 0, 704, 99
35269, V, 1, 1, 1, 1, 0, 704, 99
35270, V, 1, 1, 1, 1, 0, 704, 99
35271, V, 1, 1, 1, 1, 0, 704, 99
35272, V, 1, 1, 1, 1, 0, 704, 99
35273, V, 1, 1, 1, 1, 0, 704, 99
35274, V, 1, 1, 1, 1, 0, 704, 99
35275, V, 1, 1, 1, 1, 0, 704, 99
35276, V, 1, 1, 1, 1, 0, 704, 99
35277, V, 1, 1, 1, 1, 0, 704, 99
35278, V, 1, 1, 1, 1, 0, 704, 99
35279, V, 1, 1, 1, 1, 0, 704, 99
35280, V, 1, 1, 1, 1, 0, 704, 99
35281, V, 1, 1, 1, 1, 0, 704, 99
35282, V, 1, 1, 1, 1, 0, 704, 99
35283, V, 1, 1, 1, 1, 0, 704, 99
35284, V, 1, 1, 1, 1, 0, 704, 99
35286, V, 1, 1, 1, 1, 0, 704, 99
35287, V, 1, 1, 1, 1, 0, 704, 99
35288, V, 1, 1, 1, 1, 0, 704, 99
35289, V, 1, 1, 1, 1, 0, 704, 99
35290, V, 1, 1, 1, 1, 0, 704, 99
35291, V, 1, 1, 1, 1, 0, 704, 99
35292, V, 1, 1, 1, 1, 0, 704, 99
35293, V, 1, 1, 1, 1, 0, 704, 99
35294, V, 1, 1, 1, 1, 0, 704, 99
35295, V, 1, 1, 1, 1, 0, 704, 99
35296, V, 1, 1, 1, 1, 0, 704, 99
35297, V, 1, 1, 1, 1, 0, 704, 99
35298, V, 1, 1, 1, 1, 0, 704, 99
35299, V, 1, 1, 1, 1, 0, 704, 99
35300, V, 1, 1, 1, 1, 0, 704, 99
35301, V, 1, 1, 1, 1, 0, 704, 99
35302, V, 1, 1, 1, 1, 0, 704, 99
35303, V, 1, 1, 1, 1, 0, 704, 99
35304, V, 1, 1, 1, 1, 0, 704, 99
35305, V, 1, 1, 1, 1, 0, 704, 99
35306, V, 1, 1, 1, 1, 0, 704, 99
35307, V, 1, 1, 1, 1, 0, 704, 99
35308, V, 1, 1, 1, 1, 0, 704, 99
35309, V, 1, 1, 1, 1, 0, 704, 99
35310, V, 1, 1, 1, 1, 0, 704, 99
35311, V, 1, 1, 1, 1, 0, 704, 99
35312, V, 1, 1, 1, 1, 0, 704, 99
35313, V, 1, 1, 1, 1, 0, 704, 99
35314, V, 1, 1, 1, 1, 0, 704, 99
35315, V, 1, 1, 1, 1, 0, 704, 99
35316, V, 1, 1, 1, 1, 0, 704, 99
35317, V, 1, 1, 1, 1, 0, 704, 99
35318, V, 1, 1, 1, 1, 0, 704, 99
35319, V, 1, 1, 1, 1, 0, 704, 99
35320, V, 1, 1, 1, 1, 0, 704, 99
35321, V, 1, 1, 1, 1, 0, 704, 99
35322, V, 1, 1, 1, 1, 0, 704, 99
35323, V, 1, 1, 1, 1, 0, 704, 99
35324, V, 1, 1, 1, 1, 0, 704, 99
35325, V, 1, 1, 1, 1, 0, 704, 99
35326, V, 1, 1, 1, 1, 0, 704, 99
35328, V, 1, 1, 1, 1, 0, 704, 99
35329, V, 1, 1, 1, 1, 0, 704, 99
35330, V, 1, 1, 1, 1, 0, 704, 99
35331, V, 1, 1, 1, 1, 0, 704, 99
35332, V, 1, 1, 1, 1, 0, 704, 99
35333, V, 1, 1, 1, 1, 0, 704, 99
35334, V, 1, 1, 1, 1, 0, 704, 99
35335, V, 1, 1, 1, 1, 0, 704, 99
35336, V, 1, 1, 1, 1, 0, 704, 99
35337, V, 1, 1, 1, 1, 0, 704, 99
35338, V, 1, 1, 1, 1, 0, 704, 99
35339, V, 1, 1, 1, 1, 0, 704, 99
35340, V, 1, 1, 1, 1, 0, 704, 99
35341, V, 1, 1, 1, 1, 0, 704, 99
35342, V, 1, 1, 1, 1, 0, 704, 99
35343, V, 1, 1, 1, 1, 0, 704, 99
35344, V, 1, 1, 1, 1, 0, 704, 99
35345, V, 1, 1, 1, 1, 0, 704, 99
35346, V, 1, 1, 1, 1, 0, 704, 99
35347, V, 1, 1, 1, 1, 0, 704, 99
35348, V, 1, 1, 1, 1, 0, 704, 99
35349, V, 1, 1, 1, 1, 0, 704, 99
35350, V, 1, 1, 1, 1, 0, 704, 99
35351, V, 1, 1, 1, 1, 0, 704, 99
35352, V, 1, 1, 1, 1, 0, 704, 99
35353, V, 1, 1, 1, 1, 0, 704, 99
35354, V, 1, 1, 1, 1, 0, 704, 99
35355, V, 1, 1, 1, 1, 0, 704, 99
35356, V, 1, 1, 1, 1, 0, 704, 99
35357, V, 1, 1, 1, 1, 0, 704, 99
35358, V, 1, 1, 1, 1, 0, 704, 99
35359, V, 1, 1, 1, 1, 0, 704, 99
35360, V, 1, 1, 1, 1, 0, 704, 99
35361, V, 1, 1, 1, 1, 0, 704, 99
35362, V, 1, 1, 1, 1, 0, 704, 99
35363, V, 1, 1, 1, 1, 0, 704, 99
35364, V, 1, 1, 1, 1, 0, 704, 99
35365, V, 1, 1, 1, 1, 0, 704, 99
35366, V, 1, 1, 1, 1, 0, 704, 99
35367, V, 1, 1, 1, 1, 0, 704, 99
35368, V, 1, 1, 1, 1, 0, 704, 99
35369, V, 1, 1, 1, 1, 0, 704, 99
35371, V, 1, 1, 1, 1, 0, 704, 99
35372, V, 1, 1, 1, 1, 0, 704, 99
35373, V, 1, 1, 1, 1, 0, 704, 99
35374, V, 1, 1, 1, 1, 0, 704, 99
35375, V, 1, 1, 1, 1, 0, 704, 99
35376, V, 1, 1, 1, 1, 0, 704, 99
35377, V, 1, 1, 1, 1, 0, 704, 99
35378, V, 1, 1, 1, 1, 0, 704, 99
35379, V, 1, 1, 1, 1, 0, 704, 99
35380, V, 1, 1, 1, 1, 0, 704, 99
35381, V, 1, 1, 1, 1, 0, 704, 99
35382, V, 1, 1, 1, 1, 0, 704, 99
35383, V, 1, 1, 1, 1, 0, 704, 99
35384, V, 1, 1, 1, 1, 0, 704, 99
35385, V, 1, 1, 1, 1, 0, 704, 99
35386, V, 1, 1, 1, 1, 0, 704, 99
35387, V, 1, 1, 1, 1, 0, 704, 99
35388, V, 1, 1, 1, 1, 0, 704, 99
35389, V, 1, 1, 1, 1, 0, 704, 99
35390, V, 1, 1, 1, 1, 0, 704, 99
35391, V, 1, 1, 1, 1, 0, 704, 99
35392, V, 1, 1, 1, 1, 0, 704, 99
35393, V, 1, 1, 1, 1, 0, 704, 99
35394, V, 1, 1, 1, 1, 0, 704, 99
35395, V, 1, 1, 1, 1, 0, 704, 99
35396, V, 1, 1, 1, 1, 0, 704, 99
35397, V, 1, 1, 1, 1, 0, 704, 99
35398, V, 1, 1, 1, 1, 0, 704, 99
35399, V, 1, 1, 1, 1, 0, 704, 99
35400, V, 1, 1, 1, 1, 0, 704, 99
35401, V, 1, 1, 1, 1, 0, 704, 99
35402, V, 1, 1, 1, 1, 0, 704, 99
35403, V, 1, 1, 1, 1, 0, 704, 99
35404, V, 1, 1, 1, 1, 0, 704, 99
35405, V, 1, 1, 1, 1, 0, 704, 99
35406, V, 1, 1, 1, 1, 0, 704, 99
35407, V, 1, 1, 1, 1, 0, 704, 99
35408, V, 1, 1, 1, 1, 0, 704, 99
35409, V, 1, 1, 1, 1, 0, 704, 99
35410, V, 1, 1, 1, 1, 0, 704, 99
35411, V, 1, 1, 1, 1, 0, 704, 99
35412, V, 1, 1, 1, 1, 0, 704, 99
35414, V, 1, 1, 1, 1, 0, 704, 99
35415, V, 1, 1, 1, 1, 0, 704, 99
35416, V, 1, 1, 1, 1, 0, 704, 99
35417, V, 1, 1, 1, 1, 0, 704, 99
35418, V, 1, 1, 1, 1, 0, 704, 99
35419, V, 1, 1, 1, 1, 0, 704, 99
35420, V, 1, 1, 1, 1, 0, 704, 99
35421, V, 1, 1, 1, 1, 0, 704, 99
35422, V, 1, 1, 1, 1, 0, 704, 99
35423, V, 1, 1, 1, 1, 0, 704, 99
35424, V, 1, 1, 1, 1, 0, 704, 99
35425, V, 1, 1, 1, 1, 0, 704, 99
35426, V, 1, 1, 1, 1, 0, 704, 99
35427, V, 1, 1, 1, 1, 0, 704, 99
35428, V, 1, 1, 1, 1, 0, 704, 99
35429, V, 1, 1, 1, 1, 0, 704, 99
35430, V, 1, 1, 1, 1, 0, 704, 99
35431, V, 1, 1, 1, 1, 0, 704, 99
35432, V, 1, 1, 1, 1, 0, 704, 99
35433, V, 1, 1, 1, 1, 0, 704, 99
35434, V, 1, 1, 1, 1, 0, 704, 99
35435, V, 1, 1, 1, 1, 0, 704, 99
35436, V, 1, 1, 1, 1, 0, 704, 99
35437, V, 1, 1, 1, 1, 0, 704, 99
35438, V, 1, 1, 1, 1, 0, 704, 99
35439, V, 1, 1, 1, 1, 0, 704, 99
35440, V, 1, 1, 1, 1, 0, 704, 99
35441, V, 1, 1, 1, 1, 0, 704, 99
35442, V, 1, 1, 1, 1, 0, 704, 99
35443, V, 1, 1, 1, 1, 0, 704, 99
35444, V, 1, 1, 1, 1, 0, 704, 99
35445, V, 1, 1, 1, 1, 0, 704, 99
35446, V, 1, 1, 1, 1, 0, 704, 99
35447, V, 1, 1, 1, 1, 0, 704, 99
35448, V, 1, 1, 1, 1, 0, 704, 99
35449, V, 1, 1, 1, 1, 0, 704, 99
35450, V, 1, 1, 1, 1, 0, 704, 99
35451, V, 1, 1, 1, 1, 0, 704, 99
35452, V, 1, 1, 1, 1, 0, 704, 99
35453, V, 1, 1, 1, 1, 0, 704, 99
35454, V, 1, 1, 1, 1, 0, 704, 99
35456, V, 1, 1, 1, 1, 0, 704, 99
35457, V, 1, 1, 1, 1, 0, 704, 99
35458, V, 1, 1, 1, 1, 0, 704, 99
35459, V, 1, 1, 1, 1, 0, 704, 99
35460, V, 1, 1, 1, 1, 0, 704, 99
35461, V, 1, 1, 1, 1, 0, 704, 99
35462, V, 1, 1, 1, 1, 0, 704, 99
35463, V, 1, 1, 1, 1, 0, 704, 99
35464, V, 1, 1, 1, 1, 0, 704, 99
35465, V, 1, 1, 1, 1, 0, 704, 99
35466, V, 1, 1, 1, 1, 0, 704, 99
35467, V, 1, 1, 1, 1, 0, 704, 99
35468, V, 1, 1, 1, 1, 0, 704, 99
35469, V, 1, 1, 1, 1, 0, 704, 99
35470, V, 1, 1, 1, 1, 0, 704, 99
35471, V, 1, 1, 1, 1, 0, 704, 99
35472, V, 1, 1, 1, 1, 0, 704, 99
35473, V, 1, 1, 1, 1, 0, 704, 99
35474, V, 1, 1, 1, 1, 0, 704, 99
35475, V, 1, 1, 1, 1, 0, 704, 99
35476, V, 1, 1, 1, 1, 0, 704, 99
35477, V, 1, 1, 1, 1, 0, 704, 99
35478, V, 1, 1, 1, 1, 0, 704, 99
35479, V, 1, 1, 1, 1, 0, 704, 99
35480, V, 1, 1, 1, 1, 0, 704, 99
35481, V, 1, 1, 1, 1, 0, 704, 99
35482, V, 1, 1, 1, 1, 0, 704, 99
35483, V, 1, 1, 1, 1, 0, 704, 99
35484, V, 1, 1, 1, 1, 0, 704, 99
35485, V, 1, 1, 1, 1, 0, 704, 99
35486, V, 1, 1, 1, 1, 0, 704, 99
35487, V, 1, 1, 1, 1, 0, 704, 99
35488, V, 1, 1, 1, 1, 0, 704, 99
35489, V, 1, 1, 1, 1, 0, 704, 99
35490, V, 1, 1, 1, 1, 0, 704, 99
35491, V, 1, 1, 1, 1, 0, 704, 99
35492, V, 1, 1, 1, 1, 0, 704, 99
35493, V, 1, 1, 1, 1, 0, 704, 99
35494, V, 1, 1, 1, 1, 0, 704, 99
35495, V, 1, 1, 1, 1, 0, 704, 99
35496, V, 1, 1, 1, 1, 0, 704, 99
35497, V, 1, 1, 1, 1, 0, 704, 99
35499, V, 1, 1, 1, 1, 0, 704, 99
35500, V, 1, 1, 1, 1, 0, 704, 99
35501, V, 1, 1, 1, 1, 0, 704, 99
35502, V, 1, 1, 1, 1, 0, 704, 99
35503, V, 1, 1, 1, 1, 0, 704, 99
35504, V, 1, 1, 1, 1, 0, 704, 99
35505, V, 1, 1, 1, 1, 0, 704, 99
35506, V, 1, 1, 1, 1, 0, 704, 99
35507, V, 1, 1, 1, 1, 0, 704, 99
35508, V, 1, 1, 1, 1, 0, 704, 99
35509, V, 1, 1, 1, 1, 0, 704, 99
35510, V, 1, 1, 1, 1, 0, 704, 99
35511, V, 1, 1, 1, 1, 0, 704, 99
35512, V, 1, 1, 1, 1, 0, 704, 99
35513, V, 1, 1, 1, 1, 0, 704, 99
35514, V, 1, 1, 1, 1, 0, 704, 99
35515, V, 1, 1, 1, 1, 0, 704, 99
35516, V, 1, 1, 1, 1, 0, 704, 99
35517, V, 1, 1, 1, 1, 0, 704, 99
35518, V, 1, 1, 1, 1, 0, 704, 99
35519, V, 1, 1, 1, 1, 0, 704, 99
35520, V, 1, 1, 1, 1, 0, 704, 99
35521, V, 1, 1, 1, 1, 0, 704, 99
35522, V, 1, 1, 1, 1, 0, 704, 99
35523, V, 1, 1, 1, 1, 0, 704, 99
35524, V, 1, 1, 1, 1, 0, 704, 99
35525, V, 1, 1, 1, 1, 0, 704, 99
35526, V, 1, 1, 1, 1, 0, 704, 99
35527, V, 1, 1, 1, 1, 0, 704, 99
35528, V, 1, 1, 1, 1, 0, 704, 99
35529, V, 1, 1, 1, 1, 0, 704, 99
35530, V, 1, 1, 1, 1, 0, 704, 99
35531, V, 1, 1, 1, 1, 0, 704, 99
35532, V, 1, 1, 1, 1, 0, 704, 99
35533, V, 1, 1, 1, 1, 0, 704, 99
35534, V, 1, 1, 1, 1, 0, 704, 99
35535, V, 1, 1, 1, 1, 0, 704, 99
35536, V, 1, 1, 1, 1, 0, 704, 99
35537, V, 1, 1, 1, 1, 0, 704, 99
35538, V, 1, 1, 1, 1, 0, 704, 99
35539, V, 1, 1, 1, 1, 0, 704, 99
35540, V, 1, 1, 1, 1, 0, 704, 99
35542, V, 1, 1, 1, 1, 0, 704, 99
35543, V, 1, 1, 1, 1, 0, 704, 99
35544, V, 1, 1, 1, 1, 0, 704, 99
35545, V, 1, 1, 1, 1, 0, 704, 99
35546, V, 1, 1, 1, 1, 0, 704, 99
35547, V, 1, 1, 1, 1, 0, 704, 99
35548, V, 1, 1, 1, 1, 0, 704, 99
35549, V, 1, 1, 1, 1, 0, 704, 99
35550, V, 1, 1, 1, 1, 0, 704, 99
35551, V, 1, 1, 1, 1, 0, 704, 99
35552, V, 1, 1, 1, 1, 0, 704, 99
35553, V, 1, 1, 1, 1, 0, 704, 99
35554, V, 1, 1, 1, 1, 0, 704, 99
35555, V, 1, 1, 1, 1, 0, 704, 99
35556, V, 1, 1, 1, 1, 0, 704, 99
35557, V, 1, 1, 1, 1, 0, 704, 99
35558, V, 1, 1, 1, 1, 0, 704, 99
35559, V, 1, 1, 1, 1, 0, 704, 99
35560, V, 1, 1, 1, 1, 0, 704, 99
35561, V, 1, 1, 1, 1, 0, 704, 99
35562, V, 1, 1, 1, 1, 0, 704, 99
35563, V, 1, 1, 1, 1, 0, 704, 99
35564, V, 1, 1, 1, 1, 0, 704, 99
35565, V, 1, 1, 1, 1, 0, 704, 99
35566, V, 1, 1, 1, 1, 0, 704, 99
35567, V, 1, 1, 1, 1, 0, 704, 99
35568, V, 1, 1, 1, 1, 0, 704, 99
35569, V, 1, 1, 1, 1, 0, 704, 99
35570, V, 1, 1, 1, 1, 0, 704, 99
35571, V, 1, 1, 1, 1, 0, 704, 99
35572, V, 1, 1, 1, 1, 0, 704, 99
35573, V, 1, 1, 1, 1, 0, 704, 99
35574, V, 1, 1, 1, 1, 0, 704, 99
35575, V, 1, 1, 1, 1, 0, 704, 99
35576, V, 1, 1, 1, 1, 0, 704, 99
35577, V, 1, 1, 1, 1, 0, 704, 99
35578, V, 1, 1, 1, 1, 0, 704, 99
35579, V, 1, 1, 1, 1, 0, 704, 99
35580, V, 1, 1, 1, 1, 0, 704, 99
35581, V, 1, 1, 1, 1, 0, 704, 99
35582, V, 1, 1, 1, 1, 0, 704, 99
35584, V, 1, 1, 1, 1, 0, 704, 99
35585, V, 1, 1, 1, 1, 0, 704, 99
35586, V, 1, 1, 1, 1, 0, 704, 99
35587, V, 1, 1, 1, 1, 0, 704, 99
35588, V, 1, 1, 1, 1, 0, 704, 99
35589, V, 1, 1, 1, 1, 0, 704, 99
35590, V, 1, 1, 1, 1, 0, 704, 99
35591, V, 1, 1, 1, 1, 0, 704, 99
35592, V, 1, 1, 1, 1, 0, 704, 99
35593, V, 1, 1, 1, 1, 0, 704, 99
35594, V, 1, 1, 1, 1, 0, 704, 99
35595, V, 1, 1, 1, 1, 0, 704, 99
35596, V, 1, 1, 1, 1, 0, 704, 99
35597, V, 1, 1, 1, 1, 0, 704, 99
35598, V, 1, 1, 1, 1, 0, 704, 99
35599, V, 1, 1, 1, 1, 0, 704, 99
35600, V, 1, 1, 1, 1, 0, 704, 99
35601, V, 1, 1, 1, 1, 0, 704, 99
35602, V, 1, 1, 1, 1, 0, 704, 99
35603, V, 1, 1, 1, 1, 0, 704, 99
35604, V, 1, 1, 1, 1, 0, 704, 99
35605, V, 1, 1, 1, 1, 0, 704, 99
35606, V, 1, 1, 1, 1, 0, 704, 99
35607, V, 1, 1, 1, 1, 0, 704, 99
35608, V, 1, 1, 1, 1, 0, 704, 99
35609, V, 1, 1, 1, 1, 0, 704, 99
35610, V, 1, 1, 1, 1, 0, 704, 99
35611, V, 1, 1, 1, 1, 0, 704, 99
35612, V, 1, 1, 1, 1, 0, 704, 99
35613, V, 1, 1, 1, 1, 0, 704, 99
35614, V, 1, 1, 1, 1, 0, 704, 99
35615, V, 1, 1, 1, 1, 0, 704, 99
35616, V, 1, 1, 1, 1, 0, 704, 99
35617, V, 1, 1, 1, 1, 0, 704, 99
35618, V, 1, 1, 1, 1, 0, 704, 99
35619, V, 1, 1, 1, 1, 0, 704, 99
35620, V, 1, 1, 1, 1, 0, 704, 99
35621, V, 1, 1, 1, 1, 0, 704, 99
35622, V, 1, 1, 1, 1, 0, 704, 99
35623, V, 1, 1, 1, 1, 0, 704, 99
35624, V, 1, 1, 1, 1, 0, 704, 99
35625, V, 1, 1, 1, 1, 0, 704, 99
35627, V, 1, 1, 1, 1, 0, 704, 99
35628, V, 1, 1, 1, 1, 0, 704, 99
35629, V, 1, 1, 1, 1, 0, 704, 99
35630, V, 1, 1, 1, 1, 0, 704, 99
35631, V, 1, 1, 1, 1, 0, 704, 99
35632, V, 1, 1, 1, 1, 0, 704, 99
35633, V, 1, 1, 1, 1, 0, 704, 99
35634, V, 1, 1, 1, 1, 0, 704, 99
35635, V, 1, 1, 1, 1, 0, 704, 99
35636, V, 1, 1, 1, 1, 0, 704, 99
35637, V, 1, 1, 1, 1, 0, 704, 99
35638, V, 1, 1, 1, 1, 0, 704, 99
35639, V, 1, 1, 1, 1, 0, 704, 99
35640, V, 1, 1, 1, 1, 0, 704, 99
35641, V, 1, 1, 1, 1, 0, 704, 99
35642, V, 1, 1, 1, 1, 0, 704, 99
35643, V, 1, 1, 1, 1, 0, 704, 99
35644, V, 1, 1, 1, 1, 0, 704, 99
35645, V, 1, 1, 1, 1, 0, 704, 99
35646, V, 1, 1, 1, 1, 0, 704, 99
35647, V, 1, 1, 1, 1, 0, 704, 99
35648, V, 1, 1, 1, 1, 0, 704, 99
35649, V, 1, 1, 1, 1, 0, 704, 99
35650, V, 1, 1, 1, 1, 0, 704, 99
35651, V, 1, 1, 1, 1, 0, 704, 99
35652, V, 1, 1, 1, 1, 0, 704, 99
35653, V, 1, 1, 1, 1, 0, 704, 99
35654, V, 1, 1, 1, 1, 0, 704, 99
35655, V, 1, 1, 1, 1, 0, 704, 99
35656, V, 1, 1, 1, 1, 0, 704, 99
35657, V, 1, 1, 1, 1, 0, 704, 99
35658, V, 1, 1, 1, 1, 0, 704, 99
35659, V, 1, 1, 1, 1, 0, 704, 99
35660, V, 1, 1, 1, 1, 0, 704, 99
35661, V, 1, 1, 1, 1, 0, 704, 99
35662, V, 1, 1, 1, 1, 0, 704, 99
35663, V, 1, 1, 1, 1, 0, 704, 99
35664, V, 1, 1, 1, 1, 0, 704, 99
35665, V, 1, 1, 1, 1, 0, 704, 99
35666, V, 1, 1, 1, 1, 0, 704, 99
35667, V, 1, 1, 1, 1, 0, 704, 99
35668, V, 1, 1, 1, 1, 0, 704, 99
35670, V, 1, 1, 1, 1, 0, 704, 99
35671, V, 1, 1, 1, 1, 0, 704, 99
35672, V, 1, 1, 1, 1, 0, 704, 99
35673, V, 1, 1, 1, 1, 0, 704, 99
35674, V, 1, 1, 1, 1, 0, 704, 99
35675, V, 1, 1, 1, 1, 0, 704, 99
35676, V, 1, 1, 1, 1, 0, 704, 99
35677, V, 1, 1, 1, 1, 0, 704, 99
35678, V, 1, 1, 1, 1, 0, 704, 99
35679, V, 1, 1, 1, 1, 0, 704, 99
35680, V, 1, 1, 1, 1, 0, 704, 99
35681, V, 1, 1, 1, 1, 0, 704, 99
35682, V, 1, 1, 1, 1, 0, 704, 99
35683, V, 1, 1, 1, 1, 0, 704, 99
35684, V, 1, 1, 1, 1, 0, 704, 99
35685, V, 1, 1, 1, 1, 0, 704, 99
35686, V, 1, 1, 1, 1, 0, 704, 99
35687, V, 1, 1, 1, 1, 0, 704, 99
35688, V, 1, 1, 1, 1, 0, 704, 99
35689, V, 1, 1, 1, 1, 0, 704, 99
35690, V, 1, 1, 1, 1, 0, 704, 99
35691, V, 1, 1, 1, 1, 0, 704, 99
35692, V, 1, 1, 1, 1, 0, 704, 99
35693, V, 1, 1, 1, 1, 0, 704, 99
35694, V, 1, 1, 1, 1, 0, 704, 99
35695, V, 1, 1, 1, 1, 0, 704, 99
35696, V, 1, 1, 1, 1, 0, 704, 99
35697, V, 1, 1, 1, 1, 0, 704, 99
35698, V, 1, 1, 1, 1, 0, 704, 99
35699, V, 1, 1, 1, 1, 0, 704, 99
35700, V, 1, 1, 1, 1, 0, 704, 99
35701, V, 1, 1, 1, 1, 0, 704, 99
35702, V, 1, 1, 1, 1, 0, 704, 99
35703, V, 1, 1, 1, 1, 0, 704, 99
35704, V, 1, 1, 1, 1, 0, 704, 99
35705, V, 1, 1, 1, 1, 0, 704, 99
35706, V, 1, 1, 1, 1, 0, 704, 99
35707, V, 1, 1, 1, 1, 0, 704, 99
35708, V, 1, 1, 1, 1, 0, 704, 99
35709, V, 1, 1, 1, 1, 0, 704, 99
35710, V, 1, 1, 1, 1, 0, 704, 99
35712, V, 1, 1, 1, 1, 0, 704, 99
35713, V, 1, 1, 1, 1, 0, 704, 99
35714, V, 1, 1, 1, 1, 0, 704, 99
35715, V, 1, 1, 1, 1, 0, 704, 99
35716, V, 1, 1, 1, 1, 0, 704, 99
35717, V, 1, 1, 1, 1, 0, 704, 99
35718, V, 1, 1, 1, 1, 0, 704, 99
35719, V, 1, 1, 1, 1, 0, 704, 99
35720, V, 1, 1, 1, 1, 0, 704, 99
35721, V, 1, 1, 1, 1, 0, 704, 99
35722, V, 1, 1, 1, 1, 0, 704, 99
35723, V, 1, 1, 1, 1, 0, 704, 99
35724, V, 1, 1, 1, 1, 0, 704, 99
35725, V, 1, 1, 1, 1, 0, 704, 99
35726, V, 1, 1, 1, 1, 0, 704, 99
35727, V, 1, 1, 1, 1, 0, 704, 99
35728, V, 1, 1, 1, 1, 0, 704, 99
35729, V, 1, 1, 1, 1, 0, 704, 99
35730, V, 1, 1, 1, 1, 0, 704, 99
35731, V, 1, 1, 1, 1, 0, 704, 99
35732, V, 1, 1, 1, 1, 0, 704, 99
35733, V, 1, 1, 1, 1, 0, 704, 99
35734, V, 1, 1, 1, 1, 0, 704, 99
35735, V, 1, 1, 1, 1, 0, 704, 99
35736, V, 1, 1, 1, 1, 0, 704, 99
35737, V, 1, 1, 1, 1, 0, 704, 99
35738, V, 1, 1, 1, 1, 0, 704, 99
35739, V, 1, 1, 1, 1, 0, 704, 99
35740, V, 1, 1, 1, 1, 0, 704, 99
35741, V, 1, 1, 1, 1, 0, 704, 99
35742, V, 1, 1, 1, 1, 0, 704, 99
35743, V, 1, 1, 1, 1, 0, 704, 99
35744, V, 1, 1, 1, 1, 0, 704, 99
35745, V, 1, 1, 1, 1, 0, 704, 99
35746, V, 1, 1, 1, 1, 0, 704, 99
35747, V, 1, 1, 1, 1, 0, 704, 99
35748, V, 1, 1, 1, 1, 0, 704, 99
35749, V, 1, 1, 1, 1, 0, 704, 99
35750, V, 1, 1, 1, 1, 0, 704, 99
35751, V, 1, 1, 1, 1, 0, 704, 99
35752, V, 1, 1, 1, 1, 0, 704, 99
35753, V, 1, 1, 1, 1, 0, 704, 99
35755, V, 1, 1, 1, 1, 0, 704, 99
35756, V, 1, 1, 1, 1, 0, 704, 99
35757, V, 1, 1, 1, 1, 0, 704, 99
35758, V, 1, 1, 1, 1, 0, 704, 99
35759, V, 1, 1, 1, 1, 0, 704, 99
35760, V, 1, 1, 1, 1, 0, 704, 99
35761, V, 1, 1, 1, 1, 0, 704, 99
35762, V, 1, 1, 1, 1, 0, 704, 99
35763, V, 1, 1, 1, 1, 0, 704, 99
35764, V, 1, 1, 1, 1, 0, 704, 99
35765, V, 1, 1, 1, 1, 0, 704, 99
35766, V, 1, 1, 1, 1, 0, 704, 99
35767, V, 1, 1, 1, 1, 0, 704, 99
35768, V, 1, 1, 1, 1, 0, 704, 99
35769, V, 1, 1, 1, 1, 0, 704, 99
35770, V, 1, 1, 1, 1, 0, 704, 99
35771, V, 1, 1, 1, 1, 0, 704, 99
35772, V, 1, 1, 1, 1, 0, 704, 99
35773, V, 1, 1, 1, 1, 0, 704, 99
35774, V, 1, 1, 1, 1, 0, 704, 99
35775, V, 1, 1, 1, 1, 0, 704, 99
35776, V, 1, 1, 1, 1, 0, 704, 99
35777, V, 1, 1, 1, 1, 0, 704, 99
35778, V, 1, 1, 1, 1, 0, 704, 99
35779, V, 1, 1, 1, 1, 0, 704, 99
35780, V, 1, 1, 1, 1, 0, 704, 99
35781, V, 1, 1, 1, 1, 0, 704, 99
35782, V, 1, 1, 1, 1, 0, 704, 99
35783, V, 1, 1, 1, 1, 0, 704, 99
35784, V, 1, 1, 1, 1, 0, 704, 99
35785, V, 1, 1, 1, 1, 0, 704, 99
35786, V, 1, 1, 1, 1, 0, 704, 99
35787, V, 1, 1, 1, 1, 0, 704, 99
35788, V, 1, 1, 1, 1, 0, 704, 99
35789, V, 1, 1, 1, 1, 0, 704, 99
35790, V, 1, 1, 1, 1, 0, 704, 99
35791, V, 1, 1, 1, 1, 0, 704, 99
35792, V, 1, 1, 1, 1, 0, 704, 99
35793, V, 1, 1, 1, 1, 0, 704, 99
35794, V, 1, 1, 1, 1, 0, 704, 99
35795, V, 1, 1, 1, 1, 0, 704, 99
35796, V, 1, 1, 1, 1, 0, 704, 99
35798, V, 1, 1, 1, 1, 0, 704, 99
35799, V, 1, 1, 1, 1, 0, 704, 99
35800, V, 1, 1, 1, 1, 0, 704, 99
35801, V, 1, 1, 1, 1, 0, 704, 99
35802, V, 1, 1, 1, 1, 0, 704, 99
35803, V, 1, 1, 1, 1, 0, 704, 99
35804, V, 1, 1, 1, 1, 0, 704, 99
35805, V, 1, 1, 1, 1, 0, 704, 99
35806, V, 1, 1, 1, 1, 0, 704, 99
35807, V, 1, 1, 1, 1, 0, 704, 99
35808, V, 1, 1, 1, 1, 0, 704, 99
35809, V, 1, 1, 1, 1, 0, 704, 99
35810, V, 1, 1, 1, 1, 0, 704, 99
35811, V, 1, 1, 1, 1, 0, 704, 99
35812, V, 1, 1, 1, 1, 0, 704, 99
35813, V, 1, 1, 1, 1, 0, 704, 99
35814, V, 1, 1, 1, 1, 0, 704, 99
35815, V, 1, 1, 1, 1, 0, 704, 99
35816, V, 1, 1, 1, 1, 0, 704, 99
35817, V, 1, 1, 1, 1, 0, 704, 99
35818, V, 1, 1, 1, 1, 0, 704, 99
35819, V, 1, 1, 1, 1, 0, 704, 99
35820, V, 1, 1, 1, 1, 0, 704, 99
35821, V, 1, 1, 1, 1, 0, 704, 99
35822, V, 1, 1, 1, 1, 0, 704, 99
35823, V, 1, 1, 1, 1, 0, 704, 99
35824, V, 1, 1, 1, 1, 0, 704, 99
35825, V, 1, 1, 1, 1, 0, 704, 99
35826, V, 1, 1, 1, 1, 0, 704, 99
35827, V, 1, 1, 1, 1, 0, 704, 99
35828, V, 1, 1, 1, 1, 0, 704, 99
35829, V, 1, 1, 1, 1, 0, 704, 99
35830, V, 1, 1, 1, 1, 0, 704, 99
35831, V, 1, 1, 1, 1, 0, 704, 99
35832, V, 1, 1, 1, 1, 0, 704, 99
35833, V, 1, 1, 1, 1, 0, 704, 99
35834, V, 1, 1, 1, 1, 0, 704, 99
35835, V, 1, 1, 1, 1, 0, 704, 99
35836, V, 1, 1, 1, 1, 0, 704, 99
35837, V, 1, 1, 1, 1, 0, 704, 99
35838, V, 1, 1, 1, 1, 0, 704, 99
35840, V, 1, 1, 1, 1, 0, 704, 99
35841, V, 1, 1, 1, 1, 0, 704, 99
35842, V, 1, 1, 1, 1, 0, 704, 99
35843, V, 1, 1, 1, 1, 0, 704, 99
35844, V, 1, 1, 1, 1, 0, 704, 99
35845, V, 1, 1, 1, 1, 0, 704, 99
35846, V, 1, 1, 1, 1, 0, 704, 99
35847, V, 1, 1, 1, 1, 0, 704, 99
35848, V, 1, 1, 1, 1, 0, 704, 99
35849, V, 1, 1, 1, 1, 0, 704, 99
35850, V, 1, 1, 1, 1, 0, 704, 99
35851, V, 1, 1, 1, 1, 0, 704, 99
35852, V, 1, 1, 1, 1, 0, 704, 99
35853, V, 1, 1, 1, 1, 0, 704, 99
35854, V, 1, 1, 1, 1, 0, 704, 99
35855, V, 1, 1, 1, 1, 0, 704, 99
35856, V, 1, 1, 1, 1, 0, 704, 99
35857, V, 1, 1, 1, 1, 0, 704, 99
35858, V, 1, 1, 1, 1, 0, 704, 99
35859, V, 1, 1, 1, 1, 0, 704, 99
35860, V, 1, 1, 1, 1, 0, 704, 99
35861, V, 1, 1, 1, 1, 0, 704, 99
35862, V, 1, 1, 1, 1, 0, 704, 99
35863, V, 1, 1, 1, 1, 0, 704, 99
35864, V, 1, 1, 1, 1, 0, 704, 99
35865, V, 1, 1, 1, 1, 0, 704, 99
35866, V, 1, 1, 1, 1, 0, 704, 99
35867, V, 1, 1, 1, 1, 0, 704, 99
35868, V, 1, 1, 1, 1, 0, 704, 99
35869, V, 1, 1, 1, 1, 0, 704, 99
35870, V, 1, 1, 1, 1, 0, 704, 99
35871, V, 1, 1, 1, 1, 0, 704, 99
35872, V, 1, 1, 1, 1, 0, 704, 99
35873, V, 1, 1, 1, 1, 0, 704, 99
35874, V, 1, 1, 1, 1, 0, 704, 99
35875, V, 1, 1, 1, 1, 0, 704, 99
35876, V, 1, 1, 1, 1, 0, 704, 99
35877, V, 1, 1, 1, 1, 0, 704, 99
35878, V, 1, 1, 1, 1, 0, 704, 99
35879, V, 1, 1, 1, 1, 0, 704, 99
35880, V, 1, 1, 1, 1, 0, 704, 99
35881, V, 1, 1, 1, 1, 0, 704, 99
35883, V, 1, 1, 1, 1, 0, 704, 99
35884, V, 1, 1, 1, 1, 0, 704, 99
35885, V, 1, 1, 1, 1, 0, 704, 99
35886, V, 1, 1, 1, 1, 0, 704, 99
35887, V, 1, 1, 1, 1, 0, 704, 99
35888, V, 1, 1, 1, 1, 0, 704, 99
35889, V, 1, 1, 1, 1, 0, 704, 99
35890, V, 1, 1, 1, 1, 0, 704, 99
35891, V, 1, 1, 1, 1, 0, 704, 99
35892, V, 1, 1, 1, 1, 0, 704, 99
35893, V, 1, 1, 1, 1, 0, 704, 99
35894, V, 1, 1, 1, 1, 0, 704, 99
35895, V, 1, 1, 1, 1, 0, 704, 99
35896, V, 1, 1, 1, 1, 0, 704, 99
35897, V, 1, 1, 1, 1, 0, 704, 99
35898, V, 1, 1, 1, 1, 0, 704, 99
35899, V, 1, 1, 1, 1, 0, 704, 99
35900, V, 1, 1, 1, 1, 0, 704, 99
35901, V, 1, 1, 1, 1, 0, 704, 99
35902, V, 1, 1, 1, 1, 0, 704, 99
35903, V, 1, 1, 1, 1, 0, 704, 99
35904, V, 1, 1, 1, 1, 0, 704, 99
35905, V, 1, 1, 1, 1, 0, 704, 99
35906, V, 1, 1, 1, 1, 0, 704, 99
35907, V, 1, 1, 1, 1, 0, 704, 99
35908, V, 1, 1, 1, 1, 0, 704, 99
35909, V, 1, 1, 1, 1, 0, 704, 99
35910, V, 1, 1, 1, 1, 0, 704, 99
35911, V, 1, 1, 1, 1, 0, 704, 99
35912, V, 1, 1, 1, 1, 0, 704, 99
35913, V, 1, 1, 1, 1, 0, 704, 99
35914, V, 1, 1, 1, 1, 0, 704, 99
35915, V, 1, 1, 1, 1, 0, 704, 99
35916, V, 1, 1, 1, 1, 0, 704, 99
35917, V, 1, 1, 1, 1, 0, 704, 99
35918, V, 1, 1, 1, 1, 0, 704, 99
35919, V, 1, 1, 1, 1, 0, 704, 99
35920, V, 1, 1, 1, 1, 0, 704, 99
35921, V, 1, 1, 1, 1, 0, 704, 99
35922, V, 1, 1, 1, 1, 0, 704, 99
35923, V, 1, 1, 1, 1, 0, 704, 99
35924, V, 1, 1, 1, 1, 0, 704, 99
35926, V, 1, 1, 1, 1, 0, 704, 99
35927, V, 1, 1, 1, 1, 0, 704, 99
35928, V, 1, 1, 1, 1, 0, 704, 99
35929, V, 1, 1, 1, 1, 0, 704, 99
35930, V, 1, 1, 1, 1, 0, 704, 99
35931, V, 1, 1, 1, 1, 0, 704, 99
35932, V, 1, 1, 1, 1, 0, 704, 99
35933, V, 1, 1, 1, 1, 0, 704, 99
35934, V, 1, 1, 1, 1, 0, 704, 99
35935, V, 1, 1, 1, 1, 0, 704, 99
35936, V, 1, 1, 1, 1, 0, 704, 99
35937, V, 1, 1, 1, 1, 0, 704, 99
35938, V, 1, 1, 1, 1, 0, 704, 99
35939, V, 1, 1, 1, 1, 0, 704, 99
35940, V, 1, 1, 1, 1, 0, 704, 99
35941, V, 1, 1, 1, 1, 0, 704, 99
35942, V, 1, 1, 1, 1, 0, 704, 99
35943, V, 1, 1, 1, 1, 0, 704, 99
35944, V, 1, 1, 1, 1, 0, 704, 99
35945, V, 1, 1, 1, 1, 0, 704, 99
35946, V, 1, 1, 1, 1, 0, 704, 99
35947, V, 1, 1, 1, 1, 0, 704, 99
35948, V, 1, 1, 1, 1, 0, 704, 99
35949, V, 1, 1, 1, 1, 0, 704, 99
35950, V, 1, 1, 1, 1, 0, 704, 99
35951, V, 1, 1, 1, 1, 0, 704, 99
35952, V, 1, 1, 1, 1, 0, 704, 99
35953, V, 1, 1, 1, 1, 0, 704, 99
35954, V, 1, 1, 1, 1, 0, 704, 99
35955, V, 1, 1, 1, 1, 0, 704, 99
35956, V, 1, 1, 1, 1, 0, 704, 99
35957, V, 1, 1, 1, 1, 0, 704, 99
35958, V, 1, 1, 1, 1, 0, 704, 99
35959, V, 1, 1, 1, 1, 0, 704, 99
35960, V, 1, 1, 1, 1, 0, 704, 99
35961, V, 1, 1, 1, 1, 0, 704, 99
35962, V, 1, 1, 1, 1, 0, 704, 99
35963, V, 1, 1, 1, 1, 0, 704, 99
35964, V, 1, 1, 1, 1, 0, 704, 99
35965, V, 1, 1, 1, 1, 0, 704, 99
35966, V, 1, 1, 1, 1, 0, 704, 99
35968, V, 1, 1, 1, 1, 0, 704, 99
35969, V, 1, 1, 1, 1, 0, 704, 99
35970, V, 1, 1, 1, 1, 0, 704, 99
35971, V, 1, 1, 1, 1, 0, 704, 99
35972, V, 1, 1, 1, 1, 0, 704, 99
35973, V, 1, 1, 1, 1, 0, 704, 99
35974, V, 1, 1, 1, 1, 0, 704, 99
35975, V, 1, 1, 1, 1, 0, 704, 99
35976, V, 1, 1, 1, 1, 0, 704, 99
35977, V, 1, 1, 1, 1, 0, 704, 99
35978, V, 1, 1, 1, 1, 0, 704, 99
35979, V, 1, 1, 1, 1, 0, 704, 99
35980, V, 1, 1, 1, 1, 0, 704, 99
35981, V, 1, 1, 1, 1, 0, 704, 99
35982, V, 1, 1, 1, 1, 0, 704, 99
35983, V, 1, 1, 1, 1, 0, 704, 99
35984, V, 1, 1, 1, 1, 0, 704, 99
35985, V, 1, 1, 1, 1, 0, 704, 99
35986, V, 1, 1, 1, 1, 0, 704, 99
35987, V, 1, 1, 1, 1, 0, 704, 99
35988, V, 1, 1, 1, 1, 0, 704, 99
35989, V, 1, 1, 1, 1, 0, 704, 99
35990, V, 1, 1, 1, 1, 0, 704, 99
35991, V, 1, 1, 1, 1, 0, 704, 99
35992, V, 1, 1, 1, 1, 0, 704, 99
35993, V, 1, 1, 1, 1, 0, 704, 99
35994, V, 1, 1, 1, 1, 0, 704, 99
35995, V, 1, 1, 1, 1, 0, 704, 99
35996, V, 1, 1, 1, 1, 0, 704, 99
35997, V, 1, 1, 1, 1, 0, 704, 99
35998, V, 1, 1, 1, 1, 0, 704, 99
35999, V, 1, 1, 1, 1, 0, 704, 99
36000, V, 1, 1, 1, 1, 0, 704, 99
36001, V, 1, 1, 1, 1, 0, 704, 99
36002, V, 1, 1, 1, 1, 0, 704, 99
36003, V, 1, 1, 1, 1, 0, 704, 99
36004, V, 1, 1, 1, 1, 0, 704, 99
36005, V, 1, 1, 1, 1, 0, 704, 99
36006, V, 1, 1, 1, 1, 0, 704, 99
36007, V, 1, 1, 1, 1, 0, 704, 99
36008, V, 1, 1, 1, 1, 0, 704, 99
36009, V, 1, 1, 1, 1, 0, 704, 99
36011, V, 1, 1, 1, 1, 0, 704, 99
36012, V, 1, 1, 1, 1, 0, 704, 99
36013, V, 1, 1, 1, 1, 0, 704, 99
36014, V, 1, 1, 1, 1, 0, 704, 99
36015, V, 1, 1, 1, 1, 0, 704, 99
36016, V, 1, 1, 1, 1, 0, 704, 99
36017, V, 1, 1, 1, 1, 0, 704, 99
36018, V, 1, 1, 1, 1, 0, 704, 99
36019, V, 1, 1, 1, 1, 0, 704, 99
36020, V, 1, 1, 1, 1, 0, 704, 99
36021, V, 1, 1, 1, 1, 0, 704, 99
36022, V, 1, 1, 1, 1, 0, 704, 99
36023, V, 1, 1, 1, 1, 0, 704, 99
36024, V, 1, 1, 1, 1, 0, 704, 99
36025, V, 1, 1, 1, 1, 0, 704, 99
36026, V, 1, 1, 1, 1, 0, 704, 99
36027, V, 1, 1, 1, 1, 0, 704, 99
36028, V, 1, 1, 1, 1, 0, 704, 99
36029, V, 1, 1, 1, 1, 0, 704, 99
36030, V, 1, 1, 1, 1, 0, 704, 99
36031, V, 1, 1, 1, 1, 0, 704, 99
36032, V, 1, 1, 1, 1, 0, 704, 99
36033, V, 1, 1, 1, 1, 0, 704, 99
36034, V, 1, 1, 1, 1, 0, 704, 99
36035, V, 1, 1, 1, 1, 0, 704, 99
36036, V, 1, 1, 1, 1, 0, 704, 99
36037, V, 1, 1, 1, 1, 0, 704, 99
36038, V, 1, 1, 1, 1, 0, 704, 99
36039, V, 1, 1, 1, 1, 0, 704, 99
36040, V, 1, 1, 1, 1, 0, 704, 99
36041, V, 1, 1, 1, 1, 0, 704, 99
36042, V, 1, 1, 1, 1, 0, 704, 99
36043, V, 1, 1, 1, 1, 0, 704, 99
36044, V, 1, 1, 1, 1, 0, 704, 99
36045, V, 1, 1, 1, 1, 0, 704, 99
36046, V, 1, 1, 1, 1, 0, 704, 99
36047, V, 1, 1, 1, 1, 0, 704, 99
36048, V, 1, 1, 1, 1, 0, 704, 99
36049, V, 1, 1, 1, 1, 0, 704, 99
36050, V, 1, 1, 1, 1, 0, 704, 99
36051, V, 1, 1, 1, 1, 0, 704, 99
36052, V, 1, 1, 1, 1, 0, 704, 99
36054, V, 1, 1, 1, 1, 0, 704, 99
36055, V, 1, 1, 1, 1, 0, 704, 99
36056, V, 1, 1, 1, 1, 0, 704, 100
36057, V, 1, 1, 1, 1, 0, 704, 100
36058, V, 1, 1, 1, 1, 0, 704, 100
36059, V, 1, 1, 1, 1, 0, 704, 100
36060, V, 1, 1, 1, 1, 0, 704, 100
36061, V, 1, 1, 1, 1, 0, 704, 100
36062, V, 1, 1, 1, 1, 0, 704, 100
36063, V, 1, 1, 1, 1, 0, 704, 100
36064, V, 1, 1, 1, 1, 0, 704, 100
36065, V, 1, 1, 1, 1, 0, 704, 100
36066, V, 1, 1, 1, 1, 0, 704, 100
36067, V, 1, 1, 1, 1, 0, 704, 100
36068, V, 1, 1, 1, 1, 0, 704, 100
36069, V, 1, 1, 1, 1, 0, 704, 100
36070, V, 1, 1, 1, 1, 0, 704, 100
36071, V, 1, 1, 1, 1, 0, 704, 100
36072, V, 1, 1, 1, 1, 0, 704, 100
36073, V, 1, 1, 1, 1, 0, 704, 100
36074, V, 1, 1, 1, 1, 0, 704, 100
36075, V, 1, 1, 1, 1, 0, 704, 100
36076, V, 1, 1, 1, 1, 0, 704, 100
36077, V, 1, 1, 1, 1, 0, 704, 100
36078, V, 1, 1, 1, 1, 0, 704, 100
36079, V, 1, 1, 1, 1, 0, 704, 100
36080, V, 1, 1, 1, 1, 0, 704, 100
36081, V, 1, 1, 1, 1, 0, 704, 100
36082, V, 1, 1, 1, 1, 0, 704, 100
36083, V, 1, 1, 1, 1, 0, 704, 100
36084, V, 1, 1, 1, 1, 0, 704, 100
36085, V, 1, 1, 1, 1, 0, 704, 100
36086, V, 1, 1, 1, 1, 0, 704, 100
36087, V, 1, 1, 1, 1, 0, 704, 100
36088, V, 1, 1, 1, 1, 0, 704, 100
36089, V, 1, 1, 1, 1, 0, 704, 100
36090, V, 1, 1, 1, 1, 0, 704, 100
36091, V, 1, 1, 1, 1, 0, 704, 100
36092, V, 1, 1, 1, 1, 0, 704, 100
36093, V, 1, 1, 1, 1, 0, 704, 100
36094, V, 1, 1, 1, 1, 0, 704, 100
36096, V, 1, 1, 1, 1, 0, 704, 100
36097, V, 1, 1, 1, 1, 0, 704, 100
36098, V, 1, 1, 1, 1, 0, 704, 100
36099, V, 1, 1, 1, 1, 0, 704, 100
36100, V, 1, 1, 1, 1, 0, 704, 100
36101, V, 1, 1, 1, 1, 0, 704, 100
36102, V, 1, 1, 1, 1, 0, 704, 100
36103, V, 1, 1, 1, 1, 0, 704, 100
36104, V, 1, 1, 1, 1, 0, 704, 100
36105, V, 1, 1, 1, 1, 0, 704, 100
36106, V, 1, 1, 1, 1, 0, 704, 100
36107, V, 1, 1, 1, 1, 0, 704, 100
36108, V, 1, 1, 1, 1, 0, 704, 100
36109, V, 1, 1, 1, 1, 0, 704, 100
36110, V, 1, 1, 1, 1, 0, 704, 100
36111, V, 1, 1, 1, 1, 0, 704, 100
36112, V, 1, 1, 1, 1, 0, 704, 100
36113, V, 1, 1, 1, 1, 0, 704, 100
36114, V, 1, 1, 1, 1, 0, 704, 100
36115, V, 1, 1, 1, 1, 0, 704, 100
36116, V, 1, 1, 1, 1, 0, 704, 100
36117, V, 1, 1, 1, 1, 0, 704, 100
36118, V, 1, 1, 1, 1, 0, 704, 100
36119, V, 1, 1, 1, 1, 0, 704, 100
36120, V, 1, 1, 1, 1, 0, 704, 100
36121, V, 1, 1, 1, 1, 0, 704, 100
36122, V, 1, 1, 1, 1, 0, 704, 100
36123, V, 1, 1, 1, 1, 0, 704, 100
36124, V, 1, 1, 1, 1, 0, 704, 100
36125, V, 1, 1, 1, 1, 0, 704, 100
36126, V, 1, 1, 1, 1, 0, 704, 100
36127, V, 1, 1, 1, 1, 0, 704, 100
36128, V, 1, 1, 1, 1, 0, 704, 100
36129, V, 1, 1, 1, 1, 0, 704, 100
36130, V, 1, 1, 1, 1, 0, 704, 100
36131, V, 1, 1, 1, 1, 0, 704, 100
36132, V, 1, 1, 1, 1, 0, 704, 100
36133, V, 1, 1, 1, 1, 0, 704, 100
36134, V, 1, 1, 1, 1, 0, 704, 100
36135, V, 1, 1, 1, 1, 0, 704, 100
36136, V, 1, 1, 1, 1, 0, 704, 100
36137, V, 1, 1, 1, 1, 0, 704, 100
36139, V, 1, 1, 1, 1, 0, 704, 100
36140, V, 1, 1, 1, 1, 0, 704, 100
36141, V, 1, 1, 1, 1, 0, 704, 100
36142, V, 1, 1, 1, 1, 0, 704, 100
36143, V, 1, 1, 1, 1, 0, 704, 100
36144, V, 1, 1, 1, 1, 0, 704, 100
36145, V, 1, 1, 1, 1, 0, 704, 100
36146, V, 1, 1, 1, 1, 0, 704, 100
36147, V, 1, 1, 1, 1, 0, 704, 100
36148, V, 1, 1, 1, 1, 0, 704, 100
36149, V, 1, 1, 1, 1, 0, 704, 100
36150, V, 1, 1, 1, 1, 0, 704, 100
36151, V, 1, 1, 1, 1, 0, 704, 100
36152, V, 1, 1, 1, 1, 0, 704, 100
36153, V, 1, 1, 1, 1, 0, 704, 100
36154, V, 1, 1, 1, 1, 0, 704, 100
36155, V, 1, 1, 1, 1, 0, 704, 100
36156, V, 1, 1, 1, 1, 0, 704, 100
36157, V, 1, 1, 1, 1, 0, 704, 100
36158, V, 1, 1, 1, 1, 0, 704, 100
36159, V, 1, 1, 1, 1, 0, 704, 100
36160, V, 1, 1, 1, 1, 0, 704, 100
36161, V, 1, 1, 1, 1, 0, 704, 100
36162, V, 1, 1, 1, 1, 0, 704, 100
36163, V, 1, 1, 1, 1, 0, 704, 100
36164, V, 1, 1, 1, 1, 0, 704, 100
36165, V, 1, 1, 1, 1, 0, 704, 100
36166, V, 1, 1, 1, 1, 0, 704, 100
36167, V, 1, 1, 1, 1, 0, 704, 100
36168, V, 1, 1, 1, 1, 0, 704, 100
36169, V, 1, 1, 1, 1, 0, 704, 100
36170, V, 1, 1, 1, 1, 0, 704, 100
36171, V, 1, 1, 1, 1, 0, 704, 100
36172, V, 1, 1, 1, 1, 0, 704, 100
36173, V, 1, 1, 1, 1, 0, 704, 100
36174, V, 1, 1, 1, 1, 0, 704, 100
36175, V, 1, 1, 1, 1, 0, 704, 100
36176, V, 1, 1, 1, 1, 0, 704, 100
36177, V, 1, 1, 1, 1, 0, 704, 100
36178, V, 1, 1, 1, 1, 0, 704, 100
36179, V, 1, 1, 1, 1, 0, 704, 100
36180, V, 1, 1, 1, 1, 0, 704, 100
36182, V, 1, 1, 1, 1, 0, 704, 100
36183, V, 1, 1, 1, 1, 0, 704, 100
36184, V, 1, 1, 1, 1, 0, 704, 100
36185, V, 1, 1, 1, 1, 0, 704, 100
36186, V, 1, 1, 1, 1, 0, 704, 100
36187, V, 1, 1, 1, 1, 0, 704, 100
36188, V, 1, 1, 1, 1, 0, 704, 100
36189, V, 1, 1, 1, 1, 0, 704, 100
36190, V, 1, 1, 1, 1, 0, 704, 100
36191, V, 1, 1, 1, 1, 0, 704, 100
36192, V, 1, 1, 1, 1, 0, 704, 100
36193, V, 1, 1, 1, 1, 0, 704, 100
36194, V, 1, 1, 1, 1, 0, 704, 100
36195, V, 1, 1, 1, 1, 0, 704, 100
36196, V, 1, 1, 1, 1, 0, 704, 100
36197, V, 1, 1, 1, 1, 0, 704, 100
36198, V, 1, 1, 1, 1, 0, 704, 100
36199, V, 1, 1, 1, 1, 0, 704, 100
36200, V, 1, 1, 1, 1, 0, 704, 100
36201, V, 1, 1, 1, 1, 0, 704, 100
36202, V, 1, 1, 1, 1, 0, 704, 100
36203, V, 1, 1, 1, 1, 0, 704, 100
36204, V, 1, 1, 1, 1, 0, 704, 100
36205, V, 1, 1, 1, 1, 0, 704, 100
36206, V, 1, 1, 1, 1, 0, 704, 100
36207, V, 1, 1, 1, 1, 0, 704, 100
36208, V, 1, 1, 1, 1, 0, 704, 100
36209, V, 1, 1, 1, 1, 0, 704, 100
36210, V, 1, 1, 1, 1, 0, 704, 100
36211, V, 1, 1, 1, 1, 0, 704, 100
36212, V, 1, 1, 1, 1, 0, 704, 100
36213, V, 1, 1, 1, 1, 0, 704, 100
36214, V, 1, 1, 1, 1, 0, 704, 100
36215, V, 1, 1, 1, 1, 0, 704, 100
36216, V, 1, 1, 1, 1, 0, 704, 100
36217, V, 1, 1, 1, 1, 0, 704, 100
36218, V, 1, 1, 1, 1, 0, 704, 100
36219, V, 1, 1, 1, 1, 0, 704, 100
36220, V, 1, 1, 1, 1, 0, 704, 100
36221, V, 1, 1, 1, 1, 0, 704, 100
36222, V, 1, 1, 1, 1, 0, 704, 100
36224, V, 1, 1, 1, 1, 0, 704, 100
36225, V, 1, 1, 1, 1, 0, 704, 100
36226, V, 1, 1, 1, 1, 0, 704, 100
36227, V, 1, 1, 1, 1, 0, 704, 100
36228, V, 1, 1, 1, 1, 0, 704, 100
36229, V, 1, 1, 1, 1, 0, 704, 100
36230, V, 1, 1, 1, 1, 0, 704, 100
36231, V, 1, 1, 1, 1, 0, 704, 100
36232, V, 1, 1, 1, 1, 0, 704, 100
36233, V, 1, 1, 1, 1, 0, 704, 100
36234, V, 1, 1, 1, 1, 0, 704, 100
36235, V, 1, 1, 1, 1, 0, 704, 100
36236, V, 1, 1, 1, 1, 0, 704, 100
36237, V, 1, 1, 1, 1, 0, 704, 100
36238, V, 1, 1, 1, 1, 0, 704, 100
36239, V, 1, 1, 1, 1, 0, 704, 100
36240, V, 1, 1, 1, 1, 0, 704, 100
36241, V, 1, 1, 1, 1, 0, 704, 100
36242, V, 1, 1, 1, 1, 0, 704, 100
36243, V, 1, 1, 1, 1, 0, 704, 100
36244, V, 1, 1, 1, 1, 0, 704, 100
36245, V, 1, 1, 1, 1, 0, 704, 100
36246, V, 1, 1, 1, 1, 0, 704, 100
36247, V, 1, 1, 1, 1, 0, 704, 100
36248, V, 1, 1, 1, 1, 0, 704, 100
36249, V, 1, 1, 1, 1, 0, 704, 100
36250, V, 1, 1, 1, 1, 0, 704, 100
36251, V, 1, 1, 1, 1, 0, 704, 100
36252, V, 1, 1, 1, 1, 0, 704, 100
36253, V, 1, 1, 1, 1, 0, 704, 100
36254, V, 1, 1, 1, 1, 0, 704, 100
36255, V, 1, 1, 1, 1, 0, 704, 100
36256, V, 1, 1, 1, 1, 0, 704, 100
36257, V, 1, 1, 1, 1, 0, 704, 100
36258, V, 1, 1, 1, 1, 0, 704, 100
36259, V, 1, 1, 1, 1, 0, 704, 100
36260, V, 1, 1, 1, 1, 0, 704, 100
36261, V, 1, 1, 1, 1, 0, 704, 100
36262, V, 1, 1, 1, 1, 0, 704, 100
36263, V, 1, 1, 1, 1, 0, 704, 100
36264, V, 1, 1, 1, 1, 0, 704, 100
36265, V, 1, 1, 1, 1, 0, 704, 100
36267, V, 1, 1, 1, 1, 0, 704, 100
36268, V, 1, 1, 1, 1, 0, 704, 100
36269, V, 1, 1, 1, 1, 0, 704, 100
36270, V, 1, 1, 1, 1, 0, 704, 100
36271, V, 1, 1, 1, 1, 0, 704, 100
36272, V, 1, 1, 1, 1, 0, 704, 100
36273, V, 1, 1, 1, 1, 0, 704, 100
36274, V, 1, 1, 1, 1, 0, 704, 100
36275, V, 1, 1, 1, 1, 0, 704, 100
36276, V, 1, 1, 1, 1, 0, 704, 100
36277, V, 1, 1, 1, 1, 0, 704, 100
36278, V, 1, 1, 1, 1, 0, 704, 100
36279, V, 1, 1, 1, 1, 0, 704, 100
36280, V, 1, 1, 1, 1, 0, 704, 100
36281, V, 1, 1, 1, 1, 0, 704, 100
36282, V, 1, 1, 1, 1, 0, 704, 100
36283, V, 1, 1, 1, 1, 0, 704, 100
36284, V, 1, 1, 1, 1, 0, 704, 100
36285, V, 1, 1, 1, 1, 0, 704, 100
36286, V, 1, 1, 1, 1, 0, 704, 100
36287, V, 1, 1, 1, 1, 0, 704, 100
36288, V, 1, 1, 1, 1, 0, 704, 100
36289, V, 1, 1, 1, 1, 0, 704, 100
36290, V, 1, 1, 1, 1, 0, 704, 100
36291, V, 1, 1, 1, 1, 0, 704, 100
36292, V, 1, 1, 1, 1, 0, 704, 100
36293, V, 1, 1, 1, 1, 0, 704, 100
36294, V, 1, 1, 1, 1, 0, 704, 100
36295, V, 1, 1, 1, 1, 0, 704, 100
36296, V, 1, 1, 1, 1, 0, 704, 100
36297, V, 1, 1, 1, 1, 0, 704, 100
36298, V, 1, 1, 1, 1, 0, 704, 100
36299, V, 1, 1, 1, 1, 0, 704, 100
36300, V, 1, 1, 1, 1, 0, 704, 100
36301, V, 1, 1, 1, 1, 0, 704, 100
36302, V, 1, 1, 1, 1, 0, 704, 100
36303, V, 1, 1, 1, 1, 0, 704, 100
36304, V, 1, 1, 1, 1, 0, 704, 100
36305, V, 1, 1, 1, 1, 0, 704, 100
36306, V, 1, 1, 1, 1, 0, 704, 100
36307, V, 1, 1, 1, 1, 0, 704, 100
36308, V, 1, 1, 1, 1, 0, 704, 100
36310, V, 1, 1, 1, 1, 0, 704, 100
36311, V, 1, 1, 1, 1, 0, 704, 100
36312, V, 1, 1, 1, 1, 0, 704, 100
36313, V, 1, 1, 1, 1, 0, 704, 100
36314, V, 1, 1, 1, 1, 0, 704, 100
36315, V, 1, 1, 1, 1, 0, 704, 100
36316, V, 1, 1, 1, 1, 0, 704, 100
36317, V, 1, 1, 1, 1, 0, 704, 100
36318, V, 1, 1, 1, 1, 0, 704, 100
36319, V, 1, 1, 1, 1, 0, 704, 100
36320, V, 1, 1, 1, 1, 0, 704, 100
36321, V, 1, 1, 1, 1, 0, 704, 100
36322, V, 1, 1, 1, 1, 0, 704, 100
36323, V, 1, 1, 1, 1, 0, 704, 100
36324, V, 1, 1, 1, 1, 0, 704, 100
36325, V, 1, 1, 1, 1, 0, 704, 100
36326, V, 1, 1, 1, 1, 0, 704, 100
36327, V, 1, 1, 1, 1, 0, 704, 100
36328, V, 1, 1, 1, 1, 0, 704, 100
36329, V, 1, 1, 1, 1, 0, 704, 100
36330, V, 1, 1, 1, 1, 0, 704, 100
36331, V, 1, 1, 1, 1, 0, 704, 100
36332, V, 1, 1, 1, 1, 0, 704, 100
36333, V, 1, 1, 1, 1, 0, 704, 100
36334, V, 1, 1, 1, 1, 0, 704, 100
36335, V, 1, 1, 1, 1, 0, 704, 100
36336, V, 1, 1, 1, 1, 0, 704, 100
36337, V, 1, 1, 1, 1, 0, 704, 100
36338, V, 1, 1, 1, 1, 0, 704, 100
36339, V, 1, 1, 1, 1, 0, 704, 100
36340, V, 1, 1, 1, 1, 0, 704, 100
36341, V, 1, 1, 1, 1, 0, 704, 100
36342, V, 1, 1, 1, 1, 0, 704, 100
36343, V, 1, 1, 1, 1, 0, 704, 100
36344, V, 1, 1, 1, 1, 0, 704, 100
36345, V, 1, 1, 1, 1, 0, 704, 100
36346, V, 1, 1, 1, 1, 0, 704, 100
36347, V, 1, 1, 1, 1, 0, 704, 100
36348, V, 1, 1, 1, 1, 0, 704, 100
36349, V, 1, 1, 1, 1, 0, 704, 100
36350, V, 1, 1, 1, 1, 0, 704, 100
36352, V, 1, 1, 1, 1, 0, 704, 100
36353, V, 1, 1, 1, 1, 0, 704, 100
36354, V, 1, 1, 1, 1, 0, 704, 100
36355, V, 1, 1, 1, 1, 0, 704, 100
36356, V, 1, 1, 1, 1, 0, 704, 100
36357, V, 1, 1, 1, 1, 0, 704, 100
36358, V, 1, 1, 1, 1, 0, 704, 100
36359, V, 1, 1, 1, 1, 0, 704, 100
36360, V, 1, 1, 1, 1, 0, 704, 100
36361, V, 1, 1, 1, 1, 0, 704, 100
36362, V, 1, 1, 1, 1, 0, 704, 100
36363, V, 1, 1, 1, 1, 0, 704, 100
36364, V, 1, 1, 1, 1, 0, 704, 100
36365, V, 1, 1, 1, 1, 0, 704, 100
36366, V, 1, 1, 1, 1, 0, 704, 100
36367, V, 1, 1, 1, 1, 0, 704, 100
36368, V, 1, 1, 1, 1, 0, 704, 100
36369, V, 1, 1, 1, 1, 0, 704, 100
36370, V, 1, 1, 1, 1, 0, 704, 100
36371, V, 1, 1, 1, 1, 0, 704, 100
36372, V, 1, 1, 1, 1, 0, 704, 100
36373, V, 1, 1, 1, 1, 0, 704, 100
36374, V, 1, 1, 1, 1, 0, 704, 100
36375, V, 1, 1, 1, 1, 0, 704, 100
36376, V, 1, 1, 1, 1, 0, 704, 100
36377, V, 1, 1, 1, 1, 0, 704, 100
36378, V, 1, 1, 1, 1, 0, 704, 100
36379, V, 1, 1, 1, 1, 0, 704, 100
36380, V, 1, 1, 1, 1, 0, 704, 100
36381, V, 1, 1, 1, 1, 0, 704, 100
36382, V, 1, 1, 1, 1, 0, 704, 100
36383, V, 1, 1, 1, 1, 0, 704, 100
36384, V, 1, 1, 1, 1, 0, 704, 100
36385, V, 1, 1, 1, 1, 0, 704, 100
36386, V, 1, 1, 1, 1, 0, 704, 100
36387, V, 1, 1, 1, 1, 0, 704, 100
36388, V, 1, 1, 1, 1, 0, 704, 100
36389, V, 1, 1, 1, 1, 0, 704, 100
36390, V, 1, 1, 1, 1, 0, 704, 100
36391, V, 1, 1, 1, 1, 0, 704, 100
36392, V, 1, 1, 1, 1, 0, 704, 100
36393, V, 1, 1, 1, 1, 0, 704, 100
36395, V, 1, 1, 1, 1, 0, 704, 100
36396, V, 1, 1, 1, 1, 0, 704, 100
36397, V, 1, 1, 1, 1, 0, 704, 100
36398, V, 1, 1, 1, 1, 0, 704, 100
36399, V, 1, 1, 1, 1, 0, 704, 100
36400, V, 1, 1, 1, 1, 0, 704, 100
36401, V, 1, 1, 1, 1, 0, 704, 100
36402, V, 1, 1, 1, 1, 0, 704, 100
36403, V, 1, 1, 1, 1, 0, 704, 100
36404, V, 1, 1, 1, 1, 0, 704, 100
36405, V, 1, 1, 1, 1, 0, 704, 100
36406, V, 1, 1, 1, 1, 0, 704, 100
36407, V, 1, 1, 1, 1, 0, 704, 100
36408, V, 1, 1, 1, 1, 0, 704, 100
36409, V, 1, 1, 1, 1, 0, 704, 100
36410, V, 1, 1, 1, 1, 0, 704, 100
36411, V, 1, 1, 1, 1, 0, 704, 100
36412, V, 1, 1, 1, 1, 0, 704, 100
36413, V, 1, 1, 1, 1, 0, 704, 100
36414, V, 1, 1, 1, 1, 0, 704, 100
36415, V, 1, 1, 1, 1, 0, 704, 100
36416, V, 1, 1, 1, 1, 0, 704, 100
36417, V, 1, 1, 1, 1, 0, 704, 100
36418, V, 1, 1, 1, 1, 0, 704, 100
36419, V, 1, 1, 1, 1, 0, 704, 100
36420, V, 1, 1, 1, 1, 0, 704, 100
36421, V, 1, 1, 1, 1, 0, 704, 100
36422, V, 1, 1, 1, 1, 0, 704, 100
36423, V, 1, 1, 1, 1, 0, 704, 100
36424, V, 1, 1, 1, 1, 0, 704, 100
36425, V, 1, 1, 1, 1, 0, 704, 100
36426, V, 1, 1, 1, 1, 0, 704, 100
36427, V, 1, 1, 1, 1, 0, 704, 100
36428, V, 1, 1, 1, 1, 0, 704, 100
36429, V, 1, 1, 1, 1, 0, 704, 100
36430, V, 1, 1, 1, 1, 0, 704, 100
36431, V, 1, 1, 1, 1, 0, 704, 100
36432, V, 1, 1, 1, 1, 0, 704, 100
36433, V, 1, 1, 1, 1, 0, 704, 100
36434, V, 1, 1, 1, 1, 0, 704, 100
36435, V, 1, 1, 1, 1, 0, 704, 100
36436, V, 1, 1, 1, 1, 0, 704, 100
36438, V, 1, 1, 1, 1, 0, 704, 100
36439, V, 1, 1, 1, 1, 0, 704, 100
36440, V, 1, 1, 1, 1, 0, 704, 100
36441, V, 1, 1, 1, 1, 0, 704, 100
36442, V, 1, 1, 1, 1, 0, 704, 100
36443, V, 1, 1, 1, 1, 0, 704, 100
36444, V, 1, 1, 1, 1, 0, 704, 100
36445, V, 1, 1, 1, 1, 0, 704, 100
36446, V, 1, 1, 1, 1, 0, 704, 100
36447, V, 1, 1, 1, 1, 0, 704, 100
36448, V, 1, 1, 1, 1, 0, 704, 100
36449, V, 1, 1, 1, 1, 0, 704, 100
36450, V, 1, 1, 1, 1, 0, 704, 100
36451, V, 1, 1, 1, 1, 0, 704, 100
36452, V, 1, 1, 1, 1, 0, 704, 100
36453, V, 1, 1, 1, 1, 0, 704, 100
36454, V, 1, 1, 1, 1, 0, 704, 100
36455, V, 1, 1, 1, 1, 0, 704, 100
36456, V, 1, 1, 1, 1, 0, 704, 100
36457, V, 1, 1, 1, 1, 0, 704, 100
36458, V, 1, 1, 1, 1, 0, 704, 100
36459, V, 1, 1, 1, 1, 0, 704, 100
36460, V, 1, 1, 1, 1, 0, 704, 100
36461, V, 1, 1, 1, 1, 0, 704, 100
36462, V, 1, 1, 1, 1, 0, 704, 100
36463, V, 1, 1, 1, 1, 0, 704, 100
36464, V, 1, 1, 1, 1, 0, 704, 100
36465, V, 1, 0, 0, 1, 0, 704, 100
36465, V, 1, 0, 0, 0, 0, 704, 100
36466, V, 1, 1, 0, 0, 0, 704, 100
36466, V, 1, 1, 0, 0, 0, 704, 100
36467, V, 1, 1, 1, 1, 0, 704, 100
36468, V, 1, 1, 1, 1, 0, 704, 100
36469, V, 1, 1, 1, 1, 0, 704, 100
36470, V, 1, 1, 1, 1, 0, 704, 100
36471, V, 1, 1, 1, 1, 0, 704, 100
36472, V, 1, 1, 1, 1, 0, 704, 99
36473, V, 1, 1, 1, 1, 0, 704, 99
36474, V, 1, 1, 1, 1, 0, 704, 99
36475, V, 1, 1, 1, 1, 0, 704, 99
36476, V, 1, 1, 1, 1, 0, 704, 99
36477, V, 1, 1, 1, 1, 0, 704, 99
36478, V, 1, 1, 1, 1, 0, 704, 99
36480, V, 1, 1, 1, 1, 0, 704, 99
36481, V, 1, 1, 1, 1, 0, 704, 99
36482, V, 1, 1, 1, 1, 0, 704, 99
36483, V, 1, 1, 1, 1, 0, 704, 99
36484, V, 1, 1, 1, 1, 0, 704, 99
36485, V, 1, 1, 1, 1, 0, 704, 99
36486, V, 1, 1, 1, 1, 0, 704, 99
36487, V, 1, 1, 1, 1, 0, 704, 99
36488, V, 1, 1, 1, 1, 0, 704, 99
36489, V, 1, 1, 1, 1, 0, 704, 99
36490, V, 1, 1, 1, 1, 0, 704, 99
36491, V, 1, 1, 1, 1, 0, 704, 99
36492, V, 1, 1, 1, 1, 0, 704, 99
36493, V, 1, 1, 1, 1, 0, 704, 99
36494, V, 1, 1, 1, 1, 0, 704, 99
36495, V, 1, 1, 1, 1, 0, 704, 99
36496, V, 1, 1, 1, 1, 0, 704, 99
36497, V, 1, 1, 1, 1, 0, 704, 99
36498, V, 1, 1, 1, 1, 0, 704, 99
36499, V, 1, 1, 1, 1, 0, 704, 99
36500, V, 1, 1, 1, 1, 0, 704, 99
36501, V, 1, 1, 1, 1, 0, 704, 99
36502, V, 1, 1, 1, 1, 0, 704, 99
36503, V, 1, 1, 1, 1, 0, 704, 99
36504, V, 1, 1, 1, 1, 0, 704, 99
36505, V, 1, 1, 1, 1, 0, 704, 99
36506, V, 1, 1, 1, 1, 0, 704, 99
36507, V, 1, 1, 1, 1, 0, 704, 99
36508, V, 1, 1, 1, 1, 0, 704, 100
36509, V, 1, 1, 1, 1, 0, 704, 99
36510, V, 1, 1, 1, 1, 0, 704, 100
36511, V, 1, 1, 1, 1, 0, 704, 100
36512, V, 1, 1, 1, 1, 0, 704, 100
36513, V, 1, 1, 1, 1, 0, 704, 99
36514, V, 1, 1, 1, 1, 0, 704, 100
36515, V, 1, 1, 1, 1, 0, 704, 100
36516, V, 1, 1, 1, 1, 0, 704, 100
36517, V, 1, 1, 1, 1, 0, 704, 100
36518, V, 1, 1, 1, 1, 0, 704, 100
36519, V, 1, 1, 1, 1, 0, 704, 100
36520, V, 1, 1, 1, 1, 0, 704, 100
36521, V, 1, 1, 1, 1, 0, 704, 100
36523, V, 1, 1, 1, 1, 0, 704, 100
36524, V, 1, 1, 1, 1, 0, 704, 100
36525, V, 1, 1, 1, 1, 0, 704, 100
36526, V, 1, 1, 1, 1, 0, 704, 100
36527, V, 1, 1, 1, 1, 0, 704, 100
36528, V, 1, 1, 1, 1, 0, 704, 100
36529, V, 1, 1, 1, 1, 0, 704, 100
36530, V, 1, 1, 1, 1, 0, 704, 100
36531, V, 1, 1, 1, 1, 0, 704, 100
36532, V, 1, 1, 1, 1, 0, 704, 100
36533, V, 1, 1, 1, 1, 0, 704, 100
36534, V, 1, 1, 1, 1, 0, 704, 100
36535, V, 1, 1, 1, 1, 0, 704, 100
36536, V, 1, 1, 1, 1, 0, 704, 100
36537, V, 1, 1, 1, 1, 0, 704, 100
36538, V, 1, 1, 1, 1, 0, 704, 100
36539, V, 1, 1, 1, 1, 0, 704, 100
36540, V, 1, 1, 1, 1, 0, 704, 100
36541, V, 1, 1, 1, 1, 0, 704, 100
36542, V, 1, 1, 1, 1, 0, 704, 100
36543, V, 1, 1, 1, 1, 0, 704, 100
36544, V, 1, 1, 1, 1, 0, 704, 100
36545, V, 1, 1, 1, 1, 0, 704, 100
36546, V, 1, 1, 1, 1, 0, 704, 100
36547, V, 1, 1, 1, 1, 0, 704, 100
36548, V, 1, 1, 1, 1, 0, 704, 100
36549, V, 1, 1, 1, 1, 0, 704, 100
36550, V, 1, 1, 1, 1, 0, 704, 100
36551, V, 1, 1, 1, 1, 0, 704, 100
36552, V, 1, 1, 1, 1, 0, 704, 100
36553, V, 1, 1, 1, 1, 0, 704, 100
36554, V, 1, 1, 1, 1, 0, 704, 100
36555, V, 1, 1, 1, 1, 0, 704, 100
36556, V, 1, 1, 1, 1, 0, 704, 100
36557, V, 1, 1, 1, 1, 0, 704, 100
36558, V, 1, 1, 1, 1, 0, 704, 100
36559, V, 1, 1, 1, 1, 0, 704, 100
36560, V, 1, 1, 1, 1, 0, 704, 100
36561, V, 1, 1, 1, 1, 0, 704, 100
36562, V, 1, 1, 1, 1, 0, 704, 100
36563, V, 1, 1, 1, 1, 0, 704, 100
36564, V, 1, 1, 1, 1, 0, 704, 100
36566, V, 1, 1, 1, 1, 0, 704, 100
36567, V, 1, 1, 1, 1, 0, 704, 100
36568, V, 1, 1, 1, 1, 0, 704, 100
36569, V, 1, 1, 1, 1, 0, 704, 100
36570, V, 1, 1, 1, 1, 0, 704, 100
36571, V, 1, 1, 1, 1, 0, 704, 100
36572, V, 1, 1, 1, 1, 0, 704, 100
36573, V, 1, 1, 1, 1, 0, 704, 100
36574, V, 1, 1, 1, 1, 0, 704, 100
36575, V, 1, 1, 1, 1, 0, 704, 100
36576, V, 1, 1, 1, 1, 0, 704, 100
36577, V, 1, 1, 1, 1, 0, 704, 100
36578, V, 1, 1, 1, 1, 0, 704, 100
36579, V, 1, 1, 1, 1, 0, 704, 100
36580, V, 1, 1, 1, 1, 0, 704, 100
36581, V, 1, 1, 1, 1, 0, 704, 100
36582, V, 1, 1, 1, 1, 0, 704, 100
36583, V, 1, 1, 1, 1, 0, 704, 100
36584, V, 1, 1, 1, 1, 0, 704, 100
36585, V, 1, 1, 1, 1, 0, 704, 100
36586, V, 1, 1, 1, 1, 0, 704, 100
36587, V, 1, 1, 1, 1, 0, 704, 100
36588, V, 1, 1, 1, 1, 0, 704, 100
36589, V, 1, 1, 1, 1, 0, 704, 100
36590, V, 1, 1, 1, 1, 0, 704, 100
36591, V, 1, 1, 1, 1, 0, 704, 100
36592, V, 1, 1, 1, 1, 0, 704, 100
36593, V, 1, 1, 1, 1, 0, 704, 100
36594, V, 1, 1, 1, 1, 0, 704, 100
36595, V, 1, 1, 1, 1, 0, 704, 100
36596, V, 1, 1, 1, 1, 0, 704, 100
36597, V, 1, 1, 1, 1, 0, 704, 100
36598, V, 1, 1, 1, 1, 0, 704, 100
36599, V, 1, 1, 1, 1, 0, 704, 100
36600, V, 1, 1, 1, 1, 0, 704, 100
36601, V, 1, 1, 1, 1, 0, 704, 100
36602, V, 1, 1, 1, 1, 0, 704, 100
36603, V, 1, 1, 1, 1, 0, 704, 100
36604, V, 1, 1, 1, 1, 0, 704, 100
36605, V, 1, 1, 1, 1, 0, 704, 100
36606, V, 1, 1, 1, 1, 0, 704, 100
36608, V, 1, 1, 1, 1, 0, 704, 100
36609, V, 1, 1, 1, 1, 0, 704, 100
36610, V, 1, 1, 1, 1, 0, 704, 100
36611, V, 1, 1, 1, 1, 0, 704, 100
36612, V, 1, 1, 1, 1, 0, 704, 100
36613, V, 1, 1, 1, 1, 0, 704, 100
36614, V, 1, 1, 1, 1, 0, 704, 100
36615, V, 1, 1, 1, 1, 0, 704, 100
36616, V, 1, 1, 1, 1, 0, 704, 100
36617, V, 1, 1, 1, 1, 0, 704, 100
36618, V, 1, 1, 1, 1, 0, 704, 100
36619, V, 1, 1, 1, 1, 0, 704, 100
36620, V, 1, 1, 1, 1, 0, 704, 100
36621, V, 1, 1, 1, 1, 0, 704, 100
36622, V, 1, 1, 1, 1, 0, 704, 100
36623, V, 1, 1, 1, 1, 0, 704, 100
36624, V, 1, 1, 1, 1, 0, 704, 100
36625, V, 1, 1, 1, 1, 0, 704, 100
36626, V, 1, 1, 1, 1, 0, 704, 100
36627, V, 1, 1, 1, 1, 0, 704, 100
36628, V, 1, 1, 1, 1, 0, 704, 100
36629, V, 1, 1, 1, 1, 0, 704, 100
36630, V, 1, 1, 1, 1, 0, 704, 100
36631, V, 1, 1, 1, 1, 0, 704, 100
36632, V, 1, 1, 1, 1, 0, 704, 100
36633, V, 1, 1, 1, 1, 0, 704, 100
36634, V, 1, 1, 1, 1, 0, 704, 100
36635, V, 1, 1, 1, 1, 0, 704, 100
36636, V, 1, 1, 1, 1, 0, 704, 100
36637, V, 1, 1, 1, 1, 0, 704, 100
36638, V, 1, 1, 1, 1, 0, 704, 100
36639, V, 1, 1, 1, 1, 0, 704, 100
36640, V, 1, 1, 1, 1, 0, 704, 100
36641, V, 1, 1, 1, 1, 0, 704, 100
36642, V, 1, 1, 1, 1, 0, 704, 100
36643, V, 1, 1, 1, 1, 0, 704, 100
36644, V, 1, 1, 1, 1, 0, 704, 100
36645, V, 1, 1, 1, 1, 0, 704, 100
36646, V, 1, 1, 1, 1, 0, 704, 100
36647, V, 1, 1, 1, 1, 0, 704, 100
36648, V, 1, 1, 1, 1, 0, 704, 100
36649, V, 1, 1, 1, 1, 0, 704, 100
36651, V, 1, 1, 1, 1, 0, 704, 100
36652, V, 1, 1, 1, 1, 0, 704, 100
36653, V, 1, 1, 1, 1, 0, 704, 100
36654, V, 1, 1, 1, 1, 0, 704, 100
36655, V, 1, 1, 1, 1, 0, 704, 100
36656, V, 1, 1, 1, 1, 0, 704, 100
36657, V, 1, 1, 1, 1, 0, 704, 100
36658, V, 1, 1, 1, 1, 0, 704, 100
36659, V, 1, 1, 1, 1, 0, 704, 100
36660, V, 1, 1, 1, 1, 0, 704, 100
36661, V, 1, 1, 1, 1, 0, 704, 100
36662, V, 1, 1, 1, 1, 0, 704, 100
36663, V, 1, 1, 1, 1, 0, 704, 100
36664, V, 1, 1, 1, 1, 0, 704, 100
36665, V, 1, 1, 1, 1, 0, 704, 100
36666, V, 1, 1, 1, 1, 0, 704, 100
36667, V, 1, 1, 1, 1, 0, 704, 100
36668, V, 1, 1, 1, 1, 0, 704, 100
36669, V, 1, 1, 1, 1, 0, 704, 100
36670, V, 1, 1, 1, 1, 0, 704, 100
36671, V, 1, 1, 1, 1, 0, 704, 100
36672, V, 1, 1, 1, 1, 0, 704, 100
36673, V, 1, 1, 1, 1, 0, 704, 100
36674, V, 1, 1, 1, 1, 0, 704, 100
36675, V, 1, 1, 1, 1, 0, 704, 100
36676, V, 1, 1, 1, 1, 0, 704, 100
36677, V, 1, 1, 1, 1, 0, 704, 100
36678, V, 1, 1, 1, 1, 0, 704, 100
36679, V, 1, 1, 1, 1, 0, 704, 100
36680, V, 1, 1, 1, 1, 0, 704, 100
36681, V, 1, 1, 1, 1, 0, 704, 100
36682, V, 1, 1, 1, 1, 0, 704, 100
36683, V, 1, 1, 1, 1, 0, 704, 100
36684, V, 1, 1, 1, 1, 0, 704, 100
36685, V, 1, 1, 1, 1, 0, 704, 100
36686, V, 1, 1, 1, 1, 0, 704, 100
36687, V, 1, 1, 1, 1, 0, 704, 100
36688, V, 1, 1, 1, 1, 0, 704, 100
36689, V, 1, 1, 1, 1, 0, 704, 100
36690, V, 1, 1, 1, 1, 0, 704, 100
36691, V, 1, 1, 1, 1, 0, 704, 100
36692, V, 1, 1, 1, 1, 0, 704, 100
36694, V, 1, 1, 1, 1, 0, 704, 100
36695, V, 1, 1, 1, 1, 0, 704, 100
36696, V, 1, 1, 1, 1, 0, 704, 100
36697, V, 1, 1, 1, 1, 0, 704, 100
36698, V, 1, 1, 1, 1, 0, 704, 100
36699, V, 1, 1, 1, 1, 0, 704, 100
36700, V, 1, 1, 1, 1, 0, 704, 100
36701, V, 1, 1, 1, 1, 0, 704, 100
36702, V, 1, 1, 1, 1, 0, 704, 100
36703, V, 1, 1, 1, 1, 0, 704, 100
36704, V, 1, 1, 1, 1, 0, 704, 100
36705, V, 1, 1, 1, 1, 0, 704, 100
36706, V, 1, 1, 1, 1, 0, 704, 100
36707, V, 1, 1, 1, 1, 0, 704, 100
36708, V, 1, 1, 1, 1, 0, 704, 100
36709, V, 1, 1, 1, 1, 0, 704, 100
36710, V, 1, 1, 1, 1, 0, 704, 100
36711, V, 1, 1, 1, 1, 0, 704, 100
36712, V, 1, 1, 1, 1, 0, 704, 100
36713, V, 1, 1, 1, 1, 0, 704, 100
36714, V, 1, 1, 1, 1, 0, 704, 100
36715, V, 1, 1, 1, 1, 0, 704, 100
36716, V, 1, 1, 1, 1, 0, 704, 100
36717, V, 1, 1, 1, 1, 0, 704, 100
36718, V, 1, 1, 1, 1, 0, 704, 100
36719, V, 1, 1, 1, 1, 0, 704, 100
36720, V, 1, 1, 1, 1, 0, 704, 100
36721, V, 1, 1, 1, 1, 0, 704, 100
36722, V, 1, 1, 1, 1, 0, 704, 100
36723, V, 1, 1, 1, 1, 0, 704, 100
36724, V, 1, 1, 1, 1, 0, 704, 100
36725, V, 1, 1, 1, 1, 0, 704, 100
36726, V, 1, 1, 1, 1, 0, 704, 100
36727, V, 1, 1, 1, 1, 0, 704, 100
36728, V, 1, 1, 1, 1, 0, 704, 100
36729, V, 1, 1, 1, 1, 0, 704, 100
36730, V, 1, 1, 1, 1, 0, 704, 100
36731, V, 1, 1, 1, 1, 0, 704, 100
36732, V, 1, 1, 1, 1, 0, 704, 100
36733, V, 1, 1, 1, 1, 0, 704, 100
36734, V, 1, 1, 1, 1, 0, 704, 100
36736, V, 1, 1, 1, 1, 0, 704, 100
36737, V, 1, 1, 1, 1, 0, 704, 100
36738, V, 1, 1, 1, 1, 0, 704, 100
36739, V, 1, 1, 1, 1, 0, 704, 100
36740, V, 1, 1, 1, 1, 0, 704, 100
36741, V, 1, 1, 1, 1, 0, 704, 100
36742, V, 1, 1, 1, 1, 0, 704, 100
36743, V, 1, 1, 1, 1, 0, 704, 100
36744, V, 1, 1, 1, 1, 0, 704, 100
36745, V, 1, 1, 1, 1, 0, 704, 100
36746, V, 1, 1, 1, 1, 0, 704, 100
36747, V, 1, 1, 1, 1, 0, 704, 100
36748, V, 1, 1, 1, 1, 0, 704, 100
36749, V, 1, 1, 1, 1, 0, 704, 100
36750, V, 1, 1, 1, 1, 0, 704, 100
36751, V, 1, 1, 1, 1, 0, 704, 100
36752, V, 1, 1, 1, 1, 0, 704, 100
36753, V, 1, 1, 1, 1, 0, 704, 100
36754, V, 1, 1, 1, 1, 0, 704, 100
36755, V, 1, 1, 1, 1, 0, 704, 100
36756, V, 1, 1, 1, 1, 0, 704, 100
36757, V, 1, 1, 1, 1, 0, 704, 100
36758, V, 1, 1, 1, 1, 0, 704, 100
36759, V, 1, 1, 1, 1, 0, 704, 100
36760, V, 1, 1, 1, 1, 0, 704, 100
36761, V, 1, 1, 1, 1, 0, 704, 100
36762, V, 1, 1, 1, 1, 0, 704, 100
36763, V, 1, 1, 1, 1, 0, 704, 100
36764, V, 1, 1, 1, 1, 0, 704, 100
36765, V, 1, 1, 1, 1, 0, 704, 100
36766, V, 1, 1, 1, 1, 0, 704, 100
36767, V, 1, 1, 1, 1, 0, 704, 100
36768, V, 1, 1, 1, 1, 0, 704, 100
36769, V, 1, 1, 1, 1, 0, 704, 100
36770, V, 1, 1, 1, 1, 0, 704, 100
36771, V, 1, 1, 1, 1, 0, 704, 100
36772, V, 1, 1, 1, 1, 0, 704, 100
36773, V, 1, 1, 1, 1, 0, 704, 100
36774, V, 1, 1, 1, 1, 0, 704, 100
36775, V, 1, 1, 1, 1, 0, 704, 100
36776, V, 1, 1, 1, 1, 0, 704, 100
36777, V, 1, 1, 1, 1, 0, 704, 100
36779, V, 1, 1, 1, 1, 0, 704, 100
36780, V, 1, 1, 1, 1, 0, 704, 100
36781, V, 1, 1, 1, 1, 0, 704, 100
36782, V, 1, 1, 1, 1, 0, 704, 100
36783, V, 1, 1, 1, 1, 0, 704, 100
36784, V, 1, 1, 1, 1, 0, 704, 100
36785, V, 1, 1, 1, 1, 0, 704, 100
36786, V, 1, 1, 1, 1, 0, 704, 100
36787, V, 1, 1, 1, 1, 0, 704, 100
36788, V, 1, 1, 1, 1, 0, 704, 100
36789, V, 1, 1, 1, 1, 0, 704, 100
36790, V, 1, 1, 1, 1, 0, 704, 100
36791, V, 1, 1, 1, 1, 0, 704, 100
36792, V, 1, 1, 1, 1, 0, 704, 100
36793, V, 1, 1, 1, 1, 0, 704, 100
36794, V, 1, 1, 1, 1, 0, 704, 100
36795, V, 1, 1, 1, 1, 0, 704, 100
36796, V, 1, 1, 1, 1, 0, 704, 100
36797, V, 1, 1, 1, 1, 0, 704, 100
36798, V, 1, 1, 1, 1, 0, 704, 100
36799, V, 1, 1, 1, 1, 0, 704, 100
36800, V, 1, 1, 1, 1, 0, 704, 100
36801, V, 1, 1, 1, 1, 0, 704, 100
36802, V, 1, 1, 1, 1, 0, 704, 100
36803, V, 1, 1, 1, 1, 0, 704, 100
36804, V, 1, 1, 1, 1, 0, 704, 100
36805, V, 1, 1, 1, 1, 0, 704, 100
36806, V, 1, 1, 1, 1, 0, 704, 100
36807, V, 1, 1, 1, 1, 0, 704, 100
36808, V, 1, 1, 1, 1, 0, 704, 100
36809, V, 1, 1, 1, 1, 0, 704, 100
36810, V, 1, 1, 1, 1, 0, 704, 100
36811, V, 1, 1, 1, 1, 0, 704, 100
36812, V, 1, 1, 1, 1, 0, 704, 100
36813, V, 1, 1, 1, 1, 0, 704, 100
36814, V, 1, 1, 1, 1, 0, 704, 100
36815, V, 1, 1, 1, 1, 0, 704, 100
36816, V, 1, 1, 1, 1, 0, 704, 100
36817, V, 1, 1, 1, 1, 0, 704, 100
36818, V, 1, 1, 1, 1, 0, 704, 100
36819, V, 1, 1, 1, 1, 0, 704, 100
36820, V, 1, 1, 1, 1, 0, 704, 100
36822, V, 1, 1, 1, 1, 0, 704, 100
36823, V, 1, 1, 1, 1, 0, 704, 100
36824, V, 1, 1, 1, 1, 0, 704, 100
36825, V, 1, 1, 1, 1, 0, 704, 100
36826, V, 1, 1, 1, 1, 0, 704, 100
36827, V, 1, 1, 1, 1, 0, 704, 100
36828, V, 1, 1, 1, 1, 0, 704, 100
36829, V, 1, 1, 1, 1, 0, 704, 100
36830, V, 1, 1, 1, 1, 0, 704, 100
36831, V, 1, 1, 1, 1, 0, 704, 100
36832, V, 1, 1, 1, 1, 0, 704, 100
36833, V, 1, 1, 1, 1, 0, 704, 100
36834, V, 1, 1, 1, 1, 0, 704, 100
36835, V, 1, 1, 1, 1, 0, 704, 100
36836, V, 1, 1, 1, 1, 0, 704, 100
36837, V, 1, 1, 1, 1, 0, 704, 100
36838, V, 1, 1, 1, 1, 0, 704, 100
36839, V, 1, 1, 1, 1, 0, 704, 100
36840, V, 1, 1, 1, 1, 0, 704, 100
36841, V, 1, 1, 1, 1, 0, 704, 100
36842, V, 1, 1, 1, 1, 0, 704, 100
36843, V, 1, 1, 1, 1, 0, 704, 100
36844, V, 1, 1, 1, 1, 0, 704, 100
36845, V, 1, 1, 1, 1, 0, 704, 100
36846, V, 1, 1, 1, 1, 0, 704, 100
36847, V, 1, 1, 1, 1, 0, 704, 100
36848, V, 1, 1, 1, 1, 0, 704, 100
36849, V, 1, 1, 1, 1, 0, 704, 100
36850, V, 1, 1, 1, 1, 0, 704, 100
36851, V, 1, 1, 1, 1, 0, 704, 100
36852, V, 1, 1, 1, 1, 0, 704, 100
36853, V, 1, 1, 1, 1, 0, 704, 100
36854, V, 1, 1, 1, 1, 0, 704, 100
36855, V, 1, 1, 1, 1, 0, 704, 100
36856, V, 1, 1, 1, 1, 0, 704, 100
36857, V, 1, 1, 1, 1, 0, 704, 100
36858, V, 1, 1, 1, 1, 0, 704, 100
36859, V, 1, 1, 1, 1, 0, 704, 100
36860, V, 1, 1, 1, 1, 0, 704, 100
36861, V, 1, 1, 1, 1, 0, 704, 100
36862, V, 1, 1, 1, 1, 0, 704, 100
36864, V, 1, 1, 1, 1, 0, 704, 100
36865, V, 1, 1, 1, 1, 0, 704, 100
36866, V, 1, 1, 1, 1, 0, 704, 100
36867, V, 1, 1, 1, 1, 0, 704, 100
36868, V, 1, 1, 1, 1, 0, 704, 100
36869, V, 1, 1, 1, 1, 0, 704, 100
36870, V, 1, 1, 1, 1, 0, 704, 100
36871, V, 1, 1, 1, 1, 0, 704, 100
36872, V, 1, 1, 1, 1, 0, 704, 100
36873, V, 1, 1, 1, 1, 0, 704, 100
36874, V, 1, 1, 1, 1, 0, 704, 100
36875, V, 1, 1, 1, 1, 0, 704, 100
36876, V, 1, 1, 1, 1, 0, 704, 100
36877, V, 1, 1, 1, 1, 0, 704, 100
36878, V, 1, 1, 1, 1, 0, 704, 100
36879, V, 1, 1, 1, 1, 0, 704, 100
36880, V, 1, 1, 1, 1, 0, 704, 100
36881, V, 1, 1, 1, 1, 0, 704, 100
36882, V, 1, 1, 1, 1, 0, 704, 100
36883, V, 1, 1, 1, 1, 0, 704, 100
36884, V, 1, 1, 1, 1, 0, 704, 100
36885, V, 1, 1, 1, 1, 0, 704, 100
36886, V, 1, 1, 1, 1, 0, 704, 100
36887, V, 1, 1, 1, 1, 0, 704, 100
36888, V, 1, 1, 1, 1, 0, 704, 100
36889, V, 1, 1, 1, 1, 0, 704, 100
36890, V, 1, 1, 1, 1, 0, 704, 100
36891, V, 1, 1, 1, 1, 0, 704, 100
36892, V, 1, 1, 1, 1, 0, 704, 100
36893, V, 1, 1, 1, 1, 0, 704, 100
36894, V, 1, 1, 1, 1, 0, 704, 100
36895, V, 1, 1, 1, 1, 0, 704, 100
36896, V, 1, 1, 1, 1, 0, 704, 100
36897, V, 1, 1, 1, 1, 0, 704, 100
36898, V, 1, 1, 1, 1, 0, 704, 100
36899, V, 1, 1, 1, 1, 0, 704, 100
36900, V, 1, 1, 1, 1, 0, 704, 100
36901, V, 1, 1, 1, 1, 0, 704, 100
36902, V, 1, 1, 1, 1, 0, 704, 100
36903, V, 1, 1, 1, 1, 0, 704, 100
36904, V, 1, 1, 1, 1, 0, 704, 100
36905, V, 1, 1, 1, 1, 0, 704, 100
36907, V, 1, 1, 1, 1, 0, 704, 100
36908, V, 1, 1, 1, 1, 0, 704, 100
36909, V, 1, 1, 1, 1, 0, 704, 100
36910, V, 1, 1, 1, 1, 0, 704, 100
36911, V, 1, 1, 1, 1, 0, 704, 100
36912, V, 1, 1, 1, 1, 0, 704, 100
36913, V, 1, 1, 1, 1, 0, 704, 100
36914, V, 1, 1, 1, 1, 0, 704, 100
36915, V, 1, 1, 1, 1, 0, 704, 100
36916, V, 1, 1, 1, 1, 0, 704, 100
36917, V, 1, 1, 1, 1, 0, 704, 100
36918, V, 1, 1, 1, 1, 0, 704, 100
36919, V, 1, 1, 1, 1, 0, 704, 100
36920, V, 1, 1, 1, 1, 0, 704, 100
36921, V, 1, 1, 1, 1, 0, 704, 100
36922, V, 1, 1, 1, 1, 0, 704, 100
36923, V, 1, 1, 1, 1, 0, 704, 100
36924, V, 1, 1, 1, 1, 0, 704, 100
36925, V, 1, 1, 1, 1, 0, 704, 100
36926, V, 1, 1, 1, 1, 0, 704, 100
36927, V, 1, 1, 1, 1, 0, 704, 100
36928, V, 1, 1, 1, 1, 0, 704, 100
36929, V, 1, 1, 1, 1, 0, 704, 100
36930, V, 1, 1, 1, 1, 0, 704, 100
36931, V, 1, 1, 1, 1, 0, 704, 100
36932, V, 1, 1, 1, 1, 0, 704, 100
36933, V, 1, 1, 1, 1, 0, 704, 100
36934, V, 1, 1, 1, 1, 0, 704, 100
36935, V, 1, 1, 1, 1, 0, 704, 100
36936, V, 1, 1, 1, 1, 0, 704, 100
36937, V, 1, 1, 1, 1, 0, 704, 100
36938, V, 1, 1, 1, 1, 0, 704, 100
36939, V, 1, 1, 1, 1, 0, 704, 100
36940, V, 1, 1, 1, 1, 0, 704, 100
36941, V, 1, 1, 1, 1, 0, 704, 100
36942, V, 1, 1, 1, 1, 0, 704, 100
36943, V, 1, 1, 1, 1, 0, 704, 100
36944, V, 1, 1, 1, 1, 0, 704, 100
36945, V, 1, 1, 1, 1, 0, 704, 100
36946, V, 1, 1, 1, 1, 0, 704, 100
36947, V, 1, 1, 1, 1, 0, 704, 100
36948, V, 1, 1, 1, 1, 0, 704, 100
36950, V, 1, 1, 1, 1, 0, 704, 100
36951, V, 1, 1, 1, 1, 0, 704, 100
36952, V, 1, 1, 1, 1, 0, 704, 100
36953, V, 1, 1, 1, 1, 0, 704, 100
36954, V, 1, 1, 1, 1, 0, 704, 100
36955, V, 1, 1, 1, 1, 0, 704, 100
36956, V, 1, 1, 1, 1, 0, 704, 100
36957, V, 1, 1, 1, 1, 0, 704, 100
36958, V, 1, 1, 1, 1, 0, 704, 100
36959, V, 1, 1, 1, 1, 0, 704, 100
36960, V, 1, 1, 1, 1, 0, 704, 100
36961, V, 1, 1, 1, 1, 0, 704, 100
36962, V, 1, 1, 1, 1, 0, 704, 100
36963, V, 1, 1, 1, 1, 0, 704, 100
36964, V, 1, 1, 1, 1, 0, 704, 100
36965, V, 1, 1, 1, 1, 0, 704, 100
36966, V, 1, 1, 1, 1, 0, 704, 100
36967, V, 1, 1, 1, 1, 0, 704, 100
36968, V, 1, 1, 1, 1, 0, 704, 100
36969, V, 1, 1, 1, 1, 0, 704, 100
36970, V, 1, 1, 1, 1, 0, 704, 100
36971, V, 1, 1, 1, 1, 0, 704, 100
36972, V, 1, 1, 1, 1, 0, 704, 100
36973, V, 1, 1, 1, 1, 0, 704, 100
36974, V, 1, 1, 1, 1, 0, 704, 100
36975, V, 1, 1, 1, 1, 0, 704, 100
36976, V, 1, 1, 1, 1, 0, 704, 100
36977, V, 1, 1, 1, 1, 0, 704, 100
36978, V, 1, 1, 1, 1, 0, 704, 100
36979, V, 1, 1, 1, 1, 0, 704, 100
36980, V, 1, 1, 1, 1, 0, 704, 100
36981, V, 1, 1, 1, 1, 0, 704, 100
36982, V, 1, 1, 1, 1, 0, 704, 100
36983, V, 1, 1, 1, 1, 0, 704, 100
36984, V, 1, 1, 1, 1, 0, 704, 100
36985, V, 1, 1, 1, 1, 0, 704, 100
36986, V, 1, 1, 1, 1, 0, 704, 100
36987, V, 1, 1, 1, 1, 0, 704, 100
36988, V, 1, 1, 1, 1, 0, 704, 100
36989, V, 1, 1, 1, 1, 0, 704, 100
36990, V, 1, 1, 1, 1, 0, 704, 100
36992, V, 1, 1, 1, 1, 0, 704, 100
36993, V, 1, 1, 1, 1, 0, 704, 100
36994, V, 1, 1, 1, 1, 0, 704, 100
36995, V, 1, 1, 1, 1, 0, 704, 100
36996, V, 1, 1, 1, 1, 0, 704, 100
36997, V, 1, 1, 1, 1, 0, 704, 100
36998, V, 1, 1, 1, 1, 0, 704, 100
36999, V, 1, 1, 1, 1, 0, 704, 100
37000, V, 1, 1, 1, 1, 0, 704, 100
37001, V, 1, 1, 1, 1, 0, 704, 100
37002, V, 1, 1, 1, 1, 0, 704, 100
37003, V, 1, 1, 1, 1, 0, 704, 100
37004, V, 1, 1, 1, 1, 0, 704, 100
37005, V, 1, 1, 1, 1, 0, 704, 100
37006, V, 1, 1, 1, 1, 0, 704, 100
37007, V, 1, 1, 1, 1, 0, 704, 100
37008, V, 1, 1, 1, 1, 0, 704, 100
37009, V, 1, 1, 1, 1, 0, 704, 100
37010, V, 1, 1, 1, 1, 0, 704, 100
37011, V, 1, 1, 1, 1, 0, 704, 100
37012, V, 1, 1, 1, 1, 0, 704, 100
37013, V, 1, 1, 1, 1, 0, 704, 100
37014, V, 1, 1, 1, 1, 0, 704, 100
37015, V, 1, 1, 1, 1, 0, 704, 100
37016, V, 1, 1, 1, 1, 0, 704, 100
37017, V, 1, 1, 1, 1, 0, 704, 100
37018, V, 1, 1, 1, 1, 0, 704, 100
37019, V, 1, 1, 1, 1, 0, 704, 100
37020, V, 1, 1, 1, 1, 0, 704, 100
37021, V, 1, 1, 1, 1, 0, 704, 100
37022, V, 1, 1, 1, 1, 0, 704, 100
37023, V, 1, 1, 1, 1, 0, 704, 100
37024, V, 1, 1, 1, 1, 0, 704, 100
37025, V, 1, 1, 1, 1, 0, 704, 100
37026, V, 1, 1, 1, 1, 0, 704, 100
37027, V, 1, 1, 1, 1, 0, 704, 100
37028, V, 1, 1, 1, 1, 0, 704, 100
37029, V, 1, 1, 1, 1, 0, 704, 100
37030, V, 1, 1, 1, 1, 0, 704, 100
37031, V, 1, 1, 1, 1, 0, 704, 100
37032, V, 1, 1, 1, 1, 0, 704, 100
37033, V, 1, 1, 1, 1, 0, 704, 100
37035, V, 1, 1, 1, 1, 0, 704, 100
37036, V, 1, 1, 1, 1, 0, 704, 100
37037, V, 1, 1, 1, 1, 0, 704, 100
37038, V, 1, 1, 1, 1, 0, 704, 100
37039, V, 1, 1, 1, 1, 0, 704, 100
37040, V, 1, 1, 1, 1, 0, 704, 100
37041, V, 1, 1, 1, 1, 0, 704, 100
37042, V, 1, 1, 1, 1, 0, 704, 100
37043, V, 1, 1, 1, 1, 0, 704, 100
37044, V, 1, 1, 1, 1, 0, 704, 100
37045, V, 1, 1, 1, 1, 0, 704, 100
37046, V, 1, 1, 1, 1, 0, 704, 100
37047, V, 1, 1, 1, 1, 0, 704, 100
37048, V, 1, 1, 1, 1, 0, 704, 100
37049, V, 1, 1, 1, 1, 0, 704, 100
37050, V, 1, 1, 1, 1, 0, 704, 100
37051, V, 1, 1, 1, 1, 0, 704, 100
37052, V, 1, 1, 1, 1, 0, 704, 100
37053, V, 1, 1, 1, 1, 0, 704, 100
37054, V, 1, 1, 1, 1, 0, 704, 100
37055, V, 1, 1, 1, 1, 0, 704, 100
37056, V, 1, 1, 1, 1, 0, 704, 100
37057, V, 1, 1, 1, 1, 0, 704, 100
37058, V, 1, 1, 1, 1, 0, 704, 100
37059, V, 1, 1, 1, 1, 0, 704, 100
37060, V, 1, 1, 1, 1, 0, 704, 100
37061, V, 1, 1, 1, 1, 0, 704, 100
37062, V, 1, 1, 1, 1, 0, 704, 100
37063, V, 1, 1, 1, 1, 0, 704, 100
37064, V, 1, 1, 1, 1, 0, 704, 100
37065, V, 1, 1, 1, 1, 0, 704, 100
37066, V, 1, 1, 1, 1, 0, 704, 100
37067, V, 1, 1, 1, 1, 0, 704, 100
37068, V, 1, 1, 1, 1, 0, 704, 100
37069, V, 1, 1, 1, 1, 0, 704, 100
37070, V, 1, 1, 1, 1, 0, 704, 100
37071, V, 1, 1, 1, 1, 0, 704, 100
37072, V, 1, 1, 1, 1, 0, 704, 100
37073, V, 1, 1, 1, 1, 0, 704, 100
37074, V, 1, 1, 1, 1, 0, 704, 100
37075, V, 1, 1, 1, 1, 0, 704, 100
37076, V, 1, 1, 1, 1, 0, 704, 100
37078, V, 1, 1, 1, 1, 0, 704, 100
37079, V, 1, 1, 1, 1, 0, 704, 100
37080, V, 1, 1, 1, 1, 0, 704, 100
37081, V, 1, 1, 1, 1, 0, 704, 100
37082, V, 1, 1, 1, 1, 0, 704, 100
37083, V, 1, 1, 1, 1, 0, 704, 100
37084, V, 1, 1, 1, 1, 0, 704, 100
37085, V, 1, 1, 1, 1, 0, 704, 100
37086, V, 1, 1, 1, 1, 0, 704, 100
37087, V, 1, 1, 1, 1, 0, 704, 100
37088, V, 1, 1, 1, 1, 0, 704, 100
37089, V, 1, 1, 1, 1, 0, 704, 100
37090, V, 1, 1, 1, 1, 0, 704, 100
37091, V, 1, 1, 1, 1, 0, 704, 100
37092, V, 1, 1, 1, 1, 0, 704, 100
37093, V, 1, 1, 1, 1, 0, 704, 100
37094, V, 1, 1, 1, 1, 0, 704, 100
37095, V, 1, 1, 1, 1, 0, 704, 100
37096, V, 1, 1, 1, 1, 0, 704, 100
37097, V, 1, 1, 1, 1, 0, 704, 100
37098, V, 1, 1, 1, 1, 0, 704, 100
37099, V, 1, 1, 1, 1, 0, 704, 100
37100, V, 1, 1, 1, 1, 0, 704, 100
37101, V, 1, 1, 1, 1, 0, 704, 100
37102, V, 1, 1, 1, 1, 0, 704, 100
37103, V, 1, 1, 1, 1, 0, 704, 100
37104, V, 1, 1, 1, 1, 0, 704, 100
37105, V, 1, 1, 1, 1, 0, 704, 100
37106, V, 1, 1, 1, 1, 0, 704, 100
37107, V, 1, 1, 1, 1, 0, 704, 100
37108, V, 1, 1, 1, 1, 0, 704, 100
37109, V, 1, 1, 1, 1, 0, 704, 100
37110, V, 1, 1, 1, 1, 0, 704, 100
37111, V, 1, 1, 1, 1, 0, 704, 100
37112, V, 1, 1, 1, 1, 0, 704, 100
37113, V, 1, 1, 1, 1, 0, 704, 100
37114, V, 1, 1, 1, 1, 0, 704, 100
37115, V, 1, 1, 1, 1, 0, 704, 100
37116, V, 1, 1, 1, 1, 0, 704, 100
37117, V, 1, 1, 1, 1, 0, 704, 100
37118, V, 1, 1, 1, 1, 0, 704, 100
37120, V, 1, 1, 1, 1, 0, 704, 100
37121, V, 1, 1, 1, 1, 0, 704, 100
37122, V, 1, 1, 1, 1, 0, 704, 100
37123, V, 1, 1, 1, 1, 0, 704, 100
37124, V, 1, 1, 1, 1, 0, 704, 100
37125, V, 1, 1, 1, 1, 0, 704, 100
37126, V, 1, 1, 1, 1, 0, 704, 100
37127, V, 1, 1, 1, 1, 0, 704, 100
37128, V, 1, 1, 1, 1, 0, 704, 100
37129, V, 1, 1, 1, 1, 0, 704, 100
37130, V, 1, 1, 1, 1, 0, 704, 100
37131, V, 1, 1, 1, 1, 0, 704, 100
37132, V, 1, 1, 1, 1, 0, 704, 100
37133, V, 1, 1, 1, 1, 0, 704, 100
37134, V, 1, 1, 1, 1, 0, 704, 100
37135, V, 1, 1, 1, 1, 0, 704, 100
37136, V, 1, 1, 1, 1, 0, 704, 100
37137, V, 1, 1, 1, 1, 0, 704, 100
37138, V, 1, 1, 1, 1, 0, 704, 100
37139, V, 1, 1, 1, 1, 0, 704, 100
37140, V, 1, 1, 1, 1, 0, 704, 100
37141, V, 1, 1, 1, 1, 0, 704, 100
37142, V, 1, 1, 1, 1, 0, 704, 100
37143, V, 1, 1, 1, 1, 0, 704, 100
37144, V, 1, 1, 1, 1, 0, 704, 100
37145, V, 1, 1, 1, 1, 0, 704, 100
37146, V, 1, 1, 1, 1, 0, 704, 100
37147, V, 1, 1, 1, 1, 0, 704, 100
37148, V, 1, 1, 1, 1, 0, 704, 100
37149, V, 1, 1, 1, 1, 0, 704, 100
37150, V, 1, 1, 1, 1, 0, 704, 100
37151, V, 1, 1, 1, 1, 0, 704, 100
37152, V, 1, 1, 1, 1, 0, 704, 100
37153, V, 1, 1, 1, 1, 0, 704, 100
37154, V, 1, 1, 1, 1, 0, 704, 100
37155, V, 1, 1, 1, 1, 0, 704, 100
37156, V, 1, 1, 1, 1, 0, 704, 100
37157, V, 1, 1, 1, 1, 0, 704, 100
37158, V, 1, 1, 1, 1, 0, 704, 100
37159, V, 1, 1, 1, 1, 0, 704, 100
37160, V, 1, 1, 1, 1, 0, 704, 100
37161, V, 1, 1, 1, 1, 0, 704, 100
37163, V, 1, 1, 1, 1, 0, 704, 100
37164, V, 1, 1, 1, 1, 0, 704, 100
37165, V, 1, 1, 1, 1, 0, 704, 100
37166, V, 1, 1, 1, 1, 0, 704, 100
37167, V, 1, 1, 1, 1, 0, 704, 100
37168, V, 1, 1, 1, 1, 0, 704, 100
37169, V, 1, 1, 1, 1, 0, 704, 100
37170, V, 1, 1, 1, 1, 0, 704, 100
37171, V, 1, 1, 1, 1, 0, 704, 100
37172, V, 1, 1, 1, 1, 0, 704, 100
37173, V, 1, 1, 1, 1, 0, 704, 100
37174, V, 1, 1, 1, 1, 0, 704, 100
37175, V, 1, 1, 1, 1, 0, 704, 100
37176, V, 1, 1, 1, 1, 0, 704, 100
37177, V, 1, 1, 1, 1, 0, 704, 100
37178, V, 1, 1, 1, 1, 0, 704, 100
37179, V, 1, 1, 1, 1, 0, 704, 100
37180, V, 1, 1, 1, 1, 0, 704, 100
37181, V, 1, 1, 1, 1, 0, 704, 100
37182, V, 1, 1, 1, 1, 0, 704, 100
37183, V, 1, 1, 1, 1, 0, 704, 100
37184, V, 1, 1, 1, 1, 0, 704, 100
37185, V, 1, 1, 1, 1, 0, 704, 100
37186, V, 1, 1, 1, 1, 0, 704, 100
37187, V, 1, 1, 1, 1, 0, 704, 100
37188, V, 1, 1, 1, 1, 0, 704, 100
37189, V, 1, 1, 1, 1, 0, 704, 100
37190, V, 1, 1, 1, 1, 0, 704, 100
37191, V, 1, 1, 1, 1, 0, 704, 100
37192, V, 1, 1, 1, 1, 0, 704, 100
37193, V, 1, 1, 1, 1, 0, 704, 100
37194, V, 1, 1, 1, 1, 0, 704, 100
37195, V, 1, 1, 1, 1, 0, 704, 100
37196, V, 1, 1, 1, 1, 0, 704, 100
37197, V, 1, 1, 1, 1, 0, 704, 100
37198, V, 1, 1, 1, 1, 0, 704, 100
37199, V, 1, 1, 1, 1, 0, 704, 100
37200, V, 1, 1, 1, 1, 0, 704, 100
37201, V, 1, 1, 1, 1, 0, 704, 100
37202, V, 1, 1, 1, 1, 0, 704, 100
37203, V, 1, 1, 1, 1, 0, 704, 100
37204, V, 1, 1, 1, 1, 0, 704, 100
37206, V, 1, 1, 1, 1, 0, 704, 100
37207, V, 1, 1, 1, 1, 0, 704, 100
37208, V, 1, 1, 1, 1, 0, 704, 100
37209, V, 1, 1, 1, 1, 0, 704, 100
37210, V, 1, 1, 1, 1, 0, 704, 100
37211, V, 1, 1, 1, 1, 0, 704, 100
37212, V, 1, 1, 1, 1, 0, 704, 100
37213, V, 1, 1, 1, 1, 0, 704, 100
37214, V, 1, 1, 1, 1, 0, 704, 100
37215, V, 1, 1, 1, 1, 0, 704, 100
37216, V, 1, 1, 1, 1, 0, 704, 100
37217, V, 1, 1, 1, 1, 0, 704, 100
37218, V, 1, 1, 1, 1, 0, 704, 100
37219, V, 1, 1, 1, 1, 0, 704, 100
37220, V, 1, 1, 1, 1, 0, 704, 100
37221, V, 1, 1, 1, 1, 0, 704, 100
37222, V, 1, 1, 1, 1, 0, 704, 100
37223, V, 1, 1, 1, 1, 0, 704, 100
37224, V, 1, 1, 1, 1, 0, 704, 100
37225, V, 1, 1, 1, 1, 0, 704, 100
37226, V, 1, 1, 1, 1, 0, 704, 100
37227, V, 1, 1, 1, 1, 0, 704, 100
37228, V, 1, 1, 1, 1, 0, 704, 100
37229, V, 1, 1, 1, 1, 0, 704, 100
37230, V, 1, 1, 1, 1, 0, 704, 100
37231, V, 1, 1, 1, 1, 0, 704, 100
37232, V, 1, 1, 1, 1, 0, 704, 100
37233, V, 1, 1, 1, 1, 0, 704, 100
37234, V, 1, 1, 1, 1, 0, 704, 100
37235, V, 1, 1, 1, 1, 0, 704, 100
37236, V, 1, 1, 1, 1, 0, 704, 100
37237, V, 1, 1, 1, 1, 0, 704, 100
37238, V, 1, 1, 1, 1, 0, 704, 100
37239, V, 1, 1, 1, 1, 0, 704, 100
37240, V, 1, 1, 1, 1, 0, 704, 100
37241, V, 1, 1, 1, 1, 0, 704, 100
37242, V, 1, 1, 1, 1, 0, 704, 100
37243, V, 1, 1, 1, 1, 0, 704, 100
37244, V, 1, 1, 1, 1, 0, 704, 100
37245, V, 1, 1, 1, 1, 0, 704, 100
37246, V, 1, 1, 1, 1, 0, 704, 100
37248, V, 1, 1, 1, 1, 0, 704, 100
37249, V, 1, 1, 1, 1, 0, 704, 100
37250, V, 1, 1, 1, 1, 0, 704, 100
37251, V, 1, 1, 1, 1, 0, 704, 100
37252, V, 1, 1, 1, 1, 0, 704, 100
37253, V, 1, 1, 1, 1, 0, 704, 100
37254, V, 1, 1, 1, 1, 0, 704, 100
37255, V, 1, 1, 1, 1, 0, 704, 100
37256, V, 1, 1, 1, 1, 0, 704, 100
37257, V, 1, 1, 1, 1, 0, 704, 100
37258, V, 1, 1, 1, 1, 0, 704, 100
37259, V, 1, 1, 1, 1, 0, 704, 100
37260, V, 1, 1, 1, 1, 0, 704, 100
37261, V, 1, 1, 1, 1, 0, 704, 100
37262, V, 1, 1, 1, 1, 0, 704, 100
37263, V, 1, 1, 1, 1, 0, 704, 100
37264, V, 1, 1, 1, 1, 0, 704, 100
37265, V, 1, 1, 1, 1, 0, 704, 100
37266, V, 1, 1, 1, 1, 0, 704, 100
37267, V, 1, 1, 1, 1, 0, 704, 100
37268, V, 1, 1, 1, 1, 0, 704, 100
37269, V, 1, 1, 1, 1, 0, 704, 100
37270, V, 1, 1, 1, 1, 0, 704, 100
37271, V, 1, 1, 1, 1, 0, 704, 100
37272, V, 1, 1, 1, 1, 0, 704, 100
37273, V, 1, 1, 1, 1, 0, 704, 100
37274, V, 1, 1, 1, 1, 0, 704, 100
37275, V, 1, 1, 1, 1, 0, 704, 100
37276, V, 1, 1, 1, 1, 0, 704, 100
37277, V, 1, 1, 1, 1, 0, 704, 100
37278, V, 1, 1, 1, 1, 0, 704, 100
37279, V, 1, 1, 1, 1, 0, 704, 100
37280, V, 1, 1, 1, 1, 0, 704, 100
37281, V, 1, 1, 1, 1, 0, 704, 100
37282, V, 1, 1, 1, 1, 0, 704, 100
37283, V, 1, 1, 1, 1, 0, 704, 100
37284, V, 1, 1, 1, 1, 0, 704, 100
37285, V, 1, 1, 1, 1, 0, 704, 100
37286, V, 1, 1, 1, 1, 0, 704, 100
37287, V, 1, 1, 1, 1, 0, 704, 100
37288, V, 1, 1, 1, 1, 0, 704, 100
37289, V, 1, 1, 1, 1, 0, 704, 100
37291, V, 1, 1, 1, 1, 0, 704, 100
37292, V, 1, 1, 1, 1, 0, 704, 100
37293, V, 1, 1, 1, 1, 0, 704, 100
37294, V, 1, 1, 1, 1, 0, 704, 100
37295, V, 1, 1, 1, 1, 0, 704, 100
37296, V, 1, 1, 1, 1, 0, 704, 100
37297, V, 1, 1, 1, 1, 0, 704, 100
37298, V, 1, 1, 1, 1, 0, 704, 100
37299, V, 1, 1, 1, 1, 0, 704, 100
37300, V, 1, 1, 1, 1, 0, 704, 100
37301, V, 1, 1, 1, 1, 0, 704, 100
37302, V, 1, 1, 1, 1, 0, 704, 100
37303, V, 1, 1, 1, 1, 0, 704, 100
37304, V, 1, 1, 1, 1, 0, 704, 100
37305, V, 1, 1, 1, 1, 0, 704, 100
37306, V, 1, 1, 1, 1, 0, 704, 100
37307, V, 1, 1, 1, 1, 0, 704, 100
37308, V, 1, 1, 1, 1, 0, 704, 100
37309, V, 1, 1, 1, 1, 0, 704, 100
37310, V, 1, 1, 1, 1, 0, 704, 100
37311, V, 1, 1, 1, 1, 0, 704, 100
37312, V, 1, 1, 1, 1, 0, 704, 100
37313, V, 1, 1, 1, 1, 0, 704, 100
37314, V, 1, 1, 1, 1, 0, 704, 100
37315, V, 1, 1, 1, 1, 0, 704, 100
37316, V, 1, 1, 1, 1, 0, 704, 100
37317, V, 1, 1, 1, 1, 0, 704, 100
37318, V, 1, 1, 1, 1, 0, 704, 100
37319, V, 1, 1, 1, 1, 0, 704, 100
37320, V, 1, 1, 1, 1, 0, 704, 100
37321, V, 1, 1, 1, 1, 0, 704, 100
37322, V, 1, 1, 1, 1, 0, 704, 100
37323, V, 1, 1, 1, 1, 0, 704, 100
37324, V, 1, 1, 1, 1, 0, 704, 100
37325, V, 1, 1, 1, 1, 0, 704, 100
37326, V, 1, 1, 1, 1, 0, 704, 100
37327, V, 1, 1, 1, 1, 0, 704, 100
37328, V, 1, 1, 1, 1, 0, 704, 100
37329, V, 1, 1, 1, 1, 0, 704, 100
37330, V, 1, 1, 1, 1, 0, 704, 100
37331, V, 1, 1, 1, 1, 0, 704, 100
37332, V, 1, 1, 1, 1, 0, 704, 100
37334, V, 1, 1, 1, 1, 0, 704, 100
37335, V, 1, 1, 1, 1, 0, 704, 100
37336, V, 1, 1, 1, 1, 0, 704, 100
37337, V, 1, 1, 1, 1, 0, 704, 100
37338, V, 1, 1, 1, 1, 0, 704, 100
37339, V, 1, 1, 1, 1, 0, 704, 100
37340, V, 1, 1, 1, 1, 0, 704, 100
37341, V, 1, 1, 1, 1, 0, 704, 100
37342, V, 1, 1, 1, 1, 0, 704, 100
37343, V, 1, 1, 1, 1, 0, 704, 100
37344, V, 1, 1, 1, 1, 0, 704, 100
37345, V, 1, 1, 1, 1, 0, 704, 100
37346, V, 1, 1, 1, 1, 0, 704, 100
37347, V, 1, 1, 1, 1, 0, 704, 100
37348, V, 1, 1, 1, 1, 0, 704, 100
37349, V, 1, 1, 1, 1, 0, 704, 100
37350, V, 1, 1, 1, 1, 0, 704, 100
37351, V, 1, 1, 1, 1, 0, 704, 100
37352, V, 1, 1, 1, 1, 0, 704, 100
37353, V, 1, 1, 1, 1, 0, 704, 100
37354, V, 1, 1, 1, 1, 0, 704, 100
37355, V, 1, 1, 1, 1, 0, 704, 100
37356, V, 1, 1, 1, 1, 0, 704, 100
37357, V, 1, 1, 1, 1, 0, 704, 100
37358, V, 1, 1, 1, 1, 0, 704, 100
37359, V, 1, 1, 1, 1, 0, 704, 100
37360, V, 1, 1, 1, 1, 0, 704, 100
37361, V, 1, 1, 1, 1, 0, 704, 100
37362, V, 1, 1, 1, 1, 0, 704, 100
37363, V, 1, 1, 1, 1, 0, 704, 100
37364, V, 1, 1, 1, 1, 0, 704, 100
37365, V, 1, 1, 1, 1, 0, 704, 100
37366, V, 1, 1, 1, 1, 0, 704, 100
37367, V, 1, 1, 1, 1, 0, 704, 100
37368, V, 1, 1, 1, 1, 0, 704, 100
37369, V, 1, 1, 1, 1, 0, 704, 100
37370, V, 1, 1, 1, 1, 0, 704, 100
37371, V, 1, 1, 1, 1, 0, 704, 100
37372, V, 1, 1, 1, 1, 0, 704, 100
37373, V, 1, 1, 1, 1, 0, 704, 100
37374, V, 1, 1, 1, 1, 0, 704, 100
37376, V, 1, 1, 1, 1, 0, 704, 100
37377, V, 1, 1, 1, 1, 0, 704, 100
37378, V, 1, 1, 1, 1, 0, 704, 100
37379, V, 1, 1, 1, 1, 0, 704, 100
37380, V, 1, 1, 1, 1, 0, 704, 100
37381, V, 1, 1, 1, 1, 0, 704, 100
37382, V, 1, 1, 1, 1, 0, 704, 100
37383, V, 1, 1, 1, 1, 0, 704, 100
37384, V, 1, 1, 1, 1, 0, 704, 100
37385, V, 1, 1, 1, 1, 0, 704, 100
37386, V, 1, 1, 1, 1, 0, 704, 100
37387, V, 1, 1, 1, 1, 0, 704, 100
37388, V, 1, 1, 1, 1, 0, 704, 100
37389, V, 1, 1, 1, 1, 0, 704, 100
37390, V, 1, 1, 1, 1, 0, 704, 100
37391, V, 1, 1, 1, 1, 0, 704, 100
37392, V, 1, 1, 1, 1, 0, 704, 100
37393, V, 1, 1, 1, 1, 0, 704, 100
37394, V, 1, 1, 1, 1, 0, 704, 100
37395, V, 1, 1, 1, 1, 0, 704, 100
37396, V, 1, 1, 1, 1, 0, 704, 100
37397, V, 1, 1, 1, 1, 0, 704, 100
37398, V, 1, 1, 1, 1, 0, 704, 100
37399, V, 1, 1, 1, 1, 0, 704, 100
37400, V, 1, 1, 1, 1, 0, 704, 100
37401, V, 1, 1, 1, 1, 0, 704, 100
37402, V, 1, 1, 1, 1, 0, 704, 100
37403, V, 1, 1, 1, 1, 0, 704, 100
37404, V, 1, 1, 1, 1, 0, 704, 100
37405, V, 1, 1, 1, 1, 0, 704, 100
37406, V, 1, 1, 1, 1, 0, 704, 100
37407, V, 1, 1, 1, 1, 0, 704, 100
37408, V, 1, 1, 1, 1, 0, 704, 100
37409, V, 1, 1, 1, 1, 0, 704, 100
37410, V, 1, 1, 1, 1, 0, 704, 100
37411, V, 1, 1, 1, 1, 0, 704, 100
37412, V, 1, 1, 1, 1, 0, 704, 100
37413, V, 1, 1, 1, 1, 0, 704, 100
37414, V, 1, 1, 1, 1, 0, 704, 100
37415, V, 1, 1, 1, 1, 0, 704, 100
37416, V, 1, 1, 1, 1, 0, 704, 100
37417, V, 1, 1, 1, 1, 0, 704, 99
37419, V, 1, 1, 1, 1, 0, 704, 100
37420, V, 1, 1, 1, 1, 0, 704, 100
37421, V, 1, 1, 1, 1, 0, 704, 100
37422, V, 1, 1, 1, 1, 0, 704, 100
37423, V, 1, 1, 1, 1, 0, 704, 100
37424, V, 1, 1, 1, 1, 0, 704, 99
37425, V, 1, 1, 1, 1, 0, 704, 100
37426, V, 1, 1, 1, 1, 0, 704, 99
37427, V, 1, 1, 1, 1, 0, 704, 99
37428, V, 1, 1, 1, 1, 0, 704, 100
37429, V, 1, 1, 1, 1, 0, 704, 99
37430, V, 1, 1, 1, 1, 0, 704, 100
37431, V, 1, 1, 1, 1, 0, 704, 99
37432, V, 1, 1, 1, 1, 0, 704, 100
37433, V, 1, 1, 1, 1, 0, 704, 100
37434, V, 1, 1, 1, 1, 0, 704, 100
37435, V, 1, 1, 1, 1, 0, 704, 100
37436, V, 1, 1, 1, 1, 0, 704, 100
37437, V, 1, 1, 1, 1, 0, 704, 100
37438, V, 1, 1, 1, 1, 0, 704, 100
37439, V, 1, 1, 1, 1, 0, 704, 100
37440, V, 1, 1, 1, 1, 0, 704, 100
37441, V, 1, 1, 1, 1, 0, 704, 100
37442, V, 1, 1, 1, 1, 0, 704, 100
37443, V, 1, 1, 1, 1, 0, 704, 100
37444, V, 1, 1, 1, 1, 0, 704, 100
37445, V, 1, 1, 1, 1, 0, 704, 100
37446, V, 1, 1, 1, 1, 0, 704, 100
37447, V, 1, 1, 1, 1, 0, 704, 100
37448, V, 1, 1, 1, 1, 0, 704, 100
37449, V, 1, 1, 1, 1, 0, 704, 100
37450, V, 1, 1, 1, 1, 0, 704, 100
37451, V, 1, 1, 1, 1, 0, 704, 100
37452, V, 1, 1, 1, 1, 0, 704, 100
37453, V, 1, 1, 1, 1, 0, 704, 100
37454, V, 1, 1, 1, 1, 0, 704, 100
37455, V, 1, 1, 1, 1, 0, 704, 100
37456, V, 1, 1, 1, 1, 0, 704, 100
37457, V, 1, 1, 1, 1, 0, 704, 100
37458, V, 1, 1, 1, 1, 0, 704, 100
37459, V, 1, 1, 1, 1, 0, 704, 100
37460, V, 1, 1, 1, 1, 0, 704, 100
37462, V, 1, 1, 1, 1, 0, 704, 100
37463, V, 1, 1, 1, 1, 0, 704, 100
37464, V, 1, 1, 1, 1, 0, 704, 100
37465, V, 1, 1, 1, 1, 0, 704, 100
37466, V, 1, 1, 1, 1, 0, 704, 100
37467, V, 1, 1, 1, 1, 0, 704, 100
37468, V, 1, 1, 1, 1, 0, 704, 100
37469, V, 1, 1, 1, 1, 0, 704, 100
37470, V, 1, 1, 1, 1, 0, 704, 100
37471, V, 1, 1, 1, 1, 0, 704, 100
37472, V, 1, 1, 1, 1, 0, 704, 100
37473, V, 1, 1, 1, 1, 0, 704, 100
37474, V, 1, 1, 1, 1, 0, 704, 100
37475, V, 1, 1, 1, 1, 0, 704, 100
37476, V, 1, 1, 1, 1, 0, 704, 100
37477, V, 1, 1, 1, 1, 0, 704, 100
37478, V, 1, 1, 1, 1, 0, 704, 100
37479, V, 1, 1, 1, 1, 0, 704, 100
37480, V, 1, 1, 1, 1, 0, 704, 100
37481, V, 1, 1, 1, 1, 0, 704, 100
37482, V, 1, 1, 1, 1, 0, 704, 100
37483, V, 1, 1, 1, 1, 0, 704, 100
37484, V, 1, 1, 1, 1, 0, 704, 100
37485, V, 1, 1, 1, 1, 0, 704, 100
37486, V, 1, 1, 1, 1, 0, 704, 100
37487, V, 1, 1, 1, 1, 0, 704, 100
37488, V, 1, 1, 1, 1, 0, 704, 100
37489, V, 1, 1, 1, 1, 0, 704, 100
37490, V, 1, 1, 1, 1, 0, 704, 100
37491, V, 1, 1, 1, 1, 0, 704, 100
37492, V, 1, 1, 1, 1, 0, 704, 100
37493, V, 1, 1, 1, 1, 0, 704, 100
37494, V, 1, 1, 1, 1, 0, 704, 100
37495, V, 1, 1, 1, 1, 0, 704, 99
37496, V, 1, 1, 1, 1, 0, 704, 100
37497, V, 1, 1, 1, 1, 0, 704, 100
37498, V, 1, 1, 1, 1, 0, 704, 100
37499, V, 1, 1, 1, 1, 0, 704, 100
37500, V, 1, 1, 1, 1, 0, 704, 100
37501, V, 1, 1, 1, 1, 0, 704, 100
37502, V, 1, 1, 1, 1, 0, 704, 100
37504, V, 1, 1, 1, 1, 0, 704, 100
37505, V, 1, 1, 1, 1, 0, 704, 100
37506, V, 1, 1, 1, 1, 0, 704, 100
37507, V, 1, 1, 1, 1, 0, 704, 100
37508, V, 1, 1, 1, 1, 0, 704, 100
37509, V, 1, 1, 1, 1, 0, 704, 100
37510, V, 1, 1, 1, 1, 0, 704, 100
37511, V, 1, 1, 1, 1, 0, 704, 100
37512, V, 1, 1, 1, 1, 0, 704, 100
37513, V, 1, 1, 1, 1, 0, 704, 100
37514, V, 1, 1, 1, 1, 0, 704, 100
37515, V, 1, 1, 1, 1, 0, 704, 100
37516, V, 1, 1, 1, 1, 0, 704, 100
37517, V, 1, 1, 1, 1, 0, 704, 100
37518, V, 1, 1, 1, 1, 0, 704, 100
37519, V, 1, 1, 1, 1, 0, 704, 100
37520, V, 1, 1, 1, 1, 0, 704, 100
37521, V, 1, 1, 1, 1, 0, 704, 100
37522, V, 1, 1, 1, 1, 0, 704, 100
37523, V, 1, 1, 1, 1, 0, 704, 99
37524, V, 1, 1, 1, 1, 0, 704, 100
37525, V, 1, 1, 1, 1, 0, 704, 100
37526, V, 1, 1, 1, 1, 0, 704, 100
37527, V, 1, 1, 1, 1, 0, 704, 100
37528, V, 1, 1, 1, 1, 0, 704, 100
37529, V, 1, 1, 1, 1, 0, 704, 100
37530, V, 1, 1, 1, 1, 0, 704, 100
37531, V, 1, 1, 1, 1, 0, 704, 100
37532, V, 1, 1, 1, 1, 0, 704, 100
37533, V, 1, 1, 1, 1, 0, 704, 100
37534, V, 1, 1, 1, 1, 0, 704, 100
37535, V, 1, 1, 1, 1, 0, 704, 100
37536, V, 1, 1, 1, 1, 0, 704, 100
37537, V, 1, 1, 1, 1, 0, 704, 100
37538, V, 1, 1, 1, 1, 0, 704, 100
37539, V, 1, 1, 1, 1, 0, 704, 100
37540, V, 1, 1, 1, 1, 0, 704, 100
37541, V, 1, 1, 1, 1, 0, 704, 100
37542, V, 1, 1, 1, 1, 0, 704, 100
37543, V, 1, 1, 1, 1, 0, 704, 100
37544, V, 1, 1, 1, 1, 0, 704, 100
37545, V, 1, 1, 1, 1, 0, 704, 100
37547, V, 1, 1, 1, 1, 0, 704, 100
37548, V, 1, 1, 1, 1, 0, 704, 100
37549, V, 1, 1, 1, 1, 0, 704, 100
37550, V, 1, 1, 1, 1, 0, 704, 100
37551, V, 1, 1, 1, 1, 0, 704, 100
37552, V, 1, 1, 1, 1, 0, 704, 100
37553, V, 1, 1, 1, 1, 0, 704, 100
37554, V, 1, 1, 1, 1, 0, 704, 100
37555, V, 1, 1, 1, 1, 0, 704, 100
37556, V, 1, 1, 1, 1, 0, 704, 100
37557, V, 1, 1, 1, 1, 0, 704, 100
37558, V, 1, 1, 1, 1, 0, 704, 99
37559, V, 1, 1, 1, 1, 0, 704, 100
37560, V, 1, 1, 1, 1, 0, 704, 100
37561, V, 1, 1, 1, 1, 0, 704, 99
37562, V, 1, 1, 1, 1, 0, 704, 100
37563, V, 1, 1, 1, 1, 0, 704, 99
37564, V, 1, 1, 1, 1, 0, 704, 100
37565, V, 1, 1, 1, 1, 0, 704, 99
37566, V, 1, 1, 1, 1, 0, 704, 100
37567, V, 1, 1, 1, 1, 0, 704, 100
37568, V, 1, 1, 1, 1, 0, 704, 100
37569, V, 1, 1, 1, 1, 0, 704, 100
37570, V, 1, 1, 1, 1, 0, 704, 100
37571, V, 1, 1, 1, 1, 0, 704, 100
37572, V, 1, 1, 1, 1, 0, 704, 99
37573, V, 1, 1, 1, 1, 0, 704, 100
37574, V, 1, 1, 1, 1, 0, 704, 100
37575, V, 1, 1, 1, 1, 0, 704, 100
37576, V, 1, 1, 1, 1, 0, 704, 100
37577, V, 1, 1, 1, 1, 0, 704, 100
37578, V, 1, 1, 1, 1, 0, 704, 100
37579, V, 1, 1, 1, 1, 0, 704, 100
37580, V, 1, 1, 1, 1, 0, 704, 100
37581, V, 1, 1, 1, 1, 0, 704, 100
37582, V, 1, 1, 1, 1, 0, 704, 100
37583, V, 1, 1, 1, 1, 0, 704, 100
37584, V, 1, 1, 1, 1, 0, 704, 100
37585, V, 1, 1, 1, 1, 0, 704, 100
37586, V, 1, 1, 1, 1, 0, 704, 100
37587, V, 1, 1, 1, 1, 0, 704, 100
37588, V, 1, 1, 1, 1, 0, 704, 100
37590, V, 1, 1, 1, 1, 0, 704, 100
37591, V, 1, 1, 1, 1, 0, 704, 100
37592, V, 1, 1, 1, 1, 0, 704, 100
37593, V, 1, 1, 1, 1, 0, 704, 100
37594, V, 1, 1, 1, 1, 0, 704, 100
37595, V, 1, 1, 1, 1, 0, 704, 100
37596, V, 1, 1, 1, 1, 0, 704, 100
37597, V, 1, 1, 1, 1, 0, 704, 100
37598, V, 1, 1, 1, 1, 0, 704, 100
37599, V, 1, 1, 1, 1, 0, 704, 100
37600, V, 1, 1, 1, 1, 0, 704, 100
37601, V, 1, 1, 1, 1, 0, 704, 100
37602, V, 1, 1, 1, 1, 0, 704, 100
37603, V, 1, 1, 1, 1, 0, 704, 100
37604, V, 1, 1, 1, 1, 0, 704, 100
37605, V, 1, 1, 1, 1, 0, 704, 100
37606, V, 1, 1, 1, 1, 0, 704, 100
37607, V, 1, 1, 1, 1, 0, 704, 100
37608, V, 1, 1, 1, 1, 0, 704, 100
37609, V, 1, 1, 1, 1, 0, 704, 100
37610, V, 1, 1, 1, 1, 0, 704, 100
37611, V, 1, 1, 1, 1, 0, 704, 100
37612, V, 1, 1, 1, 1, 0, 704, 100
37613, V, 1, 1, 1, 1, 0, 704, 100
37614, V, 1, 1, 1, 1, 0, 704, 100
37615, V, 1, 1, 1, 1, 0, 704, 100
37616, V, 1, 1, 1, 1, 0, 704, 100
37617, V, 1, 1, 1, 1, 0, 704, 100
37618, V, 1, 1, 1, 1, 0, 704, 100
37619, V, 1, 1, 1, 1, 0, 704, 100
37620, V, 1, 1, 1, 1, 0, 704, 100
37621, V, 1, 1, 1, 1, 0, 704, 100
37622, V, 1, 1, 1, 1, 0, 704, 100
37623, V, 1, 1, 1, 1, 0, 704, 100
37624, V, 1, 1, 1, 1, 0, 704, 100
37625, V, 1, 1, 1, 1, 0, 704, 100
37626, V, 1, 1, 1, 1, 0, 704, 100
37627, V, 1, 1, 1, 1, 0, 704, 100
37628, V, 1, 1, 1, 1, 0, 704, 100
37629, V, 1, 1, 1, 1, 0, 704, 100
37630, V, 1, 1, 1, 1, 0, 704, 100
37632, V, 1, 1, 1, 1, 0, 704, 100
37633, V, 1, 1, 1, 1, 0, 704, 100
37634, V, 1, 1, 1, 1, 0, 704, 100
37635, V, 1, 1, 1, 1, 0, 704, 100
37636, V, 1, 1, 1, 1, 0, 704, 100
37637, V, 1, 1, 1, 1, 0, 704, 100
37638, V, 1, 1, 1, 1, 0, 704, 100
37639, V, 1, 1, 1, 1, 0, 704, 100
37640, V, 1, 1, 1, 1, 0, 704, 100
37641, V, 1, 1, 1, 1, 0, 704, 100
37642, V, 1, 1, 1, 1, 0, 704, 100
37643, V, 1, 1, 1, 1, 0, 704, 100
37644, V, 1, 1, 1, 1, 0, 704, 100
37645, V, 1, 1, 1, 1, 0, 704, 100
37646, V, 1, 1, 1, 1, 0, 704, 100
37647, V, 1, 1, 1, 1, 0, 704, 100
37648, V, 1, 1, 1, 1, 0, 704, 100
37649, V, 1, 1, 1, 1, 0, 704, 100
37650, V, 1, 1, 1, 1, 0, 704, 100
37651, V, 1, 1, 1, 1, 0, 704, 100
37652, V, 1, 1, 1, 1, 0, 704, 100
37653, V, 1, 1, 1, 1, 0, 704, 100
37654, V, 1, 1, 1, 1, 0, 704, 100
37655, V, 1, 1, 1, 1, 0, 704, 100
37656, V, 1, 1, 1, 1, 0, 704, 100
37657, V, 1, 1, 1, 1, 0, 704, 100
37658, V, 1, 1, 1, 1, 0, 704, 100
37659, V, 1, 1, 1, 1, 0, 704, 100
37660, V, 1, 1, 1, 1, 0, 704, 100
37661, V, 1, 1, 1, 1, 0, 704, 100
37662, V, 1, 1, 1, 1, 0, 704, 100
37663, V, 1, 1, 1, 1, 0, 704, 100
37664, V, 1, 1, 1, 1, 0, 704, 100
37665, V, 1, 1, 1, 1, 0, 704, 100
37666, V, 1, 1, 1, 1, 0, 704, 100
37667, V, 1, 1, 1, 1, 0, 704, 100
37668, V, 1, 1, 1, 1, 0, 704, 100
37669, V, 1, 1, 1, 1, 0, 704, 100
37670, V, 1, 1, 1, 1, 0, 704, 100
37671, V, 1, 1, 1, 1, 0, 704, 100
37672, V, 1, 1, 1, 1, 0, 704, 100
37673, V, 1, 1, 1, 1, 0, 704, 100
37675, V, 1, 1, 1, 1, 0, 704, 100
37676, V, 1, 1, 1, 1, 0, 704, 100
37677, V, 1, 1, 1, 1, 0, 704, 100
37678, V, 1, 1, 1, 1, 0, 704, 100
37679, V, 1, 1, 1, 1, 0, 704, 100
37680, V, 1, 1, 1, 1, 0, 704, 100
37681, V, 1, 1, 1, 1, 0, 704, 100
37682, V, 1, 1, 1, 1, 0, 704, 100
37683, V, 1, 1, 1, 1, 0, 704, 100
37684, V, 1, 1, 1, 1, 0, 704, 100
37685, V, 1, 1, 1, 1, 0, 704, 100
37686, V, 1, 1, 1, 1, 0, 704, 100
37687, V, 1, 1, 1, 1, 0, 704, 99
37688, V, 1, 1, 1, 1, 0, 704, 99
37689, V, 1, 1, 1, 1, 0, 704, 99
37690, V, 1, 1, 1, 1, 0, 704, 99
37691, V, 1, 1, 1, 1, 0, 704, 99
37692, V, 1, 1, 1, 1, 0, 704, 99
37693, V, 1, 1, 1, 1, 0, 704, 99
37694, V, 1, 1, 1, 1, 0, 704, 99
37695, V, 1, 1, 1, 1, 0, 704, 99
37696, V, 1, 1, 1, 1, 0, 704, 99
37697, V, 1, 1, 1, 1, 0, 704, 99
37698, V, 1, 1, 1, 1, 0, 704, 99
37699, V, 1, 0, 0, 1, 0, 704, 99
37699, V, 1, 0, 0, 0, 0, 704, 99
37700, V, 1, 0, 0, 0, 0, 704, 99
37701, V, 1, 0, 0, 0, 0, 704, 99
37702, V, 1, 0, 0, 0, 0, 704, 99
37703, V, 1, 0, 0, 0, 0, 704, 99
37704, V, 1, 0, 0, 0, 0, 704, 99
37705, V, 1, 0, 0, 0, 0, 704, 99
37706, V, 1, 0, 0, 0, 0, 704, 99
37707, V, 1, 0, 0, 0, 0, 704, 99
37708, V, 1, 0, 0, 0, 0, 704, 98
37709, V, 1, 0, 0, 0, 0, 704, 98
37710, V, 1, 0, 0, 0, 0, 704, 98
37711, V, 1, 0, 0, 0, 0, 704, 98
37712, V, 1, 0, 0, 0, 0, 704, 98
37713, V, 1, 0, 0, 0, 0, 704, 98
37714, V, 1, 0, 0, 0, 0, 704, 98
37715, V, 1, 0, 0, 0, 0, 704, 97
37716, V, 1, 0, 0, 0, 0, 704, 97
37718, V, 1, 0, 0, 0, 0, 704, 97
37719, V, 1, 0, 0, 0, 0, 704, 97
37720, V, 1, 0, 0, 0, 0, 704, 97
37721, V, 1, 0, 0, 0, 0, 704, 97
37722, V, 1, 0, 0, 0, 0, 704, 96
37723, V, 1, 0, 0, 0, 0, 704, 96
37724, V, 1, 0, 0, 0, 0, 704, 96
37725, V, 1, 0, 0, 0, 0, 704, 96
37726, V, 1, 0, 0, 0, 0, 704, 96
37727, V, 1, 0, 0, 0, 0, 704, 96
37728, V, 1, 0, 0, 0, 0, 704, 96
37729, V, 1, 0, 0, 0, 0, 704, 96
37730, V, 1, 0, 0, 0, 0, 704, 96
37731, V, 1, 0, 0, 0, 0, 704, 96
37732, V, 1, 0, 0, 0, 0, 704, 95
37733, V, 1, 0, 0, 0, 0, 704, 95
37734, V, 1, 0, 0, 0, 0, 704, 95
37735, V, 1, 0, 0, 0, 0, 704, 95
37736, V, 1, 0, 0, 0, 0, 704, 95
37737, V, 1, 0, 0, 0, 0, 704, 95
37738, V, 1, 0, 0, 0, 0, 704, 95
37739, V, 1, 0, 0, 0, 0, 704, 95
37740, V, 1, 0, 0, 0, 0, 704, 95
37741, V, 1, 0, 0, 0, 0, 704, 95
37742, V, 1, 0, 0, 0, 0, 704, 95
37743, V, 1, 0, 0, 0, 0, 704, 94
37744, V, 1, 0, 0, 0, 0, 704, 94
37745, V, 1, 0, 0, 0, 0, 704, 94
37746, V, 1, 0, 0, 0, 0, 704, 94
37747, V, 1, 0, 0, 0, 0, 704, 94
37748, V, 1, 0, 0, 0, 0, 704, 94
37749, V, 1, 0, 0, 0, 0, 704, 94
37750, V, 1, 0, 0, 0, 0, 704, 94
37751, V, 1, 0, 0, 0, 0, 704, 94
37752, V, 1, 0, 0, 0, 0, 704, 94
37753, V, 1, 0, 0, 0, 0, 704, 94
37754, V, 1, 0, 0, 0, 0, 704, 94
37755, V, 1, 0, 0, 0, 0, 704, 94
37756, V, 1, 0, 0, 0, 0, 704, 94
37757, V, 1, 0, 0, 0, 0, 704, 94
37758, V, 1, 0, 0, 0, 0, 704, 94
37760, V, 1, 0, 0, 0, 0, 704, 94
37761, V, 1, 0, 0, 0, 0, 704, 94
37762, V, 1, 0, 0, 0, 0, 704, 94
37763, V, 1, 0, 0, 0, 0, 704, 93
37764, V, 1, 0, 0, 0, 0, 704, 93
37765, V, 1, 0, 0, 0, 0, 704, 93
37766, V, 1, 0, 0, 0, 0, 704, 93
37767, V, 1, 0, 0, 0, 0, 704, 93
37768, V, 1, 0, 0, 0, 0, 704, 93
37769, V, 1, 0, 0, 0, 0, 704, 93
37770, V, 1, 0, 0, 0, 0, 704, 93
37771, V, 1, 0, 0, 0, 0, 704, 93
37772, V, 1, 0, 0, 0, 0, 704, 93
37773, V, 1, 0, 0, 0, 0, 704, 93
37774, V, 1, 0, 0, 0, 0, 704, 93
37775, V, 1, 0, 0, 0, 0, 704, 93
37776, V, 1, 0, 0, 0, 0, 704, 93
37777, V, 1, 0, 0, 0, 0, 704, 93
37778, V, 1, 0, 0, 0, 0, 704, 93
37779, V, 1, 0, 0, 0, 0, 704, 93
37780, V, 1, 0, 0, 0, 0, 704, 93
37781, V, 1, 0, 0, 0, 0, 704, 93
37782, V, 1, 0, 0, 0, 0, 704, 93
37783, V, 1, 0, 0, 0, 0, 704, 93
37784, V, 1, 0, 0, 0, 0, 704, 93
37785, V, 1, 0, 0, 0, 0, 704, 93
37786, V, 1, 0, 0, 0, 0, 704, 93
37787, V, 1, 0, 0, 0, 0, 704, 93
37788, V, 1, 0, 0, 0, 0, 704, 93
37789, V, 1, 0, 0, 0, 0, 704, 93
37790, V, 1, 0, 0, 0, 0, 704, 93
37791, V, 1, 0, 0, 0, 0, 704, 93
37792, V, 1, 0, 0, 0, 0, 704, 93
37793, V, 1, 0, 0, 0, 0, 704, 93
37794, V, 1, 0, 0, 0, 0, 704, 93
37795, V, 1, 0, 0, 0, 0, 704, 93
37796, V, 1, 0, 0, 0, 0, 704, 93
37797, V, 1, 0, 0, 0, 0, 704, 93
37798, V, 1, 0, 0, 0, 0, 704, 93
37799, V, 1, 0, 0, 0, 0, 704, 93
37800, V, 1, 0, 0, 0, 0, 704, 93
37801, V, 1, 0, 0, 0, 0, 704, 93
37803, V, 1, 0, 0, 0, 0, 704, 92
37804, V, 1, 0, 0, 0, 0, 704, 93
37805, V, 1, 0, 0, 0, 0, 704, 92
37806, V, 1, 0, 0, 0, 0, 704, 92
37807, V, 1, 0, 0, 0, 0, 704, 92
37808, V, 1, 0, 0, 0, 0, 704, 92
37809, V, 1, 0, 0, 0, 0, 704, 92
37810, V, 1, 0, 0, 0, 0, 704, 92
37811, V, 1, 0, 0, 0, 0, 704, 92
37812, V, 1, 0, 0, 0, 0, 704, 92
37813, V, 1, 0, 0, 0, 0, 704, 92
37814, V, 1, 0, 0, 0, 0, 704, 92
37815, V, 1, 0, 0, 0, 0, 704, 92
37816, V, 1, 0, 0, 0, 0, 704, 92
37817, V, 1, 0, 0, 0, 0, 704, 92
37818, V, 1, 0, 0, 0, 0, 704, 92
37819, V, 1, 0, 0, 0, 0, 704, 92
37820, V, 1, 0, 0, 0, 0, 704, 92
37821, V, 1, 0, 0, 0, 0, 704, 92
37822, V, 1, 0, 0, 0, 0, 704, 92
37823, V, 1, 0, 0, 0, 0, 704, 92
37824, V, 1, 0, 0, 0, 0, 704, 92
37825, V, 1, 0, 0, 0, 0, 704, 92
37826, V, 1, 0, 0, 0, 0, 704, 92
37827, V, 1, 0, 0, 0, 0, 704, 92
37828, V, 1, 0, 0, 0, 0, 704, 92
37829, V, 1, 0, 0, 0, 0, 704, 92
37830, V, 1, 0, 0, 0, 0, 704, 92
37831, V, 1, 0, 0, 0, 0, 704, 92
37832, V, 1, 0, 0, 0, 0, 704, 92
37833, V, 1, 0, 0, 0, 0, 704, 92
37834, V, 1, 0, 0, 0, 0, 704, 92
37835, V, 1, 0, 0, 0, 0, 704, 92
37836, V, 1, 0, 0, 0, 0, 704, 92
37837, V, 1, 0, 0, 0, 0, 704, 92
37838, V, 1, 0, 0, 0, 0, 704, 92
37839, V, 1, 0, 0, 0, 0, 704, 92
37840, V, 1, 0, 0, 0, 0, 704, 92
37841, V, 1, 0, 0, 0, 0, 704, 92
37842, V, 1, 0, 0, 0, 0, 704, 92
37843, V, 1, 0, 0, 0, 0, 704, 92
37844, V, 1, 0, 0, 0, 0, 704, 92
37846, V, 1, 0, 0, 0, 0, 704, 92
37847, V, 1, 0, 0, 0, 0, 704, 92
37848, V, 1, 0, 0, 0, 0, 704, 92
37849, V, 1, 0, 0, 0, 0, 704, 92
37850, V, 1, 0, 0, 0, 0, 704, 92
37851, V, 1, 0, 0, 0, 0, 704, 92
37852, V, 1, 0, 0, 0, 0, 704, 92
37853, V, 1, 0, 0, 0, 0, 704, 92
37854, V, 1, 0, 0, 0, 0, 704, 92
37855, V, 1, 0, 0, 0, 0, 704, 92
37856, V, 1, 0, 0, 0, 0, 704, 92
37857, V, 1, 0, 0, 0, 0, 704, 92
37858, V, 1, 0, 0, 0, 0, 704, 92
37859, V, 1, 0, 0, 0, 0, 704, 92
37860, V, 1, 0, 0, 0, 0, 704, 92
37861, V, 1, 0, 0, 0, 0, 704, 92
37862, V, 1, 0, 0, 0, 0, 704, 92
37863, V, 1, 0, 0, 0, 0, 704, 92
37864, V, 1, 0, 0, 0, 0, 704, 92
37865, V, 1, 0, 0, 0, 0, 704, 92
37866, V, 1, 0, 0, 0, 0, 704, 92
37867, V, 1, 0, 0, 0, 0, 704, 92
37868, V, 1, 0, 0, 0, 0, 704, 92
37869, V, 1, 0, 0, 0, 0, 704, 92
37870, V, 1, 0, 0, 0, 0, 704, 92
37871, V, 1, 0, 0, 0, 0, 704, 92
37872, V, 1, 0, 0, 0, 0, 704, 92
37873, V, 1, 0, 0, 0, 0, 704, 92
37874, V, 1, 0, 0, 0, 0, 704, 92
37875, V, 1, 0, 0, 0, 0, 704, 92
37876, V, 1, 0, 0, 0, 0, 704, 92
37877, V, 1, 0, 0, 0, 0, 704, 92
37878, V, 1, 0, 0, 0, 0, 704, 92
37879, V, 1, 0, 0, 0, 0, 704, 92
37880, V, 1, 0, 0, 0, 0, 704, 92
37881, V, 1, 0, 0, 0, 0, 704, 92
37882, V, 1, 0, 0, 0, 0, 704, 92
37883, V, 1, 0, 0, 0, 0, 704, 92
37884, V, 1, 0, 0, 0, 0, 704, 92
37885, V, 1, 0, 0, 0, 0, 704, 92
37886, V, 1, 0, 0, 0, 0, 704, 92
37888, V, 1, 0, 0, 0, 0, 704, 92
37889, V, 1, 0, 0, 0, 0, 704, 92
37890, V, 1, 0, 0, 0, 0, 704, 92
37891, V, 1, 0, 0, 0, 0, 704, 92
37892, V, 1, 0, 0, 0, 0, 704, 92
37893, V, 1, 0, 0, 0, 0, 704, 92
37894, V, 1, 0, 0, 0, 0, 704, 92
37895, V, 1, 0, 0, 0, 0, 704, 92
37896, V, 1, 0, 0, 0, 0, 704, 92
37897, V, 1, 0, 0, 0, 0, 704, 92
37898, V, 1, 0, 0, 0, 0, 704, 92
37899, V, 1, 0, 0, 0, 0, 704, 92
37900, V, 1, 0, 0, 0, 0, 704, 92
37901, V, 1, 0, 0, 0, 0, 704, 92
37902, V, 1, 0, 0, 0, 0, 704, 92
37903, V, 1, 0, 0, 0, 0, 704, 92
37904, V, 1, 0, 0, 0, 0, 704, 92
37905, V, 1, 0, 0, 0, 0, 704, 92
37906, V, 1, 0, 0, 0, 0, 704, 92
37907, V, 1, 0, 0, 0, 0, 704, 92
37908, V, 1, 0, 0, 0, 0, 704, 92
37909, V, 1, 0, 0, 0, 0, 704, 92
37910, V, 1, 0, 0, 0, 0, 704, 92
37911, V, 1, 0, 0, 0, 0, 704, 92
37912, V, 1, 0, 0, 0, 0, 704, 92
37913, V, 1, 0, 0, 0, 0, 704, 92
37914, V, 1, 0, 0, 0, 0, 704, 92
37915, V, 1, 0, 0, 0, 0, 704, 92
37916, V, 1, 0, 0, 0, 0, 704, 92
37917, V, 1, 0, 0, 0, 0, 704, 92
37918, V, 1, 0, 0, 0, 0, 704, 92
37919, V, 1, 0, 0, 0, 0, 704, 92
37920, V, 1, 0, 0, 0, 0, 704, 92
37921, V, 1, 0, 0, 0, 0, 704, 92
37922, V, 1, 0, 0, 0, 0, 704, 92
37923, V, 1, 0, 0, 0, 0, 704, 92
37924, V, 1, 0, 0, 0, 0, 704, 92
37925, V, 1, 0, 0, 0, 0, 704, 92
37926, V, 1, 0, 0, 0, 0, 704, 92
37927, V, 1, 0, 0, 0, 0, 704, 92
37928, V, 1, 0, 0, 0, 0, 704, 92
37929, V, 1, 0, 0, 0, 0, 704, 92
37931, V, 1, 0, 0, 0, 0, 704, 92
37932, V, 1, 0, 0, 0, 0, 704, 92
37933, V, 1, 0, 0, 0, 0, 704, 92
37934, V, 1, 0, 0, 0, 0, 704, 92
37935, V, 1, 0, 0, 0, 0, 704, 92
37936, V, 1, 0, 0, 0, 0, 704, 92
37937, V, 1, 0, 0, 0, 0, 704, 92
37938, V, 1, 0, 0, 0, 0, 704, 92
37939, V, 1, 0, 0, 0, 0, 704, 92
37940, V, 1, 0, 0, 0, 0, 704, 92
37941, V, 1, 0, 0, 0, 0, 704, 92
37942, V, 1, 0, 0, 0, 0, 704, 92
37943, V, 1, 0, 0, 0, 0, 704, 92
37944, V, 1, 0, 0, 0, 0, 704, 92
37945, V, 1, 0, 0, 0, 0, 704, 92
37946, V, 1, 0, 0, 0, 0, 704, 92
37947, V, 1, 0, 0, 0, 0, 704, 92
37948, V, 1, 0, 0, 0, 0, 704, 92
37949, V, 1, 0, 0, 0, 0, 704, 92
37950, V, 1, 0, 0, 0, 0, 704, 92
37951, V, 1, 0, 0, 0, 0, 704, 92
37952, V, 1, 0, 0, 0, 0, 704, 92
37953, V, 1, 0, 0, 0, 0, 704, 92
37954, V, 1, 0, 0, 0, 0, 704, 92
37955, V, 1, 0, 0, 0, 0, 704, 92
37956, V, 1, 0, 0, 0, 0, 704, 92
37957, V, 1, 0, 0, 0, 0, 704, 92
37958, V, 1, 0, 0, 0, 0, 704, 92
37959, V, 1, 0, 0, 0, 0, 704, 92
37960, V, 1, 0, 0, 0, 0, 704, 92
37961, V, 1, 0, 0, 0, 0, 704, 92
37962, V, 1, 0, 0, 0, 0, 704, 92
37963, V, 1, 0, 0, 0, 0, 704, 92
37964, V, 1, 0, 0, 0, 0, 704, 92
37965, V, 1, 0, 0, 0, 0, 704, 92
37966, V, 1, 0, 0, 0, 0, 704, 92
37967, V, 1, 0, 0, 0, 0, 704, 92
37968, V, 1, 0, 0, 0, 0, 704, 92
37969, V, 1, 0, 0, 0, 0, 704, 92
37970, V, 1, 0, 0, 0, 0, 704, 92
37971, V, 1, 0, 0, 0, 0, 704, 92
37972, V, 1, 0, 0, 0, 0, 704, 92
37974, V, 1, 0, 0, 0, 0, 704, 92
37975, V, 1, 0, 0, 0, 0, 704, 92
37976, V, 1, 0, 0, 0, 0, 704, 92
37977, V, 1, 0, 0, 0, 0, 704, 92
37978, V, 1, 0, 0, 0, 0, 704, 92
37979, V, 1, 0, 0, 0, 0, 704, 92
37980, V, 1, 0, 0, 0, 0, 704, 92
37981, V, 1, 0, 0, 0, 0, 704, 92
37982, V, 1, 0, 0, 0, 0, 704, 92
37983, V, 1, 0, 0, 0, 0, 704, 92
37984, V, 1, 0, 0, 0, 0, 704, 92
37985, V, 1, 0, 0, 0, 0, 704, 92
37986, V, 1, 0, 0, 0, 0, 704, 92
37987, V, 1, 0, 0, 0, 0, 704, 92
37988, V, 1, 0, 0, 0, 0, 704, 92
37989, V, 1, 0, 0, 0, 0, 704, 92
37990, V, 1, 0, 0, 0, 0, 704, 92
37991, V, 1, 0, 0, 0, 0, 704, 92
37992, V, 1, 0, 0, 0, 0, 704, 92
37993, V, 1, 0, 0, 0, 0, 704, 92
37994, V, 1, 0, 0, 0, 0, 704, 92
37995, V, 1, 0, 0, 0, 0, 704, 92
37996, V, 1, 0, 0, 0, 0, 704, 92
37997, V, 1, 0, 0, 0, 0, 704, 92
37998, V, 1, 0, 0, 0, 0, 704, 92
37999, V, 1, 0, 0, 0, 0, 704, 92
38000, V, 1, 0, 0, 0, 0, 704, 92
38001, V, 1, 0, 0, 0, 0, 704, 92
38002, V, 1, 0, 0, 0, 0, 704, 92
38003, V, 1, 0, 0, 0, 0, 704, 92
38004, V, 1, 0, 0, 0, 0, 704, 92
38005, V, 1, 0, 0, 0, 0, 704, 92
38006, V, 1, 0, 0, 0, 0, 704, 92
38007, V, 1, 0, 0, 0, 0, 704, 92
38008, V, 1, 0, 0, 0, 0, 704, 92
38009, V, 1, 0, 0, 0, 0, 704, 92
38010, V, 1, 0, 0, 0, 0, 704, 92
38011, V, 1, 0, 0, 0, 0, 704, 92
38012, V, 1, 0, 0, 0, 0, 704, 92
38013, V, 1, 0, 0, 0, 0, 704, 92
38014, V, 1, 0, 0, 0, 0, 704, 92
38016, V, 1, 0, 0, 0, 0, 704, 92
38017, V, 1, 0, 0, 0, 0, 704, 92
38018, V, 1, 0, 0, 0, 0, 704, 92
38019, V, 1, 0, 0, 0, 0, 704, 92
38020, V, 1, 0, 0, 0, 0, 704, 92
38021, V, 1, 0, 0, 0, 0, 704, 92
38022, V, 1, 0, 0, 0, 0, 704, 92
38023, V, 1, 0, 0, 0, 0, 704, 92
38024, V, 1, 0, 0, 0, 0, 704, 92
38025, V, 1, 0, 0, 0, 0, 704, 92
38026, V, 1, 0, 0, 0, 0, 704, 92
38027, V, 1, 0, 0, 0, 0, 704, 92
38028, V, 1, 0, 0, 0, 0, 704, 92
38029, V, 1, 0, 0, 0, 0, 704, 92
38030, V, 1, 0, 0, 0, 0, 704, 92
38031, V, 1, 0, 0, 0, 0, 704, 92
38032, V, 1, 0, 0, 0, 0, 704, 92
38033, V, 1, 0, 0, 0, 0, 704, 92
38034, V, 1, 0, 0, 0, 0, 704, 92
38035, V, 1, 0, 0, 0, 0, 704, 92
38036, V, 1, 0, 0, 0, 0, 704, 92
38037, V, 1, 0, 0, 0, 0, 704, 92
38038, V, 1, 0, 0, 0, 0, 704, 92
38039, V, 1, 0, 0, 0, 0, 704, 92
38040, V, 1, 0, 0, 0, 0, 704, 92
38041, V, 1, 0, 0, 0, 0, 704, 92
38042, V, 1, 0, 0, 0, 0, 704, 92
38043, V, 1, 0, 0, 0, 0, 704, 92
38044, V, 1, 0, 0, 0, 0, 704, 92
38045, V, 1, 0, 0, 0, 0, 704, 92
38046, V, 1, 0, 0, 0, 0, 704, 92
38047, V, 1, 0, 0, 0, 0, 704, 92
38048, V, 1, 0, 0, 0, 0, 704, 92
38049, V, 1, 0, 0, 0, 0, 704, 92
38050, V, 1, 0, 0, 0, 0, 704, 92
38051, V, 1, 0, 0, 0, 0, 704, 92
38052, V, 1, 0, 0, 0, 0, 704, 92
38053, V, 1, 0, 0, 0, 0, 704, 92
38054, V, 1, 0, 0, 0, 0, 704, 92
38055, V, 1, 0, 0, 0, 0, 704, 92
38056, V, 1, 0, 0, 0, 0, 704, 92
38057, V, 1, 0, 0, 0, 0, 704, 92
38059, V, 1, 0, 0, 0, 0, 704, 92
38060, V, 1, 0, 0, 0, 0, 704, 92
38061, V, 1, 0, 0, 0, 0, 704, 92
38062, V, 1, 0, 0, 0, 0, 704, 92
38063, V, 1, 0, 0, 0, 0, 704, 92
38064, V, 1, 0, 0, 0, 0, 704, 92
38065, V, 1, 0, 0, 0, 0, 704, 92
38066, V, 1, 0, 0, 0, 0, 704, 92
38067, V, 1, 0, 0, 0, 0, 704, 92
38068, V, 1, 0, 0, 0, 0, 704, 92
38069, V, 1, 0, 0, 0, 0, 704, 92
38070, V, 1, 0, 0, 0, 0, 704, 92
38071, V, 1, 0, 0, 0, 0, 704, 92
38072, V, 1, 0, 0, 0, 0, 704, 92
38073, V, 1, 0, 0, 0, 0, 704, 92
38074, V, 1, 0, 0, 0, 0, 704, 92
38075, V, 1, 0, 0, 0, 0, 704, 92
38076, V, 1, 0, 0, 0, 0, 704, 92
38077, V, 1, 0, 0, 0, 0, 704, 92
38078, V, 1, 0, 0, 0, 0, 704, 92
38079, V, 1, 0, 0, 0, 0, 704, 92
38080, V, 1, 0, 0, 0, 0, 704, 92
38081, V, 1, 0, 0, 0, 0, 704, 92
38082, V, 1, 0, 0, 0, 0, 704, 92
38083, V, 1, 0, 0, 0, 0, 704, 92
38084, V, 1, 0, 0, 0, 0, 704, 92
38085, V, 1, 0, 0, 0, 0, 704, 92
38086, V, 1, 0, 0, 0, 0, 704, 92
38087, V, 1, 0, 0, 0, 0, 704, 92
38088, V, 1, 0, 0, 0, 0, 704, 92
38089, V, 1, 0, 0, 0, 0, 704, 92
38090, V, 1, 0, 0, 0, 0, 704, 92
38091, V, 1, 0, 0, 0, 0, 704, 92
38092, V, 1, 0, 0, 0, 0, 704, 92
38093, V, 1, 0, 0, 0, 0, 704, 92
38094, V, 1, 0, 0, 0, 0, 704, 92
38095, V, 1, 0, 0, 0, 0, 704, 92
38096, V, 1, 0, 0, 0, 0, 704, 92
38097, V, 1, 0, 0, 0, 0, 704, 92
38098, V, 1, 0, 0, 0, 0, 704, 92
38099, V, 1, 0, 0, 0, 0, 704, 92
38100, V, 1, 0, 0, 0, 0, 704, 92
38102, V, 1, 0, 0, 0, 0, 704, 92
38103, V, 1, 0, 0, 0, 0, 704, 92
38104, V, 1, 0, 0, 0, 0, 704, 92
38105, V, 1, 0, 0, 0, 0, 704, 92
38106, V, 1, 0, 0, 0, 0, 704, 92
38107, V, 1, 0, 0, 0, 0, 704, 92
38108, V, 1, 0, 0, 0, 0, 704, 92
38109, V, 1, 0, 0, 0, 0, 704, 92
38110, V, 1, 0, 0, 0, 0, 704, 92
38111, V, 1, 0, 0, 0, 0, 704, 92
38112, V, 1, 0, 0, 0, 0, 704, 92
38113, V, 1, 0, 0, 0, 0, 704, 92
38114, V, 1, 0, 0, 0, 0, 704, 92
38115, V, 1, 0, 0, 0, 0, 704, 92
38116, V, 1, 0, 0, 0, 0, 704, 92
38117, V, 1, 0, 0, 0, 0, 704, 92
38118, V, 1, 0, 0, 0, 0, 704, 92
38119, V, 1, 0, 0, 0, 0, 704, 92
38120, V, 1, 0, 0, 0, 0, 704, 92
38121, V, 1, 0, 0, 0, 0, 704, 92
38122, V, 1, 0, 0, 0, 0, 704, 92
38123, V, 1, 0, 0, 0, 0, 704, 92
38124, V, 1, 0, 0, 0, 0, 704, 92
38125, V, 1, 0, 0, 0, 0, 704, 92
38126, V, 1, 0, 0, 0, 0, 704, 92
38127, V, 1, 0, 0, 0, 0, 704, 92
38128, V, 1, 0, 0, 0, 0, 704, 92
38129, V, 1, 0, 0, 0, 0, 704, 92
38130, V, 1, 0, 0, 0, 0, 704, 92
38131, V, 1, 0, 0, 0, 0, 704, 92
38132, V, 1, 0, 0, 0, 0, 704, 92
38133, V, 1, 0, 0, 0, 0, 704, 92
38134, V, 1, 0, 0, 0, 0, 704, 92
38135, V, 1, 0, 0, 0, 0, 704, 92
38136, V, 1, 0, 0, 0, 0, 704, 92
38137, V, 1, 0, 0, 0, 0, 704, 92
38138, V, 1, 0, 0, 0, 0, 704, 92
38139, V, 1, 0, 0, 0, 0, 704, 92
38140, V, 1, 0, 0, 0, 0, 704, 92
38141, V, 1, 0, 0, 0, 0, 704, 92
38142, V, 1, 0, 0, 0, 0, 704, 92
38144, V, 1, 0, 0, 0, 0, 704, 92
38145, V, 1, 0, 0, 0, 0, 704, 92
38146, V, 1, 0, 0, 0, 0, 704, 92
38147, V, 1, 0, 0, 0, 0, 704, 92
38148, V, 1, 0, 0, 0, 0, 704, 92
38149, V, 1, 0, 0, 0, 0, 704, 92
38150, V, 1, 0, 0, 0, 0, 704, 92
38151, V, 1, 0, 0, 0, 0, 704, 92
38152, V, 1, 0, 0, 0, 0, 704, 92
38153, V, 1, 0, 0, 0, 0, 704, 92
38154, V, 1, 0, 0, 0, 0, 704, 92
38155, V, 1, 0, 0, 0, 0, 704, 92
38156, V, 1, 0, 0, 0, 0, 704, 92
38157, V, 1, 0, 0, 0, 0, 704, 92
38158, V, 1, 0, 0, 0, 0, 704, 92
38159, V, 1, 0, 0, 0, 0, 704, 92
38160, V, 1, 0, 0, 0, 0, 704, 92
38161, V, 1, 0, 0, 0, 0, 704, 92
38162, V, 1, 0, 0, 0, 0, 704, 92
38163, V, 1, 0, 0, 0, 0, 704, 92
38164, V, 1, 0, 0, 0, 0, 704, 92
38165, V, 1, 0, 0, 0, 0, 704, 92
38166, V, 1, 0, 0, 0, 0, 704, 92
38167, V, 1, 0, 0, 0, 0, 704, 92
38168, V, 1, 0, 0, 0, 0, 704, 92
38169, V, 1, 0, 0, 0, 0, 704, 92
38170, V, 1, 0, 0, 0, 0, 704, 92
38171, V, 1, 0, 0, 0, 0, 704, 92
38172, V, 1, 0, 0, 0, 0, 704, 92
38173, V, 1, 0, 0, 0, 0, 704, 92
38174, V, 1, 0, 0, 0, 0, 704, 92
38175, V, 1, 0, 0, 0, 0, 704, 92
38176, V, 1, 0, 0, 0, 0, 704, 92
38177, V, 1, 0, 0, 0, 0, 704, 92
38178, V, 1, 0, 0, 0, 0, 704, 92
38179, V, 1, 0, 0, 0, 0, 704, 92
38180, V, 1, 0, 0, 0, 0, 704, 92
38181, V, 1, 0, 0, 0, 0, 704, 92
38182, V, 1, 0, 0, 0, 0, 704, 92
38183, V, 1, 0, 0, 0, 0, 704, 92
38184, V, 1, 0, 0, 0, 0, 704, 92
38185, V, 1, 0, 0, 0, 0, 704, 92
38187, V, 1, 0, 0, 0, 0, 704, 92
38188, V, 1, 0, 0, 0, 0, 704, 92
38189, V, 1, 0, 0, 0, 0, 704, 92
38190, V, 1, 0, 0, 0, 0, 704, 92
38191, V, 1, 0, 0, 0, 0, 704, 92
38192, V, 1, 0, 0, 0, 0, 704, 92
38193, V, 1, 0, 0, 0, 0, 704, 92
38194, V, 1, 0, 0, 0, 0, 704, 92
38195, V, 1, 0, 0, 0, 0, 704, 92
38196, V, 1, 0, 0, 0, 0, 704, 92
38197, V, 1, 0, 0, 0, 0, 704, 92
38198, V, 1, 0, 0, 0, 0, 704, 92
38199, V, 1, 0, 0, 0, 0, 704, 92
38200, V, 1, 0, 0, 0, 0, 704, 92
38201, V, 1, 0, 0, 0, 0, 704, 92
38202, V, 1, 0, 0, 0, 0, 704, 92
38203, V, 1, 0, 0, 0, 0, 704, 92
38204, V, 1, 0, 0, 0, 0, 704, 92
38205, V, 1, 0, 0, 0, 0, 704, 92
38206, V, 1, 0, 0, 0, 0, 704, 92
38207, V, 1, 0, 0, 0, 0, 704, 92
38208, V, 1, 0, 0, 0, 0, 704, 92
38209, V, 1, 0, 0, 0, 0, 704, 92
38210, V, 1, 0, 0, 0, 0, 704, 92
38211, V, 1, 0, 0, 0, 0, 704, 92
38212, V, 1, 0, 0, 0, 0, 704, 92
38213, V, 1, 0, 0, 0, 0, 704, 92
38214, V, 1, 0, 0, 0, 0, 704, 92
38215, V, 1, 0, 0, 0, 0, 704, 92
38216, V, 1, 0, 0, 0, 0, 704, 92
38217, V, 1, 0, 0, 0, 0, 704, 92
38218, V, 1, 0, 0, 0, 0, 704, 92
38219, V, 1, 0, 0, 0, 0, 704, 92
38220, V, 1, 0, 0, 0, 0, 704, 92
38221, V, 1, 0, 0, 0, 0, 704, 92
38222, V, 1, 0, 0, 0, 0, 704, 92
38223, V, 1, 0, 0, 0, 0, 704, 92
38224, V, 1, 0, 0, 0, 0, 704, 92
38225, V, 1, 0, 0, 0, 0, 704, 92
38226, V, 1, 0, 0, 0, 0, 704, 92
38227, V, 1, 0, 0, 0, 0, 704, 92
38228, V, 1, 0, 0, 0, 0, 704, 92
38230, V, 1, 0, 0, 0, 0, 704, 92
38231, V, 1, 0, 0, 0, 0, 704, 92
38232, V, 1, 0, 0, 0, 0, 704, 92
38233, V, 1, 0, 0, 0, 0, 704, 92
38234, V, 1, 0, 0, 0, 0, 704, 92
38235, V, 1, 0, 0, 0, 0, 704, 92
38236, V, 1, 0, 0, 0, 0, 704, 92
38237, V, 1, 0, 0, 0, 0, 704, 92
38238, V, 1, 0, 0, 0, 0, 704, 92
38239, V, 1, 0, 0, 0, 0, 704, 92
38240, V, 1, 0, 0, 0, 0, 704, 92
38241, V, 1, 0, 0, 0, 0, 704, 92
38242, V, 1, 0, 0, 0, 0, 704, 92
38243, V, 1, 0, 0, 0, 0, 704, 92
38244, V, 1, 0, 0, 0, 0, 704, 92
38245, V, 1, 0, 0, 0, 0, 704, 92
38246, V, 1, 0, 0, 0, 0, 704, 92
38247, V, 1, 0, 0, 0, 0, 704, 92
38248, V, 1, 0, 0, 0, 0, 704, 92
38249, V, 1, 0, 0, 0, 0, 704, 92
38250, V, 1, 0, 0, 0, 0, 704, 92
38251, V, 1, 0, 0, 0, 0, 704, 92
38252, V, 1, 0, 0, 0, 0, 704, 92
38253, V, 1, 0, 0, 0, 0, 704, 92
38254, V, 1, 0, 0, 0, 0, 704, 92
38255, V, 1, 0, 0, 0, 0, 704, 92
38256, V, 1, 0, 0, 0, 0, 704, 92
38257, V, 1, 0, 0, 0, 0, 704, 92
38258, V, 1, 0, 0, 0, 0, 704, 92
38259, V, 1, 0, 0, 0, 0, 704, 92
38260, V, 1, 0, 0, 0, 0, 704, 92
38261, V, 1, 0, 0, 0, 0, 704, 92
38262, V, 1, 0, 0, 0, 0, 704, 92
38263, V, 1, 0, 0, 0, 0, 704, 92
38264, V, 1, 0, 0, 0, 0, 704, 92
38265, V, 1, 0, 0, 0, 0, 704, 92
38266, V, 1, 0, 0, 0, 0, 704, 92
38267, V, 1, 0, 0, 0, 0, 704, 92
38268, V, 1, 0, 0, 0, 0, 704, 92
38269, V, 1, 0, 0, 0, 0, 704, 92
38270, V, 1, 0, 0, 0, 0, 704, 92
38272, V, 1, 0, 0, 0, 0, 704, 92
38273, V, 1, 0, 0, 0, 0, 704, 92
38274, V, 1, 0, 0, 0, 0, 704, 92
38275, V, 1, 0, 0, 0, 0, 704, 92
38276, V, 1, 0, 0, 0, 0, 704, 92
38277, V, 1, 0, 0, 0, 0, 704, 92
38278, V, 1, 0, 0, 0, 0, 704, 92
38279, V, 1, 0, 0, 0, 0, 704, 92
38280, V, 1, 0, 0, 0, 0, 704, 92
38281, V, 1, 0, 0, 0, 0, 704, 92
38282, V, 1, 0, 0, 0, 0, 704, 92
38283, V, 1, 0, 0, 0, 0, 704, 92
38284, V, 1, 0, 0, 0, 0, 704, 92
38285, V, 1, 0, 0, 0, 0, 704, 92
38286, V, 1, 0, 0, 0, 0, 704, 92
38287, V, 1, 0, 0, 0, 0, 704, 92
38288, V, 1, 0, 0, 0, 0, 704, 92
38289, V, 1, 0, 0, 0, 0, 704, 92
38290, V, 1, 0, 0, 0, 0, 704, 92
38291, V, 1, 0, 0, 0, 0, 704, 92
38292, V, 1, 0, 0, 0, 0, 704, 92
38293, V, 1, 0, 0, 0, 0, 704, 92
38294, V, 1, 0, 0, 0, 0, 704, 92
38295, V, 1, 0, 0, 0, 0, 704, 92
38296, V, 1, 0, 0, 0, 0, 704, 92
38297, V, 1, 0, 0, 0, 0, 704, 92
38298, V, 1, 0, 0, 0, 0, 704, 92
38299, V, 1, 0, 0, 0, 0, 704, 92
38300, V, 1, 0, 0, 0, 0, 704, 92
38301, V, 1, 0, 0, 0, 0, 704, 92
38302, V, 1, 0, 0, 0, 0, 704, 92
38303, V, 1, 0, 0, 0, 0, 704, 92
38304, V, 1, 0, 0, 0, 0, 704, 92
38305, V, 1, 0, 0, 0, 0, 704, 92
38306, V, 1, 0, 0, 0, 0, 704, 92
38307, V, 1, 0, 0, 0, 0, 704, 92
38308, V, 1, 0, 0, 0, 0, 704, 92
38309, V, 1, 0, 0, 0, 0, 704, 92
38310, V, 1, 0, 0, 0, 0, 704, 92
38311, V, 1, 0, 0, 0, 0, 704, 92
38312, V, 1, 0, 0, 0, 0, 704, 92
38313, V, 1, 0, 0, 0, 0, 704, 92
38315, V, 1, 0, 0, 0, 0, 704, 92
38316, V, 1, 0, 0, 0, 0, 704, 92
38317, V, 1, 0, 0, 0, 0, 704, 92
38318, V, 1, 0, 0, 0, 0, 704, 92
38319, V, 1, 0, 0, 0, 0, 704, 92
38320, V, 1, 0, 0, 0, 0, 704, 92
38321, V, 1, 0, 0, 0, 0, 704, 92
38322, V, 1, 0, 0, 0, 0, 704, 92
38323, V, 1, 0, 0, 0, 0, 704, 92
38324, V, 1, 0, 0, 0, 0, 704, 92
38325, V, 1, 0, 0, 0, 0, 704, 92
38326, V, 1, 0, 0, 0, 0, 704, 92
38327, V, 1, 0, 0, 0, 0, 704, 92
38328, V, 1, 0, 0, 0, 0, 704, 92
38329, V, 1, 0, 0, 0, 0, 704, 92
38330, V, 1, 0, 0, 0, 0, 704, 92
38331, V, 1, 0, 0, 0, 0, 704, 92
38332, V, 1, 0, 0, 0, 0, 704, 92
38333, V, 1, 0, 0, 0, 0, 704, 92
38334, V, 1, 0, 0, 0, 0, 704, 92
38335, V, 1, 0, 0, 0, 0, 704, 92
38336, V, 1, 0, 0, 0, 0, 704, 92
38337, V, 1, 0, 0, 0, 0, 704, 92
38338, V, 1, 0, 0, 0, 0, 704, 92
38339, V, 1, 0, 0, 0, 0, 704, 92
38340, V, 1, 0, 0, 0, 0, 704, 92
38341, V, 1, 0, 0, 0, 0, 704, 92
38342, V, 1, 0, 0, 0, 0, 704, 92
38343, V, 1, 0, 0, 0, 0, 704, 92
38344, V, 1, 0, 0, 0, 0, 704, 92
38345, V, 1, 0, 0, 0, 0, 704, 92
38346, V, 1, 0, 0, 0, 0, 704, 92
38347, V, 1, 0, 0, 0, 0, 704, 92
38348, V, 1, 0, 0, 0, 0, 704, 92
38349, V, 1, 0, 0, 0, 0, 704, 92
38350, V, 1, 0, 0, 0, 0, 704, 91
38351, V, 1, 0, 0, 0, 0, 704, 91
38352, V, 1, 0, 0, 0, 0, 704, 90
38353, V, 1, 0, 0, 0, 0, 704, 89
38354, V, 1, 0, 0, 0, 0, 704, 88
38355, V, 1, 0, 0, 0, 0, 704, 87
38356, V, 1, 0, 0, 0, 0, 704, 86
38358, V, 1, 0, 0, 0, 0, 704, 85
38359, V, 1, 0, 0, 0, 0, 704, 84
38360, V, 1, 0, 0, 0, 0, 704, 83
38361, V, 1, 0, 0, 0, 0, 704, 82
38362, V, 1, 0, 0, 0, 0, 704, 81
38363, V, 1, 0, 0, 0, 0, 704, 80
38364, V, 1, 0, 0, 0, 0, 704, 79
38365, V, 1, 0, 0, 0, 0, 704, 79
38366, V, 1, 0, 0, 0, 0, 704, 78
38367, V, 1, 0, 0, 0, 0, 704, 77
38368, V, 1, 0, 0, 0, 0, 704, 76
38369, V, 1, 0, 0, 0, 0, 704, 76
38370, V, 1, 0, 0, 0, 0, 704, 75
38371, V, 1, 0, 0, 0, 0, 704, 74
38372, V, 1, 0, 0, 0, 0, 704, 74
38373, V, 1, 0, 0, 0, 0, 704, 73
38374, V, 1, 0, 0, 0, 0, 704, 73
38375, V, 1, 0, 0, 0, 0, 704, 72
38376, V, 1, 0, 0, 0, 0, 704, 72
38377, V, 1, 0, 0, 0, 0, 704, 71
38378, V, 1, 0, 0, 0, 0, 704, 70
38379, V, 1, 0, 0, 0, 0, 704, 70
38380, V, 1, 0, 0, 0, 0, 704, 70
38381, V, 1, 0, 0, 0, 0, 704, 69
38382, V, 1, 0, 0, 0, 0, 704, 68
38383, V, 1, 0, 0, 0, 0, 704, 68
38384, V, 1, 0, 0, 0, 0, 704, 68
38385, V, 1, 0, 0, 0, 0, 704, 67
38386, V, 1, 0, 0, 0, 0, 704, 67
38387, V, 1, 0, 0, 0, 0, 704, 66
38388, V, 1, 0, 0, 0, 0, 704, 66
38389, V, 1, 0, 0, 0, 0, 704, 66
38390, V, 1, 0, 0, 0, 0, 704, 65
38391, V, 1, 0, 0, 0, 0, 704, 65
38392, V, 1, 0, 0, 0, 0, 704, 65
38393, V, 1, 0, 0, 0, 0, 704, 64
38394, V, 1, 0, 0, 0, 0, 704, 64
38395, V, 1, 0, 0, 0, 0, 704, 64
38396, V, 1, 0, 0, 0, 0, 704, 63
38397, V, 1, 0, 0, 0, 0, 704, 63
38398, V, 1, 0, 0, 0, 0, 704, 63
38400, V, 1, 0, 0, 0, 0, 704, 62
38401, V, 1, 0, 0, 0, 0, 704, 62
38402, V, 1, 0, 0, 0, 0, 704, 62
38403, V, 1, 0, 0, 0, 0, 704, 62
38404, V, 1, 0, 0, 0, 0, 704, 61
38405, V, 1, 0, 0, 0, 0, 704, 61
38406, V, 1, 0, 0, 0, 0, 704, 61
38407, V, 1, 0, 0, 0, 0, 704, 61
38408, V, 1, 0, 0, 0, 0, 704, 60
38409, V, 1, 0, 0, 0, 0, 704, 60
38410, V, 1, 0, 0, 0, 0, 704, 60
38411, V, 1, 0, 0, 0, 0, 704, 60
38412, V, 1, 0, 0, 0, 0, 704, 60
38413, V, 1, 0, 0, 0, 0, 704, 59
38414, V, 1, 0, 0, 0, 0, 704, 59
38415, V, 1, 0, 0, 0, 0, 704, 59
38416, V, 1, 0, 0, 0, 0, 704, 59
38417, V, 1, 0, 0, 0, 0, 704, 59
38418, V, 1, 0, 0, 0, 0, 704, 59
38419, V, 1, 0, 0, 0, 0, 704, 58
38420, V, 1, 0, 0, 0, 0, 704, 58
38421, V, 1, 0, 0, 0, 0, 704, 58
38422, V, 1, 0, 0, 0, 0, 704, 58
38423, V, 1, 0, 0, 0, 0, 704, 58
38424, V, 1, 0, 0, 0, 0, 704, 58
38425, V, 1, 0, 0, 0, 0, 704, 58
38426, V, 1, 0, 0, 0, 0, 704, 57
38427, V, 1, 0, 0, 0, 0, 704, 57
38428, V, 1, 0, 0, 0, 0, 704, 57
38429, V, 1, 0, 0, 0, 0, 704, 57
38430, V, 1, 0, 0, 0, 0, 704, 57
38431, V, 1, 0, 0, 0, 0, 704, 57
38432, V, 1, 0, 0, 0, 0, 704, 57
38433, V, 1, 0, 0, 0, 0, 704, 57
38434, V, 1, 0, 0, 0, 0, 704, 57
38435, V, 1, 0, 0, 0, 0, 704, 57
38436, V, 1, 0, 0, 0, 0, 704, 56
38437, V, 1, 0, 0, 0, 0, 704, 56
38438, V, 1, 0, 0, 0, 0, 704, 56
38439, V, 1, 0, 0, 0, 0, 704, 56
38440, V, 1, 0, 0, 0, 0, 704, 56
38441, V, 1, 0, 0, 0, 0, 704, 56
38443, V, 1, 0, 0, 0, 0, 704, 56
38444, V, 1, 0, 0, 0, 0, 704, 56
38445, V, 1, 0, 0, 0, 0, 704, 56
38446, V, 1, 0, 0, 0, 0, 704, 56
38447, V, 1, 0, 0, 0, 0, 704, 56
38448, V, 1, 0, 0, 0, 0, 704, 56
38449, V, 1, 0, 0, 0, 0, 704, 56
38450, V, 1, 0, 0, 0, 0, 704, 55
38451, V, 1, 0, 0, 0, 0, 704, 55
38452, V, 1, 0, 0, 0, 0, 704, 55
38453, V, 1, 0, 0, 0, 0, 704, 55
38454, V, 1, 0, 0, 0, 0, 704, 55
38455, V, 1, 0, 0, 0, 0, 704, 55
38456, V, 1, 0, 0, 0, 0, 704, 55
38457, V, 1, 0, 0, 0, 0, 704, 55
38458, V, 1, 0, 0, 0, 0, 704, 55
38459, V, 1, 0, 0, 0, 0, 704, 55
38460, V, 1, 0, 0, 0, 0, 704, 55
38461, V, 1, 0, 0, 0, 0, 704, 55
38462, V, 1, 0, 0, 0, 0, 704, 55
38463, V, 1, 0, 0, 0, 0, 704, 55
38464, V, 1, 0, 0, 0, 0, 704, 55
38465, V, 1, 0, 0, 0, 0, 704, 55
38466, V, 1, 0, 0, 0, 0, 704, 55
38467, V, 1, 0, 0, 0, 0, 704, 55
38468, V, 1, 0, 0, 0, 0, 704, 54
38469, V, 1, 0, 0, 0, 0, 704, 54
38470, V, 1, 0, 0, 0, 0, 704, 54
38471, V, 1, 0, 0, 0, 0, 704, 54
38472, V, 1, 0, 0, 0, 0, 704, 54
38473, V, 1, 0, 0, 0, 0, 704, 54
38474, V, 1, 0, 0, 0, 0, 704, 54
38475, V, 1, 0, 0, 0, 0, 704, 54
38476, V, 1, 0, 0, 0, 0, 704, 54
38477, V, 1, 0, 0, 0, 0, 704, 54
38478, V, 1, 0, 0, 0, 0, 704, 54
38479, V, 1, 0, 0, 0, 0, 704, 54
38480, V, 1, 0, 0, 0, 0, 704, 54
38481, V, 1, 0, 0, 0, 0, 704, 54
38482, V, 1, 0, 0, 0, 0, 704, 54
38483, V, 1, 0, 0, 0, 0, 704, 54
38484, V, 1, 0, 0, 0, 0, 704, 54
38486, V, 1, 0, 0, 0, 0, 704, 54
38487, V, 1, 0, 0, 0, 0, 704, 54
38488, V, 1, 0, 0, 0, 0, 704, 54
38489, V, 1, 0, 0, 0, 0, 704, 54
38490, V, 1, 0, 0, 0, 0, 704, 54
38491, V, 1, 0, 0, 0, 0, 704, 54
38492, V, 1, 0, 0, 0, 0, 704, 54
38493, V, 1, 0, 0, 0, 0, 704, 54
38494, V, 1, 0, 0, 0, 0, 704, 54
38495, V, 1, 0, 0, 0, 0, 704, 54
38496, V, 1, 0, 0, 0, 0, 704, 54
38497, V, 1, 0, 0, 0, 0, 704, 54
38498, V, 1, 0, 0, 0, 0, 704, 54
38499, V, 1, 0, 0, 0, 0, 704, 54
38500, V, 1, 0, 0, 0, 0, 704, 54
38501, V, 1, 0, 0, 0, 0, 704, 54
38502, V, 1, 0, 0, 0, 0, 704, 54
38503, V, 1, 0, 0, 0, 0, 704, 54
38504, V, 1, 0, 0, 0, 0, 704, 54
38505, V, 1, 0, 0, 0, 0, 704, 54
38506, V, 1, 0, 0, 0, 0, 704, 54
38507, V, 1, 0, 0, 0, 0, 704, 54
38508, V, 1, 0, 0, 0, 0, 704, 54
38509, V, 1, 0, 0, 0, 0, 704, 54
38510, V, 1, 0, 0, 0, 0, 704, 54
38511, V, 1, 0, 0, 0, 0, 704, 54
38512, V, 1, 0, 0, 0, 0, 704, 54
38513, V, 1, 0, 0, 0, 0, 704, 54
38514, V, 1, 0, 0, 0, 0, 704, 54
38515, V, 1, 0, 0, 0, 0, 704, 54
38516, V, 1, 0, 0, 0, 0, 704, 54
38517, V, 1, 0, 0, 0, 0, 704, 54
38518, V, 1, 0, 0, 0, 0, 704, 54
38519, V, 1, 0, 0, 0, 0, 704, 54
38520, V, 1, 0, 0, 0, 0, 704, 54
38521, V, 1, 0, 0, 0, 0, 704, 54
38522, V, 1, 0, 0, 0, 0, 704, 54
38523, V, 1, 0, 0, 0, 0, 704, 54
38524, V, 1, 0, 0, 0, 0, 704, 54
38525, V, 1, 0, 0, 0, 0, 704, 54
38526, V, 1, 0, 0, 0, 0, 704, 54
38528, V, 1, 0, 0, 0, 0, 704, 54
38529, V, 1, 0, 0, 0, 0, 704, 54
38530, V, 1, 0, 0, 0, 0, 704, 54
38531, V, 1, 0, 0, 0, 0, 704, 54
38532, V, 1, 0, 0, 0, 0, 704, 54
38533, V, 1, 0, 0, 0, 0, 704, 54
38534, V, 1, 0, 0, 0, 0, 704, 54
38535, V, 1, 0, 0, 0, 0, 704, 54
38536, V, 1, 0, 0, 0, 0, 704, 54
38537, V, 1, 0, 0, 0, 0, 704, 54
38538, V, 1, 0, 0, 0, 0, 704, 54
38539, V, 1, 0, 0, 0, 0, 704, 54
38540, V, 1, 0, 0, 0, 0, 704, 54
38541, V, 1, 0, 0, 0, 0, 704, 54
38542, V, 1, 0, 0, 0, 0, 704, 54
38543, V, 1, 0, 0, 0, 0, 704, 54
38544, V, 1, 0, 0, 0, 0, 704, 54
38545, V, 1, 0, 0, 0, 0, 704, 54
38546, V, 1, 0, 0, 0, 0, 704, 54
38547, V, 1, 0, 0, 0, 0, 704, 54
38548, V, 1, 0, 0, 0, 0, 704, 55
38549, V, 1, 0, 0, 0, 0, 704, 54
38550, V, 1, 0, 0, 0, 0, 704, 55
38551, V, 1, 0, 0, 0, 0, 704, 55
38552, V, 1, 0, 0, 0, 0, 704, 55
38553, V, 1, 0, 0, 0, 0, 704, 55
38554, V, 1, 0, 0, 0, 0, 704, 55
38555, V, 1, 0, 0, 0, 0, 704, 55
38556, V, 1, 0, 0, 0, 0, 704, 55
38557, V, 1, 0, 0, 0, 0, 704, 55
38558, V, 1, 0, 0, 0, 0, 704, 55
38559, V, 1, 0, 0, 0, 0, 704, 55
38560, V, 1, 0, 0, 0, 0, 704, 55
38561, V, 1, 0, 0, 0, 0, 704, 55
38562, V, 1, 0, 0, 0, 0, 704, 55
38563, V, 1, 0, 0, 0, 0, 704, 55
38564, V, 1, 0, 0, 0, 0, 704, 55
38565, V, 1, 0, 0, 0, 0, 704, 55
38566, V, 1, 0, 0, 0, 0, 704, 55
38567, V, 1, 0, 0, 0, 0, 704, 55
38568, V, 1, 0, 0, 0, 0, 704, 55
38569, V, 1, 0, 0, 0, 0, 704, 55
38571, V, 1, 0, 0, 0, 0, 704, 55
38572, V, 1, 0, 0, 0, 0, 704, 55
38573, V, 1, 0, 0, 0, 0, 704, 55
38574, V, 1, 0, 0, 0, 0, 704, 55
38575, V, 1, 0, 0, 0, 0, 704, 55
38576, V, 1, 0, 0, 0, 0, 704, 55
38577, V, 1, 0, 0, 0, 0, 704, 55
38578, V, 1, 0, 0, 0, 0, 704, 55
38579, V, 1, 0, 0, 0, 0, 704, 55
38580, V, 1, 0, 0, 0, 0, 704, 55
38581, V, 1, 0, 0, 0, 0, 704, 55
38582, V, 1, 0, 0, 0, 0, 704, 55
38583, V, 1, 0, 0, 0, 0, 704, 55
38584, V, 1, 0, 0, 0, 0, 704, 55
38585, V, 1, 0, 0, 0, 0, 704, 55
38586, V, 1, 0, 0, 0, 0, 704, 55
38587, V, 1, 0, 0, 0, 0, 704, 55
38588, V, 1, 0, 0, 0, 0, 704, 55
38589, V, 1, 0, 0, 0, 0, 704, 55
38590, V, 1, 0, 0, 0, 0, 704, 55
38591, V, 1, 0, 0, 0, 0, 704, 55
38592, V, 1, 0, 0, 0, 0, 704, 55
38593, V, 1, 0, 0, 0, 0, 704, 55
38594, V, 1, 0, 0, 0, 0, 704, 55
38595, V, 1, 0, 0, 0, 0, 704, 55
38596, V, 1, 0, 0, 0, 0, 704, 55
38597, V, 1, 0, 0, 0, 0, 704, 55
38598, V, 1, 0, 0, 0, 0, 704, 55
38599, V, 1, 0, 0, 0, 0, 704, 55
38600, V, 1, 0, 0, 0, 0, 704, 55
38601, V, 1, 0, 0, 0, 0, 704, 55
38602, V, 1, 0, 0, 0, 0, 704, 55
38603, V, 1, 0, 0, 0, 0, 704, 55
38604, V, 1, 0, 0, 0, 0, 704, 55
38605, V, 1, 0, 0, 0, 0, 704, 55
38606, V, 1, 0, 0, 0, 0, 704, 55
38607, V, 1, 0, 0, 0, 0, 704, 55
38608, V, 1, 0, 0, 0, 0, 704, 55
38609, V, 1, 0, 0, 0, 0, 704, 55
38610, V, 1, 0, 0, 0, 0, 704, 55
38611, V, 1, 0, 0, 0, 0, 704, 55
38612, V, 1, 0, 0, 0, 0, 704, 55
38614, V, 1, 0, 0, 0, 0, 704, 55
38615, V, 1, 0, 0, 0, 0, 704, 55
38616, V, 1, 0, 0, 0, 0, 704, 55
38617, V, 1, 0, 0, 0, 0, 704, 55
38618, V, 1, 0, 0, 0, 0, 704, 55
38619, V, 1, 0, 0, 0, 0, 704, 55
38620, V, 1, 0, 0, 0, 0, 704, 55
38621, V, 1, 0, 0, 0, 0, 704, 56
38622, V, 1, 0, 0, 0, 0, 704, 56
38623, V, 1, 0, 0, 0, 0, 704, 56
38624, V, 1, 0, 0, 0, 0, 704, 56
38625, V, 1, 0, 0, 0, 0, 704, 57
38626, V, 1, 0, 0, 0, 0, 704, 57
38627, V, 1, 0, 0, 0, 0, 704, 58
38628, V, 1, 0, 0, 0, 0, 704, 58
38629, V, 1, 1, 0, 0, 0, 704, 58
38629, V, 1, 1, 0, 0, 0, 704, 58
38630, V, 1, 1, 1, 1, 0, 704, 59
38631, V, 1, 1, 1, 1, 0, 704, 59
38632, V, 1, 1, 1, 1, 0, 704, 60
38633, V, 1, 1, 1, 1, 0, 704, 60
38634, V, 1, 1, 1, 1, 0, 704, 61
38635, V, 1, 1, 1, 1, 0, 704, 62
38636, V, 1, 1, 1, 1, 0, 704, 62
38637, V, 1, 1, 1, 1, 0, 704, 63
38638, V, 1, 1, 1, 1, 0, 704, 64
38639, V, 1, 1, 1, 1, 0, 704, 65
38640, V, 1, 1, 1, 1, 0, 704, 66
38641, V, 1, 1, 1, 1, 0, 704, 67
38642, V, 1, 1, 1, 1, 0, 704, 68
38643, V, 1, 1, 1, 1, 0, 704, 69
38644, V, 1, 1, 1, 1, 0, 704, 70
38645, V, 1, 1, 1, 1, 0, 704, 71
38646, V, 1, 1, 1, 1, 0, 704, 72
38647, V, 1, 1, 1, 1, 0, 704, 72
38648, V, 1, 1, 1, 1, 0, 704, 73
38649, V, 1, 1, 1, 1, 0, 704, 74
38650, V, 1, 1, 1, 1, 0, 704, 75
38651, V, 1, 1, 1, 1, 0, 704, 75
38652, V, 1, 1, 1, 1, 0, 704, 76
38653, V, 1, 1, 1, 1, 0, 704, 77
38654, V, 1, 1, 1, 1, 0, 704, 77
38656, V, 1, 1, 1, 1, 0, 704, 78
38657, V, 1, 1, 1, 1, 0, 704, 79
38658, V, 1, 1, 1, 1, 0, 704, 79
38659, V, 1, 1, 1, 1, 0, 704, 80
38660, V, 1, 1, 1, 1, 0, 704, 80
38661, V, 1, 1, 1, 1, 0, 704, 81
38662, V, 1, 1, 1, 1, 0, 704, 81
38663, V, 1, 1, 1, 1, 0, 704, 82
38664, V, 1, 1, 1, 1, 0, 704, 82
38665, V, 1, 1, 1, 1, 0, 704, 83
38666, V, 1, 1, 1, 1, 0, 704, 83
38667, V, 1, 1, 1, 1, 0, 704, 84
38668, V, 1, 1, 1, 1, 0, 704, 84
38669, V, 1, 1, 1, 1, 0, 704, 84
38670, V, 1, 1, 1, 1, 0, 704, 85
38671, V, 1, 1, 1, 1, 0, 704, 85
38672, V, 1, 1, 1, 1, 0, 704, 86
38673, V, 1, 1, 1, 1, 0, 704, 86
38674, V, 1, 1, 1, 1, 0, 704, 86
38675, V, 1, 1, 1, 1, 0, 704, 87
38676, V, 1, 1, 1, 1, 0, 704, 87
38677, V, 1, 1, 1, 1, 0, 704, 87
38678, V, 1, 1, 1, 1, 0, 704, 88
38679, V, 1, 1, 1, 1, 0, 704, 88
38680, V, 1, 1, 1, 1, 0, 704, 88
38681, V, 1, 1, 1, 1, 0, 704, 89
38682, V, 1, 1, 1, 1, 0, 704, 89
38683, V, 1, 1, 1, 1, 0, 704, 89
38684, V, 1, 1, 1, 1, 0, 704, 89
38685, V, 1, 1, 1, 1, 0, 704, 90
38686, V, 1, 1, 1, 1, 0, 704, 90
38687, V, 1, 1, 1, 1, 0, 704, 90
38688, V, 1, 1, 1, 1, 0, 704, 90
38689, V, 1, 1, 1, 1, 0, 704, 91
38690, V, 1, 1, 1, 1, 0, 704, 91
38691, V, 1, 1, 1, 1, 0, 704, 91
38692, V, 1, 1, 1, 1, 0, 704, 91
38693, V, 1, 1, 1, 1, 0, 704, 91
38694, V, 1, 1, 1, 1, 0, 704, 92
38695, V, 1, 1, 1, 1, 0, 704, 92
38696, V, 1, 1, 1, 1, 0, 704, 92
38697, V, 1, 1, 1, 1, 0, 704, 92
38699, V, 1, 1, 1, 1, 0, 704, 92
38700, V, 1, 1, 1, 1, 0, 704, 93
38701, V, 1, 1, 1, 1, 0, 704, 93
38702, V, 1, 1, 1, 1, 0, 704, 93
38703, V, 1, 1, 1, 1, 0, 704, 93
38704, V, 1, 1, 1, 1, 0, 704, 93
38705, V, 1, 1, 1, 1, 0, 704, 93
38706, V, 1, 1, 1, 1, 0, 704, 94
38707, V, 1, 1, 1, 1, 0, 704, 94
38708, V, 1, 1, 1, 1, 0, 704, 94
38709, V, 1, 1, 1, 1, 0, 704, 94
38710, V, 1, 1, 1, 1, 0, 704, 94
38711, V, 1, 1, 1, 1, 0, 704, 94
38712, V, 1, 1, 1, 1, 0, 704, 94
38713, V, 1, 1, 1, 1, 0, 704, 95
38714, V, 1, 1, 1, 1, 0, 704, 95
38715, V, 1, 1, 1, 1, 0, 704, 95
38716, V, 1, 1, 1, 1, 0, 704, 95
38717, V, 1, 1, 1, 1, 0, 704, 95
38718, V, 1, 1, 1, 1, 0, 704, 95
38719, V, 1, 1, 1, 1, 0, 704, 95
38720, V, 1, 1, 1, 1, 0, 704, 95
38721, V, 1, 1, 1, 1, 0, 704, 95
38722, V, 1, 1, 1, 1, 0, 704, 95
38723, V, 1, 1, 1, 1, 0, 704, 96
38724, V, 1, 1, 1, 1, 0, 704, 96
38725, V, 1, 1, 1, 1, 0, 704, 96
38726, V, 1, 1, 1, 1, 0, 704, 96
38727, V, 1, 1, 1, 1, 0, 704, 96
38728, V, 1, 1, 1, 1, 0, 704, 96
38729, V, 1, 1, 1, 1, 0, 704, 96
38730, V, 1, 1, 1, 1, 0, 704, 96
38731, V, 1, 1, 1, 1, 0, 704, 96
38732, V, 1, 1, 1, 1, 0, 704, 96
38733, V, 1, 1, 1, 1, 0, 704, 96
38734, V, 1, 1, 1, 1, 0, 704, 96
38735, V, 1, 1, 1, 1, 0, 704, 97
38736, V, 1, 1, 1, 1, 0, 704, 97
38737, V, 1, 1, 1, 1, 0, 704, 97
38738, V, 1, 1, 1, 1, 0, 704, 97
38739, V, 1, 1, 1, 1, 0, 704, 97
38740, V, 1, 1, 1, 1, 0, 704, 97
38742, V, 1, 1, 1, 1, 0, 704, 97
38743, V, 1, 1, 1, 1, 0, 704, 97
38744, V, 1, 1, 1, 1, 0, 704, 97
38745, V, 1, 1, 1, 1, 0, 704, 97
38746, V, 1, 1, 1, 1, 0, 704, 97
38747, V, 1, 1, 1, 1, 0, 704, 97
38748, V, 1, 1, 1, 1, 0, 704, 97
38749, V, 1, 1, 1, 1, 0, 704, 97
38750, V, 1, 1, 1, 1, 0, 704, 97
38751, V, 1, 1, 1, 1, 0, 704, 97
38752, V, 1, 1, 1, 1, 0, 704, 97
38753, V, 1, 1, 1, 1, 0, 704, 97
38754, V, 1, 1, 1, 1, 0, 704, 97
38755, V, 1, 1, 1, 1, 0, 704, 98
38756, V, 1, 1, 1, 1, 0, 704, 98
38757, V, 1, 1, 1, 1, 0, 704, 98
38758, V, 1, 1, 1, 1, 0, 704, 98
38759, V, 1, 1, 1, 1, 0, 704, 98
38760, V, 1, 1, 1, 1, 0, 704, 98
38761, V, 1, 1, 1, 1, 0, 704, 98
38762, V, 1, 1, 1, 1, 0, 704, 98
38763, V, 1, 1, 1, 1, 0, 704, 98
38764, V, 1, 1, 1, 1, 0, 704, 98
38765, V, 1, 1, 1, 1, 0, 704, 98
38766, V, 1, 1, 1, 1, 0, 704, 98
38767, V, 1, 1, 1, 1, 0, 704, 98
38768, V, 1, 1, 1, 1, 0, 704, 98
38769, V, 1, 1, 1, 1, 0, 704, 98
38770, V, 1, 1, 1, 1, 0, 704, 98
38771, V, 1, 1, 1, 1, 0, 704, 98
38772, V, 1, 1, 1, 1, 0, 704, 98
38773, V, 1, 1, 1, 1, 0, 704, 98
38774, V, 1, 1, 1, 1, 0, 704, 98
38775, V, 1, 1, 1, 1, 0, 704, 98
38776, V, 1, 1, 1, 1, 0, 704, 98
38777, V, 1, 1, 1, 1, 0, 704, 98
38778, V, 1, 1, 1, 1, 0, 704, 98
38779, V, 1, 1, 1, 1, 0, 704, 98
38780, V, 1, 1, 1, 1, 0, 704, 98
38781, V, 1, 1, 1, 1, 0, 704, 98
38782, V, 1, 1, 1, 1, 0, 704, 98
38784, V, 1, 1, 1, 1, 0, 704, 98
38785, V, 1, 1, 1, 1, 0, 704, 98
38786, V, 1, 1, 1, 1, 0, 704, 98
38787, V, 1, 1, 1, 1, 0, 704, 98
38788, V, 1, 1, 1, 1, 0, 704, 98
38789, V, 1, 1, 1, 1, 0, 704, 98
38790, V, 1, 1, 1, 1, 0, 704, 98
38791, V, 1, 1, 1, 1, 0, 704, 98
38792, V, 1, 1, 1, 1, 0, 704, 98
38793, V, 1, 1, 1, 1, 0, 704, 98
38794, V, 1, 1, 1, 1, 0, 704, 98
38795, V, 1, 1, 1, 1, 0, 704, 98
38796, V, 1, 1, 1, 1, 0, 704, 98
38797, V, 1, 1, 1, 1, 0, 704, 98
38798, V, 1, 1, 1, 1, 0, 704, 98
38799, V, 1, 1, 1, 1, 0, 704, 98
38800, V, 1, 1, 1, 1, 0, 704, 98
38801, V, 1, 1, 1, 1, 0, 704, 98
38802, V, 1, 1, 1, 1, 0, 704, 98
38803, V, 1, 1, 1, 1, 0, 704, 99
38804, V, 1, 1, 1, 1, 0, 704, 99
38805, V, 1, 1, 1, 1, 0, 704, 99
38806, V, 1, 1, 1, 1, 0, 704, 99
38807, V, 1, 1, 1, 1, 0, 704, 99
38808, V, 1, 1, 1, 1, 0, 704, 99
38809, V, 1, 1, 1, 1, 0, 704, 99
38810, V, 1, 1, 1, 1, 0, 704, 99
38811, V, 1, 1, 1, 1, 0, 704, 99
38812, V, 1, 1, 1, 1, 0, 704, 99
38813, V, 1, 1, 1, 1, 0, 704, 99
38814, V, 1, 1, 1, 1, 0, 704, 99
38815, V, 1, 1, 1, 1, 0, 704, 99
38816, V, 1, 1, 1, 1, 0, 704, 99
38817, V, 1, 1, 1, 1, 0, 704, 99
38818, V, 1, 1, 1, 1, 0, 704, 99
38819, V, 1, 1, 1, 1, 0, 704, 99
38820, V, 1, 1, 1, 1, 0, 704, 99
38821, V, 1, 1, 1, 1, 0, 704, 99
38822, V, 1, 1, 1, 1, 0, 704, 99
38823, V, 1, 1, 1, 1, 0, 704, 99
38824, V, 1, 1, 1, 1, 0, 704, 99
38825, V, 1, 1, 1, 1, 0, 704, 99
38827, V, 1, 1, 1, 1, 0, 704, 99
38828, V, 1, 1, 1, 1, 0, 704, 99
38829, V, 1, 1, 1, 1, 0, 704, 99
38830, V, 1, 1, 1, 1, 0, 704, 99
38831, V, 1, 1, 1, 1, 0, 704, 99
38832, V, 1, 1, 1, 1, 0, 704, 99
38833, V, 1, 1, 1, 1, 0, 704, 99
38834, V, 1, 1, 1, 1, 0, 704, 99
38835, V, 1, 1, 1, 1, 0, 704, 99
38836, V, 1, 1, 1, 1, 0, 704, 99
38837, V, 1, 1, 1, 1, 0, 704, 99
38838, V, 1, 1, 1, 1, 0, 704, 99
38839, V, 1, 1, 1, 1, 0, 704, 99
38840, V, 1, 1, 1, 1, 0, 704, 99
38841, V, 1, 1, 1, 1, 0, 704, 99
38842, V, 1, 1, 1, 1, 0, 704, 99
38843, V, 1, 1, 1, 1, 0, 704, 99
38844, V, 1, 1, 1, 1, 0, 704, 99
38845, V, 1, 1, 1, 1, 0, 704, 99
38846, V, 1, 1, 1, 1, 0, 704, 99
38847, V, 1, 1, 1, 1, 0, 704, 99
38848, V, 1, 1, 1, 1, 0, 704, 99
38849, V, 1, 1, 1, 1, 0, 704, 99
38850, V, 1, 1, 1, 1, 0, 704, 99
38851, V, 1, 1, 1, 1, 0, 704, 99
38852, V, 1, 1, 1, 1, 0, 704, 99
38853, V, 1, 1, 1, 1, 0, 704, 99
38854, V, 1, 1, 1, 1, 0, 704, 99
38855, V, 1, 1, 1, 1, 0, 704, 99
38856, V, 1, 1, 1, 1, 0, 704, 99
38857, V, 1, 1, 1, 1, 0, 704, 99
38858, V, 1, 1, 1, 1, 0, 704, 99
38859, V, 1, 1, 1, 1, 0, 704, 99
38860, V, 1, 1, 1, 1, 0, 704, 99
38861, V, 1, 1, 1, 1, 0, 704, 99
38862, V, 1, 1, 1, 1, 0, 704, 99
38863, V, 1, 1, 1, 1, 0, 704, 99
38864, V, 1, 1, 1, 1, 0, 704, 99
38865, V, 1, 1, 1, 1, 0, 704, 99
38866, V, 1, 1, 1, 1, 0, 704, 99
38867, V, 1, 1, 1, 1, 0, 704, 99
38868, V, 1, 1, 1, 1, 0, 704, 99
38870, V, 1, 1, 1, 1, 0, 704, 99
38871, V, 1, 1, 1, 1, 0, 704, 99
38872, V, 1, 1, 1, 1, 0, 704, 99
38873, V, 1, 1, 1, 1, 0, 704, 99
38874, V, 1, 1, 1, 1, 0, 704, 99
38875, V, 1, 1, 1, 1, 0, 704, 99
38876, V, 1, 1, 1, 1, 0, 704, 99
38877, V, 1, 1, 1, 1, 0, 704, 99
38878, V, 1, 1, 1, 1, 0, 704, 99
38879, V, 1, 1, 1, 1, 0, 704, 99
38880, V, 1, 1, 1, 1, 0, 704, 99
38881, V, 1, 1, 1, 1, 0, 704, 99
38882, V, 1, 1, 1, 1, 0, 704, 99
38883, V, 1, 1, 1, 1, 0, 704, 99
38884, V, 1, 1, 1, 1, 0, 704, 99
38885, V, 1, 1, 1, 1, 0, 704, 99
38886, V, 1, 1, 1, 1, 0, 704, 99
38887, V, 1, 1, 1, 1, 0, 704, 99
38888, V, 1, 1, 1, 1, 0, 704, 99
38889, V, 1, 1, 1, 1, 0, 704, 99
38890, V, 1, 1, 1, 1, 0, 704, 99
38891, V, 1, 1, 1, 1, 0, 704, 99
38892, V, 1, 1, 1, 1, 0, 704, 99
38893, V, 1, 1, 1, 1, 0, 704, 99
38894, V, 1, 1, 1, 1, 0, 704, 99
38895, V, 1, 1, 1, 1, 0, 704, 99
38896, V, 1, 1, 1, 1, 0, 704, 99
38897, V, 1, 1, 1, 1, 0, 704, 99
38898, V, 1, 1, 1, 1, 0, 704, 99
38899, V, 1, 1, 1, 1, 0, 704, 99
38900, V, 1, 1, 1, 1, 0, 704, 99
38901, V, 1, 1, 1, 1, 0, 704, 99
38902, V, 1, 1, 1, 1, 0, 704, 99
38903, V, 1, 1, 1, 1, 0, 704, 99
38904, V, 1, 1, 1, 1, 0, 704, 99
38905, V, 1, 1, 1, 1, 0, 704, 99
38906, V, 1, 1, 1, 1, 0, 704, 99
38907, V, 1, 1, 1, 1, 0, 704, 99
38908, V, 1, 1, 1, 1, 0, 704, 99
38909, V, 1, 1, 1, 1, 0, 704, 99
38910, V, 1, 1, 1, 1, 0, 704, 99
38912, V, 1, 1, 1, 1, 0, 704, 99
38913, V, 1, 1, 1, 1, 0, 704, 99
38914, V, 1, 1, 1, 1, 0, 704, 99
38915, V, 1, 1, 1, 1, 0, 704, 99
38916, V, 1, 1, 1, 1, 0, 704, 99
38917, V, 1, 1, 1, 1, 0, 704, 99
38918, V, 1, 1, 1, 1, 0, 704, 99
38919, V, 1, 1, 1, 1, 0, 704, 99
38920, V, 1, 1, 1, 1, 0, 704, 99
38921, V, 1, 1, 1, 1, 0, 704, 99
38922, V, 1, 1, 1, 1, 0, 704, 99
38923, V, 1, 1, 1, 1, 0, 704, 99
38924, V, 1, 1, 1, 1, 0, 704, 99
38925, V, 1, 1, 1, 1, 0, 704, 99
38926, V, 1, 1, 1, 1, 0, 704, 99
38927, V, 1, 1, 1, 1, 0, 704, 99
38928, V, 1, 1, 1, 1, 0, 704, 99
38929, V, 1, 1, 1, 1, 0, 704, 99
38930, V, 1, 1, 1, 1, 0, 704, 99
38931, V, 1, 1, 1, 1, 0, 704, 99
38932, V, 1, 1, 1, 1, 0, 704, 99
38933, V, 1, 1, 1, 1, 0, 704, 99
38934, V, 1, 1, 1, 1, 0, 704, 99
38935, V, 1, 1, 1, 1, 0, 704, 99
38936, V, 1, 1, 1, 1, 0, 704, 99
38937, V, 1, 1, 1, 1, 0, 704, 99
38938, V, 1, 1, 1, 1, 0, 704, 99
38939, V, 1, 1, 1, 1, 0, 704, 99
38940, V, 1, 1, 1, 1, 0, 704, 99
38941, V, 1, 1, 1, 1, 0, 704, 99
38942, V, 1, 1, 1, 1, 0, 704, 99
38943, V, 1, 1, 1, 1, 0, 704, 99
38944, V, 1, 1, 1, 1, 0, 704, 99
38945, V, 1, 1, 1, 1, 0, 704, 99
38946, V, 1, 1, 1, 1, 0, 704, 99
38947, V, 1, 1, 1, 1, 0, 704, 99
38948, V, 1, 1, 1, 1, 0, 704, 99
38949, V, 1, 1, 1, 1, 0, 704, 99
38950, V, 1, 1, 1, 1, 0, 704, 99
38951, V, 1, 1, 1, 1, 0, 704, 99
38952, V, 1, 1, 1, 1, 0, 704, 99
38953, V, 1, 1, 1, 1, 0, 704, 99
38955, V, 1, 1, 1, 1, 0, 704, 99
38956, V, 1, 1, 1, 1, 0, 704, 99
38957, V, 1, 1, 1, 1, 0, 704, 99
38958, V, 1, 1, 1, 1, 0, 704, 99
38959, V, 1, 1, 1, 1, 0, 704, 99
38960, V, 1, 1, 1, 1, 0, 704, 99
38961, V, 1, 1, 1, 1, 0, 704, 99
38962, V, 1, 1, 1, 1, 0, 704, 99
38963, V, 1, 1, 1, 1, 0, 704, 99
38964, V, 1, 1, 1, 1, 0, 704, 99
38965, V, 1, 1, 1, 1, 0, 704, 99
38966, V, 1, 1, 1, 1, 0, 704, 99
38967, V, 1, 1, 1, 1, 0, 704, 99
38968, V, 1, 1, 1, 1, 0, 704, 99
38969, V, 1, 1, 1, 1, 0, 704, 99
38970, V, 1, 1, 1, 1, 0, 704, 99
38971, V, 1, 1, 1, 1, 0, 704, 99
38972, V, 1, 1, 1, 1, 0, 704, 99
38973, V, 1, 1, 1, 1, 0, 704, 99
38974, V, 1, 1, 1, 1, 0, 704, 99
38975, V, 1, 1, 1, 1, 0, 704, 99
38976, V, 1, 1, 1, 1, 0, 704, 99
38977, V, 1, 1, 1, 1, 0, 704, 99
38978, V, 1, 1, 1, 1, 0, 704, 99
38979, V, 1, 1, 1, 1, 0, 704, 99
38980, V, 1, 1, 1, 1, 0, 704, 99
38981, V, 1, 1, 1, 1, 0, 704, 99
38982, V, 1, 1, 1, 1, 0, 704, 99
38983, V, 1, 1, 1, 1, 0, 704, 99
38984, V, 1, 1, 1, 1, 0, 704, 99
38985, V, 1, 1, 1, 1, 0, 704, 99
38986, V, 1, 1, 1, 1, 0, 704, 99
38987, V, 1, 1, 1, 1, 0, 704, 99
38988, V, 1, 1, 1, 1, 0, 704, 99
38989, V, 1, 1, 1, 1, 0, 704, 99
38990, V, 1, 1, 1, 1, 0, 704, 99
38991, V, 1, 1, 1, 1, 0, 704, 99
38992, V, 1, 1, 1, 1, 0, 704, 99
38993, V, 1, 1, 1, 1, 0, 704, 99
38994, V, 1, 1, 1, 1, 0, 704, 99
38995, V, 1, 1, 1, 1, 0, 704, 99
38996, V, 1, 1, 1, 1, 0, 704, 99
38998, V, 1, 1, 1, 1, 0, 704, 99
38999, V, 1, 1, 1, 1, 0, 704, 99
39000, V, 1, 1, 1, 1, 0, 704, 99
39001, V, 1, 1, 1, 1, 0, 704, 99
39002, V, 1, 1, 1, 1, 0, 704, 99
39003, V, 1, 1, 1, 1, 0, 704, 99
39004, V, 1, 1, 1, 1, 0, 704, 99
39005, V, 1, 1, 1, 1, 0, 704, 99
39006, V, 1, 1, 1, 1, 0, 704, 99
39007, V, 1, 1, 1, 1, 0, 704, 99
39008, V, 1, 1, 1, 1, 0, 704, 99
39009, V, 1, 1, 1, 1, 0, 704, 99
39010, V, 1, 1, 1, 1, 0, 704, 99
39011, V, 1, 1, 1, 1, 0, 704, 99
39012, V, 1, 1, 1, 1, 0, 704, 99
39013, V, 1, 1, 1, 1, 0, 704, 99
39014, V, 1, 1, 1, 1, 0, 704, 99
39015, V, 1, 1, 1, 1, 0, 704, 99
39016, V, 1, 1, 1, 1, 0, 704, 99
39017, V, 1, 1, 1, 1, 0, 704, 99
39018, V, 1, 1, 1, 1, 0, 704, 99
39019, V, 1, 1, 1, 1, 0, 704, 99
39020, V, 1, 1, 1, 1, 0, 704, 99
39021, V, 1, 1, 1, 1, 0, 704, 99
39022, V, 1, 1, 1, 1, 0, 704, 99
39023, V, 1, 1, 1, 1, 0, 704, 99
39024, V, 1, 1, 1, 1, 0, 704, 99
39025, V, 1, 1, 1, 1, 0, 704, 99
39026, V, 1, 1, 1, 1, 0, 704, 99
39027, V, 1, 1, 1, 1, 0, 704, 100
39028, V, 1, 1, 1, 1, 0, 704, 99
39029, V, 1, 1, 1, 1, 0, 704, 99
39030, V, 1, 1, 1, 1, 0, 704, 99
39031, V, 1, 1, 1, 1, 0, 704, 99
39032, V, 1, 1, 1, 1, 0, 704, 100
39033, V, 1, 1, 1, 1, 0, 704, 100
39034, V, 1, 1, 1, 1, 0, 704, 100
39035, V, 1, 1, 1, 1, 0, 704, 100
39036, V, 1, 1, 1, 1, 0, 704, 100
39037, V, 1, 1, 1, 1, 0, 704, 100
39038, V, 1, 1, 1, 1, 0, 704, 99
39040, V, 1, 1, 1, 1, 0, 704, 100
39041, V, 1, 1, 1, 1, 0, 704, 100
39042, V, 1, 1, 1, 1, 0, 704, 100
39043, V, 1, 1, 1, 1, 0, 704, 100
39044, V, 1, 1, 1, 1, 0, 704, 100
39045, V, 1, 1, 1, 1, 0, 704, 100
39046, V, 1, 1, 1, 1, 0, 704, 100
39047, V, 1, 1, 1, 1, 0, 704, 100
39048, V, 1, 1, 1, 1, 0, 704, 100
39049, V, 1, 1, 1, 1, 0, 704, 100
39050, V, 1, 1, 1, 1, 0, 704, 100
39051, V, 1, 1, 1, 1, 0, 704, 100
39052, V, 1, 1, 1, 1, 0, 704, 100
39053, V, 1, 1, 1, 1, 0, 704, 100
39054, V, 1, 1, 1, 1, 0, 704, 100
39055, V, 1, 1, 1, 1, 0, 704, 100
39056, V, 1, 1, 1, 1, 0, 704, 100
39057, V, 1, 1, 1, 1, 0, 704, 100
39058, V, 1, 1, 1, 1, 0, 704, 100
39059, V, 1, 1, 1, 1, 0, 704, 100
39060, V, 1, 1, 1, 1, 0, 704, 100
39061, V, 1, 1, 1, 1, 0, 704, 100
39062, V, 1, 1, 1, 1, 0, 704, 100
39063, V, 1, 1, 1, 1, 0, 704, 100
39064, V, 1, 1, 1, 1, 0, 704, 100
39065, V, 1, 1, 1, 1, 0, 704, 100
39066, V, 1, 1, 1, 1, 0, 704, 100
39067, V, 1, 1, 1, 1, 0, 704, 100
39068, V, 1, 1, 1, 1, 0, 704, 100
39069, V, 1, 1, 1, 1, 0, 704, 100
39070, V, 1, 1, 1, 1, 0, 704, 100
39071, V, 1, 1, 1, 1, 0, 704, 100
39072, V, 1, 1, 1, 1, 0, 704, 100
39073, V, 1, 1, 1, 1, 0, 704, 100
39074, V, 1, 1, 1, 1, 0, 704, 100
39075, V, 1, 1, 1, 1, 0, 704, 100
39076, V, 1, 1, 1, 1, 0, 704, 100
39077, V, 1, 1, 1, 1, 0, 704, 100
39078, V, 1, 1, 1, 1, 0, 704, 100
39079, V, 1, 1, 1, 1, 0, 704, 100
39080, V, 1, 1, 1, 1, 0, 704, 100
39081, V, 1, 1, 1, 1, 0, 704, 99
39083, V, 1, 1, 1, 1, 0, 704, 99
39084, V, 1, 1, 1, 1, 0, 704, 99
39085, V, 1, 1, 1, 1, 0, 704, 100
39086, V, 1, 1, 1, 1, 0, 704, 99
39087, V, 1, 1, 1, 1, 0, 704, 100
39088, V, 1, 1, 1, 1, 0, 704, 100
39089, V, 1, 1, 1, 1, 0, 704, 99
39090, V, 1, 1, 1, 1, 0, 704, 100
39091, V, 1, 1, 1, 1, 0, 704, 100
39092, V, 1, 1, 1, 1, 0, 704, 100
39093, V, 1, 1, 1, 1, 0, 704, 100
39094, V, 1, 1, 1, 1, 0, 704, 100
39095, V, 1, 1, 1, 1, 0, 704, 100
39096, V, 1, 1, 1, 1, 0, 704, 99
39097, V, 1, 1, 1, 1, 0, 704, 100
39098, V, 1, 1, 1, 1, 0, 704, 99
39099, V, 1, 1, 1, 1, 0, 704, 99
39100, V, 1, 1, 1, 1, 0, 704, 100
39101, V, 1, 1, 1, 1, 0, 704, 100
39102, V, 1, 1, 1, 1, 0, 704, 100
39103, V, 1, 1, 1, 1, 0, 704, 99
39104, V, 1, 1, 1, 1, 0, 704, 100
39105, V, 1, 1, 1, 1, 0, 704, 100
39106, V, 1, 1, 1, 1, 0, 704, 100
39107, V, 1, 1, 1, 1, 0, 704, 100
39108, V, 1, 1, 1, 1, 0, 704, 100
39109, V, 1, 1, 1, 1, 0, 704, 100
39110, V, 1, 1, 1, 1, 0, 704, 100
39111, V, 1, 1, 1, 1, 0, 704, 100
39112, V, 1, 1, 1, 1, 0, 704, 100
39113, V, 1, 1, 1, 1, 0, 704, 100
39114, V, 1, 1, 1, 1, 0, 704, 100
39115, V, 1, 1, 1, 1, 0, 704, 100
39116, V, 1, 1, 1, 1, 0, 704, 100
39117, V, 1, 1, 1, 1, 0, 704, 100
39118, V, 1, 1, 1, 1, 0, 704, 100
39119, V, 1, 1, 1, 1, 0, 704, 100
39120, V, 1, 1, 1, 1, 0, 704, 100
39121, V, 1, 1, 1, 1, 0, 704, 100
39122, V, 1, 1, 1, 1, 0, 704, 100
39123, V, 1, 1, 1, 1, 0, 704, 100
39124, V, 1, 1, 1, 1, 0, 704, 100
39126, V, 1, 1, 1, 1, 0, 704, 100
39127, V, 1, 1, 1, 1, 0, 704, 100
39128, V, 1, 1, 1, 1, 0, 704, 100
39129, V, 1, 1, 1, 1, 0, 704, 100
39130, V, 1, 1, 1, 1, 0, 704, 100
39131, V, 1, 1, 1, 1, 0, 704, 100
39132, V, 1, 1, 1, 1, 0, 704, 100
39133, V, 1, 1, 1, 1, 0, 704, 100
39134, V, 1, 1, 1, 1, 0, 704, 100
39135, V, 1, 1, 1, 1, 0, 704, 100
39136, V, 1, 1, 1, 1, 0, 704, 100
39137, V, 1, 1, 1, 1, 0, 704, 100
39138, V, 1, 1, 1, 1, 0, 704, 100
39139, V, 1, 1, 1, 1, 0, 704, 100
39140, V, 1, 1, 1, 1, 0, 704, 100
39141, V, 1, 1, 1, 1, 0, 704, 100
39142, V, 1, 1, 1, 1, 0, 704, 100
39143, V, 1, 1, 1, 1, 0, 704, 100
39144, V, 1, 1, 1, 1, 0, 704, 100
39145, V, 1, 1, 1, 1, 0, 704, 100
39146, V, 1, 1, 1, 1, 0, 704, 100
39147, V, 1, 1, 1, 1, 0, 704, 100
39148, V, 1, 1, 1, 1, 0, 704, 99
39149, V, 1, 1, 1, 1, 0, 704, 100
39150, V, 1, 1, 1, 1, 0, 704, 99
39151, V, 1, 1, 1, 1, 0, 704, 99
39152, V, 1, 1, 1, 1, 0, 704, 99
39153, V, 1, 1, 1, 1, 0, 704, 99
39154, V, 1, 1, 1, 1, 0, 704, 99
39155, V, 1, 1, 1, 1, 0, 704, 99
39156, V, 1, 1, 1, 1, 0, 704, 99
39157, V, 1, 1, 1, 1, 0, 704, 99
39158, V, 1, 1, 1, 1, 0, 704, 99
39159, V, 1, 1, 1, 1, 0, 704, 99
39160, V, 1, 1, 1, 1, 0, 704, 99
39161, V, 1, 1, 1, 1, 0, 704, 99
39162, V, 1, 1, 1, 1, 0, 704, 99
39163, V, 1, 1, 1, 1, 0, 704, 99
39164, V, 1, 1, 1, 1, 0, 704, 99
39165, V, 1, 1, 1, 1, 0, 704, 99
39166, V, 1, 1, 1, 1, 0, 704, 99
39168, V, 1, 1, 1, 1, 0, 704, 99
39169, V, 1, 1, 1, 1, 0, 704, 99
39170, V, 1, 1, 1, 1, 0, 704, 99
39171, V, 1, 1, 1, 1, 0, 704, 99
39172, V, 1, 1, 1, 1, 0, 704, 99
39173, V, 1, 1, 1, 1, 0, 704, 99
39174, V, 1, 1, 1, 1, 0, 704, 99
39175, V, 1, 1, 1, 1, 0, 704, 99
39176, V, 1, 1, 1, 1, 0, 704, 99
39177, V, 1, 1, 1, 1, 0, 704, 99
39178, V, 1, 1, 1, 1, 0, 704, 99
39179, V, 1, 1, 1, 1, 0, 704, 99
39180, V, 1, 1, 1, 1, 0, 704, 99
39181, V, 1, 1, 1, 1, 0, 704, 99
39182, V, 1, 1, 1, 1, 0, 704, 99
39183, V, 1, 1, 1, 1, 0, 704, 99
39184, V, 1, 1, 1, 1, 0, 704, 99
39185, V, 1, 1, 1, 1, 0, 704, 99
39186, V, 1, 1, 1, 1, 0, 704, 99
39187, V, 1, 1, 1, 1, 0, 704, 99
39188, V, 1, 1, 1, 1, 0, 704, 99
39189, V, 1, 1, 1, 1, 0, 704, 99
39190, V, 1, 1, 1, 1, 0, 704, 99
39191, V, 1, 1, 1, 1, 0, 704, 99
39192, V, 1, 1, 1, 1, 0, 704, 99
39193, V, 1, 1, 1, 1, 0, 704, 99
39194, V, 1, 1, 1, 1, 0, 704, 99
39195, V, 1, 1, 1, 1, 0, 704, 99
39196, V, 1, 1, 1, 1, 0, 704, 99
39197, V, 1, 1, 1, 1, 0, 704, 99
39198, V, 1, 1, 1, 1, 0, 704, 99
39199, V, 1, 1, 1, 1, 0, 704, 99
39200, V, 1, 1, 1, 1, 0, 704, 99
39201, V, 1, 1, 1, 1, 0, 704, 100
39202, V, 1, 1, 1, 1, 0, 704, 99
39203, V, 1, 1, 1, 1, 0, 704, 100
39204, V, 1, 1, 1, 1, 0, 704, 99
39205, V, 1, 1, 1, 1, 0, 704, 100
39206, V, 1, 1, 1, 1, 0, 704, 100
39207, V, 1, 1, 1, 1, 0, 704, 100
39208, V, 1, 1, 1, 1, 0, 704, 100
39209, V, 1, 1, 1, 1, 0, 704, 100
39211, V, 1, 1, 1, 1, 0, 704, 100
39212, V, 1, 1, 1, 1, 0, 704, 100
39213, V, 1, 1, 1, 1, 0, 704, 100
39214, V, 1, 1, 1, 1, 0, 704, 100
39215, V, 1, 1, 1, 1, 0, 704, 100
39216, V, 1, 1, 1, 1, 0, 704, 100
39217, V, 1, 1, 1, 1, 0, 704, 100
39218, V, 1, 1, 1, 1, 0, 704, 100
39219, V, 1, 1, 1, 1, 0, 704, 100
39220, V, 1, 1, 1, 1, 0, 704, 100
39221, V, 1, 1, 1, 1, 0, 704, 100
39222, V, 1, 1, 1, 1, 0, 704, 100
39223, V, 1, 1, 1, 1, 0, 704, 100
39224, V, 1, 1, 1, 1, 0, 704, 100
39225, V, 1, 1, 1, 1, 0, 704, 100
39226, V, 1, 1, 1, 1, 0, 704, 100
39227, V, 1, 1, 1, 1, 0, 704, 100
39228, V, 1, 1, 1, 1, 0, 704, 100
39229, V, 1, 1, 1, 1, 0, 704, 100
39230, V, 1, 1, 1, 1, 0, 704, 100
39231, V, 1, 1, 1, 1, 0, 704, 100
39232, V, 1, 1, 1, 1, 0, 704, 100
39233, V, 1, 1, 1, 1, 0, 704, 100
39234, V, 1, 1, 1, 1, 0, 704, 100
39235, V, 1, 1, 1, 1, 0, 704, 100
39236, V, 1, 1, 1, 1, 0, 704, 100
39237, V, 1, 1, 1, 1, 0, 704, 100
39238, V, 1, 1, 1, 1, 0, 704, 100
39239, V, 1, 1, 1, 1, 0, 704, 100
39240, V, 1, 1, 1, 1, 0, 704, 100
39241, V, 1, 1, 1, 1, 0, 704, 100
39242, V, 1, 1, 1, 1, 0, 704, 100
39243, V, 1, 1, 1, 1, 0, 704, 100
39244, V, 1, 1, 1, 1, 0, 704, 100
39245, V, 1, 1, 1, 1, 0, 704, 100
39246, V, 1, 1, 1, 1, 0, 704, 100
39247, V, 1, 1, 1, 1, 0, 704, 100
39248, V, 1, 1, 1, 1, 0, 704, 100
39249, V, 1, 1, 1, 1, 0, 704, 100
39250, V, 1, 1, 1, 1, 0, 704, 100
39251, V, 1, 1, 1, 1, 0, 704, 100
39252, V, 1, 1, 1, 1, 0, 704, 100
39254, V, 1, 1, 1, 1, 0, 704, 100
39255, V, 1, 1, 1, 1, 0, 704, 100
39256, V, 1, 1, 1, 1, 0, 704, 100
39257, V, 1, 1, 1, 1, 0, 704, 100
39258, V, 1, 1, 1, 1, 0, 704, 100
39259, V, 1, 1, 1, 1, 0, 704, 100
39260, V, 1, 1, 1, 1, 0, 704, 100
39261, V, 1, 1, 1, 1, 0, 704, 100
39262, V, 1, 1, 1, 1, 0, 704, 100
39263, V, 1, 1, 1, 1, 0, 704, 100
39264, V, 1, 1, 1, 1, 0, 704, 100
39265, V, 1, 1, 1, 1, 0, 704, 100
39266, V, 1, 1, 1, 1, 0, 704, 100
39267, V, 1, 1, 1, 1, 0, 704, 100
39268, V, 1, 1, 1, 1, 0, 704, 100
39269, V, 1, 1, 1, 1, 0, 704, 100
39270, V, 1, 1, 1, 1, 0, 704, 100
39271, V, 1, 1, 1, 1, 0, 704, 100
39272, V, 1, 1, 1, 1, 0, 704, 100
39273, V, 1, 1, 1, 1, 0, 704, 100
39274, V, 1, 1, 1, 1, 0, 704, 100
39275, V, 1, 1, 1, 1, 0, 704, 100
39276, V, 1, 1, 1, 1, 0, 704, 100
39277, V, 1, 1, 1, 1, 0, 704, 100
39278, V, 1, 1, 1, 1, 0, 704, 100
39279, V, 1, 1, 1, 1, 0, 704, 100
39280, V, 1, 1, 1, 1, 0, 704, 100
39281, V, 1, 1, 1, 1, 0, 704, 100
39282, V, 1, 1, 1, 1, 0, 704, 100
39283, V, 1, 1, 1, 1, 0, 704, 100
39284, V, 1, 1, 1, 1, 0, 704, 100
39285, V, 1, 1, 1, 1, 0, 704, 100
39286, V, 1, 1, 1, 1, 0, 704, 100
39287, V, 1, 1, 1, 1, 0, 704, 100
39288, V, 1, 1, 1, 1, 0, 704, 100
39289, V, 1, 1, 1, 1, 0, 704, 100
39290, V, 1, 1, 1, 1, 0, 704, 100
39291, V, 1, 1, 1, 1, 0, 704, 100
39292, V, 1, 1, 1, 1, 0, 704, 100
39293, V, 1, 1, 1, 1, 0, 704, 100
39294, V, 1, 1, 1, 1, 0, 704, 100
39296, V, 1, 1, 1, 1, 0, 704, 100
39297, V, 1, 1, 1, 1, 0, 704, 100
39298, V, 1, 1, 1, 1, 0, 704, 100
39299, V, 1, 1, 1, 1, 0, 704, 100
39300, V, 1, 1, 1, 1, 0, 704, 100
39301, V, 1, 1, 1, 1, 0, 704, 100
39302, V, 1, 1, 1, 1, 0, 704, 100
39303, V, 1, 1, 1, 1, 0, 704, 100
39304, V, 1, 1, 1, 1, 0, 704, 100
39305, V, 1, 1, 1, 1, 0, 704, 100
39306, V, 1, 1, 1, 1, 0, 704, 100
39307, V, 1, 1, 1, 1, 0, 704, 100
39308, V, 1, 1, 1, 1, 0, 704, 100
39309, V, 1, 1, 1, 1, 0, 704, 100
39310, V, 1, 1, 1, 1, 0, 704, 100
39311, V, 1, 1, 1, 1, 0, 704, 100
39312, V, 1, 1, 1, 1, 0, 704, 100
39313, V, 1, 1, 1, 1, 0, 704, 100
39314, V, 1, 1, 1, 1, 0, 704, 100
39315, V, 1, 1, 1, 1, 0, 704, 100
39316, V, 1, 1, 1, 1, 0, 704, 100
39317, V, 1, 1, 1, 1, 0, 704, 100
39318, V, 1, 1, 1, 1, 0, 704, 100
39319, V, 1, 1, 1, 1, 0, 704, 100
39320, V, 1, 1, 1, 1, 0, 704, 100
39321, V, 1, 1, 1, 1, 0, 704, 100
39322, V, 1, 1, 1, 1, 0, 704, 100
39323, V, 1, 1, 1, 1, 0, 704, 100
39324, V, 1, 1, 1, 1, 0, 704, 100
39325, V, 1, 1, 1, 1, 0, 704, 100
39326, V, 1, 1, 1, 1, 0, 704, 100
39327, V, 1, 1, 1, 1, 0, 704, 100
39328, V, 1, 1, 1, 1, 0, 704, 100
39329, V, 1, 1, 1, 1, 0, 704, 100
39330, V, 1, 1, 1, 1, 0, 704, 100
39331, V, 1, 1, 1, 1, 0, 704, 100
39332, V, 1, 1, 1, 1, 0, 704, 100
39333, V, 1, 1, 1, 1, 0, 704, 100
39334, V, 1, 1, 1, 1, 0, 704, 100
39335, V, 1, 1, 1, 1, 0, 704, 100
39336, V, 1, 1, 1, 1, 0, 704, 100
39337, V, 1, 1, 1, 1, 0, 704, 100
39339, V, 1, 1, 1, 1, 0, 704, 100
39340, V, 1, 1, 1, 1, 0, 704, 100
39341, V, 1, 1, 1, 1, 0, 704, 100
39342, V, 1, 1, 1, 1, 0, 704, 100
39343, V, 1, 1, 1, 1, 0, 704, 100
39344, V, 1, 1, 1, 1, 0, 704, 100
39345, V, 1, 1, 1, 1, 0, 704, 100
39346, V, 1, 1, 1, 1, 0, 704, 100
39347, V, 1, 1, 1, 1, 0, 704, 100
39348, V, 1, 1, 1, 1, 0, 704, 100
39349, V, 1, 1, 1, 1, 0, 704, 100
39350, V, 1, 1, 1, 1, 0, 704, 100
39351, V, 1, 1, 1, 1, 0, 704, 100
39352, V, 1, 1, 1, 1, 0, 704, 100
39353, V, 1, 1, 1, 1, 0, 704, 100
39354, V, 1, 1, 1, 1, 0, 704, 100
39355, V, 1, 1, 1, 1, 0, 704, 100
39356, V, 1, 1, 1, 1, 0, 704, 100
39357, V, 1, 1, 1, 1, 0, 704, 100
39358, V, 1, 1, 1, 1, 0, 704, 100
39359, V, 1, 1, 1, 1, 0, 704, 100
39360, V, 1, 1, 1, 1, 0, 704, 100
39361, V, 1, 1, 1, 1, 0, 704, 100
39362, V, 1, 1, 1, 1, 0, 704, 100
39363, V, 1, 1, 1, 1, 0, 704, 100
39364, V, 1, 1, 1, 1, 0, 704, 100
39365, V, 1, 1, 1, 1, 0, 704, 100
39366, V, 1, 1, 1, 1, 0, 704, 100
39367, V, 1, 1, 1, 1, 0, 704, 100
39368, V, 1, 1, 1, 1, 0, 704, 100
39369, V, 1, 1, 1, 1, 0, 704, 100
39370, V, 1, 1, 1, 1, 0, 704, 100
39371, V, 1, 1, 1, 1, 0, 704, 100
39372, V, 1, 1, 1, 1, 0, 704, 100
39373, V, 1, 1, 1, 1, 0, 704, 100
39374, V, 1, 1, 1, 1, 0, 704, 100
39375, V, 1, 1, 1, 1, 0, 704, 100
39376, V, 1, 1, 1, 1, 0, 704, 100
39377, V, 1, 1, 1, 1, 0, 704, 100
39378, V, 1, 1, 1, 1, 0, 704, 100
39379, V, 1, 1, 1, 1, 0, 704, 100
39380, V, 1, 1, 1, 1, 0, 704, 100
39382, V, 1, 1, 1, 1, 0, 704, 100
39383, V, 1, 1, 1, 1, 0, 704, 100
39384, V, 1, 1, 1, 1, 0, 704, 100
39385, V, 1, 1, 1, 1, 0, 704, 100
39386, V, 1, 1, 1, 1, 0, 704, 100
39387, V, 1, 1, 1, 1, 0, 704, 100
39388, V, 1, 1, 1, 1, 0, 704, 100
39389, V, 1, 1, 1, 1, 0, 704, 100
39390, V, 1, 1, 1, 1, 0, 704, 100
39391, V, 1, 1, 1, 1, 0, 704, 100
39392, V, 1, 1, 1, 1, 0, 704, 100
39393, V, 1, 1, 1, 1, 0, 704, 100
39394, V, 1, 1, 1, 1, 0, 704, 100
39395, V, 1, 1, 1, 1, 0, 704, 100
39396, V, 1, 1, 1, 1, 0, 704, 100
39397, V, 1, 1, 1, 1, 0, 704, 100
39398, V, 1, 1, 1, 1, 0, 704, 100
39399, V, 1, 1, 1, 1, 0, 704, 100
39400, V, 1, 1, 1, 1, 0, 704, 100
39401, V, 1, 1, 1, 1, 0, 704, 100
39402, V, 1, 1, 1, 1, 0, 704, 100
39403, V, 1, 1, 1, 1, 0, 704, 100
39404, V, 1, 1, 1, 1, 0, 704, 100
39405, V, 1, 1, 1, 1, 0, 704, 100
39406, V, 1, 1, 1, 1, 0, 704, 100
39407, V, 1, 1, 1, 1, 0, 704, 100
39408, V, 1, 1, 1, 1, 0, 704, 100
39409, V, 1, 1, 1, 1, 0, 704, 100
39410, V, 1, 1, 1, 1, 0, 704, 100
39411, V, 1, 1, 1, 1, 0, 704, 100
39412, V, 1, 1, 1, 1, 0, 704, 100
39413, V, 1, 1, 1, 1, 0, 704, 100
39414, V, 1, 1, 1, 1, 0, 704, 100
39415, V, 1, 1, 1, 1, 0, 704, 100
39416, V, 1, 1, 1, 1, 0, 704, 100
39417, V, 1, 1, 1, 1, 0, 704, 100
39418, V, 1, 1, 1, 1, 0, 704, 100
39419, V, 1, 1, 1, 1, 0, 704, 100
39420, V, 1, 1, 1, 1, 0, 704, 100
39421, V, 1, 1, 1, 1, 0, 704, 100
39422, V, 1, 1, 1, 1, 0, 704, 100
39424, V, 1, 1, 1, 1, 0, 704, 100
39425, V, 1, 1, 1, 1, 0, 704, 100
39426, V, 1, 1, 1, 1, 0, 704, 100
39427, V, 1, 1, 1, 1, 0, 704, 100
39428, V, 1, 1, 1, 1, 0, 704, 100
39429, V, 1, 1, 1, 1, 0, 704, 100
39430, V, 1, 1, 1, 1, 0, 704, 100
39431, V, 1, 1, 1, 1, 0, 704, 100
39432, V, 1, 1, 1, 1, 0, 704, 100
39433, V, 1, 1, 1, 1, 0, 704, 100
39434, V, 1, 1, 1, 1, 0, 704, 100
39435, V, 1, 1, 1, 1, 0, 704, 100
39436, V, 1, 1, 1, 1, 0, 704, 100
39437, V, 1, 1, 1, 1, 0, 704, 100
39438, V, 1, 1, 1, 1, 0, 704, 100
39439, V, 1, 1, 1, 1, 0, 704, 100
39440, V, 1, 1, 1, 1, 0, 704, 100
39441, V, 1, 1, 1, 1, 0, 704, 100
39442, V, 1, 1, 1, 1, 0, 704, 100
39443, V, 1, 1, 1, 1, 0, 704, 100
39444, V, 1, 1, 1, 1, 0, 704, 100
39445, V, 1, 1, 1, 1, 0, 704, 100
39446, V, 1, 1, 1, 1, 0, 704, 100
39447, V, 1, 1, 1, 1, 0, 704, 100
39448, V, 1, 1, 1, 1, 0, 704, 100
39449, V, 1, 1, 1, 1, 0, 704, 100
39450, V, 1, 1, 1, 1, 0, 704, 100
39451, V, 1, 1, 1, 1, 0, 704, 100
39452, V, 1, 1, 1, 1, 0, 704, 100
39453, V, 1, 1, 1, 1, 0, 704, 100
39454, V, 1, 1, 1, 1, 0, 704, 100
39455, V, 1, 1, 1, 1, 0, 704, 100
39456, V, 1, 1, 1, 1, 0, 704, 100
39457, V, 1, 1, 1, 1, 0, 704, 100
39458, V, 1, 1, 1, 1, 0, 704, 100
39459, V, 1, 1, 1, 1, 0, 704, 100
39460, V, 1, 1, 1, 1, 0, 704, 100
39461, V, 1, 1, 1, 1, 0, 704, 100
39462, V, 1, 1, 1, 1, 0, 704, 100
39463, V, 1, 1, 1, 1, 0, 704, 100
39464, V, 1, 1, 1, 1, 0, 704, 100
39465, V, 1, 1, 1, 1, 0, 704, 100
39467, V, 1, 1, 1, 1, 0, 704, 100
39468, V, 1, 1, 1, 1, 0, 704, 100
39469, V, 1, 1, 1, 1, 0, 704, 100
39470, V, 1, 1, 1, 1, 0, 704, 100
39471, V, 1, 1, 1, 1, 0, 704, 100
39472, V, 1, 1, 1, 1, 0, 704, 100
39473, V, 1, 1, 1, 1, 0, 704, 100
39474, V, 1, 1, 1, 1, 0, 704, 100
39475, V, 1, 1, 1, 1, 0, 704, 100
39476, V, 1, 1, 1, 1, 0, 704, 100
39477, V, 1, 1, 1, 1, 0, 704, 100
39478, V, 1, 1, 1, 1, 0, 704, 100
39479, V, 1, 1, 1, 1, 0, 704, 100
39480, V, 1, 1, 1, 1, 0, 704, 100
39481, V, 1, 1, 1, 1, 0, 704, 100
39482, V, 1, 1, 1, 1, 0, 704, 100
39483, V, 1, 1, 1, 1, 0, 704, 100
39484, V, 1, 1, 1, 1, 0, 704, 100
39485, V, 1, 1, 1, 1, 0, 704, 100
39486, V, 1, 1, 1, 1, 0, 704, 100
39487, V, 1, 1, 1, 1, 0, 704, 100
39488, V, 1, 1, 1, 1, 0, 704, 100
39489, V, 1, 1, 1, 1, 0, 704, 100
39490, V, 1, 1, 1, 1, 0, 704, 100
39491, V, 1, 1, 1, 1, 0, 704, 100
39492, V, 1, 1, 1, 1, 0, 704, 100
39493, V, 1, 1, 1, 1, 0, 704, 100
39494, V, 1, 1, 1, 1, 0, 704, 100
39495, V, 1, 1, 1, 1, 0, 704, 100
39496, V, 1, 1, 1, 1, 0, 704, 100
39497, V, 1, 1, 1, 1, 0, 704, 100
39498, V, 1, 1, 1, 1, 0, 704, 100
39499, V, 1, 1, 1, 1, 0, 704, 100
39500, V, 1, 1, 1, 1, 0, 704, 100
39501, V, 1, 1, 1, 1, 0, 704, 100
39502, V, 1, 1, 1, 1, 0, 704, 100
39503, V, 1, 1, 1, 1, 0, 704, 100
39504, V, 1, 1, 1, 1, 0, 704, 100
39505, V, 1, 1, 1, 1, 0, 704, 100
39506, V, 1, 1, 1, 1, 0, 704, 100
39507, V, 1, 1, 1, 1, 0, 704, 100
39508, V, 1, 1, 1, 1, 0, 704, 100
39510, V, 1, 1, 1, 1, 0, 704, 100
39511, V, 1, 1, 1, 1, 0, 704, 100
39512, V, 1, 1, 1, 1, 0, 704, 100
39513, V, 1, 1, 1, 1, 0, 704, 100
39514, V, 1, 1, 1, 1, 0, 704, 100
39515, V, 1, 1, 1, 1, 0, 704, 100
39516, V, 1, 1, 1, 1, 0, 704, 100
39517, V, 1, 1, 1, 1, 0, 704, 100
39518, V, 1, 1, 1, 1, 0, 704, 100
39519, V, 1, 1, 1, 1, 0, 704, 100
39520, V, 1, 1, 1, 1, 0, 704, 100
39521, V, 1, 1, 1, 1, 0, 704, 100
39522, V, 1, 1, 1, 1, 0, 704, 100
39523, V, 1, 1, 1, 1, 0, 704, 100
39524, V, 1, 1, 1, 1, 0, 704, 100
39525, V, 1, 1, 1, 1, 0, 704, 100
39526, V, 1, 1, 1, 1, 0, 704, 100
39527, V, 1, 1, 1, 1, 0, 704, 100
39528, V, 1, 1, 1, 1, 0, 704, 100
39529, V, 1, 1, 1, 1, 0, 704, 100
39530, V, 1, 1, 1, 1, 0, 704, 100
39531, V, 1, 1, 1, 1, 0, 704, 100
39532, V, 1, 1, 1, 1, 0, 704, 100
39533, V, 1, 1, 1, 1, 0, 704, 100
39534, V, 1, 1, 1, 1, 0, 704, 100
39535, V, 1, 1, 1, 1, 0, 704, 100
39536, V, 1, 1, 1, 1, 0, 704, 100
39537, V, 1, 1, 1, 1, 0, 704, 100
39538, V, 1, 1, 1, 1, 0, 704, 100
39539, V, 1, 1, 1, 1, 0, 704, 100
39540, V, 1, 1, 1, 1, 0, 704, 100
39541, V, 1, 1, 1, 1, 0, 704, 100
39542, V, 1, 1, 1, 1, 0, 704, 100
39543, V, 1, 1, 1, 1, 0, 704, 100
39544, V, 1, 1, 1, 1, 0, 704, 100
39545, V, 1, 1, 1, 1, 0, 704, 100
39546, V, 1, 1, 1, 1, 0, 704, 100
39547, V, 1, 1, 1, 1, 0, 704, 100
39548, V, 1, 1, 1, 1, 0, 704, 100
39549, V, 1, 1, 1, 1, 0, 704, 100
39550, V, 1, 1, 1, 1, 0, 704, 100
39552, V, 1, 1, 1, 1, 0, 704, 100
39553, V, 1, 1, 1, 1, 0, 704, 100
39554, V, 1, 1, 1, 1, 0, 704, 100
39555, V, 1, 1, 1, 1, 0, 704, 100
39556, V, 1, 1, 1, 1, 0, 704, 100
39557, V, 1, 1, 1, 1, 0, 704, 100
39558, V, 1, 1, 1, 1, 0, 704, 100
39559, V, 1, 1, 1, 1, 0, 704, 100
39560, V, 1, 1, 1, 1, 0, 704, 100
39561, V, 1, 1, 1, 1, 0, 704, 100
39562, V, 1, 1, 1, 1, 0, 704, 100
39563, V, 1, 1, 1, 1, 0, 704, 100
39564, V, 1, 1, 1, 1, 0, 704, 100
39565, V, 1, 1, 1, 1, 0, 704, 100
39566, V, 1, 1, 1, 1, 0, 704, 100
39567, V, 1, 1, 1, 1, 0, 704, 100
39568, V, 1, 1, 1, 1, 0, 704, 100
39569, V, 1, 1, 1, 1, 0, 704, 100
39570, V, 1, 1, 1, 1, 0, 704, 100
39571, V, 1, 1, 1, 1, 0, 704, 100
39572, V, 1, 1, 1, 1, 0, 704, 100
39573, V, 1, 1, 1, 1, 0, 704, 100
39574, V, 1, 1, 1, 1, 0, 704, 100
39575, V, 1, 1, 1, 1, 0, 704, 100
39576, V, 1, 1, 1, 1, 0, 704, 100
39577, V, 1, 1, 1, 1, 0, 704, 100
39578, V, 1, 1, 1, 1, 0, 704, 100
39579, V, 1, 1, 1, 1, 0, 704, 100
39580, V, 1, 1, 1, 1, 0, 704, 100
39581, V, 1, 1, 1, 1, 0, 704, 100
39582, V, 1, 1, 1, 1, 0, 704, 100
39583, V, 1, 1, 1, 1, 0, 704, 100
39584, V, 1, 1, 1, 1, 0, 704, 100
39585, V, 1, 1, 1, 1, 0, 704, 100
39586, V, 1, 1, 1, 1, 0, 704, 100
39587, V, 1, 1, 1, 1, 0, 704, 100
39588, V, 1, 1, 1, 1, 0, 704, 100
39589, V, 1, 1, 1, 1, 0, 704, 100
39590, V, 1, 1, 1, 1, 0, 704, 100
39591, V, 1, 1, 1, 1, 0, 704, 100
39592, V, 1, 1, 1, 1, 0, 704, 100
39593, V, 1, 1, 1, 1, 0, 704, 100
39595, V, 1, 1, 1, 1, 0, 704, 100
39596, V, 1, 1, 1, 1, 0, 704, 100
39597, V, 1, 1, 1, 1, 0, 704, 100
39598, V, 1, 1, 1, 1, 0, 704, 100
39599, V, 1, 1, 1, 1, 0, 704, 100
39600, V, 1, 1, 1, 1, 0, 704, 100
39601, V, 1, 1, 1, 1, 0, 704, 100
39602, V, 1, 1, 1, 1, 0, 704, 100
39603, V, 1, 1, 1, 1, 0, 704, 100
39604, V, 1, 1, 1, 1, 0, 704, 100
39605, V, 1, 1, 1, 1, 0, 704, 100
39606, V, 1, 1, 1, 1, 0, 704, 100
39607, V, 1, 1, 1, 1, 0, 704, 100
39608, V, 1, 1, 1, 1, 0, 704, 100
39609, V, 1, 1, 1, 1, 0, 704, 100
39610, V, 1, 1, 1, 1, 0, 704, 100
39611, V, 1, 1, 1, 1, 0, 704, 100
39612, V, 1, 1, 1, 1, 0, 704, 100
39613, V, 1, 1, 1, 1, 0, 704, 100
39614, V, 1, 1, 1, 1, 0, 704, 100
39615, V, 1, 1, 1, 1, 0, 704, 100
39616, V, 1, 1, 1, 1, 0, 704, 100
39617, V, 1, 1, 1, 1, 0, 704, 100
39618, V, 1, 1, 1, 1, 0, 704, 100
39619, V, 1, 1, 1, 1, 0, 704, 100
39620, V, 1, 1, 1, 1, 0, 704, 100
39621, V, 1, 1, 1, 1, 0, 704, 100
39622, V, 1, 1, 1, 1, 0, 704, 100
39623, V, 1, 1, 1, 1, 0, 704, 100
39624, V, 1, 1, 1, 1, 0, 704, 100
39625, V, 1, 1, 1, 1, 0, 704, 100
39626, V, 1, 1, 1, 1, 0, 704, 100
39627, V, 1, 1, 1, 1, 0, 704, 100
39628, V, 1, 1, 1, 1, 0, 704, 100
39629, V, 1, 1, 1, 1, 0, 704, 100
39630, V, 1, 1, 1, 1, 0, 704, 100
39631, V, 1, 1, 1, 1, 0, 704, 100
39632, V, 1, 1, 1, 1, 0, 704, 100
39633, V, 1, 1, 1, 1, 0, 704, 100
39634, V, 1, 1, 1, 1, 0, 704, 100
39635, V, 1, 1, 1, 1, 0, 704, 100
39636, V, 1, 1, 1, 1, 0, 704, 100
39638, V, 1, 1, 1, 1, 0, 704, 100
39639, V, 1, 1, 1, 1, 0, 704, 100
39640, V, 1, 1, 1, 1, 0, 704, 100
39641, V, 1, 1, 1, 1, 0, 704, 100
39642, V, 1, 1, 1, 1, 0, 704, 100
39643, V, 1, 1, 1, 1, 0, 704, 100
39644, V, 1, 1, 1, 1, 0, 704, 100
39645, V, 1, 1, 1, 1, 0, 704, 100
39646, V, 1, 1, 1, 1, 0, 704, 100
39647, V, 1, 1, 1, 1, 0, 704, 100
39648, V, 1, 1, 1, 1, 0, 704, 100
39649, V, 1, 1, 1, 1, 0, 704, 100
39650, V, 1, 1, 1, 1, 0, 704, 100
39651, V, 1, 1, 1, 1, 0, 704, 100
39652, V, 1, 1, 1, 1, 0, 704, 100
39653, V, 1, 1, 1, 1, 0, 704, 100
39654, V, 1, 1, 1, 1, 0, 704, 100
39655, V, 1, 1, 1, 1, 0, 704, 100
39656, V, 1, 1, 1, 1, 0, 704, 100
39657, V, 1, 1, 1, 1, 0, 704, 100
39658, V, 1, 1, 1, 1, 0, 704, 100
39659, V, 1, 1, 1, 1, 0, 704, 100
39660, V, 1, 1, 1, 1, 0, 704, 100
39661, V, 1, 1, 1, 1, 0, 704, 100
39662, V, 1, 1, 1, 1, 0, 704, 100
39663, V, 1, 1, 1, 1, 0, 704, 100
39664, V, 1, 1, 1, 1, 0, 704, 100
39665, V, 1, 1, 1, 1, 0, 704, 100
39666, V, 1, 1, 1, 1, 0, 704, 100
39667, V, 1, 1, 1, 1, 0, 704, 100
39668, V, 1, 1, 1, 1, 0, 704, 100
39669, V, 1, 1, 1, 1, 0, 704, 100
39670, V, 1, 1, 1, 1, 0, 704, 100
39671, V, 1, 1, 1, 1, 0, 704, 100
39672, V, 1, 1, 1, 1, 0, 704, 100
39673, V, 1, 1, 1, 1, 0, 704, 100
39674, V, 1, 1, 1, 1, 0, 704, 100
39675, V, 1, 1, 1, 1, 0, 704, 100
39676, V, 1, 1, 1, 1, 0, 704, 100
39677, V, 1, 1, 1, 1, 0, 704, 100
39678, V, 1, 1, 1, 1, 0, 704, 100
39680, V, 1, 1, 1, 1, 0, 704, 100
39681, V, 1, 1, 1, 1, 0, 704, 100
39682, V, 1, 1, 1, 1, 0, 704, 100
39683, V, 1, 1, 1, 1, 0, 704, 100
39684, V, 1, 1, 1, 1, 0, 704, 100
39685, V, 1, 1, 1, 1, 0, 704, 100
39686, V, 1, 1, 1, 1, 0, 704, 100
39687, V, 1, 1, 1, 1, 0, 704, 100
39688, V, 1, 1, 1, 1, 0, 704, 100
39689, V, 1, 1, 1, 1, 0, 704, 100
39690, V, 1, 1, 1, 1, 0, 704, 100
39691, V, 1, 1, 1, 1, 0, 704, 100
39692, V, 1, 1, 1, 1, 0, 704, 100
39693, V, 1, 1, 1, 1, 0, 704, 100
39694, V, 1, 1, 1, 1, 0, 704, 100
39695, V, 1, 1, 1, 1, 0, 704, 100
39696, V, 1, 1, 1, 1, 0, 704, 100
39697, V, 1, 1, 1, 1, 0, 704, 100
39698, V, 1, 1, 1, 1, 0, 704, 100
39699, V, 1, 1, 1, 1, 0, 704, 100
39700, V, 1, 1, 1, 1, 0, 704, 100
39701, V, 1, 1, 1, 1, 0, 704, 100
39702, V, 1, 1, 1, 1, 0, 704, 100
39703, V, 1, 1, 1, 1, 0, 704, 100
39704, V, 1, 1, 1, 1, 0, 704, 100
39705, V, 1, 1, 1, 1, 0, 704, 100
39706, V, 1, 1, 1, 1, 0, 704, 100
39707, V, 1, 1, 1, 1, 0, 704, 100
39708, V, 1, 1, 1, 1, 0, 704, 100
39709, V, 1, 1, 1, 1, 0, 704, 100
39710, V, 1, 1, 1, 1, 0, 704, 100
39711, V, 1, 1, 1, 1, 0, 704, 100
39712, V, 1, 1, 1, 1, 0, 704, 100
39713, V, 1, 1, 1, 1, 0, 704, 100
39714, V, 1, 1, 1, 1, 0, 704, 100
39715, V, 1, 1, 1, 1, 0, 704, 100
39716, V, 1, 1, 1, 1, 0, 704, 100
39717, V, 1, 1, 1, 1, 0, 704, 100
39718, V, 1, 1, 1, 1, 0, 704, 100
39719, V, 1, 1, 1, 1, 0, 704, 100
39720, V, 1, 1, 1, 1, 0, 704, 100
39721, V, 1, 1, 1, 1, 0, 704, 100
39723, V, 1, 1, 1, 1, 0, 704, 100
39724, V, 1, 1, 1, 1, 0, 704, 100
39725, V, 1, 1, 1, 1, 0, 704, 100
39726, V, 1, 1, 1, 1, 0, 704, 100
39727, V, 1, 1, 1, 1, 0, 704, 100
39728, V, 1, 1, 1, 1, 0, 704, 100
39729, V, 1, 1, 1, 1, 0, 704, 100
39730, V, 1, 1, 1, 1, 0, 704, 100
39731, V, 1, 1, 1, 1, 0, 704, 100
39732, V, 1, 1, 1, 1, 0, 704, 100
39733, V, 1, 1, 1, 1, 0, 704, 100
39734, V, 1, 1, 1, 1, 0, 704, 100
39735, V, 1, 1, 1, 1, 0, 704, 100
39736, V, 1, 1, 1, 1, 0, 704, 100
39737, V, 1, 1, 1, 1, 0, 704, 100
39738, V, 1, 1, 1, 1, 0, 704, 100
39739, V, 1, 1, 1, 1, 0, 704, 100
39740, V, 1, 1, 1, 1, 0, 704, 100
39741, V, 1, 1, 1, 1, 0, 704, 100
39742, V, 1, 1, 1, 1, 0, 704, 100
39743, V, 1, 1, 1, 1, 0, 704, 100
39744, V, 1, 1, 1, 1, 0, 704, 100
39745, V, 1, 1, 1, 1, 0, 704, 100
39746, V, 1, 1, 1, 1, 0, 704, 100
39747, V, 1, 1, 1, 1, 0, 704, 100
39748, V, 1, 1, 1, 1, 0, 704, 100
39749, V, 1, 1, 1, 1, 0, 704, 100
39750, V, 1, 1, 1, 1, 0, 704, 100
39751, V, 1, 1, 1, 1, 0, 704, 100
39752, V, 1, 1, 1, 1, 0, 704, 100
39753, V, 1, 1, 1, 1, 0, 704, 100
39754, V, 1, 1, 1, 1, 0, 704, 100
39755, V, 1, 1, 1, 1, 0, 704, 100
39756, V, 1, 1, 1, 1, 0, 704, 100
39757, V, 1, 1, 1, 1, 0, 704, 100
39758, V, 1, 1, 1, 1, 0, 704, 100
39759, V, 1, 1, 1, 1, 0, 704, 100
39760, V, 1, 1, 1, 1, 0, 704, 100
39761, V, 1, 1, 1, 1, 0, 704, 100
39762, V, 1, 1, 1, 1, 0, 704, 100
39763, V, 1, 1, 1, 1, 0, 704, 100
39764, V, 1, 1, 1, 1, 0, 704, 100
39766, V, 1, 1, 1, 1, 0, 704, 100
39767, V, 1, 1, 1, 1, 0, 704, 100
39768, V, 1, 1, 1, 1, 0, 704, 100
39769, V, 1, 1, 1, 1, 0, 704, 100
39770, V, 1, 1, 1, 1, 0, 704, 100
39771, V, 1, 1, 1, 1, 0, 704, 100
39772, V, 1, 1, 1, 1, 0, 704, 100
39773, V, 1, 1, 1, 1, 0, 704, 100
39774, V, 1, 1, 1, 1, 0, 704, 100
39775, V, 1, 1, 1, 1, 0, 704, 100
39776, V, 1, 1, 1, 1, 0, 704, 100
39777, V, 1, 1, 1, 1, 0, 704, 100
39778, V, 1, 1, 1, 1, 0, 704, 100
39779, V, 1, 1, 1, 1, 0, 704, 100
39780, V, 1, 1, 1, 1, 0, 704, 100
39781, V, 1, 1, 1, 1, 0, 704, 100
39782, V, 1, 1, 1, 1, 0, 704, 100
39783, V, 1, 1, 1, 1, 0, 704, 100
39784, V, 1, 1, 1, 1, 0, 704, 100
39785, V, 1, 1, 1, 1, 0, 704, 100
39786, V, 1, 1, 1, 1, 0, 704, 100
39787, V, 1, 1, 1, 1, 0, 704, 100
39788, V, 1, 1, 1, 1, 0, 704, 100
39789, V, 1, 1, 1, 1, 0, 704, 100
39790, V, 1, 1, 1, 1, 0, 704, 100
39791, V, 1, 1, 1, 1, 0, 704, 100
39792, V, 1, 1, 1, 1, 0, 704, 100
39793, V, 1, 1, 1, 1, 0, 704, 100
39794, V, 1, 1, 1, 1, 0, 704, 100
39795, V, 1, 1, 1, 1, 0, 704, 100
39796, V, 1, 1, 1, 1, 0, 704, 100
39797, V, 1, 1, 1, 1, 0, 704, 100
39798, V, 1, 1, 1, 1, 0, 704, 100
39799, V, 1, 1, 1, 1, 0, 704, 100
39800, V, 1, 1, 1, 1, 0, 704, 100
39801, V, 1, 1, 1, 1, 0, 704, 100
39802, V, 1, 1, 1, 1, 0, 704, 100
39803, V, 1, 1, 1, 1, 0, 704, 100
39804, V, 1, 1, 1, 1, 0, 704, 100
39805, V, 1, 1, 1, 1, 0, 704, 100
39806, V, 1, 1, 1, 1, 0, 704, 100
39808, V, 1, 1, 1, 1, 0, 704, 100
39809, V, 1, 1, 1, 1, 0, 704, 100
39810, V, 1, 1, 1, 1, 0, 704, 100
39811, V, 1, 1, 1, 1, 0, 704, 100
39812, V, 1, 1, 1, 1, 0, 704, 100
39813, V, 1, 1, 1, 1, 0, 704, 100
39814, V, 1, 1, 1, 1, 0, 704, 100
39815, V, 1, 1, 1, 1, 0, 704, 100
39816, V, 1, 1, 1, 1, 0, 704, 100
39817, V, 1, 1, 1, 1, 0, 704, 100
39818, V, 1, 1, 1, 1, 0, 704, 100
39819, V, 1, 1, 1, 1, 0, 704, 100
39820, V, 1, 1, 1, 1, 0, 704, 100
39821, V, 1, 1, 1, 1, 0, 704, 100
39822, V, 1, 1, 1, 1, 0, 704, 100
39823, V, 1, 1, 1, 1, 0, 704, 100
39824, V, 1, 1, 1, 1, 0, 704, 100
39825, V, 1, 1, 1, 1, 0, 704, 100
39826, V, 1, 1, 1, 1, 0, 704, 100
39827, V, 1, 1, 1, 1, 0, 704, 100
39828, V, 1, 1, 1, 1, 0, 704, 100
39829, V, 1, 1, 1, 1, 0, 704, 100
39830, V, 1, 1, 1, 1, 0, 704, 100
39831, V, 1, 1, 1, 1, 0, 704, 100
39832, V, 1, 1, 1, 1, 0, 704, 100
39833, V, 1, 1, 1, 1, 0, 704, 100
39834, V, 1, 1, 1, 1, 0, 704, 100
39835, V, 1, 1, 1, 1, 0, 704, 100
39836, V, 1, 1, 1, 1, 0, 704, 100
39837, V, 1, 1, 1, 1, 0, 704, 100
39838, V, 1, 1, 1, 1, 0, 704, 100
39839, V, 1, 1, 1, 1, 0, 704, 100
39840, V, 1, 1, 1, 1, 0, 704, 100
39841, V, 1, 1, 1, 1, 0, 704, 100
39842, V, 1, 1, 1, 1, 0, 704, 100
39843, V, 1, 1, 1, 1, 0, 704, 100
39844, V, 1, 1, 1, 1, 0, 704, 100
39845, V, 1, 1, 1, 1, 0, 704, 100
39846, V, 1, 1, 1, 1, 0, 704, 100
39847, V, 1, 1, 1, 1, 0, 704, 100
39848, V, 1, 1, 1, 1, 0, 704, 100
39849, V, 1, 1, 1, 1, 0, 704, 100
39851, V, 1, 1, 1, 1, 0, 704, 100
39852, V, 1, 1, 1, 1, 0, 704, 100
39853, V, 1, 1, 1, 1, 0, 704, 100
39854, V, 1, 1, 1, 1, 0, 704, 100
39855, V, 1, 1, 1, 1, 0, 704, 100
39856, V, 1, 1, 1, 1, 0, 704, 100
39857, V, 1, 1, 1, 1, 0, 704, 100
39858, V, 1, 1, 1, 1, 0, 704, 100
39859, V, 1, 1, 1, 1, 0, 704, 100
39860, V, 1, 1, 1, 1, 0, 704, 100
39861, V, 1, 1, 1, 1, 0, 704, 100
39862, V, 1, 1, 1, 1, 0, 704, 100
39863, V, 1, 1, 1, 1, 0, 704, 100
39864, V, 1, 1, 1, 1, 0, 704, 100
39865, V, 1, 1, 1, 1, 0, 704, 100
39866, V, 1, 1, 1, 1, 0, 704, 100
39867, V, 1, 1, 1, 1, 0, 704, 100
39868, V, 1, 1, 1, 1, 0, 704, 100
39869, V, 1, 1, 1, 1, 0, 704, 100
39870, V, 1, 1, 1, 1, 0, 704, 100
39871, V, 1, 1, 1, 1, 0, 704, 100
39872, V, 1, 1, 1, 1, 0, 704, 100
39873, V, 1, 1, 1, 1, 0, 704, 100
39874, V, 1, 1, 1, 1, 0, 704, 100
39875, V, 1, 1, 1, 1, 0, 704, 100
39876, V, 1, 1, 1, 1, 0, 704, 100
39877, V, 1, 1, 1, 1, 0, 704, 100
39878, V, 1, 1, 1, 1, 0, 704, 100
39879, V, 1, 1, 1, 1, 0, 704, 100
39880, V, 1, 1, 1, 1, 0, 704, 100
39881, V, 1, 1, 1, 1, 0, 704, 100
39882, V, 1, 1, 1, 1, 0, 704, 100
39883, V, 1, 1, 1, 1, 0, 704, 100
39884, V, 1, 1, 1, 1, 0, 704, 100
39885, V, 1, 1, 1, 1, 0, 704, 100
39886, V, 1, 1, 1, 1, 0, 704, 100
39887, V, 1, 1, 1, 1, 0, 704, 100
39888, V, 1, 1, 1, 1, 0, 704, 100
39889, V, 1, 1, 1, 1, 0, 704, 100
39890, V, 1, 1, 1, 1, 0, 704, 100
39891, V, 1, 1, 1, 1, 0, 704, 100
39892, V, 1, 1, 1, 1, 0, 704, 100
39894, V, 1, 1, 1, 1, 0, 704, 100
39895, V, 1, 1, 1, 1, 0, 704, 100
39896, V, 1, 1, 1, 1, 0, 704, 100
39897, V, 1, 1, 1, 1, 0, 704, 100
39898, V, 1, 1, 1, 1, 0, 704, 100
39899, V, 1, 1, 1, 1, 0, 704, 100
39900, V, 1, 1, 1, 1, 0, 704, 100
39901, V, 1, 1, 1, 1, 0, 704, 100
39902, V, 1, 1, 1, 1, 0, 704, 100
39903, V, 1, 1, 1, 1, 0, 704, 100
39904, V, 1, 1, 1, 1, 0, 704, 100
39905, V, 1, 1, 1, 1, 0, 704, 100
39906, V, 1, 1, 1, 1, 0, 704, 100
39907, V, 1, 1, 1, 1, 0, 704, 100
39908, V, 1, 1, 1, 1, 0, 704, 100
39909, V, 1, 1, 1, 1, 0, 704, 100
39910, V, 1, 1, 1, 1, 0, 704, 100
39911, V, 1, 1, 1, 1, 0, 704, 100
39912, V, 1, 1, 1, 1, 0, 704, 100
39913, V, 1, 1, 1, 1, 0, 704, 100
39914, V, 1, 1, 1, 1, 0, 704, 100
39915, V, 1, 1, 1, 1, 0, 704, 100
39916, V, 1, 1, 1, 1, 0, 704, 100
39917, V, 1, 1, 1, 1, 0, 704, 100
39918, V, 1, 1, 1, 1, 0, 704, 100
39919, V, 1, 1, 1, 1, 0, 704, 100
39920, V, 1, 1, 1, 1, 0, 704, 100
39921, V, 1, 1, 1, 1, 0, 704, 100
39922, V, 1, 1, 1, 1, 0, 704, 100
39923, V, 1, 1, 1, 1, 0, 704, 100
39924, V, 1, 1, 1, 1, 0, 704, 100
39925, V, 1, 1, 1, 1, 0, 704, 100
39926, V, 1, 1, 1, 1, 0, 704, 100
39927, V, 1, 1, 1, 1, 0, 704, 100
39928, V, 1, 1, 1, 1, 0, 704, 100
39929, V, 1, 1, 1, 1, 0, 704, 100
39930, V, 1, 1, 1, 1, 0, 704, 100
39931, V, 1, 1, 1, 1, 0, 704, 100
39932, V, 1, 1, 1, 1, 0, 704, 100
39933, V, 1, 1, 1, 1, 0, 704, 100
39934, V, 1, 1, 1, 1, 0, 704, 100
39936, V, 1, 1, 1, 1, 0, 704, 100
39937, V, 1, 1, 1, 1, 0, 704, 100
39938, V, 1, 1, 1, 1, 0, 704, 100
39939, V, 1, 1, 1, 1, 0, 704, 100
39940, V, 1, 1, 1, 1, 0, 704, 100
39941, V, 1, 1, 1, 1, 0, 704, 100
39942, V, 1, 1, 1, 1, 0, 704, 100
39943, V, 1, 1, 1, 1, 0, 704, 100
39944, V, 1, 1, 1, 1, 0, 704, 100
39945, V, 1, 1, 1, 1, 0, 704, 100
39946, V, 1, 1, 1, 1, 0, 704, 100
39947, V, 1, 1, 1, 1, 0, 704, 100
39948, V, 1, 1, 1, 1, 0, 704, 100
39949, V, 1, 1, 1, 1, 0, 704, 100
39950, V, 1, 1, 1, 1, 0, 704, 100
39951, V, 1, 1, 1, 1, 0, 704, 100
39952, V, 1, 1, 1, 1, 0, 704, 100
39953, V, 1, 1, 1, 1, 0, 704, 100
39954, V, 1, 1, 1, 1, 0, 704, 100
39955, V, 1, 1, 1, 1, 0, 704, 100
39956, V, 1, 1, 1, 1, 0, 704, 100
39957, V, 1, 1, 1, 1, 0, 704, 100
39958, V, 1, 1, 1, 1, 0, 704, 100
39959, V, 1, 1, 1, 1, 0, 704, 100
39960, V, 1, 1, 1, 1, 0, 704, 100
39961, V, 1, 1, 1, 1, 0, 704, 100
39962, V, 1, 1, 1, 1, 0, 704, 100
39963, V, 1, 1, 1, 1, 0, 704, 100
39964, V, 1, 1, 1, 1, 0, 704, 100
39965, V, 1, 1, 1, 1, 0, 704, 100
39966, V, 1, 1, 1, 1, 0, 704, 100
39967, V, 1, 1, 1, 1, 0, 704, 100
39968, V, 1, 1, 1, 1, 0, 704, 100
39969, V, 1, 1, 1, 1, 0, 704, 100
39970, V, 1, 1, 1, 1, 0, 704, 100
39971, V, 1, 1, 1, 1, 0, 704, 100
39972, V, 1, 1, 1, 1, 0, 704, 100
39973, V, 1, 1, 1, 1, 0, 704, 100
39974, V, 1, 1, 1, 1, 0, 704, 100
39975, V, 1, 1, 1, 1, 0, 704, 100
39976, V, 1, 1, 1, 1, 0, 704, 100
39977, V, 1, 1, 1, 1, 0, 704, 100
39979, V, 1, 1, 1, 1, 0, 704, 100
39980, V, 1, 1, 1, 1, 0, 704, 100
39981, V, 1, 1, 1, 1, 0, 704, 100
39982, V, 1, 1, 1, 1, 0, 704, 100
39983, V, 1, 1, 1, 1, 0, 704, 100
39984, V, 1, 1, 1, 1, 0, 704, 100
39985, V, 1, 1, 1, 1, 0, 704, 100
39986, V, 1, 1, 1, 1, 0, 704, 100
39987, V, 1, 1, 1, 1, 0, 704, 100
39988, V, 1, 1, 1, 1, 0, 704, 100
39989, V, 1, 1, 1, 1, 0, 704, 100
39990, V, 1, 1, 1, 1, 0, 704, 100
39991, V, 1, 1, 1, 1, 0, 704, 100
39992, V, 1, 1, 1, 1, 0, 704, 100
39993, V, 1, 1, 1, 1, 0, 704, 100
39994, V, 1, 1, 1, 1, 0, 704, 100
39995, V, 1, 1, 1, 1, 0, 704, 100
39996, V, 1, 1, 1, 1, 0, 704, 100
39997, V, 1, 1, 1, 1, 0, 704, 100
39998, V, 1, 1, 1, 1, 0, 704, 100
39999, V, 1, 1, 1, 1, 0, 704, 100
40000, V, 1, 1, 1, 1, 0, 704, 100
40001, V, 1, 1, 1, 1, 0, 704, 100
40002, V, 1, 1, 1, 1, 0, 704, 100
40003, V, 1, 1, 1, 1, 0, 704, 100
40004, V, 1, 1, 1, 1, 0, 704, 100
40005, V, 1, 1, 1, 1, 0, 704, 100
40006, V, 1, 1, 1, 1, 0, 704, 100
40007, V, 1, 1, 1, 1, 0, 704, 100
40008, V, 1, 1, 1, 1, 0, 704, 100
40009, V, 1, 1, 1, 1, 0, 704, 100
40010, V, 1, 1, 1, 1, 0, 704, 100
40011, V, 1, 0, 0, 1, 0, 704, 100
40011, V, 1, 0, 0, 0, 0, 704, 100
40012, V, 1, 0, 0, 0, 0, 704, 100
40013, V, 1, 0, 0, 0, 0, 704, 100
40014, V, 1, 0, 0, 0, 0, 704, 100
40015, V, 1, 0, 0, 0, 0, 704, 100
40016, V, 1, 0, 0, 0, 0, 704, 100
40017, V, 1, 0, 0, 0, 0, 704, 100
40018, V, 1, 0, 0, 0, 0, 704, 99
40019, V, 1, 0, 0, 0, 0, 704, 99
40020, V, 1, 0, 0, 0, 0, 704, 99
40022, V, 1, 0, 0, 0, 0, 704, 99
40023, V, 1, 0, 0, 0, 0, 704, 99
40024, V, 1, 0, 0, 0, 0, 704, 99
40025, V, 1, 0, 0, 0, 0, 704, 98
40026, V, 1, 0, 0, 0, 0, 704, 98
40027, V, 1, 0, 0, 0, 0, 704, 98
40028, V, 1, 0, 0, 0, 0, 704, 98
40029, V, 1, 0, 0, 0, 0, 704, 98
40030, V, 1, 0, 0, 0, 0, 704, 98
40031, V, 1, 0, 0, 0, 0, 704, 98
40032, V, 1, 0, 0, 0, 0, 704, 97
40033, V, 1, 0, 0, 0, 0, 704, 97
40034, V, 1, 0, 0, 0, 0, 704, 97
40035, V, 1, 0, 0, 0, 0, 704, 97
40036, V, 1, 0, 0, 0, 0, 704, 97
40037, V, 1, 0, 0, 0, 0, 704, 97
40038, V, 1, 0, 0, 0, 0, 704, 97
40039, V, 1, 0, 0, 0, 0, 704, 97
40040, V, 1, 0, 0, 0, 0, 704, 96
40041, V, 1, 0, 0, 0, 0, 704, 96
40042, V, 1, 0, 0, 0, 0, 704, 96
40043, V, 1, 0, 0, 0, 0, 704, 96
40044, V, 1, 0, 0, 0, 0, 704, 96
40045, V, 1, 0, 0, 0, 0, 704, 96
40046, V, 1, 0, 0, 0, 0, 704, 96
40047, V, 1, 0, 0, 0, 0, 704, 96
40048, V, 1, 0, 0, 0, 0, 704, 96
40049, V, 1, 0, 0, 0, 0, 704, 96
40050, V, 1, 0, 0, 0, 0, 704, 96
40051, V, 1, 0, 0, 0, 0, 704, 96
40052, V, 1, 0, 0, 0, 0, 704, 96
40053, V, 1, 0, 0, 0, 0, 704, 95
40054, V, 1, 0, 0, 0, 0, 704, 95
40055, V, 1, 0, 0, 0, 0, 704, 95
40056, V, 1, 0, 0, 0, 0, 704, 95
40057, V, 1, 0, 0, 0, 0, 704, 95
40058, V, 1, 0, 0, 0, 0, 704, 95
40059, V, 1, 0, 0, 0, 0, 704, 95
40060, V, 1, 0, 0, 0, 0, 704, 95
40061, V, 1, 0, 0, 0, 0, 704, 95
40062, V, 1, 0, 0, 0, 0, 704, 95
40064, V, 1, 0, 0, 0, 0, 704, 95
40065, V, 1, 0, 0, 0, 0, 704, 95
40066, V, 1, 0, 0, 0, 0, 704, 95
40067, V, 1, 0, 0, 0, 0, 704, 95
40068, V, 1, 0, 0, 0, 0, 704, 95
40069, V, 1, 0, 0, 0, 0, 704, 95
40070, V, 1, 0, 0, 0, 0, 704, 95
40071, V, 1, 0, 0, 0, 0, 704, 94
40072, V, 1, 0, 0, 0, 0, 704, 94
40073, V, 1, 0, 0, 0, 0, 704, 94
40074, V, 1, 0, 0, 0, 0, 704, 94
40075, V, 1, 0, 0, 0, 0, 704, 94
40076, V, 1, 0, 0, 0, 0, 704, 94
40077, V, 1, 0, 0, 0, 0, 704, 94
40078, V, 1, 0, 0, 0, 0, 704, 94
40079, V, 1, 0, 0, 0, 0, 704, 94
40080, V, 1, 0, 0, 0, 0, 704, 94
40081, V, 1, 0, 0, 0, 0, 704, 94
40082, V, 1, 0, 0, 0, 0, 704, 94
40083, V, 1, 0, 0, 0, 0, 704, 94
40084, V, 1, 0, 0, 0, 0, 704, 94
40085, V, 1, 0, 0, 0, 0, 704, 94
40086, V, 1, 0, 0, 0, 0, 704, 94
40087, V, 1, 0, 0, 0, 0, 704, 94
40088, V, 1, 0, 0, 0, 0, 704, 93
40089, V, 1, 0, 0, 0, 0, 704, 93
40090, V, 1, 0, 0, 0, 0, 704, 93
40091, V, 1, 0, 0, 0, 0, 704, 93
40092, V, 1, 0, 0, 0, 0, 704, 93
40093, V, 1, 0, 0, 0, 0, 704, 93
40094, V, 1, 0, 0, 0, 0, 704, 93
40095, V, 1, 0, 0, 0, 0, 704, 93
40096, V, 1, 0, 0, 0, 0, 704, 93
40097, V, 1, 0, 0, 0, 0, 704, 93
40098, V, 1, 0, 0, 0, 0, 704, 93
40099, V, 1, 0, 0, 0, 0, 704, 93
40100, V, 1, 0, 0, 0, 0, 704, 93
40101, V, 1, 0, 0, 0, 0, 704, 93
40102, V, 1, 0, 0, 0, 0, 704, 93
40103, V, 1, 0, 0, 0, 0, 704, 93
40104, V, 1, 0, 0, 0, 0, 704, 93
40105, V, 1, 0, 0, 0, 0, 704, 93
40107, V, 1, 0, 0, 0, 0, 704, 93
40108, V, 1, 0, 0, 0, 0, 704, 93
40109, V, 1, 0, 0, 0, 0, 704, 93
40110, V, 1, 0, 0, 0, 0, 704, 93
40111, V, 1, 0, 0, 0, 0, 704, 93
40112, V, 1, 0, 0, 0, 0, 704, 93
40113, V, 1, 0, 0, 0, 0, 704, 93
40114, V, 1, 0, 0, 0, 0, 704, 93
40115, V, 1, 0, 0, 0, 0, 704, 93
40116, V, 1, 0, 0, 0, 0, 704, 93
40117, V, 1, 0, 0, 0, 0, 704, 93
40118, V, 1, 0, 0, 0, 0, 704, 93
40119, V, 1, 0, 0, 0, 0, 704, 93
40120, V, 1, 0, 0, 0, 0, 704, 93
40121, V, 1, 0, 0, 0, 0, 704, 93
40122, V, 1, 0, 0, 0, 0, 704, 93
40123, V, 1, 0, 0, 0, 0, 704, 93
40124, V, 1, 0, 0, 0, 0, 704, 93
40125, V, 1, 0, 0, 0, 0, 704, 93
40126, V, 1, 0, 0, 0, 0, 704, 93
40127, V, 1, 0, 0, 0, 0, 704, 93
40128, V, 1, 0, 0, 0, 0, 704, 93
40129, V, 1, 0, 0, 0, 0, 704, 93
40130, V, 1, 0, 0, 0, 0, 704, 93
40131, V, 1, 0, 0, 0, 0, 704, 93
40132, V, 1, 0, 0, 0, 0, 704, 93
40133, V, 1, 0, 0, 0, 0, 704, 93
40134, V, 1, 0, 0, 0, 0, 704, 93
40135, V, 1, 0, 0, 0, 0, 704, 93
40136, V, 1, 0, 0, 0, 0, 704, 93
40137, V, 1, 0, 0, 0, 0, 704, 93
40138, V, 1, 0, 0, 0, 0, 704, 93
40139, V, 1, 0, 0, 0, 0, 704, 93
40140, V, 1, 0, 0, 0, 0, 704, 93
40141, V, 1, 0, 0, 0, 0, 704, 93
40142, V, 1, 0, 0, 0, 0, 704, 93
40143, V, 1, 0, 0, 0, 0, 704, 93
40144, V, 1, 0, 0, 0, 0, 704, 93
40145, V, 1, 0, 0, 0, 0, 704, 93
40146, V, 1, 0, 0, 0, 0, 704, 93
40147, V, 1, 0, 0, 0, 0, 704, 93
40148, V, 1, 0, 0, 0, 0, 704, 93
40150, V, 1, 0, 0, 0, 0, 704, 93
40151, V, 1, 0, 0, 0, 0, 704, 93
40152, V, 1, 0, 0, 0, 0, 704, 93
40153, V, 1, 0, 0, 0, 0, 704, 93
40154, V, 1, 0, 0, 0, 0, 704, 93
40155, V, 1, 0, 0, 0, 0, 704, 93
40156, V, 1, 0, 0, 0, 0, 704, 93
40157, V, 1, 0, 0, 0, 0, 704, 93
40158, V, 1, 0, 0, 0, 0, 704, 93
40159, V, 1, 0, 0, 0, 0, 704, 93
40160, V, 1, 0, 0, 0, 0, 704, 93
40161, V, 1, 0, 0, 0, 0, 704, 93
40162, V, 1, 0, 0, 0, 0, 704, 93
40163, V, 1, 0, 0, 0, 0, 704, 93
40164, V, 1, 0, 0, 0, 0, 704, 93
40165, V, 1, 0, 0, 0, 0, 704, 93
40166, V, 1, 0, 0, 0, 0, 704, 93
40167, V, 1, 0, 0, 0, 0, 704, 93
40168, V, 1, 0, 0, 0, 0, 704, 93
40169, V, 1, 0, 0, 0, 0, 704, 93
40170, V, 1, 0, 0, 0, 0, 704, 93
40171, V, 1, 0, 0, 0, 0, 704, 93
40172, V, 1, 0, 0, 0, 0, 704, 93
40173, V, 1, 0, 0, 0, 0, 704, 93
40174, V, 1, 0, 0, 0, 0, 704, 93
40175, V, 1, 0, 0, 0, 0, 704, 93
40176, V, 1, 0, 0, 0, 0, 704, 93
40177, V, 1, 0, 0, 0, 0, 704, 93
40178, V, 1, 0, 0, 0, 0, 704, 93
40179, V, 1, 0, 0, 0, 0, 704, 93
40180, V, 1, 0, 0, 0, 0, 704, 93
40181, V, 1, 0, 0, 0, 0, 704, 93
40182, V, 1, 0, 0, 0, 0, 704, 93
40183, V, 1, 0, 0, 0, 0, 704, 93
40184, V, 1, 0, 0, 0, 0, 704, 93
40185, V, 1, 0, 0, 0, 0, 704, 93
40186, V, 1, 0, 0, 0, 0, 704, 93
40187, V, 1, 0, 0, 0, 0, 704, 93
40188, V, 1, 0, 0, 0, 0, 704, 93
40189, V, 1, 0, 0, 0, 0, 704, 93
40190, V, 1, 0, 0, 0, 0, 704, 93
40192, V, 1, 0, 0, 0, 0, 704, 93
40193, V, 1, 0, 0, 0, 0, 704, 93
40194, V, 1, 0, 0, 0, 0, 704, 93
40195, V, 1, 0, 0, 0, 0, 704, 93
40196, V, 1, 0, 0, 0, 0, 704, 93
40197, V, 1, 0, 0, 0, 0, 704, 93
40198, V, 1, 0, 0, 0, 0, 704, 93
40199, V, 1, 0, 0, 0, 0, 704, 93
40200, V, 1, 0, 0, 0, 0, 704, 93
40201, V, 1, 0, 0, 0, 0, 704, 93
40202, V, 1, 0, 0, 0, 0, 704, 93
40203, V, 1, 0, 0, 0, 0, 704, 93
40204, V, 1, 0, 0, 0, 0, 704, 93
40205, V, 1, 0, 0, 0, 0, 704, 93
40206, V, 1, 0, 0, 0, 0, 704, 93
40207, V, 1, 0, 0, 0, 0, 704, 93
40208, V, 1, 0, 0, 0, 0, 704, 93
40209, V, 1, 0, 0, 0, 0, 704, 93
40210, V, 1, 0, 0, 0, 0, 704, 93
40211, V, 1, 0, 0, 0, 0, 704, 93
40212, V, 1, 0, 0, 0, 0, 704, 93
40213, V, 1, 0, 0, 0, 0, 704, 93
40214, V, 1, 0, 0, 0, 0, 704, 93
40215, V, 1, 0, 0, 0, 0, 704, 93
40216, V, 1, 0, 0, 0, 0, 704, 93
40217, V, 1, 0, 0, 0, 0, 704, 93
40218, V, 1, 0, 0, 0, 0, 704, 93
40219, V, 1, 0, 0, 0, 0, 704, 93
40220, V, 1, 0, 0, 0, 0, 704, 93
40221, V, 1, 0, 0, 0, 0, 704, 93
40222, V, 1, 0, 0, 0, 0, 704, 93
40223, V, 1, 0, 0, 0, 0, 704, 93
40224, V, 1, 0, 0, 0, 0, 704, 93
40225, V, 1, 0, 0, 0, 0, 704, 93
40226, V, 1, 0, 0, 0, 0, 704, 93
40227, V, 1, 0, 0, 0, 0, 704, 93
40228, V, 1, 0, 0, 0, 0, 704, 93
40229, V, 1, 0, 0, 0, 0, 704, 93
40230, V, 1, 0, 0, 0, 0, 704, 93
40231, V, 1, 0, 0, 0, 0, 704, 93
40232, V, 1, 0, 0, 0, 0, 704, 93
40233, V, 1, 0, 0, 0, 0, 704, 93
40235, V, 1, 0, 0, 0, 0, 704, 93
40236, V, 1, 0, 0, 0, 0, 704, 93
40237, V, 1, 0, 0, 0, 0, 704, 93
40238, V, 1, 0, 0, 0, 0, 704, 93
40239, V, 1, 0, 0, 0, 0, 704, 93
40240, V, 1, 0, 0, 0, 0, 704, 93
40241, V, 1, 0, 0, 0, 0, 704, 93
40242, V, 1, 0, 0, 0, 0, 704, 93
40243, V, 1, 0, 0, 0, 0, 704, 93
40244, V, 1, 0, 0, 0, 0, 704, 93
40245, V, 1, 0, 0, 0, 0, 704, 93
40246, V, 1, 0, 0, 0, 0, 704, 93
40247, V, 1, 0, 0, 0, 0, 704, 93
40248, V, 1, 0, 0, 0, 0, 704, 93
40249, V, 1, 0, 0, 0, 0, 704, 93
40250, V, 1, 0, 0, 0, 0, 704, 93
40251, V, 1, 0, 0, 0, 0, 704, 93
40252, V, 1, 0, 0, 0, 0, 704, 93
40253, V, 1, 0, 0, 0, 0, 704, 93
40254, V, 1, 0, 0, 0, 0, 704, 93
40255, V, 1, 0, 0, 0, 0, 704, 93
40256, V, 1, 0, 0, 0, 0, 704, 93
40257, V, 1, 0, 0, 0, 0, 704, 93
40258, V, 1, 0, 0, 0, 0, 704, 93
40259, V, 1, 0, 0, 0, 0, 704, 93
40260, V, 1, 0, 0, 0, 0, 704, 93
40261, V, 1, 0, 0, 0, 0, 704, 93
40262, V, 1, 0, 0, 0, 0, 704, 93
40263, V, 1, 0, 0, 0, 0, 704, 93
40264, V, 1, 0, 0, 0, 0, 704, 93
40265, V, 1, 0, 0, 0, 0, 704, 93
40266, V, 1, 0, 0, 0, 0, 704, 93
40267, V, 1, 0, 0, 0, 0, 704, 93
40268, V, 1, 0, 0, 0, 0, 704, 93
40269, V, 1, 0, 0, 0, 0, 704, 93
40270, V, 1, 0, 0, 0, 0, 704, 93
40271, V, 1, 0, 0, 0, 0, 704, 93
40272, V, 1, 0, 0, 0, 0, 704, 93
40273, V, 1, 0, 0, 0, 0, 704, 93
40274, V, 1, 0, 0, 0, 0, 704, 93
40275, V, 1, 0, 0, 0, 0, 704, 93
40276, V, 1, 0, 0, 0, 0, 704, 93
40278, V, 1, 0, 0, 0, 0, 704, 93
40279, V, 1, 0, 0, 0, 0, 704, 93
40280, V, 1, 0, 0, 0, 0, 704, 93
40281, V, 1, 0, 0, 0, 0, 704, 93
40282, V, 1, 0, 0, 0, 0, 704, 93
40283, V, 1, 0, 0, 0, 0, 704, 93
40284, V, 1, 0, 0, 0, 0, 704, 93
40285, V, 1, 0, 0, 0, 0, 704, 93
40286, V, 1, 0, 0, 0, 0, 704, 93
40287, V, 1, 0, 0, 0, 0, 704, 93
40288, V, 1, 0, 0, 0, 0, 704, 93
40289, V, 1, 0, 0, 0, 0, 704, 93
40290, V, 1, 0, 0, 0, 0, 704, 93
40291, V, 1, 0, 0, 0, 0, 704, 93
40292, V, 1, 0, 0, 0, 0, 704, 93
40293, V, 1, 0, 0, 0, 0, 704, 93
40294, V, 1, 0, 0, 0, 0, 704, 93
40295, V, 1, 0, 0, 0, 0, 704, 93
40296, V, 1, 0, 0, 0, 0, 704, 93
40297, V, 1, 0, 0, 0, 0, 704, 93
40298, V, 1, 0, 0, 0, 0, 704, 93
40299, V, 1, 0, 0, 0, 0, 704, 93
40300, V, 1, 0, 0, 0, 0, 704, 93
40301, V, 1, 0, 0, 0, 0, 704, 93
40302, V, 1, 0, 0, 0, 0, 704, 93
40303, V, 1, 0, 0, 0, 0, 704, 93
40304, V, 1, 0, 0, 0, 0, 704, 93
40305, V, 1, 0, 0, 0, 0, 704, 93
40306, V, 1, 0, 0, 0, 0, 704, 93
40307, V, 1, 0, 0, 0, 0, 704, 93
40308, V, 1, 0, 0, 0, 0, 704, 93
40309, V, 1, 0, 0, 0, 0, 704, 93
40310, V, 1, 0, 0, 0, 0, 704, 93
40311, V, 1, 0, 0, 0, 0, 704, 93
40312, V, 1, 0, 0, 0, 0, 704, 93
40313, V, 1, 0, 0, 0, 0, 704, 93
40314, V, 1, 0, 0, 0, 0, 704, 93
40315, V, 1, 0, 0, 0, 0, 704, 93
40316, V, 1, 0, 0, 0, 0, 704, 93
40317, V, 1, 0, 0, 0, 0, 704, 93
40318, V, 1, 0, 0, 0, 0, 704, 93
40320, V, 1, 0, 0, 0, 0, 704, 93
40321, V, 1, 0, 0, 0, 0, 704, 93
40322, V, 1, 0, 0, 0, 0, 704, 93
40323, V, 1, 0, 0, 0, 0, 704, 93
40324, V, 1, 0, 0, 0, 0, 704, 93
40325, V, 1, 0, 0, 0, 0, 704, 93
40326, V, 1, 0, 0, 0, 0, 704, 93
40327, V, 1, 0, 0, 0, 0, 704, 93
40328, V, 1, 0, 0, 0, 0, 704, 93
40329, V, 1, 0, 0, 0, 0, 704, 93
40330, V, 1, 0, 0, 0, 0, 704, 93
40331, V, 1, 0, 0, 0, 0, 704, 93
40332, V, 1, 0, 0, 0, 0, 704, 93
40333, V, 1, 0, 0, 0, 0, 704, 93
40334, V, 1, 0, 0, 0, 0, 704, 93
40335, V, 1, 0, 0, 0, 0, 704, 93
40336, V, 1, 0, 0, 0, 0, 704, 93
40337, V, 1, 0, 0, 0, 0, 704, 93
40338, V, 1, 0, 0, 0, 0, 704, 93
40339, V, 1, 0, 0, 0, 0, 704, 93
40340, V, 1, 0, 0, 0, 0, 704, 93
40341, V, 1, 0, 0, 0, 0, 704, 93
40342, V, 1, 0, 0, 0, 0, 704, 93
40343, V, 1, 0, 0, 0, 0, 704, 93
40344, V, 1, 0, 0, 0, 0, 704, 93
40345, V, 1, 0, 0, 0, 0, 704, 93
40346, V, 1, 0, 0, 0, 0, 704, 93
40347, V, 1, 0, 0, 0, 0, 704, 93
40348, V, 1, 0, 0, 0, 0, 704, 93
40349, V, 1, 0, 0, 0, 0, 704, 93
40350, V, 1, 0, 0, 0, 0, 704, 93
40351, V, 1, 0, 0, 0, 0, 704, 93
40352, V, 1, 0, 0, 0, 0, 704, 93
40353, V, 1, 0, 0, 0, 0, 704, 93
40354, V, 1, 0, 0, 0, 0, 704, 93
40355, V, 1, 0, 0, 0, 0, 704, 93
40356, V, 1, 0, 0, 0, 0, 704, 93
40357, V, 1, 0, 0, 0, 0, 704, 93
40358, V, 1, 0, 0, 0, 0, 704, 93
40359, V, 1, 0, 0, 0, 0, 704, 93
40360, V, 1, 0, 0, 0, 0, 704, 93
40361, V, 1, 0, 0, 0, 0, 704, 93
40363, V, 1, 0, 0, 0, 0, 704, 93
40364, V, 1, 0, 0, 0, 0, 704, 93
40365, V, 1, 0, 0, 0, 0, 704, 93
40366, V, 1, 0, 0, 0, 0, 704, 93
40367, V, 1, 0, 0, 0, 0, 704, 93
40368, V, 1, 0, 0, 0, 0, 704, 93
40369, V, 1, 0, 0, 0, 0, 704, 93
40370, V, 1, 0, 0, 0, 0, 704, 93
40371, V, 1, 0, 0, 0, 0, 704, 93
40372, V, 1, 0, 0, 0, 0, 704, 93
40373, V, 1, 0, 0, 0, 0, 704, 93
40374, V, 1, 0, 0, 0, 0, 704, 93
40375, V, 1, 0, 0, 0, 0, 704, 93
40376, V, 1, 0, 0, 0, 0, 704, 93
40377, V, 1, 0, 0, 0, 0, 704, 93
40378, V, 1, 0, 0, 0, 0, 704, 93
40379, V, 1, 0, 0, 0, 0, 704, 93
40380, V, 1, 0, 0, 0, 0, 704, 93
40381, V, 1, 0, 0, 0, 0, 704, 93
40382, V, 1, 0, 0, 0, 0, 704, 93
40383, V, 1, 0, 0, 0, 0, 704, 93
40384, V, 1, 0, 0, 0, 0, 704, 93
40385, V, 1, 0, 0, 0, 0, 704, 93
40386, V, 1, 0, 0, 0, 0, 704, 93
40387, V, 1, 0, 0, 0, 0, 704, 93
40388, V, 1, 0, 0, 0, 0, 704, 93
40389, V, 1, 0, 0, 0, 0, 704, 93
40390, V, 1, 0, 0, 0, 0, 704, 93
40391, V, 1, 0, 0, 0, 0, 704, 93
40392, V, 1, 0, 0, 0, 0, 704, 93
40393, V, 1, 0, 0, 0, 0, 704, 93
40394, V, 1, 0, 0, 0, 0, 704, 93
40395, V, 1, 0, 0, 0, 0, 704, 93
40396, V, 1, 0, 0, 0, 0, 704, 93
40397, V, 1, 0, 0, 0, 0, 704, 93
40398, V, 1, 0, 0, 0, 0, 704, 93
40399, V, 1, 0, 0, 0, 0, 704, 93
40400, V, 1, 0, 0, 0, 0, 704, 93
40401, V, 1, 0, 0, 0, 0, 704, 93
40402, V, 1, 0, 0, 0, 0, 704, 93
40403, V, 1, 0, 0, 0, 0, 704, 93
40404, V, 1, 0, 0, 0, 0, 704, 93
40406, V, 1, 0, 0, 0, 0, 704, 93
40407, V, 1, 0, 0, 0, 0, 704, 93
40408, V, 1, 0, 0, 0, 0, 704, 93
40409, V, 1, 0, 0, 0, 0, 704, 93
40410, V, 1, 0, 0, 0, 0, 704, 93
40411, V, 1, 0, 0, 0, 0, 704, 93
40412, V, 1, 0, 0, 0, 0, 704, 93
40413, V, 1, 0, 0, 0, 0, 704, 93
40414, V, 1, 0, 0, 0, 0, 704, 93
40415, V, 1, 0, 0, 0, 0, 704, 93
40416, V, 1, 0, 0, 0, 0, 704, 93
40417, V, 1, 0, 0, 0, 0, 704, 93
40418, V, 1, 0, 0, 0, 0, 704, 93
40419, V, 1, 0, 0, 0, 0, 704, 93
40420, V, 1, 0, 0, 0, 0, 704, 93
40421, V, 1, 0, 0, 0, 0, 704, 93
40422, V, 1, 0, 0, 0, 0, 704, 93
40423, V, 1, 0, 0, 0, 0, 704, 93
40424, V, 1, 0, 0, 0, 0, 704, 93
40425, V, 1, 0, 0, 0, 0, 704, 93
40426, V, 1, 0, 0, 0, 0, 704, 93
40427, V, 1, 0, 0, 0, 0, 704, 93
40428, V, 1, 0, 0, 0, 0, 704, 93
40429, V, 1, 0, 0, 0, 0, 704, 93
40430, V, 1, 0, 0, 0, 0, 704, 93
40431, V, 1, 0, 0, 0, 0, 704, 93
40432, V, 1, 0, 0, 0, 0, 704, 93
40433, V, 1, 0, 0, 0, 0, 704, 93
40434, V, 1, 0, 0, 0, 0, 704, 93
40435, V, 1, 0, 0, 0, 0, 704, 93
40436, V, 1, 0, 0, 0, 0, 704, 93
40437, V, 1, 0, 0, 0, 0, 704, 93
40438, V, 1, 0, 0, 0, 0, 704, 93
40439, V, 1, 0, 0, 0, 0, 704, 93
40440, V, 1, 0, 0, 0, 0, 704, 93
40441, V, 1, 0, 0, 0, 0, 704, 93
40442, V, 1, 0, 0, 0, 0, 704, 93
40443, V, 1, 0, 0, 0, 0, 704, 93
40444, V, 1, 0, 0, 0, 0, 704, 93
40445, V, 1, 0, 0, 0, 0, 704, 93
40446, V, 1, 0, 0, 0, 0, 704, 93
40448, V, 1, 0, 0, 0, 0, 704, 93
40449, V, 1, 0, 0, 0, 0, 704, 93
40450, V, 1, 0, 0, 0, 0, 704, 93
40451, V, 1, 0, 0, 0, 0, 704, 93
40452, V, 1, 0, 0, 0, 0, 704, 93
40453, V, 1, 0, 0, 0, 0, 704, 93
40454, V, 1, 0, 0, 0, 0, 704, 93
40455, V, 1, 0, 0, 0, 0, 704, 93
40456, V, 1, 0, 0, 0, 0, 704, 93
40457, V, 1, 0, 0, 0, 0, 704, 93
40458, V, 1, 0, 0, 0, 0, 704, 93
40459, V, 1, 0, 0, 0, 0, 704, 93
40460, V, 1, 0, 0, 0, 0, 704, 93
40461, V, 1, 0, 0, 0, 0, 704, 93
40462, V, 1, 0, 0, 0, 0, 704, 93
40463, V, 1, 0, 0, 0, 0, 704, 93
40464, V, 1, 0, 0, 0, 0, 704, 93
40465, V, 1, 0, 0, 0, 0, 704, 93
40466, V, 1, 0, 0, 0, 0, 704, 93
40467, V, 1, 0, 0, 0, 0, 704, 93
40468, V, 1, 0, 0, 0, 0, 704, 93
40469, V, 1, 0, 0, 0, 0, 704, 93
40470, V, 1, 0, 0, 0, 0, 704, 93
40471, V, 1, 0, 0, 0, 0, 704, 93
40472, V, 1, 0, 0, 0, 0, 704, 93
40473, V, 1, 0, 0, 0, 0, 704, 93
40474, V, 1, 0, 0, 0, 0, 704, 93
40475, V, 1, 0, 0, 0, 0, 704, 93
40476, V, 1, 0, 0, 0, 0, 704, 93
40477, V, 1, 0, 0, 0, 0, 704, 93
40478, V, 1, 0, 0, 0, 0, 704, 93
40479, V, 1, 0, 0, 0, 0, 704, 93
40480, V, 1, 0, 0, 0, 0, 704, 93
40481, V, 1, 0, 0, 0, 0, 704, 93
40482, V, 1, 0, 0, 0, 0, 704, 93
40483, V, 1, 0, 0, 0, 0, 704, 93
40484, V, 1, 0, 0, 0, 0, 704, 93
40485, V, 1, 0, 0, 0, 0, 704, 93
40486, V, 1, 0, 0, 0, 0, 704, 93
40487, V, 1, 0, 0, 0, 0, 704, 93
40488, V, 1, 0, 0, 0, 0, 704, 93
40489, V, 1, 0, 0, 0, 0, 704, 93
40491, V, 1, 0, 0, 0, 0, 704, 93
40492, V, 1, 0, 0, 0, 0, 704, 93
40493, V, 1, 0, 0, 0, 0, 704, 93
40494, V, 1, 0, 0, 0, 0, 704, 93
40495, V, 1, 0, 0, 0, 0, 704, 93
40496, V, 1, 0, 0, 0, 0, 704, 93
40497, V, 1, 0, 0, 0, 0, 704, 93
40498, V, 1, 0, 0, 0, 0, 704, 93
40499, V, 1, 0, 0, 0, 0, 704, 93
40500, V, 1, 0, 0, 0, 0, 704, 93
40501, V, 1, 0, 0, 0, 0, 704, 93
40502, V, 1, 0, 0, 0, 0, 704, 93
40503, V, 1, 0, 0, 0, 0, 704, 93
40504, V, 1, 0, 0, 0, 0, 704, 93
40505, V, 1, 0, 0, 0, 0, 704, 93
40506, V, 1, 0, 0, 0, 0, 704, 93
40507, V, 1, 0, 0, 0, 0, 704, 93
40508, V, 1, 0, 0, 0, 0, 704, 93
40509, V, 1, 0, 0, 0, 0, 704, 93
40510, V, 1, 0, 0, 0, 0, 704, 93
40511, V, 1, 0, 0, 0, 0, 704, 93
40512, V, 1, 0, 0, 0, 0, 704, 93
40513, V, 1, 0, 0, 0, 0, 704, 93
40514, V, 1, 0, 0, 0, 0, 704, 93
40515, V, 1, 0, 0, 0, 0, 704, 93
40516, V, 1, 0, 0, 0, 0, 704, 93
40517, V, 1, 0, 0, 0, 0, 704, 93
40518, V, 1, 0, 0, 0, 0, 704, 93
40519, V, 1, 0, 0, 0, 0, 704, 93
40520, V, 1, 0, 0, 0, 0, 704, 93
40521, V, 1, 0, 0, 0, 0, 704, 93
40522, V, 1, 0, 0, 0, 0, 704, 93
40523, V, 1, 0, 0, 0, 0, 704, 93
40524, V, 1, 0, 0, 0, 0, 704, 93
40525, V, 1, 0, 0, 0, 0, 704, 93
40526, V, 1, 0, 0, 0, 0, 704, 93
40527, V, 1, 0, 0, 0, 0, 704, 93
40528, V, 1, 0, 0, 0, 0, 704, 93
40529, V, 1, 0, 0, 0, 0, 704, 93
40530, V, 1, 0, 0, 0, 0, 704, 93
40531, V, 1, 0, 0, 0, 0, 704, 93
40532, V, 1, 0, 0, 0, 0, 704, 93
40534, V, 1, 0, 0, 0, 0, 704, 93
40535, V, 1, 0, 0, 0, 0, 704, 93
40536, V, 1, 0, 0, 0, 0, 704, 93
40537, V, 1, 0, 0, 0, 0, 704, 93
40538, V, 1, 0, 0, 0, 0, 704, 93
40539, V, 1, 0, 0, 0, 0, 704, 93
40540, V, 1, 0, 0, 0, 0, 704, 93
40541, V, 1, 0, 0, 0, 0, 704, 93
40542, V, 1, 0, 0, 0, 0, 704, 93
40543, V, 1, 0, 0, 0, 0, 704, 92
40544, V, 1, 0, 0, 0, 0, 704, 93
40545, V, 1, 0, 0, 0, 0, 704, 93
40546, V, 1, 0, 0, 0, 0, 704, 93
40547, V, 1, 0, 0, 0, 0, 704, 93
40548, V, 1, 0, 0, 0, 0, 704, 93
40549, V, 1, 0, 0, 0, 0, 704, 93
40550, V, 1, 0, 0, 0, 0, 704, 93
40551, V, 1, 0, 0, 0, 0, 704, 93
40552, V, 1, 0, 0, 0, 0, 704, 93
40553, V, 1, 0, 0, 0, 0, 704, 93
40554, V, 1, 0, 0, 0, 0, 704, 93
40555, V, 1, 0, 0, 0, 0, 704, 93
40556, V, 1, 0, 0, 0, 0, 704, 93
40557, V, 1, 0, 0, 0, 0, 704, 93
40558, V, 1, 0, 0, 0, 0, 704, 93
40559, V, 1, 0, 0, 0, 0, 704, 93
40560, V, 1, 0, 0, 0, 0, 704, 93
40561, V, 1, 0, 0, 0, 0, 704, 93
40562, V, 1, 0, 0, 0, 0, 704, 93
40563, V, 1, 0, 0, 0, 0, 704, 93
40564, V, 1, 0, 0, 0, 0, 704, 93
40565, V, 1, 0, 0, 0, 0, 704, 93
40566, V, 1, 0, 0, 0, 0, 704, 93
40567, V, 1, 0, 0, 0, 0, 704, 93
40568, V, 1, 0, 0, 0, 0, 704, 93
40569, V, 1, 0, 0, 0, 0, 704, 93
40570, V, 1, 0, 0, 0, 0, 704, 93
40571, V, 1, 0, 0, 0, 0, 704, 93
40572, V, 1, 0, 0, 0, 0, 704, 93
40573, V, 1, 0, 0, 0, 0, 704, 93
40574, V, 1, 0, 0, 0, 0, 704, 93
40576, V, 1, 0, 0, 0, 0, 704, 93
40577, V, 1, 0, 0, 0, 0, 704, 93
40578, V, 1, 0, 0, 0, 0, 704, 93
40579, V, 1, 0, 0, 0, 0, 704, 93
40580, V, 1, 0, 0, 0, 0, 704, 93
40581, V, 1, 0, 0, 0, 0, 704, 92
40582, V, 1, 0, 0, 0, 0, 704, 93
40583, V, 1, 0, 0, 0, 0, 704, 93
40584, V, 1, 0, 0, 0, 0, 704, 93
40585, V, 1, 0, 0, 0, 0, 704, 93
40586, V, 1, 0, 0, 0, 0, 704, 93
40587, V, 1, 0, 0, 0, 0, 704, 93
40588, V, 1, 0, 0, 0, 0, 704, 93
40589, V, 1, 0, 0, 0, 0, 704, 93
40590, V, 1, 0, 0, 0, 0, 704, 93
40591, V, 1, 0, 0, 0, 0, 704, 93
40592, V, 1, 0, 0, 0, 0, 704, 93
40593, V, 1, 0, 0, 0, 0, 704, 93
40594, V, 1, 0, 0, 0, 0, 704, 93
40595, V, 1, 0, 0, 0, 0, 704, 93
40596, V, 1, 0, 0, 0, 0, 704, 93
40597, V, 1, 0, 0, 0, 0, 704, 93
40598, V, 1, 0, 0, 0, 0, 704, 93
40599, V, 1, 0, 0, 0, 0, 704, 93
40600, V, 1, 0, 0, 0, 0, 704, 93
40601, V, 1, 0, 0, 0, 0, 704, 93
40602, V, 1, 0, 0, 0, 0, 704, 93
40603, V, 1, 0, 0, 0, 0, 704, 93
40604, V, 1, 0, 0, 0, 0, 704, 93
40605, V, 1, 0, 0, 0, 0, 704, 93
40606, V, 1, 0, 0, 0, 0, 704, 93
40607, V, 1, 0, 0, 0, 0, 704, 93
40608, V, 1, 0, 0, 0, 0, 704, 93
40609, V, 1, 0, 0, 0, 0, 704, 93
40610, V, 1, 0, 0, 0, 0, 704, 93
40611, V, 1, 0, 0, 0, 0, 704, 93
40612, V, 1, 0, 0, 0, 0, 704, 93
40613, V, 1, 0, 0, 0, 0, 704, 93
40614, V, 1, 0, 0, 0, 0, 704, 93
40615, V, 1, 0, 0, 0, 0, 704, 93
40616, V, 1, 0, 0, 0, 0, 704, 93
40617, V, 1, 0, 0, 0, 0, 704, 93
40619, V, 1, 0, 0, 0, 0, 704, 93
40620, V, 1, 0, 0, 0, 0, 704, 93
40621, V, 1, 0, 0, 0, 0, 704, 93
40622, V, 1, 0, 0, 0, 0, 704, 93
40623, V, 1, 0, 0, 0, 0, 704, 93
40624, V, 1, 0, 0, 0, 0, 704, 93
40625, V, 1, 0, 0, 0, 0, 704, 93
40626, V, 1, 0, 0, 0, 0, 704, 93
40627, V, 1, 0, 0, 0, 0, 704, 93
40628, V, 1, 0, 0, 0, 0, 704, 93
40629, V, 1, 0, 0, 0, 0, 704, 93
40630, V, 1, 0, 0, 0, 0, 704, 93
40631, V, 1, 0, 0, 0, 0, 704, 93
40632, V, 1, 0, 0, 0, 0, 704, 93
40633, V, 1, 0, 0, 0, 0, 704, 93
40634, V, 1, 0, 0, 0, 0, 704, 93
40635, V, 1, 0, 0, 0, 0, 704, 93
40636, V, 1, 0, 0, 0, 0, 704, 93
40637, V, 1, 0, 0, 0, 0, 704, 93
40638, V, 1, 0, 0, 0, 0, 704, 93
40639, V, 1, 0, 0, 0, 0, 704, 93
40640, V, 1, 0, 0, 0, 0, 704, 93
40641, V, 1, 0, 0, 0, 0, 704, 93
40642, V, 1, 0, 0, 0, 0, 704, 93
40643, V, 1, 0, 0, 0, 0, 704, 93
40644, V, 1, 0, 0, 0, 0, 704, 93
40645, V, 1, 0, 0, 0, 0, 704, 93
40646, V, 1, 0, 0, 0, 0, 704, 93
40647, V, 1, 0, 0, 0, 0, 704, 93
40648, V, 1, 0, 0, 0, 0, 704, 93
40649, V, 1, 0, 0, 0, 0, 704, 93
40650, V, 1, 0, 0, 0, 0, 704, 93
40651, V, 1, 0, 0, 0, 0, 704, 93
40652, V, 1, 0, 0, 0, 0, 704, 93
40653, V, 1, 0, 0, 0, 0, 704, 93
40654, V, 1, 0, 0, 0, 0, 704, 93
40655, V, 1, 0, 0, 0, 0, 704, 93
40656, V, 1, 0, 0, 0, 0, 704, 93
40657, V, 1, 0, 0, 0, 0, 704, 93
40658, V, 1, 0, 0, 0, 0, 704, 93
40659, V, 1, 0, 0, 0, 0, 704, 93
40660, V, 1, 0, 0, 0, 0, 704, 93
40662, V, 1, 0, 0, 0, 0, 704, 93
40663, V, 1, 0, 0, 0, 0, 704, 93
40664, V, 1, 0, 0, 0, 0, 704, 93
40665, V, 1, 0, 0, 0, 0, 704, 93
40666, V, 1, 0, 0, 0, 0, 704, 93
40667, V, 1, 0, 0, 0, 0, 704, 93
40668, V, 1, 0, 0, 0, 0, 704, 93
40669, V, 1, 0, 0, 0, 0, 704, 92
40670, V, 1, 0, 0, 0, 0, 704, 92
40671, V, 1, 0, 0, 0, 0, 704, 92
40672, V, 1, 0, 0, 0, 0, 704, 91
40673, V, 1, 0, 0, 0, 0, 704, 90
40674, V, 1, 0, 0, 0, 0, 704, 89
40675, V, 1, 0, 0, 0, 0, 704, 88
40676, V, 1, 0, 0, 0, 0, 704, 87
40677, V, 1, 0, 0, 0, 0, 704, 86
40678, V, 1, 0, 0, 0, 0, 704, 84
40679, V, 1, 0, 0, 0, 0, 704, 83
40680, V, 1, 0, 0, 0, 0, 704, 82
40681, V, 1, 0, 0, 0, 0, 704, 82
40682, V, 1, 0, 0, 0, 0, 704, 81
40683, V, 1, 0, 0, 0, 0, 704, 80
40684, V, 1, 0, 0, 0, 0, 704, 79
40685, V, 1, 0, 0, 0, 0, 704, 78
40686, V, 1, 0, 0, 0, 0, 704, 77
40687, V, 1, 0, 0, 0, 0, 704, 77
40688, V, 1, 0, 0, 0, 0, 704, 76
40689, V, 1, 0, 0, 0, 0, 704, 75
40690, V, 1, 0, 0, 0, 0, 704, 74
40691, V, 1, 0, 0, 0, 0, 704, 74
40692, V, 1, 0, 0, 0, 0, 704, 73
40693, V, 1, 0, 0, 0, 0, 704, 73
40694, V, 1, 0, 0, 0, 0, 704, 72
40695, V, 1, 0, 0, 0, 0, 704, 71
40696, V, 1, 0, 0, 0, 0, 704, 71
40697, V, 1, 0, 0, 0, 0, 704, 70
40698, V, 1, 0, 0, 0, 0, 704, 70
40699, V, 1, 0, 0, 0, 0, 704, 69
40700, V, 1, 0, 0, 0, 0, 704, 69
40701, V, 1, 0, 0, 0, 0, 704, 68
40702, V, 1, 0, 0, 0, 0, 704, 68
40704, V, 1, 0, 0, 0, 0, 704, 67
40705, V, 1, 0, 0, 0, 0, 704, 67
40706, V, 1, 0, 0, 0, 0, 704, 66
40707, V, 1, 0, 0, 0, 0, 704, 66
40708, V, 1, 0, 0, 0, 0, 704, 66
40709, V, 1, 0, 0, 0, 0, 704, 65
40710, V, 1, 0, 0, 0, 0, 704, 65
40711, V, 1, 0, 0, 0, 0, 704, 64
40712, V, 1, 0, 0, 0, 0, 704, 64
40713, V, 1, 0, 0, 0, 0, 704, 64
40714, V, 1, 0, 0, 0, 0, 704, 63
40715, V, 1, 0, 0, 0, 0, 704, 63
40716, V, 1, 0, 0, 0, 0, 704, 63
40717, V, 1, 0, 0, 0, 0, 704, 62
40718, V, 1, 0, 0, 0, 0, 704, 62
40719, V, 1, 0, 0, 0, 0, 704, 62
40720, V, 1, 0, 0, 0, 0, 704, 61
40721, V, 1, 0, 0, 0, 0, 704, 61
40722, V, 1, 0, 0, 0, 0, 704, 61
40723, V, 1, 0, 0, 0, 0, 704, 61
40724, V, 1, 0, 0, 0, 0, 704, 60
40725, V, 1, 0, 0, 0, 0, 704, 60
40726, V, 1, 0, 0, 0, 0, 704, 60
40727, V, 1, 0, 0, 0, 0, 704, 60
40728, V, 1, 0, 0, 0, 0, 704, 60
40729, V, 1, 0, 0, 0, 0, 704, 59
40730, V, 1, 0, 0, 0, 0, 704, 59
40731, V, 1, 0, 0, 0, 0, 704, 59
40732, V, 1, 0, 0, 0, 0, 704, 59
40733, V, 1, 0, 0, 0, 0, 704, 58
40734, V, 1, 0, 0, 0, 0, 704, 58
40735, V, 1, 0, 0, 0, 0, 704, 58
40736, V, 1, 0, 0, 0, 0, 704, 58
40737, V, 1, 0, 0, 0, 0, 704, 58
40738, V, 1, 0, 0, 0, 0, 704, 58
40739, V, 1, 0, 0, 0, 0, 704, 57
40740, V, 1, 0, 0, 0, 0, 704, 57
40741, V, 1, 0, 0, 0, 0, 704, 57
40742, V, 1, 0, 0, 0, 0, 704, 57
40743, V, 1, 0, 0, 0, 0, 704, 57
40744, V, 1, 0, 0, 0, 0, 704, 57
40745, V, 1, 0, 0, 0, 0, 704, 57
40747, V, 1, 0, 0, 0, 0, 704, 57
40748, V, 1, 0, 0, 0, 0, 704, 56
40749, V, 1, 0, 0, 0, 0, 704, 56
40750, V, 1, 0, 0, 0, 0, 704, 56
40751, V, 1, 0, 0, 0, 0, 704, 56
40752, V, 1, 0, 0, 0, 0, 704, 56
40753, V, 1, 0, 0, 0, 0, 704, 56
40754, V, 1, 0, 0, 0, 0, 704, 56
40755, V, 1, 0, 0, 0, 0, 704, 56
40756, V, 1, 0, 0, 0, 0, 704, 56
40757, V, 1, 0, 0, 0, 0, 704, 55
40758, V, 1, 0, 0, 0, 0, 704, 55
40759, V, 1, 0, 0, 0, 0, 704, 55
40760, V, 1, 0, 0, 0, 0, 704, 55
40761, V, 1, 0, 0, 0, 0, 704, 55
40762, V, 1, 0, 0, 0, 0, 704, 55
40763, V, 1, 0, 0, 0, 0, 704, 55
40764, V, 1, 0, 0, 0, 0, 704, 55
40765, V, 1, 0, 0, 0, 0, 704, 55
40766, V, 1, 0, 0, 0, 0, 704, 55
40767, V, 1, 0, 0, 0, 0, 704, 55
40768, V, 1, 0, 0, 0, 0, 704, 55
40769, V, 1, 0, 0, 0, 0, 704, 54
40770, V, 1, 0, 0, 0, 0, 704, 54
40771, V, 1, 0, 0, 0, 0, 704, 54
40772, V, 1, 0, 0, 0, 0, 704, 54
40773, V, 1, 0, 0, 0, 0, 704, 54
40774, V, 1, 0, 0, 0, 0, 704, 54
40775, V, 1, 0, 0, 0, 0, 704, 54
40776, V, 1, 0, 0, 0, 0, 704, 54
40777, V, 1, 0, 0, 0, 0, 704, 54
40778, V, 1, 0, 0, 0, 0, 704, 54
40779, V, 1, 0, 0, 0, 0, 704, 54
40780, V, 1, 0, 0, 0, 0, 704, 54
40781, V, 1, 0, 0, 0, 0, 704, 54
40782, V, 1, 0, 0, 0, 0, 704, 54
40783, V, 1, 0, 0, 0, 0, 704, 54
40784, V, 1, 0, 0, 0, 0, 704, 54
40785, V, 1, 0, 0, 0, 0, 704, 54
40786, V, 1, 0, 0, 0, 0, 704, 53
40787, V, 1, 0, 0, 0, 0, 704, 53
40788, V, 1, 0, 0, 0, 0, 704, 53
40790, V, 1, 0, 0, 0, 0, 704, 53
40791, V, 1, 0, 0, 0, 0, 704, 53
40792, V, 1, 0, 0, 0, 0, 704, 53
40793, V, 1, 0, 0, 0, 0, 704, 53
40794, V, 1, 0, 0, 0, 0, 704, 53
40795, V, 1, 0, 0, 0, 0, 704, 53
40796, V, 1, 0, 0, 0, 0, 704, 53
40797, V, 1, 0, 0, 0, 0, 704, 53
40798, V, 1, 0, 0, 0, 0, 704, 53
40799, V, 1, 0, 0, 0, 0, 704, 53
40800, V, 1, 0, 0, 0, 0, 704, 53
40801, V, 1, 0, 0, 0, 0, 704, 53
40802, V, 1, 0, 0, 0, 0, 704, 53
40803, V, 1, 0, 0, 0, 0, 704, 53
40804, V, 1, 0, 0, 0, 0, 704, 53
40805, V, 1, 0, 0, 0, 0, 704, 53
40806, V, 1, 0, 0, 0, 0, 704, 53
40807, V, 1, 0, 0, 0, 0, 704, 53
40808, V, 1, 0, 0, 0, 0, 704, 53
40809, V, 1, 0, 0, 0, 0, 704, 53
40810, V, 1, 0, 0, 0, 0, 704, 53
40811, V, 1, 0, 0, 0, 0, 704, 53
40812, V, 1, 0, 0, 0, 0, 704, 53
40813, V, 1, 0, 0, 0, 0, 704, 53
40814, V, 1, 0, 0, 0, 0, 704, 53
40815, V, 1, 0, 0, 0, 0, 704, 53
40816, V, 1, 0, 0, 0, 0, 704, 53
40817, V, 1, 0, 0, 0, 0, 704, 53
40818, V, 1, 0, 0, 0, 0, 704, 53
40819, V, 1, 0, 0, 0, 0, 704, 53
40820, V, 1, 0, 0, 0, 0, 704, 53
40821, V, 1, 0, 0, 0, 0, 704, 53
40822, V, 1, 0, 0, 0, 0, 704, 53
40823, V, 1, 0, 0, 0, 0, 704, 53
40824, V, 1, 0, 0, 0, 0, 704, 53
40825, V, 1, 0, 0, 0, 0, 704, 53
40826, V, 1, 0, 0, 0, 0, 704, 53
40827, V, 1, 0, 0, 0, 0, 704, 53
40828, V, 1, 0, 0, 0, 0, 704, 53
40829, V, 1, 0, 0, 0, 0, 704, 53
40830, V, 1, 0, 0, 0, 0, 704, 53
40832, V, 1, 0, 0, 0, 0, 704, 53
40833, V, 1, 0, 0, 0, 0, 704, 53
40834, V, 1, 0, 0, 0, 0, 704, 53
40835, V, 1, 0, 0, 0, 0, 704, 53
40836, V, 1, 0, 0, 0, 0, 704, 53
40837, V, 1, 0, 0, 0, 0, 704, 53
40838, V, 1, 0, 0, 0, 0, 704, 54
40839, V, 1, 0, 0, 0, 0, 704, 54
40840, V, 1, 0, 0, 0, 0, 704, 54
40841, V, 1, 0, 0, 0, 0, 704, 54
40842, V, 1, 0, 0, 0, 0, 704, 54
40843, V, 1, 0, 0, 0, 0, 704, 54
40844, V, 1, 0, 0, 0, 0, 704, 54
40845, V, 1, 0, 0, 0, 0, 704, 54
40846, V, 1, 0, 0, 0, 0, 704, 54
40847, V, 1, 0, 0, 0, 0, 704, 54
40848, V, 1, 0, 0, 0, 0, 704, 54
40849, V, 1, 0, 0, 0, 0, 704, 54
40850, V, 1, 0, 0, 0, 0, 704, 54
40851, V, 1, 0, 0, 0, 0, 704, 54
40852, V, 1, 0, 0, 0, 0, 704, 54
40853, V, 1, 0, 0, 0, 0, 704, 54
40854, V, 1, 0, 0, 0, 0, 704, 54
40855, V, 1, 0, 0, 0, 0, 704, 54
40856, V, 1, 0, 0, 0, 0, 704, 54
40857, V, 1, 0, 0, 0, 0, 704, 54
40858, V, 1, 0, 0, 0, 0, 704, 54
40859, V, 1, 0, 0, 0, 0, 704, 54
40860, V, 1, 0, 0, 0, 0, 704, 54
40861, V, 1, 0, 0, 0, 0, 704, 54
40862, V, 1, 0, 0, 0, 0, 704, 54
40863, V, 1, 0, 0, 0, 0, 704, 54
40864, V, 1, 0, 0, 0, 0, 704, 54
40865, V, 1, 0, 0, 0, 0, 704, 54
40866, V, 1, 0, 0, 0, 0, 704, 54
40867, V, 1, 0, 0, 0, 0, 704, 54
40868, V, 1, 0, 0, 0, 0, 704, 54
40869, V, 1, 0, 0, 0, 0, 704, 54
40870, V, 1, 0, 0, 0, 0, 704, 54
40871, V, 1, 0, 0, 0, 0, 704, 54
40872, V, 1, 0, 0, 0, 0, 704, 54
40873, V, 1, 0, 0, 0, 0, 704, 54
40875, V, 1, 0, 0, 0, 0, 704, 54
40876, V, 1, 0, 0, 0, 0, 704, 54
40877, V, 1, 0, 0, 0, 0, 704, 54
40878, V, 1, 0, 0, 0, 0, 704, 54
40879, V, 1, 0, 0, 0, 0, 704, 54
40880, V, 1, 0, 0, 0, 0, 704, 54
40881, V, 1, 0, 0, 0, 0, 704, 54
40882, V, 1, 0, 0, 0, 0, 704, 55
40883, V, 1, 0, 0, 0, 0, 704, 55
40884, V, 1, 0, 0, 0, 0, 704, 55
40885, V, 1, 0, 0, 0, 0, 704, 55
40886, V, 1, 0, 0, 0, 0, 704, 55
40887, V, 1, 0, 0, 0, 0, 704, 55
40888, V, 1, 0, 0, 0, 0, 704, 55
40889, V, 1, 0, 0, 0, 0, 704, 55
40890, V, 1, 0, 0, 0, 0, 704, 55
40891, V, 1, 0, 0, 0, 0, 704, 55
40892, V, 1, 0, 0, 0, 0, 704, 55
40893, V, 1, 0, 0, 0, 0, 704, 55
40894, V, 1, 0, 0, 0, 0, 704, 55
40895, V, 1, 0, 0, 0, 0, 704, 55
40896, V, 1, 0, 0, 0, 0, 704, 55
40897, V, 1, 0, 0, 0, 0, 704, 55
40898, V, 1, 0, 0, 0, 0, 704, 55
40899, V, 1, 0, 0, 0, 0, 704, 55
40900, V, 1, 0, 0, 0, 0, 704, 55
40901, V, 1, 0, 0, 0, 0, 704, 55
40902, V, 1, 0, 0, 0, 0, 704, 55
40903, V, 1, 0, 0, 0, 0, 704, 55
40904, V, 1, 0, 0, 0, 0, 704, 55
40905, V, 1, 0, 0, 0, 0, 704, 55
40906, V, 1, 0, 0, 0, 0, 704, 55
40907, V, 1, 0, 0, 0, 0, 704, 55
40908, V, 1, 0, 0, 0, 0, 704, 55
40909, V, 1, 0, 0, 0, 0, 704, 55
40910, V, 1, 0, 0, 0, 0, 704, 55
40911, V, 1, 0, 0, 0, 0, 704, 55
40912, V, 1, 0, 0, 0, 0, 704, 55
40913, V, 1, 0, 0, 0, 0, 704, 55
40914, V, 1, 0, 0, 0, 0, 704, 55
40915, V, 1, 0, 0, 0, 0, 704, 56
40916, V, 1, 0, 0, 0, 0, 704, 56
40918, V, 1, 0, 0, 0, 0, 704, 56
40919, V, 1, 0, 0, 0, 0, 704, 56
40920, V, 1, 0, 0, 0, 0, 704, 57
40921, V, 1, 0, 0, 0, 0, 704, 57
40922, V, 1, 0, 0, 0, 0, 704, 57
40923, V, 1, 0, 0, 0, 0, 704, 58
40924, V, 1, 0, 0, 0, 0, 704, 58
40925, V, 1, 0, 0, 0, 0, 704, 58
40926, V, 1, 0, 0, 0, 0, 704, 59
40927, V, 1, 0, 0, 0, 0, 704, 59
40928, V, 1, 0, 0, 0, 0, 704, 59
40929, V, 1, 0, 0, 0, 0, 704, 60
40930, V, 1, 0, 0, 0, 0, 704, 60
40931, V, 1, 0, 0, 0, 0, 704, 60
40932, V, 1, 0, 0, 0, 0, 704, 60
40933, V, 1, 0, 0, 0, 0, 704, 61
40934, V, 1, 0, 0, 0, 0, 704, 61
40935, V, 1, 0, 0, 0, 0, 704, 61
40936, V, 1, 0, 0, 0, 0, 704, 61
40937, V, 1, 0, 0, 0, 0, 704, 62
40938, V, 1, 0, 0, 0, 0, 704, 62
40939, V, 1, 0, 0, 0, 0, 704, 62
40940, V, 1, 0, 0, 0, 0, 704, 62
40941, V, 1, 0, 0, 0, 0, 704, 63
40942, V, 1, 0, 0, 0, 0, 704, 63
40943, V, 1, 0, 0, 0, 0, 704, 63
40944, V, 1, 0, 0, 0, 0, 704, 63
40945, V, 1, 0, 0, 0, 0, 704, 63
40946, V, 1, 0, 0, 0, 0, 704, 64
40947, V, 1, 0, 0, 0, 0, 704, 64
40948, V, 1, 0, 0, 0, 0, 704, 64
40949, V, 1, 0, 0, 0, 0, 704, 64
40950, V, 1, 0, 0, 0, 0, 704, 64
40951, V, 1, 0, 0, 0, 0, 704, 64
40952, V, 1, 0, 0, 0, 0, 704, 65
40953, V, 1, 0, 0, 0, 0, 704, 65
40954, V, 1, 0, 0, 0, 0, 704, 65
40955, V, 1, 0, 0, 0, 0, 704, 65
40956, V, 1, 0, 0, 0, 0, 704, 65
40957, V, 1, 0, 0, 0, 0, 704, 65
40958, V, 1, 0, 0, 0, 0, 704, 65
40960, V, 1, 1, 0, 0, 0, 704, 66
40960, V, 1, 1, 0, 0, 0, 704, 66
40961, V, 1, 1, 1, 1, 0, 704, 66
40962, V, 1, 1, 1, 1, 0, 704, 66
40963, V, 1, 1, 1, 1, 0, 704, 66
40964, V, 1, 1, 1, 1, 0, 704, 66
40965, V, 1, 1, 1, 1, 0, 704, 67
40966, V, 1, 1, 1, 1, 0, 704, 67
40967, V, 1, 1, 1, 1, 0, 704, 68
40968, V, 1, 1, 1, 1, 0, 704, 69
40969, V, 1, 1, 1, 1, 0, 704, 70
40970, V, 1, 1, 1, 1, 0, 704, 71
40971, V, 1, 1, 1, 1, 0, 704, 71
40972, V, 1, 1, 1, 1, 0, 704, 72
40973, V, 1, 1, 1, 1, 0, 704, 73
40974, V, 1, 1, 1, 1, 0, 704, 74
40975, V, 1, 1, 1, 1, 0, 704, 75
40976, V, 1, 1, 1, 1, 0, 704, 75
40977, V, 1, 1, 1, 1, 0, 704, 76
40978, V, 1, 1, 1, 1, 0, 704, 77
40979, V, 1, 1, 1, 1, 0, 704, 77
40980, V, 1, 1, 1, 1, 0, 704, 78
40981, V, 1, 1, 1, 1, 0, 704, 79
40982, V, 1, 1, 1, 1, 0, 704, 79
40983, V, 1, 1, 1, 1, 0, 704, 80
40984, V, 1, 1, 1, 1, 0, 704, 80
40985, V, 1, 1, 1, 1, 0, 704, 81
40986, V, 1, 1, 1, 1, 0, 704, 81
40987, V, 1, 1, 1, 1, 0, 704, 82
40988, V, 1, 1, 1, 1, 0, 704, 82
40989, V, 1, 1, 1, 1, 0, 704, 83
40990, V, 1, 1, 1, 1, 0, 704, 83
40991, V, 1, 1, 1, 1, 0, 704, 84
40992, V, 1, 1, 1, 1, 0, 704, 84
40993, V, 1, 1, 1, 1, 0, 704, 84
40994, V, 1, 1, 1, 1, 0, 704, 85
40995, V, 1, 1, 1, 1, 0, 704, 85
40996, V, 1, 1, 1, 1, 0, 704, 86
40997, V, 1, 1, 1, 1, 0, 704, 86
40998, V, 1, 1, 1, 1, 0, 704, 86
40999, V, 1, 1, 1, 1, 0, 704, 87
41000, V, 1, 1, 1, 1, 0, 704, 87
41001, V, 1, 1, 1, 1, 0, 704, 88
41003, V, 1, 1, 1, 1, 0, 704, 88
41004, V, 1, 1, 1, 1, 0, 704, 88
41005, V, 1, 1, 1, 1, 0, 704, 89
41006, V, 1, 1, 1, 1, 0, 704, 89
41007, V, 1, 1, 1, 1, 0, 704, 89
41008, V, 1, 1, 1, 1, 0, 704, 89
41009, V, 1, 1, 1, 1, 0, 704, 90
41010, V, 1, 1, 1, 1, 0, 704, 90
41011, V, 1, 1, 1, 1, 0, 704, 90
41012, V, 1, 1, 1, 1, 0, 704, 90
41013, V, 1, 1, 1, 1, 0, 704, 91
41014, V, 1, 1, 1, 1, 0, 704, 91
41015, V, 1, 1, 1, 1, 0, 704, 91
41016, V, 1, 1, 1, 1, 0, 704, 91
41017, V, 1, 1, 1, 1, 0, 704, 92
41018, V, 1, 1, 1, 1, 0, 704, 92
41019, V, 1, 1, 1, 1, 0, 704, 92
41020, V, 1, 1, 1, 1, 0, 704, 92
41021, V, 1, 1, 1, 1, 0, 704, 92
41022, V, 1, 1, 1, 1, 0, 704, 93
41023, V, 1, 1, 1, 1, 0, 704, 93
41024, V, 1, 1, 1, 1, 0, 704, 93
41025, V, 1, 1, 1, 1, 0, 704, 93
41026, V, 1, 1, 1, 1, 0, 704, 93
41027, V, 1, 1, 1, 1, 0, 704, 93
41028, V, 1, 1, 1, 1, 0, 704, 94
41029, V, 1, 1, 1, 1, 0, 704, 94
41030, V, 1, 1, 1, 1, 0, 704, 94
41031, V, 1, 1, 1, 1, 0, 704, 94
41032, V, 1, 1, 1, 1, 0, 704, 94
41033, V, 1, 1, 1, 1, 0, 704, 94
41034, V, 1, 1, 1, 1, 0, 704, 94
41035, V, 1, 1, 1, 1, 0, 704, 95
41036, V, 1, 1, 1, 1, 0, 704, 95
41037, V, 1, 1, 1, 1, 0, 704, 95
41038, V, 1, 1, 1, 1, 0, 704, 95
41039, V, 1, 1, 1, 1, 0, 704, 95
41040, V, 1, 1, 1, 1, 0, 704, 95
41041, V, 1, 1, 1, 1, 0, 704, 95
41042, V, 1, 1, 1, 1, 0, 704, 95
41043, V, 1, 1, 1, 1, 0, 704, 95
41044, V, 1, 1, 1, 1, 0, 704, 96
41046, V, 1, 1, 1, 1, 0, 704, 96
41047, V, 1, 1, 1, 1, 0, 704, 96
41048, V, 1, 1, 1, 1, 0, 704, 96
41049, V, 1, 1, 1, 1, 0, 704, 96
41050, V, 1, 1, 1, 1, 0, 704, 96
41051, V, 1, 1, 1, 1, 0, 704, 96
41052, V, 1, 1, 1, 1, 0, 704, 96
41053, V, 1, 1, 1, 1, 0, 704, 96
41054, V, 1, 1, 1, 1, 0, 704, 96
41055, V, 1, 1, 1, 1, 0, 704, 96
41056, V, 1, 1, 1, 1, 0, 704, 96
41057, V, 1, 1, 1, 1, 0, 704, 97
41058, V, 1, 1, 1, 1, 0, 704, 97
41059, V, 1, 1, 1, 1, 0, 704, 97
41060, V, 1, 1, 1, 1, 0, 704, 97
41061, V, 1, 1, 1, 1, 0, 704, 97
41062, V, 1, 1, 1, 1, 0, 704, 97
41063, V, 1, 1, 1, 1, 0, 704, 97
41064, V, 1, 1, 1, 1, 0, 704, 97
41065, V, 1, 1, 1, 1, 0, 704, 97
41066, V, 1, 1, 1, 1, 0, 704, 97
41067, V, 1, 1, 1, 1, 0, 704, 97
41068, V, 1, 1, 1, 1, 0, 704, 97
41069, V, 1, 1, 1, 1, 0, 704, 97
41070, V, 1, 1, 1, 1, 0, 704, 97
41071, V, 1, 1, 1, 1, 0, 704, 97
41072, V, 1, 1, 1, 1, 0, 704, 97
41073, V, 1, 1, 1, 1, 0, 704, 98
41074, V, 1, 1, 1, 1, 0, 704, 98
41075, V, 1, 1, 1, 1, 0, 704, 98
41076, V, 1, 1, 1, 1, 0, 704, 98
41077, V, 1, 1, 1, 1, 0, 704, 98
41078, V, 1, 1, 1, 1, 0, 704, 98
41079, V, 1, 1, 1, 1, 0, 704, 98
41080, V, 1, 1, 1, 1, 0, 704, 98
41081, V, 1, 1, 1, 1, 0, 704, 98
41082, V, 1, 1, 1, 1, 0, 704, 98
41083, V, 1, 1, 1, 1, 0, 704, 98
41084, V, 1, 1, 1, 1, 0, 704, 98
41085, V, 1, 1, 1, 1, 0, 704, 98
41086, V, 1, 1, 1, 1, 0, 704, 98
41088, V, 1, 1, 1, 1, 0, 704, 98
41089, V, 1, 1, 1, 1, 0, 704, 98
41090, V, 1, 1, 1, 1, 0, 704, 98
41091, V, 1, 1, 1, 1, 0, 704, 98
41092, V, 1, 1, 1, 1, 0, 704, 98
41093, V, 1, 1, 1, 1, 0, 704, 98
41094, V, 1, 1, 1, 1, 0, 704, 98
41095, V, 1, 1, 1, 1, 0, 704, 98
41096, V, 1, 1, 1, 1, 0, 704, 98
41097, V, 1, 1, 1, 1, 0, 704, 98
41098, V, 1, 1, 1, 1, 0, 704, 98
41099, V, 1, 1, 1, 1, 0, 704, 98
41100, V, 1, 1, 1, 1, 0, 704, 98
41101, V, 1, 1, 1, 1, 0, 704, 98
41102, V, 1, 1, 1, 1, 0, 704, 98
41103, V, 1, 1, 1, 1, 0, 704, 98
41104, V, 1, 1, 1, 1, 0, 704, 98
41105, V, 1, 1, 1, 1, 0, 704, 98
41106, V, 1, 1, 1, 1, 0, 704, 98
41107, V, 1, 1, 1, 1, 0, 704, 98
41108, V, 1, 1, 1, 1, 0, 704, 98
41109, V, 1, 1, 1, 1, 0, 704, 98
41110, V, 1, 1, 1, 1, 0, 704, 98
41111, V, 1, 1, 1, 1, 0, 704, 99
41112, V, 1, 1, 1, 1, 0, 704, 99
41113, V, 1, 1, 1, 1, 0, 704, 99
41114, V, 1, 1, 1, 1, 0, 704, 99
41115, V, 1, 1, 1, 1, 0, 704, 99
41116, V, 1, 1, 1, 1, 0, 704, 99
41117, V, 1, 1, 1, 1, 0, 704, 98
41118, V, 1, 1, 1, 1, 0, 704, 99
41119, V, 1, 1, 1, 1, 0, 704, 99
41120, V, 1, 1, 1, 1, 0, 704, 99
41121, V, 1, 1, 1, 1, 0, 704, 99
41122, V, 1, 1, 1, 1, 0, 704, 99
41123, V, 1, 1, 1, 1, 0, 704, 99
41124, V, 1, 1, 1, 1, 0, 704, 99
41125, V, 1, 1, 1, 1, 0, 704, 99
41126, V, 1, 1, 1, 1, 0, 704, 99
41127, V, 1, 1, 1, 1, 0, 704, 99
41128, V, 1, 1, 1, 1, 0, 704, 99
41129, V, 1, 1, 1, 1, 0, 704, 99
41131, V, 1, 1, 1, 1, 0, 704, 99
41132, V, 1, 1, 1, 1, 0, 704, 99
41133, V, 1, 1, 1, 1, 0, 704, 99
41134, V, 1, 1, 1, 1, 0, 704, 99
41135, V, 1, 1, 1, 1, 0, 704, 99
41136, V, 1, 1, 1, 1, 0, 704, 99
41137, V, 1, 1, 1, 1, 0, 704, 99
41138, V, 1, 1, 1, 1, 0, 704, 99
41139, V, 1, 1, 1, 1, 0, 704, 99
41140, V, 1, 1, 1, 1, 0, 704, 99
41141, V, 1, 1, 1, 1, 0, 704, 99
41142, V, 1, 1, 1, 1, 0, 704, 99
41143, V, 1, 1, 1, 1, 0, 704, 99
41144, V, 1, 1, 1, 1, 0, 704, 99
41145, V, 1, 1, 1, 1, 0, 704, 99
41146, V, 1, 1, 1, 1, 0, 704, 99
41147, V, 1, 1, 1, 1, 0, 704, 99
41148, V, 1, 1, 1, 1, 0, 704, 99
41149, V, 1, 1, 1, 1, 0, 704, 99
41150, V, 1, 1, 1, 1, 0, 704, 99
41151, V, 1, 1, 1, 1, 0, 704, 99
41152, V, 1, 1, 1, 1, 0, 704, 99
41153, V, 1, 1, 1, 1, 0, 704, 99
41154, V, 1, 1, 1, 1, 0, 704, 99
41155, V, 1, 1, 1, 1, 0, 704, 99
41156, V, 1, 1, 1, 1, 0, 704, 99
41157, V, 1, 1, 1, 1, 0, 704, 99
41158, V, 1, 1, 1, 1, 0, 704, 99
41159, V, 1, 1, 1, 1, 0, 704, 99
41160, V, 1, 1, 1, 1, 0, 704, 99
41161, V, 1, 1, 1, 1, 0, 704, 99
41162, V, 1, 1, 1, 1, 0, 704, 99
41163, V, 1, 1, 1, 1, 0, 704, 99
41164, V, 1, 1, 1, 1, 0, 704, 99
41165, V, 1, 1, 1, 1, 0, 704, 99
41166, V, 1, 1, 1, 1, 0, 704, 99
41167, V, 1, 1, 1, 1, 0, 704, 99
41168, V, 1, 1, 1, 1, 0, 704, 99
41169, V, 1, 1, 1, 1, 0, 704, 99
41170, V, 1, 1, 1, 1, 0, 704, 99
41171, V, 1, 1, 1, 1, 0, 704, 99
41172, V, 1, 1, 1, 1, 0, 704, 99
41174, V, 1, 1, 1, 1, 0, 704, 99
41175, V, 1, 1, 1, 1, 0, 704, 99
41176, V, 1, 1, 1, 1, 0, 704, 99
41177, V, 1, 1, 1, 1, 0, 704, 99
41178, V, 1, 1, 1, 1, 0, 704, 99
41179, V, 1, 1, 1, 1, 0, 704, 99
41180, V, 1, 1, 1, 1, 0, 704, 99
41181, V, 1, 1, 1, 1, 0, 704, 99
41182, V, 1, 1, 1, 1, 0, 704, 99
41183, V, 1, 1, 1, 1, 0, 704, 99
41184, V, 1, 1, 1, 1, 0, 704, 99
41185, V, 1, 1, 1, 1, 0, 704, 99
41186, V, 1, 1, 1, 1, 0, 704, 99
41187, V, 1, 1, 1, 1, 0, 704, 99
41188, V, 1, 1, 1, 1, 0, 704, 99
41189, V, 1, 1, 1, 1, 0, 704, 99
41190, V, 1, 1, 1, 1, 0, 704, 99
41191, V, 1, 1, 1, 1, 0, 704, 99
41192, V, 1, 1, 1, 1, 0, 704, 99
41193, V, 1, 1, 1, 1, 0, 704, 99
41194, V, 1, 1, 1, 1, 0, 704, 99
41195, V, 1, 1, 1, 1, 0, 704, 99
41196, V, 1, 1, 1, 1, 0, 704, 99
41197, V, 1, 1, 1, 1, 0, 704, 99
41198, V, 1, 1, 1, 1, 0, 704, 99
41199, V, 1, 1, 1, 1, 0, 704, 99
41200, V, 1, 1, 1, 1, 0, 704, 99
41201, V, 1, 1, 1, 1, 0, 704, 99
41202, V, 1, 1, 1, 1, 0, 704, 99
41203, V, 1, 1, 1, 1, 0, 704, 99
41204, V, 1, 1, 1, 1, 0, 704, 99
41205, V, 1, 1, 1, 1, 0, 704, 99
41206, V, 1, 1, 1, 1, 0, 704, 99
41207, V, 1, 1, 1, 1, 0, 704, 99
41208, V, 1, 1, 1, 1, 0, 704, 99
41209, V, 1, 1, 1, 1, 0, 704, 99
41210, V, 1, 1, 1, 1, 0, 704, 99
41211, V, 1, 1, 1, 1, 0, 704, 99
41212, V, 1, 1, 1, 1, 0, 704, 99
41213, V, 1, 1, 1, 1, 0, 704, 99
41214, V, 1, 1, 1, 1, 0, 704, 99
41216, V, 1, 1, 1, 1, 0, 704, 99
41217, V, 1, 1, 1, 1, 0, 704, 99
41218, V, 1, 1, 1, 1, 0, 704, 99
41219, V, 1, 1, 1, 1, 0, 704, 99
41220, V, 1, 1, 1, 1, 0, 704, 99
41221, V, 1, 1, 1, 1, 0, 704, 99
41222, V, 1, 1, 1, 1, 0, 704, 99
41223, V, 1, 1, 1, 1, 0, 704, 99
41224, V, 1, 1, 1, 1, 0, 704, 99
41225, V, 1, 1, 1, 1, 0, 704, 99
41226, V, 1, 1, 1, 1, 0, 704, 99
41227, V, 1, 1, 1, 1, 0, 704, 99
41228, V, 1, 1, 1, 1, 0, 704, 99
41229, V, 1, 1, 1, 1, 0, 704, 99
41230, V, 1, 1, 1, 1, 0, 704, 99
41231, V, 1, 1, 1, 1, 0, 704, 99
41232, V, 1, 1, 1, 1, 0, 704, 99
41233, V, 1, 1, 1, 1, 0, 704, 99
41234, V, 1, 1, 1, 1, 0, 704, 99
41235, V, 1, 1, 1, 1, 0, 704, 99
41236, V, 1, 1, 1, 1, 0, 704, 99
41237, V, 1, 1, 1, 1, 0, 704, 99
41238, V, 1, 1, 1, 1, 0, 704, 99
41239, V, 1, 1, 1, 1, 0, 704, 99
41240, V, 1, 1, 1, 1, 0, 704, 99
41241, V, 1, 1, 1, 1, 0, 704, 99
41242, V, 1, 1, 1, 1, 0, 704, 99
41243, V, 1, 1, 1, 1, 0, 704, 99
41244, V, 1, 1, 1, 1, 0, 704, 99
41245, V, 1, 1, 1, 1, 0, 704, 99
41246, V, 1, 1, 1, 1, 0, 704, 99
41247, V, 1, 1, 1, 1, 0, 704, 99
41248, V, 1, 1, 1, 1, 0, 704, 99
41249, V, 1, 1, 1, 1, 0, 704, 99
41250, V, 1, 1, 1, 1, 0, 704, 99
41251, V, 1, 1, 1, 1, 0, 704, 99
41252, V, 1, 1, 1, 1, 0, 704, 99
41253, V, 1, 1, 1, 1, 0, 704, 99
41254, V, 1, 1, 1, 1, 0, 704, 99
41255, V, 1, 1, 1, 1, 0, 704, 99
41256, V, 1, 1, 1, 1, 0, 704, 99
41257, V, 1, 1, 1, 1, 0, 704, 99
41259, V, 1, 1, 1, 1, 0, 704, 99
41260, V, 1, 1, 1, 1, 0, 704, 99
41261, V, 1, 1, 1, 1, 0, 704, 99
41262, V, 1, 1, 1, 1, 0, 704, 99
41263, V, 1, 1, 1, 1, 0, 704, 99
41264, V, 1, 1, 1, 1, 0, 704, 99
41265, V, 1, 1, 1, 1, 0, 704, 99
41266, V, 1, 1, 1, 1, 0, 704, 99
41267, V, 1, 1, 1, 1, 0, 704, 99
41268, V, 1, 1, 1, 1, 0, 704, 99
41269, V, 1, 1, 1, 1, 0, 704, 100
41270, V, 1, 1, 1, 1, 0, 704, 100
41271, V, 1, 1, 1, 1, 0, 704, 99
41272, V, 1, 1, 1, 1, 0, 704, 100
41273, V, 1, 1, 1, 1, 0, 704, 100
41274, V, 1, 1, 1, 1, 0, 704, 99
41275, V, 1, 1, 1, 1, 0, 704, 100
41276, V, 1, 1, 1, 1, 0, 704, 100
41277, V, 1, 1, 1, 1, 0, 704, 99
41278, V, 1, 1, 1, 1, 0, 704, 99
41279, V, 1, 1, 1, 1, 0, 704, 99
41280, V, 1, 1, 1, 1, 0, 704, 99
41281, V, 1, 1, 1, 1, 0, 704, 99
41282, V, 1, 1, 1, 1, 0, 704, 99
41283, V, 1, 1, 1, 1, 0, 704, 99
41284, V, 1, 1, 1, 1, 0, 704, 99
41285, V, 1, 1, 1, 1, 0, 704, 99
41286, V, 1, 1, 1, 1, 0, 704, 99
41287, V, 1, 1, 1, 1, 0, 704, 99
41288, V, 1, 1, 1, 1, 0, 704, 99
41289, V, 1, 1, 1, 1, 0, 704, 99
41290, V, 1, 1, 1, 1, 0, 704, 100
41291, V, 1, 1, 1, 1, 0, 704, 99
41292, V, 1, 1, 1, 1, 0, 704, 99
41293, V, 1, 1, 1, 1, 0, 704, 100
41294, V, 1, 1, 1, 1, 0, 704, 99
41295, V, 1, 1, 1, 1, 0, 704, 100
41296, V, 1, 1, 1, 1, 0, 704, 99
41297, V, 1, 1, 1, 1, 0, 704, 99
41298, V, 1, 1, 1, 1, 0, 704, 99
41299, V, 1, 1, 1, 1, 0, 704, 99
41300, V, 1, 1, 1, 1, 0, 704, 100
41302, V, 1, 1, 1, 1, 0, 704, 99
41303, V, 1, 1, 1, 1, 0, 704, 100
41304, V, 1, 1, 1, 1, 0, 704, 99
41305, V, 1, 1, 1, 1, 0, 704, 99
41306, V, 1, 1, 1, 1, 0, 704, 100
41307, V, 1, 1, 1, 1, 0, 704, 100
41308, V, 1, 1, 1, 1, 0, 704, 100
41309, V, 1, 1, 1, 1, 0, 704, 100
41310, V, 1, 1, 1, 1, 0, 704, 100
41311, V, 1, 1, 1, 1, 0, 704, 100
41312, V, 1, 1, 1, 1, 0, 704, 100
41313, V, 1, 1, 1, 1, 0, 704, 100
41314, V, 1, 1, 1, 1, 0, 704, 100
41315, V, 1, 1, 1, 1, 0, 704, 100
41316, V, 1, 1, 1, 1, 0, 704, 100
41317, V, 1, 1, 1, 1, 0, 704, 100
41318, V, 1, 1, 1, 1, 0, 704, 100
41319, V, 1, 1, 1, 1, 0, 704, 100
41320, V, 1, 1, 1, 1, 0, 704, 100
41321, V, 1, 1, 1, 1, 0, 704, 100
41322, V, 1, 1, 1, 1, 0, 704, 100
41323, V, 1, 1, 1, 1, 0, 704, 100
41324, V, 1, 1, 1, 1, 0, 704, 100
41325, V, 1, 1, 1, 1, 0, 704, 100
41326, V, 1, 1, 1, 1, 0, 704, 100
41327, V, 1, 1, 1, 1, 0, 704, 100
41328, V, 1, 1, 1, 1, 0, 704, 100
41329, V, 1, 1, 1, 1, 0, 704, 100
41330, V, 1, 1, 1, 1, 0, 704, 100
41331, V, 1, 1, 1, 1, 0, 704, 100
41332, V, 1, 1, 1, 1, 0, 704, 100
41333, V, 1, 1, 1, 1, 0, 704, 100
41334, V, 1, 1, 1, 1, 0, 704, 100
41335, V, 1, 1, 1, 1, 0, 704, 100
41336, V, 1, 1, 1, 1, 0, 704, 100
41337, V, 1, 1, 1, 1, 0, 704, 100
41338, V, 1, 1, 1, 1, 0, 704, 100
41339, V, 1, 1, 1, 1, 0, 704, 100
41340, V, 1, 1, 1, 1, 0, 704, 100
41341, V, 1, 1, 1, 1, 0, 704, 100
41342, V, 1, 1, 1, 1, 0, 704, 100
41344, V, 1, 1, 1, 1, 0, 704, 100
41345, V, 1, 1, 1, 1, 0, 704, 100
41346, V, 1, 1, 1, 1, 0, 704, 100
41347, V, 1, 1, 1, 1, 0, 704, 100
41348, V, 1, 1, 1, 1, 0, 704, 100
41349, V, 1, 1, 1, 1, 0, 704, 100
41350, V, 1, 1, 1, 1, 0, 704, 100
41351, V, 1, 1, 1, 1, 0, 704, 100
41352, V, 1, 1, 1, 1, 0, 704, 100
41353, V, 1, 1, 1, 1, 0, 704, 100
41354, V, 1, 1, 1, 1, 0, 704, 100
41355, V, 1, 1, 1, 1, 0, 704, 100
41356, V, 1, 1, 1, 1, 0, 704, 100
41357, V, 1, 1, 1, 1, 0, 704, 100
41358, V, 1, 1, 1, 1, 0, 704, 100
41359, V, 1, 1, 1, 1, 0, 704, 100
41360, V, 1, 1, 1, 1, 0, 704, 100
41361, V, 1, 1, 1, 1, 0, 704, 100
41362, V, 1, 1, 1, 1, 0, 704, 100
41363, V, 1, 1, 1, 1, 0, 704, 100
41364, V, 1, 1, 1, 1, 0, 704, 100
41365, V, 1, 1, 1, 1, 0, 704, 100
41366, V, 1, 1, 1, 1, 0, 704, 100
41367, V, 1, 1, 1, 1, 0, 704, 100
41368, V, 1, 1, 1, 1, 0, 704, 100
41369, V, 1, 1, 1, 1, 0, 704, 100
41370, V, 1, 1, 1, 1, 0, 704, 100
41371, V, 1, 1, 1, 1, 0, 704, 100
41372, V, 1, 1, 1, 1, 0, 704, 100
41373, V, 1, 1, 1, 1, 0, 704, 100
41374, V, 1, 1, 1, 1, 0, 704, 100
41375, V, 1, 1, 1, 1, 0, 704, 100
41376, V, 1, 1, 1, 1, 0, 704, 100
41377, V, 1, 1, 1, 1, 0, 704, 100
41378, V, 1, 1, 1, 1, 0, 704, 100
41379, V, 1, 1, 1, 1, 0, 704, 100
41380, V, 1, 1, 1, 1, 0, 704, 100
41381, V, 1, 1, 1, 1, 0, 704, 100
41382, V, 1, 1, 1, 1, 0, 704, 100
41383, V, 1, 1, 1, 1, 0, 704, 100
41384, V, 1, 1, 1, 1, 0, 704, 100
41385, V, 1, 1, 1, 1, 0, 704, 100
41387, V, 1, 1, 1, 1, 0, 704, 100
41388, V, 1, 1, 1, 1, 0, 704, 100
41389, V, 1, 1, 1, 1, 0, 704, 100
41390, V, 1, 1, 1, 1, 0, 704, 100
41391, V, 1, 1, 1, 1, 0, 704, 100
41392, V, 1, 1, 1, 1, 0, 704, 100
41393, V, 1, 1, 1, 1, 0, 704, 100
41394, V, 1, 1, 1, 1, 0, 704, 100
41395, V, 1, 1, 1, 1, 0, 704, 100
41396, V, 1, 1, 1, 1, 0, 704, 100
41397, V, 1, 1, 1, 1, 0, 704, 100
41398, V, 1, 1, 1, 1, 0, 704, 100
41399, V, 1, 1, 1, 1, 0, 704, 100
41400, V, 1, 1, 1, 1, 0, 704, 100
41401, V, 1, 1, 1, 1, 0, 704, 100
41402, V, 1, 1, 1, 1, 0, 704, 100
41403, V, 1, 1, 1, 1, 0, 704, 100
41404, V, 1, 1, 1, 1, 0, 704, 100
41405, V, 1, 1, 1, 1, 0, 704, 100
41406, V, 1, 1, 1, 1, 0, 704, 100
41407, V, 1, 1, 1, 1, 0, 704, 100
41408, V, 1, 1, 1, 1, 0, 704, 100
41409, V, 1, 1, 1, 1, 0, 704, 100
41410, V, 1, 1, 1, 1, 0, 704, 100
41411, V, 1, 1, 1, 1, 0, 704, 100
41412, V, 1, 1, 1, 1, 0, 704, 100
41413, V, 1, 1, 1, 1, 0, 704, 100
41414, V, 1, 1, 1, 1, 0, 704, 100
41415, V, 1, 1, 1, 1, 0, 704, 100
41416, V, 1, 1, 1, 1, 0, 704, 100
41417, V, 1, 1, 1, 1, 0, 704, 100
41418, V, 1, 1, 1, 1, 0, 704, 100
41419, V, 1, 1, 1, 1, 0, 704, 100
41420, V, 1, 1, 1, 1, 0, 704, 100
41421, V, 1, 1, 1, 1, 0, 704, 100
41422, V, 1, 1, 1, 1, 0, 704, 100
41423, V, 1, 1, 1, 1, 0, 704, 100
41424, V, 1, 1, 1, 1, 0, 704, 100
41425, V, 1, 1, 1, 1, 0, 704, 100
41426, V, 1, 1, 1, 1, 0, 704, 100
41427, V, 1, 1, 1, 1, 0, 704, 100
41428, V, 1, 1, 1, 1, 0, 704, 100
41430, V, 1, 1, 1, 1, 0, 704, 100
41431, V, 1, 1, 1, 1, 0, 704, 100
41432, V, 1, 1, 1, 1, 0, 704, 100
41433, V, 1, 1, 1, 1, 0, 704, 100
41434, V, 1, 1, 1, 1, 0, 704, 100
41435, V, 1, 1, 1, 1, 0, 704, 100
41436, V, 1, 1, 1, 1, 0, 704, 100
41437, V, 1, 1, 1, 1, 0, 704, 100
41438, V, 1, 1, 1, 1, 0, 704, 100
41439, V, 1, 1, 1, 1, 0, 704, 100
41440, V, 1, 1, 1, 1, 0, 704, 100
41441, V, 1, 1, 1, 1, 0, 704, 100
41442, V, 1, 1, 1, 1, 0, 704, 100
41443, V, 1, 1, 1, 1, 0, 704, 100
41444, V, 1, 1, 1, 1, 0, 704, 100
41445, V, 1, 1, 1, 1, 0, 704, 100
41446, V, 1, 1, 1, 1, 0, 704, 100
41447, V, 1, 1, 1, 1, 0, 704, 100
41448, V, 1, 1, 1, 1, 0, 704, 100
41449, V, 1, 1, 1, 1, 0, 704, 100
41450, V, 1, 1, 1, 1, 0, 704, 100
41451, V, 1, 1, 1, 1, 0, 704, 100
41452, V, 1, 1, 1, 1, 0, 704, 100
41453, V, 1, 1, 1, 1, 0, 704, 100
41454, V, 1, 1, 1, 1, 0, 704, 100
41455, V, 1, 1, 1, 1, 0, 704, 100
41456, V, 1, 1, 1, 1, 0, 704, 100
41457, V, 1, 1, 1, 1, 0, 704, 100
41458, V, 1, 1, 1, 1, 0, 704, 100
41459, V, 1, 1, 1, 1, 0, 704, 100
41460, V, 1, 1, 1, 1, 0, 704, 100
41461, V, 1, 1, 1, 1, 0, 704, 100
41462, V, 1, 1, 1, 1, 0, 704, 100
41463, V, 1, 1, 1, 1, 0, 704, 100
41464, V, 1, 1, 1, 1, 0, 704, 100
41465, V, 1, 1, 1, 1, 0, 704, 100
41466, V, 1, 1, 1, 1, 0, 704, 100
41467, V, 1, 1, 1, 1, 0, 704, 100
41468, V, 1, 1, 1, 1, 0, 704, 100
41469, V, 1, 1, 1, 1, 0, 704, 100
41470, V, 1, 1, 1, 1, 0, 704, 100
41472, V, 1, 1, 1, 1, 0, 704, 100
41473, V, 1, 1, 1, 1, 0, 704, 100
41474, V, 1, 1, 1, 1, 0, 704, 100
41475, V, 1, 1, 1, 1, 0, 704, 100
41476, V, 1, 1, 1, 1, 0, 704, 100
41477, V, 1, 1, 1, 1, 0, 704, 100
41478, V, 1, 1, 1, 1, 0, 704, 100
41479, V, 1, 1, 1, 1, 0, 704, 100
41480, V, 1, 1, 1, 1, 0, 704, 100
41481, V, 1, 1, 1, 1, 0, 704, 100
41482, V, 1, 1, 1, 1, 0, 704, 100
41483, V, 1, 1, 1, 1, 0, 704, 100
41484, V, 1, 1, 1, 1, 0, 704, 100
41485, V, 1, 1, 1, 1, 0, 704, 100
41486, V, 1, 1, 1, 1, 0, 704, 100
41487, V, 1, 1, 1, 1, 0, 704, 100
41488, V, 1, 1, 1, 1, 0, 704, 100
41489, V, 1, 1, 1, 1, 0, 704, 100
41490, V, 1, 1, 1, 1, 0, 704, 100
41491, V, 1, 1, 1, 1, 0, 704, 100
41492, V, 1, 1, 1, 1, 0, 704, 100
41493, V, 1, 1, 1, 1, 0, 704, 100
41494, V, 1, 1, 1, 1, 0, 704, 100
41495, V, 1, 1, 1, 1, 0, 704, 100
41496, V, 1, 1, 1, 1, 0, 704, 100
41497, V, 1, 1, 1, 1, 0, 704, 100
41498, V, 1, 1, 1, 1, 0, 704, 100
41499, V, 1, 1, 1, 1, 0, 704, 100
41500, V, 1, 1, 1, 1, 0, 704, 100
41501, V, 1, 1, 1, 1, 0, 704, 100
41502, V, 1, 1, 1, 1, 0, 704, 100
41503, V, 1, 1, 1, 1, 0, 704, 100
41504, V, 1, 1, 1, 1, 0, 704, 100
41505, V, 1, 1, 1, 1, 0, 704, 100
41506, V, 1, 1, 1, 1, 0, 704, 100
41507, V, 1, 1, 1, 1, 0, 704, 100
41508, V, 1, 1, 1, 1, 0, 704, 100
41509, V, 1, 1, 1, 1, 0, 704, 100
41510, V, 1, 1, 1, 1, 0, 704, 100
41511, V, 1, 1, 1, 1, 0, 704, 100
41512, V, 1, 1, 1, 1, 0, 704, 100
41513, V, 1, 1, 1, 1, 0, 704, 100
41515, V, 1, 1, 1, 1, 0, 704, 100
41516, V, 1, 1, 1, 1, 0, 704, 100
41517, V, 1, 1, 1, 1, 0, 704, 100
41518, V, 1, 1, 1, 1, 0, 704, 100
41519, V, 1, 1, 1, 1, 0, 704, 100
41520, V, 1, 1, 1, 1, 0, 704, 100
41521, V, 1, 1, 1, 1, 0, 704, 100
41522, V, 1, 1, 1, 1, 0, 704, 100
41523, V, 1, 1, 1, 1, 0, 704, 100
41524, V, 1, 1, 1, 1, 0, 704, 100
41525, V, 1, 1, 1, 1, 0, 704, 100
41526, V, 1, 1, 1, 1, 0, 704, 100
41527, V, 1, 1, 1, 1, 0, 704, 100
41528, V, 1, 1, 1, 1, 0, 704, 100
41529, V, 1, 1, 1, 1, 0, 704, 100
41530, V, 1, 1, 1, 1, 0, 704, 100
41531, V, 1, 1, 1, 1, 0, 704, 100
41532, V, 1, 1, 1, 1, 0, 704, 100
41533, V, 1, 1, 1, 1, 0, 704, 100
41534, V, 1, 1, 1, 1, 0, 704, 100
41535, V, 1, 1, 1, 1, 0, 704, 100
41536, V, 1, 1, 1, 1, 0, 704, 100
41537, V, 1, 1, 1, 1, 0, 704, 100
41538, V, 1, 1, 1, 1, 0, 704, 100
41539, V, 1, 1, 1, 1, 0, 704, 100
41540, V, 1, 1, 1, 1, 0, 704, 100
41541, V, 1, 1, 1, 1, 0, 704, 100
41542, V, 1, 1, 1, 1, 0, 704, 100
41543, V, 1, 1, 1, 1, 0, 704, 100
41544, V, 1, 1, 1, 1, 0, 704, 100
41545, V, 1, 1, 1, 1, 0, 704, 100
41546, V, 1, 1, 1, 1, 0, 704, 100
41547, V, 1, 1, 1, 1, 0, 704, 100
41548, V, 1, 1, 1, 1, 0, 704, 100
41549, V, 1, 1, 1, 1, 0, 704, 100
41550, V, 1, 1, 1, 1, 0, 704, 100
41551, V, 1, 1, 1, 1, 0, 704, 100
41552, V, 1, 1, 1, 1, 0, 704, 100
41553, V, 1, 1, 1, 1, 0, 704, 100
41554, V, 1, 1, 1, 1, 0, 704, 100
41555, V, 1, 1, 1, 1, 0, 704, 100
41556, V, 1, 1, 1, 1, 0, 704, 100
41558, V, 1, 1, 1, 1, 0, 704, 100
41559, V, 1, 1, 1, 1, 0, 704, 100
41560, V, 1, 1, 1, 1, 0, 704, 100
41561, V, 1, 1, 1, 1, 0, 704, 100
41562, V, 1, 1, 1, 1, 0, 704, 100
41563, V, 1, 1, 1, 1, 0, 704, 100
41564, V, 1, 1, 1, 1, 0, 704, 100
41565, V, 1, 1, 1, 1, 0, 704, 100
41566, V, 1, 1, 1, 1, 0, 704, 100
41567, V, 1, 1, 1, 1, 0, 704, 100
41568, V, 1, 1, 1, 1, 0, 704, 100
41569, V, 1, 1, 1, 1, 0, 704, 100
41570, V, 1, 1, 1, 1, 0, 704, 100
41571, V, 1, 1, 1, 1, 0, 704, 100
41572, V, 1, 1, 1, 1, 0, 704, 100
41573, V, 1, 1, 1, 1, 0, 704, 100
41574, V, 1, 1, 1, 1, 0, 704, 100
41575, V, 1, 1, 1, 1, 0, 704, 100
41576, V, 1, 1, 1, 1, 0, 704, 100
41577, V, 1, 1, 1, 1, 0, 704, 100
41578, V, 1, 1, 1, 1, 0, 704, 100
41579, V, 1, 1, 1, 1, 0, 704, 100
41580, V, 1, 1, 1, 1, 0, 704, 100
41581, V, 1, 1, 1, 1, 0, 704, 100
41582, V, 1, 1, 1, 1, 0, 704, 100
41583, V, 1, 1, 1, 1, 0, 704, 100
41584, V, 1, 1, 1, 1, 0, 704, 100
41585, V, 1, 1, 1, 1, 0, 704, 100
41586, V, 1, 1, 1, 1, 0, 704, 100
41587, V, 1, 1, 1, 1, 0, 704, 100
41588, V, 1, 1, 1, 1, 0, 704, 100
41589, V, 1, 1, 1, 1, 0, 704, 100
41590, V, 1, 1, 1, 1, 0, 704, 100
41591, V, 1, 1, 1, 1, 0, 704, 100
41592, V, 1, 1, 1, 1, 0, 704, 100
41593, V, 1, 1, 1, 1, 0, 704, 100
41594, V, 1, 1, 1, 1, 0, 704, 100
41595, V, 1, 1, 1, 1, 0, 704, 100
41596, V, 1, 1, 1, 1, 0, 704, 100
41597, V, 1, 1, 1, 1, 0, 704, 100
41598, V, 1, 1, 1, 1, 0, 704, 100
41600, V, 1, 1, 1, 1, 0, 704, 100
41601, V, 1, 1, 1, 1, 0, 704, 100
41602, V, 1, 1, 1, 1, 0, 704, 100
41603, V, 1, 1, 1, 1, 0, 704, 100
41604, V, 1, 1, 1, 1, 0, 704, 100
41605, V, 1, 1, 1, 1, 0, 704, 100
41606, V, 1, 1, 1, 1, 0, 704, 100
41607, V, 1, 1, 1, 1, 0, 704, 100
41608, V, 1, 1, 1, 1, 0, 704, 100
41609, V, 1, 1, 1, 1, 0, 704, 100
41610, V, 1, 1, 1, 1, 0, 704, 100
41611, V, 1, 1, 1, 1, 0, 704, 100
41612, V, 1, 1, 1, 1, 0, 704, 100
41613, V, 1, 1, 1, 1, 0, 704, 100
41614, V, 1, 1, 1, 1, 0, 704, 100
41615, V, 1, 1, 1, 1, 0, 704, 100
41616, V, 1, 1, 1, 1, 0, 704, 100
41617, V, 1, 1, 1, 1, 0, 704, 100
41618, V, 1, 1, 1, 1, 0, 704, 100
41619, V, 1, 1, 1, 1, 0, 704, 100
41620, V, 1, 1, 1, 1, 0, 704, 100
41621, V, 1, 1, 1, 1, 0, 704, 100
41622, V, 1, 1, 1, 1, 0, 704, 100
41623, V, 1, 1, 1, 1, 0, 704, 100
41624, V, 1, 1, 1, 1, 0, 704, 100
41625, V, 1, 1, 1, 1, 0, 704, 100
41626, V, 1, 1, 1, 1, 0, 704, 100
41627, V, 1, 1, 1, 1, 0, 704, 100
41628, V, 1, 1, 1, 1, 0, 704, 100
41629, V, 1, 1, 1, 1, 0, 704, 100
41630, V, 1, 1, 1, 1, 0, 704, 100
41631, V, 1, 1, 1, 1, 0, 704, 100
41632, V, 1, 1, 1, 1, 0, 704, 100
41633, V, 1, 1, 1, 1, 0, 704, 100
41634, V, 1, 1, 1, 1, 0, 704, 100
41635, V, 1, 1, 1, 1, 0, 704, 100
41636, V, 1, 1, 1, 1, 0, 704, 100
41637, V, 1, 1, 1, 1, 0, 704, 100
41638, V, 1, 1, 1, 1, 0, 704, 100
41639, V, 1, 1, 1, 1, 0, 704, 100
41640, V, 1, 1, 1, 1, 0, 704, 100
41641, V, 1, 1, 1, 1, 0, 704, 100
41643, V, 1, 1, 1, 1, 0, 704, 100
41644, V, 1, 1, 1, 1, 0, 704, 100
41645, V, 1, 1, 1, 1, 0, 704, 100
41646, V, 1, 1, 1, 1, 0, 704, 100
41647, V, 1, 1, 1, 1, 0, 704, 100
41648, V, 1, 1, 1, 1, 0, 704, 100
41649, V, 1, 1, 1, 1, 0, 704, 100
41650, V, 1, 1, 1, 1, 0, 704, 100
41651, V, 1, 1, 1, 1, 0, 704, 100
41652, V, 1, 1, 1, 1, 0, 704, 100
41653, V, 1, 1, 1, 1, 0, 704, 100
41654, V, 1, 1, 1, 1, 0, 704, 100
41655, V, 1, 1, 1, 1, 0, 704, 100
41656, V, 1, 1, 1, 1, 0, 704, 100
41657, V, 1, 1, 1, 1, 0, 704, 100
41658, V, 1, 1, 1, 1, 0, 704, 100
41659, V, 1, 1, 1, 1, 0, 704, 100
41660, V, 1, 1, 1, 1, 0, 704, 100
41661, V, 1, 1, 1, 1, 0, 704, 100
41662, V, 1, 1, 1, 1, 0, 704, 100
41663, V, 1, 1, 1, 1, 0, 704, 100
41664, V, 1, 1, 1, 1, 0, 704, 99
41665, V, 1, 1, 1, 1, 0, 704, 99
41666, V, 1, 1, 1, 1, 0, 704, 99
41667, V, 1, 1, 1, 1, 0, 704, 99
41668, V, 1, 1, 1, 1, 0, 704, 99
41669, V, 1, 1, 1, 1, 0, 704, 99
41670, V, 1, 1, 1, 1, 0, 704, 99
41671, V, 1, 1, 1, 1, 0, 704, 99
41672, V, 1, 1, 1, 1, 0, 704, 99
41673, V, 1, 1, 1, 1, 0, 704, 99
41674, V, 1, 1, 1, 1, 0, 704, 99
41675, V, 1, 1, 1, 1, 0, 704, 99
41676, V, 1, 1, 1, 1, 0, 704, 99
41677, V, 1, 1, 1, 1, 0, 704, 99
41678, V, 1, 1, 1, 1, 0, 704, 99
41679, V, 1, 1, 1, 1, 0, 704, 99
41680, V, 1, 1, 1, 1, 0, 704, 99
41681, V, 1, 1, 1, 1, 0, 704, 99
41682, V, 1, 1, 1, 1, 0, 704, 99
41683, V, 1, 1, 1, 1, 0, 704, 99
41684, V, 1, 1, 1, 1, 0, 704, 99
41686, V, 1, 1, 1, 1, 0, 704, 99
41687, V, 1, 1, 1, 1, 0, 704, 99
41688, V, 1, 1, 1, 1, 0, 704, 99
41689, V, 1, 1, 1, 1, 0, 704, 99
41690, V, 1, 1, 1, 1, 0, 704, 99
41691, V, 1, 1, 1, 1, 0, 704, 99
41692, V, 1, 1, 1, 1, 0, 704, 99
41693, V, 1, 1, 1, 1, 0, 704, 99
41694, V, 1, 1, 1, 1, 0, 704, 99
41695, V, 1, 1, 1, 1, 0, 704, 99
41696, V, 1, 1, 1, 1, 0, 704, 99
41697, V, 1, 1, 1, 1, 0, 704, 99
41698, V, 1, 1, 1, 1, 0, 704, 99
41699, V, 1, 1, 1, 1, 0, 704, 99
41700, V, 1, 1, 1, 1, 0, 704, 99
41701, V, 1, 1, 1, 1, 0, 704, 99
41702, V, 1, 1, 1, 1, 0, 704, 99
41703, V, 1, 1, 1, 1, 0, 704, 99
41704, V, 1, 1, 1, 1, 0, 704, 99
41705, V, 1, 1, 1, 1, 0, 704, 99
41706, V, 1, 1, 1, 1, 0, 704, 99
41707, V, 1, 1, 1, 1, 0, 704, 99
41708, V, 1, 1, 1, 1, 0, 704, 99
41709, V, 1, 1, 1, 1, 0, 704, 99
41710, V, 1, 1, 1, 1, 0, 704, 99
41711, V, 1, 1, 1, 1, 0, 704, 99
41712, V, 1, 1, 1, 1, 0, 704, 99
41713, V, 1, 1, 1, 1, 0, 704, 99
41714, V, 1, 1, 1, 1, 0, 704, 99
41715, V, 1, 1, 1, 1, 0, 704, 99
41716, V, 1, 1, 1, 1, 0, 704, 99
41717, V, 1, 1, 1, 1, 0, 704, 99
41718, V, 1, 1, 1, 1, 0, 704, 99
41719, V, 1, 1, 1, 1, 0, 704, 99
41720, V, 1, 1, 1, 1, 0, 704, 99
41721, V, 1, 1, 1, 1, 0, 704, 99
41722, V, 1, 1, 1, 1, 0, 704, 99
41723, V, 1, 1, 1, 1, 0, 704, 99
41724, V, 1, 1, 1, 1, 0, 704, 99
41725, V, 1, 1, 1, 1, 0, 704, 99
41726, V, 1, 1, 1, 1, 0, 704, 99
41728, V, 1, 1, 1, 1, 0, 704, 99
41729, V, 1, 1, 1, 1, 0, 704, 99
41730, V, 1, 1, 1, 1, 0, 704, 99
41731, V, 1, 1, 1, 1, 0, 704, 99
41732, V, 1, 1, 1, 1, 0, 704, 99
41733, V, 1, 1, 1, 1, 0, 704, 99
41734, V, 1, 1, 1, 1, 0, 704, 99
41735, V, 1, 1, 1, 1, 0, 704, 99
41736, V, 1, 1, 1, 1, 0, 704, 99
41737, V, 1, 1, 1, 1, 0, 704, 99
41738, V, 1, 1, 1, 1, 0, 704, 99
41739, V, 1, 1, 1, 1, 0, 704, 99
41740, V, 1, 1, 1, 1, 0, 704, 99
41741, V, 1, 1, 1, 1, 0, 704, 99
41742, V, 1, 1, 1, 1, 0, 704, 99
41743, V, 1, 1, 1, 1, 0, 704, 99
41744, V, 1, 1, 1, 1, 0, 704, 99
41745, V, 1, 1, 1, 1, 0, 704, 99
41746, V, 1, 1, 1, 1, 0, 704, 99
41747, V, 1, 1, 1, 1, 0, 704, 99
41748, V, 1, 1, 1, 1, 0, 704, 99
41749, V, 1, 1, 1, 1, 0, 704, 99
41750, V, 1, 1, 1, 1, 0, 704, 99
41751, V, 1, 1, 1, 1, 0, 704, 99
41752, V, 1, 1, 1, 1, 0, 704, 99
41753, V, 1, 1, 1, 1, 0, 704, 99
41754, V, 1, 1, 1, 1, 0, 704, 99
41755, V, 1, 1, 1, 1, 0, 704, 99
41756, V, 1, 1, 1, 1, 0, 704, 99
41757, V, 1, 1, 1, 1, 0, 704, 99
41758, V, 1, 1, 1, 1, 0, 704, 99
41759, V, 1, 1, 1, 1, 0, 704, 99
41760, V, 1, 1, 1, 1, 0, 704, 99
41761, V, 1, 1, 1, 1, 0, 704, 99
41762, V, 1, 1, 1, 1, 0, 704, 99
41763, V, 1, 1, 1, 1, 0, 704, 99
41764, V, 1, 1, 1, 1, 0, 704, 99
41765, V, 1, 1, 1, 1, 0, 704, 99
41766, V, 1, 1, 1, 1, 0, 704, 99
41767, V, 1, 1, 1, 1, 0, 704, 99
41768, V, 1, 1, 1, 1, 0, 704, 99
41769, V, 1, 1, 1, 1, 0, 704, 99
41771, V, 1, 1, 1, 1, 0, 704, 99
41772, V, 1, 1, 1, 1, 0, 704, 99
41773, V, 1, 1, 1, 1, 0, 704, 99
41774, V, 1, 1, 1, 1, 0, 704, 99
41775, V, 1, 1, 1, 1, 0, 704, 99
41776, V, 1, 1, 1, 1, 0, 704, 99
41777, V, 1, 1, 1, 1, 0, 704, 99
41778, V, 1, 1, 1, 1, 0, 704, 99
41779, V, 1, 1, 1, 1, 0, 704, 100
41780, V, 1, 1, 1, 1, 0, 704, 100
41781, V, 1, 1, 1, 1, 0, 704, 100
41782, V, 1, 1, 1, 1, 0, 704, 100
41783, V, 1, 1, 1, 1, 0, 704, 100
41784, V, 1, 1, 1, 1, 0, 704, 100
41785, V, 1, 1, 1, 1, 0, 704, 100
41786, V, 1, 1, 1, 1, 0, 704, 100
41787, V, 1, 1, 1, 1, 0, 704, 100
41788, V, 1, 1, 1, 1, 0, 704, 100
41789, V, 1, 1, 1, 1, 0, 704, 100
41790, V, 1, 1, 1, 1, 0, 704, 100
41791, V, 1, 1, 1, 1, 0, 704, 100
41792, V, 1, 1, 1, 1, 0, 704, 100
41793, V, 1, 1, 1, 1, 0, 704, 100
41794, V, 1, 1, 1, 1, 0, 704, 100
41795, V, 1, 1, 1, 1, 0, 704, 100
41796, V, 1, 1, 1, 1, 0, 704, 100
41797, V, 1, 1, 1, 1, 0, 704, 100
41798, V, 1, 1, 1, 1, 0, 704, 100
41799, V, 1, 1, 1, 1, 0, 704, 100
41800, V, 1, 1, 1, 1, 0, 704, 100
41801, V, 1, 1, 1, 1, 0, 704, 100
41802, V, 1, 1, 1, 1, 0, 704, 100
41803, V, 1, 1, 1, 1, 0, 704, 100
41804, V, 1, 1, 1, 1, 0, 704, 100
41805, V, 1, 1, 1, 1, 0, 704, 100
41806, V, 1, 1, 1, 1, 0, 704, 100
41807, V, 1, 1, 1, 1, 0, 704, 100
41808, V, 1, 1, 1, 1, 0, 704, 100
41809, V, 1, 1, 1, 1, 0, 704, 100
41810, V, 1, 1, 1, 1, 0, 704, 100
41811, V, 1, 1, 1, 1, 0, 704, 100
41812, V, 1, 1, 1, 1, 0, 704, 100
41814, V, 1, 1, 1, 1, 0, 704, 100
41815, V, 1, 1, 1, 1, 0, 704, 100
41816, V, 1, 1, 1, 1, 0, 704, 100
41817, V, 1, 1, 1, 1, 0, 704, 100
41818, V, 1, 1, 1, 1, 0, 704, 100
41819, V, 1, 1, 1, 1, 0, 704, 100
41820, V, 1, 1, 1, 1, 0, 704, 100
41821, V, 1, 1, 1, 1, 0, 704, 100
41822, V, 1, 1, 1, 1, 0, 704, 100
41823, V, 1, 1, 1, 1, 0, 704, 99
41824, V, 1, 1, 1, 1, 0, 704, 100
41825, V, 1, 1, 1, 1, 0, 704, 100
41826, V, 1, 1, 1, 1, 0, 704, 100
41827, V, 1, 1, 1, 1, 0, 704, 100
41828, V, 1, 1, 1, 1, 0, 704, 99
41829, V, 1, 1, 1, 1, 0, 704, 100
41830, V, 1, 1, 1, 1, 0, 704, 99
41831, V, 1, 1, 1, 1, 0, 704, 100
41832, V, 1, 1, 1, 1, 0, 704, 100
41833, V, 1, 1, 1, 1, 0, 704, 100
41834, V, 1, 1, 1, 1, 0, 704, 100
41835, V, 1, 1, 1, 1, 0, 704, 99
41836, V, 1, 1, 1, 1, 0, 704, 99
41837, V, 1, 1, 1, 1, 0, 704, 100
41838, V, 1, 1, 1, 1, 0, 704, 99
41839, V, 1, 1, 1, 1, 0, 704, 100
41840, V, 1, 1, 1, 1, 0, 704, 100
41841, V, 1, 1, 1, 1, 0, 704, 99
41842, V, 1, 1, 1, 1, 0, 704, 100
41843, V, 1, 1, 1, 1, 0, 704, 100
41844, V, 1, 1, 1, 1, 0, 704, 100
41845, V, 1, 1, 1, 1, 0, 704, 100
41846, V, 1, 1, 1, 1, 0, 704, 100
41847, V, 1, 1, 1, 1, 0, 704, 100
41848, V, 1, 1, 1, 1, 0, 704, 100
41849, V, 1, 1, 1, 1, 0, 704, 100
41850, V, 1, 1, 1, 1, 0, 704, 100
41851, V, 1, 1, 1, 1, 0, 704, 100
41852, V, 1, 1, 1, 1, 0, 704, 100
41853, V, 1, 1, 1, 1, 0, 704, 100
41854, V, 1, 1, 1, 1, 0, 704, 100
41856, V, 1, 1, 1, 1, 0, 704, 100
41857, V, 1, 1, 1, 1, 0, 704, 100
41858, V, 1, 1, 1, 1, 0, 704, 100
41859, V, 1, 1, 1, 1, 0, 704, 100
41860, V, 1, 1, 1, 1, 0, 704, 100
41861, V, 1, 1, 1, 1, 0, 704, 100
41862, V, 1, 1, 1, 1, 0, 704, 100
41863, V, 1, 1, 1, 1, 0, 704, 100
41864, V, 1, 1, 1, 1, 0, 704, 100
41865, V, 1, 1, 1, 1, 0, 704, 100
41866, V, 1, 1, 1, 1, 0, 704, 100
41867, V, 1, 1, 1, 1, 0, 704, 100
41868, V, 1, 1, 1, 1, 0, 704, 100
41869, V, 1, 1, 1, 1, 0, 704, 100
41870, V, 1, 1, 1, 1, 0, 704, 100
41871, V, 1, 1, 1, 1, 0, 704, 100
41872, V, 1, 1, 1, 1, 0, 704, 100
41873, V, 1, 1, 1, 1, 0, 704, 100
41874, V, 1, 1, 1, 1, 0, 704, 100
41875, V, 1, 1, 1, 1, 0, 704, 100
41876, V, 1, 1, 1, 1, 0, 704, 100
41877, V, 1, 1, 1, 1, 0, 704, 100
41878, V, 1, 1, 1, 1, 0, 704, 100
41879, V, 1, 1, 1, 1, 0, 704, 100
41880, V, 1, 1, 1, 1, 0, 704, 100
41881, V, 1, 1, 1, 1, 0, 704, 100
41882, V, 1, 1, 1, 1, 0, 704, 100
41883, V, 1, 1, 1, 1, 0, 704, 100
41884, V, 1, 1, 1, 1, 0, 704, 100
41885, V, 1, 1, 1, 1, 0, 704, 100
41886, V, 1, 1, 1, 1, 0, 704, 100
41887, V, 1, 1, 1, 1, 0, 704, 100
41888, V, 1, 1, 1, 1, 0, 704, 100
41889, V, 1, 1, 1, 1, 0, 704, 100
41890, V, 1, 1, 1, 1, 0, 704, 100
41891, V, 1, 1, 1, 1, 0, 704, 100
41892, V, 1, 1, 1, 1, 0, 704, 100
41893, V, 1, 1, 1, 1, 0, 704, 99
41894, V, 1, 1, 1, 1, 0, 704, 100
41895, V, 1, 1, 1, 1, 0, 704, 100
41896, V, 1, 1, 1, 1, 0, 704, 99
41897, V, 1, 1, 1, 1, 0, 704, 100
41899, V, 1, 1, 1, 1, 0, 704, 99
41900, V, 1, 1, 1, 1, 0, 704, 100
41901, V, 1, 1, 1, 1, 0, 704, 99
41902, V, 1, 1, 1, 1, 0, 704, 100
41903, V, 1, 1, 1, 1, 0, 704, 99
41904, V, 1, 1, 1, 1, 0, 704, 99
41905, V, 1, 1, 1, 1, 0, 704, 99
41906, V, 1, 1, 1, 1, 0, 704, 99
41907, V, 1, 1, 1, 1, 0, 704, 99
41908, V, 1, 1, 1, 1, 0, 704, 99
41909, V, 1, 1, 1, 1, 0, 704, 99
41910, V, 1, 1, 1, 1, 0, 704, 99
41911, V, 1, 1, 1, 1, 0, 704, 99
41912, V, 1, 1, 1, 1, 0, 704, 99
41913, V, 1, 1, 1, 1, 0, 704, 99
41914, V, 1, 1, 1, 1, 0, 704, 99
41915, V, 1, 1, 1, 1, 0, 704, 99
41916, V, 1, 1, 1, 1, 0, 704, 99
41917, V, 1, 1, 1, 1, 0, 704, 99
41918, V, 1, 1, 1, 1, 0, 704, 99
41919, V, 1, 1, 1, 1, 0, 704, 99
41920, V, 1, 1, 1, 1, 0, 704, 99
41921, V, 1, 1, 1, 1, 0, 704, 99
41922, V, 1, 1, 1, 1, 0, 704, 99
41923, V, 1, 1, 1, 1, 0, 704, 100
41924, V, 1, 1, 1, 1, 0, 704, 99
41925, V, 1, 1, 1, 1, 0, 704, 99
41926, V, 1, 1, 1, 1, 0, 704, 99
41927, V, 1, 1, 1, 1, 0, 704, 99
41928, V, 1, 1, 1, 1, 0, 704, 99
41929, V, 1, 1, 1, 1, 0, 704, 99
41930, V, 1, 1, 1, 1, 0, 704, 100
41931, V, 1, 1, 1, 1, 0, 704, 99
41932, V, 1, 1, 1, 1, 0, 704, 100
41933, V, 1, 1, 1, 1, 0, 704, 100
41934, V, 1, 1, 1, 1, 0, 704, 99
41935, V, 1, 1, 1, 1, 0, 704, 100
41936, V, 1, 1, 1, 1, 0, 704, 100
41937, V, 1, 1, 1, 1, 0, 704, 100
41938, V, 1, 1, 1, 1, 0, 704, 100
41939, V, 1, 1, 1, 1, 0, 704, 100
41940, V, 1, 1, 1, 1, 0, 704, 100
41942, V, 1, 1, 1, 1, 0, 704, 100
41943, V, 1, 1, 1, 1, 0, 704, 100
41944, V, 1, 1, 1, 1, 0, 704, 100
41945, V, 1, 1, 1, 1, 0, 704, 100
41946, V, 1, 1, 1, 1, 0, 704, 100
41947, V, 1, 1, 1, 1, 0, 704, 100
41948, V, 1, 1, 1, 1, 0, 704, 100
41949, V, 1, 1, 1, 1, 0, 704, 100
41950, V, 1, 1, 1, 1, 0, 704, 100
41951, V, 1, 1, 1, 1, 0, 704, 100
41952, V, 1, 1, 1, 1, 0, 704, 100
41953, V, 1, 1, 1, 1, 0, 704, 100
41954, V, 1, 1, 1, 1, 0, 704, 100
41955, V, 1, 1, 1, 1, 0, 704, 100
41956, V, 1, 1, 1, 1, 0, 704, 100
41957, V, 1, 1, 1, 1, 0, 704, 100
41958, V, 1, 1, 1, 1, 0, 704, 100
41959, V, 1, 1, 1, 1, 0, 704, 100
41960, V, 1, 1, 1, 1, 0, 704, 100
41961, V, 1, 1, 1, 1, 0, 704, 100
41962, V, 1, 1, 1, 1, 0, 704, 100
41963, V, 1, 1, 1, 1, 0, 704, 100
41964, V, 1, 1, 1, 1, 0, 704, 100
41965, V, 1, 1, 1, 1, 0, 704, 100
41966, V, 1, 1, 1, 1, 0, 704, 100
41967, V, 1, 1, 1, 1, 0, 704, 99
41968, V, 1, 1, 1, 1, 0, 704, 100
41969, V, 1, 1, 1, 1, 0, 704, 99
41970, V, 1, 1, 1, 1, 0, 704, 100
41971, V, 1, 1, 1, 1, 0, 704, 100
41972, V, 1, 1, 1, 1, 0, 704, 100
41973, V, 1, 1, 1, 1, 0, 704, 100
41974, V, 1, 1, 1, 1, 0, 704, 99
41975, V, 1, 1, 1, 1, 0, 704, 99
41976, V, 1, 1, 1, 1, 0, 704, 100
41977, V, 1, 1, 1, 1, 0, 704, 99
41978, V, 1, 1, 1, 1, 0, 704, 99
41979, V, 1, 1, 1, 1, 0, 704, 99
41980, V, 1, 1, 1, 1, 0, 704, 99
41981, V, 1, 1, 1, 1, 0, 704, 100
41982, V, 1, 1, 1, 1, 0, 704, 99
41984, V, 1, 1, 1, 1, 0, 704, 100
41985, V, 1, 1, 1, 1, 0, 704, 99
41986, V, 1, 1, 1, 1, 0, 704, 99
41987, V, 1, 1, 1, 1, 0, 704, 99
41988, V, 1, 1, 1, 1, 0, 704, 99
41989, V, 1, 1, 1, 1, 0, 704, 100
41990, V, 1, 1, 1, 1, 0, 704, 99
41991, V, 1, 1, 1, 1, 0, 704, 100
41992, V, 1, 1, 1, 1, 0, 704, 99
41993, V, 1, 1, 1, 1, 0, 704, 100
41994, V, 1, 1, 1, 1, 0, 704, 99
41995, V, 1, 1, 1, 1, 0, 704, 100
41996, V, 1, 1, 1, 1, 0, 704, 100
41997, V, 1, 1, 1, 1, 0, 704, 100
41998, V, 1, 1, 1, 1, 0, 704, 99
41999, V, 1, 1, 1, 1, 0, 704, 100
42000, V, 1, 1, 1, 1, 0, 704, 100
42001, V, 1, 1, 1, 1, 0, 704, 100
42002, V, 1, 1, 1, 1, 0, 704, 100
42003, V, 1, 1, 1, 1, 0, 704, 100
42004, V, 1, 1, 1, 1, 0, 704, 100
42005, V, 1, 1, 1, 1, 0, 704, 100
42006, V, 1, 1, 1, 1, 0, 704, 100
42007, V, 1, 1, 1, 1, 0, 704, 100
42008, V, 1, 1, 1, 1, 0, 704, 100
42009, V, 1, 1, 1, 1, 0, 704, 100
42010, V, 1, 1, 1, 1, 0, 704, 100
42011, V, 1, 1, 1, 1, 0, 704, 100
42012, V, 1, 1, 1, 1, 0, 704, 100
42013, V, 1, 1, 1, 1, 0, 704, 100
42014, V, 1, 1, 1, 1, 0, 704, 100
42015, V, 1, 1, 1, 1, 0, 704, 100
42016, V, 1, 1, 1, 1, 0, 704, 100
42017, V, 1, 1, 1, 1, 0, 704, 100
42018, V, 1, 1, 1, 1, 0, 704, 100
42019, V, 1, 1, 1, 1, 0, 704, 100
42020, V, 1, 1, 1, 1, 0, 704, 100
42021, V, 1, 1, 1, 1, 0, 704, 100
42022, V, 1, 1, 1, 1, 0, 704, 100
42023, V, 1, 1, 1, 1, 0, 704, 100
42024, V, 1, 1, 1, 1, 0, 704, 100
42025, V, 1, 1, 1, 1, 0, 704, 100
42027, V, 1, 1, 1, 1, 0, 704, 100
42028, V, 1, 1, 1, 1, 0, 704, 100
42029, V, 1, 1, 1, 1, 0, 704, 100
42030, V, 1, 1, 1, 1, 0, 704, 100
42031, V, 1, 1, 1, 1, 0, 704, 100
42032, V, 1, 1, 1, 1, 0, 704, 100
42033, V, 1, 1, 1, 1, 0, 704, 100
42034, V, 1, 1, 1, 1, 0, 704, 100
42035, V, 1, 1, 1, 1, 0, 704, 100
42036, V, 1, 1, 1, 1, 0, 704, 100
42037, V, 1, 1, 1, 1, 0, 704, 100
42038, V, 1, 1, 1, 1, 0, 704, 100
42039, V, 1, 1, 1, 1, 0, 704, 100
42040, V, 1, 1, 1, 1, 0, 704, 100
42041, V, 1, 1, 1, 1, 0, 704, 100
42042, V, 1, 1, 1, 1, 0, 704, 100
42043, V, 1, 1, 1, 1, 0, 704, 99
42044, V, 1, 1, 1, 1, 0, 704, 100
42045, V, 1, 1, 1, 1, 0, 704, 99
42046, V, 1, 1, 1, 1, 0, 704, 100
42047, V, 1, 1, 1, 1, 0, 704, 100
42048, V, 1, 1, 1, 1, 0, 704, 99
42049, V, 1, 1, 1, 1, 0, 704, 99
42050, V, 1, 1, 1, 1, 0, 704, 99
42051, V, 1, 1, 1, 1, 0, 704, 99
42052, V, 1, 1, 1, 1, 0, 704, 100
42053, V, 1, 1, 1, 1, 0, 704, 99
42054, V, 1, 1, 1, 1, 0, 704, 99
42055, V, 1, 1, 1, 1, 0, 704, 99
42056, V, 1, 1, 1, 1, 0, 704, 100
42057, V, 1, 1, 1, 1, 0, 704, 99
42058, V, 1, 1, 1, 1, 0, 704, 99
42059, V, 1, 1, 1, 1, 0, 704, 99
42060, V, 1, 1, 1, 1, 0, 704, 99
42061, V, 1, 1, 1, 1, 0, 704, 99
42062, V, 1, 1, 1, 1, 0, 704, 99
42063, V, 1, 1, 1, 1, 0, 704, 99
42064, V, 1, 1, 1, 1, 0, 704, 100
42065, V, 1, 1, 1, 1, 0, 704, 99
42066, V, 1, 1, 1, 1, 0, 704, 99
42067, V, 1, 1, 1, 1, 0, 704, 99
42068, V, 1, 1, 1, 1, 0, 704, 99
42070, V, 1, 1, 1, 1, 0, 704, 100
42071, V, 1, 1, 1, 1, 0, 704, 99
42072, V, 1, 1, 1, 1, 0, 704, 99
42073, V, 1, 1, 1, 1, 0, 704, 99
42074, V, 1, 1, 1, 1, 0, 704, 99
42075, V, 1, 1, 1, 1, 0, 704, 100
42076, V, 1, 1, 1, 1, 0, 704, 99
42077, V, 1, 1, 1, 1, 0, 704, 100
42078, V, 1, 1, 1, 1, 0, 704, 100
42079, V, 1, 1, 1, 1, 0, 704, 99
42080, V, 1, 1, 1, 1, 0, 704, 100
42081, V, 1, 1, 1, 1, 0, 704, 100
42082, V, 1, 1, 1, 1, 0, 704, 100
42083, V, 1, 1, 1, 1, 0, 704, 100
42084, V, 1, 1, 1, 1, 0, 704, 100
42085, V, 1, 1, 1, 1, 0, 704, 100
42086, V, 1, 1, 1, 1, 0, 704, 100
42087, V, 1, 1, 1, 1, 0, 704, 100
42088, V, 1, 1, 1, 1, 0, 704, 100
42089, V, 1, 1, 1, 1, 0, 704, 100
42090, V, 1, 1, 1, 1, 0, 704, 100
42091, V, 1, 1, 1, 1, 0, 704, 100
42092, V, 1, 1, 1, 1, 0, 704, 100
42093, V, 1, 1, 1, 1, 0, 704, 100
42094, V, 1, 1, 1, 1, 0, 704, 100
42095, V, 1, 1, 1, 1, 0, 704, 100
42096, V, 1, 1, 1, 1, 0, 704, 100
42097, V, 1, 1, 1, 1, 0, 704, 100
42098, V, 1, 1, 1, 1, 0, 704, 100
42099, V, 1, 1, 1, 1, 0, 704, 100
42100, V, 1, 1, 1, 1, 0, 704, 100
42101, V, 1, 1, 1, 1, 0, 704, 100
42102, V, 1, 1, 1, 1, 0, 704, 100
42103, V, 1, 1, 1, 1, 0, 704, 100
42104, V, 1, 1, 1, 1, 0, 704, 100
42105, V, 1, 1, 1, 1, 0, 704, 100
42106, V, 1, 1, 1, 1, 0, 704, 100
42107, V, 1, 1, 1, 1, 0, 704, 100
42108, V, 1, 1, 1, 1, 0, 704, 100
42109, V, 1, 1, 1, 1, 0, 704, 100
42110, V, 1, 1, 1, 1, 0, 704, 100
42112, V, 1, 1, 1, 1, 0, 704, 99
42113, V, 1, 1, 1, 1, 0, 704, 100
42114, V, 1, 1, 1, 1, 0, 704, 100
42115, V, 1, 1, 1, 1, 0, 704, 100
42116, V, 1, 1, 1, 1, 0, 704, 99
42117, V, 1, 1, 1, 1, 0, 704, 99
42118, V, 1, 1, 1, 1, 0, 704, 100
42119, V, 1, 1, 1, 1, 0, 704, 99
42120, V, 1, 1, 1, 1, 0, 704, 100
42121, V, 1, 1, 1, 1, 0, 704, 99
42122, V, 1, 1, 1, 1, 0, 704, 100
42123, V, 1, 1, 1, 1, 0, 704, 100
42124, V, 1, 1, 1, 1, 0, 704, 99
42125, V, 1, 1, 1, 1, 0, 704, 100
42126, V, 1, 1, 1, 1, 0, 704, 100
42127, V, 1, 1, 1, 1, 0, 704, 100
42128, V, 1, 1, 1, 1, 0, 704, 100
42129, V, 1, 1, 1, 1, 0, 704, 99
42130, V, 1, 1, 1, 1, 0, 704, 100
42131, V, 1, 1, 1, 1, 0, 704, 99
42132, V, 1, 1, 1, 1, 0, 704, 100
42133, V, 1, 1, 1, 1, 0, 704, 100
42134, V, 1, 1, 1, 1, 0, 704, 100
42135, V, 1, 1, 1, 1, 0, 704, 99
42136, V, 1, 1, 1, 1, 0, 704, 99
42137, V, 1, 1, 1, 1, 0, 704, 100
42138, V, 1, 1, 1, 1, 0, 704, 100
42139, V, 1, 1, 1, 1, 0, 704, 100
42140, V, 1, 1, 1, 1, 0, 704, 100
42141, V, 1, 1, 1, 1, 0, 704, 100
42142, V, 1, 1, 1, 1, 0, 704, 100
42143, V, 1, 1, 1, 1, 0, 704, 100
42144, V, 1, 1, 1, 1, 0, 704, 100
42145, V, 1, 1, 1, 1, 0, 704, 100
42146, V, 1, 1, 1, 1, 0, 704, 100
42147, V, 1, 1, 1, 1, 0, 704, 100
42148, V, 1, 1, 1, 1, 0, 704, 100
42149, V, 1, 1, 1, 1, 0, 704, 100
42150, V, 1, 1, 1, 1, 0, 704, 100
42151, V, 1, 1, 1, 1, 0, 704, 100
42152, V, 1, 1, 1, 1, 0, 704, 100
42153, V, 1, 1, 1, 1, 0, 704, 100
42155, V, 1, 1, 1, 1, 0, 704, 100
42156, V, 1, 1, 1, 1, 0, 704, 100
42157, V, 1, 1, 1, 1, 0, 704, 100
42158, V, 1, 1, 1, 1, 0, 704, 100
42159, V, 1, 1, 1, 1, 0, 704, 100
42160, V, 1, 1, 1, 1, 0, 704, 100
42161, V, 1, 1, 1, 1, 0, 704, 100
42162, V, 1, 1, 1, 1, 0, 704, 100
42163, V, 1, 1, 1, 1, 0, 704, 100
42164, V, 1, 1, 1, 1, 0, 704, 100
42165, V, 1, 1, 1, 1, 0, 704, 100
42166, V, 1, 1, 1, 1, 0, 704, 100
42167, V, 1, 1, 1, 1, 0, 704, 100
42168, V, 1, 1, 1, 1, 0, 704, 100
42169, V, 1, 1, 1, 1, 0, 704, 100
42170, V, 1, 1, 1, 1, 0, 704, 100
42171, V, 1, 1, 1, 1, 0, 704, 100
42172, V, 1, 1, 1, 1, 0, 704, 100
42173, V, 1, 1, 1, 1, 0, 704, 100
42174, V, 1, 1, 1, 1, 0, 704, 100
42175, V, 1, 1, 1, 1, 0, 704, 100
42176, V, 1, 1, 1, 1, 0, 704, 100
42177, V, 1, 1, 1, 1, 0, 704, 100
42178, V, 1, 1, 1, 1, 0, 704, 100
42179, V, 1, 1, 1, 1, 0, 704, 100
42180, V, 1, 1, 1, 1, 0, 704, 100
42181, V, 1, 1, 1, 1, 0, 704, 100
42182, V, 1, 1, 1, 1, 0, 704, 100
42183, V, 1, 1, 1, 1, 0, 704, 100
42184, V, 1, 1, 1, 1, 0, 704, 100
42185, V, 1, 1, 1, 1, 0, 704, 100
42186, V, 1, 1, 1, 1, 0, 704, 100
42187, V, 1, 1, 1, 1, 0, 704, 100
42188, V, 1, 1, 1, 1, 0, 704, 100
42189, V, 1, 1, 1, 1, 0, 704, 99
42190, V, 1, 1, 1, 1, 0, 704, 100
42191, V, 1, 1, 1, 1, 0, 704, 100
42192, V, 1, 1, 1, 1, 0, 704, 99
42193, V, 1, 1, 1, 1, 0, 704, 99
42194, V, 1, 1, 1, 1, 0, 704, 99
42195, V, 1, 1, 1, 1, 0, 704, 99
42196, V, 1, 1, 1, 1, 0, 704, 99
42198, V, 1, 1, 1, 1, 0, 704, 99
42199, V, 1, 1, 1, 1, 0, 704, 99
42200, V, 1, 1, 1, 1, 0, 704, 99
42201, V, 1, 1, 1, 1, 0, 704, 99
42202, V, 1, 1, 1, 1, 0, 704, 99
42203, V, 1, 1, 1, 1, 0, 704, 99
42204, V, 1, 1, 1, 1, 0, 704, 99
42205, V, 1, 1, 1, 1, 0, 704, 99
42206, V, 1, 1, 1, 1, 0, 704, 99
42207, V, 1, 1, 1, 1, 0, 704, 99
42208, V, 1, 1, 1, 1, 0, 704, 99
42209, V, 1, 1, 1, 1, 0, 704, 99
42210, V, 1, 1, 1, 1, 0, 704, 99
42211, V, 1, 1, 1, 1, 0, 704, 99
42212, V, 1, 1, 1, 1, 0, 704, 99
42213, V, 1, 1, 1, 1, 0, 704, 99
42214, V, 1, 1, 1, 1, 0, 704, 99
42215, V, 1, 1, 1, 1, 0, 704, 99
42216, V, 1, 1, 1, 1, 0, 704, 99
42217, V, 1, 1, 1, 1, 0, 704, 99
42218, V, 1, 1, 1, 1, 0, 704, 99
42219, V, 1, 1, 1, 1, 0, 704, 99
42220, V, 1, 1, 1, 1, 0, 704, 99
42221, V, 1, 1, 1, 1, 0, 704, 99
42222, V, 1, 1, 1, 1, 0, 704, 99
42223, V, 1, 1, 1, 1, 0, 704, 99
42224, V, 1, 1, 1, 1, 0, 704, 99
42225, V, 1, 1, 1, 1, 0, 704, 99
42226, V, 1, 1, 1, 1, 0, 704, 99
42227, V, 1, 1, 1, 1, 0, 704, 99
42228, V, 1, 1, 1, 1, 0, 704, 99
42229, V, 1, 1, 1, 1, 0, 704, 99
42230, V, 1, 1, 1, 1, 0, 704, 99
42231, V, 1, 1, 1, 1, 0, 704, 99
42232, V, 1, 1, 1, 1, 0, 704, 99
42233, V, 1, 1, 1, 1, 0, 704, 99
42234, V, 1, 1, 1, 1, 0, 704, 99
42235, V, 1, 1, 1, 1, 0, 704, 99
42236, V, 1, 1, 1, 1, 0, 704, 99
42237, V, 1, 1, 1, 1, 0, 704, 99
42238, V, 1, 1, 1, 1, 0, 704, 99
42240, V, 1, 1, 1, 1, 0, 704, 99
42241, V, 1, 1, 1, 1, 0, 704, 99
42242, V, 1, 1, 1, 1, 0, 704, 99
42243, V, 1, 1, 1, 1, 0, 704, 100
42244, V, 1, 1, 1, 1, 0, 704, 99
42245, V, 1, 1, 1, 1, 0, 704, 99
42246, V, 1, 1, 1, 1, 0, 704, 100
42247, V, 1, 1, 1, 1, 0, 704, 100
42248, V, 1, 1, 1, 1, 0, 704, 99
42249, V, 1, 1, 1, 1, 0, 704, 99
42250, V, 1, 1, 1, 1, 0, 704, 99
42251, V, 1, 1, 1, 1, 0, 704, 100
42252, V, 1, 1, 1, 1, 0, 704, 100
42253, V, 1, 1, 1, 1, 0, 704, 99
42254, V, 1, 1, 1, 1, 0, 704, 100
42255, V, 1, 1, 1, 1, 0, 704, 100
42256, V, 1, 1, 1, 1, 0, 704, 99
42257, V, 1, 1, 1, 1, 0, 704, 99
42258, V, 1, 1, 1, 1, 0, 704, 99
42259, V, 1, 1, 1, 1, 0, 704, 100
42260, V, 1, 1, 1, 1, 0, 704, 99
42261, V, 1, 1, 1, 1, 0, 704, 99
42262, V, 1, 1, 1, 1, 0, 704, 99
42263, V, 1, 1, 1, 1, 0, 704, 99
42264, V, 1, 1, 1, 1, 0, 704, 99
42265, V, 1, 1, 1, 1, 0, 704, 99
42266, V, 1, 1, 1, 1, 0, 704, 99
42267, V, 1, 1, 1, 1, 0, 704, 99
42268, V, 1, 1, 1, 1, 0, 704, 99
42269, V, 1, 1, 1, 1, 0, 704, 99
42270, V, 1, 1, 1, 1, 0, 704, 99
42271, V, 1, 1, 1, 1, 0, 704, 99
42272, V, 1, 1, 1, 1, 0, 704, 99
42273, V, 1, 1, 1, 1, 0, 704, 99
42274, V, 1, 1, 1, 1, 0, 704, 99
42275, V, 1, 1, 1, 1, 0, 704, 99
42276, V, 1, 1, 1, 1, 0, 704, 99
42277, V, 1, 1, 1, 1, 0, 704, 99
42278, V, 1, 1, 1, 1, 0, 704, 99
42279, V, 1, 1, 1, 1, 0, 704, 99
42280, V, 1, 1, 1, 1, 0, 704, 99
42281, V, 1, 1, 1, 1, 0, 704, 99
42283, V, 1, 1, 1, 1, 0, 704, 99
42284, V, 1, 1, 1, 1, 0, 704, 99
42285, V, 1, 1, 1, 1, 0, 704, 99
42286, V, 1, 1, 1, 1, 0, 704, 99
42287, V, 1, 1, 1, 1, 0, 704, 99
42288, V, 1, 1, 1, 1, 0, 704, 99
42289, V, 1, 1, 1, 1, 0, 704, 99
42290, V, 1, 1, 1, 1, 0, 704, 99
42291, V, 1, 1, 1, 1, 0, 704, 99
42292, V, 1, 1, 1, 1, 0, 704, 99
42293, V, 1, 1, 1, 1, 0, 704, 99
42294, V, 1, 1, 1, 1, 0, 704, 99
42295, V, 1, 1, 1, 1, 0, 704, 99
42296, V, 1, 1, 1, 1, 0, 704, 99
42297, V, 1, 1, 1, 1, 0, 704, 99
42298, V, 1, 1, 1, 1, 0, 704, 99
42299, V, 1, 1, 1, 1, 0, 704, 99
42300, V, 1, 1, 1, 1, 0, 704, 99
42301, V, 1, 1, 1, 1, 0, 704, 99
42302, V, 1, 1, 1, 1, 0, 704, 99
42303, V, 1, 1, 1, 1, 0, 704, 99
42304, V, 1, 1, 1, 1, 0, 704, 99
42305, V, 1, 1, 1, 1, 0, 704, 99
42306, V, 1, 1, 1, 1, 0, 704, 99
42307, V, 1, 1, 1, 1, 0, 704, 99
42308, V, 1, 1, 1, 1, 0, 704, 99
42309, V, 1, 1, 1, 1, 0, 704, 99
42310, V, 1, 1, 1, 1, 0, 704, 99
42311, V, 1, 1, 1, 1, 0, 704, 99
42312, V, 1, 1, 1, 1, 0, 704, 99
42313, V, 1, 1, 1, 1, 0, 704, 99
42314, V, 1, 1, 1, 1, 0, 704, 100
42315, V, 1, 1, 1, 1, 0, 704, 100
42316, V, 1, 1, 1, 1, 0, 704, 99
42317, V, 1, 1, 1, 1, 0, 704, 100
42318, V, 1, 1, 1, 1, 0, 704, 99
42319, V, 1, 1, 1, 1, 0, 704, 99
42320, V, 1, 1, 1, 1, 0, 704, 99
42321, V, 1, 1, 1, 1, 0, 704, 99
42322, V, 1, 1, 1, 1, 0, 704, 99
42323, V, 1, 1, 1, 1, 0, 704, 99
42324, V, 1, 1, 1, 1, 0, 704, 100
42326, V, 1, 1, 1, 1, 0, 704, 99
42327, V, 1, 1, 1, 1, 0, 704, 99
42328, V, 1, 1, 1, 1, 0, 704, 99
42329, V, 1, 1, 1, 1, 0, 704, 99
42330, V, 1, 1, 1, 1, 0, 704, 100
42331, V, 1, 1, 1, 1, 0, 704, 99
42332, V, 1, 1, 1, 1, 0, 704, 99
42333, V, 1, 1, 1, 1, 0, 704, 100
42334, V, 1, 1, 1, 1, 0, 704, 99
42335, V, 1, 1, 1, 1, 0, 704, 100
42336, V, 1, 1, 1, 1, 0, 704, 99
42337, V, 1, 1, 1, 1, 0, 704, 99
42338, V, 1, 1, 1, 1, 0, 704, 99
42339, V, 1, 1, 1, 1, 0, 704, 99
42340, V, 1, 1, 1, 1, 0, 704, 100
42341, V, 1, 1, 1, 1, 0, 704, 99
42342, V, 1, 1, 1, 1, 0, 704, 99
42343, V, 1, 1, 1, 1, 0, 704, 99
42344, V, 1, 1, 1, 1, 0, 704, 99
42345, V, 1, 1, 1, 1, 0, 704, 99
42346, V, 1, 1, 1, 1, 0, 704, 99
42347, V, 1, 1, 1, 1, 0, 704, 99
42348, V, 1, 1, 1, 1, 0, 704, 100
42349, V, 1, 1, 1, 1, 0, 704, 99
42350, V, 1, 1, 1, 1, 0, 704, 99
42351, V, 1, 1, 1, 1, 0, 704, 99
42352, V, 1, 1, 1, 1, 0, 704, 99
42353, V, 1, 1, 1, 1, 0, 704, 99
42354, V, 1, 1, 1, 1, 0, 704, 99
42355, V, 1, 1, 1, 1, 0, 704, 99
42356, V, 1, 1, 1, 1, 0, 704, 99
42357, V, 1, 1, 1, 1, 0, 704, 99
42358, V, 1, 1, 1, 1, 0, 704, 99
42359, V, 1, 1, 1, 1, 0, 704, 99
42360, V, 1, 1, 1, 1, 0, 704, 99
42361, V, 1, 1, 1, 1, 0, 704, 99
42362, V, 1, 1, 1, 1, 0, 704, 99
42363, V, 1, 1, 1, 1, 0, 704, 99
42364, V, 1, 1, 1, 1, 0, 704, 99
42365, V, 1, 1, 1, 1, 0, 704, 99
42366, V, 1, 1, 1, 1, 0, 704, 99
42368, V, 1, 1, 1, 1, 0, 704, 99
42369, V, 1, 1, 1, 1, 0, 704, 99
42370, V, 1, 1, 1, 1, 0, 704, 99
42371, V, 1, 1, 1, 1, 0, 704, 99
42372, V, 1, 1, 1, 1, 0, 704, 99
42373, V, 1, 1, 1, 1, 0, 704, 99
42374, V, 1, 1, 1, 1, 0, 704, 99
42375, V, 1, 1, 1, 1, 0, 704, 99
42376, V, 1, 1, 1, 1, 0, 704, 99
42377, V, 1, 1, 1, 1, 0, 704, 99
42378, V, 1, 1, 1, 1, 0, 704, 99
42379, V, 1, 1, 1, 1, 0, 704, 99
42380, V, 1, 1, 1, 1, 0, 704, 99
42381, V, 1, 1, 1, 1, 0, 704, 99
42382, V, 1, 1, 1, 1, 0, 704, 99
42383, V, 1, 1, 1, 1, 0, 704, 99
42384, V, 1, 1, 1, 1, 0, 704, 99
42385, V, 1, 1, 1, 1, 0, 704, 99
42386, V, 1, 1, 1, 1, 0, 704, 99
42387, V, 1, 1, 1, 1, 0, 704, 99
42388, V, 1, 1, 1, 1, 0, 704, 100
42389, V, 1, 1, 1, 1, 0, 704, 99
42390, V, 1, 1, 1, 1, 0, 704, 99
42391, V, 1, 1, 1, 1, 0, 704, 99
42392, V, 1, 1, 1, 1, 0, 704, 100
42393, V, 1, 1, 1, 1, 0, 704, 99
42394, V, 1, 1, 1, 1, 0, 704, 99
42395, V, 1, 1, 1, 1, 0, 704, 99
42396, V, 1, 1, 1, 1, 0, 704, 99
42397, V, 1, 1, 1, 1, 0, 704, 99
42398, V, 1, 1, 1, 1, 0, 704, 100
42399, V, 1, 1, 1, 1, 0, 704, 99
42400, V, 1, 1, 1, 1, 0, 704, 99
42401, V, 1, 1, 1, 1, 0, 704, 99
42402, V, 1, 1, 1, 1, 0, 704, 99
42403, V, 1, 1, 1, 1, 0, 704, 99
42404, V, 1, 1, 1, 1, 0, 704, 100
42405, V, 1, 1, 1, 1, 0, 704, 99
42406, V, 1, 1, 1, 1, 0, 704, 99
42407, V, 1, 1, 1, 1, 0, 704, 99
42408, V, 1, 1, 1, 1, 0, 704, 99
42409, V, 1, 1, 1, 1, 0, 704, 99
42411, V, 1, 1, 1, 1, 0, 704, 100
42412, V, 1, 1, 1, 1, 0, 704, 99
42413, V, 1, 1, 1, 1, 0, 704, 99
42414, V, 1, 1, 1, 1, 0, 704, 99
42415, V, 1, 1, 1, 1, 0, 704, 99
42416, V, 1, 1, 1, 1, 0, 704, 99
42417, V, 1, 1, 1, 1, 0, 704, 100
42418, V, 1, 1, 1, 1, 0, 704, 99
42419, V, 1, 1, 1, 1, 0, 704, 99
42420, V, 1, 1, 1, 1, 0, 704, 99
42421, V, 1, 1, 1, 1, 0, 704, 99
42422, V, 1, 1, 1, 1, 0, 704, 99
42423, V, 1, 1, 1, 1, 0, 704, 99
42424, V, 1, 1, 1, 1, 0, 704, 100
42425, V, 1, 1, 1, 1, 0, 704, 99
42426, V, 1, 1, 1, 1, 0, 704, 99
42427, V, 1, 1, 1, 1, 0, 704, 99
42428, V, 1, 1, 1, 1, 0, 704, 99
42429, V, 1, 1, 1, 1, 0, 704, 99
42430, V, 1, 1, 1, 1, 0, 704, 99
42431, V, 1, 1, 1, 1, 0, 704, 99
42432, V, 1, 1, 1, 1, 0, 704, 99
42433, V, 1, 1, 1, 1, 0, 704, 99
42434, V, 1, 1, 1, 1, 0, 704, 99
42435, V, 1, 1, 1, 1, 0, 704, 99
42436, V, 1, 1, 1, 1, 0, 704, 99
42437, V, 1, 1, 1, 1, 0, 704, 99
42438, V, 1, 1, 1, 1, 0, 704, 99
42439, V, 1, 1, 1, 1, 0, 704, 99
42440, V, 1, 1, 1, 1, 0, 704, 99
42441, V, 1, 1, 1, 1, 0, 704, 99
42442, V, 1, 1, 1, 1, 0, 704, 99
42443, V, 1, 1, 1, 1, 0, 704, 99
42444, V, 1, 1, 1, 1, 0, 704, 99
42445, V, 1, 1, 1, 1, 0, 704, 99
42446, V, 1, 1, 1, 1, 0, 704, 99
42447, V, 1, 1, 1, 1, 0, 704, 99
42448, V, 1, 1, 1, 1, 0, 704, 99
42449, V, 1, 1, 1, 1, 0, 704, 99
42450, V, 1, 1, 1, 1, 0, 704, 99
42451, V, 1, 1, 1, 1, 0, 704, 100
42452, V, 1, 1, 1, 1, 0, 704, 99
42454, V, 1, 1, 1, 1, 0, 704, 99
42455, V, 1, 1, 1, 1, 0, 704, 99
42456, V, 1, 1, 1, 1, 0, 704, 99
42457, V, 1, 1, 1, 1, 0, 704, 99
42458, V, 1, 1, 1, 1, 0, 704, 99
42459, V, 1, 1, 1, 1, 0, 704, 99
42460, V, 1, 1, 1, 1, 0, 704, 99
42461, V, 1, 1, 1, 1, 0, 704, 99
42462, V, 1, 1, 1, 1, 0, 704, 99
42463, V, 1, 1, 1, 1, 0, 704, 99
42464, V, 1, 1, 1, 1, 0, 704, 99
42465, V, 1, 1, 1, 1, 0, 704, 99
42466, V, 1, 1, 1, 1, 0, 704, 99
42467, V, 1, 1, 1, 1, 0, 704, 99
42468, V, 1, 1, 1, 1, 0, 704, 99
42469, V, 1, 1, 1, 1, 0, 704, 99
42470, V, 1, 1, 1, 1, 0, 704, 99
42471, V, 1, 1, 1, 1, 0, 704, 99
42472, V, 1, 1, 1, 1, 0, 704, 99
42473, V, 1, 1, 1, 1, 0, 704, 100
42474, V, 1, 1, 1, 1, 0, 704, 100
42475, V, 1, 1, 1, 1, 0, 704, 100
42476, V, 1, 1, 1, 1, 0, 704, 99
42477, V, 1, 1, 1, 1, 0, 704, 99
42478, V, 1, 1, 1, 1, 0, 704, 99
42479, V, 1, 1, 1, 1, 0, 704, 99
42480, V, 1, 1, 1, 1, 0, 704, 99
42481, V, 1, 1, 1, 1, 0, 704, 99
42482, V, 1, 1, 1, 1, 0, 704, 99
42483, V, 1, 1, 1, 1, 0, 704, 99
42484, V, 1, 1, 1, 1, 0, 704, 99
42485, V, 1, 1, 1, 1, 0, 704, 99
42486, V, 1, 1, 1, 1, 0, 704, 99
42487, V, 1, 1, 1, 1, 0, 704, 100
42488, V, 1, 1, 1, 1, 0, 704, 99
42489, V, 1, 1, 1, 1, 0, 704, 99
42490, V, 1, 1, 1, 1, 0, 704, 99
42491, V, 1, 1, 1, 1, 0, 704, 99
42492, V, 1, 1, 1, 1, 0, 704, 99
42493, V, 1, 1, 1, 1, 0, 704, 99
42494, V, 1, 1, 1, 1, 0, 704, 99
42496, V, 1, 1, 1, 1, 0, 704, 99
42497, V, 1, 1, 1, 1, 0, 704, 99
42498, V, 1, 1, 1, 1, 0, 704, 99
42499, V, 1, 1, 1, 1, 0, 704, 99
42500, V, 1, 1, 1, 1, 0, 704, 99
42501, V, 1, 1, 1, 1, 0, 704, 99
42502, V, 1, 1, 1, 1, 0, 704, 99
42503, V, 1, 1, 1, 1, 0, 704, 99
42504, V, 1, 1, 1, 1, 0, 704, 99
42505, V, 1, 1, 1, 1, 0, 704, 99
42506, V, 1, 1, 1, 1, 0, 704, 99
42507, V, 1, 1, 1, 1, 0, 704, 99
42508, V, 1, 1, 1, 1, 0, 704, 99
42509, V, 1, 1, 1, 1, 0, 704, 99
42510, V, 1, 1, 1, 1, 0, 704, 99
42511, V, 1, 1, 1, 1, 0, 704, 99
42512, V, 1, 1, 1, 1, 0, 704, 99
42513, V, 1, 1, 1, 1, 0, 704, 99
42514, V, 1, 1, 1, 1, 0, 704, 99
42515, V, 1, 1, 1, 1, 0, 704, 99
42516, V, 1, 1, 1, 1, 0, 704, 99
42517, V, 1, 1, 1, 1, 0, 704, 99
42518, V, 1, 1, 1, 1, 0, 704, 99
42519, V, 1, 1, 1, 1, 0, 704, 99
42520, V, 1, 1, 1, 1, 0, 704, 99
42521, V, 1, 1, 1, 1, 0, 704, 99
42522, V, 1, 1, 1, 1, 0, 704, 99
42523, V, 1, 1, 1, 1, 0, 704, 99
42524, V, 1, 1, 1, 1, 0, 704, 99
42525, V, 1, 1, 1, 1, 0, 704, 99
42526, V, 1, 1, 1, 1, 0, 704, 99
42527, V, 1, 1, 1, 1, 0, 704, 99
42528, V, 1, 1, 1, 1, 0, 704, 99
42529, V, 1, 1, 1, 1, 0, 704, 99
42530, V, 1, 1, 1, 1, 0, 704, 99
42531, V, 1, 1, 1, 1, 0, 704, 99
42532, V, 1, 1, 1, 1, 0, 704, 99
42533, V, 1, 1, 1, 1, 0, 704, 99
42534, V, 1, 1, 1, 1, 0, 704, 99
42535, V, 1, 1, 1, 1, 0, 704, 99
42536, V, 1, 1, 1, 1, 0, 704, 99
42537, V, 1, 1, 1, 1, 0, 704, 99
42539, V, 1, 1, 1, 1, 0, 704, 99
42540, V, 1, 1, 1, 1, 0, 704, 99
42541, V, 1, 1, 1, 1, 0, 704, 99
42542, V, 1, 1, 1, 1, 0, 704, 99
42543, V, 1, 1, 1, 1, 0, 704, 99
42544, V, 1, 1, 1, 1, 0, 704, 99
42545, V, 1, 1, 1, 1, 0, 704, 99
42546, V, 1, 1, 1, 1, 0, 704, 99
42547, V, 1, 1, 1, 1, 0, 704, 99
42548, V, 1, 1, 1, 1, 0, 704, 99
42549, V, 1, 1, 1, 1, 0, 704, 99
42550, V, 1, 1, 1, 1, 0, 704, 99
42551, V, 1, 1, 1, 1, 0, 704, 99
42552, V, 1, 1, 1, 1, 0, 704, 99
42553, V, 1, 1, 1, 1, 0, 704, 100
42554, V, 1, 1, 1, 1, 0, 704, 99
42555, V, 1, 1, 1, 1, 0, 704, 99
42556, V, 1, 1, 1, 1, 0, 704, 100
42557, V, 1, 1, 1, 1, 0, 704, 99
42558, V, 1, 1, 1, 1, 0, 704, 99
42559, V, 1, 1, 1, 1, 0, 704, 99
42560, V, 1, 1, 1, 1, 0, 704, 99
42561, V, 1, 1, 1, 1, 0, 704, 99
42562, V, 1, 1, 1, 1, 0, 704, 99
42563, V, 1, 1, 1, 1, 0, 704, 99
42564, V, 1, 1, 1, 1, 0, 704, 99
42565, V, 1, 1, 1, 1, 0, 704, 99
42566, V, 1, 1, 1, 1, 0, 704, 99
42567, V, 1, 1, 1, 1, 0, 704, 99
42568, V, 1, 1, 1, 1, 0, 704, 99
42569, V, 1, 1, 1, 1, 0, 704, 99
42570, V, 1, 1, 1, 1, 0, 704, 99
42571, V, 1, 1, 1, 1, 0, 704, 99
42572, V, 1, 1, 1, 1, 0, 704, 99
42573, V, 1, 1, 1, 1, 0, 704, 99
42574, V, 1, 1, 1, 1, 0, 704, 99
42575, V, 1, 1, 1, 1, 0, 704, 99
42576, V, 1, 1, 1, 1, 0, 704, 99
42577, V, 1, 1, 1, 1, 0, 704, 99
42578, V, 1, 1, 1, 1, 0, 704, 99
42579, V, 1, 1, 1, 1, 0, 704, 99
42580, V, 1, 1, 1, 1, 0, 704, 99
42582, V, 1, 1, 1, 1, 0, 704, 99
42583, V, 1, 1, 1, 1, 0, 704, 99
42584, V, 1, 1, 1, 1, 0, 704, 99
42585, V, 1, 1, 1, 1, 0, 704, 99
42586, V, 1, 1, 1, 1, 0, 704, 99
42587, V, 1, 1, 1, 1, 0, 704, 99
42588, V, 1, 1, 1, 1, 0, 704, 99
42589, V, 1, 1, 1, 1, 0, 704, 99
42590, V, 1, 1, 1, 1, 0, 704, 99
42591, V, 1, 1, 1, 1, 0, 704, 99
42592, V, 1, 1, 1, 1, 0, 704, 99
42593, V, 1, 1, 1, 1, 0, 704, 99
42594, V, 1, 1, 1, 1, 0, 704, 99
42595, V, 1, 1, 1, 1, 0, 704, 99
42596, V, 1, 1, 1, 1, 0, 704, 99
42597, V, 1, 1, 1, 1, 0, 704, 99
42598, V, 1, 1, 1, 1, 0, 704, 99
42599, V, 1, 1, 1, 1, 0, 704, 99
42600, V, 1, 1, 1, 1, 0, 704, 99
42601, V, 1, 1, 1, 1, 0, 704, 99
42602, V, 1, 1, 1, 1, 0, 704, 99
42603, V, 1, 1, 1, 1, 0, 704, 99
42604, V, 1, 1, 1, 1, 0, 704, 99
42605, V, 1, 1, 1, 1, 0, 704, 99
42606, V, 1, 1, 1, 1, 0, 704, 99
42607, V, 1, 1, 1, 1, 0, 704, 99
42608, V, 1, 1, 1, 1, 0, 704, 99
42609, V, 1, 1, 1, 1, 0, 704, 99
42610, V, 1, 1, 1, 1, 0, 704, 99
42611, V, 1, 1, 1, 1, 0, 704, 99
42612, V, 1, 1, 1, 1, 0, 704, 99
42613, V, 1, 1, 1, 1, 0, 704, 99
42614, V, 1, 1, 1, 1, 0, 704, 99
42615, V, 1, 1, 1, 1, 0, 704, 99
42616, V, 1, 1, 1, 1, 0, 704, 99
42617, V, 1, 1, 1, 1, 0, 704, 99
42618, V, 1, 1, 1, 1, 0, 704, 99
42619, V, 1, 1, 1, 1, 0, 704, 99
42620, V, 1, 1, 1, 1, 0, 704, 99
42621, V, 1, 1, 1, 1, 0, 704, 99
42622, V, 1, 1, 1, 1, 0, 704, 99
42624, V, 1, 1, 1, 1, 0, 704, 99
42625, V, 1, 1, 1, 1, 0, 704, 99
42626, V, 1, 1, 1, 1, 0, 704, 99
42627, V, 1, 1, 1, 1, 0, 704, 99
42628, V, 1, 1, 1, 1, 0, 704, 99
42629, V, 1, 1, 1, 1, 0, 704, 99
42630, V, 1, 1, 1, 1, 0, 704, 99
42631, V, 1, 1, 1, 1, 0, 704, 99
42632, V, 1, 1, 1, 1, 0, 704, 99
42633, V, 1, 1, 1, 1, 0, 704, 99
42634, V, 1, 1, 1, 1, 0, 704, 99
42635, V, 1, 1, 1, 1, 0, 704, 99
42636, V, 1, 1, 1, 1, 0, 704, 99
42637, V, 1, 1, 1, 1, 0, 704, 99
42638, V, 1, 1, 1, 1, 0, 704, 99
42639, V, 1, 1, 1, 1, 0, 704, 99
42640, V, 1, 1, 1, 1, 0, 704, 99
42641, V, 1, 1, 1, 1, 0, 704, 99
42642, V, 1, 1, 1, 1, 0, 704, 99
42643, V, 1, 1, 1, 1, 0, 704, 99
42644, V, 1, 1, 1, 1, 0, 704, 99
42645, V, 1, 1, 1, 1, 0, 704, 99
42646, V, 1, 1, 1, 1, 0, 704, 99
42647, V, 1, 1, 1, 1, 0, 704, 99
42648, V, 1, 1, 1, 1, 0, 704, 99
42649, V, 1, 1, 1, 1, 0, 704, 99
42650, V, 1, 1, 1, 1, 0, 704, 99
42651, V, 1, 1, 1, 1, 0, 704, 99
42652, V, 1, 1, 1, 1, 0, 704, 99
42653, V, 1, 1, 1, 1, 0, 704, 99
42654, V, 1, 1, 1, 1, 0, 704, 99
42655, V, 1, 1, 1, 1, 0, 704, 99
42656, V, 1, 1, 1, 1, 0, 704, 99
42657, V, 1, 1, 1, 1, 0, 704, 99
42658, V, 1, 1, 1, 1, 0, 704, 99
42659, V, 1, 1, 1, 1, 0, 704, 99
42660, V, 1, 1, 1, 1, 0, 704, 99
42661, V, 1, 1, 1, 1, 0, 704, 99
42662, V, 1, 1, 1, 1, 0, 704, 99
42663, V, 1, 1, 1, 1, 0, 704, 99
42664, V, 1, 1, 1, 1, 0, 704, 99
42665, V, 1, 1, 1, 1, 0, 704, 99
42667, V, 1, 1, 1, 1, 0, 704, 99
42668, V, 1, 1, 1, 1, 0, 704, 99
42669, V, 1, 1, 1, 1, 0, 704, 99
42670, V, 1, 1, 1, 1, 0, 704, 99
42671, V, 1, 1, 1, 1, 0, 704, 99
42672, V, 1, 1, 1, 1, 0, 704, 99
42673, V, 1, 1, 1, 1, 0, 704, 99
42674, V, 1, 1, 1, 1, 0, 704, 99
42675, V, 1, 1, 1, 1, 0, 704, 99
42676, V, 1, 1, 1, 1, 0, 704, 99
42677, V, 1, 1, 1, 1, 0, 704, 99
42678, V, 1, 1, 1, 1, 0, 704, 99
42679, V, 1, 1, 1, 1, 0, 704, 99
42680, V, 1, 1, 1, 1, 0, 704, 99
42681, V, 1, 1, 1, 1, 0, 704, 99
42682, V, 1, 1, 1, 1, 0, 704, 99
42683, V, 1, 1, 1, 1, 0, 704, 99
42684, V, 1, 1, 1, 1, 0, 704, 99
42685, V, 1, 1, 1, 1, 0, 704, 99
42686, V, 1, 1, 1, 1, 0, 704, 99
42687, V, 1, 1, 1, 1, 0, 704, 99
42688, V, 1, 1, 1, 1, 0, 704, 99
42689, V, 1, 1, 1, 1, 0, 704, 99
42690, V, 1, 1, 1, 1, 0, 704, 99
42691, V, 1, 1, 1, 1, 0, 704, 99
42692, V, 1, 1, 1, 1, 0, 704, 99
42693, V, 1, 1, 1, 1, 0, 704, 100
42694, V, 1, 1, 1, 1, 0, 704, 100
42695, V, 1, 1, 1, 1, 0, 704, 99
42696, V, 1, 1, 1, 1, 0, 704, 100
42697, V, 1, 1, 1, 1, 0, 704, 100
42698, V, 1, 1, 1, 1, 0, 704, 99
42699, V, 1, 1, 1, 1, 0, 704, 100
42700, V, 1, 1, 1, 1, 0, 704, 99
42701, V, 1, 1, 1, 1, 0, 704, 100
42702, V, 1, 1, 1, 1, 0, 704, 100
42703, V, 1, 1, 1, 1, 0, 704, 100
42704, V, 1, 1, 1, 1, 0, 704, 100
42705, V, 1, 1, 1, 1, 0, 704, 100
42706, V, 1, 1, 1, 1, 0, 704, 100
42707, V, 1, 1, 1, 1, 0, 704, 100
42708, V, 1, 1, 1, 1, 0, 704, 99
42710, V, 1, 1, 1, 1, 0, 704, 100
42711, V, 1, 1, 1, 1, 0, 704, 99
42712, V, 1, 1, 1, 1, 0, 704, 100
42713, V, 1, 1, 1, 1, 0, 704, 100
42714, V, 1, 1, 1, 1, 0, 704, 99
42715, V, 1, 1, 1, 1, 0, 704, 100
42716, V, 1, 1, 1, 1, 0, 704, 99
42717, V, 1, 1, 1, 1, 0, 704, 100
42718, V, 1, 1, 1, 1, 0, 704, 100
42719, V, 1, 1, 1, 1, 0, 704, 100
42720, V, 1, 1, 1, 1, 0, 704, 100
42721, V, 1, 1, 1, 1, 0, 704, 99
42722, V, 1, 1, 1, 1, 0, 704, 100
42723, V, 1, 1, 1, 1, 0, 704, 99
42724, V, 1, 1, 1, 1, 0, 704, 99
42725, V, 1, 1, 1, 1, 0, 704, 100
42726, V, 1, 1, 1, 1, 0, 704, 99
42727, V, 1, 1, 1, 1, 0, 704, 100
42728, V, 1, 1, 1, 1, 0, 704, 99
42729, V, 1, 1, 1, 1, 0, 704, 99
42730, V, 1, 1, 1, 1, 0, 704, 100
42731, V, 1, 1, 1, 1, 0, 704, 99
42732, V, 1, 1, 1, 1, 0, 704, 99
42733, V, 1, 1, 1, 1, 0, 704, 99
42734, V, 1, 1, 1, 1, 0, 704, 99
42735, V, 1, 1, 1, 1, 0, 704, 99
42736, V, 1, 1, 1, 1, 0, 704, 99
42737, V, 1, 1, 1, 1, 0, 704, 99
42738, V, 1, 1, 1, 1, 0, 704, 99
42739, V, 1, 1, 1, 1, 0, 704, 99
42740, V, 1, 1, 1, 1, 0, 704, 99
42741, V, 1, 1, 1, 1, 0, 704, 99
42742, V, 1, 1, 1, 1, 0, 704, 99
42743, V, 1, 1, 1, 1, 0, 704, 99
42744, V, 1, 1, 1, 1, 0, 704, 99
42745, V, 1, 1, 1, 1, 0, 704, 99
42746, V, 1, 1, 1, 1, 0, 704, 99
42747, V, 1, 1, 1, 1, 0, 704, 99
42748, V, 1, 1, 1, 1, 0, 704, 99
42749, V, 1, 1, 1, 1, 0, 704, 99
42750, V, 1, 1, 1, 1, 0, 704, 99
42752, V, 1, 1, 1, 1, 0, 704, 99
42753, V, 1, 1, 1, 1, 0, 704, 100
42754, V, 1, 1, 1, 1, 0, 704, 100
42755, V, 1, 1, 1, 1, 0, 704, 100
42756, V, 1, 1, 1, 1, 0, 704, 99
42757, V, 1, 1, 1, 1, 0, 704, 100
42758, V, 1, 1, 1, 1, 0, 704, 99
42759, V, 1, 1, 1, 1, 0, 704, 99
42760, V, 1, 1, 1, 1, 0, 704, 100
42761, V, 1, 1, 1, 1, 0, 704, 100
42762, V, 1, 1, 1, 1, 0, 704, 100
42763, V, 1, 1, 1, 1, 0, 704, 100
42764, V, 1, 1, 1, 1, 0, 704, 99
42765, V, 1, 1, 1, 1, 0, 704, 100
42766, V, 1, 1, 1, 1, 0, 704, 100
42767, V, 1, 1, 1, 1, 0, 704, 100
42768, V, 1, 1, 1, 1, 0, 704, 100
42769, V, 1, 1, 1, 1, 0, 704, 100
42770, V, 1, 1, 1, 1, 0, 704, 100
42771, V, 1, 1, 1, 1, 0, 704, 100
42772, V, 1, 1, 1, 1, 0, 704, 100
42773, V, 1, 1, 1, 1, 0, 704, 100
42774, V, 1, 1, 1, 1, 0, 704, 100
42775, V, 1, 1, 1, 1, 0, 704, 100
42776, V, 1, 1, 1, 1, 0, 704, 100
42777, V, 1, 1, 1, 1, 0, 704, 100
42778, V, 1, 1, 1, 1, 0, 704, 100
42779, V, 1, 1, 1, 1, 0, 704, 100
42780, V, 1, 1, 1, 1, 0, 704, 100
42781, V, 1, 1, 1, 1, 0, 704, 100
42782, V, 1, 1, 1, 1, 0, 704, 100
42783, V, 1, 1, 1, 1, 0, 704, 100
42784, V, 1, 1, 1, 1, 0, 704, 100
42785, V, 1, 1, 1, 1, 0, 704, 100
42786, V, 1, 1, 1, 1, 0, 704, 100
42787, V, 1, 1, 1, 1, 0, 704, 100
42788, V, 1, 1, 1, 1, 0, 704, 100
42789, V, 1, 1, 1, 1, 0, 704, 100
42790, V, 1, 1, 1, 1, 0, 704, 100
42791, V, 1, 1, 1, 1, 0, 704, 100
42792, V, 1, 1, 1, 1, 0, 704, 100
42793, V, 1, 1, 1, 1, 0, 704, 100
42795, V, 1, 1, 1, 1, 0, 704, 100
42796, V, 1, 1, 1, 1, 0, 704, 100
42797, V, 1, 1, 1, 1, 0, 704, 100
42798, V, 1, 1, 1, 1, 0, 704, 100
42799, V, 1, 1, 1, 1, 0, 704, 100
42800, V, 1, 1, 1, 1, 0, 704, 100
42801, V, 1, 1, 1, 1, 0, 704, 100
42802, V, 1, 1, 1, 1, 0, 704, 100
42803, V, 1, 1, 1, 1, 0, 704, 100
42804, V, 1, 1, 1, 1, 0, 704, 100
42805, V, 1, 1, 1, 1, 0, 704, 100
42806, V, 1, 1, 1, 1, 0, 704, 100
42807, V, 1, 1, 1, 1, 0, 704, 100
42808, V, 1, 1, 1, 1, 0, 704, 100
42809, V, 1, 1, 1, 1, 0, 704, 100
42810, V, 1, 1, 1, 1, 0, 704, 100
42811, V, 1, 1, 1, 1, 0, 704, 100
42812, V, 1, 1, 1, 1, 0, 704, 100
42813, V, 1, 1, 1, 1, 0, 704, 100
42814, V, 1, 1, 1, 1, 0, 704, 100
42815, V, 1, 1, 1, 1, 0, 704, 99
42816, V, 1, 1, 1, 1, 0, 704, 100
42817, V, 1, 1, 1, 1, 0, 704, 99
42818, V, 1, 1, 1, 1, 0, 704, 99
42819, V, 1, 1, 1, 1, 0, 704, 99
42820, V, 1, 1, 1, 1, 0, 704, 99
42821, V, 1, 1, 1, 1, 0, 704, 99
42822, V, 1, 1, 1, 1, 0, 704, 99
42823, V, 1, 1, 1, 1, 0, 704, 99
42824, V, 1, 1, 1, 1, 0, 704, 99
42825, V, 1, 1, 1, 1, 0, 704, 99
42826, V, 1, 1, 1, 1, 0, 704, 99
42827, V, 1, 1, 1, 1, 0, 704, 99
42828, V, 1, 1, 1, 1, 0, 704, 99
42829, V, 1, 1, 1, 1, 0, 704, 99
42830, V, 1, 1, 1, 1, 0, 704, 99
42831, V, 1, 1, 1, 1, 0, 704, 100
42832, V, 1, 1, 1, 1, 0, 704, 99
42833, V, 1, 1, 1, 1, 0, 704, 99
42834, V, 1, 1, 1, 1, 0, 704, 99
42835, V, 1, 1, 1, 1, 0, 704, 99
42836, V, 1, 1, 1, 1, 0, 704, 99
42838, V, 1, 1, 1, 1, 0, 704, 99
42839, V, 1, 1, 1, 1, 0, 704, 99
42840, V, 1, 1, 1, 1, 0, 704, 99
42841, V, 1, 1, 1, 1, 0, 704, 100
42842, V, 1, 1, 1, 1, 0, 704, 100
42843, V, 1, 1, 1, 1, 0, 704, 100
42844, V, 1, 1, 1, 1, 0, 704, 100
42845, V, 1, 1, 1, 1, 0, 704, 99
42846, V, 1, 1, 1, 1, 0, 704, 100
42847, V, 1, 1, 1, 1, 0, 704, 100
42848, V, 1, 1, 1, 1, 0, 704, 100
42849, V, 1, 1, 1, 1, 0, 704, 100
42850, V, 1, 1, 1, 1, 0, 704, 100
42851, V, 1, 1, 1, 1, 0, 704, 100
42852, V, 1, 1, 1, 1, 0, 704, 100
42853, V, 1, 1, 1, 1, 0, 704, 100
42854, V, 1, 1, 1, 1, 0, 704, 100
42855, V, 1, 1, 1, 1, 0, 704, 100
42856, V, 1, 1, 1, 1, 0, 704, 100
42857, V, 1, 1, 1, 1, 0, 704, 100
42858, V, 1, 1, 1, 1, 0, 704, 100
42859, V, 1, 1, 1, 1, 0, 704, 100
42860, V, 1, 1, 1, 1, 0, 704, 100
42861, V, 1, 1, 1, 1, 0, 704, 100
42862, V, 1, 1, 1, 1, 0, 704, 100
42863, V, 1, 1, 1, 1, 0, 704, 100
42864, V, 1, 1, 1, 1, 0, 704, 100
42865, V, 1, 1, 1, 1, 0, 704, 99
42866, V, 1, 1, 1, 1, 0, 704, 100
42867, V, 1, 1, 1, 1, 0, 704, 100
42868, V, 1, 1, 1, 1, 0, 704, 100
42869, V, 1, 1, 1, 1, 0, 704, 100
42870, V, 1, 1, 1, 1, 0, 704, 100
42871, V, 1, 1, 1, 1, 0, 704, 100
42872, V, 1, 1, 1, 1, 0, 704, 100
42873, V, 1, 1, 1, 1, 0, 704, 100
42874, V, 1, 1, 1, 1, 0, 704, 100
42875, V, 1, 1, 1, 1, 0, 704, 100
42876, V, 1, 1, 1, 1, 0, 704, 100
42877, V, 1, 1, 1, 1, 0, 704, 100
42878, V, 1, 1, 1, 1, 0, 704, 99
42880, V, 1, 1, 1, 1, 0, 704, 100
42881, V, 1, 1, 1, 1, 0, 704, 99
42882, V, 1, 1, 1, 1, 0, 704, 100
42883, V, 1, 1, 1, 1, 0, 704, 99
42884, V, 1, 1, 1, 1, 0, 704, 100
42885, V, 1, 1, 1, 1, 0, 704, 99
42886, V, 1, 1, 1, 1, 0, 704, 99
42887, V, 1, 1, 1, 1, 0, 704, 99
42888, V, 1, 1, 1, 1, 0, 704, 99
42889, V, 1, 1, 1, 1, 0, 704, 100
42890, V, 1, 1, 1, 1, 0, 704, 99
42891, V, 1, 1, 1, 1, 0, 704, 100
42892, V, 1, 1, 1, 1, 0, 704, 99
42893, V, 1, 1, 1, 1, 0, 704, 99
42894, V, 1, 1, 1, 1, 0, 704, 99
42895, V, 1, 1, 1, 1, 0, 704, 99
42896, V, 1, 1, 1, 1, 0, 704, 99
42897, V, 1, 1, 1, 1, 0, 704, 99
42898, V, 1, 1, 1, 1, 0, 704, 99
42899, V, 1, 1, 1, 1, 0, 704, 100
42900, V, 1, 1, 1, 1, 0, 704, 99
42901, V, 1, 1, 1, 1, 0, 704, 99
42902, V, 1, 1, 1, 1, 0, 704, 99
42903, V, 1, 1, 1, 1, 0, 704, 99
42904, V, 1, 1, 1, 1, 0, 704, 99
42905, V, 1, 1, 1, 1, 0, 704, 100
42906, V, 1, 1, 1, 1, 0, 704, 99
42907, V, 1, 1, 1, 1, 0, 704, 100
42908, V, 1, 1, 1, 1, 0, 704, 99
42909, V, 1, 1, 1, 1, 0, 704, 99
42910, V, 1, 1, 1, 1, 0, 704, 99
42911, V, 1, 1, 1, 1, 0, 704, 100
42912, V, 1, 1, 1, 1, 0, 704, 100
42913, V, 1, 1, 1, 1, 0, 704, 100
42914, V, 1, 1, 1, 1, 0, 704, 100
42915, V, 1, 1, 1, 1, 0, 704, 99
42916, V, 1, 1, 1, 1, 0, 704, 100
42917, V, 1, 1, 1, 1, 0, 704, 100
42918, V, 1, 1, 1, 1, 0, 704, 100
42919, V, 1, 1, 1, 1, 0, 704, 100
42920, V, 1, 1, 1, 1, 0, 704, 100
42921, V, 1, 1, 1, 1, 0, 704, 100
42923, V, 1, 1, 1, 1, 0, 704, 100
42924, V, 1, 1, 1, 1, 0, 704, 100
42925, V, 1, 1, 1, 1, 0, 704, 100
42926, V, 1, 1, 1, 1, 0, 704, 100
42927, V, 1, 1, 1, 1, 0, 704, 100
42928, V, 1, 1, 1, 1, 0, 704, 100
42929, V, 1, 1, 1, 1, 0, 704, 100
42930, V, 1, 1, 1, 1, 0, 704, 100
42931, V, 1, 1, 1, 1, 0, 704, 100
42932, V, 1, 1, 1, 1, 0, 704, 100
42933, V, 1, 1, 1, 1, 0, 704, 100
42934, V, 1, 1, 1, 1, 0, 704, 100
42935, V, 1, 1, 1, 1, 0, 704, 100
42936, V, 1, 1, 1, 1, 0, 704, 100
42937, V, 1, 1, 1, 1, 0, 704, 100
42938, V, 1, 1, 1, 1, 0, 704, 99
42939, V, 1, 1, 1, 1, 0, 704, 100
42940, V, 1, 1, 1, 1, 0, 704, 100
42941, V, 1, 1, 1, 1, 0, 704, 99
42942, V, 1, 1, 1, 1, 0, 704, 100
42943, V, 1, 1, 1, 1, 0, 704, 99
42944, V, 1, 1, 1, 1, 0, 704, 100
42945, V, 1, 1, 1, 1, 0, 704, 99
42946, V, 1, 1, 1, 1, 0, 704, 99
42947, V, 1, 1, 1, 1, 0, 704, 99
42948, V, 1, 1, 1, 1, 0, 704, 99
42949, V, 1, 1, 1, 1, 0, 704, 99
42950, V, 1, 1, 1, 1, 0, 704, 99
42951, V, 1, 1, 1, 1, 0, 704, 99
42952, V, 1, 1, 1, 1, 0, 704, 100
42953, V, 1, 1, 1, 1, 0, 704, 99
42954, V, 1, 1, 1, 1, 0, 704, 99
42955, V, 1, 1, 1, 1, 0, 704, 99
42956, V, 1, 1, 1, 1, 0, 704, 99
42957, V, 1, 1, 1, 1, 0, 704, 99
42958, V, 1, 1, 1, 1, 0, 704, 99
42959, V, 1, 1, 1, 1, 0, 704, 99
42960, V, 1, 1, 1, 1, 0, 704, 99
42961, V, 1, 1, 1, 1, 0, 704, 99
42962, V, 1, 1, 1, 1, 0, 704, 99
42963, V, 1, 1, 1, 1, 0, 704, 99
42964, V, 1, 1, 1, 1, 0, 704, 99
42966, V, 1, 1, 1, 1, 0, 704, 99
42967, V, 1, 1, 1, 1, 0, 704, 99
42968, V, 1, 1, 1, 1, 0, 704, 99
42969, V, 1, 1, 1, 1, 0, 704, 99
42970, V, 1, 1, 1, 1, 0, 704, 99
42971, V, 1, 1, 1, 1, 0, 704, 99
42972, V, 1, 1, 1, 1, 0, 704, 99
42973, V, 1, 1, 1, 1, 0, 704, 99
42974, V, 1, 1, 1, 1, 0, 704, 99
42975, V, 1, 1, 1, 1, 0, 704, 99
42976, V, 1, 1, 1, 1, 0, 704, 99
42977, V, 1, 1, 1, 1, 0, 704, 99
42978, V, 1, 1, 1, 1, 0, 704, 99
42979, V, 1, 1, 1, 1, 0, 704, 99
42980, V, 1, 1, 1, 1, 0, 704, 99
42981, V, 1, 1, 1, 1, 0, 704, 99
42982, V, 1, 1, 1, 1, 0, 704, 99
42983, V, 1, 1, 1, 1, 0, 704, 99
42984, V, 1, 1, 1, 1, 0, 704, 99
42985, V, 1, 1, 1, 1, 0, 704, 99
42986, V, 1, 1, 1, 1, 0, 704, 99
42987, V, 1, 1, 1, 1, 0, 704, 99
42988, V, 1, 1, 1, 1, 0, 704, 99
42989, V, 1, 1, 1, 1, 0, 704, 99
42990, V, 1, 1, 1, 1, 0, 704, 100
42991, V, 1, 1, 1, 1, 0, 704, 99
42992, V, 1, 1, 1, 1, 0, 704, 99
42993, V, 1, 1, 1, 1, 0, 704, 99
42994, V, 1, 1, 1, 1, 0, 704, 99
42995, V, 1, 1, 1, 1, 0, 704, 100
42996, V, 1, 1, 1, 1, 0, 704, 99
42997, V, 1, 1, 1, 1, 0, 704, 99
42998, V, 1, 1, 1, 1, 0, 704, 100
42999, V, 1, 1, 1, 1, 0, 704, 100
43000, V, 1, 1, 1, 1, 0, 704, 100
43001, V, 1, 1, 1, 1, 0, 704, 100
43002, V, 1, 1, 1, 1, 0, 704, 100
43003, V, 1, 1, 1, 1, 0, 704, 100
43004, V, 1, 1, 1, 1, 0, 704, 99
43005, V, 1, 1, 1, 1, 0, 704, 100
43006, V, 1, 1, 1, 1, 0, 704, 100
43008, V, 1, 1, 1, 1, 0, 704, 100
43009, V, 1, 1, 1, 1, 0, 704, 100
43010, V, 1, 1, 1, 1, 0, 704, 100
43011, V, 1, 1, 1, 1, 0, 704, 100
43012, V, 1, 1, 1, 1, 0, 704, 100
43013, V, 1, 1, 1, 1, 0, 704, 100
43014, V, 1, 1, 1, 1, 0, 704, 100
43015, V, 1, 1, 1, 1, 0, 704, 100
43016, V, 1, 1, 1, 1, 0, 704, 100
43017, V, 1, 1, 1, 1, 0, 704, 100
43018, V, 1, 1, 1, 1, 0, 704, 100
43019, V, 1, 1, 1, 1, 0, 704, 99
43020, V, 1, 1, 1, 1, 0, 704, 100
43021, V, 1, 1, 1, 1, 0, 704, 100
43022, V, 1, 1, 1, 1, 0, 704, 100
43023, V, 1, 1, 1, 1, 0, 704, 100
43024, V, 1, 1, 1, 1, 0, 704, 100
43025, V, 1, 1, 1, 1, 0, 704, 100
43026, V, 1, 1, 1, 1, 0, 704, 100
43027, V, 1, 1, 1, 1, 0, 704, 100
43028, V, 1, 1, 1, 1, 0, 704, 100
43029, V, 1, 1, 1, 1, 0, 704, 100
43030, V, 1, 1, 1, 1, 0, 704, 100
43031, V, 1, 1, 1, 1, 0, 704, 100
43032, V, 1, 1, 1, 1, 0, 704, 100
43033, V, 1, 1, 1, 1, 0, 704, 100
43034, V, 1, 1, 1, 1, 0, 704, 100
43035, V, 1, 1, 1, 1, 0, 704, 100
43036, V, 1, 1, 1, 1, 0, 704, 100
43037, V, 1, 1, 1, 1, 0, 704, 100
43038, V, 1, 1, 1, 1, 0, 704, 100
43039, V, 1, 1, 1, 1, 0, 704, 100
43040, V, 1, 1, 1, 1, 0, 704, 100
43041, V, 1, 1, 1, 1, 0, 704, 100
43042, V, 1, 1, 1, 1, 0, 704, 100
43043, V, 1, 1, 1, 1, 0, 704, 100
43044, V, 1, 1, 1, 1, 0, 704, 100
43045, V, 1, 1, 1, 1, 0, 704, 100
43046, V, 1, 1, 1, 1, 0, 704, 100
43047, V, 1, 1, 1, 1, 0, 704, 99
43048, V, 1, 1, 1, 1, 0, 704, 99
43049, V, 1, 1, 1, 1, 0, 704, 99
43051, V, 1, 1, 1, 1, 0, 704, 100
43052, V, 1, 1, 1, 1, 0, 704, 99
43053, V, 1, 1, 1, 1, 0, 704, 100
43054, V, 1, 1, 1, 1, 0, 704, 99
43055, V, 1, 1, 1, 1, 0, 704, 99
43056, V, 1, 1, 1, 1, 0, 704, 100
43057, V, 1, 1, 1, 1, 0, 704, 99
43058, V, 1, 1, 1, 1, 0, 704, 99
43059, V, 1, 1, 1, 1, 0, 704, 99
43060, V, 1, 1, 1, 1, 0, 704, 100
43061, V, 1, 1, 1, 1, 0, 704, 100
43062, V, 1, 1, 1, 1, 0, 704, 99
43063, V, 1, 1, 1, 1, 0, 704, 99
43064, V, 1, 1, 1, 1, 0, 704, 100
43065, V, 1, 1, 1, 1, 0, 704, 99
43066, V, 1, 1, 1, 1, 0, 704, 99
43067, V, 1, 1, 1, 1, 0, 704, 99
43068, V, 1, 1, 1, 1, 0, 704, 100
43069, V, 1, 1, 1, 1, 0, 704, 100
43070, V, 1, 1, 1, 1, 0, 704, 100
43071, V, 1, 1, 1, 1, 0, 704, 100
43072, V, 1, 1, 1, 1, 0, 704, 100
43073, V, 1, 1, 1, 1, 0, 704, 100
43074, V, 1, 1, 1, 1, 0, 704, 100
43075, V, 1, 1, 1, 1, 0, 704, 100
43076, V, 1, 1, 1, 1, 0, 704, 100
43077, V, 1, 1, 1, 1, 0, 704, 100
43078, V, 1, 1, 1, 1, 0, 704, 100
43079, V, 1, 1, 1, 1, 0, 704, 100
43080, V, 1, 1, 1, 1, 0, 704, 100
43081, V, 1, 1, 1, 1, 0, 704, 100
43082, V, 1, 1, 1, 1, 0, 704, 100
43083, V, 1, 1, 1, 1, 0, 704, 100
43084, V, 1, 1, 1, 1, 0, 704, 100
43085, V, 1, 1, 1, 1, 0, 704, 100
43086, V, 1, 1, 1, 1, 0, 704, 100
43087, V, 1, 1, 1, 1, 0, 704, 100
43088, V, 1, 1, 1, 1, 0, 704, 100
43089, V, 1, 1, 1, 1, 0, 704, 100
43090, V, 1, 1, 1, 1, 0, 704, 100
43091, V, 1, 1, 1, 1, 0, 704, 100
43092, V, 1, 1, 1, 1, 0, 704, 100
43094, V, 1, 1, 1, 1, 0, 704, 100
43095, V, 1, 1, 1, 1, 0, 704, 100
43096, V, 1, 1, 1, 1, 0, 704, 100
43097, V, 1, 1, 1, 1, 0, 704, 100
43098, V, 1, 1, 1, 1, 0, 704, 100
43099, V, 1, 1, 1, 1, 0, 704, 100
43100, V, 1, 1, 1, 1, 0, 704, 100
43101, V, 1, 1, 1, 1, 0, 704, 100
43102, V, 1, 1, 1, 1, 0, 704, 100
43103, V, 1, 1, 1, 1, 0, 704, 100
43104, V, 1, 1, 1, 1, 0, 704, 100
43105, V, 1, 1, 1, 1, 0, 704, 100
43106, V, 1, 1, 1, 1, 0, 704, 100
43107, V, 1, 1, 1, 1, 0, 704, 100
43108, V, 1, 1, 1, 1, 0, 704, 100
43109, V, 1, 1, 1, 1, 0, 704, 100
43110, V, 1, 1, 1, 1, 0, 704, 100
43111, V, 1, 1, 1, 1, 0, 704, 100
43112, V, 1, 1, 1, 1, 0, 704, 100
43113, V, 1, 1, 1, 1, 0, 704, 100
43114, V, 1, 1, 1, 1, 0, 704, 100
43115, V, 1, 1, 1, 1, 0, 704, 99
43116, V, 1, 1, 1, 1, 0, 704, 99
43117, V, 1, 1, 1, 1, 0, 704, 99
43118, V, 1, 1, 1, 1, 0, 704, 99
43119, V, 1, 1, 1, 1, 0, 704, 99
43120, V, 1, 1, 1, 1, 0, 704, 99
43121, V, 1, 1, 1, 1, 0, 704, 99
43122, V, 1, 1, 1, 1, 0, 704, 99
43123, V, 1, 1, 1, 1, 0, 704, 99
43124, V, 1, 1, 1, 1, 0, 704, 99
43125, V, 1, 1, 1, 1, 0, 704, 99
43126, V, 1, 1, 1, 1, 0, 704, 99
43127, V, 1, 1, 1, 1, 0, 704, 99
43128, V, 1, 1, 1, 1, 0, 704, 99
43129, V, 1, 1, 1, 1, 0, 704, 99
43130, V, 1, 1, 1, 1, 0, 704, 99
43131, V, 1, 1, 1, 1, 0, 704, 99
43132, V, 1, 1, 1, 1, 0, 704, 100
43133, V, 1, 1, 1, 1, 0, 704, 99
43134, V, 1, 1, 1, 1, 0, 704, 99
43136, V, 1, 1, 1, 1, 0, 704, 99
43137, V, 1, 1, 1, 1, 0, 704, 99
43138, V, 1, 1, 1, 1, 0, 704, 99
43139, V, 1, 1, 1, 1, 0, 704, 99
43140, V, 1, 1, 1, 1, 0, 704, 99
43141, V, 1, 1, 1, 1, 0, 704, 99
43142, V, 1, 1, 1, 1, 0, 704, 99
43143, V, 1, 1, 1, 1, 0, 704, 99
43144, V, 1, 1, 1, 1, 0, 704, 99
43145, V, 1, 1, 1, 1, 0, 704, 100
43146, V, 1, 1, 1, 1, 0, 704, 99
43147, V, 1, 1, 1, 1, 0, 704, 100
43148, V, 1, 1, 1, 1, 0, 704, 100
43149, V, 1, 1, 1, 1, 0, 704, 100
43150, V, 1, 1, 1, 1, 0, 704, 100
43151, V, 1, 1, 1, 1, 0, 704, 100
43152, V, 1, 1, 1, 1, 0, 704, 100
43153, V, 1, 1, 1, 1, 0, 704, 100
43154, V, 1, 1, 1, 1, 0, 704, 99
43155, V, 1, 1, 1, 1, 0, 704, 100
43156, V, 1, 1, 1, 1, 0, 704, 100
43157, V, 1, 1, 1, 1, 0, 704, 100
43158, V, 1, 1, 1, 1, 0, 704, 100
43159, V, 1, 1, 1, 1, 0, 704, 99
43160, V, 1, 1, 1, 1, 0, 704, 100
43161, V, 1, 1, 1, 1, 0, 704, 99
43162, V, 1, 1, 1, 1, 0, 704, 100
43163, V, 1, 1, 1, 1, 0, 704, 100
43164, V, 1, 1, 1, 1, 0, 704, 100
43165, V, 1, 1, 1, 1, 0, 704, 100
43166, V, 1, 1, 1, 1, 0, 704, 99
43167, V, 1, 1, 1, 1, 0, 704, 100
43168, V, 1, 1, 1, 1, 0, 704, 100
43169, V, 1, 1, 1, 1, 0, 704, 100
43170, V, 1, 1, 1, 1, 0, 704, 99
43171, V, 1, 1, 1, 1, 0, 704, 100
43172, V, 1, 1, 1, 1, 0, 704, 100
43173, V, 1, 1, 1, 1, 0, 704, 100
43174, V, 1, 1, 1, 1, 0, 704, 100
43175, V, 1, 1, 1, 1, 0, 704, 100
43176, V, 1, 1, 1, 1, 0, 704, 100
43177, V, 1, 1, 1, 1, 0, 704, 100
43179, V, 1, 1, 1, 1, 0, 704, 100
43180, V, 1, 1, 1, 1, 0, 704, 100
43181, V, 1, 1, 1, 1, 0, 704, 100
43182, V, 1, 1, 1, 1, 0, 704, 99
43183, V, 1, 1, 1, 1, 0, 704, 100
43184, V, 1, 1, 1, 1, 0, 704, 99
43185, V, 1, 1, 1, 1, 0, 704, 99
43186, V, 1, 1, 1, 1, 0, 704, 100
43187, V, 1, 1, 1, 1, 0, 704, 99
43188, V, 1, 1, 1, 1, 0, 704, 100
43189, V, 1, 1, 1, 1, 0, 704, 100
43190, V, 1, 1, 1, 1, 0, 704, 100
43191, V, 1, 1, 1, 1, 0, 704, 99
43192, V, 1, 1, 1, 1, 0, 704, 99
43193, V, 1, 1, 1, 1, 0, 704, 99
43194, V, 1, 1, 1, 1, 0, 704, 99
43195, V, 1, 1, 1, 1, 0, 704, 99
43196, V, 1, 1, 1, 1, 0, 704, 99
43197, V, 1, 1, 1, 1, 0, 704, 99
43198, V, 1, 1, 1, 1, 0, 704, 99
43199, V, 1, 1, 1, 1, 0, 704, 99
43200, V, 1, 1, 1, 1, 0, 704, 99
43201, V, 1, 1, 1, 1, 0, 704, 99
43202, V, 1, 1, 1, 1, 0, 704, 99
43203, V, 1, 1, 1, 1, 0, 704, 99
43204, V, 1, 1, 1, 1, 0, 704, 99
43205, V, 1, 1, 1, 1, 0, 704, 99
43206, V, 1, 1, 1, 1, 0, 704, 99
43207, V, 1, 1, 1, 1, 0, 704, 99
43208, V, 1, 1, 1, 1, 0, 704, 99
43209, V, 1, 1, 1, 1, 0, 704, 99
43210, V, 1, 1, 1, 1, 0, 704, 99
43211, V, 1, 1, 1, 1, 0, 704, 99
43212, V, 1, 1, 1, 1, 0, 704, 99
43213, V, 1, 1, 1, 1, 0, 704, 99
43214, V, 1, 1, 1, 1, 0, 704, 99
43215, V, 1, 1, 1, 1, 0, 704, 100
43216, V, 1, 1, 1, 1, 0, 704, 99
43217, V, 1, 1, 1, 1, 0, 704, 99
43218, V, 1, 1, 1, 1, 0, 704, 99
43219, V, 1, 1, 1, 1, 0, 704, 99
43220, V, 1, 1, 1, 1, 0, 704, 100
43222, V, 1, 1, 1, 1, 0, 704, 99
43223, V, 1, 1, 1, 1, 0, 704, 99
43224, V, 1, 1, 1, 1, 0, 704, 99
43225, V, 1, 1, 1, 1, 0, 704, 99
43226, V, 1, 1, 1, 1, 0, 704, 100
43227, V, 1, 1, 1, 1, 0, 704, 99
43228, V, 1, 1, 1, 1, 0, 704, 100
43229, V, 1, 1, 1, 1, 0, 704, 99
43230, V, 1, 1, 1, 1, 0, 704, 100
43231, V, 1, 1, 1, 1, 0, 704, 100
43232, V, 1, 1, 1, 1, 0, 704, 100
43233, V, 1, 1, 1, 1, 0, 704, 100
43234, V, 1, 1, 1, 1, 0, 704, 100
43235, V, 1, 1, 1, 1, 0, 704, 100
43236, V, 1, 1, 1, 1, 0, 704, 99
43237, V, 1, 1, 1, 1, 0, 704, 99
43238, V, 1, 1, 1, 1, 0, 704, 100
43239, V, 1, 1, 1, 1, 0, 704, 100
43240, V, 1, 1, 1, 1, 0, 704, 100
43241, V, 1, 1, 1, 1, 0, 704, 99
43242, V, 1, 1, 1, 1, 0, 704, 100
43243, V, 1, 1, 1, 1, 0, 704, 100
43244, V, 1, 1, 1, 1, 0, 704, 100
43245, V, 1, 1, 1, 1, 0, 704, 100
43246, V, 1, 1, 1, 1, 0, 704, 100
43247, V, 1, 1, 1, 1, 0, 704, 99
43248, V, 1, 1, 1, 1, 0, 704, 100
43249, V, 1, 1, 1, 1, 0, 704, 100
43250, V, 1, 1, 1, 1, 0, 704, 99
43251, V, 1, 1, 1, 1, 0, 704, 100
43252, V, 1, 1, 1, 1, 0, 704, 99
43253, V, 1, 1, 1, 1, 0, 704, 99
43254, V, 1, 1, 1, 1, 0, 704, 99
43255, V, 1, 1, 1, 1, 0, 704, 99
43256, V, 1, 1, 1, 1, 0, 704, 99
43257, V, 1, 1, 1, 1, 0, 704, 99
43258, V, 1, 1, 1, 1, 0, 704, 99
43259, V, 1, 1, 1, 1, 0, 704, 99
43260, V, 1, 1, 1, 1, 0, 704, 99
43261, V, 1, 1, 1, 1, 0, 704, 99
43262, V, 1, 1, 1, 1, 0, 704, 99
43264, V, 1, 1, 1, 1, 0, 704, 99
43265, V, 1, 1, 1, 1, 0, 704, 99
43266, V, 1, 1, 1, 1, 0, 704, 99
43267, V, 1, 1, 1, 1, 0, 704, 99
43268, V, 1, 1, 1, 1, 0, 704, 99
43269, V, 1, 1, 1, 1, 0, 704, 99
43270, V, 1, 1, 1, 1, 0, 704, 99
43271, V, 1, 1, 1, 1, 0, 704, 99
43272, V, 1, 1, 1, 1, 0, 704, 99
43273, V, 1, 1, 1, 1, 0, 704, 99
43274, V, 1, 1, 1, 1, 0, 704, 99
43275, V, 1, 1, 1, 1, 0, 704, 99
43276, V, 1, 1, 1, 1, 0, 704, 99
43277, V, 1, 1, 1, 1, 0, 704, 99
43278, V, 1, 1, 1, 1, 0, 704, 99
43279, V, 1, 1, 1, 1, 0, 704, 99
43280, V, 1, 1, 1, 1, 0, 704, 99
43281, V, 1, 1, 1, 1, 0, 704, 99
43282, V, 1, 1, 1, 1, 0, 704, 99
43283, V, 1, 1, 1, 1, 0, 704, 99
43284, V, 1, 1, 1, 1, 0, 704, 99
43285, V, 1, 1, 1, 1, 0, 704, 99
43286, V, 1, 1, 1, 1, 0, 704, 99
43287, V, 1, 1, 1, 1, 0, 704, 99
43288, V, 1, 1, 1, 1, 0, 704, 99
43289, V, 1, 1, 1, 1, 0, 704, 99
43290, V, 1, 1, 1, 1, 0, 704, 99
43291, V, 1, 1, 1, 1, 0, 704, 99
43292, V, 1, 1, 1, 1, 0, 704, 99
43293, V, 1, 1, 1, 1, 0, 704, 99
43294, V, 1, 1, 1, 1, 0, 704, 99
43295, V, 1, 1, 1, 1, 0, 704, 99
43296, V, 1, 1, 1, 1, 0, 704, 99
43297, V, 1, 1, 1, 1, 0, 704, 99
43298, V, 1, 1, 1, 1, 0, 704, 99
43299, V, 1, 1, 1, 1, 0, 704, 99
43300, V, 1, 1, 1, 1, 0, 704, 99
43301, V, 1, 1, 1, 1, 0, 704, 99
43302, V, 1, 1, 1, 1, 0, 704, 99
43303, V, 1, 1, 1, 1, 0, 704, 100
43304, V, 1, 1, 1, 1, 0, 704, 100
43305, V, 1, 1, 1, 1, 0, 704, 99
43307, V, 1, 1, 1, 1, 0, 704, 100
43308, V, 1, 1, 1, 1, 0, 704, 100
43309, V, 1, 1, 1, 1, 0, 704, 100
43310, V, 1, 1, 1, 1, 0, 704, 100
43311, V, 1, 1, 1, 1, 0, 704, 99
43312, V, 1, 1, 1, 1, 0, 704, 100
43313, V, 1, 1, 1, 1, 0, 704, 99
43314, V, 1, 1, 1, 1, 0, 704, 100
43315, V, 1, 1, 1, 1, 0, 704, 100
43316, V, 1, 1, 1, 1, 0, 704, 100
43317, V, 1, 1, 1, 1, 0, 704, 100
43318, V, 1, 1, 1, 1, 0, 704, 100
43319, V, 1, 1, 1, 1, 0, 704, 100
43320, V, 1, 1, 1, 1, 0, 704, 100
43321, V, 1, 1, 1, 1, 0, 704, 100
43322, V, 1, 1, 1, 1, 0, 704, 100
43323, V, 1, 1, 1, 1, 0, 704, 99
43324, V, 1, 1, 1, 1, 0, 704, 100
43325, V, 1, 1, 1, 1, 0, 704, 100
43326, V, 1, 1, 1, 1, 0, 704, 100
43327, V, 1, 1, 1, 1, 0, 704, 100
43328, V, 1, 1, 1, 1, 0, 704, 100
43329, V, 1, 1, 1, 1, 0, 704, 100
43330, V, 1, 1, 1, 1, 0, 704, 99
43331, V, 1, 1, 1, 1, 0, 704, 100
43332, V, 1, 1, 1, 1, 0, 704, 100
43333, V, 1, 1, 1, 1, 0, 704, 100
43334, V, 1, 1, 1, 1, 0, 704, 100
43335, V, 1, 1, 1, 1, 0, 704, 99
43336, V, 1, 1, 1, 1, 0, 704, 99
43337, V, 1, 1, 1, 1, 0, 704, 100
43338, V, 1, 1, 1, 1, 0, 704, 99
43339, V, 1, 1, 1, 1, 0, 704, 100
43340, V, 1, 1, 1, 1, 0, 704, 99
43341, V, 1, 1, 1, 1, 0, 704, 100
43342, V, 1, 1, 1, 1, 0, 704, 99
43343, V, 1, 1, 1, 1, 0, 704, 99
43344, V, 1, 1, 1, 1, 0, 704, 99
43345, V, 1, 1, 1, 1, 0, 704, 99
43346, V, 1, 1, 1, 1, 0, 704, 99
43347, V, 1, 1, 1, 1, 0, 704, 99
43348, V, 1, 1, 1, 1, 0, 704, 99
43350, V, 1, 1, 1, 1, 0, 704, 99
43351, V, 1, 1, 1, 1, 0, 704, 99
43352, V, 1, 1, 1, 1, 0, 704, 99
43353, V, 1, 1, 1, 1, 0, 704, 99
43354, V, 1, 1, 1, 1, 0, 704, 99
43355, V, 1, 1, 1, 1, 0, 704, 99
43356, V, 1, 1, 1, 1, 0, 704, 99
43357, V, 1, 1, 1, 1, 0, 704, 99
43358, V, 1, 1, 1, 1, 0, 704, 99
43359, V, 1, 1, 1, 1, 0, 704, 99
43360, V, 1, 1, 1, 1, 0, 704, 100
43361, V, 1, 1, 1, 1, 0, 704, 99
43362, V, 1, 1, 1, 1, 0, 704, 99
43363, V, 1, 1, 1, 1, 0, 704, 100
43364, V, 1, 1, 1, 1, 0, 704, 100
43365, V, 1, 1, 1, 1, 0, 704, 99
43366, V, 1, 1, 1, 1, 0, 704, 99
43367, V, 1, 1, 1, 1, 0, 704, 99
43368, V, 1, 1, 1, 1, 0, 704, 100
43369, V, 1, 1, 1, 1, 0, 704, 100
43370, V, 1, 1, 1, 1, 0, 704, 100
43371, V, 1, 1, 1, 1, 0, 704, 100
43372, V, 1, 1, 1, 1, 0, 704, 100
43373, V, 1, 1, 1, 1, 0, 704, 100
43374, V, 1, 1, 1, 1, 0, 704, 100
43375, V, 1, 1, 1, 1, 0, 704, 100
43376, V, 1, 1, 1, 1, 0, 704, 100
43377, V, 1, 1, 1, 1, 0, 704, 100
43378, V, 1, 1, 1, 1, 0, 704, 100
43379, V, 1, 1, 1, 1, 0, 704, 100
43380, V, 1, 1, 1, 1, 0, 704, 100
43381, V, 1, 1, 1, 1, 0, 704, 100
43382, V, 1, 1, 1, 1, 0, 704, 100
43383, V, 1, 1, 1, 1, 0, 704, 100
43384, V, 1, 1, 1, 1, 0, 704, 100
43385, V, 1, 1, 1, 1, 0, 704, 100
43386, V, 1, 1, 1, 1, 0, 704, 100
43387, V, 1, 1, 1, 1, 0, 704, 100
43388, V, 1, 1, 1, 1, 0, 704, 100
43389, V, 1, 1, 1, 1, 0, 704, 100
43390, V, 1, 1, 1, 1, 0, 704, 100
43392, V, 1, 1, 1, 1, 0, 704, 100
43393, V, 1, 1, 1, 1, 0, 704, 100
43394, V, 1, 1, 1, 1, 0, 704, 100
43395, V, 1, 1, 1, 1, 0, 704, 100
43396, V, 1, 1, 1, 1, 0, 704, 100
43397, V, 1, 1, 1, 1, 0, 704, 100
43398, V, 1, 1, 1, 1, 0, 704, 100
43399, V, 1, 1, 1, 1, 0, 704, 100
43400, V, 1, 1, 1, 1, 0, 704, 100
43401, V, 1, 1, 1, 1, 0, 704, 100
43402, V, 1, 1, 1, 1, 0, 704, 100
43403, V, 1, 1, 1, 1, 0, 704, 100
43404, V, 1, 1, 1, 1, 0, 704, 100
43405, V, 1, 1, 1, 1, 0, 704, 100
43406, V, 1, 1, 1, 1, 0, 704, 100
43407, V, 1, 1, 1, 1, 0, 704, 100
43408, V, 1, 1, 1, 1, 0, 704, 100
43409, V, 1, 1, 1, 1, 0, 704, 100
43410, V, 1, 1, 1, 1, 0, 704, 100
43411, V, 1, 1, 1, 1, 0, 704, 100
43412, V, 1, 1, 1, 1, 0, 704, 100
43413, V, 1, 1, 1, 1, 0, 704, 100
43414, V, 1, 1, 1, 1, 0, 704, 100
43415, V, 1, 1, 1, 1, 0, 704, 100
43416, V, 1, 1, 1, 1, 0, 704, 100
43417, V, 1, 1, 1, 1, 0, 704, 100
43418, V, 1, 1, 1, 1, 0, 704, 100
43419, V, 1, 1, 1, 1, 0, 704, 100
43420, V, 1, 1, 1, 1, 0, 704, 100
43421, V, 1, 1, 1, 1, 0, 704, 100
43422, V, 1, 1, 1, 1, 0, 704, 100
43423, V, 1, 1, 1, 1, 0, 704, 100
43424, V, 1, 1, 1, 1, 0, 704, 100
43425, V, 1, 1, 1, 1, 0, 704, 100
43426, V, 1, 1, 1, 1, 0, 704, 100
43427, V, 1, 1, 1, 1, 0, 704, 100
43428, V, 1, 1, 1, 1, 0, 704, 100
43429, V, 1, 1, 1, 1, 0, 704, 99
43430, V, 1, 1, 1, 1, 0, 704, 100
43431, V, 1, 1, 1, 1, 0, 704, 100
43432, V, 1, 1, 1, 1, 0, 704, 100
43433, V, 1, 1, 1, 1, 0, 704, 100
43435, V, 1, 1, 1, 1, 0, 704, 100
43436, V, 1, 1, 1, 1, 0, 704, 100
43437, V, 1, 1, 1, 1, 0, 704, 100
43438, V, 1, 1, 1, 1, 0, 704, 100
43439, V, 1, 1, 1, 1, 0, 704, 100
43440, V, 1, 1, 1, 1, 0, 704, 100
43441, V, 1, 1, 1, 1, 0, 704, 100
43442, V, 1, 1, 1, 1, 0, 704, 100
43443, V, 1, 1, 1, 1, 0, 704, 100
43444, V, 1, 1, 1, 1, 0, 704, 100
43445, V, 1, 1, 1, 1, 0, 704, 100
43446, V, 1, 1, 1, 1, 0, 704, 100
43447, V, 1, 1, 1, 1, 0, 704, 100
43448, V, 1, 1, 1, 1, 0, 704, 100
43449, V, 1, 1, 1, 1, 0, 704, 100
43450, V, 1, 1, 1, 1, 0, 704, 100
43451, V, 1, 1, 1, 1, 0, 704, 100
43452, V, 1, 1, 1, 1, 0, 704, 100
43453, V, 1, 1, 1, 1, 0, 704, 100
43454, V, 1, 1, 1, 1, 0, 704, 100
43455, V, 1, 1, 1, 1, 0, 704, 100
43456, V, 1, 1, 1, 1, 0, 704, 100
43457, V, 1, 1, 1, 1, 0, 704, 100
43458, V, 1, 1, 1, 1, 0, 704, 100
43459, V, 1, 1, 1, 1, 0, 704, 100
43460, V, 1, 1, 1, 1, 0, 704, 100
43461, V, 1, 1, 1, 1, 0, 704, 100
43462, V, 1, 1, 1, 1, 0, 704, 100
43463, V, 1, 1, 1, 1, 0, 704, 100
43464, V, 1, 1, 1, 1, 0, 704, 100
43465, V, 1, 1, 1, 1, 0, 704, 100
43466, V, 1, 1, 1, 1, 0, 704, 100
43467, V, 1, 1, 1, 1, 0, 704, 100
43468, V, 1, 1, 1, 1, 0, 704, 100
43469, V, 1, 1, 1, 1, 0, 704, 100
43470, V, 1, 1, 1, 1, 0, 704, 100
43471, V, 1, 1, 1, 1, 0, 704, 100
43472, V, 1, 1, 1, 1, 0, 704, 100
43473, V, 1, 1, 1, 1, 0, 704, 100
43474, V, 1, 1, 1, 1, 0, 704, 100
43475, V, 1, 1, 1, 1, 0, 704, 100
43476, V, 1, 1, 1, 1, 0, 704, 100
43478, V, 1, 1, 1, 1, 0, 704, 100
43479, V, 1, 1, 1, 1, 0, 704, 100
43480, V, 1, 1, 1, 1, 0, 704, 100
43481, V, 1, 1, 1, 1, 0, 704, 100
43482, V, 1, 1, 1, 1, 0, 704, 100
43483, V, 1, 1, 1, 1, 0, 704, 100
43484, V, 1, 1, 1, 1, 0, 704, 100
43485, V, 1, 1, 1, 1, 0, 704, 100
43486, V, 1, 1, 1, 1, 0, 704, 100
43487, V, 1, 1, 1, 1, 0, 704, 100
43488, V, 1, 1, 1, 1, 0, 704, 100
43489, V, 1, 1, 1, 1, 0, 704, 100
43490, V, 1, 1, 1, 1, 0, 704, 100
43491, V, 1, 1, 1, 1, 0, 704, 100
43492, V, 1, 1, 1, 1, 0, 704, 100
43493, V, 1, 1, 1, 1, 0, 704, 100
43494, V, 1, 1, 1, 1, 0, 704, 100
43495, V, 1, 1, 1, 1, 0, 704, 100
43496, V, 1, 1, 1, 1, 0, 704, 100
43497, V, 1, 1, 1, 1, 0, 704, 100
43498, V, 1, 1, 1, 1, 0, 704, 100
43499, V, 1, 1, 1, 1, 0, 704, 100
43500, V, 1, 1, 1, 1, 0, 704, 100
43501, V, 1, 1, 1, 1, 0, 704, 100
43502, V, 1, 1, 1, 1, 0, 704, 100
43503, V, 1, 1, 1, 1, 0, 704, 100
43504, V, 1, 1, 1, 1, 0, 704, 100
43505, V, 1, 1, 1, 1, 0, 704, 100
43506, V, 1, 1, 1, 1, 0, 704, 100
43507, V, 1, 1, 1, 1, 0, 704, 100
43508, V, 1, 1, 1, 1, 0, 704, 100
43509, V, 1, 1, 1, 1, 0, 704, 100
43510, V, 1, 1, 1, 1, 0, 704, 100
43511, V, 1, 1, 1, 1, 0, 704, 100
43512, V, 1, 1, 1, 1, 0, 704, 100
43513, V, 1, 1, 1, 1, 0, 704, 100
43514, V, 1, 1, 1, 1, 0, 704, 100
43515, V, 1, 1, 1, 1, 0, 704, 100
43516, V, 1, 1, 1, 1, 0, 704, 100
43517, V, 1, 1, 1, 1, 0, 704, 100
43518, V, 1, 1, 1, 1, 0, 704, 100
43520, V, 1, 1, 1, 1, 0, 704, 100
43521, V, 1, 1, 1, 1, 0, 704, 100
43522, V, 1, 1, 1, 1, 0, 704, 100
43523, V, 1, 1, 1, 1, 0, 704, 100
43524, V, 1, 1, 1, 1, 0, 704, 100
43525, V, 1, 1, 1, 1, 0, 704, 100
43526, V, 1, 1, 1, 1, 0, 704, 100
43527, V, 1, 1, 1, 1, 0, 704, 100
43528, V, 1, 1, 1, 1, 0, 704, 100
43529, V, 1, 1, 1, 1, 0, 704, 100
43530, V, 1, 1, 1, 1, 0, 704, 100
43531, V, 1, 1, 1, 1, 0, 704, 100
43532, V, 1, 1, 1, 1, 0, 704, 100
43533, V, 1, 1, 1, 1, 0, 704, 100
43534, V, 1, 1, 1, 1, 0, 704, 100
43535, V, 1, 1, 1, 1, 0, 704, 100
43536, V, 1, 1, 1, 1, 0, 704, 100
43537, V, 1, 1, 1, 1, 0, 704, 100
43538, V, 1, 1, 1, 1, 0, 704, 100
43539, V, 1, 1, 1, 1, 0, 704, 100
43540, V, 1, 1, 1, 1, 0, 704, 100
43541, V, 1, 1, 1, 1, 0, 704, 100
43542, V, 1, 1, 1, 1, 0, 704, 100
43543, V, 1, 1, 1, 1, 0, 704, 100
43544, V, 1, 1, 1, 1, 0, 704, 100
43545, V, 1, 1, 1, 1, 0, 704, 100
43546, V, 1, 1, 1, 1, 0, 704, 100
43547, V, 1, 1, 1, 1, 0, 704, 100
43548, V, 1, 1, 1, 1, 0, 704, 100
43549, V, 1, 1, 1, 1, 0, 704, 100
43550, V, 1, 1, 1, 1, 0, 704, 100
43551, V, 1, 1, 1, 1, 0, 704, 100
43552, V, 1, 1, 1, 1, 0, 704, 100
43553, V, 1, 1, 1, 1, 0, 704, 100
43554, V, 1, 1, 1, 1, 0, 704, 100
43555, V, 1, 1, 1, 1, 0, 704, 100
43556, V, 1, 1, 1, 1, 0, 704, 100
43557, V, 1, 1, 1, 1, 0, 704, 100
43558, V, 1, 1, 1, 1, 0, 704, 100
43559, V, 1, 1, 1, 1, 0, 704, 100
43560, V, 1, 1, 1, 1, 0, 704, 100
43561, V, 1, 1, 1, 1, 0, 704, 100
43563, V, 1, 1, 1, 1, 0, 704, 100
43564, V, 1, 1, 1, 1, 0, 704, 100
43565, V, 1, 1, 1, 1, 0, 704, 100
43566, V, 1, 1, 1, 1, 0, 704, 100
43567, V, 1, 1, 1, 1, 0, 704, 100
43568, V, 1, 1, 1, 1, 0, 704, 100
43569, V, 1, 1, 1, 1, 0, 704, 100
43570, V, 1, 1, 1, 1, 0, 704, 100
43571, V, 1, 1, 1, 1, 0, 704, 100
43572, V, 1, 1, 1, 1, 0, 704, 100
43573, V, 1, 1, 1, 1, 0, 704, 100
43574, V, 1, 1, 1, 1, 0, 704, 100
43575, V, 1, 1, 1, 1, 0, 704, 100
43576, V, 1, 1, 1, 1, 0, 704, 100
43577, V, 1, 1, 1, 1, 0, 704, 100
43578, V, 1, 1, 1, 1, 0, 704, 100
43579, V, 1, 1, 1, 1, 0, 704, 100
43580, V, 1, 1, 1, 1, 0, 704, 100
43581, V, 1, 1, 1, 1, 0, 704, 99
43582, V, 1, 1, 1, 1, 0, 704, 100
43583, V, 1, 1, 1, 1, 0, 704, 100
43584, V, 1, 1, 1, 1, 0, 704, 100
43585, V, 1, 1, 1, 1, 0, 704, 100
43586, V, 1, 1, 1, 1, 0, 704, 100
43587, V, 1, 1, 1, 1, 0, 704, 100
43588, V, 1, 1, 1, 1, 0, 704, 100
43589, V, 1, 1, 1, 1, 0, 704, 100
43590, V, 1, 1, 1, 1, 0, 704, 100
43591, V, 1, 1, 1, 1, 0, 704, 100
43592, V, 1, 1, 1, 1, 0, 704, 100
43593, V, 1, 1, 1, 1, 0, 704, 99
43594, V, 1, 1, 1, 1, 0, 704, 100
43595, V, 1, 1, 1, 1, 0, 704, 100
43596, V, 1, 1, 1, 1, 0, 704, 100
43597, V, 1, 1, 1, 1, 0, 704, 100
43598, V, 1, 1, 1, 1, 0, 704, 100
43599, V, 1, 1, 1, 1, 0, 704, 100
43600, V, 1, 1, 1, 1, 0, 704, 100
43601, V, 1, 1, 1, 1, 0, 704, 100
43602, V, 1, 1, 1, 1, 0, 704, 100
43603, V, 1, 1, 1, 1, 0, 704, 100
43604, V, 1, 1, 1, 1, 0, 704, 100
43606, V, 1, 1, 1, 1, 0, 704, 100
43607, V, 1, 1, 1, 1, 0, 704, 100
43608, V, 1, 1, 1, 1, 0, 704, 100
43609, V, 1, 1, 1, 1, 0, 704, 100
43610, V, 1, 1, 1, 1, 0, 704, 100
43611, V, 1, 1, 1, 1, 0, 704, 100
43612, V, 1, 1, 1, 1, 0, 704, 100
43613, V, 1, 1, 1, 1, 0, 704, 100
43614, V, 1, 1, 1, 1, 0, 704, 100
43615, V, 1, 1, 1, 1, 0, 704, 100
43616, V, 1, 1, 1, 1, 0, 704, 100
43617, V, 1, 1, 1, 1, 0, 704, 100
43618, V, 1, 1, 1, 1, 0, 704, 100
43619, V, 1, 1, 1, 1, 0, 704, 100
43620, V, 1, 1, 1, 1, 0, 704, 100
43621, V, 1, 1, 1, 1, 0, 704, 100
43622, V, 1, 1, 1, 1, 0, 704, 100
43623, V, 1, 1, 1, 1, 0, 704, 100
43624, V, 1, 1, 1, 1, 0, 704, 100
43625, V, 1, 1, 1, 1, 0, 704, 100
43626, V, 1, 1, 1, 1, 0, 704, 100
43627, V, 1, 1, 1, 1, 0, 704, 100
43628, V, 1, 1, 1, 1, 0, 704, 100
43629, V, 1, 1, 1, 1, 0, 704, 100
43630, V, 1, 1, 1, 1, 0, 704, 100
43631, V, 1, 1, 1, 1, 0, 704, 100
43632, V, 1, 1, 1, 1, 0, 704, 100
43633, V, 1, 1, 1, 1, 0, 704, 100
43634, V, 1, 1, 1, 1, 0, 704, 100
43635, V, 1, 1, 1, 1, 0, 704, 100
43636, V, 1, 1, 1, 1, 0, 704, 100
43637, V, 1, 1, 1, 1, 0, 704, 100
43638, V, 1, 1, 1, 1, 0, 704, 100
43639, V, 1, 1, 1, 1, 0, 704, 100
43640, V, 1, 1, 1, 1, 0, 704, 100
43641, V, 1, 1, 1, 1, 0, 704, 100
43642, V, 1, 1, 1, 1, 0, 704, 100
43643, V, 1, 1, 1, 1, 0, 704, 100
43644, V, 1, 1, 1, 1, 0, 704, 100
43645, V, 1, 1, 1, 1, 0, 704, 100
43646, V, 1, 1, 1, 1, 0, 704, 100
43648, V, 1, 1, 1, 1, 0, 704, 100
43649, V, 1, 1, 1, 1, 0, 704, 100
43650, V, 1, 1, 1, 1, 0, 704, 100
43651, V, 1, 1, 1, 1, 0, 704, 100
43652, V, 1, 1, 1, 1, 0, 704, 100
43653, V, 1, 1, 1, 1, 0, 704, 100
43654, V, 1, 1, 1, 1, 0, 704, 100
43655, V, 1, 1, 1, 1, 0, 704, 100
43656, V, 1, 1, 1, 1, 0, 704, 100
43657, V, 1, 1, 1, 1, 0, 704, 100
43658, V, 1, 1, 1, 1, 0, 704, 100
43659, V, 1, 1, 1, 1, 0, 704, 100
43660, V, 1, 1, 1, 1, 0, 704, 100
43661, V, 1, 1, 1, 1, 0, 704, 100
43662, V, 1, 1, 1, 1, 0, 704, 100
43663, V, 1, 1, 1, 1, 0, 704, 100
43664, V, 1, 1, 1, 1, 0, 704, 100
43665, V, 1, 1, 1, 1, 0, 704, 100
43666, V, 1, 1, 1, 1, 0, 704, 100
43667, V, 1, 1, 1, 1, 0, 704, 100
43668, V, 1, 1, 1, 1, 0, 704, 100
43669, V, 1, 1, 1, 1, 0, 704, 100
43670, V, 1, 1, 1, 1, 0, 704, 100
43671, V, 1, 1, 1, 1, 0, 704, 100
43672, V, 1, 1, 1, 1, 0, 704, 100
43673, V, 1, 1, 1, 1, 0, 704, 100
43674, V, 1, 1, 1, 1, 0, 704, 100
43675, V, 1, 1, 1, 1, 0, 704, 100
43676, V, 1, 1, 1, 1, 0, 704, 100
43677, V, 1, 1, 1, 1, 0, 704, 100
43678, V, 1, 1, 1, 1, 0, 704, 100
43679, V, 1, 1, 1, 1, 0, 704, 100
43680, V, 1, 1, 1, 1, 0, 704, 100
43681, V, 1, 1, 1, 1, 0, 704, 100
43682, V, 1, 1, 1, 1, 0, 704, 100
43683, V, 1, 1, 1, 1, 0, 704, 100
43684, V, 1, 1, 1, 1, 0, 704, 100
43685, V, 1, 1, 1, 1, 0, 704, 100
43686, V, 1, 1, 1, 1, 0, 704, 100
43687, V, 1, 1, 1, 1, 0, 704, 100
43688, V, 1, 1, 1, 1, 0, 704, 100
43689, V, 1, 1, 1, 1, 0, 704, 100
43691, V, 1, 1, 1, 1, 0, 704, 100
43692, V, 1, 1, 1, 1, 0, 704, 100
43693, V, 1, 1, 1, 1, 0, 704, 100
43694, V, 1, 1, 1, 1, 0, 704, 100
43695, V, 1, 1, 1, 1, 0, 704, 100
43696, V, 1, 1, 1, 1, 0, 704, 100
43697, V, 1, 1, 1, 1, 0, 704, 100
43698, V, 1, 1, 1, 1, 0, 704, 100
43699, V, 1, 1, 1, 1, 0, 704, 100
43700, V, 1, 1, 1, 1, 0, 704, 100
43701, V, 1, 1, 1, 1, 0, 704, 100
43702, V, 1, 1, 1, 1, 0, 704, 100
43703, V, 1, 1, 1, 1, 0, 704, 100
43704, V, 1, 1, 1, 1, 0, 704, 100
43705, V, 1, 1, 1, 1, 0, 704, 100
43706, V, 1, 1, 1, 1, 0, 704, 100
43707, V, 1, 1, 1, 1, 0, 704, 100
43708, V, 1, 1, 1, 1, 0, 704, 100
43709, V, 1, 1, 1, 1, 0, 704, 100
43710, V, 1, 1, 1, 1, 0, 704, 100
43711, V, 1, 1, 1, 1, 0, 704, 100
43712, V, 1, 1, 1, 1, 0, 704, 100
43713, V, 1, 1, 1, 1, 0, 704, 100
43714, V, 1, 1, 1, 1, 0, 704, 100
43715, V, 1, 1, 1, 1, 0, 704, 99
43716, V, 1, 1, 1, 1, 0, 704, 99
43717, V, 1, 1, 1, 1, 0, 704, 99
43718, V, 1, 1, 1, 1, 0, 704, 99
43719, V, 1, 1, 1, 1, 0, 704, 99
43720, V, 1, 1, 1, 1, 0, 704, 99
43721, V, 1, 1, 1, 1, 0, 704, 99
43722, V, 1, 1, 1, 1, 0, 704, 99
43723, V, 1, 1, 1, 1, 0, 704, 99
43724, V, 1, 1, 1, 1, 0, 704, 99
43725, V, 1, 1, 1, 1, 0, 704, 99
43726, V, 1, 1, 1, 1, 0, 704, 99
43727, V, 1, 1, 1, 1, 0, 704, 99
43728, V, 1, 1, 1, 1, 0, 704, 99
43729, V, 1, 1, 1, 1, 0, 704, 99
43730, V, 1, 1, 1, 1, 0, 704, 99
43731, V, 1, 1, 1, 1, 0, 704, 99
43732, V, 1, 1, 1, 1, 0, 704, 99
43734, V, 1, 1, 1, 1, 0, 704, 99
43735, V, 1, 1, 1, 1, 0, 704, 99
43736, V, 1, 1, 1, 1, 0, 704, 99
43737, V, 1, 1, 1, 1, 0, 704, 99
43738, V, 1, 1, 1, 1, 0, 704, 99
43739, V, 1, 1, 1, 1, 0, 704, 99
43740, V, 1, 1, 1, 1, 0, 704, 99
43741, V, 1, 1, 1, 1, 0, 704, 99
43742, V, 1, 1, 1, 1, 0, 704, 99
43743, V, 1, 1, 1, 1, 0, 704, 99
43744, V, 1, 1, 1, 1, 0, 704, 99
43745, V, 1, 1, 1, 1, 0, 704, 99
43746, V, 1, 1, 1, 1, 0, 704, 99
43747, V, 1, 1, 1, 1, 0, 704, 99
43748, V, 1, 1, 1, 1, 0, 704, 99
43749, V, 1, 1, 1, 1, 0, 704, 99
43750, V, 1, 1, 1, 1, 0, 704, 99
43751, V, 1, 1, 1, 1, 0, 704, 99
43752, V, 1, 1, 1, 1, 0, 704, 99
43753, V, 1, 1, 1, 1, 0, 704, 99
43754, V, 1, 1, 1, 1, 0, 704, 99
43755, V, 1, 1, 1, 1, 0, 704, 99
43756, V, 1, 1, 1, 1, 0, 704, 99
43757, V, 1, 1, 1, 1, 0, 704, 99
43758, V, 1, 1, 1, 1, 0, 704, 99
43759, V, 1, 1, 1, 1, 0, 704, 99
43760, V, 1, 1, 1, 1, 0, 704, 99
43761, V, 1, 1, 1, 1, 0, 704, 99
43762, V, 1, 1, 1, 1, 0, 704, 99
43763, V, 1, 1, 1, 1, 0, 704, 99
43764, V, 1, 1, 1, 1, 0, 704, 99
43765, V, 1, 1, 1, 1, 0, 704, 99
43766, V, 1, 1, 1, 1, 0, 704, 99
43767, V, 1, 1, 1, 1, 0, 704, 99
43768, V, 1, 1, 1, 1, 0, 704, 99
43769, V, 1, 1, 1, 1, 0, 704, 99
43770, V, 1, 1, 1, 1, 0, 704, 99
43771, V, 1, 1, 1, 1, 0, 704, 99
43772, V, 1, 1, 1, 1, 0, 704, 99
43773, V, 1, 1, 1, 1, 0, 704, 99
43774, V, 1, 1, 1, 1, 0, 704, 99
43776, V, 1, 1, 1, 1, 0, 704, 99
43777, V, 1, 1, 1, 1, 0, 704, 99
43778, V, 1, 1, 1, 1, 0, 704, 99
43779, V, 1, 1, 1, 1, 0, 704, 99
43780, V, 1, 1, 1, 1, 0, 704, 99
43781, V, 1, 1, 1, 1, 0, 704, 99
43782, V, 1, 1, 1, 1, 0, 704, 99
43783, V, 1, 1, 1, 1, 0, 704, 99
43784, V, 1, 1, 1, 1, 0, 704, 99
43785, V, 1, 1, 1, 1, 0, 704, 99
43786, V, 1, 1, 1, 1, 0, 704, 99
43787, V, 1, 1, 1, 1, 0, 704, 99
43788, V, 1, 1, 1, 1, 0, 704, 99
43789, V, 1, 1, 1, 1, 0, 704, 99
43790, V, 1, 1, 1, 1, 0, 704, 99
43791, V, 1, 1, 1, 1, 0, 704, 99
43792, V, 1, 1, 1, 1, 0, 704, 99
43793, V, 1, 1, 1, 1, 0, 704, 99
43794, V, 1, 1, 1, 1, 0, 704, 99
43795, V, 1, 1, 1, 1, 0, 704, 99
43796, V, 1, 1, 1, 1, 0, 704, 99
43797, V, 1, 1, 1, 1, 0, 704, 99
43798, V, 1, 1, 1, 1, 0, 704, 99
43799, V, 1, 1, 1, 1, 0, 704, 99
43800, V, 1, 1, 1, 1, 0, 704, 99
43801, V, 1, 1, 1, 1, 0, 704, 99
43802, V, 1, 1, 1, 1, 0, 704, 99
43803, V, 1, 1, 1, 1, 0, 704, 99
43804, V, 1, 1, 1, 1, 0, 704, 99
43805, V, 1, 1, 1, 1, 0, 704, 99
43806, V, 1, 1, 1, 1, 0, 704, 99
43807, V, 1, 1, 1, 1, 0, 704, 99
43808, V, 1, 1, 1, 1, 0, 704, 99
43809, V, 1, 1, 1, 1, 0, 704, 99
43810, V, 1, 1, 1, 1, 0, 704, 99
43811, V, 1, 1, 1, 1, 0, 704, 99
43812, V, 1, 1, 1, 1, 0, 704, 99
43813, V, 1, 1, 1, 1, 0, 704, 99
43814, V, 1, 1, 1, 1, 0, 704, 99
43815, V, 1, 1, 1, 1, 0, 704, 99
43816, V, 1, 1, 1, 1, 0, 704, 99
43817, V, 1, 1, 1, 1, 0, 704, 99
43819, V, 1, 1, 1, 1, 0, 704, 99
43820, V, 1, 1, 1, 1, 0, 704, 99
43821, V, 1, 1, 1, 1, 0, 704, 99
43822, V, 1, 1, 1, 1, 0, 704, 99
43823, V, 1, 1, 1, 1, 0, 704, 99
43824, V, 1, 1, 1, 1, 0, 704, 99
43825, V, 1, 1, 1, 1, 0, 704, 99
43826, V, 1, 1, 1, 1, 0, 704, 99
43827, V, 1, 1, 1, 1, 0, 704, 99
43828, V, 1, 1, 1, 1, 0, 704, 99
43829, V, 1, 1, 1, 1, 0, 704, 99
43830, V, 1, 1, 1, 1, 0, 704, 99
43831, V, 1, 1, 1, 1, 0, 704, 99
43832, V, 1, 1, 1, 1, 0, 704, 99
43833, V, 1, 1, 1, 1, 0, 704, 99
43834, V, 1, 1, 1, 1, 0, 704, 99
43835, V, 1, 1, 1, 1, 0, 704, 99
43836, V, 1, 1, 1, 1, 0, 704, 99
43837, V, 1, 1, 1, 1, 0, 704, 99
43838, V, 1, 1, 1, 1, 0, 704, 99
43839, V, 1, 1, 1, 1, 0, 704, 99
43840, V, 1, 1, 1, 1, 0, 704, 99
43841, V, 1, 1, 1, 1, 0, 704, 99
43842, V, 1, 1, 1, 1, 0, 704, 99
43843, V, 1, 1, 1, 1, 0, 704, 99
43844, V, 1, 1, 1, 1, 0, 704, 99
43845, V, 1, 1, 1, 1, 0, 704, 99
43846, V, 1, 1, 1, 1, 0, 704, 99
43847, V, 1, 1, 1, 1, 0, 704, 99
43848, V, 1, 1, 1, 1, 0, 704, 99
43849, V, 1, 1, 1, 1, 0, 704, 99
43850, V, 1, 1, 1, 1, 0, 704, 99
43851, V, 1, 1, 1, 1, 0, 704, 99
43852, V, 1, 1, 1, 1, 0, 704, 99
43853, V, 1, 1, 1, 1, 0, 704, 99
43854, V, 1, 1, 1, 1, 0, 704, 99
43855, V, 1, 1, 1, 1, 0, 704, 99
43856, V, 1, 1, 1, 1, 0, 704, 99
43857, V, 1, 1, 1, 1, 0, 704, 99
43858, V, 1, 1, 1, 1, 0, 704, 99
43859, V, 1, 1, 1, 1, 0, 704, 99
43860, V, 1, 1, 1, 1, 0, 704, 99
43862, V, 1, 1, 1, 1, 0, 704, 99
43863, V, 1, 1, 1, 1, 0, 704, 99
43864, V, 1, 1, 1, 1, 0, 704, 99
43865, V, 1, 1, 1, 1, 0, 704, 99
43866, V, 1, 1, 1, 1, 0, 704, 99
43867, V, 1, 1, 1, 1, 0, 704, 99
43868, V, 1, 1, 1, 1, 0, 704, 99
43869, V, 1, 1, 1, 1, 0, 704, 99
43870, V, 1, 1, 1, 1, 0, 704, 99
43871, V, 1, 1, 1, 1, 0, 704, 99
43872, V, 1, 1, 1, 1, 0, 704, 99
43873, V, 1, 1, 1, 1, 0, 704, 99
43874, V, 1, 1, 1, 1, 0, 704, 99
43875, V, 1, 1, 1, 1, 0, 704, 99
43876, V, 1, 1, 1, 1, 0, 704, 99
43877, V, 1, 1, 1, 1, 0, 704, 99
43878, V, 1, 1, 1, 1, 0, 704, 99
43879, V, 1, 1, 1, 1, 0, 704, 99
43880, V, 1, 1, 1, 1, 0, 704, 99
43881, V, 1, 1, 1, 1, 0, 704, 99
43882, V, 1, 1, 1, 1, 0, 704, 99
43883, V, 1, 1, 1, 1, 0, 704, 99
43884, V, 1, 1, 1, 1, 0, 704, 99
43885, V, 1, 1, 1, 1, 0, 704, 99
43886, V, 1, 1, 1, 1, 0, 704, 99
43887, V, 1, 1, 1, 1, 0, 704, 99
43888, V, 1, 1, 1, 1, 0, 704, 99
43889, V, 1, 1, 1, 1, 0, 704, 99
43890, V, 1, 1, 1, 1, 0, 704, 99
43891, V, 1, 1, 1, 1, 0, 704, 99
43892, V, 1, 1, 1, 1, 0, 704, 99
43893, V, 1, 1, 1, 1, 0, 704, 100
43894, V, 1, 1, 1, 1, 0, 704, 99
43895, V, 1, 1, 1, 1, 0, 704, 99
43896, V, 1, 1, 1, 1, 0, 704, 99
43897, V, 1, 1, 1, 1, 0, 704, 99
43898, V, 1, 1, 1, 1, 0, 704, 100
43899, V, 1, 1, 1, 1, 0, 704, 100
43900, V, 1, 1, 1, 1, 0, 704, 100
43901, V, 1, 1, 1, 1, 0, 704, 100
43902, V, 1, 1, 1, 1, 0, 704, 100
43904, V, 1, 1, 1, 1, 0, 704, 100
43905, V, 1, 1, 1, 1, 0, 704, 100
43906, V, 1, 1, 1, 1, 0, 704, 100
43907, V, 1, 1, 1, 1, 0, 704, 100
43908, V, 1, 1, 1, 1, 0, 704, 100
43909, V, 1, 1, 1, 1, 0, 704, 100
43910, V, 1, 1, 1, 1, 0, 704, 100
43911, V, 1, 1, 1, 1, 0, 704, 100
43912, V, 1, 1, 1, 1, 0, 704, 100
43913, V, 1, 1, 1, 1, 0, 704, 100
43914, V, 1, 1, 1, 1, 0, 704, 100
43915, V, 1, 1, 1, 1, 0, 704, 100
43916, V, 1, 1, 1, 1, 0, 704, 100
43917, V, 1, 1, 1, 1, 0, 704, 100
43918, V, 1, 1, 1, 1, 0, 704, 100
43919, V, 1, 1, 1, 1, 0, 704, 100
43920, V, 1, 1, 1, 1, 0, 704, 100
43921, V, 1, 1, 1, 1, 0, 704, 100
43922, V, 1, 1, 1, 1, 0, 704, 100
43923, V, 1, 1, 1, 1, 0, 704, 100
43924, V, 1, 1, 1, 1, 0, 704, 100
43925, V, 1, 1, 1, 1, 0, 704, 100
43926, V, 1, 1, 1, 1, 0, 704, 100
43927, V, 1, 1, 1, 1, 0, 704, 100
43928, V, 1, 1, 1, 1, 0, 704, 100
43929, V, 1, 1, 1, 1, 0, 704, 100
43930, V, 1, 1, 1, 1, 0, 704, 100
43931, V, 1, 1, 1, 1, 0, 704, 100
43932, V, 1, 1, 1, 1, 0, 704, 100
43933, V, 1, 1, 1, 1, 0, 704, 100
43934, V, 1, 1, 1, 1, 0, 704, 100
43935, V, 1, 1, 1, 1, 0, 704, 100
43936, V, 1, 1, 1, 1, 0, 704, 100
43937, V, 1, 1, 1, 1, 0, 704, 100
43938, V, 1, 1, 1, 1, 0, 704, 100
43939, V, 1, 1, 1, 1, 0, 704, 100
43940, V, 1, 1, 1, 1, 0, 704, 100
43941, V, 1, 1, 1, 1, 0, 704, 100
43942, V, 1, 1, 1, 1, 0, 704, 100
43943, V, 1, 1, 1, 1, 0, 704, 100
43944, V, 1, 1, 1, 1, 0, 704, 100
43945, V, 1, 1, 1, 1, 0, 704, 100
43947, V, 1, 1, 1, 1, 0, 704, 100
43948, V, 1, 1, 1, 1, 0, 704, 100
43949, V, 1, 1, 1, 1, 0, 704, 100
43950, V, 1, 1, 1, 1, 0, 704, 100
43951, V, 1, 1, 1, 1, 0, 704, 100
43952, V, 1, 1, 1, 1, 0, 704, 100
43953, V, 1, 1, 1, 1, 0, 704, 100
43954, V, 1, 1, 1, 1, 0, 704, 100
43955, V, 1, 1, 1, 1, 0, 704, 100
43956, V, 1, 1, 1, 1, 0, 704, 100
43957, V, 1, 1, 1, 1, 0, 704, 100
43958, V, 1, 1, 1, 1, 0, 704, 100
43959, V, 1, 1, 1, 1, 0, 704, 100
43960, V, 1, 1, 1, 1, 0, 704, 100
43961, V, 1, 1, 1, 1, 0, 704, 100
43962, V, 1, 1, 1, 1, 0, 704, 100
43963, V, 1, 1, 1, 1, 0, 704, 100
43964, V, 1, 1, 1, 1, 0, 704, 100
43965, V, 1, 1, 1, 1, 0, 704, 100
43966, V, 1, 1, 1, 1, 0, 704, 100
43967, V, 1, 1, 1, 1, 0, 704, 100
43968, V, 1, 1, 1, 1, 0, 704, 100
43969, V, 1, 1, 1, 1, 0, 704, 100
43970, V, 1, 1, 1, 1, 0, 704, 100
43971, V, 1, 1, 1, 1, 0, 704, 100
43972, V, 1, 1, 1, 1, 0, 704, 100
43973, V, 1, 1, 1, 1, 0, 704, 100
43974, V, 1, 1, 1, 1, 0, 704, 100
43975, V, 1, 1, 1, 1, 0, 704, 100
43976, V, 1, 1, 1, 1, 0, 704, 100
43977, V, 1, 1, 1, 1, 0, 704, 100
43978, V, 1, 1, 1, 1, 0, 704, 100
43979, V, 1, 1, 1, 1, 0, 704, 100
43980, V, 1, 1, 1, 1, 0, 704, 100
43981, V, 1, 1, 1, 1, 0, 704, 100
43982, V, 1, 1, 1, 1, 0, 704, 100
43983, V, 1, 1, 1, 1, 0, 704, 100
43984, V, 1, 1, 1, 1, 0, 704, 100
43985, V, 1, 1, 1, 1, 0, 704, 100
43986, V, 1, 1, 1, 1, 0, 704, 100
43987, V, 1, 1, 1, 1, 0, 704, 100
43988, V, 1, 1, 1, 1, 0, 704, 100
43990, V, 1, 1, 1, 1, 0, 704, 100
43991, V, 1, 1, 1, 1, 0, 704, 100
43992, V, 1, 1, 1, 1, 0, 704, 100
43993, V, 1, 1, 1, 1, 0, 704, 100
43994, V, 1, 1, 1, 1, 0, 704, 100
43995, V, 1, 1, 1, 1, 0, 704, 100
43996, V, 1, 1, 1, 1, 0, 704, 100
43997, V, 1, 1, 1, 1, 0, 704, 100
43998, V, 1, 1, 1, 1, 0, 704, 100
43999, V, 1, 1, 1, 1, 0, 704, 100
44000, V, 1, 1, 1, 1, 0, 704, 100
44001, V, 1, 1, 1, 1, 0, 704, 100
44002, V, 1, 1, 1, 1, 0, 704, 100
44003, V, 1, 1, 1, 1, 0, 704, 100
44004, V, 1, 1, 1, 1, 0, 704, 100
44005, V, 1, 1, 1, 1, 0, 704, 100
44006, V, 1, 1, 1, 1, 0, 704, 100
44007, V, 1, 1, 1, 1, 0, 704, 100
44008, V, 1, 1, 1, 1, 0, 704, 100
44009, V, 1, 1, 1, 1, 0, 704, 100
44010, V, 1, 1, 1, 1, 0, 704, 100
44011, V, 1, 1, 1, 1, 0, 704, 100
44012, V, 1, 1, 1, 1, 0, 704, 100
44013, V, 1, 1, 1, 1, 0, 704, 100
44014, V, 1, 1, 1, 1, 0, 704, 100
44015, V, 1, 1, 1, 1, 0, 704, 100
44016, V, 1, 1, 1, 1, 0, 704, 100
44017, V, 1, 1, 1, 1, 0, 704, 100
44018, V, 1, 1, 1, 1, 0, 704, 100
44019, V, 1, 1, 1, 1, 0, 704, 100
44020, V, 1, 1, 1, 1, 0, 704, 100
44021, V, 1, 1, 1, 1, 0, 704, 100
44022, V, 1, 1, 1, 1, 0, 704, 100
44023, V, 1, 1, 1, 1, 0, 704, 100
44024, V, 1, 1, 1, 1, 0, 704, 100
44025, V, 1, 1, 1, 1, 0, 704, 100
44026, V, 1, 1, 1, 1, 0, 704, 100
44027, V, 1, 1, 1, 1, 0, 704, 100
44028, V, 1, 1, 1, 1, 0, 704, 100
44029, V, 1, 1, 1, 1, 0, 704, 100
44030, V, 1, 1, 1, 1, 0, 704, 100
44032, V, 1, 1, 1, 1, 0, 704, 100
44033, V, 1, 1, 1, 1, 0, 704, 100
44034, V, 1, 1, 1, 1, 0, 704, 100
44035, V, 1, 1, 1, 1, 0, 704, 100
44036, V, 1, 1, 1, 1, 0, 704, 100
44037, V, 1, 1, 1, 1, 0, 704, 100
44038, V, 1, 1, 1, 1, 0, 704, 100
44039, V, 1, 1, 1, 1, 0, 704, 100
44040, V, 1, 1, 1, 1, 0, 704, 100
44041, V, 1, 1, 1, 1, 0, 704, 100
44042, V, 1, 1, 1, 1, 0, 704, 100
44043, V, 1, 1, 1, 1, 0, 704, 100
44044, V, 1, 1, 1, 1, 0, 704, 100
44045, V, 1, 1, 1, 1, 0, 704, 100
44046, V, 1, 1, 1, 1, 0, 704, 100
44047, V, 1, 1, 1, 1, 0, 704, 100
44048, V, 1, 1, 1, 1, 0, 704, 100
44049, V, 1, 1, 1, 1, 0, 704, 100
44050, V, 1, 1, 1, 1, 0, 704, 100
44051, V, 1, 1, 1, 1, 0, 704, 100
44052, V, 1, 1, 1, 1, 0, 704, 100
44053, V, 1, 1, 1, 1, 0, 704, 100
44054, V, 1, 1, 1, 1, 0, 704, 100
44055, V, 1, 1, 1, 1, 0, 704, 100
44056, V, 1, 1, 1, 1, 0, 704, 100
44057, V, 1, 1, 1, 1, 0, 704, 100
44058, V, 1, 1, 1, 1, 0, 704, 100
44059, V, 1, 1, 1, 1, 0, 704, 100
44060, V, 1, 1, 1, 1, 0, 704, 100
44061, V, 1, 1, 1, 1, 0, 704, 100
44062, V, 1, 1, 1, 1, 0, 704, 100
44063, V, 1, 1, 1, 1, 0, 704, 100
44064, V, 1, 1, 1, 1, 0, 704, 100
44065, V, 1, 1, 1, 1, 0, 704, 100
44066, V, 1, 1, 1, 1, 0, 704, 100
44067, V, 1, 1, 1, 1, 0, 704, 100
44068, V, 1, 1, 1, 1, 0, 704, 100
44069, V, 1, 1, 1, 1, 0, 704, 100
44070, V, 1, 1, 1, 1, 0, 704, 100
44071, V, 1, 1, 1, 1, 0, 704, 100
44072, V, 1, 1, 1, 1, 0, 704, 100
44073, V, 1, 1, 1, 1, 0, 704, 100
44075, V, 1, 1, 1, 1, 0, 704, 100
44076, V, 1, 1, 1, 1, 0, 704, 100
44077, V, 1, 1, 1, 1, 0, 704, 100
44078, V, 1, 1, 1, 1, 0, 704, 100
44079, V, 1, 1, 1, 1, 0, 704, 100
44080, V, 1, 1, 1, 1, 0, 704, 100
44081, V, 1, 1, 1, 1, 0, 704, 100
44082, V, 1, 1, 1, 1, 0, 704, 100
44083, V, 1, 1, 1, 1, 0, 704, 100
44084, V, 1, 1, 1, 1, 0, 704, 100
44085, V, 1, 1, 1, 1, 0, 704, 100
44086, V, 1, 1, 1, 1, 0, 704, 100
44087, V, 1, 1, 1, 1, 0, 704, 100
44088, V, 1, 1, 1, 1, 0, 704, 100
44089, V, 1, 1, 1, 1, 0, 704, 100
44090, V, 1, 1, 1, 1, 0, 704, 100
44091, V, 1, 1, 1, 1, 0, 704, 100
44092, V, 1, 1, 1, 1, 0, 704, 100
44093, V, 1, 1, 1, 1, 0, 704, 100
44094, V, 1, 1, 1, 1, 0, 704, 100
44095, V, 1, 1, 1, 1, 0, 704, 100
44096, V, 1, 1, 1, 1, 0, 704, 100
44097, V, 1, 1, 1, 1, 0, 704, 100
44098, V, 1, 1, 1, 1, 0, 704, 100
44099, V, 1, 1, 1, 1, 0, 704, 100
44100, V, 1, 1, 1, 1, 0, 704, 100
44101, V, 1, 1, 1, 1, 0, 704, 100
44102, V, 1, 1, 1, 1, 0, 704, 100
44103, V, 1, 1, 1, 1, 0, 704, 100
44104, V, 1, 1, 1, 1, 0, 704, 100
44105, V, 1, 1, 1, 1, 0, 704, 100
44106, V, 1, 1, 1, 1, 0, 704, 100
44107, V, 1, 1, 1, 1, 0, 704, 100
44108, V, 1, 1, 1, 1, 0, 704, 100
44109, V, 1, 1, 1, 1, 0, 704, 100
44110, V, 1, 1, 1, 1, 0, 704, 100
44111, V, 1, 1, 1, 1, 0, 704, 100
44112, V, 1, 1, 1, 1, 0, 704, 100
44113, V, 1, 1, 1, 1, 0, 704, 100
44114, V, 1, 1, 1, 1, 0, 704, 100
44115, V, 1, 1, 1, 1, 0, 704, 100
44116, V, 1, 1, 1, 1, 0, 704, 100
44118, V, 1, 1, 1, 1, 0, 704, 100
44119, V, 1, 1, 1, 1, 0, 704, 100
44120, V, 1, 1, 1, 1, 0, 704, 100
44121, V, 1, 1, 1, 1, 0, 704, 100
44122, V, 1, 1, 1, 1, 0, 704, 100
44123, V, 1, 1, 1, 1, 0, 704, 100
44124, V, 1, 1, 1, 1, 0, 704, 100
44125, V, 1, 1, 1, 1, 0, 704, 100
44126, V, 1, 1, 1, 1, 0, 704, 100
44127, V, 1, 1, 1, 1, 0, 704, 100
44128, V, 1, 1, 1, 1, 0, 704, 100
44129, V, 1, 1, 1, 1, 0, 704, 100
44130, V, 1, 1, 1, 1, 0, 704, 100
44131, V, 1, 1, 1, 1, 0, 704, 100
44132, V, 1, 1, 1, 1, 0, 704, 100
44133, V, 1, 1, 1, 1, 0, 704, 100
44134, V, 1, 1, 1, 1, 0, 704, 100
44135, V, 1, 1, 1, 1, 0, 704, 100
44136, V, 1, 1, 1, 1, 0, 704, 100
44137, V, 1, 1, 1, 1, 0, 704, 100
44138, V, 1, 1, 1, 1, 0, 704, 100
44139, V, 1, 1, 1, 1, 0, 704, 100
44140, V, 1, 1, 1, 1, 0, 704, 100
44141, V, 1, 1, 1, 1, 0, 704, 100
44142, V, 1, 1, 1, 1, 0, 704, 100
44143, V, 1, 1, 1, 1, 0, 704, 100
44144, V, 1, 1, 1, 1, 0, 704, 100
44145, V, 1, 1, 1, 1, 0, 704, 100
44146, V, 1, 1, 1, 1, 0, 704, 100
44147, V, 1, 1, 1, 1, 0, 704, 100
44148, V, 1, 1, 1, 1, 0, 704, 100
44149, V, 1, 1, 1, 1, 0, 704, 100
44150, V, 1, 1, 1, 1, 0, 704, 100
44151, V, 1, 1, 1, 1, 0, 704, 100
44152, V, 1, 1, 1, 1, 0, 704, 100
44153, V, 1, 1, 1, 1, 0, 704, 100
44154, V, 1, 1, 1, 1, 0, 704, 100
44155, V, 1, 1, 1, 1, 0, 704, 100
44156, V, 1, 1, 1, 1, 0, 704, 100
44157, V, 1, 1, 1, 1, 0, 704, 100
44158, V, 1, 1, 1, 1, 0, 704, 100
44160, V, 1, 1, 1, 1, 0, 704, 100
44161, V, 1, 1, 1, 1, 0, 704, 100
44162, V, 1, 1, 1, 1, 0, 704, 100
44163, V, 1, 1, 1, 1, 0, 704, 100
44164, V, 1, 1, 1, 1, 0, 704, 100
44165, V, 1, 1, 1, 1, 0, 704, 100
44166, V, 1, 1, 1, 1, 0, 704, 100
44167, V, 1, 1, 1, 1, 0, 704, 100
44168, V, 1, 1, 1, 1, 0, 704, 100
44169, V, 1, 1, 1, 1, 0, 704, 100
44170, V, 1, 1, 1, 1, 0, 704, 100
44171, V, 1, 1, 1, 1, 0, 704, 100
44172, V, 1, 1, 1, 1, 0, 704, 100
44173, V, 1, 1, 1, 1, 0, 704, 100
44174, V, 1, 1, 1, 1, 0, 704, 100
44175, V, 1, 1, 1, 1, 0, 704, 100
44176, V, 1, 1, 1, 1, 0, 704, 100
44177, V, 1, 1, 1, 1, 0, 704, 100
44178, V, 1, 1, 1, 1, 0, 704, 100
44179, V, 1, 1, 1, 1, 0, 704, 100
44180, V, 1, 1, 1, 1, 0, 704, 100
44181, V, 1, 1, 1, 1, 0, 704, 100
44182, V, 1, 1, 1, 1, 0, 704, 100
44183, V, 1, 1, 1, 1, 0, 704, 100
44184, V, 1, 1, 1, 1, 0, 704, 100
44185, V, 1, 1, 1, 1, 0, 704, 100
44186, V, 1, 1, 1, 1, 0, 704, 100
44187, V, 1, 1, 1, 1, 0, 704, 100
44188, V, 1, 1, 1, 1, 0, 704, 100
44189, V, 1, 1, 1, 1, 0, 704, 100
44190, V, 1, 1, 1, 1, 0, 704, 100
44191, V, 1, 1, 1, 1, 0, 704, 100
44192, V, 1, 1, 1, 1, 0, 704, 100
44193, V, 1, 1, 1, 1, 0, 704, 100
44194, V, 1, 1, 1, 1, 0, 704, 100
44195, V, 1, 1, 1, 1, 0, 704, 100
44196, V, 1, 1, 1, 1, 0, 704, 100
44197, V, 1, 1, 1, 1, 0, 704, 100
44198, V, 1, 1, 1, 1, 0, 704, 100
44199, V, 1, 1, 1, 1, 0, 704, 100
44200, V, 1, 1, 1, 1, 0, 704, 100
44201, V, 1, 1, 1, 1, 0, 704, 100
44203, V, 1, 1, 1, 1, 0, 704, 100
44204, V, 1, 1, 1, 1, 0, 704, 100
44205, V, 1, 1, 1, 1, 0, 704, 100
44206, V, 1, 1, 1, 1, 0, 704, 99
44207, V, 1, 1, 1, 1, 0, 704, 100
44208, V, 1, 1, 1, 1, 0, 704, 100
44209, V, 1, 1, 1, 1, 0, 704, 100
44210, V, 1, 1, 1, 1, 0, 704, 100
44211, V, 1, 1, 1, 1, 0, 704, 100
44212, V, 1, 1, 1, 1, 0, 704, 100
44213, V, 1, 1, 1, 1, 0, 704, 100
44214, V, 1, 1, 1, 1, 0, 704, 100
44215, V, 1, 1, 1, 1, 0, 704, 100
44216, V, 1, 1, 1, 1, 0, 704, 100
44217, V, 1, 1, 1, 1, 0, 704, 100
44218, V, 1, 1, 1, 1, 0, 704, 100
44219, V, 1, 1, 1, 1, 0, 704, 100
44220, V, 1, 1, 1, 1, 0, 704, 100
44221, V, 1, 1, 1, 1, 0, 704, 100
44222, V, 1, 1, 1, 1, 0, 704, 100
44223, V, 1, 1, 1, 1, 0, 704, 100
44224, V, 1, 1, 1, 1, 0, 704, 100
44225, V, 1, 1, 1, 1, 0, 704, 100
44226, V, 1, 1, 1, 1, 0, 704, 100
44227, V, 1, 1, 1, 1, 0, 704, 100
44228, V, 1, 1, 1, 1, 0, 704, 100
44229, V, 1, 1, 1, 1, 0, 704, 100
44230, V, 1, 1, 1, 1, 0, 704, 100
44231, V, 1, 1, 1, 1, 0, 704, 100
44232, V, 1, 1, 1, 1, 0, 704, 100
44233, V, 1, 1, 1, 1, 0, 704, 100
44234, V, 1, 1, 1, 1, 0, 704, 100
44235, V, 1, 1, 1, 1, 0, 704, 100
44236, V, 1, 1, 1, 1, 0, 704, 100
44237, V, 1, 1, 1, 1, 0, 704, 100
44238, V, 1, 1, 1, 1, 0, 704, 100
44239, V, 1, 1, 1, 1, 0, 704, 100
44240, V, 1, 1, 1, 1, 0, 704, 100
44241, V, 1, 1, 1, 1, 0, 704, 100
44242, V, 1, 1, 1, 1, 0, 704, 100
44243, V, 1, 1, 1, 1, 0, 704, 100
44244, V, 1, 1, 1, 1, 0, 704, 100
44246, V, 1, 1, 1, 1, 0, 704, 100
44247, V, 1, 1, 1, 1, 0, 704, 100
44248, V, 1, 1, 1, 1, 0, 704, 100
44249, V, 1, 1, 1, 1, 0, 704, 100
44250, V, 1, 1, 1, 1, 0, 704, 100
44251, V, 1, 1, 1, 1, 0, 704, 100
44252, V, 1, 1, 1, 1, 0, 704, 100
44253, V, 1, 1, 1, 1, 0, 704, 100
44254, V, 1, 1, 1, 1, 0, 704, 100
44255, V, 1, 1, 1, 1, 0, 704, 100
44256, V, 1, 1, 1, 1, 0, 704, 100
44257, V, 1, 1, 1, 1, 0, 704, 100
44258, V, 1, 1, 1, 1, 0, 704, 100
44259, V, 1, 1, 1, 1, 0, 704, 100
44260, V, 1, 1, 1, 1, 0, 704, 100
44261, V, 1, 1, 1, 1, 0, 704, 100
44262, V, 1, 1, 1, 1, 0, 704, 100
44263, V, 1, 1, 1, 1, 0, 704, 100
44264, V, 1, 1, 1, 1, 0, 704, 100
44265, V, 1, 1, 1, 1, 0, 704, 100
44266, V, 1, 1, 1, 1, 0, 704, 100
44267, V, 1, 1, 1, 1, 0, 704, 100
44268, V, 1, 1, 1, 1, 0, 704, 100
44269, V, 1, 1, 1, 1, 0, 704, 100
44270, V, 1, 1, 1, 1, 0, 704, 100
44271, V, 1, 1, 1, 1, 0, 704, 100
44272, V, 1, 1, 1, 1, 0, 704, 100
44273, V, 1, 1, 1, 1, 0, 704, 100
44274, V, 1, 1, 1, 1, 0, 704, 100
44275, V, 1, 1, 1, 1, 0, 704, 100
44276, V, 1, 1, 1, 1, 0, 704, 100
44277, V, 1, 1, 1, 1, 0, 704, 100
44278, V, 1, 1, 1, 1, 0, 704, 100
44279, V, 1, 1, 1, 1, 0, 704, 100
44280, V, 1, 1, 1, 1, 0, 704, 100
44281, V, 1, 1, 1, 1, 0, 704, 100
44282, V, 1, 1, 1, 1, 0, 704, 100
44283, V, 1, 1, 1, 1, 0, 704, 100
44284, V, 1, 1, 1, 1, 0, 704, 100
44285, V, 1, 1, 1, 1, 0, 704, 100
44286, V, 1, 1, 1, 1, 0, 704, 100
44288, V, 1, 1, 1, 1, 0, 704, 100
44289, V, 1, 1, 1, 1, 0, 704, 100
44290, V, 1, 1, 1, 1, 0, 704, 100
44291, V, 1, 1, 1, 1, 0, 704, 100
44292, V, 1, 1, 1, 1, 0, 704, 100
44293, V, 1, 1, 1, 1, 0, 704, 100
44294, V, 1, 1, 1, 1, 0, 704, 100
44295, V, 1, 1, 1, 1, 0, 704, 100
44296, V, 1, 1, 1, 1, 0, 704, 100
44297, V, 1, 1, 1, 1, 0, 704, 100
44298, V, 1, 1, 1, 1, 0, 704, 100
44299, V, 1, 1, 1, 1, 0, 704, 100
44300, V, 1, 1, 1, 1, 0, 704, 100
44301, V, 1, 1, 1, 1, 0, 704, 100
44302, V, 1, 1, 1, 1, 0, 704, 100
44303, V, 1, 1, 1, 1, 0, 704, 100
44304, V, 1, 1, 1, 1, 0, 704, 100
44305, V, 1, 1, 1, 1, 0, 704, 100
44306, V, 1, 1, 1, 1, 0, 704, 100
44307, V, 1, 1, 1, 1, 0, 704, 100
44308, V, 1, 1, 1, 1, 0, 704, 100
44309, V, 1, 1, 1, 1, 0, 704, 100
44310, V, 1, 1, 1, 1, 0, 704, 100
44311, V, 1, 1, 1, 1, 0, 704, 100
44312, V, 1, 1, 1, 1, 0, 704, 100
44313, V, 1, 1, 1, 1, 0, 704, 100
44314, V, 1, 1, 1, 1, 0, 704, 100
44315, V, 1, 1, 1, 1, 0, 704, 100
44316, V, 1, 1, 1, 1, 0, 704, 100
44317, V, 1, 1, 1, 1, 0, 704, 100
44318, V, 1, 1, 1, 1, 0, 704, 100
44319, V, 1, 1, 1, 1, 0, 704, 100
44320, V, 1, 1, 1, 1, 0, 704, 100
44321, V, 1, 1, 1, 1, 0, 704, 100
44322, V, 1, 1, 1, 1, 0, 704, 100
44323, V, 1, 1, 1, 1, 0, 704, 100
44324, V, 1, 1, 1, 1, 0, 704, 100
44325, V, 1, 1, 1, 1, 0, 704, 100
44326, V, 1, 1, 1, 1, 0, 704, 100
44327, V, 1, 1, 1, 1, 0, 704, 100
44328, V, 1, 1, 1, 1, 0, 704, 100
44329, V, 1, 1, 1, 1, 0, 704, 100
44331, V, 1, 1, 1, 1, 0, 704, 100
44332, V, 1, 1, 1, 1, 0, 704, 100
44333, V, 1, 1, 1, 1, 0, 704, 100
44334, V, 1, 1, 1, 1, 0, 704, 100
44335, V, 1, 1, 1, 1, 0, 704, 100
44336, V, 1, 1, 1, 1, 0, 704, 100
44337, V, 1, 1, 1, 1, 0, 704, 100
44338, V, 1, 1, 1, 1, 0, 704, 100
44339, V, 1, 1, 1, 1, 0, 704, 100
44340, V, 1, 1, 1, 1, 0, 704, 100
44341, V, 1, 1, 1, 1, 0, 704, 100
44342, V, 1, 1, 1, 1, 0, 704, 100
44343, V, 1, 1, 1, 1, 0, 704, 100
44344, V, 1, 1, 1, 1, 0, 704, 100
44345, V, 1, 1, 1, 1, 0, 704, 100
44346, V, 1, 1, 1, 1, 0, 704, 100
44347, V, 1, 1, 1, 1, 0, 704, 100
44348, V, 1, 1, 1, 1, 0, 704, 100
44349, V, 1, 1, 1, 1, 0, 704, 100
44350, V, 1, 1, 1, 1, 0, 704, 100
44351, V, 1, 1, 1, 1, 0, 704, 100
44352, V, 1, 1, 1, 1, 0, 704, 100
44353, V, 1, 1, 1, 1, 0, 704, 100
44354, V, 1, 1, 1, 1, 0, 704, 100
44355, V, 1, 1, 1, 1, 0, 704, 99
44356, V, 1, 1, 1, 1, 0, 704, 100
44357, V, 1, 1, 1, 1, 0, 704, 100
44358, V, 1, 1, 1, 1, 0, 704, 100
44359, V, 1, 1, 1, 1, 0, 704, 100
44360, V, 1, 1, 1, 1, 0, 704, 100
44361, V, 1, 1, 1, 1, 0, 704, 100
44362, V, 1, 1, 1, 1, 0, 704, 100
44363, V, 1, 1, 1, 1, 0, 704, 100
44364, V, 1, 1, 1, 1, 0, 704, 100
44365, V, 1, 1, 1, 1, 0, 704, 100
44366, V, 1, 1, 1, 1, 0, 704, 100
44367, V, 1, 1, 1, 1, 0, 704, 100
44368, V, 1, 1, 1, 1, 0, 704, 100
44369, V, 1, 1, 1, 1, 0, 704, 100
44370, V, 1, 1, 1, 1, 0, 704, 100
44371, V, 1, 1, 1, 1, 0, 704, 100
44372, V, 1, 1, 1, 1, 0, 704, 100
44374, V, 1, 1, 1, 1, 0, 704, 100
44375, V, 1, 1, 1, 1, 0, 704, 100
44376, V, 1, 1, 1, 1, 0, 704, 100
44377, V, 1, 1, 1, 1, 0, 704, 100
44378, V, 1, 1, 1, 1, 0, 704, 100
44379, V, 1, 1, 1, 1, 0, 704, 100
44380, V, 1, 1, 1, 1, 0, 704, 100
44381, V, 1, 1, 1, 1, 0, 704, 100
44382, V, 1, 1, 1, 1, 0, 704, 100
44383, V, 1, 1, 1, 1, 0, 704, 100
44384, V, 1, 1, 1, 1, 0, 704, 100
44385, V, 1, 1, 1, 1, 0, 704, 100
44386, V, 1, 1, 1, 1, 0, 704, 100
44387, V, 1, 1, 1, 1, 0, 704, 100
44388, V, 1, 1, 1, 1, 0, 704, 100
44389, V, 1, 1, 1, 1, 0, 704, 100
44390, V, 1, 1, 1, 1, 0, 704, 100
44391, V, 1, 1, 1, 1, 0, 704, 100
44392, V, 1, 1, 1, 1, 0, 704, 100
44393, V, 1, 1, 1, 1, 0, 704, 100
44394, V, 1, 1, 1, 1, 0, 704, 100
44395, V, 1, 1, 1, 1, 0, 704, 100
44396, V, 1, 1, 1, 1, 0, 704, 100
44397, V, 1, 1, 1, 1, 0, 704, 100
44398, V, 1, 1, 1, 1, 0, 704, 100
44399, V, 1, 1, 1, 1, 0, 704, 100
44400, V, 1, 1, 1, 1, 0, 704, 100
44401, V, 1, 1, 1, 1, 0, 704, 100
44402, V, 1, 1, 1, 1, 0, 704, 100
44403, V, 1, 1, 1, 1, 0, 704, 99
44404, V, 1, 1, 1, 1, 0, 704, 100
44405, V, 1, 1, 1, 1, 0, 704, 100
44406, V, 1, 1, 1, 1, 0, 704, 100
44407, V, 1, 1, 1, 1, 0, 704, 100
44408, V, 1, 1, 1, 1, 0, 704, 100
44409, V, 1, 1, 1, 1, 0, 704, 100
44410, V, 1, 1, 1, 1, 0, 704, 100
44411, V, 1, 1, 1, 1, 0, 704, 100
44412, V, 1, 1, 1, 1, 0, 704, 100
44413, V, 1, 1, 1, 1, 0, 704, 100
44414, V, 1, 1, 1, 1, 0, 704, 100
44416, V, 1, 1, 1, 1, 0, 704, 100
44417, V, 1, 1, 1, 1, 0, 704, 100
44418, V, 1, 1, 1, 1, 0, 704, 100
44419, V, 1, 1, 1, 1, 0, 704, 100
44420, V, 1, 1, 1, 1, 0, 704, 100
44421, V, 1, 1, 1, 1, 0, 704, 100
44422, V, 1, 1, 1, 1, 0, 704, 100
44423, V, 1, 1, 1, 1, 0, 704, 100
44424, V, 1, 1, 1, 1, 0, 704, 100
44425, V, 1, 1, 1, 1, 0, 704, 100
44426, V, 1, 1, 1, 1, 0, 704, 100
44427, V, 1, 1, 1, 1, 0, 704, 100
44428, V, 1, 1, 1, 1, 0, 704, 100
44429, V, 1, 1, 1, 1, 0, 704, 100
44430, V, 1, 1, 1, 1, 0, 704, 100
44431, V, 1, 1, 1, 1, 0, 704, 100
44432, V, 1, 1, 1, 1, 0, 704, 100
44433, V, 1, 1, 1, 1, 0, 704, 100
44434, V, 1, 1, 1, 1, 0, 704, 100
44435, V, 1, 1, 1, 1, 0, 704, 100
44436, V, 1, 1, 1, 1, 0, 704, 100
44437, V, 1, 1, 1, 1, 0, 704, 100
44438, V, 1, 1, 1, 1, 0, 704, 100
44439, V, 1, 1, 1, 1, 0, 704, 100
44440, V, 1, 1, 1, 1, 0, 704, 100
44441, V, 1, 1, 1, 1, 0, 704, 100
44442, V, 1, 1, 1, 1, 0, 704, 100
44443, V, 1, 1, 1, 1, 0, 704, 100
44444, V, 1, 1, 1, 1, 0, 704, 100
44445, V, 1, 1, 1, 1, 0, 704, 100
44446, V, 1, 1, 1, 1, 0, 704, 100
44447, V, 1, 1, 1, 1, 0, 704, 100
44448, V, 1, 1, 1, 1, 0, 704, 100
44449, V, 1, 1, 1, 1, 0, 704, 100
44450, V, 1, 1, 1, 1, 0, 704, 100
44451, V, 1, 1, 1, 1, 0, 704, 100
44452, V, 1, 1, 1, 1, 0, 704, 100
44453, V, 1, 1, 1, 1, 0, 704, 100
44454, V, 1, 1, 1, 1, 0, 704, 100
44455, V, 1, 1, 1, 1, 0, 704, 100
44456, V, 1, 1, 1, 1, 0, 704, 100
44457, V, 1, 1, 1, 1, 0, 704, 100
44459, V, 1, 1, 1, 1, 0, 704, 100
44460, V, 1, 1, 1, 1, 0, 704, 100
44461, V, 1, 1, 1, 1, 0, 704, 100
44462, V, 1, 1, 1, 1, 0, 704, 100
44463, V, 1, 1, 1, 1, 0, 704, 100
44464, V, 1, 1, 1, 1, 0, 704, 100
44465, V, 1, 1, 1, 1, 0, 704, 100
44466, V, 1, 1, 1, 1, 0, 704, 100
44467, V, 1, 1, 1, 1, 0, 704, 100
44468, V, 1, 1, 1, 1, 0, 704, 100
44469, V, 1, 1, 1, 1, 0, 704, 100
44470, V, 1, 1, 1, 1, 0, 704, 100
44471, V, 1, 1, 1, 1, 0, 704, 100
44472, V, 1, 1, 1, 1, 0, 704, 100
44473, V, 1, 1, 1, 1, 0, 704, 100
44474, V, 1, 1, 1, 1, 0, 704, 100
44475, V, 1, 1, 1, 1, 0, 704, 100
44476, V, 1, 1, 1, 1, 0, 704, 100
44477, V, 1, 1, 1, 1, 0, 704, 100
44478, V, 1, 1, 1, 1, 0, 704, 100
44479, V, 1, 1, 1, 1, 0, 704, 100
44480, V, 1, 1, 1, 1, 0, 704, 100
44481, V, 1, 1, 1, 1, 0, 704, 100
44482, V, 1, 1, 1, 1, 0, 704, 100
44483, V, 1, 1, 1, 1, 0, 704, 100
44484, V, 1, 1, 1, 1, 0, 704, 100
44485, V, 1, 1, 1, 1, 0, 704, 100
44486, V, 1, 1, 1, 1, 0, 704, 100
44487, V, 1, 1, 1, 1, 0, 704, 100
44488, V, 1, 1, 1, 1, 0, 704, 100
44489, V, 1, 1, 1, 1, 0, 704, 100
44490, V, 1, 1, 1, 1, 0, 704, 100
44491, V, 1, 1, 1, 1, 0, 704, 100
44492, V, 1, 1, 1, 1, 0, 704, 100
44493, V, 1, 1, 1, 1, 0, 704, 100
44494, V, 1, 1, 1, 1, 0, 704, 100
44495, V, 1, 1, 1, 1, 0, 704, 100
44496, V, 1, 1, 1, 1, 0, 704, 100
44497, V, 1, 1, 1, 1, 0, 704, 100
44498, V, 1, 1, 1, 1, 0, 704, 100
44499, V, 1, 1, 1, 1, 0, 704, 100
44500, V, 1, 1, 1, 1, 0, 704, 100
44502, V, 1, 1, 1, 1, 0, 704, 100
44503, V, 1, 1, 1, 1, 0, 704, 100
44504, V, 1, 1, 1, 1, 0, 704, 100
44505, V, 1, 1, 1, 1, 0, 704, 100
44506, V, 1, 1, 1, 1, 0, 704, 100
44507, V, 1, 1, 1, 1, 0, 704, 100
44508, V, 1, 1, 1, 1, 0, 704, 100
44509, V, 1, 1, 1, 1, 0, 704, 100
44510, V, 1, 1, 1, 1, 0, 704, 100
44511, V, 1, 1, 1, 1, 0, 704, 100
44512, V, 1, 1, 1, 1, 0, 704, 100
44513, V, 1, 1, 1, 1, 0, 704, 100
44514, V, 1, 1, 1, 1, 0, 704, 100
44515, V, 1, 1, 1, 1, 0, 704, 100
44516, V, 1, 1, 1, 1, 0, 704, 100
44517, V, 1, 1, 1, 1, 0, 704, 100
44518, V, 1, 1, 1, 1, 0, 704, 100
44519, V, 1, 1, 1, 1, 0, 704, 100
44520, V, 1, 1, 1, 1, 0, 704, 100
44521, V, 1, 1, 1, 1, 0, 704, 100
44522, V, 1, 1, 1, 1, 0, 704, 100
44523, V, 1, 1, 1, 1, 0, 704, 100
44524, V, 1, 1, 1, 1, 0, 704, 100
44525, V, 1, 1, 1, 1, 0, 704, 100
44526, V, 1, 1, 1, 1, 0, 704, 100
44527, V, 1, 1, 1, 1, 0, 704, 100
44528, V, 1, 1, 1, 1, 0, 704, 100
44529, V, 1, 1, 1, 1, 0, 704, 100
44530, V, 1, 1, 1, 1, 0, 704, 100
44531, V, 1, 1, 1, 1, 0, 704, 100
44532, V, 1, 1, 1, 1, 0, 704, 100
44533, V, 1, 1, 1, 1, 0, 704, 100
44534, V, 1, 1, 1, 1, 0, 704, 100
44535, V, 1, 1, 1, 1, 0, 704, 100
44536, V, 1, 1, 1, 1, 0, 704, 100
44537, V, 1, 1, 1, 1, 0, 704, 100
44538, V, 1, 1, 1, 1, 0, 704, 100
44539, V, 1, 1, 1, 1, 0, 704, 100
44540, V, 1, 1, 1, 1, 0, 704, 100
44541, V, 1, 1, 1, 1, 0, 704, 100
44542, V, 1, 1, 1, 1, 0, 704, 100
44544, V, 1, 1, 1, 1, 0, 704, 100
44545, V, 1, 1, 1, 1, 0, 704, 100
44546, V, 1, 1, 1, 1, 0, 704, 100
44547, V, 1, 1, 1, 1, 0, 704, 100
44548, V, 1, 1, 1, 1, 0, 704, 100
44549, V, 1, 1, 1, 1, 0, 704, 100
44550, V, 1, 1, 1, 1, 0, 704, 100
44551, V, 1, 1, 1, 1, 0, 704, 100
44552, V, 1, 1, 1, 1, 0, 704, 100
44553, V, 1, 1, 1, 1, 0, 704, 100
44554, V, 1, 1, 1, 1, 0, 704, 100
44555, V, 1, 1, 1, 1, 0, 704, 100
44556, V, 1, 1, 1, 1, 0, 704, 100
44557, V, 1, 1, 1, 1, 0, 704, 100
44558, V, 1, 1, 1, 1, 0, 704, 100
44559, V, 1, 1, 1, 1, 0, 704, 100
44560, V, 1, 1, 1, 1, 0, 704, 100
44561, V, 1, 1, 1, 1, 0, 704, 100
44562, V, 1, 1, 1, 1, 0, 704, 100
44563, V, 1, 1, 1, 1, 0, 704, 100
44564, V, 1, 1, 1, 1, 0, 704, 100
44565, V, 1, 1, 1, 1, 0, 704, 100
44566, V, 1, 1, 1, 1, 0, 704, 100
44567, V, 1, 1, 1, 1, 0, 704, 100
44568, V, 1, 1, 1, 1, 0, 704, 100
44569, V, 1, 1, 1, 1, 0, 704, 100
44570, V, 1, 1, 1, 1, 0, 704, 100
44571, V, 1, 1, 1, 1, 0, 704, 100
44572, V, 1, 1, 1, 1, 0, 704, 100
44573, V, 1, 1, 1, 1, 0, 704, 100
44574, V, 1, 1, 1, 1, 0, 704, 100
44575, V, 1, 1, 1, 1, 0, 704, 100
44576, V, 1, 1, 1, 1, 0, 704, 100
44577, V, 1, 1, 1, 1, 0, 704, 100
44578, V, 1, 1, 1, 1, 0, 704, 100
44579, V, 1, 1, 1, 1, 0, 704, 100
44580, V, 1, 1, 1, 1, 0, 704, 100
44581, V, 1, 1, 1, 1, 0, 704, 100
44582, V, 1, 1, 1, 1, 0, 704, 100
44583, V, 1, 1, 1, 1, 0, 704, 100
44584, V, 1, 1, 1, 1, 0, 704, 100
44585, V, 1, 1, 1, 1, 0, 704, 100
44587, V, 1, 1, 1, 1, 0, 704, 100
44588, V, 1, 1, 1, 1, 0, 704, 100
44589, V, 1, 1, 1, 1, 0, 704, 100
44590, V, 1, 1, 1, 1, 0, 704, 100
44591, V, 1, 1, 1, 1, 0, 704, 100
44592, V, 1, 1, 1, 1, 0, 704, 100
44593, V, 1, 1, 1, 1, 0, 704, 100
44594, V, 1, 1, 1, 1, 0, 704, 100
44595, V, 1, 1, 1, 1, 0, 704, 100
44596, V, 1, 1, 1, 1, 0, 704, 100
44597, V, 1, 1, 1, 1, 0, 704, 100
44598, V, 1, 1, 1, 1, 0, 704, 100
44599, V, 1, 1, 1, 1, 0, 704, 100
44600, V, 1, 1, 1, 1, 0, 704, 100
44601, V, 1, 1, 1, 1, 0, 704, 100
44602, V, 1, 1, 1, 1, 0, 704, 100
44603, V, 1, 1, 1, 1, 0, 704, 100
44604, V, 1, 1, 1, 1, 0, 704, 100
44605, V, 1, 1, 1, 1, 0, 704, 100
44606, V, 1, 1, 1, 1, 0, 704, 100
44607, V, 1, 1, 1, 1, 0, 704, 100
44608, V, 1, 1, 1, 1, 0, 704, 100
44609, V, 1, 1, 1, 1, 0, 704, 100
44610, V, 1, 1, 1, 1, 0, 704, 100
44611, V, 1, 1, 1, 1, 0, 704, 100
44612, V, 1, 1, 1, 1, 0, 704, 100
44613, V, 1, 1, 1, 1, 0, 704, 100
44614, V, 1, 1, 1, 1, 0, 704, 100
44615, V, 1, 1, 1, 1, 0, 704, 100
44616, V, 1, 1, 1, 1, 0, 704, 100
44617, V, 1, 1, 1, 1, 0, 704, 100
44618, V, 1, 1, 1, 1, 0, 704, 100
44619, V, 1, 1, 1, 1, 0, 704, 100
44620, V, 1, 1, 1, 1, 0, 704, 100
44621, V, 1, 1, 1, 1, 0, 704, 100
44622, V, 1, 1, 1, 1, 0, 704, 100
44623, V, 1, 1, 1, 1, 0, 704, 100
44624, V, 1, 1, 1, 1, 0, 704, 100
44625, V, 1, 1, 1, 1, 0, 704, 100
44626, V, 1, 1, 1, 1, 0, 704, 100
44627, V, 1, 1, 1, 1, 0, 704, 100
44628, V, 1, 1, 1, 1, 0, 704, 100
44630, V, 1, 1, 1, 1, 0, 704, 100
44631, V, 1, 1, 1, 1, 0, 704, 100
44632, V, 1, 1, 1, 1, 0, 704, 100
44633, V, 1, 1, 1, 1, 0, 704, 100
44634, V, 1, 1, 1, 1, 0, 704, 100
44635, V, 1, 1, 1, 1, 0, 704, 100
44636, V, 1, 1, 1, 1, 0, 704, 100
44637, V, 1, 1, 1, 1, 0, 704, 100
44638, V, 1, 1, 1, 1, 0, 704, 100
44639, V, 1, 1, 1, 1, 0, 704, 100
44640, V, 1, 1, 1, 1, 0, 704, 100
44641, V, 1, 1, 1, 1, 0, 704, 100
44642, V, 1, 1, 1, 1, 0, 704, 100
44643, V, 1, 1, 1, 1, 0, 704, 100
44644, V, 1, 1, 1, 1, 0, 704, 100
44645, V, 1, 1, 1, 1, 0, 704, 100
44646, V, 1, 1, 1, 1, 0, 704, 100
44647, V, 1, 1, 1, 1, 0, 704, 100
44648, V, 1, 1, 1, 1, 0, 704, 100
44649, V, 1, 1, 1, 1, 0, 704, 100
44650, V, 1, 1, 1, 1, 0, 704, 100
44651, V, 1, 1, 1, 1, 0, 704, 100
44652, V, 1, 1, 1, 1, 0, 704, 100
44653, V, 1, 1, 1, 1, 0, 704, 100
44654, V, 1, 1, 1, 1, 0, 704, 100
44655, V, 1, 1, 1, 1, 0, 704, 100
44656, V, 1, 1, 1, 1, 0, 704, 100
44657, V, 1, 1, 1, 1, 0, 704, 100
44658, V, 1, 1, 1, 1, 0, 704, 100
44659, V, 1, 1, 1, 1, 0, 704, 100
44660, V, 1, 1, 1, 1, 0, 704, 100
44661, V, 1, 1, 1, 1, 0, 704, 100
44662, V, 1, 1, 1, 1, 0, 704, 100
44663, V, 1, 1, 1, 1, 0, 704, 100
44664, V, 1, 1, 1, 1, 0, 704, 100
44665, V, 1, 1, 1, 1, 0, 704, 100
44666, V, 1, 1, 1, 1, 0, 704, 100
44667, V, 1, 1, 1, 1, 0, 704, 100
44668, V, 1, 1, 1, 1, 0, 704, 100
44669, V, 1, 1, 1, 1, 0, 704, 100
44670, V, 1, 1, 1, 1, 0, 704, 100
44672, V, 1, 1, 1, 1, 0, 704, 100
44673, V, 1, 1, 1, 1, 0, 704, 100
44674, V, 1, 1, 1, 1, 0, 704, 100
44675, V, 1, 1, 1, 1, 0, 704, 100
44676, V, 1, 1, 1, 1, 0, 704, 100
44677, V, 1, 1, 1, 1, 0, 704, 100
44678, V, 1, 1, 1, 1, 0, 704, 100
44679, V, 1, 1, 1, 1, 0, 704, 100
44680, V, 1, 1, 1, 1, 0, 704, 100
44681, V, 1, 1, 1, 1, 0, 704, 100
44682, V, 1, 1, 1, 1, 0, 704, 100
44683, V, 1, 1, 1, 1, 0, 704, 100
44684, V, 1, 1, 1, 1, 0, 704, 100
44685, V, 1, 1, 1, 1, 0, 704, 100
44686, V, 1, 1, 1, 1, 0, 704, 100
44687, V, 1, 1, 1, 1, 0, 704, 100
44688, V, 1, 1, 1, 1, 0, 704, 100
44689, V, 1, 1, 1, 1, 0, 704, 100
44690, V, 1, 1, 1, 1, 0, 704, 100
44691, V, 1, 1, 1, 1, 0, 704, 100
44692, V, 1, 1, 1, 1, 0, 704, 100
44693, V, 1, 1, 1, 1, 0, 704, 100
44694, V, 1, 1, 1, 1, 0, 704, 100
44695, V, 1, 1, 1, 1, 0, 704, 100
44696, V, 1, 1, 1, 1, 0, 704, 100
44697, V, 1, 1, 1, 1, 0, 704, 100
44698, V, 1, 1, 1, 1, 0, 704, 100
44699, V, 1, 1, 1, 1, 0, 704, 100
44700, V, 1, 1, 1, 1, 0, 704, 100
44701, V, 1, 1, 1, 1, 0, 704, 100
44702, V, 1, 1, 1, 1, 0, 704, 100
44703, V, 1, 1, 1, 1, 0, 704, 100
44704, V, 1, 1, 1, 1, 0, 704, 100
44705, V, 1, 1, 1, 1, 0, 704, 100
44706, V, 1, 1, 1, 1, 0, 704, 100
44707, V, 1, 1, 1, 1, 0, 704, 100
44708, V, 1, 1, 1, 1, 0, 704, 100
44709, V, 1, 1, 1, 1, 0, 704, 100
44710, V, 1, 1, 1, 1, 0, 704, 100
44711, V, 1, 1, 1, 1, 0, 704, 100
44712, V, 1, 1, 1, 1, 0, 704, 100
44713, V, 1, 1, 1, 1, 0, 704, 100
44715, V, 1, 1, 1, 1, 0, 704, 100
44716, V, 1, 1, 1, 1, 0, 704, 100
44717, V, 1, 1, 1, 1, 0, 704, 100
44718, V, 1, 1, 1, 1, 0, 704, 100
44719, V, 1, 1, 1, 1, 0, 704, 100
44720, V, 1, 1, 1, 1, 0, 704, 100
44721, V, 1, 1, 1, 1, 0, 704, 100
44722, V, 1, 1, 1, 1, 0, 704, 100
44723, V, 1, 1, 1, 1, 0, 704, 100
44724, V, 1, 1, 1, 1, 0, 704, 100
44725, V, 1, 1, 1, 1, 0, 704, 100
44726, V, 1, 1, 1, 1, 0, 704, 100
44727, V, 1, 1, 1, 1, 0, 704, 100
44728, V, 1, 1, 1, 1, 0, 704, 100
44729, V, 1, 1, 1, 1, 0, 704, 100
44730, V, 1, 1, 1, 1, 0, 704, 100
44731, V, 1, 1, 1, 1, 0, 704, 100
44732, V, 1, 1, 1, 1, 0, 704, 100
44733, V, 1, 1, 1, 1, 0, 704, 100
44734, V, 1, 1, 1, 1, 0, 704, 100
44735, V, 1, 1, 1, 1, 0, 704, 100
44736, V, 1, 1, 1, 1, 0, 704, 100
44737, V, 1, 1, 1, 1, 0, 704, 100
44738, V, 1, 1, 1, 1, 0, 704, 100
44739, V, 1, 1, 1, 1, 0, 704, 100
44740, V, 1, 1, 1, 1, 0, 704, 100
44741, V, 1, 1, 1, 1, 0, 704, 100
44742, V, 1, 1, 1, 1, 0, 704, 100
44743, V, 1, 1, 1, 1, 0, 704, 100
44744, V, 1, 1, 1, 1, 0, 704, 100
44745, V, 1, 1, 1, 1, 0, 704, 100
44746, V, 1, 1, 1, 1, 0, 704, 100
44747, V, 1, 1, 1, 1, 0, 704, 100
44748, V, 1, 1, 1, 1, 0, 704, 100
44749, V, 1, 1, 1, 1, 0, 704, 100
44750, V, 1, 1, 1, 1, 0, 704, 100
44751, V, 1, 1, 1, 1, 0, 704, 100
44752, V, 1, 1, 1, 1, 0, 704, 100
44753, V, 1, 1, 1, 1, 0, 704, 100
44754, V, 1, 1, 1, 1, 0, 704, 100
44755, V, 1, 1, 1, 1, 0, 704, 100
44756, V, 1, 1, 1, 1, 0, 704, 100
44758, V, 1, 1, 1, 1, 0, 704, 100
44759, V, 1, 1, 1, 1, 0, 704, 100
44760, V, 1, 1, 1, 1, 0, 704, 100
44761, V, 1, 1, 1, 1, 0, 704, 100
44762, V, 1, 1, 1, 1, 0, 704, 100
44763, V, 1, 1, 1, 1, 0, 704, 100
44764, V, 1, 1, 1, 1, 0, 704, 100
44765, V, 1, 1, 1, 1, 0, 704, 100
44766, V, 1, 1, 1, 1, 0, 704, 100
44767, V, 1, 1, 1, 1, 0, 704, 100
44768, V, 1, 1, 1, 1, 0, 704, 100
44769, V, 1, 1, 1, 1, 0, 704, 100
44770, V, 1, 1, 1, 1, 0, 704, 100
44771, V, 1, 1, 1, 1, 0, 704, 100
44772, V, 1, 1, 1, 1, 0, 704, 100
44773, V, 1, 1, 1, 1, 0, 704, 100
44774, V, 1, 1, 1, 1, 0, 704, 100
44775, V, 1, 1, 1, 1, 0, 704, 100
44776, V, 1, 1, 1, 1, 0, 704, 100
44777, V, 1, 1, 1, 1, 0, 704, 100
44778, V, 1, 1, 1, 1, 0, 704, 100
44779, V, 1, 1, 1, 1, 0, 704, 100
44780, V, 1, 1, 1, 1, 0, 704, 100
44781, V, 1, 1, 1, 1, 0, 704, 100
44782, V, 1, 1, 1, 1, 0, 704, 100
44783, V, 1, 1, 1, 1, 0, 704, 100
44784, V, 1, 1, 1, 1, 0, 704, 100
44785, V, 1, 1, 1, 1, 0, 704, 100
44786, V, 1, 1, 1, 1, 0, 704, 100
44787, V, 1, 1, 1, 1, 0, 704, 100
44788, V, 1, 1, 1, 1, 0, 704, 100
44789, V, 1, 1, 1, 1, 0, 704, 100
44790, V, 1, 1, 1, 1, 0, 704, 100
44791, V, 1, 1, 1, 1, 0, 704, 100
44792, V, 1, 1, 1, 1, 0, 704, 100
44793, V, 1, 1, 1, 1, 0, 704, 100
44794, V, 1, 1, 1, 1, 0, 704, 100
44795, V, 1, 1, 1, 1, 0, 704, 99
44796, V, 1, 1, 1, 1, 0, 704, 100
44797, V, 1, 1, 1, 1, 0, 704, 100
44798, V, 1, 1, 1, 1, 0, 704, 99
44800, V, 1, 1, 1, 1, 0, 704, 99
44801, V, 1, 1, 1, 1, 0, 704, 100
44802, V, 1, 1, 1, 1, 0, 704, 100
44803, V, 1, 1, 1, 1, 0, 704, 100
44804, V, 1, 1, 1, 1, 0, 704, 100
44805, V, 1, 1, 1, 1, 0, 704, 100
44806, V, 1, 1, 1, 1, 0, 704, 100
44807, V, 1, 1, 1, 1, 0, 704, 100
44808, V, 1, 1, 1, 1, 0, 704, 100
44809, V, 1, 1, 1, 1, 0, 704, 100
44810, V, 1, 1, 1, 1, 0, 704, 100
44811, V, 1, 1, 1, 1, 0, 704, 100
44812, V, 1, 1, 1, 1, 0, 704, 100
44813, V, 1, 1, 1, 1, 0, 704, 100
44814, V, 1, 1, 1, 1, 0, 704, 100
44815, V, 1, 1, 1, 1, 0, 704, 100
44816, V, 1, 1, 1, 1, 0, 704, 100
44817, V, 1, 1, 1, 1, 0, 704, 100
44818, V, 1, 1, 1, 1, 0, 704, 100
44819, V, 1, 1, 1, 1, 0, 704, 100
44820, V, 1, 1, 1, 1, 0, 704, 100
44821, V, 1, 1, 1, 1, 0, 704, 100
44822, V, 1, 1, 1, 1, 0, 704, 100
44823, V, 1, 1, 1, 1, 0, 704, 100
44824, V, 1, 1, 1, 1, 0, 704, 100
44825, V, 1, 1, 1, 1, 0, 704, 100
44826, V, 1, 1, 1, 1, 0, 704, 100
44827, V, 1, 1, 1, 1, 0, 704, 100
44828, V, 1, 1, 1, 1, 0, 704, 100
44829, V, 1, 1, 1, 1, 0, 704, 100
44830, V, 1, 1, 1, 1, 0, 704, 100
44831, V, 1, 1, 1, 1, 0, 704, 100
44832, V, 1, 1, 1, 1, 0, 704, 100
44833, V, 1, 1, 1, 1, 0, 704, 100
44834, V, 1, 1, 1, 1, 0, 704, 100
44835, V, 1, 1, 1, 1, 0, 704, 100
44836, V, 1, 1, 1, 1, 0, 704, 100
44837, V, 1, 1, 1, 1, 0, 704, 100
44838, V, 1, 1, 1, 1, 0, 704, 100
44839, V, 1, 1, 1, 1, 0, 704, 100
44840, V, 1, 1, 1, 1, 0, 704, 100
44841, V, 1, 1, 1, 1, 0, 704, 100
44843, V, 1, 1, 1, 1, 0, 704, 100
44844, V, 1, 1, 1, 1, 0, 704, 100
44845, V, 1, 1, 1, 1, 0, 704, 100
44846, V, 1, 1, 1, 1, 0, 704, 100
44847, V, 1, 1, 1, 1, 0, 704, 100
44848, V, 1, 1, 1, 1, 0, 704, 100
44849, V, 1, 1, 1, 1, 0, 704, 100
44850, V, 1, 1, 1, 1, 0, 704, 100
44851, V, 1, 1, 1, 1, 0, 704, 100
44852, V, 1, 1, 1, 1, 0, 704, 100
44853, V, 1, 1, 1, 1, 0, 704, 100
44854, V, 1, 1, 1, 1, 0, 704, 100
44855, V, 1, 1, 1, 1, 0, 704, 100
44856, V, 1, 1, 1, 1, 0, 704, 100
44857, V, 1, 1, 1, 1, 0, 704, 100
44858, V, 1, 1, 1, 1, 0, 704, 100
44859, V, 1, 1, 1, 1, 0, 704, 100
44860, V, 1, 1, 1, 1, 0, 704, 100
44861, V, 1, 1, 1, 1, 0, 704, 100
44862, V, 1, 1, 1, 1, 0, 704, 100
44863, V, 1, 1, 1, 1, 0, 704, 100
44864, V, 1, 1, 1, 1, 0, 704, 100
44865, V, 1, 1, 1, 1, 0, 704, 100
44866, V, 1, 1, 1, 1, 0, 704, 100
44867, V, 1, 1, 1, 1, 0, 704, 100
44868, V, 1, 1, 1, 1, 0, 704, 100
44869, V, 1, 1, 1, 1, 0, 704, 100
44870, V, 1, 1, 1, 1, 0, 704, 100
44871, V, 1, 1, 1, 1, 0, 704, 100
44872, V, 1, 1, 1, 1, 0, 704, 100
44873, V, 1, 1, 1, 1, 0, 704, 100
44874, V, 1, 1, 1, 1, 0, 704, 100
44875, V, 1, 1, 1, 1, 0, 704, 100
44876, V, 1, 1, 1, 1, 0, 704, 100
44877, V, 1, 1, 1, 1, 0, 704, 100
44878, V, 1, 1, 1, 1, 0, 704, 100
44879, V, 1, 1, 1, 1, 0, 704, 100
44880, V, 1, 1, 1, 1, 0, 704, 100
44881, V, 1, 1, 1, 1, 0, 704, 100
44882, V, 1, 1, 1, 1, 0, 704, 100
44883, V, 1, 1, 1, 1, 0, 704, 100
44884, V, 1, 1, 1, 1, 0, 704, 100
44886, V, 1, 1, 1, 1, 0, 704, 100
44887, V, 1, 1, 1, 1, 0, 704, 100
44888, V, 1, 1, 1, 1, 0, 704, 100
44889, V, 1, 1, 1, 1, 0, 704, 100
44890, V, 1, 1, 1, 1, 0, 704, 100
44891, V, 1, 1, 1, 1, 0, 704, 100
44892, V, 1, 1, 1, 1, 0, 704, 100
44893, V, 1, 1, 1, 1, 0, 704, 100
44894, V, 1, 1, 1, 1, 0, 704, 100
44895, V, 1, 1, 1, 1, 0, 704, 100
44896, V, 1, 1, 1, 1, 0, 704, 100
44897, V, 1, 1, 1, 1, 0, 704, 100
44898, V, 1, 1, 1, 1, 0, 704, 100
44899, V, 1, 1, 1, 1, 0, 704, 100
44900, V, 1, 1, 1, 1, 0, 704, 100
44901, V, 1, 1, 1, 1, 0, 704, 100
44902, V, 1, 1, 1, 1, 0, 704, 100
44903, V, 1, 1, 1, 1, 0, 704, 100
44904, V, 1, 1, 1, 1, 0, 704, 100
44905, V, 1, 1, 1, 1, 0, 704, 100
44906, V, 1, 1, 1, 1, 0, 704, 100
44907, V, 1, 1, 1, 1, 0, 704, 100
44908, V, 1, 1, 1, 1, 0, 704, 100
44909, V, 1, 1, 1, 1, 0, 704, 100
44910, V, 1, 1, 1, 1, 0, 704, 100
44911, V, 1, 1, 1, 1, 0, 704, 100
44912, V, 1, 1, 1, 1, 0, 704, 100
44913, V, 1, 1, 1, 1, 0, 704, 100
44914, V, 1, 1, 1, 1, 0, 704, 100
44915, V, 1, 1, 1, 1, 0, 704, 100
44916, V, 1, 1, 1, 1, 0, 704, 100
44917, V, 1, 1, 1, 1, 0, 704, 100
44918, V, 1, 1, 1, 1, 0, 704, 100
44919, V, 1, 1, 1, 1, 0, 704, 100
44920, V, 1, 1, 1, 1, 0, 704, 100
44921, V, 1, 1, 1, 1, 0, 704, 100
44922, V, 1, 1, 1, 1, 0, 704, 100
44923, V, 1, 1, 1, 1, 0, 704, 100
44924, V, 1, 1, 1, 1, 0, 704, 100
44925, V, 1, 1, 1, 1, 0, 704, 100
44926, V, 1, 1, 1, 1, 0, 704, 100
44928, V, 1, 1, 1, 1, 0, 704, 100
44929, V, 1, 1, 1, 1, 0, 704, 100
44930, V, 1, 1, 1, 1, 0, 704, 100
44931, V, 1, 1, 1, 1, 0, 704, 100
44932, V, 1, 1, 1, 1, 0, 704, 100
44933, V, 1, 1, 1, 1, 0, 704, 100
44934, V, 1, 1, 1, 1, 0, 704, 100
44935, V, 1, 1, 1, 1, 0, 704, 100
44936, V, 1, 1, 1, 1, 0, 704, 100
44937, V, 1, 1, 1, 1, 0, 704, 100
44938, V, 1, 1, 1, 1, 0, 704, 100
44939, V, 1, 1, 1, 1, 0, 704, 100
44940, V, 1, 1, 1, 1, 0, 704, 100
44941, V, 1, 1, 1, 1, 0, 704, 100
44942, V, 1, 1, 1, 1, 0, 704, 100
44943, V, 1, 1, 1, 1, 0, 704, 100
44944, V, 1, 1, 1, 1, 0, 704, 100
44945, V, 1, 1, 1, 1, 0, 704, 100
44946, V, 1, 1, 1, 1, 0, 704, 100
44947, V, 1, 1, 1, 1, 0, 704, 100
44948, V, 1, 1, 1, 1, 0, 704, 100
44949, V, 1, 1, 1, 1, 0, 704, 100
44950, V, 1, 1, 1, 1, 0, 704, 100
44951, V, 1, 1, 1, 1, 0, 704, 100
44952, V, 1, 1, 1, 1, 0, 704, 100
44953, V, 1, 1, 1, 1, 0, 704, 100
44954, V, 1, 1, 1, 1, 0, 704, 100
44955, V, 1, 1, 1, 1, 0, 704, 100
44956, V, 1, 1, 1, 1, 0, 704, 100
44957, V, 1, 1, 1, 1, 0, 704, 100
44958, V, 1, 1, 1, 1, 0, 704, 100
44959, V, 1, 1, 1, 1, 0, 704, 100
44960, V, 1, 1, 1, 1, 0, 704, 100
44961, V, 1, 1, 1, 1, 0, 704, 100
44962, V, 1, 1, 1, 1, 0, 704, 100
44963, V, 1, 1, 1, 1, 0, 704, 100
44964, V, 1, 1, 1, 1, 0, 704, 100
44965, V, 1, 1, 1, 1, 0, 704, 100
44966, V, 1, 1, 1, 1, 0, 704, 100
44967, V, 1, 1, 1, 1, 0, 704, 100
44968, V, 1, 1, 1, 1, 0, 704, 100
44969, V, 1, 1, 1, 1, 0, 704, 100
44971, V, 1, 1, 1, 1, 0, 704, 100
44972, V, 1, 1, 1, 1, 0, 704, 100
44973, V, 1, 1, 1, 1, 0, 704, 100
44974, V, 1, 1, 1, 1, 0, 704, 100
44975, V, 1, 1, 1, 1, 0, 704, 100
44976, V, 1, 1, 1, 1, 0, 704, 100
44977, V, 1, 1, 1, 1, 0, 704, 100
44978, V, 1, 1, 1, 1, 0, 704, 100
44979, V, 1, 1, 1, 1, 0, 704, 100
44980, V, 1, 1, 1, 1, 0, 704, 100
44981, V, 1, 1, 1, 1, 0, 704, 100
44982, V, 1, 1, 1, 1, 0, 704, 100
44983, V, 1, 1, 1, 1, 0, 704, 100
44984, V, 1, 1, 1, 1, 0, 704, 100
44985, V, 1, 1, 1, 1, 0, 704, 100
44986, V, 1, 1, 1, 1, 0, 704, 100
44987, V, 1, 1, 1, 1, 0, 704, 100
44988, V, 1, 1, 1, 1, 0, 704, 100
44989, V, 1, 1, 1, 1, 0, 704, 100
44990, V, 1, 1, 1, 1, 0, 704, 100
44991, V, 1, 1, 1, 1, 0, 704, 100
44992, V, 1, 1, 1, 1, 0, 704, 100
44993, V, 1, 1, 1, 1, 0, 704, 100
44994, V, 1, 1, 1, 1, 0, 704, 100
44995, V, 1, 1, 1, 1, 0, 704, 100
44996, V, 1, 1, 1, 1, 0, 704, 100
44997, V, 1, 1, 1, 1, 0, 704, 100
44998, V, 1, 1, 1, 1, 0, 704, 99
44999, V, 1, 1, 1, 1, 0, 704, 100
45000, V, 1, 1, 1, 1, 0, 704, 100
45001, V, 1, 1, 1, 1, 0, 704, 100
45002, V, 1, 1, 1, 1, 0, 704, 100
45003, V, 1, 1, 1, 1, 0, 704, 100
45004, V, 1, 1, 1, 1, 0, 704, 100
45005, V, 1, 1, 1, 1, 0, 704, 100
45006, V, 1, 1, 1, 1, 0, 704, 100
45007, V, 1, 1, 1, 1, 0, 704, 100
45008, V, 1, 1, 1, 1, 0, 704, 100
45009, V, 1, 1, 1, 1, 0, 704, 100
45010, V, 1, 1, 1, 1, 0, 704, 100
45011, V, 1, 1, 1, 1, 0, 704, 100
45012, V, 1, 1, 1, 1, 0, 704, 100
45014, V, 1, 1, 1, 1, 0, 704, 100
45015, V, 1, 1, 1, 1, 0, 704, 99
45016, V, 1, 1, 1, 1, 0, 704, 100
45017, V, 1, 1, 1, 1, 0, 704, 100
45018, V, 1, 1, 1, 1, 0, 704, 100
45019, V, 1, 1, 1, 1, 0, 704, 100
45020, V, 1, 1, 1, 1, 0, 704, 100
45021, V, 1, 1, 1, 1, 0, 704, 100
45022, V, 1, 1, 1, 1, 0, 704, 100
45023, V, 1, 1, 1, 1, 0, 704, 99
45024, V, 1, 1, 1, 1, 0, 704, 100
45025, V, 1, 1, 1, 1, 0, 704, 100
45026, V, 1, 1, 1, 1, 0, 704, 100
45027, V, 1, 1, 1, 1, 0, 704, 100
45028, V, 1, 1, 1, 1, 0, 704, 99
45029, V, 1, 1, 1, 1, 0, 704, 100
45030, V, 1, 1, 1, 1, 0, 704, 99
45031, V, 1, 1, 1, 1, 0, 704, 100
45032, V, 1, 1, 1, 1, 0, 704, 100
45033, V, 1, 1, 1, 1, 0, 704, 99
45034, V, 1, 1, 1, 1, 0, 704, 99
45035, V, 1, 1, 1, 1, 0, 704, 99
45036, V, 1, 1, 1, 1, 0, 704, 100
45037, V, 1, 1, 1, 1, 0, 704, 100
45038, V, 1, 1, 1, 1, 0, 704, 100
45039, V, 1, 1, 1, 1, 0, 704, 100
45040, V, 1, 1, 1, 1, 0, 704, 99
45041, V, 1, 1, 1, 1, 0, 704, 100
45042, V, 1, 1, 1, 1, 0, 704, 100
45043, V, 1, 1, 1, 1, 0, 704, 100
45044, V, 1, 1, 1, 1, 0, 704, 100
45045, V, 1, 1, 1, 1, 0, 704, 100
45046, V, 1, 1, 1, 1, 0, 704, 100
45047, V, 1, 1, 1, 1, 0, 704, 100
45048, V, 1, 1, 1, 1, 0, 704, 100
45049, V, 1, 1, 1, 1, 0, 704, 100
45050, V, 1, 1, 1, 1, 0, 704, 100
45051, V, 1, 1, 1, 1, 0, 704, 100
45052, V, 1, 1, 1, 1, 0, 704, 100
45053, V, 1, 1, 1, 1, 0, 704, 100
45054, V, 1, 1, 1, 1, 0, 704, 100
45056, V, 1, 1, 1, 1, 0, 704, 100
45057, V, 1, 1, 1, 1, 0, 704, 100
45058, V, 1, 1, 1, 1, 0, 704, 100
45059, V, 1, 1, 1, 1, 0, 704, 100
45060, V, 1, 1, 1, 1, 0, 704, 100
45061, V, 1, 1, 1, 1, 0, 704, 100
45062, V, 1, 1, 1, 1, 0, 704, 100
45063, V, 1, 1, 1, 1, 0, 704, 100
45064, V, 1, 1, 1, 1, 0, 704, 100
45065, V, 1, 1, 1, 1, 0, 704, 100
45066, V, 1, 1, 1, 1, 0, 704, 100
45067, V, 1, 1, 1, 1, 0, 704, 100
45068, V, 1, 1, 1, 1, 0, 704, 100
45069, V, 1, 1, 1, 1, 0, 704, 100
45070, V, 1, 1, 1, 1, 0, 704, 100
45071, V, 1, 1, 1, 1, 0, 704, 100
45072, V, 1, 1, 1, 1, 0, 704, 100
45073, V, 1, 1, 1, 1, 0, 704, 100
45074, V, 1, 1, 1, 1, 0, 704, 100
45075, V, 1, 1, 1, 1, 0, 704, 100
45076, V, 1, 1, 1, 1, 0, 704, 100
45077, V, 1, 1, 1, 1, 0, 704, 100
45078, V, 1, 1, 1, 1, 0, 704, 100
45079, V, 1, 1, 1, 1, 0, 704, 100
45080, V, 1, 1, 1, 1, 0, 704, 100
45081, V, 1, 1, 1, 1, 0, 704, 100
45082, V, 1, 1, 1, 1, 0, 704, 100
45083, V, 1, 1, 1, 1, 0, 704, 100
45084, V, 1, 1, 1, 1, 0, 704, 100
45085, V, 1, 1, 1, 1, 0, 704, 100
45086, V, 1, 1, 1, 1, 0, 704, 100
45087, V, 1, 1, 1, 1, 0, 704, 100
45088, V, 1, 1, 1, 1, 0, 704, 100
45089, V, 1, 1, 1, 1, 0, 704, 100
45090, V, 1, 1, 1, 1, 0, 704, 100
45091, V, 1, 1, 1, 1, 0, 704, 100
45092, V, 1, 1, 1, 1, 0, 704, 100
45093, V, 1, 1, 1, 1, 0, 704, 100
45094, V, 1, 1, 1, 1, 0, 704, 100
45095, V, 1, 1, 1, 1, 0, 704, 100
45096, V, 1, 1, 1, 1, 0, 704, 99
45097, V, 1, 1, 1, 1, 0, 704, 99
45099, V, 1, 1, 1, 1, 0, 704, 99
45100, V, 1, 1, 1, 1, 0, 704, 99
45101, V, 1, 1, 1, 1, 0, 704, 99
45102, V, 1, 1, 1, 1, 0, 704, 99
45103, V, 1, 1, 1, 1, 0, 704, 99
45104, V, 1, 1, 1, 1, 0, 704, 99
45105, V, 1, 1, 1, 1, 0, 704, 99
45106, V, 1, 1, 1, 1, 0, 704, 100
45107, V, 1, 1, 1, 1, 0, 704, 99
45108, V, 1, 1, 1, 1, 0, 704, 99
45109, V, 1, 1, 1, 1, 0, 704, 99
45110, V, 1, 1, 1, 1, 0, 704, 99
45111, V, 1, 1, 1, 1, 0, 704, 99
45112, V, 1, 1, 1, 1, 0, 704, 99
45113, V, 1, 1, 1, 1, 0, 704, 99
45114, V, 1, 1, 1, 1, 0, 704, 99
45115, V, 1, 1, 1, 1, 0, 704, 99
45116, V, 1, 1, 1, 1, 0, 704, 99
45117, V, 1, 1, 1, 1, 0, 704, 99
45118, V, 1, 1, 1, 1, 0, 704, 99
45119, V, 1, 1, 1, 1, 0, 704, 99
45120, V, 1, 1, 1, 1, 0, 704, 99
45121, V, 1, 1, 1, 1, 0, 704, 99
45122, V, 1, 1, 1, 1, 0, 704, 99
45123, V, 1, 1, 1, 1, 0, 704, 99
45124, V, 1, 1, 1, 1, 0, 704, 99
45125, V, 1, 1, 1, 1, 0, 704, 99
45126, V, 1, 1, 1, 1, 0, 704, 99
45127, V, 1, 1, 1, 1, 0, 704, 99
45128, V, 1, 1, 1, 1, 0, 704, 99
45129, V, 1, 1, 1, 1, 0, 704, 99
45130, V, 1, 1, 1, 1, 0, 704, 100
45131, V, 1, 1, 1, 1, 0, 704, 99
45132, V, 1, 1, 1, 1, 0, 704, 100
45133, V, 1, 1, 1, 1, 0, 704, 100
45134, V, 1, 1, 1, 1, 0, 704, 99
45135, V, 1, 1, 1, 1, 0, 704, 100
45136, V, 1, 1, 1, 1, 0, 704, 100
45137, V, 1, 1, 1, 1, 0, 704, 100
45138, V, 1, 1, 1, 1, 0, 704, 100
45139, V, 1, 1, 1, 1, 0, 704, 100
45140, V, 1, 1, 1, 1, 0, 704, 100
45142, V, 1, 1, 1, 1, 0, 704, 100
45143, V, 1, 1, 1, 1, 0, 704, 100
45144, V, 1, 1, 1, 1, 0, 704, 100
45145, V, 1, 1, 1, 1, 0, 704, 100
45146, V, 1, 1, 1, 1, 0, 704, 100
45147, V, 1, 1, 1, 1, 0, 704, 100
45148, V, 1, 1, 1, 1, 0, 704, 100
45149, V, 1, 1, 1, 1, 0, 704, 100
45150, V, 1, 1, 1, 1, 0, 704, 100
45151, V, 1, 1, 1, 1, 0, 704, 100
45152, V, 1, 1, 1, 1, 0, 704, 100
45153, V, 1, 1, 1, 1, 0, 704, 100
45154, V, 1, 1, 1, 1, 0, 704, 100
45155, V, 1, 1, 1, 1, 0, 704, 100
45156, V, 1, 1, 1, 1, 0, 704, 100
45157, V, 1, 1, 1, 1, 0, 704, 99
45158, V, 1, 1, 1, 1, 0, 704, 100
45159, V, 1, 1, 1, 1, 0, 704, 100
45160, V, 1, 1, 1, 1, 0, 704, 100
45161, V, 1, 1, 1, 1, 0, 704, 100
45162, V, 1, 1, 1, 1, 0, 704, 100
45163, V, 1, 1, 1, 1, 0, 704, 100
45164, V, 1, 1, 1, 1, 0, 704, 100
45165, V, 1, 1, 1, 1, 0, 704, 100
45166, V, 1, 1, 1, 1, 0, 704, 100
45167, V, 1, 1, 1, 1, 0, 704, 100
45168, V, 1, 1, 1, 1, 0, 704, 100
45169, V, 1, 1, 1, 1, 0, 704, 100
45170, V, 1, 1, 1, 1, 0, 704, 100
45171, V, 1, 1, 1, 1, 0, 704, 100
45172, V, 1, 1, 1, 1, 0, 704, 100
45173, V, 1, 1, 1, 1, 0, 704, 100
45174, V, 1, 1, 1, 1, 0, 704, 100
45175, V, 1, 1, 1, 1, 0, 704, 100
45176, V, 1, 1, 1, 1, 0, 704, 100
45177, V, 1, 1, 1, 1, 0, 704, 100
45178, V, 1, 1, 1, 1, 0, 704, 100
45179, V, 1, 1, 1, 1, 0, 704, 100
45180, V, 1, 1, 1, 1, 0, 704, 99
45181, V, 1, 1, 1, 1, 0, 704, 100
45182, V, 1, 1, 1, 1, 0, 704, 99
45184, V, 1, 1, 1, 1, 0, 704, 100
45185, V, 1, 1, 1, 1, 0, 704, 100
45186, V, 1, 1, 1, 1, 0, 704, 100
45187, V, 1, 1, 1, 1, 0, 704, 100
45188, V, 1, 1, 1, 1, 0, 704, 100
45189, V, 1, 1, 1, 1, 0, 704, 100
45190, V, 1, 1, 1, 1, 0, 704, 100
45191, V, 1, 1, 1, 1, 0, 704, 100
45192, V, 1, 1, 1, 1, 0, 704, 100
45193, V, 1, 1, 1, 1, 0, 704, 100
45194, V, 1, 1, 1, 1, 0, 704, 100
45195, V, 1, 1, 1, 1, 0, 704, 100
45196, V, 1, 1, 1, 1, 0, 704, 100
45197, V, 1, 1, 1, 1, 0, 704, 100
45198, V, 1, 1, 1, 1, 0, 704, 100
45199, V, 1, 1, 1, 1, 0, 704, 100
45200, V, 1, 1, 1, 1, 0, 704, 100
45201, V, 1, 1, 1, 1, 0, 704, 100
45202, V, 1, 1, 1, 1, 0, 704, 100
45203, V, 1, 1, 1, 1, 0, 704, 100
45204, V, 1, 1, 1, 1, 0, 704, 100
45205, V, 1, 1, 1, 1, 0, 704, 100
45206, V, 1, 1, 1, 1, 0, 704, 100
45207, V, 1, 1, 1, 1, 0, 704, 100
45208, V, 1, 1, 1, 1, 0, 704, 100
45209, V, 1, 1, 1, 1, 0, 704, 100
45210, V, 1, 1, 1, 1, 0, 704, 100
45211, V, 1, 1, 1, 1, 0, 704, 100
45212, V, 1, 1, 1, 1, 0, 704, 100
45213, V, 1, 1, 1, 1, 0, 704, 100
45214, V, 1, 1, 1, 1, 0, 704, 100
45215, V, 1, 1, 1, 1, 0, 704, 100
45216, V, 1, 1, 1, 1, 0, 704, 100
45217, V, 1, 1, 1, 1, 0, 704, 100
45218, V, 1, 1, 1, 1, 0, 704, 100
45219, V, 1, 1, 1, 1, 0, 704, 100
45220, V, 1, 1, 1, 1, 0, 704, 100
45221, V, 1, 1, 1, 1, 0, 704, 100
45222, V, 1, 1, 1, 1, 0, 704, 100
45223, V, 1, 1, 1, 1, 0, 704, 100
45224, V, 1, 1, 1, 1, 0, 704, 100
45225, V, 1, 1, 1, 1, 0, 704, 100
45227, V, 1, 1, 1, 1, 0, 704, 100
45228, V, 1, 1, 1, 1, 0, 704, 100
45229, V, 1, 1, 1, 1, 0, 704, 100
45230, V, 1, 1, 1, 1, 0, 704, 100
45231, V, 1, 1, 1, 1, 0, 704, 100
45232, V, 1, 1, 1, 1, 0, 704, 100
45233, V, 1, 1, 1, 1, 0, 704, 100
45234, V, 1, 1, 1, 1, 0, 704, 100
45235, V, 1, 1, 1, 1, 0, 704, 100
45236, V, 1, 1, 1, 1, 0, 704, 100
45237, V, 1, 1, 1, 1, 0, 704, 100
45238, V, 1, 1, 1, 1, 0, 704, 100
45239, V, 1, 1, 1, 1, 0, 704, 100
45240, V, 1, 1, 1, 1, 0, 704, 100
45241, V, 1, 1, 1, 1, 0, 704, 100
45242, V, 1, 1, 1, 1, 0, 704, 100
45243, V, 1, 1, 1, 1, 0, 704, 100
45244, V, 1, 1, 1, 1, 0, 704, 100
45245, V, 1, 1, 1, 1, 0, 704, 100
45246, V, 1, 1, 1, 1, 0, 704, 100
45247, V, 1, 1, 1, 1, 0, 704, 100
45248, V, 1, 1, 1, 1, 0, 704, 100
45249, V, 1, 1, 1, 1, 0, 704, 100
45250, V, 1, 1, 1, 1, 0, 704, 100
45251, V, 1, 1, 1, 1, 0, 704, 100
45252, V, 1, 1, 1, 1, 0, 704, 100
45253, V, 1, 1, 1, 1, 0, 704, 99
45254, V, 1, 1, 1, 1, 0, 704, 100
45255, V, 1, 1, 1, 1, 0, 704, 99
45256, V, 1, 1, 1, 1, 0, 704, 99
45257, V, 1, 1, 1, 1, 0, 704, 99
45258, V, 1, 1, 1, 1, 0, 704, 99
45259, V, 1, 1, 1, 1, 0, 704, 99
45260, V, 1, 1, 1, 1, 0, 704, 99
45261, V, 1, 1, 1, 1, 0, 704, 99
45262, V, 1, 1, 1, 1, 0, 704, 99
45263, V, 1, 1, 1, 1, 0, 704, 99
45264, V, 1, 1, 1, 1, 0, 704, 99
45265, V, 1, 1, 1, 1, 0, 704, 99
45266, V, 1, 1, 1, 1, 0, 704, 99
45267, V, 1, 1, 1, 1, 0, 704, 99
45268, V, 1, 1, 1, 1, 0, 704, 99
45270, V, 1, 1, 1, 1, 0, 704, 99
45271, V, 1, 1, 1, 1, 0, 704, 99
45272, V, 1, 1, 1, 1, 0, 704, 99
45273, V, 1, 1, 1, 1, 0, 704, 99
45274, V, 1, 1, 1, 1, 0, 704, 99
45275, V, 1, 1, 1, 1, 0, 704, 99
45276, V, 1, 1, 1, 1, 0, 704, 99
45277, V, 1, 1, 1, 1, 0, 704, 99
45278, V, 1, 1, 1, 1, 0, 704, 99
45279, V, 1, 1, 1, 1, 0, 704, 99
45280, V, 1, 1, 1, 1, 0, 704, 99
45281, V, 1, 1, 1, 1, 0, 704, 99
45282, V, 1, 1, 1, 1, 0, 704, 99
45283, V, 1, 1, 1, 1, 0, 704, 99
45284, V, 1, 1, 1, 1, 0, 704, 99
45285, V, 1, 1, 1, 1, 0, 704, 99
45286, V, 1, 1, 1, 1, 0, 704, 100
45287, V, 1, 1, 1, 1, 0, 704, 100
45288, V, 1, 1, 1, 1, 0, 704, 100
45289, V, 1, 1, 1, 1, 0, 704, 100
45290, V, 1, 1, 1, 1, 0, 704, 100
45291, V, 1, 1, 1, 1, 0, 704, 100
45292, V, 1, 1, 1, 1, 0, 704, 100
45293, V, 1, 1, 1, 1, 0, 704, 100
45294, V, 1, 1, 1, 1, 0, 704, 100
45295, V, 1, 1, 1, 1, 0, 704, 100
45296, V, 1, 1, 1, 1, 0, 704, 100
45297, V, 1, 1, 1, 1, 0, 704, 100
45298, V, 1, 1, 1, 1, 0, 704, 100
45299, V, 1, 1, 1, 1, 0, 704, 100
45300, V, 1, 1, 1, 1, 0, 704, 100
45301, V, 1, 1, 1, 1, 0, 704, 100
45302, V, 1, 1, 1, 1, 0, 704, 100
45303, V, 1, 1, 1, 1, 0, 704, 100
45304, V, 1, 1, 1, 1, 0, 704, 100
45305, V, 1, 1, 1, 1, 0, 704, 100
45306, V, 1, 1, 1, 1, 0, 704, 100
45307, V, 1, 1, 1, 1, 0, 704, 100
45308, V, 1, 1, 1, 1, 0, 704, 100
45309, V, 1, 1, 1, 1, 0, 704, 100
45310, V, 1, 1, 1, 1, 0, 704, 100
45312, V, 1, 1, 1, 1, 0, 704, 100
45313, V, 1, 1, 1, 1, 0, 704, 100
45314, V, 1, 1, 1, 1, 0, 704, 100
45315, V, 1, 1, 1, 1, 0, 704, 100
45316, V, 1, 1, 1, 1, 0, 704, 100
45317, V, 1, 1, 1, 1, 0, 704, 100
45318, V, 1, 1, 1, 1, 0, 704, 100
45319, V, 1, 1, 1, 1, 0, 704, 100
45320, V, 1, 1, 1, 1, 0, 704, 100
45321, V, 1, 1, 1, 1, 0, 704, 100
45322, V, 1, 1, 1, 1, 0, 704, 100
45323, V, 1, 1, 1, 1, 0, 704, 100
45324, V, 1, 1, 1, 1, 0, 704, 100
45325, V, 1, 1, 1, 1, 0, 704, 100
45326, V, 1, 1, 1, 1, 0, 704, 100
45327, V, 1, 1, 1, 1, 0, 704, 100
45328, V, 1, 1, 1, 1, 0, 704, 100
45329, V, 1, 1, 1, 1, 0, 704, 100
45330, V, 1, 1, 1, 1, 0, 704, 100
45331, V, 1, 1, 1, 1, 0, 704, 100
45332, V, 1, 1, 1, 1, 0, 704, 100
45333, V, 1, 1, 1, 1, 0, 704, 100
45334, V, 1, 1, 1, 1, 0, 704, 100
45335, V, 1, 1, 1, 1, 0, 704, 100
45336, V, 1, 1, 1, 1, 0, 704, 100
45337, V, 1, 1, 1, 1, 0, 704, 100
45338, V, 1, 1, 1, 1, 0, 704, 100
45339, V, 1, 1, 1, 1, 0, 704, 100
45340, V, 1, 1, 1, 1, 0, 704, 100
45341, V, 1, 1, 1, 1, 0, 704, 100
45342, V, 1, 1, 1, 1, 0, 704, 100
45343, V, 1, 1, 1, 1, 0, 704, 100
45344, V, 1, 1, 1, 1, 0, 704, 100
45345, V, 1, 1, 1, 1, 0, 704, 100
45346, V, 1, 1, 1, 1, 0, 704, 100
45347, V, 1, 1, 1, 1, 0, 704, 100
45348, V, 1, 1, 1, 1, 0, 704, 100
45349, V, 1, 1, 1, 1, 0, 704, 100
45350, V, 1, 1, 1, 1, 0, 704, 100
45351, V, 1, 1, 1, 1, 0, 704, 100
45352, V, 1, 1, 1, 1, 0, 704, 100
45353, V, 1, 1, 1, 1, 0, 704, 100
45355, V, 1, 1, 1, 1, 0, 704, 100
45356, V, 1, 1, 1, 1, 0, 704, 100
45357, V, 1, 1, 1, 1, 0, 704, 100
45358, V, 1, 1, 1, 1, 0, 704, 100
45359, V, 1, 1, 1, 1, 0, 704, 100
45360, V, 1, 1, 1, 1, 0, 704, 100
45361, V, 1, 1, 1, 1, 0, 704, 100
45362, V, 1, 1, 1, 1, 0, 704, 100
45363, V, 1, 1, 1, 1, 0, 704, 100
45364, V, 1, 1, 1, 1, 0, 704, 100
45365, V, 1, 1, 1, 1, 0, 704, 100
45366, V, 1, 1, 1, 1, 0, 704, 100
45367, V, 1, 1, 1, 1, 0, 704, 100
45368, V, 1, 1, 1, 1, 0, 704, 100
45369, V, 1, 1, 1, 1, 0, 704, 100
45370, V, 1, 1, 1, 1, 0, 704, 100
45371, V, 1, 1, 1, 1, 0, 704, 100
45372, V, 1, 1, 1, 1, 0, 704, 100
45373, V, 1, 1, 1, 1, 0, 704, 100
45374, V, 1, 1, 1, 1, 0, 704, 100
45375, V, 1, 1, 1, 1, 0, 704, 100
45376, V, 1, 1, 1, 1, 0, 704, 100
45377, V, 1, 1, 1, 1, 0, 704, 100
45378, V, 1, 1, 1, 1, 0, 704, 100
45379, V, 1, 1, 1, 1, 0, 704, 100
45380, V, 1, 1, 1, 1, 0, 704, 100
45381, V, 1, 1, 1, 1, 0, 704, 100
45382, V, 1, 1, 1, 1, 0, 704, 100
45383, V, 1, 1, 1, 1, 0, 704, 100
45384, V, 1, 1, 1, 1, 0, 704, 100
45385, V, 1, 1, 1, 1, 0, 704, 100
45386, V, 1, 1, 1, 1, 0, 704, 100
45387, V, 1, 1, 1, 1, 0, 704, 100
45388, V, 1, 1, 1, 1, 0, 704, 100
45389, V, 1, 1, 1, 1, 0, 704, 100
45390, V, 1, 1, 1, 1, 0, 704, 100
45391, V, 1, 1, 1, 1, 0, 704, 100
45392, V, 1, 1, 1, 1, 0, 704, 100
45393, V, 1, 1, 1, 1, 0, 704, 100
45394, V, 1, 1, 1, 1, 0, 704, 100
45395, V, 1, 1, 1, 1, 0, 704, 100
45396, V, 1, 1, 1, 1, 0, 704, 100
45398, V, 1, 1, 1, 1, 0, 704, 100
45399, V, 1, 1, 1, 1, 0, 704, 100
45400, V, 1, 1, 1, 1, 0, 704, 100
45401, V, 1, 1, 1, 1, 0, 704, 100
45402, V, 1, 1, 1, 1, 0, 704, 100
45403, V, 1, 1, 1, 1, 0, 704, 100
45404, V, 1, 1, 1, 1, 0, 704, 100
45405, V, 1, 1, 1, 1, 0, 704, 100
45406, V, 1, 1, 1, 1, 0, 704, 100
45407, V, 1, 1, 1, 1, 0, 704, 100
45408, V, 1, 1, 1, 1, 0, 704, 100
45409, V, 1, 1, 1, 1, 0, 704, 100
45410, V, 1, 1, 1, 1, 0, 704, 100
45411, V, 1, 1, 1, 1, 0, 704, 100
45412, V, 1, 1, 1, 1, 0, 704, 100
45413, V, 1, 1, 1, 1, 0, 704, 99
45414, V, 1, 1, 1, 1, 0, 704, 100
45415, V, 1, 1, 1, 1, 0, 704, 99
45416, V, 1, 1, 1, 1, 0, 704, 99
45417, V, 1, 1, 1, 1, 0, 704, 100
45418, V, 1, 1, 1, 1, 0, 704, 100
45419, V, 1, 1, 1, 1, 0, 704, 100
45420, V, 1, 1, 1, 1, 0, 704, 99
45421, V, 1, 1, 1, 1, 0, 704, 100
45422, V, 1, 1, 1, 1, 0, 704, 100
45423, V, 1, 1, 1, 1, 0, 704, 100
45424, V, 1, 1, 1, 1, 0, 704, 100
45425, V, 1, 1, 1, 1, 0, 704, 100
45426, V, 1, 1, 1, 1, 0, 704, 100
45427, V, 1, 1, 1, 1, 0, 704, 100
45428, V, 1, 1, 1, 1, 0, 704, 100
45429, V, 1, 1, 1, 1, 0, 704, 100
45430, V, 1, 1, 1, 1, 0, 704, 100
45431, V, 1, 1, 1, 1, 0, 704, 100
45432, V, 1, 1, 1, 1, 0, 704, 100
45433, V, 1, 1, 1, 1, 0, 704, 100
45434, V, 1, 1, 1, 1, 0, 704, 100
45435, V, 1, 1, 1, 1, 0, 704, 100
45436, V, 1, 1, 1, 1, 0, 704, 100
45437, V, 1, 1, 1, 1, 0, 704, 100
45438, V, 1, 1, 1, 1, 0, 704, 100
45440, V, 1, 1, 1, 1, 0, 704, 100
45441, V, 1, 1, 1, 1, 0, 704, 100
45442, V, 1, 1, 1, 1, 0, 704, 100
45443, V, 1, 1, 1, 1, 0, 704, 100
45444, V, 1, 1, 1, 1, 0, 704, 100
45445, V, 1, 1, 1, 1, 0, 704, 100
45446, V, 1, 1, 1, 1, 0, 704, 100
45447, V, 1, 1, 1, 1, 0, 704, 100
45448, V, 1, 1, 1, 1, 0, 704, 100
45449, V, 1, 1, 1, 1, 0, 704, 100
45450, V, 1, 1, 1, 1, 0, 704, 100
45451, V, 1, 1, 1, 1, 0, 704, 100
45452, V, 1, 1, 1, 1, 0, 704, 100
45453, V, 1, 1, 1, 1, 0, 704, 100
45454, V, 1, 1, 1, 1, 0, 704, 100
45455, V, 1, 1, 1, 1, 0, 704, 100
45456, V, 1, 1, 1, 1, 0, 704, 100
45457, V, 1, 1, 1, 1, 0, 704, 100
45458, V, 1, 1, 1, 1, 0, 704, 100
45459, V, 1, 1, 1, 1, 0, 704, 100
45460, V, 1, 1, 1, 1, 0, 704, 100
45461, V, 1, 1, 1, 1, 0, 704, 100
45462, V, 1, 1, 1, 1, 0, 704, 100
45463, V, 1, 1, 1, 1, 0, 704, 100
45464, V, 1, 1, 1, 1, 0, 704, 100
45465, V, 1, 1, 1, 1, 0, 704, 100
45466, V, 1, 1, 1, 1, 0, 704, 100
45467, V, 1, 1, 1, 1, 0, 704, 100
45468, V, 1, 1, 1, 1, 0, 704, 100
45469, V, 1, 1, 1, 1, 0, 704, 100
45470, V, 1, 1, 1, 1, 0, 704, 100
45471, V, 1, 1, 1, 1, 0, 704, 100
45472, V, 1, 1, 1, 1, 0, 704, 100
45473, V, 1, 1, 1, 1, 0, 704, 99
45474, V, 1, 1, 1, 1, 0, 704, 100
45475, V, 1, 1, 1, 1, 0, 704, 100
45476, V, 1, 1, 1, 1, 0, 704, 100
45477, V, 1, 1, 1, 1, 0, 704, 100
45478, V, 1, 1, 1, 1, 0, 704, 100
45479, V, 1, 1, 1, 1, 0, 704, 100
45480, V, 1, 1, 1, 1, 0, 704, 100
45481, V, 1, 1, 1, 1, 0, 704, 100
45483, V, 1, 1, 1, 1, 0, 704, 100
45484, V, 1, 1, 1, 1, 0, 704, 100
45485, V, 1, 1, 1, 1, 0, 704, 100
45486, V, 1, 1, 1, 1, 0, 704, 100
45487, V, 1, 1, 1, 1, 0, 704, 100
45488, V, 1, 1, 1, 1, 0, 704, 100
45489, V, 1, 1, 1, 1, 0, 704, 100
45490, V, 1, 1, 1, 1, 0, 704, 100
45491, V, 1, 1, 1, 1, 0, 704, 100
45492, V, 1, 1, 1, 1, 0, 704, 100
45493, V, 1, 1, 1, 1, 0, 704, 100
45494, V, 1, 1, 1, 1, 0, 704, 100
45495, V, 1, 1, 1, 1, 0, 704, 100
45496, V, 1, 1, 1, 1, 0, 704, 100
45497, V, 1, 1, 1, 1, 0, 704, 100
45498, V, 1, 1, 1, 1, 0, 704, 100
45499, V, 1, 1, 1, 1, 0, 704, 100
45500, V, 1, 1, 1, 1, 0, 704, 100
45501, V, 1, 1, 1, 1, 0, 704, 100
45502, V, 1, 1, 1, 1, 0, 704, 100
45503, V, 1, 1, 1, 1, 0, 704, 100
45504, V, 1, 1, 1, 1, 0, 704, 100
45505, V, 1, 1, 1, 1, 0, 704, 100
45506, V, 1, 1, 1, 1, 0, 704, 100
45507, V, 1, 1, 1, 1, 0, 704, 100
45508, V, 1, 1, 1, 1, 0, 704, 100
45509, V, 1, 1, 1, 1, 0, 704, 100
45510, V, 1, 1, 1, 1, 0, 704, 100
45511, V, 1, 1, 1, 1, 0, 704, 100
45512, V, 1, 1, 1, 1, 0, 704, 100
45513, V, 1, 1, 1, 1, 0, 704, 100
45514, V, 1, 1, 1, 1, 0, 704, 100
45515, V, 1, 1, 1, 1, 0, 704, 100
45516, V, 1, 1, 1, 1, 0, 704, 100
45517, V, 1, 1, 1, 1, 0, 704, 100
45518, V, 1, 1, 1, 1, 0, 704, 100
45519, V, 1, 1, 1, 1, 0, 704, 100
45520, V, 1, 1, 1, 1, 0, 704, 100
45521, V, 1, 1, 1, 1, 0, 704, 100
45522, V, 1, 1, 1, 1, 0, 704, 100
45523, V, 1, 1, 1, 1, 0, 704, 100
45524, V, 1, 1, 1, 1, 0, 704, 100
45526, V, 1, 1, 1, 1, 0, 704, 100
45527, V, 1, 1, 1, 1, 0, 704, 100
45528, V, 1, 1, 1, 1, 0, 704, 100
45529, V, 1, 1, 1, 1, 0, 704, 100
45530, V, 1, 1, 1, 1, 0, 704, 100
45531, V, 1, 1, 1, 1, 0, 704, 100
45532, V, 1, 1, 1, 1, 0, 704, 100
45533, V, 1, 1, 1, 1, 0, 704, 100
45534, V, 1, 1, 1, 1, 0, 704, 100
45535, V, 1, 1, 1, 1, 0, 704, 100
45536, V, 1, 1, 1, 1, 0, 704, 100
45537, V, 1, 1, 1, 1, 0, 704, 100
45538, V, 1, 1, 1, 1, 0, 704, 100
45539, V, 1, 1, 1, 1, 0, 704, 100
45540, V, 1, 1, 1, 1, 0, 704, 100
45541, V, 1, 1, 1, 1, 0, 704, 100
45542, V, 1, 1, 1, 1, 0, 704, 100
45543, V, 1, 1, 1, 1, 0, 704, 100
45544, V, 1, 1, 1, 1, 0, 704, 99
45545, V, 1, 1, 1, 1, 0, 704, 99
45546, V, 1, 1, 1, 1, 0, 704, 99
45547, V, 1, 1, 1, 1, 0, 704, 99
45548, V, 1, 1, 1, 1, 0, 704, 99
45549, V, 1, 1, 1, 1, 0, 704, 99
45550, V, 1, 1, 1, 1, 0, 704, 99
45551, V, 1, 1, 1, 1, 0, 704, 99
45552, V, 1, 1, 1, 1, 0, 704, 99
45553, V, 1, 1, 1, 1, 0, 704, 99
45554, V, 1, 1, 1, 1, 0, 704, 99
45555, V, 1, 1, 1, 1, 0, 704, 99
45556, V, 1, 1, 1, 1, 0, 704, 99
45557, V, 1, 1, 1, 1, 0, 704, 99
45558, V, 1, 1, 1, 1, 0, 704, 99
45559, V, 1, 1, 1, 1, 0, 704, 99
45560, V, 1, 1, 1, 1, 0, 704, 99
45561, V, 1, 1, 1, 1, 0, 704, 99
45562, V, 1, 1, 1, 1, 0, 704, 99
45563, V, 1, 1, 1, 1, 0, 704, 99
45564, V, 1, 1, 1, 1, 0, 704, 99
45565, V, 1, 1, 1, 1, 0, 704, 99
45566, V, 1, 1, 1, 1, 0, 704, 99
45568, V, 1, 1, 1, 1, 0, 704, 99
45569, V, 1, 1, 1, 1, 0, 704, 99
45570, V, 1, 1, 1, 1, 0, 704, 99
45571, V, 1, 1, 1, 1, 0, 704, 99
45572, V, 1, 1, 1, 1, 0, 704, 99
45573, V, 1, 1, 1, 1, 0, 704, 99
45574, V, 1, 1, 1, 1, 0, 704, 99
45575, V, 1, 1, 1, 1, 0, 704, 99
45576, V, 1, 1, 1, 1, 0, 704, 99
45577, V, 1, 1, 1, 1, 0, 704, 99
45578, V, 1, 1, 1, 1, 0, 704, 99
45579, V, 1, 1, 1, 1, 0, 704, 99
45580, V, 1, 1, 1, 1, 0, 704, 99
45581, V, 1, 1, 1, 1, 0, 704, 99
45582, V, 1, 1, 1, 1, 0, 704, 99
45583, V, 1, 1, 1, 1, 0, 704, 99
45584, V, 1, 1, 1, 1, 0, 704, 99
45585, V, 1, 1, 1, 1, 0, 704, 99
45586, V, 1, 1, 1, 1, 0, 704, 99
45587, V, 1, 1, 1, 1, 0, 704, 99
45588, V, 1, 1, 1, 1, 0, 704, 99
45589, V, 1, 1, 1, 1, 0, 704, 99
45590, V, 1, 1, 1, 1, 0, 704, 99
45591, V, 1, 1, 1, 1, 0, 704, 99
45592, V, 1, 1, 1, 1, 0, 704, 99
45593, V, 1, 1, 1, 1, 0, 704, 99
45594, V, 1, 1, 1, 1, 0, 704, 99
45595, V, 1, 1, 1, 1, 0, 704, 99
45596, V, 1, 1, 1, 1, 0, 704, 99
45597, V, 1, 1, 1, 1, 0, 704, 99
45598, V, 1, 1, 1, 1, 0, 704, 100
45599, V, 1, 1, 1, 1, 0, 704, 99
45600, V, 1, 1, 1, 1, 0, 704, 99
45601, V, 1, 1, 1, 1, 0, 704, 100
45602, V, 1, 1, 1, 1, 0, 704, 99
45603, V, 1, 1, 1, 1, 0, 704, 99
45604, V, 1, 1, 1, 1, 0, 704, 99
45605, V, 1, 1, 1, 1, 0, 704, 100
45606, V, 1, 1, 1, 1, 0, 704, 100
45607, V, 1, 1, 1, 1, 0, 704, 99
45608, V, 1, 1, 1, 1, 0, 704, 100
45609, V, 1, 1, 1, 1, 0, 704, 100
45611, V, 1, 1, 1, 1, 0, 704, 100
45612, V, 1, 1, 1, 1, 0, 704, 100
45613, V, 1, 1, 1, 1, 0, 704, 100
45614, V, 1, 1, 1, 1, 0, 704, 100
45615, V, 1, 1, 1, 1, 0, 704, 99
45616, V, 1, 1, 1, 1, 0, 704, 99
45617, V, 1, 1, 1, 1, 0, 704, 99
45618, V, 1, 1, 1, 1, 0, 704, 99
45619, V, 1, 1, 1, 1, 0, 704, 99
45620, V, 1, 1, 1, 1, 0, 704, 99
45621, V, 1, 1, 1, 1, 0, 704, 99
45622, V, 1, 1, 1, 1, 0, 704, 99
45623, V, 1, 1, 1, 1, 0, 704, 99
45624, V, 1, 1, 1, 1, 0, 704, 99
45625, V, 1, 1, 1, 1, 0, 704, 99
45626, V, 1, 1, 1, 1, 0, 704, 99
45627, V, 1, 1, 1, 1, 0, 704, 99
45628, V, 1, 1, 1, 1, 0, 704, 99
45629, V, 1, 1, 1, 1, 0, 704, 99
45630, V, 1, 1, 1, 1, 0, 704, 99
45631, V, 1, 1, 1, 1, 0, 704, 99
45632, V, 1, 1, 1, 1, 0, 704, 99
45633, V, 1, 1, 1, 1, 0, 704, 99
45634, V, 1, 1, 1, 1, 0, 704, 99
45635, V, 1, 1, 1, 1, 0, 704, 99
45636, V, 1, 1, 1, 1, 0, 704, 99
45637, V, 1, 1, 1, 1, 0, 704, 99
45638, V, 1, 1, 1, 1, 0, 704, 99
45639, V, 1, 1, 1, 1, 0, 704, 100
45640, V, 1, 1, 1, 1, 0, 704, 99
45641, V, 1, 1, 1, 1, 0, 704, 100
45642, V, 1, 1, 1, 1, 0, 704, 99
45643, V, 1, 1, 1, 1, 0, 704, 99
45644, V, 1, 1, 1, 1, 0, 704, 100
45645, V, 1, 1, 1, 1, 0, 704, 99
45646, V, 1, 1, 1, 1, 0, 704, 100
45647, V, 1, 1, 1, 1, 0, 704, 100
45648, V, 1, 1, 1, 1, 0, 704, 99
45649, V, 1, 1, 1, 1, 0, 704, 100
45650, V, 1, 1, 1, 1, 0, 704, 100
45651, V, 1, 1, 1, 1, 0, 704, 100
45652, V, 1, 1, 1, 1, 0, 704, 100
45654, V, 1, 1, 1, 1, 0, 704, 99
45655, V, 1, 1, 1, 1, 0, 704, 100
45656, V, 1, 1, 1, 1, 0, 704, 99
45657, V, 1, 1, 1, 1, 0, 704, 100
45658, V, 1, 1, 1, 1, 0, 704, 99
45659, V, 1, 1, 1, 1, 0, 704, 100
45660, V, 1, 1, 1, 1, 0, 704, 99
45661, V, 1, 1, 1, 1, 0, 704, 99
45662, V, 1, 1, 1, 1, 0, 704, 100
45663, V, 1, 1, 1, 1, 0, 704, 100
45664, V, 1, 1, 1, 1, 0, 704, 100
45665, V, 1, 1, 1, 1, 0, 704, 100
45666, V, 1, 1, 1, 1, 0, 704, 100
45667, V, 1, 1, 1, 1, 0, 704, 100
45668, V, 1, 1, 1, 1, 0, 704, 100
45669, V, 1, 1, 1, 1, 0, 704, 100
45670, V, 1, 1, 1, 1, 0, 704, 100
45671, V, 1, 1, 1, 1, 0, 704, 100
45672, V, 1, 1, 1, 1, 0, 704, 100
45673, V, 1, 1, 1, 1, 0, 704, 100
45674, V, 1, 1, 1, 1, 0, 704, 99
45675, V, 1, 1, 1, 1, 0, 704, 99
45676, V, 1, 1, 1, 1, 0, 704, 100
45677, V, 1, 1, 1, 1, 0, 704, 99
45678, V, 1, 1, 1, 1, 0, 704, 99
45679, V, 1, 1, 1, 1, 0, 704, 99
45680, V, 1, 1, 1, 1, 0, 704, 99
45681, V, 1, 1, 1, 1, 0, 704, 99
45682, V, 1, 1, 1, 1, 0, 704, 99
45683, V, 1, 1, 1, 1, 0, 704, 99
45684, V, 1, 1, 1, 1, 0, 704, 99
45685, V, 1, 1, 1, 1, 0, 704, 99
45686, V, 1, 1, 1, 1, 0, 704, 99
45687, V, 1, 1, 1, 1, 0, 704, 99
45688, V, 1, 1, 1, 1, 0, 704, 99
45689, V, 1, 1, 1, 1, 0, 704, 99
45690, V, 1, 1, 1, 1, 0, 704, 99
45691, V, 1, 1, 1, 1, 0, 704, 99
45692, V, 1, 1, 1, 1, 0, 704, 99
45693, V, 1, 1, 1, 1, 0, 704, 99
45694, V, 1, 1, 1, 1, 0, 704, 99
45696, V, 1, 1, 1, 1, 0, 704, 99
45697, V, 1, 1, 1, 1, 0, 704, 99
45698, V, 1, 1, 1, 1, 0, 704, 99
45699, V, 1, 1, 1, 1, 0, 704, 99
45700, V, 1, 1, 1, 1, 0, 704, 99
45701, V, 1, 1, 1, 1, 0, 704, 99
45702, V, 1, 1, 1, 1, 0, 704, 99
45703, V, 1, 1, 1, 1, 0, 704, 99
45704, V, 1, 1, 1, 1, 0, 704, 99
45705, V, 1, 1, 1, 1, 0, 704, 99
45706, V, 1, 1, 1, 1, 0, 704, 99
45707, V, 1, 1, 1, 1, 0, 704, 99
45708, V, 1, 1, 1, 1, 0, 704, 99
45709, V, 1, 1, 1, 1, 0, 704, 99
45710, V, 1, 1, 1, 1, 0, 704, 99
45711, V, 1, 1, 1, 1, 0, 704, 99
45712, V, 1, 1, 1, 1, 0, 704, 99
45713, V, 1, 1, 1, 1, 0, 704, 99
45714, V, 1, 1, 1, 1, 0, 704, 99
45715, V, 1, 1, 1, 1, 0, 704, 99
45716, V, 1, 1, 1, 1, 0, 704, 99
45717, V, 1, 1, 1, 1, 0, 704, 99
45718, V, 1, 1, 1, 1, 0, 704, 99
45719, V, 1, 1, 1, 1, 0, 704, 99
45720, V, 1, 1, 1, 1, 0, 704, 99
45721, V, 1, 1, 1, 1, 0, 704, 99
45722, V, 1, 1, 1, 1, 0, 704, 99
45723, V, 1, 1, 1, 1, 0, 704, 99
45724, V, 1, 1, 1, 1, 0, 704, 99
45725, V, 1, 1, 1, 1, 0, 704, 99
45726, V, 1, 1, 1, 1, 0, 704, 99
45727, V, 1, 1, 1, 1, 0, 704, 99
45728, V, 1, 1, 1, 1, 0, 704, 99
45729, V, 1, 1, 1, 1, 0, 704, 99
45730, V, 1, 1, 1, 1, 0, 704, 100
45731, V, 1, 1, 1, 1, 0, 704, 99
45732, V, 1, 1, 1, 1, 0, 704, 99
45733, V, 1, 1, 1, 1, 0, 704, 99
45734, V, 1, 1, 1, 1, 0, 704, 100
45735, V, 1, 1, 1, 1, 0, 704, 99
45736, V, 1, 1, 1, 1, 0, 704, 99
45737, V, 1, 1, 1, 1, 0, 704, 100
45739, V, 1, 1, 1, 1, 0, 704, 100
45740, V, 1, 1, 1, 1, 0, 704, 100
45741, V, 1, 1, 1, 1, 0, 704, 100
45742, V, 1, 1, 1, 1, 0, 704, 100
45743, V, 1, 1, 1, 1, 0, 704, 100
45744, V, 1, 1, 1, 1, 0, 704, 100
45745, V, 1, 1, 1, 1, 0, 704, 100
45746, V, 1, 1, 1, 1, 0, 704, 100
45747, V, 1, 1, 1, 1, 0, 704, 100
45748, V, 1, 1, 1, 1, 0, 704, 100
45749, V, 1, 1, 1, 1, 0, 704, 100
45750, V, 1, 1, 1, 1, 0, 704, 100
45751, V, 1, 1, 1, 1, 0, 704, 100
45752, V, 1, 1, 1, 1, 0, 704, 100
45753, V, 1, 1, 1, 1, 0, 704, 100
45754, V, 1, 1, 1, 1, 0, 704, 100
45755, V, 1, 1, 1, 1, 0, 704, 100
45756, V, 1, 1, 1, 1, 0, 704, 100
45757, V, 1, 1, 1, 1, 0, 704, 100
45758, V, 1, 1, 1, 1, 0, 704, 100
45759, V, 1, 1, 1, 1, 0, 704, 100
45760, V, 1, 1, 1, 1, 0, 704, 100
45761, V, 1, 1, 1, 1, 0, 704, 100
45762, V, 1, 1, 1, 1, 0, 704, 100
45763, V, 1, 1, 1, 1, 0, 704, 100
45764, V, 1, 1, 1, 1, 0, 704, 100
45765, V, 1, 1, 1, 1, 0, 704, 100
45766, V, 1, 1, 1, 1, 0, 704, 100
45767, V, 1, 1, 1, 1, 0, 704, 100
45768, V, 1, 1, 1, 1, 0, 704, 100
45769, V, 1, 1, 1, 1, 0, 704, 100
45770, V, 1, 1, 1, 1, 0, 704, 100
45771, V, 1, 1, 1, 1, 0, 704, 100
45772, V, 1, 1, 1, 1, 0, 704, 100
45773, V, 1, 1, 1, 1, 0, 704, 100
45774, V, 1, 1, 1, 1, 0, 704, 100
45775, V, 1, 1, 1, 1, 0, 704, 100
45776, V, 1, 1, 1, 1, 0, 704, 99
45777, V, 1, 1, 1, 1, 0, 704, 99
45778, V, 1, 1, 1, 1, 0, 704, 100
45779, V, 1, 1, 1, 1, 0, 704, 99
45780, V, 1, 1, 1, 1, 0, 704, 100
45782, V, 1, 1, 1, 1, 0, 704, 99
45783, V, 1, 1, 1, 1, 0, 704, 100
45784, V, 1, 1, 1, 1, 0, 704, 99
45785, V, 1, 1, 1, 1, 0, 704, 99
45786, V, 1, 1, 1, 1, 0, 704, 100
45787, V, 1, 1, 1, 1, 0, 704, 100
45788, V, 1, 1, 1, 1, 0, 704, 100
45789, V, 1, 1, 1, 1, 0, 704, 100
45790, V, 1, 1, 1, 1, 0, 704, 99
45791, V, 1, 1, 1, 1, 0, 704, 100
45792, V, 1, 1, 1, 1, 0, 704, 100
45793, V, 1, 1, 1, 1, 0, 704, 100
45794, V, 1, 1, 1, 1, 0, 704, 100
45795, V, 1, 1, 1, 1, 0, 704, 99
45796, V, 1, 1, 1, 1, 0, 704, 99
45797, V, 1, 1, 1, 1, 0, 704, 100
45798, V, 1, 1, 1, 1, 0, 704, 100
45799, V, 1, 1, 1, 1, 0, 704, 100
45800, V, 1, 1, 1, 1, 0, 704, 100
45801, V, 1, 1, 1, 1, 0, 704, 100
45802, V, 1, 1, 1, 1, 0, 704, 100
45803, V, 1, 1, 1, 1, 0, 704, 100
45804, V, 1, 1, 1, 1, 0, 704, 100
45805, V, 1, 1, 1, 1, 0, 704, 100
45806, V, 1, 1, 1, 1, 0, 704, 100
45807, V, 1, 1, 1, 1, 0, 704, 100
45808, V, 1, 1, 1, 1, 0, 704, 100
45809, V, 1, 1, 1, 1, 0, 704, 100
45810, V, 1, 1, 1, 1, 0, 704, 100
45811, V, 1, 1, 1, 1, 0, 704, 100
45812, V, 1, 1, 1, 1, 0, 704, 100
45813, V, 1, 1, 1, 1, 0, 704, 100
45814, V, 1, 1, 1, 1, 0, 704, 100
45815, V, 1, 1, 1, 1, 0, 704, 100
45816, V, 1, 1, 1, 1, 0, 704, 100
45817, V, 1, 1, 1, 1, 0, 704, 100
45818, V, 1, 1, 1, 1, 0, 704, 100
45819, V, 1, 1, 1, 1, 0, 704, 100
45820, V, 1, 1, 1, 1, 0, 704, 100
45821, V, 1, 1, 1, 1, 0, 704, 100
45822, V, 1, 1, 1, 1, 0, 704, 100
45824, V, 1, 1, 1, 1, 0, 704, 100
45825, V, 1, 1, 1, 1, 0, 704, 100
45826, V, 1, 1, 1, 1, 0, 704, 100
45827, V, 1, 1, 1, 1, 0, 704, 100
45828, V, 1, 1, 1, 1, 0, 704, 100
45829, V, 1, 1, 1, 1, 0, 704, 100
45830, V, 1, 1, 1, 1, 0, 704, 100
45831, V, 1, 1, 1, 1, 0, 704, 100
45832, V, 1, 1, 1, 1, 0, 704, 100
45833, V, 1, 1, 1, 1, 0, 704, 100
45834, V, 1, 1, 1, 1, 0, 704, 100
45835, V, 1, 1, 1, 1, 0, 704, 100
45836, V, 1, 1, 1, 1, 0, 704, 100
45837, V, 1, 1, 1, 1, 0, 704, 100
45838, V, 1, 1, 1, 1, 0, 704, 100
45839, V, 1, 1, 1, 1, 0, 704, 100
45840, V, 1, 1, 1, 1, 0, 704, 100
45841, V, 1, 1, 1, 1, 0, 704, 100
45842, V, 1, 1, 1, 1, 0, 704, 100
45843, V, 1, 1, 1, 1, 0, 704, 100
45844, V, 1, 1, 1, 1, 0, 704, 100
45845, V, 1, 1, 1, 1, 0, 704, 100
45846, V, 1, 1, 1, 1, 0, 704, 100
45847, V, 1, 1, 1, 1, 0, 704, 100
45848, V, 1, 1, 1, 1, 0, 704, 100
45849, V, 1, 1, 1, 1, 0, 704, 100
45850, V, 1, 1, 1, 1, 0, 704, 100
45851, V, 1, 1, 1, 1, 0, 704, 100
45852, V, 1, 1, 1, 1, 0, 704, 100
45853, V, 1, 1, 1, 1, 0, 704, 100
45854, V, 1, 1, 1, 1, 0, 704, 100
45855, V, 1, 1, 1, 1, 0, 704, 100
45856, V, 1, 1, 1, 1, 0, 704, 100
45857, V, 1, 1, 1, 1, 0, 704, 100
45858, V, 1, 1, 1, 1, 0, 704, 100
45859, V, 1, 1, 1, 1, 0, 704, 100
45860, V, 1, 1, 1, 1, 0, 704, 100
45861, V, 1, 1, 1, 1, 0, 704, 100
45862, V, 1, 1, 1, 1, 0, 704, 100
45863, V, 1, 1, 1, 1, 0, 704, 100
45864, V, 1, 1, 1, 1, 0, 704, 100
45865, V, 1, 1, 1, 1, 0, 704, 100
45867, V, 1, 1, 1, 1, 0, 704, 100
45868, V, 1, 1, 1, 1, 0, 704, 100
45869, V, 1, 1, 1, 1, 0, 704, 100
45870, V, 1, 1, 1, 1, 0, 704, 100
45871, V, 1, 1, 1, 1, 0, 704, 100
45872, V, 1, 1, 1, 1, 0, 704, 100
45873, V, 1, 1, 1, 1, 0, 704, 100
45874, V, 1, 1, 1, 1, 0, 704, 100
45875, V, 1, 1, 1, 1, 0, 704, 99
45876, V, 1, 1, 1, 1, 0, 704, 100
45877, V, 1, 1, 1, 1, 0, 704, 100
45878, V, 1, 1, 1, 1, 0, 704, 100
45879, V, 1, 1, 1, 1, 0, 704, 100
45880, V, 1, 1, 1, 1, 0, 704, 100
45881, V, 1, 1, 1, 1, 0, 704, 99
45882, V, 1, 1, 1, 1, 0, 704, 100
45883, V, 1, 1, 1, 1, 0, 704, 100
45884, V, 1, 1, 1, 1, 0, 704, 100
45885, V, 1, 1, 1, 1, 0, 704, 100
45886, V, 1, 1, 1, 1, 0, 704, 100
45887, V, 1, 1, 1, 1, 0, 704, 100
45888, V, 1, 1, 1, 1, 0, 704, 100
45889, V, 1, 1, 1, 1, 0, 704, 100
45890, V, 1, 1, 1, 1, 0, 704, 100
45891, V, 1, 1, 1, 1, 0, 704, 100
45892, V, 1, 1, 1, 1, 0, 704, 100
45893, V, 1, 1, 1, 1, 0, 704, 100
45894, V, 1, 1, 1, 1, 0, 704, 100
45895, V, 1, 1, 1, 1, 0, 704, 100
45896, V, 1, 1, 1, 1, 0, 704, 100
45897, V, 1, 1, 1, 1, 0, 704, 100
45898, V, 1, 1, 1, 1, 0, 704, 100
45899, V, 1, 1, 1, 1, 0, 704, 100
45900, V, 1, 1, 1, 1, 0, 704, 100
45901, V, 1, 1, 1, 1, 0, 704, 100
45902, V, 1, 1, 1, 1, 0, 704, 100
45903, V, 1, 1, 1, 1, 0, 704, 100
45904, V, 1, 1, 1, 1, 0, 704, 100
45905, V, 1, 1, 1, 1, 0, 704, 100
45906, V, 1, 1, 1, 1, 0, 704, 100
45907, V, 1, 1, 1, 1, 0, 704, 100
45908, V, 1, 1, 1, 1, 0, 704, 100
45910, V, 1, 1, 1, 1, 0, 704, 100
45911, V, 1, 1, 1, 1, 0, 704, 100
45912, V, 1, 1, 1, 1, 0, 704, 100
45913, V, 1, 1, 1, 1, 0, 704, 100
45914, V, 1, 1, 1, 1, 0, 704, 100
45915, V, 1, 1, 1, 1, 0, 704, 100
45916, V, 1, 1, 1, 1, 0, 704, 100
45917, V, 1, 1, 1, 1, 0, 704, 100
45918, V, 1, 1, 1, 1, 0, 704, 100
45919, V, 1, 1, 1, 1, 0, 704, 100
45920, V, 1, 1, 1, 1, 0, 704, 100
45921, V, 1, 1, 1, 1, 0, 704, 100
45922, V, 1, 1, 1, 1, 0, 704, 100
45923, V, 1, 1, 1, 1, 0, 704, 100
45924, V, 1, 1, 1, 1, 0, 704, 100
45925, V, 1, 1, 1, 1, 0, 704, 100
45926, V, 1, 1, 1, 1, 0, 704, 100
45927, V, 1, 1, 1, 1, 0, 704, 100
45928, V, 1, 1, 1, 1, 0, 704, 100
45929, V, 1, 1, 1, 1, 0, 704, 100
45930, V, 1, 1, 1, 1, 0, 704, 100
45931, V, 1, 1, 1, 1, 0, 704, 100
45932, V, 1, 1, 1, 1, 0, 704, 100
45933, V, 1, 1, 1, 1, 0, 704, 100
45934, V, 1, 1, 1, 1, 0, 704, 100
45935, V, 1, 1, 1, 1, 0, 704, 100
45936, V, 1, 1, 1, 1, 0, 704, 100
45937, V, 1, 1, 1, 1, 0, 704, 100
45938, V, 1, 1, 1, 1, 0, 704, 99
45939, V, 1, 1, 1, 1, 0, 704, 100
45940, V, 1, 1, 1, 1, 0, 704, 100
45941, V, 1, 1, 1, 1, 0, 704, 100
45942, V, 1, 1, 1, 1, 0, 704, 99
45943, V, 1, 1, 1, 1, 0, 704, 100
45944, V, 1, 1, 1, 1, 0, 704, 99
45945, V, 1, 1, 1, 1, 0, 704, 100
45946, V, 1, 1, 1, 1, 0, 704, 100
45947, V, 1, 1, 1, 1, 0, 704, 100
45948, V, 1, 1, 1, 1, 0, 704, 100
45949, V, 1, 1, 1, 1, 0, 704, 100
45950, V, 1, 1, 1, 1, 0, 704, 100
45952, V, 1, 1, 1, 1, 0, 704, 100
45953, V, 1, 1, 1, 1, 0, 704, 100
45954, V, 1, 1, 1, 1, 0, 704, 100
45955, V, 1, 1, 1, 1, 0, 704, 100
45956, V, 1, 1, 1, 1, 0, 704, 100
45957, V, 1, 1, 1, 1, 0, 704, 100
45958, V, 1, 1, 1, 1, 0, 704, 100
45959, V, 1, 1, 1, 1, 0, 704, 100
45960, V, 1, 1, 1, 1, 0, 704, 100
45961, V, 1, 1, 1, 1, 0, 704, 100
45962, V, 1, 1, 1, 1, 0, 704, 100
45963, V, 1, 1, 1, 1, 0, 704, 99
45964, V, 1, 1, 1, 1, 0, 704, 100
45965, V, 1, 1, 1, 1, 0, 704, 100
45966, V, 1, 1, 1, 1, 0, 704, 100
45967, V, 1, 1, 1, 1, 0, 704, 100
45968, V, 1, 1, 1, 1, 0, 704, 100
45969, V, 1, 1, 1, 1, 0, 704, 100
45970, V, 1, 1, 1, 1, 0, 704, 100
45971, V, 1, 1, 1, 1, 0, 704, 100
45972, V, 1, 1, 1, 1, 0, 704, 100
45973, V, 1, 1, 1, 1, 0, 704, 100
45974, V, 1, 1, 1, 1, 0, 704, 100
45975, V, 1, 1, 1, 1, 0, 704, 100
45976, V, 1, 1, 1, 1, 0, 704, 100
45977, V, 1, 1, 1, 1, 0, 704, 100
45978, V, 1, 1, 1, 1, 0, 704, 100
45979, V, 1, 1, 1, 1, 0, 704, 100
45980, V, 1, 1, 1, 1, 0, 704, 100
45981, V, 1, 1, 1, 1, 0, 704, 100
45982, V, 1, 1, 1, 1, 0, 704, 100
45983, V, 1, 1, 1, 1, 0, 704, 100
45984, V, 1, 1, 1, 1, 0, 704, 100
45985, V, 1, 1, 1, 1, 0, 704, 100
45986, V, 1, 1, 1, 1, 0, 704, 100
45987, V, 1, 1, 1, 1, 0, 704, 100
45988, V, 1, 1, 1, 1, 0, 704, 100
45989, V, 1, 1, 1, 1, 0, 704, 100
45990, V, 1, 1, 1, 1, 0, 704, 100
45991, V, 1, 1, 1, 1, 0, 704, 100
45992, V, 1, 1, 1, 1, 0, 704, 100
45993, V, 1, 1, 1, 1, 0, 704, 100
45995, V, 1, 1, 1, 1, 0, 704, 100
45996, V, 1, 1, 1, 1, 0, 704, 100
45997, V, 1, 1, 1, 1, 0, 704, 100
45998, V, 1, 1, 1, 1, 0, 704, 100
45999, V, 1, 1, 1, 1, 0, 704, 100
46000, V, 1, 1, 1, 1, 0, 704, 100
46001, V, 1, 1, 1, 1, 0, 704, 100
46002, V, 1, 1, 1, 1, 0, 704, 100
46003, V, 1, 1, 1, 1, 0, 704, 100
46004, V, 1, 1, 1, 1, 0, 704, 100
46005, V, 1, 1, 1, 1, 0, 704, 99
46006, V, 1, 1, 1, 1, 0, 704, 100
46007, V, 1, 1, 1, 1, 0, 704, 100
46008, V, 1, 1, 1, 1, 0, 704, 100
46009, V, 1, 1, 1, 1, 0, 704, 100
46010, V, 1, 1, 1, 1, 0, 704, 100
46011, V, 1, 1, 1, 1, 0, 704, 100
46012, V, 1, 1, 1, 1, 0, 704, 100
46013, V, 1, 1, 1, 1, 0, 704, 100
46014, V, 1, 1, 1, 1, 0, 704, 100
46015, V, 1, 1, 1, 1, 0, 704, 100
46016, V, 1, 1, 1, 1, 0, 704, 100
46017, V, 1, 1, 1, 1, 0, 704, 99
46018, V, 1, 1, 1, 1, 0, 704, 99
46019, V, 1, 1, 1, 1, 0, 704, 99
46020, V, 1, 1, 1, 1, 0, 704, 100
46021, V, 1, 1, 1, 1, 0, 704, 100
46022, V, 1, 1, 1, 1, 0, 704, 100
46023, V, 1, 1, 1, 1, 0, 704, 100
46024, V, 1, 1, 1, 1, 0, 704, 100
46025, V, 1, 1, 1, 1, 0, 704, 100
46026, V, 1, 1, 1, 1, 0, 704, 100
46027, V, 1, 1, 1, 1, 0, 704, 100
46028, V, 1, 1, 1, 1, 0, 704, 100
46029, V, 1, 1, 1, 1, 0, 704, 99
46030, V, 1, 1, 1, 1, 0, 704, 100
46031, V, 1, 1, 1, 1, 0, 704, 100
46032, V, 1, 1, 1, 1, 0, 704, 100
46033, V, 1, 1, 1, 1, 0, 704, 100
46034, V, 1, 1, 1, 1, 0, 704, 99
46035, V, 1, 1, 1, 1, 0, 704, 100
46036, V, 1, 1, 1, 1, 0, 704, 100
46038, V, 1, 1, 1, 1, 0, 704, 100
46039, V, 1, 1, 1, 1, 0, 704, 100
46040, V, 1, 1, 1, 1, 0, 704, 100
46041, V, 1, 1, 1, 1, 0, 704, 100
46042, V, 1, 1, 1, 1, 0, 704, 100
46043, V, 1, 1, 1, 1, 0, 704, 100
46044, V, 1, 1, 1, 1, 0, 704, 100
46045, V, 1, 1, 1, 1, 0, 704, 100
46046, V, 1, 1, 1, 1, 0, 704, 100
46047, V, 1, 1, 1, 1, 0, 704, 100
46048, V, 1, 1, 1, 1, 0, 704, 100
46049, V, 1, 1, 1, 1, 0, 704, 100
46050, V, 1, 1, 1, 1, 0, 704, 100
46051, V, 1, 1, 1, 1, 0, 704, 100
46052, V, 1, 1, 1, 1, 0, 704, 100
46053, V, 1, 1, 1, 1, 0, 704, 100
46054, V, 1, 1, 1, 1, 0, 704, 100
46055, V, 1, 1, 1, 1, 0, 704, 100
46056, V, 1, 1, 1, 1, 0, 704, 100
46057, V, 1, 1, 1, 1, 0, 704, 100
46058, V, 1, 1, 1, 1, 0, 704, 100
46059, V, 1, 1, 1, 1, 0, 704, 100
46060, V, 1, 1, 1, 1, 0, 704, 100
46061, V, 1, 1, 1, 1, 0, 704, 100
46062, V, 1, 1, 1, 1, 0, 704, 100
46063, V, 1, 1, 1, 1, 0, 704, 100
46064, V, 1, 1, 1, 1, 0, 704, 100
46065, V, 1, 1, 1, 1, 0, 704, 100
46066, V, 1, 1, 1, 1, 0, 704, 100
46067, V, 1, 1, 1, 1, 0, 704, 100
46068, V, 1, 1, 1, 1, 0, 704, 100
46069, V, 1, 1, 1, 1, 0, 704, 100
46070, V, 1, 1, 1, 1, 0, 704, 100
46071, V, 1, 1, 1, 1, 0, 704, 100
46072, V, 1, 1, 1, 1, 0, 704, 100
46073, V, 1, 1, 1, 1, 0, 704, 100
46074, V, 1, 1, 1, 1, 0, 704, 100
46075, V, 1, 1, 1, 1, 0, 704, 100
46076, V, 1, 1, 1, 1, 0, 704, 100
46077, V, 1, 1, 1, 1, 0, 704, 100
46078, V, 1, 1, 1, 1, 0, 704, 100
46080, V, 1, 1, 1, 1, 0, 704, 100
46081, V, 1, 1, 1, 1, 0, 704, 100
46082, V, 1, 1, 1, 1, 0, 704, 100
46083, V, 1, 1, 1, 1, 0, 704, 100
46084, V, 1, 1, 1, 1, 0, 704, 100
46085, V, 1, 1, 1, 1, 0, 704, 100
46086, V, 1, 1, 1, 1, 0, 704, 100
46087, V, 1, 1, 1, 1, 0, 704, 100
46088, V, 1, 1, 1, 1, 0, 704, 100
46089, V, 1, 1, 1, 1, 0, 704, 100
46090, V, 1, 1, 1, 1, 0, 704, 100
46091, V, 1, 1, 1, 1, 0, 704, 100
46092, V, 1, 1, 1, 1, 0, 704, 100
46093, V, 1, 1, 1, 1, 0, 704, 100
46094, V, 1, 1, 1, 1, 0, 704, 100
46095, V, 1, 1, 1, 1, 0, 704, 100
46096, V, 1, 1, 1, 1, 0, 704, 100
46097, V, 1, 1, 1, 1, 0, 704, 100
46098, V, 1, 1, 1, 1, 0, 704, 99
46099, V, 1, 1, 1, 1, 0, 704, 100
46100, V, 1, 1, 1, 1, 0, 704, 100
46101, V, 1, 1, 1, 1, 0, 704, 100
46102, V, 1, 1, 1, 1, 0, 704, 100
46103, V, 1, 1, 1, 1, 0, 704, 100
46104, V, 1, 1, 1, 1, 0, 704, 100
46105, V, 1, 1, 1, 1, 0, 704, 100
46106, V, 1, 1, 1, 1, 0, 704, 100
46107, V, 1, 1, 1, 1, 0, 704, 100
46108, V, 1, 1, 1, 1, 0, 704, 100
46109, V, 1, 1, 1, 1, 0, 704, 100
46110, V, 1, 1, 1, 1, 0, 704, 100
46111, V, 1, 1, 1, 1, 0, 704, 100
46112, V, 1, 1, 1, 1, 0, 704, 100
46113, V, 1, 1, 1, 1, 0, 704, 100
46114, V, 1, 1, 1, 1, 0, 704, 100
46115, V, 1, 1, 1, 1, 0, 704, 100
46116, V, 1, 1, 1, 1, 0, 704, 100
46117, V, 1, 1, 1, 1, 0, 704, 100
46118, V, 1, 1, 1, 1, 0, 704, 100
46119, V, 1, 1, 1, 1, 0, 704, 100
46120, V, 1, 1, 1, 1, 0, 704, 100
46121, V, 1, 1, 1, 1, 0, 704, 100
46123, V, 1, 1, 1, 1, 0, 704, 100
46124, V, 1, 1, 1, 1, 0, 704, 100
46125, V, 1, 1, 1, 1, 0, 704, 100
46126, V, 1, 1, 1, 1, 0, 704, 100
46127, V, 1, 1, 1, 1, 0, 704, 100
46128, V, 1, 1, 1, 1, 0, 704, 100
46129, V, 1, 1, 1, 1, 0, 704, 100
46130, V, 1, 1, 1, 1, 0, 704, 100
46131, V, 1, 1, 1, 1, 0, 704, 100
46132, V, 1, 1, 1, 1, 0, 704, 100
46133, V, 1, 1, 1, 1, 0, 704, 100
46134, V, 1, 1, 1, 1, 0, 704, 100
46135, V, 1, 1, 1, 1, 0, 704, 100
46136, V, 1, 1, 1, 1, 0, 704, 100
46137, V, 1, 1, 1, 1, 0, 704, 100
46138, V, 1, 1, 1, 1, 0, 704, 100
46139, V, 1, 1, 1, 1, 0, 704, 100
46140, V, 1, 1, 1, 1, 0, 704, 100
46141, V, 1, 1, 1, 1, 0, 704, 100
46142, V, 1, 1, 1, 1, 0, 704, 100
46143, V, 1, 1, 1, 1, 0, 704, 100
46144, V, 1, 1, 1, 1, 0, 704, 100
46145, V, 1, 1, 1, 1, 0, 704, 100
46146, V, 1, 1, 1, 1, 0, 704, 100
46147, V, 1, 1, 1, 1, 0, 704, 100
46148, V, 1, 1, 1, 1, 0, 704, 100
46149, V, 1, 1, 1, 1, 0, 704, 100
46150, V, 1, 1, 1, 1, 0, 704, 100
46151, V, 1, 1, 1, 1, 0, 704, 100
46152, V, 1, 1, 1, 1, 0, 704, 100
46153, V, 1, 1, 1, 1, 0, 704, 100
46154, V, 1, 1, 1, 1, 0, 704, 100
46155, V, 1, 1, 1, 1, 0, 704, 100
46156, V, 1, 1, 1, 1, 0, 704, 100
46157, V, 1, 1, 1, 1, 0, 704, 100
46158, V, 1, 1, 1, 1, 0, 704, 100
46159, V, 1, 1, 1, 1, 0, 704, 100
46160, V, 1, 1, 1, 1, 0, 704, 100
46161, V, 1, 1, 1, 1, 0, 704, 100
46162, V, 1, 1, 1, 1, 0, 704, 100
46163, V, 1, 1, 1, 1, 0, 704, 100
46164, V, 1, 1, 1, 1, 0, 704, 100
46166, V, 1, 1, 1, 1, 0, 704, 100
46167, V, 1, 1, 1, 1, 0, 704, 100
46168, V, 1, 1, 1, 1, 0, 704, 100
46169, V, 1, 1, 1, 1, 0, 704, 100
46170, V, 1, 1, 1, 1, 0, 704, 100
46171, V, 1, 1, 1, 1, 0, 704, 100
46172, V, 1, 1, 1, 1, 0, 704, 100
46173, V, 1, 1, 1, 1, 0, 704, 100
46174, V, 1, 1, 1, 1, 0, 704, 99
46175, V, 1, 1, 1, 1, 0, 704, 100
46176, V, 1, 1, 1, 1, 0, 704, 99
46177, V, 1, 1, 1, 1, 0, 704, 100
46178, V, 1, 1, 1, 1, 0, 704, 100
46179, V, 1, 1, 1, 1, 0, 704, 100
46180, V, 1, 1, 1, 1, 0, 704, 100
46181, V, 1, 1, 1, 1, 0, 704, 100
46182, V, 1, 1, 1, 1, 0, 704, 99
46183, V, 1, 1, 1, 1, 0, 704, 100
46184, V, 1, 1, 1, 1, 0, 704, 100
46185, V, 1, 1, 1, 1, 0, 704, 100
46186, V, 1, 1, 1, 1, 0, 704, 100
46187, V, 1, 1, 1, 1, 0, 704, 100
46188, V, 1, 1, 1, 1, 0, 704, 100
46189, V, 1, 1, 1, 1, 0, 704, 100
46190, V, 1, 1, 1, 1, 0, 704, 100
46191, V, 1, 1, 1, 1, 0, 704, 100
46192, V, 1, 1, 1, 1, 0, 704, 100
46193, V, 1, 1, 1, 1, 0, 704, 100
46194, V, 1, 1, 1, 1, 0, 704, 100
46195, V, 1, 1, 1, 1, 0, 704, 100
46196, V, 1, 1, 1, 1, 0, 704, 100
46197, V, 1, 1, 1, 1, 0, 704, 100
46198, V, 1, 1, 1, 1, 0, 704, 100
46199, V, 1, 1, 1, 1, 0, 704, 100
46200, V, 1, 1, 1, 1, 0, 704, 100
46201, V, 1, 1, 1, 1, 0, 704, 100
46202, V, 1, 1, 1, 1, 0, 704, 100
46203, V, 1, 1, 1, 1, 0, 704, 100
46204, V, 1, 1, 1, 1, 0, 704, 100
46205, V, 1, 1, 1, 1, 0, 704, 100
46206, V, 1, 1, 1, 1, 0, 704, 100
46208, V, 1, 1, 1, 1, 0, 704, 100
46209, V, 1, 1, 1, 1, 0, 704, 100
46210, V, 1, 1, 1, 1, 0, 704, 100
46211, V, 1, 1, 1, 1, 0, 704, 100
46212, V, 1, 1, 1, 1, 0, 704, 100
46213, V, 1, 1, 1, 1, 0, 704, 100
46214, V, 1, 1, 1, 1, 0, 704, 100
46215, V, 1, 1, 1, 1, 0, 704, 100
46216, V, 1, 1, 1, 1, 0, 704, 100
46217, V, 1, 1, 1, 1, 0, 704, 100
46218, V, 1, 1, 1, 1, 0, 704, 100
46219, V, 1, 1, 1, 1, 0, 704, 100
46220, V, 1, 1, 1, 1, 0, 704, 100
46221, V, 1, 1, 1, 1, 0, 704, 100
46222, V, 1, 1, 1, 1, 0, 704, 100
46223, V, 1, 1, 1, 1, 0, 704, 100
46224, V, 1, 1, 1, 1, 0, 704, 100
46225, V, 1, 1, 1, 1, 0, 704, 100
46226, V, 1, 1, 1, 1, 0, 704, 100
46227, V, 1, 1, 1, 1, 0, 704, 100
46228, V, 1, 1, 1, 1, 0, 704, 100
46229, V, 1, 1, 1, 1, 0, 704, 100
46230, V, 1, 1, 1, 1, 0, 704, 100
46231, V, 1, 1, 1, 1, 0, 704, 99
46232, V, 1, 1, 1, 1, 0, 704, 99
46233, V, 1, 1, 1, 1, 0, 704, 99
46234, V, 1, 1, 1, 1, 0, 704, 99
46235, V, 1, 1, 1, 1, 0, 704, 99
46236, V, 1, 1, 1, 1, 0, 704, 99
46237, V, 1, 1, 1, 1, 0, 704, 99
46238, V, 1, 1, 1, 1, 0, 704, 99
46239, V, 1, 1, 1, 1, 0, 704, 99
46240, V, 1, 1, 1, 1, 0, 704, 99
46241, V, 1, 1, 1, 1, 0, 704, 99
46242, V, 1, 1, 1, 1, 0, 704, 99
46243, V, 1, 1, 1, 1, 0, 704, 99
46244, V, 1, 1, 1, 1, 0, 704, 99
46245, V, 1, 1, 1, 1, 0, 704, 99
46246, V, 1, 1, 1, 1, 0, 704, 99
46247, V, 1, 1, 1, 1, 0, 704, 99
46248, V, 1, 1, 1, 1, 0, 704, 99
46249, V, 1, 1, 1, 1, 0, 704, 99
46251, V, 1, 1, 1, 1, 0, 704, 99
46252, V, 1, 1, 1, 1, 0, 704, 99
46253, V, 1, 1, 1, 1, 0, 704, 99
46254, V, 1, 1, 1, 1, 0, 704, 99
46255, V, 1, 1, 1, 1, 0, 704, 99
46256, V, 1, 1, 1, 1, 0, 704, 99
46257, V, 1, 1, 1, 1, 0, 704, 99
46258, V, 1, 1, 1, 1, 0, 704, 99
46259, V, 1, 1, 1, 1, 0, 704, 99
46260, V, 1, 1, 1, 1, 0, 704, 99
46261, V, 1, 1, 1, 1, 0, 704, 99
46262, V, 1, 1, 1, 1, 0, 704, 99
46263, V, 1, 1, 1, 1, 0, 704, 99
46264, V, 1, 1, 1, 1, 0, 704, 100
46265, V, 1, 1, 1, 1, 0, 704, 99
46266, V, 1, 1, 1, 1, 0, 704, 100
46267, V, 1, 1, 1, 1, 0, 704, 99
46268, V, 1, 1, 1, 1, 0, 704, 99
46269, V, 1, 1, 1, 1, 0, 704, 100
46270, V, 1, 1, 1, 1, 0, 704, 100
46271, V, 1, 1, 1, 1, 0, 704, 100
46272, V, 1, 1, 1, 1, 0, 704, 100
46273, V, 1, 1, 1, 1, 0, 704, 100
46274, V, 1, 1, 1, 1, 0, 704, 100
46275, V, 1, 1, 1, 1, 0, 704, 100
46276, V, 1, 1, 1, 1, 0, 704, 100
46277, V, 1, 1, 1, 1, 0, 704, 100
46278, V, 1, 1, 1, 1, 0, 704, 100
46279, V, 1, 1, 1, 1, 0, 704, 100
46280, V, 1, 1, 1, 1, 0, 704, 100
46281, V, 1, 1, 1, 1, 0, 704, 100
46282, V, 1, 1, 1, 1, 0, 704, 100
46283, V, 1, 1, 1, 1, 0, 704, 100
46284, V, 1, 1, 1, 1, 0, 704, 100
46285, V, 1, 1, 1, 1, 0, 704, 100
46286, V, 1, 1, 1, 1, 0, 704, 100
46287, V, 1, 1, 1, 1, 0, 704, 100
46288, V, 1, 1, 1, 1, 0, 704, 100
46289, V, 1, 1, 1, 1, 0, 704, 100
46290, V, 1, 1, 1, 1, 0, 704, 100
46291, V, 1, 1, 1, 1, 0, 704, 100
46292, V, 1, 1, 1, 1, 0, 704, 100
46294, V, 1, 1, 1, 1, 0, 704, 100
46295, V, 1, 1, 1, 1, 0, 704, 100
46296, V, 1, 1, 1, 1, 0, 704, 100
46297, V, 1, 1, 1, 1, 0, 704, 100
46298, V, 1, 1, 1, 1, 0, 704, 100
46299, V, 1, 1, 1, 1, 0, 704, 100
46300, V, 1, 1, 1, 1, 0, 704, 100
46301, V, 1, 1, 1, 1, 0, 704, 100
46302, V, 1, 1, 1, 1, 0, 704, 100
46303, V, 1, 1, 1, 1, 0, 704, 100
46304, V, 1, 1, 1, 1, 0, 704, 100
46305, V, 1, 1, 1, 1, 0, 704, 100
46306, V, 1, 1, 1, 1, 0, 704, 100
46307, V, 1, 1, 1, 1, 0, 704, 100
46308, V, 1, 1, 1, 1, 0, 704, 100
46309, V, 1, 1, 1, 1, 0, 704, 100
46310, V, 1, 1, 1, 1, 0, 704, 100
46311, V, 1, 1, 1, 1, 0, 704, 99
46312, V, 1, 1, 1, 1, 0, 704, 100
46313, V, 1, 1, 1, 1, 0, 704, 100
46314, V, 1, 1, 1, 1, 0, 704, 100
46315, V, 1, 1, 1, 1, 0, 704, 100
46316, V, 1, 1, 1, 1, 0, 704, 99
46317, V, 1, 1, 1, 1, 0, 704, 99
46318, V, 1, 1, 1, 1, 0, 704, 99
46319, V, 1, 1, 1, 1, 0, 704, 100
46320, V, 1, 1, 1, 1, 0, 704, 99
46321, V, 1, 1, 1, 1, 0, 704, 99
46322, V, 1, 1, 1, 1, 0, 704, 99
46323, V, 1, 1, 1, 1, 0, 704, 99
46324, V, 1, 1, 1, 1, 0, 704, 99
46325, V, 1, 1, 1, 1, 0, 704, 99
46326, V, 1, 1, 1, 1, 0, 704, 99
46327, V, 1, 1, 1, 1, 0, 704, 100
46328, V, 1, 1, 1, 1, 0, 704, 99
46329, V, 1, 1, 1, 1, 0, 704, 99
46330, V, 1, 1, 1, 1, 0, 704, 99
46331, V, 1, 1, 1, 1, 0, 704, 99
46332, V, 1, 1, 1, 1, 0, 704, 99
46333, V, 1, 1, 1, 1, 0, 704, 100
46334, V, 1, 1, 1, 1, 0, 704, 99
46336, V, 1, 1, 1, 1, 0, 704, 99
46337, V, 1, 1, 1, 1, 0, 704, 99
46338, V, 1, 1, 1, 1, 0, 704, 99
46339, V, 1, 1, 1, 1, 0, 704, 99
46340, V, 1, 1, 1, 1, 0, 704, 100
46341, V, 1, 1, 1, 1, 0, 704, 99
46342, V, 1, 1, 1, 1, 0, 704, 100
46343, V, 1, 1, 1, 1, 0, 704, 100
46344, V, 1, 1, 1, 1, 0, 704, 99
46345, V, 1, 1, 1, 1, 0, 704, 100
46346, V, 1, 1, 1, 1, 0, 704, 100
46347, V, 1, 1, 1, 1, 0, 704, 100
46348, V, 1, 1, 1, 1, 0, 704, 100
46349, V, 1, 1, 1, 1, 0, 704, 100
46350, V, 1, 1, 1, 1, 0, 704, 100
46351, V, 1, 1, 1, 1, 0, 704, 100
46352, V, 1, 1, 1, 1, 0, 704, 100
46353, V, 1, 1, 1, 1, 0, 704, 100
46354, V, 1, 1, 1, 1, 0, 704, 100
46355, V, 1, 1, 1, 1, 0, 704, 100
46356, V, 1, 1, 1, 1, 0, 704, 100
46357, V, 1, 1, 1, 1, 0, 704, 100
46358, V, 1, 1, 1, 1, 0, 704, 100
46359, V, 1, 1, 1, 1, 0, 704, 100
46360, V, 1, 1, 1, 1, 0, 704, 100
46361, V, 1, 1, 1, 1, 0, 704, 100
46362, V, 1, 1, 1, 1, 0, 704, 100
46363, V, 1, 1, 1, 1, 0, 704, 100
46364, V, 1, 1, 1, 1, 0, 704, 100
46365, V, 1, 1, 1, 1, 0, 704, 100
46366, V, 1, 1, 1, 1, 0, 704, 100
46367, V, 1, 1, 1, 1, 0, 704, 100
46368, V, 1, 1, 1, 1, 0, 704, 100
46369, V, 1, 1, 1, 1, 0, 704, 100
46370, V, 1, 1, 1, 1, 0, 704, 100
46371, V, 1, 1, 1, 1, 0, 704, 100
46372, V, 1, 1, 1, 1, 0, 704, 100
46373, V, 1, 1, 1, 1, 0, 704, 100
46374, V, 1, 1, 1, 1, 0, 704, 100
46375, V, 1, 1, 1, 1, 0, 704, 100
46376, V, 1, 1, 1, 1, 0, 704, 100
46377, V, 1, 1, 1, 1, 0, 704, 100
46379, V, 1, 1, 1, 1, 0, 704, 100
46380, V, 1, 1, 1, 1, 0, 704, 100
46381, V, 1, 1, 1, 1, 0, 704, 100
46382, V, 1, 1, 1, 1, 0, 704, 100
46383, V, 1, 1, 1, 1, 0, 704, 100
46384, V, 1, 1, 1, 1, 0, 704, 100
46385, V, 1, 1, 1, 1, 0, 704, 100
46386, V, 1, 1, 1, 1, 0, 704, 100
46387, V, 1, 1, 1, 1, 0, 704, 100
46388, V, 1, 1, 1, 1, 0, 704, 100
46389, V, 1, 1, 1, 1, 0, 704, 100
46390, V, 1, 1, 1, 1, 0, 704, 100
46391, V, 1, 1, 1, 1, 0, 704, 100
46392, V, 1, 1, 1, 1, 0, 704, 100
46393, V, 1, 1, 1, 1, 0, 704, 100
46394, V, 1, 1, 1, 1, 0, 704, 100
46395, V, 1, 1, 1, 1, 0, 704, 100
46396, V, 1, 1, 1, 1, 0, 704, 99
46397, V, 1, 1, 1, 1, 0, 704, 99
46398, V, 1, 1, 1, 1, 0, 704, 100
46399, V, 1, 1, 1, 1, 0, 704, 99
46400, V, 1, 1, 1, 1, 0, 704, 100
46401, V, 1, 1, 1, 1, 0, 704, 100
46402, V, 1, 1, 1, 1, 0, 704, 99
46403, V, 1, 1, 1, 1, 0, 704, 100
46404, V, 1, 1, 1, 1, 0, 704, 100
46405, V, 1, 1, 1, 1, 0, 704, 100
46406, V, 1, 1, 1, 1, 0, 704, 100
46407, V, 1, 1, 1, 1, 0, 704, 100
46408, V, 1, 1, 1, 1, 0, 704, 100
46409, V, 1, 1, 1, 1, 0, 704, 99
46410, V, 1, 1, 1, 1, 0, 704, 100
46411, V, 1, 1, 1, 1, 0, 704, 100
46412, V, 1, 1, 1, 1, 0, 704, 100
46413, V, 1, 1, 1, 1, 0, 704, 99
46414, V, 1, 1, 1, 1, 0, 704, 99
46415, V, 1, 1, 1, 1, 0, 704, 100
46416, V, 1, 1, 1, 1, 0, 704, 100
46417, V, 1, 1, 1, 1, 0, 704, 100
46418, V, 1, 1, 1, 1, 0, 704, 100
46419, V, 1, 1, 1, 1, 0, 704, 100
46420, V, 1, 1, 1, 1, 0, 704, 100
46422, V, 1, 1, 1, 1, 0, 704, 100
46423, V, 1, 1, 1, 1, 0, 704, 100
46424, V, 1, 1, 1, 1, 0, 704, 100
46425, V, 1, 1, 1, 1, 0, 704, 100
46426, V, 1, 1, 1, 1, 0, 704, 100
46427, V, 1, 1, 1, 1, 0, 704, 100
46428, V, 1, 1, 1, 1, 0, 704, 100
46429, V, 1, 1, 1, 1, 0, 704, 100
46430, V, 1, 1, 1, 1, 0, 704, 100
46431, V, 1, 1, 1, 1, 0, 704, 100
46432, V, 1, 1, 1, 1, 0, 704, 100
46433, V, 1, 1, 1, 1, 0, 704, 100
46434, V, 1, 1, 1, 1, 0, 704, 100
46435, V, 1, 1, 1, 1, 0, 704, 100
46436, V, 1, 1, 1, 1, 0, 704, 100
46437, V, 1, 1, 1, 1, 0, 704, 100
46438, V, 1, 1, 1, 1, 0, 704, 100
46439, V, 1, 1, 1, 1, 0, 704, 100
46440, V, 1, 1, 1, 1, 0, 704, 100
46441, V, 1, 1, 1, 1, 0, 704, 100
46442, V, 1, 1, 1, 1, 0, 704, 100
46443, V, 1, 1, 1, 1, 0, 704, 100
46444, V, 1, 1, 1, 1, 0, 704, 100
46445, V, 1, 1, 1, 1, 0, 704, 100
46446, V, 1, 1, 1, 1, 0, 704, 100
46447, V, 1, 1, 1, 1, 0, 704, 100
46448, V, 1, 1, 1, 1, 0, 704, 100
46449, V, 1, 1, 1, 1, 0, 704, 100
46450, V, 1, 1, 1, 1, 0, 704, 100
46451, V, 1, 1, 1, 1, 0, 704, 100
46452, V, 1, 1, 1, 1, 0, 704, 100
46453, V, 1, 1, 1, 1, 0, 704, 100
46454, V, 1, 1, 1, 1, 0, 704, 100
46455, V, 1, 1, 1, 1, 0, 704, 100
46456, V, 1, 1, 1, 1, 0, 704, 100
46457, V, 1, 1, 1, 1, 0, 704, 99
46458, V, 1, 1, 1, 1, 0, 704, 100
46459, V, 1, 1, 1, 1, 0, 704, 100
46460, V, 1, 1, 1, 1, 0, 704, 100
46461, V, 1, 1, 1, 1, 0, 704, 100
46462, V, 1, 1, 1, 1, 0, 704, 100
46464, V, 1, 1, 1, 1, 0, 704, 100
46465, V, 1, 1, 1, 1, 0, 704, 100
46466, V, 1, 1, 1, 1, 0, 704, 100
46467, V, 1, 1, 1, 1, 0, 704, 100
46468, V, 1, 1, 1, 1, 0, 704, 100
46469, V, 1, 1, 1, 1, 0, 704, 99
46470, V, 1, 1, 1, 1, 0, 704, 99
46471, V, 1, 1, 1, 1, 0, 704, 99
46472, V, 1, 1, 1, 1, 0, 704, 99
46473, V, 1, 1, 1, 1, 0, 704, 99
46474, V, 1, 1, 1, 1, 0, 704, 99
46475, V, 1, 1, 1, 1, 0, 704, 99
46476, V, 1, 1, 1, 1, 0, 704, 99
46477, V, 1, 1, 1, 1, 0, 704, 99
46478, V, 1, 1, 1, 1, 0, 704, 99
46479, V, 1, 1, 1, 1, 0, 704, 99
46480, V, 1, 1, 1, 1, 0, 704, 99
46481, V, 1, 1, 1, 1, 0, 704, 99
46482, V, 1, 1, 1, 1, 0, 704, 99
46483, V, 1, 1, 1, 1, 0, 704, 99
46484, V, 1, 1, 1, 1, 0, 704, 99
46485, V, 1, 1, 1, 1, 0, 704, 99
46486, V, 1, 1, 1, 1, 0, 704, 99
46487, V, 1, 1, 1, 1, 0, 704, 99
46488, V, 1, 1, 1, 1, 0, 704, 99
46489, V, 1, 1, 1, 1, 0, 704, 99
46490, V, 1, 1, 1, 1, 0, 704, 99
46491, V, 1, 1, 1, 1, 0, 704, 99
46492, V, 1, 1, 1, 1, 0, 704, 99
46493, V, 1, 1, 1, 1, 0, 704, 99
46494, V, 1, 1, 1, 1, 0, 704, 99
46495, V, 1, 1, 1, 1, 0, 704, 99
46496, V, 1, 1, 1, 1, 0, 704, 99
46497, V, 1, 1, 1, 1, 0, 704, 99
46498, V, 1, 1, 1, 1, 0, 704, 99
46499, V, 1, 1, 1, 1, 0, 704, 99
46500, V, 1, 1, 1, 1, 0, 704, 99
46501, V, 1, 1, 1, 1, 0, 704, 99
46502, V, 1, 1, 1, 1, 0, 704, 99
46503, V, 1, 1, 1, 1, 0, 704, 99
46504, V, 1, 1, 1, 1, 0, 704, 100
46505, V, 1, 1, 1, 1, 0, 704, 99
46507, V, 1, 1, 1, 1, 0, 704, 99
46508, V, 1, 1, 1, 1, 0, 704, 99
46509, V, 1, 1, 1, 1, 0, 704, 100
46510, V, 1, 1, 1, 1, 0, 704, 99
46511, V, 1, 1, 1, 1, 0, 704, 99
46512, V, 1, 1, 1, 1, 0, 704, 100
46513, V, 1, 1, 1, 1, 0, 704, 99
46514, V, 1, 1, 1, 1, 0, 704, 100
46515, V, 1, 1, 1, 1, 0, 704, 99
46516, V, 1, 1, 1, 1, 0, 704, 99
46517, V, 1, 1, 1, 1, 0, 704, 99
46518, V, 1, 1, 1, 1, 0, 704, 99
46519, V, 1, 1, 1, 1, 0, 704, 99
46520, V, 1, 1, 1, 1, 0, 704, 99
46521, V, 1, 1, 1, 1, 0, 704, 99
46522, V, 1, 1, 1, 1, 0, 704, 99
46523, V, 1, 1, 1, 1, 0, 704, 100
46524, V, 1, 1, 1, 1, 0, 704, 100
46525, V, 1, 1, 1, 1, 0, 704, 99
46526, V, 1, 1, 1, 1, 0, 704, 99
46527, V, 1, 1, 1, 1, 0, 704, 100
46528, V, 1, 1, 1, 1, 0, 704, 99
46529, V, 1, 1, 1, 1, 0, 704, 100
46530, V, 1, 1, 1, 1, 0, 704, 99
46531, V, 1, 1, 1, 1, 0, 704, 99
46532, V, 1, 1, 1, 1, 0, 704, 99
46533, V, 1, 1, 1, 1, 0, 704, 99
46534, V, 1, 1, 1, 1, 0, 704, 99
46535, V, 1, 1, 1, 1, 0, 704, 99
46536, V, 1, 1, 1, 1, 0, 704, 99
46537, V, 1, 1, 1, 1, 0, 704, 99
46538, V, 1, 1, 1, 1, 0, 704, 99
46539, V, 1, 1, 1, 1, 0, 704, 99
46540, V, 1, 1, 1, 1, 0, 704, 99
46541, V, 1, 1, 1, 1, 0, 704, 99
46542, V, 1, 1, 1, 1, 0, 704, 99
46543, V, 1, 1, 1, 1, 0, 704, 99
46544, V, 1, 1, 1, 1, 0, 704, 99
46545, V, 1, 1, 1, 1, 0, 704, 99
46546, V, 1, 1, 1, 1, 0, 704, 99
46547, V, 1, 1, 1, 1, 0, 704, 99
46548, V, 1, 1, 1, 1, 0, 704, 99
46550, V, 1, 1, 1, 1, 0, 704, 99
46551, V, 1, 1, 1, 1, 0, 704, 99
46552, V, 1, 1, 1, 1, 0, 704, 99
46553, V, 1, 1, 1, 1, 0, 704, 99
46554, V, 1, 1, 1, 1, 0, 704, 99
46555, V, 1, 1, 1, 1, 0, 704, 99
46556, V, 1, 1, 1, 1, 0, 704, 99
46557, V, 1, 1, 1, 1, 0, 704, 99
46558, V, 1, 1, 1, 1, 0, 704, 99
46559, V, 1, 1, 1, 1, 0, 704, 99
46560, V, 1, 1, 1, 1, 0, 704, 99
46561, V, 1, 1, 1, 1, 0, 704, 99
46562, V, 1, 1, 1, 1, 0, 704, 99
46563, V, 1, 1, 1, 1, 0, 704, 99
46564, V, 1, 1, 1, 1, 0, 704, 99
46565, V, 1, 1, 1, 1, 0, 704, 100
46566, V, 1, 1, 1, 1, 0, 704, 99
46567, V, 1, 1, 1, 1, 0, 704, 99
46568, V, 1, 1, 1, 1, 0, 704, 100
46569, V, 1, 1, 1, 1, 0, 704, 99
46570, V, 1, 1, 1, 1, 0, 704, 100
46571, V, 1, 1, 1, 1, 0, 704, 100
46572, V, 1, 1, 1, 1, 0, 704, 100
46573, V, 1, 1, 1, 1, 0, 704, 100
46574, V, 1, 1, 1, 1, 0, 704, 100
46575, V, 1, 1, 1, 1, 0, 704, 100
46576, V, 1, 1, 1, 1, 0, 704, 100
46577, V, 1, 1, 1, 1, 0, 704, 100
46578, V, 1, 1, 1, 1, 0, 704, 100
46579, V, 1, 1, 1, 1, 0, 704, 100
46580, V, 1, 1, 1, 1, 0, 704, 100
46581, V, 1, 1, 1, 1, 0, 704, 100
46582, V, 1, 1, 1, 1, 0, 704, 100
46583, V, 1, 1, 1, 1, 0, 704, 100
46584, V, 1, 1, 1, 1, 0, 704, 100
46585, V, 1, 1, 1, 1, 0, 704, 100
46586, V, 1, 1, 1, 1, 0, 704, 100
46587, V, 1, 1, 1, 1, 0, 704, 100
46588, V, 1, 1, 1, 1, 0, 704, 100
46589, V, 1, 1, 1, 1, 0, 704, 100
46590, V, 1, 1, 1, 1, 0, 704, 100
46592, V, 1, 1, 1, 1, 0, 704, 100
46593, V, 1, 1, 1, 1, 0, 704, 100
46594, V, 1, 1, 1, 1, 0, 704, 100
46595, V, 1, 1, 1, 1, 0, 704, 100
46596, V, 1, 1, 1, 1, 0, 704, 100
46597, V, 1, 1, 1, 1, 0, 704, 100
46598, V, 1, 1, 1, 1, 0, 704, 100
46599, V, 1, 1, 1, 1, 0, 704, 99
46600, V, 1, 1, 1, 1, 0, 704, 100
46601, V, 1, 1, 1, 1, 0, 704, 100
46602, V, 1, 1, 1, 1, 0, 704, 99
46603, V, 1, 1, 1, 1, 0, 704, 100
46604, V, 1, 1, 1, 1, 0, 704, 99
46605, V, 1, 1, 1, 1, 0, 704, 99
46606, V, 1, 1, 1, 1, 0, 704, 99
46607, V, 1, 1, 1, 1, 0, 704, 99
46608, V, 1, 1, 1, 1, 0, 704, 99
46609, V, 1, 1, 1, 1, 0, 704, 100
46610, V, 1, 1, 1, 1, 0, 704, 100
46611, V, 1, 1, 1, 1, 0, 704, 99
46612, V, 1, 1, 1, 1, 0, 704, 99
46613, V, 1, 1, 1, 1, 0, 704, 99
46614, V, 1, 1, 1, 1, 0, 704, 99
46615, V, 1, 1, 1, 1, 0, 704, 99
46616, V, 1, 1, 1, 1, 0, 704, 99
46617, V, 1, 1, 1, 1, 0, 704, 99
46618, V, 1, 1, 1, 1, 0, 704, 99
46619, V, 1, 1, 1, 1, 0, 704, 99
46620, V, 1, 1, 1, 1, 0, 704, 99
46621, V, 1, 1, 1, 1, 0, 704, 99
46622, V, 1, 1, 1, 1, 0, 704, 99
46623, V, 1, 1, 1, 1, 0, 704, 99
46624, V, 1, 1, 1, 1, 0, 704, 99
46625, V, 1, 1, 1, 1, 0, 704, 99
46626, V, 1, 1, 1, 1, 0, 704, 99
46627, V, 1, 1, 1, 1, 0, 704, 99
46628, V, 1, 1, 1, 1, 0, 704, 99
46629, V, 1, 1, 1, 1, 0, 704, 99
46630, V, 1, 1, 1, 1, 0, 704, 99
46631, V, 1, 1, 1, 1, 0, 704, 99
46632, V, 1, 1, 1, 1, 0, 704, 99
46633, V, 1, 1, 1, 1, 0, 704, 99
46635, V, 1, 1, 1, 1, 0, 704, 99
46636, V, 1, 1, 1, 1, 0, 704, 99
46637, V, 1, 1, 1, 1, 0, 704, 99
46638, V, 1, 1, 1, 1, 0, 704, 99
46639, V, 1, 1, 1, 1, 0, 704, 99
46640, V, 1, 1, 1, 1, 0, 704, 99
46641, V, 1, 1, 1, 1, 0, 704, 99
46642, V, 1, 1, 1, 1, 0, 704, 99
46643, V, 1, 1, 1, 1, 0, 704, 100
46644, V, 1, 1, 1, 1, 0, 704, 99
46645, V, 1, 1, 1, 1, 0, 704, 100
46646, V, 1, 1, 1, 1, 0, 704, 100
46647, V, 1, 1, 1, 1, 0, 704, 99
46648, V, 1, 1, 1, 1, 0, 704, 100
46649, V, 1, 1, 1, 1, 0, 704, 100
46650, V, 1, 1, 1, 1, 0, 704, 100
46651, V, 1, 1, 1, 1, 0, 704, 100
46652, V, 1, 1, 1, 1, 0, 704, 100
46653, V, 1, 1, 1, 1, 0, 704, 100
46654, V, 1, 1, 1, 1, 0, 704, 100
46655, V, 1, 1, 1, 1, 0, 704, 100
46656, V, 1, 1, 1, 1, 0, 704, 100
46657, V, 1, 1, 1, 1, 0, 704, 100
46658, V, 1, 1, 1, 1, 0, 704, 100
46659, V, 1, 1, 1, 1, 0, 704, 100
46660, V, 1, 1, 1, 1, 0, 704, 100
46661, V, 1, 1, 1, 1, 0, 704, 100
46662, V, 1, 1, 1, 1, 0, 704, 100
46663, V, 1, 1, 1, 1, 0, 704, 100
46664, V, 1, 1, 1, 1, 0, 704, 100
46665, V, 1, 1, 1, 1, 0, 704, 100
46666, V, 1, 1, 1, 1, 0, 704, 100
46667, V, 1, 1, 1, 1, 0, 704, 100
46668, V, 1, 1, 1, 1, 0, 704, 100
46669, V, 1, 1, 1, 1, 0, 704, 100
46670, V, 1, 1, 1, 1, 0, 704, 100
46671, V, 1, 1, 1, 1, 0, 704, 100
46672, V, 1, 1, 1, 1, 0, 704, 100
46673, V, 1, 1, 1, 1, 0, 704, 100
46674, V, 1, 1, 1, 1, 0, 704, 99
46675, V, 1, 1, 1, 1, 0, 704, 100
46676, V, 1, 1, 1, 1, 0, 704, 100
46678, V, 1, 1, 1, 1, 0, 704, 100
46679, V, 1, 1, 1, 1, 0, 704, 100
46680, V, 1, 1, 1, 1, 0, 704, 100
46681, V, 1, 1, 1, 1, 0, 704, 100
46682, V, 1, 1, 1, 1, 0, 704, 100
46683, V, 1, 1, 1, 1, 0, 704, 100
46684, V, 1, 1, 1, 1, 0, 704, 100
46685, V, 1, 1, 1, 1, 0, 704, 99
46686, V, 1, 1, 1, 1, 0, 704, 100
46687, V, 1, 1, 1, 1, 0, 704, 99
46688, V, 1, 1, 1, 1, 0, 704, 100
46689, V, 1, 1, 1, 1, 0, 704, 99
46690, V, 1, 1, 1, 1, 0, 704, 99
46691, V, 1, 1, 1, 1, 0, 704, 100
46692, V, 1, 1, 1, 1, 0, 704, 99
46693, V, 1, 1, 1, 1, 0, 704, 99
46694, V, 1, 1, 1, 1, 0, 704, 99
46695, V, 1, 1, 1, 1, 0, 704, 99
46696, V, 1, 1, 1, 1, 0, 704, 99
46697, V, 1, 1, 1, 1, 0, 704, 99
46698, V, 1, 1, 1, 1, 0, 704, 99
46699, V, 1, 1, 1, 1, 0, 704, 99
46700, V, 1, 1, 1, 1, 0, 704, 99
46701, V, 1, 1, 1, 1, 0, 704, 99
46702, V, 1, 1, 1, 1, 0, 704, 99
46703, V, 1, 1, 1, 1, 0, 704, 99
46704, V, 1, 1, 1, 1, 0, 704, 100
46705, V, 1, 1, 1, 1, 0, 704, 99
46706, V, 1, 1, 1, 1, 0, 704, 100
46707, V, 1, 1, 1, 1, 0, 704, 100
46708, V, 1, 1, 1, 1, 0, 704, 100
46709, V, 1, 1, 1, 1, 0, 704, 100
46710, V, 1, 1, 1, 1, 0, 704, 99
46711, V, 1, 1, 1, 1, 0, 704, 100
46712, V, 1, 1, 1, 1, 0, 704, 100
46713, V, 1, 1, 1, 1, 0, 704, 99
46714, V, 1, 1, 1, 1, 0, 704, 100
46715, V, 1, 1, 1, 1, 0, 704, 100
46716, V, 1, 1, 1, 1, 0, 704, 100
46717, V, 1, 1, 1, 1, 0, 704, 100
46718, V, 1, 1, 1, 1, 0, 704, 100
46720, V, 1, 1, 1, 1, 0, 704, 100
46721, V, 1, 1, 1, 1, 0, 704, 100
46722, V, 1, 1, 1, 1, 0, 704, 100
46723, V, 1, 1, 1, 1, 0, 704, 99
46724, V, 1, 1, 1, 1, 0, 704, 100
46725, V, 1, 1, 1, 1, 0, 704, 100
46726, V, 1, 1, 1, 1, 0, 704, 100
46727, V, 1, 1, 1, 1, 0, 704, 100
46728, V, 1, 1, 1, 1, 0, 704, 100
46729, V, 1, 1, 1, 1, 0, 704, 100
46730, V, 1, 1, 1, 1, 0, 704, 100
46731, V, 1, 1, 1, 1, 0, 704, 100
46732, V, 1, 1, 1, 1, 0, 704, 100
46733, V, 1, 1, 1, 1, 0, 704, 100
46734, V, 1, 1, 1, 1, 0, 704, 100
46735, V, 1, 1, 1, 1, 0, 704, 100
46736, V, 1, 1, 1, 1, 0, 704, 100
46737, V, 1, 1, 1, 1, 0, 704, 100
46738, V, 1, 1, 1, 1, 0, 704, 100
46739, V, 1, 1, 1, 1, 0, 704, 100
46740, V, 1, 1, 1, 1, 0, 704, 100
46741, V, 1, 1, 1, 1, 0, 704, 100
46742, V, 1, 1, 1, 1, 0, 704, 100
46743, V, 1, 1, 1, 1, 0, 704, 100
46744, V, 1, 1, 1, 1, 0, 704, 100
46745, V, 1, 1, 1, 1, 0, 704, 100
46746, V, 1, 1, 1, 1, 0, 704, 100
46747, V, 1, 1, 1, 1, 0, 704, 100
46748, V, 1, 1, 1, 1, 0, 704, 100
46749, V, 1, 1, 1, 1, 0, 704, 100
46750, V, 1, 1, 1, 1, 0, 704, 100
46751, V, 1, 1, 1, 1, 0, 704, 100
46752, V, 1, 1, 1, 1, 0, 704, 100
46753, V, 1, 1, 1, 1, 0, 704, 100
46754, V, 1, 1, 1, 1, 0, 704, 100
46755, V, 1, 1, 1, 1, 0, 704, 100
46756, V, 1, 1, 1, 1, 0, 704, 100
46757, V, 1, 1, 1, 1, 0, 704, 100
46758, V, 1, 1, 1, 1, 0, 704, 100
46759, V, 1, 1, 1, 1, 0, 704, 100
46760, V, 1, 1, 1, 1, 0, 704, 100
46761, V, 1, 1, 1, 1, 0, 704, 100
46763, V, 1, 1, 1, 1, 0, 704, 100
46764, V, 1, 1, 1, 1, 0, 704, 100
46765, V, 1, 1, 1, 1, 0, 704, 100
46766, V, 1, 1, 1, 1, 0, 704, 100
46767, V, 1, 1, 1, 1, 0, 704, 100
46768, V, 1, 1, 1, 1, 0, 704, 100
46769, V, 1, 1, 1, 1, 0, 704, 100
46770, V, 1, 1, 1, 1, 0, 704, 100
46771, V, 1, 1, 1, 1, 0, 704, 99
46772, V, 1, 1, 1, 1, 0, 704, 100
46773, V, 1, 1, 1, 1, 0, 704, 99
46774, V, 1, 1, 1, 1, 0, 704, 99
46775, V, 1, 1, 1, 1, 0, 704, 99
46776, V, 1, 1, 1, 1, 0, 704, 99
46777, V, 1, 1, 1, 1, 0, 704, 99
46778, V, 1, 1, 1, 1, 0, 704, 99
46779, V, 1, 1, 1, 1, 0, 704, 99
46780, V, 1, 1, 1, 1, 0, 704, 99
46781, V, 1, 1, 1, 1, 0, 704, 99
46782, V, 1, 1, 1, 1, 0, 704, 99
46783, V, 1, 1, 1, 1, 0, 704, 99
46784, V, 1, 1, 1, 1, 0, 704, 99
46785, V, 1, 1, 1, 1, 0, 704, 99
46786, V, 1, 1, 1, 1, 0, 704, 100
46787, V, 1, 1, 1, 1, 0, 704, 99
46788, V, 1, 1, 1, 1, 0, 704, 99
46789, V, 1, 1, 1, 1, 0, 704, 99
46790, V, 1, 1, 1, 1, 0, 704, 100
46791, V, 1, 1, 1, 1, 0, 704, 100
46792, V, 1, 1, 1, 1, 0, 704, 99
46793, V, 1, 1, 1, 1, 0, 704, 99
46794, V, 1, 1, 1, 1, 0, 704, 100
46795, V, 1, 1, 1, 1, 0, 704, 100
46796, V, 1, 1, 1, 1, 0, 704, 100
46797, V, 1, 1, 1, 1, 0, 704, 100
46798, V, 1, 1, 1, 1, 0, 704, 99
46799, V, 1, 1, 1, 1, 0, 704, 99
46800, V, 1, 1, 1, 1, 0, 704, 100
46801, V, 1, 1, 1, 1, 0, 704, 100
46802, V, 1, 1, 1, 1, 0, 704, 100
46803, V, 1, 1, 1, 1, 0, 704, 100
46804, V, 1, 1, 1, 1, 0, 704, 100
46806, V, 1, 1, 1, 1, 0, 704, 100
46807, V, 1, 1, 1, 1, 0, 704, 100
46808, V, 1, 1, 1, 1, 0, 704, 100
46809, V, 1, 1, 1, 1, 0, 704, 100
46810, V, 1, 1, 1, 1, 0, 704, 100
46811, V, 1, 1, 1, 1, 0, 704, 100
46812, V, 1, 1, 1, 1, 0, 704, 100
46813, V, 1, 1, 1, 1, 0, 704, 100
46814, V, 1, 1, 1, 1, 0, 704, 100
46815, V, 1, 1, 1, 1, 0, 704, 100
46816, V, 1, 1, 1, 1, 0, 704, 100
46817, V, 1, 1, 1, 1, 0, 704, 100
46818, V, 1, 1, 1, 1, 0, 704, 100
46819, V, 1, 1, 1, 1, 0, 704, 100
46820, V, 1, 1, 1, 1, 0, 704, 100
46821, V, 1, 1, 1, 1, 0, 704, 100
46822, V, 1, 1, 1, 1, 0, 704, 100
46823, V, 1, 1, 1, 1, 0, 704, 100
46824, V, 1, 1, 1, 1, 0, 704, 100
46825, V, 1, 1, 1, 1, 0, 704, 100
46826, V, 1, 1, 1, 1, 0, 704, 100
46827, V, 1, 1, 1, 1, 0, 704, 100
46828, V, 1, 1, 1, 1, 0, 704, 100
46829, V, 1, 1, 1, 1, 0, 704, 100
46830, V, 1, 1, 1, 1, 0, 704, 100
46831, V, 1, 1, 1, 1, 0, 704, 100
46832, V, 1, 1, 1, 1, 0, 704, 100
46833, V, 1, 1, 1, 1, 0, 704, 100
46834, V, 1, 1, 1, 1, 0, 704, 100
46835, V, 1, 1, 1, 1, 0, 704, 100
46836, V, 1, 1, 1, 1, 0, 704, 100
46837, V, 1, 1, 1, 1, 0, 704, 99
46838, V, 1, 1, 1, 1, 0, 704, 100
46839, V, 1, 1, 1, 1, 0, 704, 99
46840, V, 1, 1, 1, 1, 0, 704, 100
46841, V, 1, 1, 1, 1, 0, 704, 99
46842, V, 1, 1, 1, 1, 0, 704, 100
46843, V, 1, 1, 1, 1, 0, 704, 99
46844, V, 1, 1, 1, 1, 0, 704, 99
46845, V, 1, 1, 1, 1, 0, 704, 100
46846, V, 1, 1, 1, 1, 0, 704, 100
46848, V, 1, 1, 1, 1, 0, 704, 99
46849, V, 1, 1, 1, 1, 0, 704, 99
46850, V, 1, 1, 1, 1, 0, 704, 99
46851, V, 1, 1, 1, 1, 0, 704, 100
46852, V, 1, 1, 1, 1, 0, 704, 99
46853, V, 1, 1, 1, 1, 0, 704, 99
46854, V, 1, 1, 1, 1, 0, 704, 99
46855, V, 1, 1, 1, 1, 0, 704, 99
46856, V, 1, 1, 1, 1, 0, 704, 99
46857, V, 1, 1, 1, 1, 0, 704, 99
46858, V, 1, 1, 1, 1, 0, 704, 100
46859, V, 1, 1, 1, 1, 0, 704, 99
46860, V, 1, 1, 1, 1, 0, 704, 99
46861, V, 1, 1, 1, 1, 0, 704, 99
46862, V, 1, 1, 1, 1, 0, 704, 99
46863, V, 1, 1, 1, 1, 0, 704, 100
46864, V, 1, 1, 1, 1, 0, 704, 99
46865, V, 1, 1, 1, 1, 0, 704, 99
46866, V, 1, 1, 1, 1, 0, 704, 99
46867, V, 1, 1, 1, 1, 0, 704, 99
46868, V, 1, 1, 1, 1, 0, 704, 100
46869, V, 1, 1, 1, 1, 0, 704, 100
46870, V, 1, 1, 1, 1, 0, 704, 100
46871, V, 1, 1, 1, 1, 0, 704, 100
46872, V, 1, 1, 1, 1, 0, 704, 99
46873, V, 1, 1, 1, 1, 0, 704, 100
46874, V, 1, 1, 1, 1, 0, 704, 100
46875, V, 1, 1, 1, 1, 0, 704, 100
46876, V, 1, 1, 1, 1, 0, 704, 100
46877, V, 1, 1, 1, 1, 0, 704, 100
46878, V, 1, 1, 1, 1, 0, 704, 100
46879, V, 1, 1, 1, 1, 0, 704, 100
46880, V, 1, 1, 1, 1, 0, 704, 100
46881, V, 1, 1, 1, 1, 0, 704, 100
46882, V, 1, 1, 1, 1, 0, 704, 100
46883, V, 1, 1, 1, 1, 0, 704, 99
46884, V, 1, 1, 1, 1, 0, 704, 99
46885, V, 1, 1, 1, 1, 0, 704, 100
46886, V, 1, 1, 1, 1, 0, 704, 100
46887, V, 1, 1, 1, 1, 0, 704, 100
46888, V, 1, 1, 1, 1, 0, 704, 100
46889, V, 1, 1, 1, 1, 0, 704, 99
46891, V, 1, 1, 1, 1, 0, 704, 100
46892, V, 1, 1, 1, 1, 0, 704, 100
46893, V, 1, 1, 1, 1, 0, 704, 100
46894, V, 1, 1, 1, 1, 0, 704, 100
46895, V, 1, 1, 1, 1, 0, 704, 100
46896, V, 1, 1, 1, 1, 0, 704, 100
46897, V, 1, 1, 1, 1, 0, 704, 99
46898, V, 1, 1, 1, 1, 0, 704, 100
46899, V, 1, 1, 1, 1, 0, 704, 100
46900, V, 1, 1, 1, 1, 0, 704, 100
46901, V, 1, 1, 1, 1, 0, 704, 100
46902, V, 1, 1, 1, 1, 0, 704, 100
46903, V, 1, 1, 1, 1, 0, 704, 100
46904, V, 1, 1, 1, 1, 0, 704, 100
46905, V, 1, 1, 1, 1, 0, 704, 99
46906, V, 1, 1, 1, 1, 0, 704, 100
46907, V, 1, 1, 1, 1, 0, 704, 100
46908, V, 1, 1, 1, 1, 0, 704, 100
46909, V, 1, 1, 1, 1, 0, 704, 100
46910, V, 1, 1, 1, 1, 0, 704, 99
46911, V, 1, 1, 1, 1, 0, 704, 100
46912, V, 1, 1, 1, 1, 0, 704, 99
46913, V, 1, 1, 1, 1, 0, 704, 99
46914, V, 1, 1, 1, 1, 0, 704, 99
46915, V, 1, 1, 1, 1, 0, 704, 99
46916, V, 1, 1, 1, 1, 0, 704, 99
46917, V, 1, 1, 1, 1, 0, 704, 99
46918, V, 1, 1, 1, 1, 0, 704, 99
46919, V, 1, 1, 1, 1, 0, 704, 99
46920, V, 1, 1, 1, 1, 0, 704, 99
46921, V, 1, 1, 1, 1, 0, 704, 99
46922, V, 1, 1, 1, 1, 0, 704, 99
46923, V, 1, 1, 1, 1, 0, 704, 99
46924, V, 1, 1, 1, 1, 0, 704, 99
46925, V, 1, 1, 1, 1, 0, 704, 99
46926, V, 1, 1, 1, 1, 0, 704, 99
46927, V, 1, 1, 1, 1, 0, 704, 99
46928, V, 1, 1, 1, 1, 0, 704, 99
46929, V, 1, 1, 1, 1, 0, 704, 99
46930, V, 1, 1, 1, 1, 0, 704, 99
46931, V, 1, 1, 1, 1, 0, 704, 99
46932, V, 1, 1, 1, 1, 0, 704, 99
46934, V, 1, 1, 1, 1, 0, 704, 99
46935, V, 1, 1, 1, 1, 0, 704, 99
46936, V, 1, 1, 1, 1, 0, 704, 99
46937, V, 1, 1, 1, 1, 0, 704, 99
46938, V, 1, 1, 1, 1, 0, 704, 99
46939, V, 1, 1, 1, 1, 0, 704, 99
46940, V, 1, 1, 1, 1, 0, 704, 99
46941, V, 1, 1, 1, 1, 0, 704, 99
46942, V, 1, 1, 1, 1, 0, 704, 99
46943, V, 1, 1, 1, 1, 0, 704, 99
46944, V, 1, 1, 1, 1, 0, 704, 99
46945, V, 1, 1, 1, 1, 0, 704, 99
46946, V, 1, 1, 1, 1, 0, 704, 99
46947, V, 1, 1, 1, 1, 0, 704, 99
46948, V, 1, 1, 1, 1, 0, 704, 99
46949, V, 1, 1, 1, 1, 0, 704, 100
46950, V, 1, 1, 1, 1, 0, 704, 100
46951, V, 1, 1, 1, 1, 0, 704, 99
46952, V, 1, 1, 1, 1, 0, 704, 100
46953, V, 1, 1, 1, 1, 0, 704, 99
46954, V, 1, 1, 1, 1, 0, 704, 100
46955, V, 1, 1, 1, 1, 0, 704, 99
46956, V, 1, 1, 1, 1, 0, 704, 100
46957, V, 1, 1, 1, 1, 0, 704, 100
46958, V, 1, 1, 1, 1, 0, 704, 100
46959, V, 1, 1, 1, 1, 0, 704, 100
46960, V, 1, 1, 1, 1, 0, 704, 100
46961, V, 1, 1, 1, 1, 0, 704, 100
46962, V, 1, 1, 1, 1, 0, 704, 99
46963, V, 1, 1, 1, 1, 0, 704, 99
46964, V, 1, 1, 1, 1, 0, 704, 100
46965, V, 1, 1, 1, 1, 0, 704, 100
46966, V, 1, 1, 1, 1, 0, 704, 100
46967, V, 1, 1, 1, 1, 0, 704, 100
46968, V, 1, 1, 1, 1, 0, 704, 100
46969, V, 1, 1, 1, 1, 0, 704, 100
46970, V, 1, 1, 1, 1, 0, 704, 100
46971, V, 1, 1, 1, 1, 0, 704, 99
46972, V, 1, 1, 1, 1, 0, 704, 100
46973, V, 1, 1, 1, 1, 0, 704, 99
46974, V, 1, 1, 1, 1, 0, 704, 100
46976, V, 1, 1, 1, 1, 0, 704, 99
46977, V, 1, 1, 1, 1, 0, 704, 100
46978, V, 1, 1, 1, 1, 0, 704, 99
46979, V, 1, 1, 1, 1, 0, 704, 100
46980, V, 1, 1, 1, 1, 0, 704, 100
46981, V, 1, 1, 1, 1, 0, 704, 99
46982, V, 1, 1, 1, 1, 0, 704, 99
46983, V, 1, 1, 1, 1, 0, 704, 99
46984, V, 1, 1, 1, 1, 0, 704, 99
46985, V, 1, 1, 1, 1, 0, 704, 100
46986, V, 1, 1, 1, 1, 0, 704, 99
46987, V, 1, 1, 1, 1, 0, 704, 99
46988, V, 1, 1, 1, 1, 0, 704, 99
46989, V, 1, 1, 1, 1, 0, 704, 99
46990, V, 1, 1, 1, 1, 0, 704, 99
46991, V, 1, 1, 1, 1, 0, 704, 99
46992, V, 1, 1, 1, 1, 0, 704, 99
46993, V, 1, 1, 1, 1, 0, 704, 99
46994, V, 1, 1, 1, 1, 0, 704, 99
46995, V, 1, 1, 1, 1, 0, 704, 100
46996, V, 1, 1, 1, 1, 0, 704, 100
46997, V, 1, 1, 1, 1, 0, 704, 99
46998, V, 1, 1, 1, 1, 0, 704, 99
46999, V, 1, 1, 1, 1, 0, 704, 99
47000, V, 1, 1, 1, 1, 0, 704, 99
47001, V, 1, 1, 1, 1, 0, 704, 99
47002, V, 1, 1, 1, 1, 0, 704, 99
47003, V, 1, 1, 1, 1, 0, 704, 99
47004, V, 1, 1, 1, 1, 0, 704, 99
47005, V, 1, 1, 1, 1, 0, 704, 99
47006, V, 1, 1, 1, 1, 0, 704, 99
47007, V, 1, 1, 1, 1, 0, 704, 99
47008, V, 1, 1, 1, 1, 0, 704, 99
47009, V, 1, 1, 1, 1, 0, 704, 99
47010, V, 1, 1, 1, 1, 0, 704, 99
47011, V, 1, 1, 1, 1, 0, 704, 99
47012, V, 1, 1, 1, 1, 0, 704, 99
47013, V, 1, 1, 1, 1, 0, 704, 99
47014, V, 1, 1, 1, 1, 0, 704, 99
47015, V, 1, 1, 1, 1, 0, 704, 99
47016, V, 1, 1, 1, 1, 0, 704, 99
47017, V, 1, 1, 1, 1, 0, 704, 99
47019, V, 1, 1, 1, 1, 0, 704, 99
47020, V, 1, 1, 1, 1, 0, 704, 100
47021, V, 1, 1, 1, 1, 0, 704, 100
47022, V, 1, 1, 1, 1, 0, 704, 100
47023, V, 1, 1, 1, 1, 0, 704, 100
47024, V, 1, 1, 1, 1, 0, 704, 99
47025, V, 1, 1, 1, 1, 0, 704, 100
47026, V, 1, 1, 1, 1, 0, 704, 100
47027, V, 1, 1, 1, 1, 0, 704, 100
47028, V, 1, 1, 1, 1, 0, 704, 100
47029, V, 1, 1, 1, 1, 0, 704, 100
47030, V, 1, 1, 1, 1, 0, 704, 100
47031, V, 1, 1, 1, 1, 0, 704, 100
47032, V, 1, 1, 1, 1, 0, 704, 100
47033, V, 1, 1, 1, 1, 0, 704, 100
47034, V, 1, 1, 1, 1, 0, 704, 100
47035, V, 1, 1, 1, 1, 0, 704, 100
47036, V, 1, 1, 1, 1, 0, 704, 100
47037, V, 1, 1, 1, 1, 0, 704, 100
47038, V, 1, 1, 1, 1, 0, 704, 100
47039, V, 1, 1, 1, 1, 0, 704, 100
47040, V, 1, 1, 1, 1, 0, 704, 100
47041, V, 1, 1, 1, 1, 0, 704, 100
47042, V, 1, 1, 1, 1, 0, 704, 100
47043, V, 1, 1, 1, 1, 0, 704, 100
47044, V, 1, 1, 1, 1, 0, 704, 100
47045, V, 1, 1, 1, 1, 0, 704, 100
47046, V, 1, 1, 1, 1, 0, 704, 100
47047, V, 1, 1, 1, 1, 0, 704, 100
47048, V, 1, 1, 1, 1, 0, 704, 100
47049, V, 1, 1, 1, 1, 0, 704, 100
47050, V, 1, 1, 1, 1, 0, 704, 100
47051, V, 1, 1, 1, 1, 0, 704, 100
47052, V, 1, 1, 1, 1, 0, 704, 100
47053, V, 1, 1, 1, 1, 0, 704, 100
47054, V, 1, 1, 1, 1, 0, 704, 100
47055, V, 1, 1, 1, 1, 0, 704, 100
47056, V, 1, 1, 1, 1, 0, 704, 100
47057, V, 1, 1, 1, 1, 0, 704, 100
47058, V, 1, 1, 1, 1, 0, 704, 100
47059, V, 1, 1, 1, 1, 0, 704, 100
47060, V, 1, 1, 1, 1, 0, 704, 100
47062, V, 1, 1, 1, 1, 0, 704, 100
47063, V, 1, 1, 1, 1, 0, 704, 100
47064, V, 1, 1, 1, 1, 0, 704, 100
47065, V, 1, 1, 1, 1, 0, 704, 100
47066, V, 1, 1, 1, 1, 0, 704, 100
47067, V, 1, 1, 1, 1, 0, 704, 100
47068, V, 1, 1, 1, 1, 0, 704, 100
47069, V, 1, 1, 1, 1, 0, 704, 99
47070, V, 1, 1, 1, 1, 0, 704, 100
47071, V, 1, 1, 1, 1, 0, 704, 99
47072, V, 1, 1, 1, 1, 0, 704, 99
47073, V, 1, 1, 1, 1, 0, 704, 99
47074, V, 1, 1, 1, 1, 0, 704, 99
47075, V, 1, 1, 1, 1, 0, 704, 99
47076, V, 1, 1, 1, 1, 0, 704, 99
47077, V, 1, 1, 1, 1, 0, 704, 99
47078, V, 1, 1, 1, 1, 0, 704, 99
47079, V, 1, 1, 1, 1, 0, 704, 99
47080, V, 1, 1, 1, 1, 0, 704, 99
47081, V, 1, 1, 1, 1, 0, 704, 99
47082, V, 1, 1, 1, 1, 0, 704, 99
47083, V, 1, 1, 1, 1, 0, 704, 99
47084, V, 1, 1, 1, 1, 0, 704, 99
47085, V, 1, 1, 1, 1, 0, 704, 99
47086, V, 1, 1, 1, 1, 0, 704, 99
47087, V, 1, 1, 1, 1, 0, 704, 99
47088, V, 1, 1, 1, 1, 0, 704, 99
47089, V, 1, 1, 1, 1, 0, 704, 99
47090, V, 1, 1, 1, 1, 0, 704, 99
47091, V, 1, 1, 1, 1, 0, 704, 99
47092, V, 1, 1, 1, 1, 0, 704, 99
47093, V, 1, 1, 1, 1, 0, 704, 100
47094, V, 1, 1, 1, 1, 0, 704, 99
47095, V, 1, 1, 1, 1, 0, 704, 99
47096, V, 1, 1, 1, 1, 0, 704, 99
47097, V, 1, 1, 1, 1, 0, 704, 99
47098, V, 1, 1, 1, 1, 0, 704, 99
47099, V, 1, 1, 1, 1, 0, 704, 99
47100, V, 1, 1, 1, 1, 0, 704, 100
47101, V, 1, 1, 1, 1, 0, 704, 100
47102, V, 1, 1, 1, 1, 0, 704, 100
47104, V, 1, 1, 1, 1, 0, 704, 100
47105, V, 1, 1, 1, 1, 0, 704, 100
47106, V, 1, 1, 1, 1, 0, 704, 100
47107, V, 1, 1, 1, 1, 0, 704, 100
47108, V, 1, 1, 1, 1, 0, 704, 100
47109, V, 1, 1, 1, 1, 0, 704, 100
47110, V, 1, 1, 1, 1, 0, 704, 100
47111, V, 1, 1, 1, 1, 0, 704, 100
47112, V, 1, 1, 1, 1, 0, 704, 100
47113, V, 1, 1, 1, 1, 0, 704, 100
47114, V, 1, 1, 1, 1, 0, 704, 100
47115, V, 1, 1, 1, 1, 0, 704, 100
47116, V, 1, 1, 1, 1, 0, 704, 100
47117, V, 1, 1, 1, 1, 0, 704, 100
47118, V, 1, 1, 1, 1, 0, 704, 100
47119, V, 1, 1, 1, 1, 0, 704, 100
47120, V, 1, 1, 1, 1, 0, 704, 100
47121, V, 1, 1, 1, 1, 0, 704, 100
47122, V, 1, 1, 1, 1, 0, 704, 100
47123, V, 1, 1, 1, 1, 0, 704, 100
47124, V, 1, 1, 1, 1, 0, 704, 100
47125, V, 1, 1, 1, 1, 0, 704, 100
47126, V, 1, 1, 1, 1, 0, 704, 100
47127, V, 1, 1, 1, 1, 0, 704, 100
47128, V, 1, 1, 1, 1, 0, 704, 100
47129, V, 1, 1, 1, 1, 0, 704, 100
47130, V, 1, 1, 1, 1, 0, 704, 100
47131, V, 1, 1, 1, 1, 0, 704, 100
47132, V, 1, 1, 1, 1, 0, 704, 100
47133, V, 1, 1, 1, 1, 0, 704, 100
47134, V, 1, 1, 1, 1, 0, 704, 100
47135, V, 1, 1, 1, 1, 0, 704, 99
47136, V, 1, 1, 1, 1, 0, 704, 100
47137, V, 1, 1, 1, 1, 0, 704, 100
47138, V, 1, 1, 1, 1, 0, 704, 100
47139, V, 1, 1, 1, 1, 0, 704, 100
47140, V, 1, 1, 1, 1, 0, 704, 99
47141, V, 1, 1, 1, 1, 0, 704, 100
47142, V, 1, 1, 1, 1, 0, 704, 99
47143, V, 1, 1, 1, 1, 0, 704, 99
47144, V, 1, 1, 1, 1, 0, 704, 99
47145, V, 1, 1, 1, 1, 0, 704, 99
47147, V, 1, 1, 1, 1, 0, 704, 99
47148, V, 1, 1, 1, 1, 0, 704, 99
47149, V, 1, 1, 1, 1, 0, 704, 100
47150, V, 1, 1, 1, 1, 0, 704, 99
47151, V, 1, 1, 1, 1, 0, 704, 99
47152, V, 1, 1, 1, 1, 0, 704, 100
47153, V, 1, 1, 1, 1, 0, 704, 99
47154, V, 1, 1, 1, 1, 0, 704, 99
47155, V, 1, 1, 1, 1, 0, 704, 99
47156, V, 1, 1, 1, 1, 0, 704, 99
47157, V, 1, 1, 1, 1, 0, 704, 99
47158, V, 1, 1, 1, 1, 0, 704, 99
47159, V, 1, 1, 1, 1, 0, 704, 99
47160, V, 1, 1, 1, 1, 0, 704, 99
47161, V, 1, 1, 1, 1, 0, 704, 99
47162, V, 1, 1, 1, 1, 0, 704, 99
47163, V, 1, 1, 1, 1, 0, 704, 99
47164, V, 1, 1, 1, 1, 0, 704, 99
47165, V, 1, 1, 1, 1, 0, 704, 99
47166, V, 1, 1, 1, 1, 0, 704, 100
47167, V, 1, 1, 1, 1, 0, 704, 100
47168, V, 1, 1, 1, 1, 0, 704, 99
47169, V, 1, 1, 1, 1, 0, 704, 99
47170, V, 1, 1, 1, 1, 0, 704, 100
47171, V, 1, 1, 1, 1, 0, 704, 99
47172, V, 1, 1, 1, 1, 0, 704, 100
47173, V, 1, 1, 1, 1, 0, 704, 99
47174, V, 1, 1, 1, 1, 0, 704, 99
47175, V, 1, 1, 1, 1, 0, 704, 100
47176, V, 1, 1, 1, 1, 0, 704, 100
47177, V, 1, 1, 1, 1, 0, 704, 100
47178, V, 1, 1, 1, 1, 0, 704, 100
47179, V, 1, 1, 1, 1, 0, 704, 100
47180, V, 1, 1, 1, 1, 0, 704, 100
47181, V, 1, 1, 1, 1, 0, 704, 100
47182, V, 1, 1, 1, 1, 0, 704, 100
47183, V, 1, 1, 1, 1, 0, 704, 100
47184, V, 1, 1, 1, 1, 0, 704, 100
47185, V, 1, 1, 1, 1, 0, 704, 100
47186, V, 1, 1, 1, 1, 0, 704, 100
47187, V, 1, 1, 1, 1, 0, 704, 100
47188, V, 1, 1, 1, 1, 0, 704, 100
47190, V, 1, 1, 1, 1, 0, 704, 100
47191, V, 1, 1, 1, 1, 0, 704, 100
47192, V, 1, 1, 1, 1, 0, 704, 100
47193, V, 1, 1, 1, 1, 0, 704, 100
47194, V, 1, 1, 1, 1, 0, 704, 100
47195, V, 1, 1, 1, 1, 0, 704, 100
47196, V, 1, 1, 1, 1, 0, 704, 99
47197, V, 1, 1, 1, 1, 0, 704, 100
47198, V, 1, 1, 1, 1, 0, 704, 100
47199, V, 1, 1, 1, 1, 0, 704, 100
47200, V, 1, 1, 1, 1, 0, 704, 100
47201, V, 1, 1, 1, 1, 0, 704, 100
47202, V, 1, 1, 1, 1, 0, 704, 100
47203, V, 1, 1, 1, 1, 0, 704, 100
47204, V, 1, 1, 1, 1, 0, 704, 99
47205, V, 1, 1, 1, 1, 0, 704, 100
47206, V, 1, 1, 1, 1, 0, 704, 99
47207, V, 1, 1, 1, 1, 0, 704, 100
47208, V, 1, 1, 1, 1, 0, 704, 100
47209, V, 1, 1, 1, 1, 0, 704, 100
47210, V, 1, 1, 1, 1, 0, 704, 99
47211, V, 1, 1, 1, 1, 0, 704, 99
47212, V, 1, 1, 1, 1, 0, 704, 99
47213, V, 1, 1, 1, 1, 0, 704, 99
47214, V, 1, 1, 1, 1, 0, 704, 99
47215, V, 1, 1, 1, 1, 0, 704, 99
47216, V, 1, 1, 1, 1, 0, 704, 99
47217, V, 1, 1, 1, 1, 0, 704, 99
47218, V, 1, 1, 1, 1, 0, 704, 99
47219, V, 1, 1, 1, 1, 0, 704, 99
47220, V, 1, 1, 1, 1, 0, 704, 99
47221, V, 1, 1, 1, 1, 0, 704, 99
47222, V, 1, 1, 1, 1, 0, 704, 99
47223, V, 1, 1, 1, 1, 0, 704, 99
47224, V, 1, 1, 1, 1, 0, 704, 99
47225, V, 1, 1, 1, 1, 0, 704, 99
47226, V, 1, 1, 1, 1, 0, 704, 99
47227, V, 1, 1, 1, 1, 0, 704, 99
47228, V, 1, 1, 1, 1, 0, 704, 99
47229, V, 1, 1, 1, 1, 0, 704, 99
47230, V, 1, 1, 1, 1, 0, 704, 99
47232, V, 1, 1, 1, 1, 0, 704, 99
47233, V, 1, 1, 1, 1, 0, 704, 100
47234, V, 1, 1, 1, 1, 0, 704, 99
47235, V, 1, 1, 1, 1, 0, 704, 99
47236, V, 1, 1, 1, 1, 0, 704, 99
47237, V, 1, 1, 1, 1, 0, 704, 99
47238, V, 1, 1, 1, 1, 0, 704, 99
47239, V, 1, 1, 1, 1, 0, 704, 99
47240, V, 1, 1, 1, 1, 0, 704, 99
47241, V, 1, 1, 1, 1, 0, 704, 99
47242, V, 1, 1, 1, 1, 0, 704, 99
47243, V, 1, 1, 1, 1, 0, 704, 99
47244, V, 1, 1, 1, 1, 0, 704, 99
47245, V, 1, 1, 1, 1, 0, 704, 99
47246, V, 1, 1, 1, 1, 0, 704, 99
47247, V, 1, 1, 1, 1, 0, 704, 99
47248, V, 1, 1, 1, 1, 0, 704, 99
47249, V, 1, 1, 1, 1, 0, 704, 99
47250, V, 1, 1, 1, 1, 0, 704, 99
47251, V, 1, 1, 1, 1, 0, 704, 99
47252, V, 1, 1, 1, 1, 0, 704, 99
47253, V, 1, 1, 1, 1, 0, 704, 99
47254, V, 1, 1, 1, 1, 0, 704, 99
47255, V, 1, 1, 1, 1, 0, 704, 100
47256, V, 1, 1, 1, 1, 0, 704, 99
47257, V, 1, 1, 1, 1, 0, 704, 100
47258, V, 1, 1, 1, 1, 0, 704, 100
47259, V, 1, 1, 1, 1, 0, 704, 99
47260, V, 1, 1, 1, 1, 0, 704, 100
47261, V, 1, 1, 1, 1, 0, 704, 100
47262, V, 1, 1, 1, 1, 0, 704, 100
47263, V, 1, 1, 1, 1, 0, 704, 100
47264, V, 1, 1, 1, 1, 0, 704, 99
47265, V, 1, 1, 1, 1, 0, 704, 100
47266, V, 1, 1, 1, 1, 0, 704, 100
47267, V, 1, 1, 1, 1, 0, 704, 100
47268, V, 1, 1, 1, 1, 0, 704, 100
47269, V, 1, 1, 1, 1, 0, 704, 100
47270, V, 1, 1, 1, 1, 0, 704, 100
47271, V, 1, 1, 1, 1, 0, 704, 100
47272, V, 1, 1, 1, 1, 0, 704, 100
47273, V, 1, 1, 1, 1, 0, 704, 100
47275, V, 1, 1, 1, 1, 0, 704, 100
47276, V, 1, 1, 1, 1, 0, 704, 100
47277, V, 1, 1, 1, 1, 0, 704, 99
47278, V, 1, 1, 1, 1, 0, 704, 100
47279, V, 1, 1, 1, 1, 0, 704, 100
47280, V, 1, 1, 1, 1, 0, 704, 99
47281, V, 1, 1, 1, 1, 0, 704, 100
47282, V, 1, 1, 1, 1, 0, 704, 99
47283, V, 1, 1, 1, 1, 0, 704, 99
47284, V, 1, 1, 1, 1, 0, 704, 99
47285, V, 1, 1, 1, 1, 0, 704, 100
47286, V, 1, 1, 1, 1, 0, 704, 100
47287, V, 1, 1, 1, 1, 0, 704, 99
47288, V, 1, 1, 1, 1, 0, 704, 100
47289, V, 1, 1, 1, 1, 0, 704, 99
47290, V, 1, 1, 1, 1, 0, 704, 99
47291, V, 1, 1, 1, 1, 0, 704, 100
47292, V, 1, 1, 1, 1, 0, 704, 99
47293, V, 1, 1, 1, 1, 0, 704, 100
47294, V, 1, 1, 1, 1, 0, 704, 99
47295, V, 1, 1, 1, 1, 0, 704, 99
47296, V, 1, 1, 1, 1, 0, 704, 99
47297, V, 1, 1, 1, 1, 0, 704, 99
47298, V, 1, 1, 1, 1, 0, 704, 99
47299, V, 1, 1, 1, 1, 0, 704, 99
47300, V, 1, 1, 1, 1, 0, 704, 99
47301, V, 1, 1, 1, 1, 0, 704, 99
47302, V, 1, 1, 1, 1, 0, 704, 99
47303, V, 1, 1, 1, 1, 0, 704, 99
47304, V, 1, 1, 1, 1, 0, 704, 99
47305, V, 1, 1, 1, 1, 0, 704, 99
47306, V, 1, 1, 1, 1, 0, 704, 100
47307, V, 1, 1, 1, 1, 0, 704, 99
47308, V, 1, 1, 1, 1, 0, 704, 99
47309, V, 1, 1, 1, 1, 0, 704, 99
47310, V, 1, 1, 1, 1, 0, 704, 99
47311, V, 1, 1, 1, 1, 0, 704, 99
47312, V, 1, 1, 1, 1, 0, 704, 99
47313, V, 1, 1, 1, 1, 0, 704, 99
47314, V, 1, 1, 1, 1, 0, 704, 99
47315, V, 1, 1, 1, 1, 0, 704, 99
47316, V, 1, 1, 1, 1, 0, 704, 99
47318, V, 1, 1, 1, 1, 0, 704, 99
47319, V, 1, 1, 1, 1, 0, 704, 99
47320, V, 1, 1, 1, 1, 0, 704, 100
47321, V, 1, 1, 1, 1, 0, 704, 99
47322, V, 1, 1, 1, 1, 0, 704, 100
47323, V, 1, 1, 1, 1, 0, 704, 100
47324, V, 1, 1, 1, 1, 0, 704, 100
47325, V, 1, 1, 1, 1, 0, 704, 99
47326, V, 1, 1, 1, 1, 0, 704, 100
47327, V, 1, 1, 1, 1, 0, 704, 100
47328, V, 1, 1, 1, 1, 0, 704, 99
47329, V, 1, 1, 1, 1, 0, 704, 100
47330, V, 1, 1, 1, 1, 0, 704, 100
47331, V, 1, 1, 1, 1, 0, 704, 100
47332, V, 1, 1, 1, 1, 0, 704, 99
47333, V, 1, 1, 1, 1, 0, 704, 100
47334, V, 1, 1, 1, 1, 0, 704, 100
47335, V, 1, 1, 1, 1, 0, 704, 100
47336, V, 1, 1, 1, 1, 0, 704, 100
47337, V, 1, 1, 1, 1, 0, 704, 100
47338, V, 1, 1, 1, 1, 0, 704, 99
47339, V, 1, 1, 1, 1, 0, 704, 100
47340, V, 1, 1, 1, 1, 0, 704, 100
47341, V, 1, 1, 1, 1, 0, 704, 100
47342, V, 1, 1, 1, 1, 0, 704, 100
47343, V, 1, 1, 1, 1, 0, 704, 100
47344, V, 1, 1, 1, 1, 0, 704, 100
47345, V, 1, 1, 1, 1, 0, 704, 100
47346, V, 1, 1, 1, 1, 0, 704, 100
47347, V, 1, 1, 1, 1, 0, 704, 100
47348, V, 1, 1, 1, 1, 0, 704, 100
47349, V, 1, 1, 1, 1, 0, 704, 100
47350, V, 1, 1, 1, 1, 0, 704, 100
47351, V, 1, 1, 1, 1, 0, 704, 99
47352, V, 1, 1, 1, 1, 0, 704, 100
47353, V, 1, 1, 1, 1, 0, 704, 100
47354, V, 1, 1, 1, 1, 0, 704, 100
47355, V, 1, 1, 1, 1, 0, 704, 100
47356, V, 1, 1, 1, 1, 0, 704, 100
47357, V, 1, 1, 1, 1, 0, 704, 100
47358, V, 1, 1, 1, 1, 0, 704, 99
47360, V, 1, 1, 1, 1, 0, 704, 100
47361, V, 1, 1, 1, 1, 0, 704, 100
47362, V, 1, 1, 1, 1, 0, 704, 99
47363, V, 1, 1, 1, 1, 0, 704, 99
47364, V, 1, 1, 1, 1, 0, 704, 100
47365, V, 1, 1, 1, 1, 0, 704, 99
47366, V, 1, 1, 1, 1, 0, 704, 99
47367, V, 1, 1, 1, 1, 0, 704, 99
47368, V, 1, 1, 1, 1, 0, 704, 99
47369, V, 1, 1, 1, 1, 0, 704, 99
47370, V, 1, 1, 1, 1, 0, 704, 99
47371, V, 1, 1, 1, 1, 0, 704, 99
47372, V, 1, 1, 1, 1, 0, 704, 100
47373, V, 1, 1, 1, 1, 0, 704, 99
47374, V, 1, 1, 1, 1, 0, 704, 99
47375, V, 1, 1, 1, 1, 0, 704, 99
47376, V, 1, 1, 1, 1, 0, 704, 99
47377, V, 1, 1, 1, 1, 0, 704, 99
47378, V, 1, 1, 1, 1, 0, 704, 99
47379, V, 1, 1, 1, 1, 0, 704, 99
47380, V, 1, 1, 1, 1, 0, 704, 99
47381, V, 1, 1, 1, 1, 0, 704, 99
47382, V, 1, 1, 1, 1, 0, 704, 99
47383, V, 1, 1, 1, 1, 0, 704, 99
47384, V, 1, 1, 1, 1, 0, 704, 99
47385, V, 1, 1, 1, 1, 0, 704, 99
47386, V, 1, 1, 1, 1, 0, 704, 99
47387, V, 1, 1, 1, 1, 0, 704, 99
47388, V, 1, 1, 1, 1, 0, 704, 99
47389, V, 1, 1, 1, 1, 0, 704, 99
47390, V, 1, 1, 1, 1, 0, 704, 99
47391, V, 1, 1, 1, 1, 0, 704, 100
47392, V, 1, 1, 1, 1, 0, 704, 99
47393, V, 1, 1, 1, 1, 0, 704, 99
47394, V, 1, 1, 1, 1, 0, 704, 99
47395, V, 1, 1, 1, 1, 0, 704, 99
47396, V, 1, 1, 1, 1, 0, 704, 99
47397, V, 1, 1, 1, 1, 0, 704, 99
47398, V, 1, 1, 1, 1, 0, 704, 99
47399, V, 1, 1, 1, 1, 0, 704, 99
47400, V, 1, 1, 1, 1, 0, 704, 99
47401, V, 1, 1, 1, 1, 0, 704, 99
47403, V, 1, 1, 1, 1, 0, 704, 99
47404, V, 1, 1, 1, 1, 0, 704, 99
47405, V, 1, 1, 1, 1, 0, 704, 100
47406, V, 1, 1, 1, 1, 0, 704, 99
47407, V, 1, 1, 1, 1, 0, 704, 100
47408, V, 1, 1, 1, 1, 0, 704, 100
47409, V, 1, 1, 1, 1, 0, 704, 100
47410, V, 1, 1, 1, 1, 0, 704, 100
47411, V, 1, 1, 1, 1, 0, 704, 100
47412, V, 1, 1, 1, 1, 0, 704, 100
47413, V, 1, 1, 1, 1, 0, 704, 99
47414, V, 1, 1, 1, 1, 0, 704, 100
47415, V, 1, 1, 1, 1, 0, 704, 100
47416, V, 1, 1, 1, 1, 0, 704, 99
47417, V, 1, 1, 1, 1, 0, 704, 100
47418, V, 1, 1, 1, 1, 0, 704, 99
47419, V, 1, 1, 1, 1, 0, 704, 100
47420, V, 1, 1, 1, 1, 0, 704, 100
47421, V, 1, 1, 1, 1, 0, 704, 100
47422, V, 1, 1, 1, 1, 0, 704, 100
47423, V, 1, 1, 1, 1, 0, 704, 99
47424, V, 1, 1, 1, 1, 0, 704, 100
47425, V, 1, 1, 1, 1, 0, 704, 100
47426, V, 1, 1, 1, 1, 0, 704, 100
47427, V, 1, 1, 1, 1, 0, 704, 100
47428, V, 1, 1, 1, 1, 0, 704, 100
47429, V, 1, 1, 1, 1, 0, 704, 100
47430, V, 1, 1, 1, 1, 0, 704, 100
47431, V, 1, 1, 1, 1, 0, 704, 100
47432, V, 1, 1, 1, 1, 0, 704, 100
47433, V, 1, 1, 1, 1, 0, 704, 100
47434, V, 1, 1, 1, 1, 0, 704, 99
47435, V, 1, 1, 1, 1, 0, 704, 100
47436, V, 1, 1, 1, 1, 0, 704, 99
47437, V, 1, 1, 1, 1, 0, 704, 100
47438, V, 1, 1, 1, 1, 0, 704, 99
47439, V, 1, 1, 1, 1, 0, 704, 100
47440, V, 1, 1, 1, 1, 0, 704, 99
47441, V, 1, 1, 1, 1, 0, 704, 99
47442, V, 1, 1, 1, 1, 0, 704, 100
47443, V, 1, 1, 1, 1, 0, 704, 99
47444, V, 1, 1, 1, 1, 0, 704, 99
47446, V, 1, 1, 1, 1, 0, 704, 99
47447, V, 1, 1, 1, 1, 0, 704, 99
47448, V, 1, 1, 1, 1, 0, 704, 99
47449, V, 1, 1, 1, 1, 0, 704, 99
47450, V, 1, 1, 1, 1, 0, 704, 100
47451, V, 1, 1, 1, 1, 0, 704, 99
47452, V, 1, 1, 1, 1, 0, 704, 99
47453, V, 1, 1, 1, 1, 0, 704, 99
47454, V, 1, 1, 1, 1, 0, 704, 99
47455, V, 1, 1, 1, 1, 0, 704, 99
47456, V, 1, 1, 1, 1, 0, 704, 99
47457, V, 1, 1, 1, 1, 0, 704, 99
47458, V, 1, 1, 1, 1, 0, 704, 99
47459, V, 1, 1, 1, 1, 0, 704, 99
47460, V, 1, 1, 1, 1, 0, 704, 100
47461, V, 1, 1, 1, 1, 0, 704, 99
47462, V, 1, 1, 1, 1, 0, 704, 100
47463, V, 1, 1, 1, 1, 0, 704, 100
47464, V, 1, 1, 1, 1, 0, 704, 99
47465, V, 1, 1, 1, 1, 0, 704, 99
47466, V, 1, 1, 1, 1, 0, 704, 99
47467, V, 1, 1, 1, 1, 0, 704, 100
47468, V, 1, 1, 1, 1, 0, 704, 100
47469, V, 1, 1, 1, 1, 0, 704, 99
47470, V, 1, 1, 1, 1, 0, 704, 100
47471, V, 1, 1, 1, 1, 0, 704, 100
47472, V, 1, 1, 1, 1, 0, 704, 99
47473, V, 1, 1, 1, 1, 0, 704, 100
47474, V, 1, 1, 1, 1, 0, 704, 100
47475, V, 1, 1, 1, 1, 0, 704, 100
47476, V, 1, 1, 1, 1, 0, 704, 100
47477, V, 1, 1, 1, 1, 0, 704, 100
47478, V, 1, 1, 1, 1, 0, 704, 100
47479, V, 1, 1, 1, 1, 0, 704, 100
47480, V, 1, 1, 1, 1, 0, 704, 100
47481, V, 1, 1, 1, 1, 0, 704, 100
47482, V, 1, 1, 1, 1, 0, 704, 100
47483, V, 1, 1, 1, 1, 0, 704, 100
47484, V, 1, 1, 1, 1, 0, 704, 100
47485, V, 1, 1, 1, 1, 0, 704, 100
47486, V, 1, 1, 1, 1, 0, 704, 100
47488, V, 1, 1, 1, 1, 0, 704, 100
47489, V, 1, 1, 1, 1, 0, 704, 100
47490, V, 1, 1, 1, 1, 0, 704, 100
47491, V, 1, 1, 1, 1, 0, 704, 100
47492, V, 1, 0, 0, 1, 0, 704, 100
47492, V, 1, 0, 0, 0, 0, 704, 100
47493, V, 1, 1, 0, 0, 0, 704, 100
47493, V, 1, 1, 0, 0, 0, 704, 100
47494, V, 1, 1, 1, 1, 0, 704, 100
47495, V, 1, 1, 1, 1, 0, 704, 100
47496, V, 1, 1, 1, 1, 0, 704, 99
47497, V, 1, 1, 1, 1, 0, 704, 99
47498, V, 1, 1, 1, 1, 0, 704, 99
47499, V, 1, 1, 1, 1, 0, 704, 99
47500, V, 1, 1, 1, 1, 0, 704, 99
47501, V, 1, 1, 1, 1, 0, 704, 99
47502, V, 1, 1, 1, 1, 0, 704, 99
47503, V, 1, 1, 1, 1, 0, 704, 99
47504, V, 1, 1, 1, 1, 0, 704, 99
47505, V, 1, 1, 1, 1, 0, 704, 99
47506, V, 1, 1, 1, 1, 0, 704, 99
47507, V, 1, 1, 1, 1, 0, 704, 99
47508, V, 1, 1, 1, 1, 0, 704, 99
47509, V, 1, 1, 1, 1, 0, 704, 99
47510, V, 1, 1, 1, 1, 0, 704, 99
47511, V, 1, 1, 1, 1, 0, 704, 99
47512, V, 1, 1, 1, 1, 0, 704, 99
47513, V, 1, 1, 1, 1, 0, 704, 99
47514, V, 1, 1, 1, 1, 0, 704, 99
47515, V, 1, 1, 1, 1, 0, 704, 99
47516, V, 1, 1, 1, 1, 0, 704, 99
47517, V, 1, 1, 1, 1, 0, 704, 99
47518, V, 1, 1, 1, 1, 0, 704, 99
47519, V, 1, 1, 1, 1, 0, 704, 99
47520, V, 1, 1, 1, 1, 0, 704, 99
47521, V, 1, 1, 1, 1, 0, 704, 99
47522, V, 1, 1, 1, 1, 0, 704, 99
47523, V, 1, 1, 1, 1, 0, 704, 99
47524, V, 1, 1, 1, 1, 0, 704, 99
47525, V, 1, 1, 1, 1, 0, 704, 99
47526, V, 1, 1, 1, 1, 0, 704, 99
47527, V, 1, 1, 1, 1, 0, 704, 99
47528, V, 1, 1, 1, 1, 0, 704, 99
47529, V, 1, 1, 1, 1, 0, 704, 99
47531, V, 1, 1, 1, 1, 0, 704, 99
47532, V, 1, 1, 1, 1, 0, 704, 99
47533, V, 1, 1, 1, 1, 0, 704, 99
47534, V, 1, 1, 1, 1, 0, 704, 99
47535, V, 1, 1, 1, 1, 0, 704, 99
47536, V, 1, 1, 1, 1, 0, 704, 99
47537, V, 1, 1, 1, 1, 0, 704, 99
47538, V, 1, 1, 1, 1, 0, 704, 99
47539, V, 1, 1, 1, 1, 0, 704, 99
47540, V, 1, 1, 1, 1, 0, 704, 99
47541, V, 1, 1, 1, 1, 0, 704, 99
47542, V, 1, 1, 1, 1, 0, 704, 99
47543, V, 1, 1, 1, 1, 0, 704, 99
47544, V, 1, 1, 1, 1, 0, 704, 99
47545, V, 1, 1, 1, 1, 0, 704, 99
47546, V, 1, 1, 1, 1, 0, 704, 99
47547, V, 1, 1, 1, 1, 0, 704, 99
47548, V, 1, 1, 1, 1, 0, 704, 99
47549, V, 1, 1, 1, 1, 0, 704, 99
47550, V, 1, 1, 1, 1, 0, 704, 99
47551, V, 1, 1, 1, 1, 0, 704, 99
47552, V, 1, 1, 1, 1, 0, 704, 99
47553, V, 1, 1, 1, 1, 0, 704, 100
47554, V, 1, 1, 1, 1, 0, 704, 99
47555, V, 1, 1, 1, 1, 0, 704, 100
47556, V, 1, 1, 1, 1, 0, 704, 100
47557, V, 1, 1, 1, 1, 0, 704, 100
47558, V, 1, 1, 1, 1, 0, 704, 100
47559, V, 1, 1, 1, 1, 0, 704, 100
47560, V, 1, 1, 1, 1, 0, 704, 100
47561, V, 1, 1, 1, 1, 0, 704, 100
47562, V, 1, 1, 1, 1, 0, 704, 100
47563, V, 1, 1, 1, 1, 0, 704, 100
47564, V, 1, 1, 1, 1, 0, 704, 100
47565, V, 1, 1, 1, 1, 0, 704, 100
47566, V, 1, 1, 1, 1, 0, 704, 100
47567, V, 1, 1, 1, 1, 0, 704, 100
47568, V, 1, 1, 1, 1, 0, 704, 100
47569, V, 1, 1, 1, 1, 0, 704, 100
47570, V, 1, 1, 1, 1, 0, 704, 100
47571, V, 1, 1, 1, 1, 0, 704, 100
47572, V, 1, 1, 1, 1, 0, 704, 100
47574, V, 1, 1, 1, 1, 0, 704, 100
47575, V, 1, 1, 1, 1, 0, 704, 100
47576, V, 1, 1, 1, 1, 0, 704, 100
47577, V, 1, 1, 1, 1, 0, 704, 100
47578, V, 1, 1, 1, 1, 0, 704, 100
47579, V, 1, 1, 1, 1, 0, 704, 100
47580, V, 1, 1, 1, 1, 0, 704, 100
47581, V, 1, 1, 1, 1, 0, 704, 100
47582, V, 1, 1, 1, 1, 0, 704, 100
47583, V, 1, 1, 1, 1, 0, 704, 100
47584, V, 1, 1, 1, 1, 0, 704, 100
47585, V, 1, 1, 1, 1, 0, 704, 100
47586, V, 1, 1, 1, 1, 0, 704, 100
47587, V, 1, 1, 1, 1, 0, 704, 100
47588, V, 1, 1, 1, 1, 0, 704, 100
47589, V, 1, 1, 1, 1, 0, 704, 100
47590, V, 1, 1, 1, 1, 0, 704, 100
47591, V, 1, 1, 1, 1, 0, 704, 100
47592, V, 1, 1, 1, 1, 0, 704, 100
47593, V, 1, 1, 1, 1, 0, 704, 100
47594, V, 1, 1, 1, 1, 0, 704, 100
47595, V, 1, 1, 1, 1, 0, 704, 100
47596, V, 1, 1, 1, 1, 0, 704, 100
47597, V, 1, 1, 1, 1, 0, 704, 100
47598, V, 1, 1, 1, 1, 0, 704, 100
47599, V, 1, 1, 1, 1, 0, 704, 100
47600, V, 1, 1, 1, 1, 0, 704, 100
47601, V, 1, 1, 1, 1, 0, 704, 100
47602, V, 1, 1, 1, 1, 0, 704, 100
47603, V, 1, 1, 1, 1, 0, 704, 100
47604, V, 1, 1, 1, 1, 0, 704, 100
47605, V, 1, 1, 1, 1, 0, 704, 100
47606, V, 1, 1, 1, 1, 0, 704, 100
47607, V, 1, 1, 1, 1, 0, 704, 100
47608, V, 1, 1, 1, 1, 0, 704, 100
47609, V, 1, 1, 1, 1, 0, 704, 100
47610, V, 1, 1, 1, 1, 0, 704, 100
47611, V, 1, 1, 1, 1, 0, 704, 100
47612, V, 1, 1, 1, 1, 0, 704, 100
47613, V, 1, 1, 1, 1, 0, 704, 100
47614, V, 1, 1, 1, 1, 0, 704, 100
47616, V, 1, 1, 1, 1, 0, 704, 100
47617, V, 1, 1, 1, 1, 0, 704, 100
47618, V, 1, 1, 1, 1, 0, 704, 100
47619, V, 1, 1, 1, 1, 0, 704, 100
47620, V, 1, 1, 1, 1, 0, 704, 100
47621, V, 1, 1, 1, 1, 0, 704, 100
47622, V, 1, 1, 1, 1, 0, 704, 100
47623, V, 1, 1, 1, 1, 0, 704, 100
47624, V, 1, 1, 1, 1, 0, 704, 100
47625, V, 1, 1, 1, 1, 0, 704, 100
47626, V, 1, 1, 1, 1, 0, 704, 100
47627, V, 1, 1, 1, 1, 0, 704, 100
47628, V, 1, 1, 1, 1, 0, 704, 100
47629, V, 1, 1, 1, 1, 0, 704, 100
47630, V, 1, 1, 1, 1, 0, 704, 100
47631, V, 1, 1, 1, 1, 0, 704, 100
47632, V, 1, 1, 1, 1, 0, 704, 100
47633, V, 1, 1, 1, 1, 0, 704, 100
47634, V, 1, 1, 1, 1, 0, 704, 100
47635, V, 1, 1, 1, 1, 0, 704, 100
47636, V, 1, 1, 1, 1, 0, 704, 100
47637, V, 1, 1, 1, 1, 0, 704, 100
47638, V, 1, 1, 1, 1, 0, 704, 100
47639, V, 1, 1, 1, 1, 0, 704, 100
47640, V, 1, 1, 1, 1, 0, 704, 100
47641, V, 1, 1, 1, 1, 0, 704, 100
47642, V, 1, 1, 1, 1, 0, 704, 100
47643, V, 1, 1, 1, 1, 0, 704, 100
47644, V, 1, 1, 1, 1, 0, 704, 100
47645, V, 1, 1, 1, 1, 0, 704, 100
47646, V, 1, 1, 1, 1, 0, 704, 100
47647, V, 1, 1, 1, 1, 0, 704, 100
47648, V, 1, 1, 1, 1, 0, 704, 100
47649, V, 1, 1, 1, 1, 0, 704, 100
47650, V, 1, 1, 1, 1, 0, 704, 100
47651, V, 1, 1, 1, 1, 0, 704, 100
47652, V, 1, 1, 1, 1, 0, 704, 100
47653, V, 1, 1, 1, 1, 0, 704, 100
47654, V, 1, 1, 1, 1, 0, 704, 100
47655, V, 1, 1, 1, 1, 0, 704, 100
47656, V, 1, 1, 1, 1, 0, 704, 100
47657, V, 1, 1, 1, 1, 0, 704, 100
47659, V, 1, 1, 1, 1, 0, 704, 100
47660, V, 1, 1, 1, 1, 0, 704, 100
47661, V, 1, 1, 1, 1, 0, 704, 100
47662, V, 1, 1, 1, 1, 0, 704, 100
47663, V, 1, 1, 1, 1, 0, 704, 100
47664, V, 1, 1, 1, 1, 0, 704, 100
47665, V, 1, 1, 1, 1, 0, 704, 100
47666, V, 1, 1, 1, 1, 0, 704, 100
47667, V, 1, 1, 1, 1, 0, 704, 100
47668, V, 1, 1, 1, 1, 0, 704, 100
47669, V, 1, 1, 1, 1, 0, 704, 100
47670, V, 1, 1, 1, 1, 0, 704, 100
47671, V, 1, 1, 1, 1, 0, 704, 100
47672, V, 1, 1, 1, 1, 0, 704, 100
47673, V, 1, 1, 1, 1, 0, 704, 100
47674, V, 1, 1, 1, 1, 0, 704, 100
47675, V, 1, 1, 1, 1, 0, 704, 100
47676, V, 1, 1, 1, 1, 0, 704, 100
47677, V, 1, 1, 1, 1, 0, 704, 100
47678, V, 1, 1, 1, 1, 0, 704, 100
47679, V, 1, 1, 1, 1, 0, 704, 100
47680, V, 1, 1, 1, 1, 0, 704, 100
47681, V, 1, 1, 1, 1, 0, 704, 100
47682, V, 1, 1, 1, 1, 0, 704, 100
47683, V, 1, 1, 1, 1, 0, 704, 100
47684, V, 1, 1, 1, 1, 0, 704, 100
47685, V, 1, 1, 1, 1, 0, 704, 100
47686, V, 1, 1, 1, 1, 0, 704, 100
47687, V, 1, 1, 1, 1, 0, 704, 100
47688, V, 1, 1, 1, 1, 0, 704, 100
47689, V, 1, 1, 1, 1, 0, 704, 100
47690, V, 1, 1, 1, 1, 0, 704, 100
47691, V, 1, 1, 1, 1, 0, 704, 100
47692, V, 1, 1, 1, 1, 0, 704, 100
47693, V, 1, 1, 1, 1, 0, 704, 100
47694, V, 1, 1, 1, 1, 0, 704, 100
47695, V, 1, 1, 1, 1, 0, 704, 100
47696, V, 1, 1, 1, 1, 0, 704, 100
47697, V, 1, 1, 1, 1, 0, 704, 100
47698, V, 1, 1, 1, 1, 0, 704, 100
47699, V, 1, 1, 1, 1, 0, 704, 100
47700, V, 1, 1, 1, 1, 0, 704, 100
47702, V, 1, 1, 1, 1, 0, 704, 100
47703, V, 1, 1, 1, 1, 0, 704, 100
47704, V, 1, 1, 1, 1, 0, 704, 100
47705, V, 1, 1, 1, 1, 0, 704, 100
47706, V, 1, 1, 1, 1, 0, 704, 100
47707, V, 1, 1, 1, 1, 0, 704, 100
47708, V, 1, 1, 1, 1, 0, 704, 100
47709, V, 1, 1, 1, 1, 0, 704, 100
47710, V, 1, 1, 1, 1, 0, 704, 100
47711, V, 1, 1, 1, 1, 0, 704, 100
47712, V, 1, 1, 1, 1, 0, 704, 100
47713, V, 1, 1, 1, 1, 0, 704, 100
47714, V, 1, 1, 1, 1, 0, 704, 100
47715, V, 1, 1, 1, 1, 0, 704, 100
47716, V, 1, 1, 1, 1, 0, 704, 100
47717, V, 1, 1, 1, 1, 0, 704, 100
47718, V, 1, 1, 1, 1, 0, 704, 100
47719, V, 1, 1, 1, 1, 0, 704, 100
47720, V, 1, 1, 1, 1, 0, 704, 100
47721, V, 1, 1, 1, 1, 0, 704, 100
47722, V, 1, 1, 1, 1, 0, 704, 100
47723, V, 1, 1, 1, 1, 0, 704, 100
47724, V, 1, 1, 1, 1, 0, 704, 100
47725, V, 1, 1, 1, 1, 0, 704, 100
47726, V, 1, 1, 1, 1, 0, 704, 100
47727, V, 1, 1, 1, 1, 0, 704, 100
47728, V, 1, 1, 1, 1, 0, 704, 100
47729, V, 1, 1, 1, 1, 0, 704, 100
47730, V, 0, 1, 0, 0, 0, 704, 100
47750, V, 0, 0, 0, 0, 0, 704, 99
47855, V, 0, 0, 0, 0, 0, 704, 57
47855, V, 0, 0, 0, 0, 0, 704, 57
48112, V, 0, 0, 0, 0, 0, 704, 51
48112, V, 0, 0, 0, 0, 0, 704, 51
48369, V, 0, 0, 0, 0, 0, 704, 51
48369, V, 0, 0, 0, 0, 0, 704, 51
48626, V, 0, 0, 0, 0, 0, 704, 51
48626, V, 0, 0, 0, 0, 0, 704, 51
48883, V, 0, 0, 0, 0, 0, 704, 51
48883, V, 0, 0, 0, 0, 0, 704, 51
49140, V, 0, 0, 0, 0, 0, 704, 52
49140, V, 0, 0, 0, 0, 0, 704, 52
49397, V, 0, 0, 0, 0, 0, 704, 52
49397, V, 0, 0, 0, 0, 0, 704, 52
49654, V, 0, 0, 0, 0, 0, 704, 52
49654, V, 0, 0, 0, 0, 0, 704, 52
49911, V, 0, 0, 0, 0, 0, 704, 52
49911, V, 0, 0, 0, 0, 0, 704, 52
50168, V, 0, 0, 0, 0, 0, 704, 52
50168, V, 0, 0, 0, 0, 0, 704, 52
50425, V, 0, 0, 0, 0, 0, 704, 52
50425, V, 0, 0, 0, 0, 0, 704, 52
50682, V, 0, 0, 0, 0, 0, 704, 52
50682, V, 0, 0, 0, 0, 0, 704, 52
50939, V, 0, 0, 0, 0, 0, 704, 52
50939, V, 0, 0, 0, 0, 0, 704, 52
51196, V, 0, 0, 0, 0, 0, 704, 52
51196, V, 0, 0, 0, 0, 0, 704, 52
51453, V, 0, 0, 0, 0, 0, 704, 52
51453, V, 0, 0, 0, 0, 0, 704, 52
51710, V, 0, 0, 0, 0, 0, 704, 52
51710, V, 0, 0, 0, 0, 0, 704, 52
51968, V, 0, 0, 0, 0, 0, 704, 52
51968, V, 0, 0, 0, 0, 0, 704, 52
52225, V, 0, 0, 0, 0, 0, 704, 52
52225, V, 0, 0, 0, 0, 0, 704, 52
52482, V, 0, 0, 0, 0, 0, 704, 52
52482, V, 0, 0, 0, 0, 0, 704, 52
52739, V, 0, 0, 0, 0, 0, 704, 52
52739, V, 0, 0, 0, 0, 0, 704, 52
52996, V, 0, 0, 0, 0, 0, 704, 52
52996, V, 0, 0, 0, 0, 0, 704, 52
53253, V, 0, 0, 0, 0, 0, 704, 52
53253, V, 0, 0, 0, 0, 0, 704, 52
53510, V, 0, 0, 0, 0, 0, 704, 52
53510, V, 0, 0, 0, 0, 0, 704, 52
53767, V, 0, 0, 0, 0, 0, 704, 52
53767, V, 0, 0, 0, 0, 0, 704, 52
54024, V, 0, 0, 0, 0, 0, 704, 52
54024, V, 0, 0, 0, 0, 0, 704, 52
54281, V, 0, 0, 0, 0, 0, 704, 52
54281, V, 0, 0, 0, 0, 0, 704, 52
54538, V, 0, 0, 0, 0, 0, 704, 52
54538, V, 0, 0, 0, 0, 0, 704, 52
54795, V, 0, 0, 0, 0, 0, 704, 52
54795, V, 0, 0, 0, 0, 0, 704, 52
55052, V, 0, 0, 0, 0, 0, 704, 52
55052, V, 0, 0, 0, 0, 0, 704, 52
55309, V, 0, 0, 0, 0, 0, 704, 52
55309, V, 0, 0, 0, 0, 0, 704, 52
55566, V, 0, 0, 0, 0, 0, 704, 52
55566, V, 0, 0, 0, 0, 0, 704, 52
55823, V, 0, 0, 0, 0, 0, 704, 52
55823, V, 0, 0, 0, 0, 0, 704, 52
56080, V, 0, 0, 0, 0, 0, 704, 52
56080, V, 0, 0, 0, 0, 0, 704, 52
56337, V, 0, 0, 0, 0, 0, 704, 52
56337, V, 0, 0, 0, 0, 0, 704, 52
56594, V, 0, 0, 0, 0, 0, 704, 52
56594, V, 0, 0, 0, 0, 0, 704, 52
56851, V, 0, 0, 0, 0, 0, 704, 52
56851, V, 0, 0, 0, 0, 0, 704, 52
57108, V, 0, 0, 0, 0, 0, 704, 52
57108, V, 0, 0, 0, 0, 0, 704, 52
57365, V, 0, 0, 0, 0, 0, 704, 52
57365, V, 0, 0, 0, 0, 0, 704, 52
57622, V, 0, 0, 0, 0, 0, 704, 52
57622, V, 0, 0, 0, 0, 0, 704, 52
57879, V, 0, 0, 0, 0, 0, 704, 52
57879, V, 0, 0, 0, 0, 0, 704, 52
58136, V, 0, 0, 0, 0, 0, 704, 52
58136, V, 0, 0, 0, 0, 0, 704, 52
58393, V, 0, 0, 0, 0, 0, 704, 52
58393, V, 0, 0, 0, 0, 0, 704, 52
58650, V, 0, 0, 0, 0, 0, 704, 52
58650, V, 0, 0, 0, 0, 0, 704, 52
58907, V, 0, 0, 0, 0, 0, 704, 52
58907, V, 0, 0, 0, 0, 0, 704, 52
59164, V, 0, 0, 0, 0, 0, 704, 52
59164, V, 0, 0, 0, 0, 0, 704, 52
59421, V, 0, 0, 0, 0, 0, 704, 52
59421, V, 0, 0, 0, 0, 0, 704, 52
59678, V, 0, 0, 0, 0, 0, 704, 52
59678, V, 0, 0, 0, 0, 0, 704, 52
59935, V, 0, 0, 0, 0, 0, 704, 52
59935, V, 0, 0, 0, 0, 0, 704, 52
60192, V, 0, 0, 0, 0, 0, 704, 52
60192, V, 0, 0, 0, 0, 0, 704, 52
60449, V, 0, 0, 0, 0, 0, 704, 52
60449, V, 0, 0, 0, 0, 0, 704, 52
60706, V, 0, 0, 0, 0, 0, 704, 52
60706, V, 0, 0, 0, 0, 0, 704, 52
60963, V, 0, 0, 0, 0, 0, 704, 52
60963, V, 0, 0, 0, 0, 0, 704, 52
61220, V, 0, 0, 0, 0, 0, 704, 52
61220, V, 0, 0, 0, 0, 0, 704, 52
61477, V, 0, 0, 0, 0, 0, 704, 52
61477, V, 0, 0, 0, 0, 0, 704, 52
61734, V, 0, 0, 0, 0, 0, 704, 52
61734, V, 0, 0, 0, 0, 0, 704, 52
61991, V, 0, 0, 0, 0, 0, 704, 52
61991, V, 0, 0, 0, 0, 0, 704, 52
62248, V, 0, 0, 0, 0, 0, 704, 52
62248, V, 0, 0, 0, 0, 0, 704, 52
62505, V, 0, 0, 0, 0, 0, 704, 52
62505, V, 0, 0, 0, 0, 0, 704, 52
62763, V, 0, 0, 0, 0, 0, 704, 52
62763, V, 0, 0, 0, 0, 0, 704, 52
63020, V, 0, 0, 0, 0, 0, 704, 52
63020, V, 0, 0, 0, 0, 0, 704, 52
63277, V, 0, 0, 0, 0, 0, 704, 52
63277, V, 0, 0, 0, 0, 0, 704, 52
63534, V, 0, 0, 0, 0, 0, 704, 52
63534, V, 0, 0, 0, 0, 0, 704, 52
63791, V, 0, 0, 0, 0, 0, 704, 52
63791, V, 0, 0, 0, 0, 0, 704, 52
64048, V, 0, 0, 0, 0, 0, 704, 52
64048, V, 0, 0, 0, 0, 0, 704, 52
64305, V, 0, 0, 0, 0, 0, 704, 52
64305, V, 0, 0, 0, 0, 0, 704, 52
64562, V, 0, 0, 0, 0, 0, 704, 52
64562, V, 0, 0, 0, 0, 0, 704, 52
64819, V, 0, 0, 0, 0, 0, 704, 52
64819, V, 0, 0, 0, 0, 0, 704, 52
65076, V, 0, 0, 0, 0, 0, 704, 52
65076, V, 0, 0, 0, 0, 0, 704, 52
65333, V, 0, 0, 0, 0, 0, 704, 52
65333, V, 0, 0, 0, 0, 0, 704, 52
54, V, 0, 0, 0, 0, 0, 704, 52
54, V, 0, 0, 0, 0, 0, 704, 52
311, V, 0, 0, 0, 0, 0, 704, 52
311, V, 0, 0, 0, 0, 0, 704, 52
568, V, 0, 0, 0, 0, 0, 704, 52
568, V, 0, 0, 0, 0, 0, 704, 52
825, V, 0, 0, 0, 0, 0, 704, 52
825, V, 0, 0, 0, 0, 0, 704, 52
1082, V, 0, 0, 0, 0, 0, 704, 52
1082, V, 0, 0, 0, 0, 0, 704, 52
1339, V, 0, 0, 0, 0, 0, 704, 52
1339, V, 0, 0, 0, 0, 0, 704, 52
1596, V, 0, 0, 0, 0, 0, 704, 52
1596, V, 0, 0, 0, 0, 0, 704, 52
1853, V, 0, 0, 0, 0, 0, 704, 52
1853, V, 0, 0, 0, 0, 0, 704, 52
2110, V, 0, 0, 0, 0, 0, 704, 52
2110, V, 0, 0, 0, 0, 0, 704, 52
2367, V, 0, 0, 0, 0, 0, 704, 52
2367, V, 0, 0, 0, 0, 0, 704, 52
2624, V, 0, 0, 0, 0, 0, 704, 52
2624, V, 0, 0, 0, 0, 0, 704, 52
2881, V, 0, 0, 0, 0, 0, 704, 52
2881, V, 0, 0, 0, 0, 0, 704, 52
3138, V, 0, 0, 0, 0, 0, 704, 52
3138, V, 0, 0, 0, 0, 0, 704, 52
3395, V, 0, 0, 0, 0, 0, 704, 52
3395, V, 0, 0, 0, 0, 0, 704, 52
3652, V, 0, 0, 0, 0, 0, 704, 52
3652, V, 0, 0, 0, 0, 0, 704, 52
3909, V, 0, 0, 0, 0, 0, 704, 52
3909, V, 0, 0, 0, 0, 0, 704, 52
4166, V, 0, 0, 0, 0, 0, 704, 52
4166, V, 0, 0, 0, 0, 0, 704, 52
4423, V, 0, 0, 0, 0, 0, 704, 52
4423, V, 0, 0, 0, 0, 0, 704, 52
4680, V, 0, 0, 0, 0, 0, 704, 52
4680, V, 0, 0, 0, 0, 0, 704, 52
4937, V, 0, 0, 0, 0, 0, 704, 52
4937, V, 0, 0, 0, 0, 0, 704, 52
5194, V, 0, 0, 0, 0, 0, 704, 52
5194, V, 0, 0, 0, 0, 0, 704, 52
5451, V, 0, 0, 0, 0, 0, 704, 52
5451, V, 0, 0, 0, 0, 0, 704, 52
5708, V, 0, 0, 0, 0, 0, 704, 52
5708, V, 0, 0, 0, 0, 0, 704, 52
5965, V, 0, 0, 0, 0, 0, 704, 52
5965, V, 0, 0, 0, 0, 0, 704, 52
6222, V, 0, 0, 0, 0, 0, 704, 52
6222, V, 0, 0, 0, 0, 0, 704, 52
6479, V, 0, 0, 0, 0, 0, 704, 52
6479, V, 0, 0, 0, 0, 0, 704, 52